Solar cell and method for manufacturing the same

The solar cell design with recessed and convex portions and selective electron passage enhances light absorption and reduces reflection, improving power generation capacity.

CN117276372BActive Publication Date: 2024-12-06HUAIAN JIETAI NEW ENERGY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311175162.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-09-12
Publication Date
2024-12-06
Estimated Expiration
2043-09-12

AI Technical Summary

Technical Problem

The power generation capacity of existing solar cells is limited due to the blocking effect of grid lines on the light-collecting surface, which restricts the area available for light absorption.

Method used

A solar cell structure featuring a P-type boron diffusion layer, PN junction layer, and N-type silicon base layer with recessed and convex portions, along with a tunneling layer that allows only electron passage, enhancing light absorption area and incorporating anti-reflection and passivation layers to improve efficiency.

Benefits of technology

The novel structure increases the light-receiving area and reduces light reflection, thereby enhancing the power generation capacity of the solar cell.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117276372B_ABST
    Figure CN117276372B_ABST
Patent Text Reader

Abstract

The present invention discloses a solar cell and a preparation method thereof. The disclosed solar cell comprises a P-type boron diffusion layer, a PN junction layer, an N-type silicon base layer, a tunneling layer and an electron gathering layer stacked in sequence. The N-type silicon base layer has a first concave portion, and the region of the PN junction layer opposite to the first concave portion has a first convex portion and a second concave portion, the first convex portion and the second concave portion are located on opposite sides of the PN junction layer, and the first convex portion is located in the first concave portion. The region of the P-type boron diffusion layer opposite to the second concave portion has a second convex portion and a third concave portion, the second convex portion and the third concave portion are located on opposite sides of the P-type boron diffusion layer, and the second convex portion is located in the second concave portion; the side where the P-type boron diffusion layer is located is the light-facing side. The above scheme can solve the problem of low power generation capacity of solar cells in the related art.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of solar cells, and in particular to a solar cell and a preparation method thereof. Background Art

[0002] Solar cells are devices that directly convert light energy into electrical energy through the photoelectric effect or the photochemical effect. In the related art, the light-collecting surface of the solar cell is a planar structure, and grid lines (electrode structures) are arranged on the light-collecting surface. Since the area of ​​the light-collecting surface of the solar cell is limited, the arrangement of the grid lines will further block part of the light-collecting surface of the solar cell, thereby making the power generation capacity of the solar cell in the related art low, and unable to meet the increasingly high requirements of users for the power generation capacity of the solar cell. Summary of the invention

[0003] The invention discloses a solar cell and a preparation method thereof, so as to solve the problem of low power generation capacity of the solar cell in the related art.

[0004] In order to solve the above-mentioned technical problems, the present invention is achieved as follows:

[0005] In a first aspect, the present application discloses a solar cell, comprising a P-type boron diffusion layer, a PN junction layer, an N-type silicon base layer, a tunneling layer and an electron gathering layer stacked in sequence, wherein:

[0006] The N-type silicon-based layer has a first concave portion, the PN junction layer has a first convex portion and a second concave portion in an area opposite to the first concave portion, the first convex portion and the second concave portion are located on opposite sides of the PN junction layer, and the first convex portion is located in the first concave portion, the P-type boron diffusion layer has a second convex portion and a third concave portion in an area opposite to the second concave portion, the second convex portion and the third concave portion are located on opposite sides of the P-type boron diffusion layer, and the second convex portion is located in the second concave portion;

[0007] The side where the P-type boron diffusion layer is located is the light-facing side, and the tunneling layer is used for only allowing electrons to pass through.

[0008] In a second aspect, the present application further discloses a method for preparing a solar cell, wherein the solar cell is the solar cell described in the first aspect, and the preparation method comprises:

[0009] A groove is formed in the silicon body;

[0010] A boron diffusion process is performed on one side of the silicon body where the groove is opened, so that the silicon body forms a P-type boron diffusion layer, a PN junction layer and an N-type silicon base layer stacked in sequence, wherein the N-type silicon base layer forms a first recessed portion at a position corresponding to the groove, the PN junction layer forms a first convex portion and a second recessed portion at a position corresponding to the groove, and the P-type boron diffusion layer forms a second convex portion and a third recessed portion at a position corresponding to the groove;

[0011] Disposing a tunneling layer on a side of the N-type silicon-based layer away from the PN junction layer;

[0012] An electron gathering layer is arranged on a side of the tunneling layer away from the N-type silicon-based layer.

