A blow molding method for polyethylene antistatic film
By designing guide components and multi-layer component devices in polyethylene antistatic film blow molding technology, real-time detection and adjustment of film thickness is achieved, solving the problems of insufficient automation and efficiency in the existing technology, and improving the molding effect. .
Patent Information
- Application Number
- CN202410295129.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-15
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-03-15
AI Technical Summary
The existing polyethylene antistatic film blow molding technology lacks automation and efficiency, making it difficult to achieve real-time detection and targeted adjustment of film thickness, which affects the molding effect.
A device including an extrusion structure, a blown film structure and a blow molding cover is designed. The guide assembly drives the thickness detection part and the adjustment part to move in a circular trajectory around the film blowing die, and detects and adjusts the thickness from the outside and inside of the film. , and uses multi-layer components for cooling to achieve real-time detection and adjustment of film thickness.
It realizes the automated and efficient molding of polyethylene antistatic films, ensures accurate detection and adjustment of film thickness, and improves the molding effect and operation controllability.
Smart Images

Figure CN118003619B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of polyethylene antistatic film processing, in particular to a blow molding method of the polyethylene antistatic film. Background Art
[0002] Polyethylene antistatic film is an important variety of packaging materials, and is often an indispensable material in some specific packaging fields, and has a very important position. Common polyethylene antistatic film processing and molding methods mainly include extrusion, blow molding, calendaring, cast film and stretching. Among them, the molding characteristics of the blow molding method are that the molten resin extruded from the extruder is made into a tube blank through the annular gap die head. At the same time, compressed air is introduced from the axial direction of the mandrel, and the tubular film is clamped with a pair of clamping rods to maintain a constant internal pressure and expand it to the required diameter. After cooling and shaping, it is pulled and coiled. This method produces tubular film.
[0003] A Chinese patent with authorization announcement number CN219486550U discloses a plastic film forming device, which relates to the technical field of plastic film forming, including a frame, an extrusion device is provided on the outside of the frame, the discharge end of the extrusion device extends into the frame, and the discharge end of the extrusion device is connected to a film blowing die head. It is characterized in that a discharge port is opened on the top of the frame, and the blown film extends upward from the film blowing die head and passes through the discharge port; two rotating guide assemblies are rotatably connected to both sides of the bottom of the frame top plate, and an adjustment mechanism for adjusting the rotating guide assembly is provided on the frame.
[0004] The above-mentioned film blow molding method controls the molding process from the aspect of film blowing state. The film thickness detection needs to be detected by relevant detection equipment after molding. Since the film has been formed and rolled up at this time, even if the local thickness is detected to be substandard, it cannot be adjusted in a targeted manner. However, due to the particularity of its application field, polyethylene antistatic film has strict requirements on its thickness and molding effect. The existing film molding technology is not automated and efficient enough, which is not conducive to the control of polyethylene antistatic film blow molding process. Summary of the invention
[0005] In view of the problems existing in the background technology, a blow molding method of a polyethylene antistatic film is proposed.
[0006] On the one hand, the device involved includes an extrusion structure, a film blowing structure and a blow molding cover that are connected in sequence and cover the film blowing die head, and also includes a film discharge piece located at the top of the blow molding cover and opposite to the film blowing die head, a positioning component that is located in the blow molding cover and arranged between the film blowing die head and the film discharge piece and has an adjustable height, a guide component that is arranged at the lower end of the positioning component and is driven by the guide component to move in a circular trajectory around the film blowing die head, and a thickness detection component that emits and receives detection light from the outside of the film to detect the thickness of the film based on the different light reflection properties of films of different thicknesses, through The guide component is driven to move in a circular trajectory around the film blowing die head. Based on the principle that the film is deformed due to the force exerted by the fluid, a tension is generated from the outside of the film to adjust the thickness of the film. A thickness adjusting component is arranged at the upper end of the positioning component. By forming a gathering structure, the film is cooled from the outside. A multi-layer component is arranged at the bottom of the blow molding cover and can be raised and lowered and rotated. The multi-layer component is provided with a thickness detecting component 2 that emits and receives detection light from the inside of the film to detect the thickness of the film, a thickness adjusting component 2 that generates thrust from the inside of the film, and a cooling component that supplies air from the inside of the film for cooling.
[0007] On the other hand, the blow molding method steps are as follows:
[0008] S1, the film is blown out from the film blowing die in a bag shape;
[0009] S2, the multi-layer assembly extends layer by layer into the film bag;
[0010] S3, the thickness detection part 1 moves in a circular trajectory around the film blowing die head, emitting and receiving detection light from the outside of the film to detect the film thickness; the thickness detection part 2 rotates and rises to be opposite to the thickness detection part 1, emitting and receiving detection light from the inside of the film to detect the film thickness;
[0011] S4, the control system obtains the film thickness detection data and determines whether it meets the standard;
[0012] S5. After receiving the thickness adjustment instruction, the thickness adjustment member 1 moves in a circular trajectory around the film blowing die head, and draws air from the outside of the film to generate a pulling force; the thickness adjustment member 2 rotates and rises and falls to be opposite to the thickness adjustment member 1, and blows air from the inside of the film to generate a thrust, so as to locally adjust the thickness of the film whose thickness exceeds the set threshold;
[0013] S6. After the adjustment is completed, the film moves up to the outside and the cooling component position, and at the same time, the inside contacts the air outlet of the cooling component to cool and form;
[0014] S7, the film flows out from the film outlet to the winding end of the winding device.
