Method for detecting surface cracks of workpieces using magnetic suspension
Through magnetic suspension detection method, magnetic traces are used to form and detect cracks on the surface of special alloys, which solves the problems of low efficiency, high cost and environmental pollution in the existing technology, and realizes simple, efficient and economical crack detection, which is suitable for a variety of non-infrastructured non-consistencies. Magnetic material.
Patent Information
- Application Number
- CN202311742314.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-18
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2043-12-18
AI Technical Summary
The prior art is difficult to effectively detect surface cracks of special alloys, especially non-ferromagnetic materials and products with small production volume. The traditional methods are inefficient, costly, polluted the environment and have high leakage detection rate, which cannot meet high quality requirements.
Using magnetic suspension detection method, magnetic suspension is prepared by mixing magnetic powder with kerosene, spraying and immersing the surface of the workpiece with magnetic suspension, and detecting cracks with magnetic marks. It is suitable for non-magnetic materials, including special alloys, ceramics, plastics and Glass products.
It realizes simple, efficient, economical and environmentally friendly surface crack detection, strong adaptability, can accurately detect fine cracks, reduce leakage detection rate, and meet high-quality requirements.
Smart Images

Figure CN117929512B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of nondestructive testing and relates to a method for detecting surface cracks of a workpiece by using a magnetic suspension. Background Art
[0002] No surface cracks are the basic and conventional quality requirements for all material products. Special alloys mainly include high-temperature alloys, corrosion-resistant alloys, metal functional materials, special stainless steels, etc. Special alloys are prone to produce surface cracks visible to the naked eye during processing, and the cracks are small. Due to the important uses of special alloys, the quality requirements for billets and products are very high, and these surface cracks must be detected and removed.
[0003] Internal cracks in materials can be detected by ultrasonic testing (UT), and there are many methods for detecting surface cracks. However, there are some problems in detecting surface cracks in special alloys. The reason is that these special alloy products are produced on a large scale, but there are many varieties, specifications, and small cracks. Since most of these special alloys are not ferromagnetic, they cannot be used for magnetic particle testing (MT) (only ferromagnetic materials can be used for magnetic particle testing). Even if a few special alloys are ferromagnetic and can be used for magnetic particle testing (MT), if they exceed the applicable specifications of the self-provided magnetic particle flaw detector equipment, , magnetic particle testing (MT) is also not applicable; if liquid penetrant testing (PT) is used, it has the disadvantages of low efficiency, high cost, high toxicity and environmental pollution; if eddy current testing (ET) is used, it requires a large investment to purchase equipment, and the production volume of these special alloy products is relatively small, and eddy current testing (ET) has low adaptability to product varieties and specifications, and the cost is high; if visual testing (VT) is used, because the product surface is usually bright, the background is bright and the cracks are small, visual testing (VT) is difficult to find cracks, the missed detection rate is high, and it cannot meet the high quality requirements. For this reason, a surface crack detection method that is comprehensive and reliable, simple, efficient, economical, and highly adaptable is needed. Summary of the invention
[0004] The purpose of the present invention is to provide a method for detecting surface cracks of a workpiece using a magnetic suspension, which can detect the surface cracks of the workpiece, thereby ensuring the quality of the product and having the advantages of being simple, efficient, economical, environmentally friendly, highly adaptable and having good comprehensive effects.
[0005] The technical solution of the method of the present invention is:
[0006] A method for detecting surface cracks of a workpiece using a magnetic suspension comprises the following steps:
[0007] 1) Preparation of magnetic suspension
[0008] Use a mixture of kerosene and No. 10 machine oil in a volume ratio of 90%:10% as a dispersant, pour the magnetic powder into the dispersant, stir and mix thoroughly to obtain a magnetic suspension with a sedimentation volume value of 1.2 to 2.5 mL;
[0009] 2) Place or clamp the workpiece to be inspected on a rotating device and rinse the surface of the workpiece with magnetic suspension;
[0010] 3) Rotate the workpiece to be tested, and move the magnetic suspension spray head along the axial direction of the workpiece to continuously spray and immerse the magnetic suspension onto the workpiece surface. The magnetic suspension spray head is at a 45° angle to the workpiece surface to prevent the magnetic suspension flow from directly impacting the workpiece. The liquid flow pressure should not be too high, but should be gentle and moderate. The head of the magnetic suspension liquid sprayed by the magnetic suspension spray head is 30 to 80 mm to avoid washing away the magnetic marks that have been formed. Observe in real time whether there are magnetic marks at the spraying and immersion points. If stable magnetic marks are formed on the workpiece surface, it indicates that there are cracks on the workpiece surface.
[0011] Step 1) The magnetic powder particle size should be easy to suspend and suitable for the crack size to facilitate filling the crack. Therefore, the particle size of the magnetic powder is 1 to 10 microns.