[0013] The technical solution adopted by the present invention can achieve the following technical effects:

[0014] The solar cell disclosed in the embodiment of the present application is configured such that an N-type silicon base layer has a first recessed portion, a PN junction layer has a first convex portion and a second recessed portion in an area opposite to the first recessed portion, the first convex portion and the second recessed portion are located on opposite sides of the PN junction layer, and the first convex portion is located in the first recessed portion, and a P-type boron diffusion layer has a second convex portion and a third recessed portion in an area opposite to the second recessed portion, the second convex portion and the third recessed portion are located on opposite sides of the P-type boron diffusion layer, and the second convex portion is located in the second recessed portion, so that the solar cell can increase the area for receiving light at the position of the third recessed portion relative to the solar cell using a planar structure in the related art, thereby improving the power generation capacity of the solar cell. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 A schematic diagram of the structure of a solar cell disclosed in an embodiment of the present invention;

[0016] Figure 2 The present invention is a flow chart of the preparation of a solar cell disclosed in an embodiment of the present invention.

[0017] Description of reference numerals:

[0018] 110-first electrode, 120-second electrode,

[0019] 130-P type boron diffusion layer, 131-second protrusion, 132-third depression,

[0020] 140-PN junction layer, 141-first convex portion, 142-second concave portion,

[0021] 150-N-type silicon base layer, 151-first recessed portion,

[0022] 160 - tunneling layer, 170 - electron gathering layer, 180 - passivation layer, 190 - first anti-reflection layer, 210 - second anti-reflection layer. DETAILED DESCRIPTION

[0023] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with the specific embodiments of the present invention and the corresponding drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0024] The technical solutions disclosed in various embodiments of the present invention are described in detail below in conjunction with the accompanying drawings.

[0025] Please refer to Figure 1 to Figure 2 An embodiment of the present invention discloses a solar cell, which includes a P-type boron diffusion layer 130, a PN junction layer 140, an N-type silicon base layer 150, a tunneling layer 160 and an electron gathering layer 170 stacked in sequence.

[0026] The P-type boron diffusion layer 130, the PN junction layer 140, and the N-type silicon base layer 150 can be formed by performing a boron diffusion process on the silicon body, so that the silicon body forms a sequentially stacked P-type boron diffusion layer 130, a PN junction layer 140, and an N-type silicon base layer 150, and the P-type boron diffusion layer 130, the PN junction layer 140, and the N-type silicon base layer 150 are an integrated structure. It should be noted that the N-type silicon base layer 150 is a phosphorus-containing layer. When the P-type boron diffusion layer 130 is exposed to light, the electrons of the boron atoms in the P-type boron diffusion layer 130 are unstable, so that the electrons can pass through the PN junction layer 140 and the N-type silicon base layer 150, and then pass through the tunneling layer 160 to reach the electron gathering layer 170, wherein the tunneling layer 160 is only for electrons to pass through, and the holes that lose the electrons cannot pass through the tunneling layer 160. The tunneling layer 160 can be a SiO2 layer, and the principle of the tunneling layer 160 is a tunneling silicon oxide passivation contact technology, and only electrons can pass through, but holes cannot pass through. The electron gathering layer 170 may be a polysilicon layer (Poly silicon layer) formed by low pressure chemical vapor deposition (LPCVD) and then an N-type silicon layer formed by phosphorus diffusion.

[0027] The N-type silicon-based layer 150 has a first recessed portion 151 .

[0028] The region of the PN junction layer 140 opposite to the first recessed portion 151 has a first convex portion 141 and a second recessed portion 142 . The first convex portion 141 and the second recessed portion 142 are located on opposite sides of the PN junction layer 140 . The first convex portion 141 is located in the first recessed portion 151 .

[0029] The region of the P-type boron diffusion layer 130 opposite to the second recess 142 has a second protrusion 131 and a third recess 132 . The second protrusion 131 and the third recess 132 are located on opposite sides of the P-type boron diffusion layer 130 . The second protrusion 131 is located in the second recess 142 .

[0030] The side where the P-type boron diffusion layer 130 is located is the light-facing side. Light is used to be projected from one side of the P-type boron diffusion layer 130 to the solar cell, and the tunneling layer 160 is used to allow only electrons to pass through.