[0015] Preferably, the guide assembly includes a guide ring connected to the height positioning assembly and located above the film blowing die head; the guide ring is provided with a mounting frame that moves in a circular trajectory along the inner ring of the guide ring; the thickness detection member 1 / thickness adjustment member 1 are both arranged on the mounting frame.
[0016] Preferably, a guide groove with a gear ring is provided on the inner ring wall of the guide ring, and an outer ring groove is provided on the outer wall; an inner ring groove is provided on the groove wall of the guide groove; the mounting frame includes a U-shaped frame body slidably arranged on the inner ring of the guide ring and a positioning ball 1 extending into the outer ring groove; a parallel frame body extending into the guide groove is provided on the U-shaped frame body; an electric control gear meshing with the gear ring and a positioning ball 2 extending into the inner ring groove are provided on the parallel frame body.
[0017] Preferably, multiple groups of mounting frames are arranged on each group of guide components; and the U-shaped frames of the multiple groups of mounting frames are connected in series through a connecting frame.
[0018] Preferably, the positioning assembly includes a positioning rod with rotatable threaded sections at the upper and lower ends, an adjustment sleeve rotatably arranged on the top and bottom of the blow molding cover and threadedly connected to the corresponding threaded sections, and a connector detachably arranged on the positioning rod body and connected to the guide ring.
[0019] Preferably, the multilayer assembly includes three layers of sliding sleeves with decreasing diameters; the cylinder with the largest diameter is located at the center of the annular film blowing die; a second thickness detection component is provided on the second layer of cylinders; and a second thickness adjustment component and a cooling component are provided on the third layer of cylinders.
[0020] Preferably, the detection end of the second thickness detection member is arranged along the outer periphery of the second layer column, and cooperates with the first thickness detection member when working; the adjustment end of the second thickness adjustment member is arranged along the outer periphery of the third layer column, and cooperates with the first thickness detection member when working; the cooling end of the cooling member is located at the top of the third layer column, and cooperates with the cooling assembly when working.
[0021] Preferably, the cooling components are arranged in two groups in a mirror-like manner, each group includes a gathering plate rotatably arranged on a positioning rod; the gathering plates on both sides constitute a gathering structure with an adjustable gathering angle, and a cooling rack is arranged at the bottom of the gathering plate, and a gathering roller is arranged at the top; the air outlet ends of the cooling rack and the cooling element are opposite to each other.
[0022] Preferably, the film discharging member comprises a film discharging sleeve penetrating the top of the blow molding cover and open at both ends, and a film straightening roller group rotatably arranged on the inner wall of the film discharging sleeve.
[0023] Compared with the prior art, the present invention has the following beneficial technical effects: first, the thickness detection part 1 moves in a circular trajectory to detect the thickness of the film from the outside of the film; the thickness detection part 2 rotates and rises to detect the thickness of the film from the inside of the film. Then, the thickness adjustment part 1 moves in a circular trajectory to extract air from the outside of the film to generate a pulling force; the thickness adjustment part 2 rotates and rises to blow air from the inside of the film to generate a thrust to adjust the thickness of the film locally. Finally, the cooling component gathers and cools the film, and the cooling part cools it by blowing air from the inside of the film. The equipment has a compact structure, a high degree of coordination, a coherent detection, adjustment, and shaping operation process, strong controllability and a large range of operations, which realizes the automation and efficiency of polyethylene antistatic film blow molding and ensures the effect of polyethylene antistatic film blow molding. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a schematic diagram of the overall structure of the polyethylene antistatic film blow molding device in the present invention;
[0025] Figure 2 It is a schematic diagram of the internal structure of the blow-molded cover in the present invention;
[0026] Figure 3 A schematic diagram of the positional relationship among the positioning assembly, the guide assembly, the multi-layer assembly and the cooling assembly in the present invention;
[0027] Figure 4 It is an exploded schematic diagram of the positioning assembly, the guide assembly, the multi-layer assembly and the cooling assembly in the present invention;
[0028] Figure 5 It is a structural schematic diagram of the guide assembly in the present invention;
[0029] Figure 6 is a cross-sectional view of the guide assembly of the present invention;
[0030] Figure 7 for Figure 6 Enlarged view of point A in the middle;
[0031] Figure 8 It is a schematic diagram of the installation state of the thickness adjustment member 1 in the present invention;
[0032] Fig. 9 It is a structural schematic diagram of the positioning component in the present invention;
[0033] Fig.10 It is a schematic diagram of the structure of the multi-layer assembly in the present invention;
[0034] Fig.11 It is a schematic diagram of the structure of the cooling assembly in the present invention;
[0035] Fig.12 It is a schematic structural diagram of the film outlet member in the present invention.