[0012] Step 1) The magnetic powder has high magnetic permeability, low coercive force, and low remanence, and its magnetic properties are ≥7g according to the magnetic weighing method, so that the magnetic powder particles have weak magnetic attraction to each other and are easy to aggregate to form magnetic traces.
[0013] Step 1) The density of the magnetic powder is 4.5-6.0 g / cm 3 The density of magnetic powder should be as large as possible while being easy to suspend, so that the magnetic powder can be easily deposited by natural gravity.
[0014] Step 1) The sedimentation volume value is determined by a pear-shaped tube sedimentation method.
[0015] Step 2) The flushing is performed twice or more.
[0016] Step 3) The magnetic suspension liquid is continuously sprayed and diffused by means of a magnetic particle flaw detector, or a device similar to the magnetic suspension liquid spraying device of a magnetic particle flaw detector.
[0017] Step 3) The process can be repeated.
[0018] The dispersant is required to have good dispersibility, good wettability, stable performance, anti-rust, defoaming, and the ability to clean workpieces, remove dirt on the surface of workpieces and oil marks from previous processes, and be easy to detect.
[0019] When observing whether there are magnetic marks in the spraying and dipping of magnetic suspension, it is necessary to observe in real time whether magnetic marks are formed in the spraying and dipping, and judge whether the magnetic marks are surface cracks. Because the formed magnetic marks are relatively fragile, if you observe them after stopping the spraying and dipping of magnetic suspension, the formed magnetic marks have basically disappeared and cannot be observed; in real-time observation, the magnetic marks will disappear and form at the same time, reaching a dynamic balance, and finally forming a stable magnetic mark that can be stably observed.
[0020] The method of the present invention can detect non-magnetic materials such as metals including special alloys, non-metals, ceramics, plastics, glass products, etc.
[0021] The main features of the method of the present invention and other main surface detection methods are roughly compared in Table 1.
[0022] Table 1 Comparison of the main features of the method described in the present invention and other surface detection methods
[0023]
[0024] It can be seen that the method of the present invention is applicable to a wide range of materials for detection and has the advantages of simple operation, high efficiency, low cost, no pollution to the environment, and high adaptability.
[0025] The method of the present invention originates from the production practice of special alloys. The detectable materials are non-magnetic materials such as metals, non-metals, ceramics, plastics, glass products, etc. including special alloys. It is mainly suitable for detecting surface open cracks, folds, pores, shrinkage holes, delamination, etc. of non-magnetic and non-porous solid materials, especially large cracks. The display of defects is basically not limited by the shape, size, internal organization or chemical composition of the workpiece being inspected, and has nothing to do with the orientation of the defects.
[0026] The method of the present invention can be used for finished product inspection, semi-finished product inspection, process-to-process inspection, etc., and is suitable for inspecting workpieces with moderate production batches.
[0027] By using the method of the present invention to detect special alloy products, most surface cracks can be detected, which not only ensures the quality of the products, but also is simple, efficient, economical, environmentally friendly, and highly adaptable, and is a beneficial technical achievement with good comprehensive effects. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 This is a schematic diagram of the detection principle of the method of the present invention. Implementation
[0029] The method of the present invention is as follows:
[0030] 1) Place the workpiece on the workpiece clamping device of the magnetic particle flaw detector;
[0031] 2) Do not clamp the workpiece and do not connect the current (do not connect the current during the entire detection process);
[0032] 3) Rinse the workpiece with magnetic suspension for 2 to 3 times to remove dirt on the workpiece surface and oil stains from the previous process;
[0033] 4) Spray the workpiece according to the magnetic particle inspection spraying method. The magnetic suspension spray head is tilted at an angle of about 45° to spray and diffuse the workpiece. While spraying, the workpiece is rotated around the center axis of the workpiece. At the same time, the magnetic suspension spray head is moved along the axial direction of the workpiece to the part to be inspected. While spraying, observe in real time whether there are magnetic marks at the spraying and dipping locations, so as to find cracks. Among them, the magnetic powder is ordinary magnetic powder that has been magnetized once. Its magnetic performance is ≥7g according to the magnetic weighing method, the magnetic powder particle size is 1 to 10 microns, and the magnetic powder density is 5.0 to 5.5g / cm 3 The magnetic suspension dispersant is a mixture of kerosene and No. 10 machine oil in a volume ratio of 90%:10%. The concentration of the magnetic suspension is determined by the pear-shaped tube sedimentation method, and the sedimentation volume value is 1.8mL. The head of the magnetic suspension sprayed from the magnetic suspension spray head is 30-50mm.
[0034] See also Figure 1 During the detection, the magnetic powder particles in the magnetic suspension are at least affected by gravity F1, the suspension force F2 of the liquid medium, the weak magnetic attraction F3 between the magnetic powder particles with residual magnetism, and the electrostatic force F4, and the combined force is F.