[0031] The solar cell disclosed in the embodiment of the present application is configured such that an N-type silicon base layer 150 has a first recessed portion 151, a region of the PN junction layer 140 opposite to the first recessed portion 151 has a first convex portion 141 and a second recessed portion 142, the first convex portion 141 and the second recessed portion 142 are located on opposite sides of the PN junction layer 140, and the first convex portion 141 is located in the first recessed portion 151, and a region of the P-type boron diffusion layer 130 opposite to the second recessed portion 142 has a second convex portion 131 and a third recessed portion 132, the second convex portion 131 and the third recessed portion 132 are located on opposite sides of the P-type boron diffusion layer 130, and the second convex portion 131 is located in the second recessed portion 142, so that the solar cell can increase the area for receiving light at the position of the third recessed portion 132 compared to the solar cell adopting a planar structure in the related art, thereby improving the power generation capacity of the solar cell.

[0032] In order to further improve the power generation capacity of the solar cell, optionally, the N-type silicon base layer 150 may have a plurality of first recessed portions 151, the PN junction layer 140 may have a plurality of first protruding portions 141 and a plurality of second recessed portions 142, and the P-type boron diffusion layer 130 may have a plurality of second protruding portions 131 and a plurality of third recessed portions 132. The plurality of first recessed portions 151, the plurality of first protruding portions 141, the plurality of second recessed portions 142, the plurality of second protruding portions 131, and the plurality of third recessed portions 132 may be arranged in one-to-one correspondence.

[0033] The solar cell disclosed in the embodiment of the present application can further improve the power generation capacity of the solar cell by providing a plurality of the first recessed portion 151, the first protruding portion 141, the second recessed portion 142, the second protruding portion 131 and the third recessed portion 132, and arranging them one by one.

[0034] In an optional embodiment, the solar cell further includes a first electrode 110 and a second electrode 120 , the first electrode 110 is disposed in at least a portion of the third recess 132 , and the first electrode 110 is electrically connected to the P-type boron diffusion layer 130 , and the second electrode 120 is electrically connected to the electron gathering layer 170 .

[0035] The solar cell disclosed in the embodiment of the present application can protect the first electrode 110 by arranging the first electrode 110 in the third recessed portion 132. Moreover, when the first electrode 110 is located in the third recessed portion 132 and electrically connected to the P-type boron diffusion layer 130, compared with the first electrode 110 being directly electrically connected to the planar structure, it is beneficial to increase the contact area between the first electrode 110 and the P-type boron diffusion layer 130, thereby facilitating the stability of the electrical connection of the first electrode 110.

[0036] In order to further improve the power generation capacity of the solar cell, optionally, the surface of the P-type boron diffusion layer 130 on the side away from the PN junction layer 140 may have a plurality of anti-reflection protrusions arranged at intervals.

[0037] Specifically, the anti-reflection protrusion can be a triangular structure formed by performing a texturing process on the surface of the P-type boron diffusion layer 130 on the side away from the PN junction layer 140. The anti-reflection protrusion on the surface of the P-type boron diffusion layer 130 on the side away from the PN junction layer 140 forms a velvet structure layer, which can reduce the reflection of light.

[0038] The solar cell disclosed in the embodiment of the present application is configured with a plurality of spaced anti-reflection convex portions on the surface of the P-type boron diffusion layer 130 on the side away from the PN junction layer 140, so that the surface of the P-type boron diffusion layer 130 on the side away from the PN junction layer 140 forms a rough structure, thereby reducing the reflection of light by the P-type boron diffusion layer 130, and further improving the power generation capacity of the solar cell.

[0039] In order to reduce the problem that the electrons and holes of the solar cell are recombined on the surface of the P-type boron diffusion layer 130 and affect the power generation capacity of the solar cell, the solar cell may further include a passivation layer 180, which may be an aluminum oxide layer. The passivation layer 180 may be disposed on the side of the P-type boron diffusion layer 130 away from the PN junction layer 140, and the side of the passivation layer 180 facing the P-type boron diffusion layer 130 may have a plurality of anti-reflection concave portions arranged at intervals, and the plurality of anti-reflection convex portions are correspondingly disposed in the plurality of anti-reflection concave portions.

[0040] The solar cell disclosed in the embodiment of the present application is provided with a passivation layer 180 on the side of the P-type boron diffusion layer 130 away from the PN junction layer 140, thereby reducing the recombination of electrons and holes of the solar cell on the surface of the P-type boron diffusion layer 130, thereby alleviating the impact on the power generation capacity of the solar cell. In addition, a plurality of anti-reflection concave portions arranged at intervals are provided on the side of the passivation layer 180 facing the P-type boron diffusion layer 130, so that a plurality of anti-reflection convex portions are correspondingly arranged in the plurality of anti-reflection concave portions, thereby further reducing the reflection of light, and the passivation layer 180 and the P-type boron diffusion layer 130 are more stably connected through the coordination of the anti-reflection concave portions and the anti-reflection convex portions.

[0041] To further reduce the reflectivity of the solar cell to light, the solar cell may optionally further include a first anti-reflection layer 190, which may be disposed on a side of the P-type boron diffusion layer 130 away from the PN junction layer 140. Specifically, the first anti-reflection layer 190 may be a silicon nitride layer.

[0042] The solar cell disclosed in the embodiment of the present application can further reduce the solar cell's ability to reflect light by disposing a first anti-reflection layer 190 on the side of the P-type boron diffusion layer 130 that is away from the PN junction layer 140, thereby improving the solar cell's power generation capacity, and the first anti-reflection layer 190 can also protect the layers it covers.

[0043] In some cases, the side of the solar cell facing away from the light-facing side is also used for power generation. In order to reduce the light reflection on the side of the solar cell facing away from the light-facing side, the solar cell may further include a second anti-reflection layer 210. The second anti-reflection layer 210 may be disposed on the side of the electron collection layer 170 facing away from the tunneling layer 160. The second anti-reflection layer 210 may be a silicon nitride layer.

[0044] The solar cell disclosed in the embodiment of the present application can reduce light reflection on the side of the solar cell facing away from the light-facing side by disposing a second anti-reflection layer 210 on the side of the electron aggregation layer 170 facing away from the tunneling layer 160, thereby improving the power generation capacity of the solar cell. Moreover, the second anti-reflection layer 210 can also protect the layers it covers.

[0045] It should be noted that when preparing the first anti-reflection layer 190 and the second anti-reflection layer 210 of the solar cell, they can be prepared by a plasma enhanced chemical vapor deposition (PECVD) process.

[0046] The present application also discloses a method for preparing a solar cell. The disclosed solar cell is the solar cell disclosed in the above embodiment. The disclosed preparation method includes:

[0047] S101, a groove is formed on the silicon body.

[0048] It should be noted that the grooves on the silicon body can be formed by laser. Of course, the grooves can also be formed by chemical etching or laser.

[0049] S102 , performing a boron diffusion process on the side of the silicon body where the groove is formed, so that the silicon body forms a P-type boron diffusion layer 130 , a PN junction layer 140 and an N-type silicon base layer 150 stacked in sequence.

[0050] The N-type silicon base layer 150 forms a first recessed portion 151 at the position corresponding to the groove, the PN junction layer 140 forms a first protruding portion 141 and a second recessed portion 142 at the position corresponding to the groove, and the P-type boron diffusion layer 130 forms a second protruding portion 131 and a third recessed portion 132 at the position corresponding to the groove.

[0051] It should be noted that after the boron diffusion process is performed on the side of the silicon body with the groove to form the P-type boron diffusion layer 130 , the other part of the silicon body will automatically form the PN junction layer 140 and the N-type silicon base layer 150 .

[0052] S103 , a tunneling layer 160 is disposed on a side of the N-type silicon-based layer 150 away from the PN junction layer 140 .

[0053] Specifically, the tunneling layer 160 can be formed by low pressure chemical vapor deposition (LPCVD) and can be a SiO2 layer. The principle of the tunneling layer 160 is a tunneling silicon oxide passivation contact technology, where only electrons can pass through, but holes cannot.

[0054] S104 , an electron gathering layer 170 is disposed on a side of the tunneling layer 160 away from the N-type silicon-based layer 150 .

[0055] Specifically, the electron gathering layer 170 may be formed by forming a polysilicon layer (Poly silicon layer) through low pressure chemical vapor deposition (LPCVD), and then forming an N-type silicon layer through phosphorus diffusion.