[0035] First, when the magnetic suspension is applied to the surface of the workpiece, the surface is quickly wetted. At this time, if there is an open crack, according to the principle of capillary action, the magnetic suspension penetrates into the crack, and some magnetic powder with suitable particle size is naturally deposited at the bottom of the crack or the upper and middle parts of the inner side of the crack under the action of gravity F1. After a certain degree, the crack cannot accommodate too much magnetic powder or the crack opening is blocked, and the magnetic powder protrudes to form a magnetic trace. Secondly, the A and B ends of the open crack have an obstructive effect on the flow of adjacent magnetic powder, so some magnetic powder is blocked and retained at A and B, accumulating into magnetic traces. Thirdly, because the magnetic powder (especially the magnetized magnetic powder with weak magnetic attraction) has a weak interaction force (weak magnetic attraction F3, electrostatic force F4, etc.), the magnetic powder accumulated at the crack in advance will attract more magnetic powder to gather until equilibrium is reached, and then a more obvious magnetic trace is formed. Finally, under the influence of the above factors, obvious magnetic marks are formed at the original tiny cracks, which is equivalent to magnifying the original tiny cracks, and the cracks can be easily observed and found; also because the magnetic marks are reddish brown or black, the contrast between the magnetic marks and the bright background material matrix is large and very eye-catching, so they can be easily observed and found; therefore, the formation of magnetic marks at tiny cracks makes the cracks very easy to display and observe, thereby achieving the purpose of detection.
[0036] When the magnetic suspension is applied to the surface of the workpiece, because the magnetic suspension is fluid and has a certain flow force, if there is no open crack at this time, the surface of the material matrix is continuous and flat, and it is difficult for magnetic powder to deposit and its fluidity to be hindered on the flat surface of the material matrix. Although there is a weak interaction force between the magnetic powders and they will be attracted, they cannot stay in a fixed position and will not form magnetic marks. Naturally, cracks will not be displayed incorrectly, and the flat material matrix surface will not be covered with magnetic powder, thereby causing background interference to the observation of magnetic marks appearing at the open cracks. Example 1
[0037] By testing the finished product of 3J78 alloy φ26mm round polished bar according to the method of the present invention, surface crack defects can be accurately detected and supplied to users after being removed. After use, the user found no missed surface crack defects in the finished product, which fully met the quality requirements and had a good detection effect. Example 2
[0038] The method of the present invention can detect the φ60mm round polished bar blank for 3YC52 alloy hot-piercing pipe, and can accurately detect and remove the surface crack defects. After the hot-piercing pipe is formed into a rough pipe, the surface quality of the rough pipe is inspected, and no surface crack defects that were missed and left in the rough pipe stage are found, which fully meets the quality requirements and has a good detection effect. Example 3
[0039] The method of the present invention can detect φ204mm round polished bar blanks for hot extrusion of 316L stainless steel, and can accurately detect surface crack defects and remove them. After hot extrusion into rough pipes, the rough pipes are subjected to surface quality inspection, and no surface crack defects that were missed and left in the rough pipe stage are found, which fully meets the quality requirements and has a good detection effect.
Claims
1. A method for detecting surface cracks of a workpiece using a magnetic suspension, characterized in that: There are the following steps: 1) Preparation of magnetic suspension Use a mixture of kerosene and machine oil as a dispersant, pour the magnetic powder into the dispersant, stir and mix thoroughly to obtain a magnetic suspension with a sedimentation volume value of 1.2 to 2.5 mL; The sedimentation volume value is determined by the pear-shaped tube sedimentation method; The volume ratio of kerosene to machine oil is 90%:10%, and No. 10 machine oil is used; The magnetic powder has high magnetic permeability, low coercive force, and low remanence, and its magnetic performance is ≥7g according to the magnetic weighing method; 2) Place the workpiece to be inspected on the rotating device and rinse the surface of the workpiece with magnetic suspension; 3) Do not clamp the workpiece, do not turn on the current during the whole detection process, rotate the workpiece to be detected, move the magnetic suspension spray head along the axial direction of the workpiece to be detected, and continuously spray and immerse the magnetic suspension onto the surface of the workpiece. The magnetic suspension spray head is at a 45° angle to the workpiece surface. The head of the magnetic suspension spray head is 30 to 80 mm. Observe in real time whether there are stable magnetic marks at the spraying and immersion locations, and determine whether the magnetic marks are cracks.
2. The method according to claim 1, characterized in that: Step 1) The particle size of the magnetic powder is 1 to 10 microns.
3. The method according to claim 1, characterized in that: Step 1) The density of the magnetic powder is 4.5-6.0 g / cm 3 .
4. The method according to claim 1, characterized in that: Step 2) The flushing is performed ≥ twice.
5. The method according to claim 1, characterized in that: In step 3), if a stable magnetic mark is formed on the workpiece surface, it indicates that there is a crack on the workpiece surface.