[0056] The method for preparing a solar cell disclosed in the embodiment of the present application is to open a groove on a silicon body and perform a boron diffusion process on one side of the silicon body where the groove is opened, so that the silicon body forms a P-type boron diffusion layer 130, a PN junction layer 140 and an N-type silicon base layer 150 stacked in sequence, so that the N-type silicon base layer 150 forms a first recessed portion 151 at a position corresponding to the groove, the PN junction layer 140 forms a first convex portion 141 and a second concave portion 142 at a position corresponding to the groove, and the P-type boron diffusion layer 130 forms a second convex portion 131 and a third concave portion 132 at a position corresponding to the groove, the first convex portion 141 is located in the first concave portion 151, and the second convex portion 131 is located in the second concave portion 142, so that the solar cell can increase the area of ​​receiving light at the position of the third concave portion 132 compared with the solar cell adopting a planar structure in the related art, thereby improving the power generation capacity of the solar cell.

[0057] Optionally, the solar cell further includes a first electrode 110 and a second electrode 120 , the first electrode 110 is disposed in at least part of the third recess 132 , the first electrode 110 is electrically connected to the P-type boron diffusion layer 130 , and the second electrode 120 is electrically connected to the electron gathering layer 170 .

[0058] The disclosed preparation method also includes

[0059] S105 , disposing a first electrode 110 in at least a portion of the third recess 132 , and the first electrode 110 is electrically connected to the P-type boron diffusion layer 130 .

[0060] S106 , electrically connecting the second electrode 120 to the electron accumulation layer 170 .

[0061] The method for preparing a solar cell disclosed in the embodiment of the present application can protect the first electrode 110 by disposing the first electrode 110 in the third recess 132. Moreover, when the first electrode 110 is located in the third recess 132 and is electrically connected to the P-type boron diffusion layer 130, compared with the first electrode 110 being directly electrically connected to the planar structure, it is beneficial to increase the contact area between the first electrode 110 and the P-type boron diffusion layer 130, thereby facilitating the stability of the electrical connection of the first electrode 110.

[0062] In an achievable manner, before the first electrode 110 is disposed in at least a portion of the third recess 132 and the first electrode 110 is electrically connected to the P-type boron diffusion layer 130 , the disclosed preparation method may further include:

[0063] In step A, a laser process is performed on the bottom of the third recessed portion 132 where the first electrode 110 is disposed, so that the concentration of boron atoms in the bottom area of ​​the P-type boron diffusion layer 130 located in the third recessed portion 132 where the first electrode 110 is disposed is greater than the concentration of boron atoms in the bottom area of ​​the P-type boron diffusion layer 130 away from the third recessed portion 132.

[0064] It should be noted that when the laser process is performed on the bottom of the third recessed portion 132 , the temperature of the bottom of the third recessed portion 132 is increased, so that boron atoms can be gathered, thereby increasing the concentration of boron atoms.

[0065] The method for preparing a solar cell disclosed in the embodiment of the present application performs a laser process at the bottom of a third recessed portion 132 where a first electrode 110 is disposed, so that the concentration of boron atoms in the bottom region of the P-type boron diffusion layer 130 located in the third recessed portion 132 where the first electrode 110 is disposed is greater than the concentration of boron atoms in the bottom region of the P-type boron diffusion layer 130 away from the third recessed portion 132, thereby improving the power generation capacity of the solar cell.

[0066] Optionally, before performing the boron diffusion process on the side of the silicon body where the groove is formed, the disclosed preparation method may further include:

[0067] Step B: forming a plurality of anti-reflection protrusions arranged at intervals on the surface of the P-type boron diffusion layer 130 on the side away from the PN junction layer 140 by a texturing process.

[0068] The method for preparing a solar cell disclosed in an embodiment of the present application forms a rough structure on the surface of the P-type boron diffusion layer 130 on the side away from the PN junction layer 140 by arranging a plurality of spaced anti-reflection protrusions on the surface of the P-type boron diffusion layer 130 on the side away from the PN junction layer 140, thereby reducing the reflection of light by the P-type boron diffusion layer 130 and further improving the power generation capacity of the solar cell.

[0069] In order to reduce the problem that the electrons and holes of the solar cell are recombined on the surface of the P-type boron diffusion layer 130 and affect the power generation capacity of the solar cell, the disclosed preparation method may optionally further include:

[0070] Step C: disposing a passivation layer 180 on a side of the P-type boron diffusion layer 130 away from the PN junction layer 140 .

[0071] The passivation layer 180 covers the anti-reflection convex portions and fills the gaps between the plurality of anti-reflection convex portions, and the region of the passivation layer 180 corresponding to the plurality of anti-reflection convex portions forms an anti-reflection concave portion. The passivation layer 180 may be an aluminum oxide layer.

[0072] The method for preparing a solar cell disclosed in the embodiment of the present application can reduce the recombination of electrons and holes of the solar cell on the surface of the P-type boron diffusion layer 130 by setting a passivation layer 180 on the side of the P-type boron diffusion layer 130 away from the PN junction layer 140, thereby alleviating the impact on the power generation capacity of the solar cell.

[0073] Optionally, the method for preparing a solar cell disclosed in the present application may further include:

[0074] Step D: disposing a first anti-reflection layer 190 on a side of the P-type boron diffusion layer 130 away from the PN junction layer 140 .

[0075] The first anti-reflection layer 190 may be a silicon nitride layer.

[0076] The method for preparing a solar cell disclosed in the embodiment of the present application can further reduce the solar cell's ability to reflect light by setting a first anti-reflection layer 190 on the side of the P-type boron diffusion layer 130 that is away from the PN junction layer 140, thereby improving the solar cell's power generation capacity, and the first anti-reflection layer 190 can also protect the layers it covers.

[0077] Optionally, the method for preparing a solar cell disclosed in the present application may further include:

[0078] Step E: disposing a second anti-reflection layer 210 on the side of the electron gathering layer 170 facing away from the tunneling layer 160 .

[0079] The second anti-reflection layer 210 may be a silicon nitride layer.

[0080] The method for preparing a solar cell disclosed in the embodiment of the present application can reduce light reflection on the side of the solar cell facing away from the light-facing side by setting a second anti-reflection layer 210 on the side of the electron aggregation layer 170 facing away from the tunneling layer 160, thereby improving the power generation capacity of the solar cell. Moreover, the second anti-reflection layer 210 can also protect the layers it covers.

[0081] It should be noted that when preparing the first anti-reflection layer 190 and the second anti-reflection layer 210 of the solar cell, they can be prepared by a plasma enhanced chemical vapor deposition (PECVD) process.

[0082] The above embodiments of the present invention focus on the differences between the various embodiments. As long as the different optimization features between the various embodiments are not contradictory, they can be combined to form a better embodiment. Considering the simplicity of the text, they will not be repeated here.

[0083] The embodiments of the present invention are described above in conjunction with the accompanying drawings, but the present invention is not limited to the above-mentioned specific implementation modes, which are merely illustrative rather than restrictive. Under the guidance of the present invention, ordinary technicians in this field can also make many forms without departing from the scope of protection of the present invention and the claims, all of which are within the protection of the present invention.

Claims

1. A solar cell, characterized in that: The invention comprises a P-type boron diffusion layer (130), a PN junction layer (140), an N-type silicon base layer (150), a tunneling layer (160) and an electron gathering layer (170) which are stacked in sequence, wherein: The N-type silicon-based layer (150) has a first recessed portion (151); a region of the PN junction layer (140) opposite to the first recessed portion (151) has a first protruding portion (141) and a second recessed portion (142); the first protruding portion (141) and the second recessed portion (142) are located on opposite sides of the PN junction layer (140); the first protruding portion (141) is located in the first recessed portion (151); a region of the P-type boron diffusion layer (130) opposite to the second recessed portion (142) has a second protruding portion (131) and a third recessed portion (132); the second protruding portion (131) and the third recessed portion (132) are located on opposite sides of the P-type boron diffusion layer (130); and the second protruding portion (131) is located in the second recessed portion (142); The side where the P-type boron diffusion layer (130) is located is the light-facing side, and the tunneling layer (160) is used to allow only electrons to pass through; The surface of the P-type boron diffusion layer (130) on the side away from the PN junction layer (140) has a plurality of anti-reflection convex portions arranged at intervals; The solar cell further comprises a passivation layer (180), the passivation layer (180) being arranged on a side of the P-type boron diffusion layer (130) away from the PN junction layer (140), the side of the passivation layer (180) facing the P-type boron diffusion layer (130) comprising a plurality of anti-reflection concave portions arranged at intervals, and the plurality of anti-reflection convex portions being correspondingly arranged in the plurality of anti-reflection concave portions; The solar cell further comprises a first anti-reflection layer (190), wherein the first anti-reflection layer (190) is arranged on a side of the P-type boron diffusion layer (130) away from the PN junction layer (140); The N-type silicon-based layer (150) has a plurality of the first recessed portions (151), the PN junction layer (140) has a plurality of the first protruding portions (141) and a plurality of the second recessed portions (142), the P-type boron diffusion layer (130) has a plurality of the second protruding portions (131) and a plurality of the third recessed portions (132), and the plurality of the first recessed portions (151), the plurality of the first protruding portions (141), the plurality of the second recessed portions (142), the plurality of the second protruding portions (131) and the plurality of the third recessed portions (132) are arranged in a one-to-one correspondence; The solar cell further comprises a first electrode (110) and a second electrode (120), the first electrode (110) being disposed in at least a portion of the third recessed portion (132), the first electrode (110) being electrically connected to the P-type boron diffusion layer (130), and the second electrode (120) being electrically connected to the electron gathering layer (170); The concentration of boron atoms in the P-type boron diffusion layer (130) located in the bottom region of the third recessed portion (132) where the first electrode (110) is provided is greater than the concentration of boron atoms in the bottom region of the P-type boron diffusion layer (130) away from the third recessed portion (132); The solar cell further comprises a second anti-reflection layer (210), wherein the second anti-reflection layer (210) is arranged on a side of the electron gathering layer (170) away from the tunneling layer (160).

2. A method for preparing a solar cell, characterized in that: The solar cell is the solar cell according to claim 1, and the preparation method comprises: A groove is formed in the silicon body; A boron diffusion process is performed on the side of the silicon body where the groove is opened, so that the silicon body forms a P-type boron diffusion layer (130), a PN junction layer (140) and an N-type silicon base layer (150) stacked in sequence, wherein the N-type silicon base layer (150) forms a first recessed portion (151) at a position corresponding to the groove, the PN junction layer (140) forms a first protruding portion (141) and a second recessed portion (142) at a position corresponding to the groove, and the P-type boron diffusion layer (130) forms a second protruding portion (131) and a third recessed portion (132) at a position corresponding to the groove; A tunneling layer (160) is provided on a side of the N-type silicon-based layer (150) away from the PN junction layer (140); An electron gathering layer (170) is disposed on a side of the tunneling layer (160) that is away from the N-type silicon-based layer (150).

3. The preparation method according to claim 2, characterized in that: The solar cell further comprises a first electrode (110) and a second electrode (120); the N-type silicon-based layer (150) has a plurality of the first recessed portions (151); the PN junction layer (140) has a plurality of the first protruding portions (141) and a plurality of the second recessed portions (142); the P-type boron diffusion layer (130) has a plurality of the second protruding portions (131) and a plurality of the third recessed portions (132); the plurality of the first recessed portions (151), the plurality of the first protruding portions (141), the plurality of the second recessed portions (142), the plurality of the second protruding portions (131) and the plurality of the third recessed portions (132) are arranged in a one-to-one correspondence; The preparation method further comprises: The first electrode (110) is disposed in at least a portion of the third recessed portion (132), and the first electrode (110) is electrically connected to the P-type boron diffusion layer (130); The second electrode (120) is electrically connected to the electron gathering layer (170).

4. The preparation method according to claim 3, characterized in that: Before the first electrode (110) is arranged in at least a portion of the third recessed portion (132), and the first electrode (110) is electrically connected to the P-type boron diffusion layer (130), the preparation method further comprises: A laser process is performed on the bottom of the third recessed portion (132) where the first electrode (110) is disposed, so that the concentration of boron atoms in the P-type boron diffusion layer (130) located in the bottom region of the third recessed portion (132) where the first electrode (110) is disposed is greater than the concentration of boron atoms in the bottom region of the P-type boron diffusion layer (130) away from the third recessed portion (132).

5. The preparation method according to claim 2, characterized in that: Before performing a boron diffusion process on the side of the silicon body where the groove is formed, the preparation method further comprises: A plurality of anti-reflection convex portions arranged at intervals are formed on the surface of the P-type boron diffusion layer (130) on the side away from the PN junction layer (140) by a texturing process.