[0036] Figure numerals: 1, extrusion structure; 2, film blowing structure; 3, blow molding cover; 4, film blowing die head; 5, positioning assembly; 501, positioning rod; 502, threaded section; 503, adjustment sleeve; 6, guide assembly; 601, guide ring; 602, connecting piece; 603, gear ring; 604, mounting frame; 605, parallel frame; 607, gear; 608, positioning ball 1; 609, outer ring groove; 610, inner ring groove ; 611, positioning ball 2; 612, connecting frame; 7, cooling assembly; 701, gathering plate; 702, cooling frame; 703, gathering roller; 8, film discharging part; 801, film discharging sleeve; 802, film-forming roller group; 9, multi-layer assembly; 901, column; 902, thickness detection part 2; 903, thickness adjustment part 2; 904, cooling part; 10, thickness adjustment part 1; 11, thickness detection part 1; 12, supporting sheet. DETAILED DESCRIPTION
[0037] Embodiment 1
[0038] like Figure 1-Figure 2 As shown, a polyethylene antistatic film blow molding device proposed by the present invention comprises an extrusion structure 1, a film blowing structure 2 and a blow molding cover 3 covering a film blowing die head 4 which are connected in sequence.
[0039] like Figure 3-Figure 4 As shown, the above-mentioned equipment also includes a film discharge component 8, a positioning component 5, a guide component 6, a thickness detection component 11, a thickness adjustment component 10, a cooling component 7 and a multi-layer component 9.
[0040] The film discharging member 8 is located at the top of the blow molding hood 3 and is opposite to the film blowing die head 4. The height-adjustable positioning assembly 5 is located in the blow molding hood 3 and is arranged between the film blowing die head 4 and the film discharging member 8. The guide assembly 6 is arranged at the lower end of the positioning assembly 5. The thickness detection member 11 is driven by the guide assembly 6 and moves in a circular trajectory around the film blowing die head 4. Based on the different light reflection properties of films of different thicknesses, the detection light is emitted and received from the outside of the film to detect the thickness of the film. The thickness adjustment member 10 is driven by the guide assembly 6 and moves in a circular trajectory around the film blowing die head 4. Based on the principle that the film is deformed by the force of the fluid, a pulling force is generated from the outside of the film to adjust the thickness of the film. The cooling assembly 7 is arranged at the upper end of the positioning member 5, and the film is cooled from the outside by forming a gathering structure. The multilayer assembly 9 is arranged at the bottom of the blow molding hood 3 and can be raised, lowered and rotated. The multilayer component 9 is provided with a thickness detection component 902 for emitting and receiving detection light from inside the film to detect the thickness of the film, a thickness adjustment component 903 for generating thrust from inside the film, and a cooling component 904 for supplying air from inside the film for cooling.
[0041] like Fig.12As shown, the film discharge member 8 includes a film discharge sleeve 801 which penetrates the top of the blow molding cover 3 and is open at both ends, and a film straightening roller group 802 which is rotatably arranged on the inner wall of the film discharge sleeve 801. The film after cooling and shaping passes through the film discharge sleeve 801, and flows out after being squeezed and exhausted by the film straightening roller group 802.
[0042] The working process of this embodiment is as follows: the film is blown out from the film blowing die 4 in a bag shape; the multilayer component 9 extends into the film bag; the thickness detection component 11 moves in a circular trajectory around the film blowing die 4, emits and receives detection light from the outside of the film, and detects the thickness of the film; the thickness detection component 902 transmits and receives detection light from the inside of the film by rotating and lifting, and detects the thickness of the film; the thickness adjustment component 10 moves in a circular trajectory around the film blowing die 4, and generates tension by extracting air from the outside of the film; the thickness adjustment component 903 generates thrust by rotating and lifting, and locally adjusts the thickness of the film whose thickness exceeds the set threshold; after the adjustment is completed, the film moves up, the cooling component 7 cools the film from the outside, the cooling component 904 cools the film from the inside, and the cooled and formed film flows out from the film outlet component 8.
[0043] Embodiment 2
[0044] Based on the first embodiment, the specific structure of the guide assembly 6 is disclosed in this embodiment, such as Figure 5 As shown, the guide assembly 6 includes a guide ring 601 connected to the height positioning assembly 5 and located above the film blowing die 4; a mounting frame 604 is provided on the guide ring 601 and moves along a circular trajectory along the inner ring of the guide ring 601; the thickness detection member 11 / thickness adjustment member 10 are both arranged on the mounting frame 604.
[0045] Through the above structure, the thickness detection member 11 and the thickness adjustment member 10 move in a circular trajectory, that is, the thickness detection and adjustment of the film at 360 degrees are realized, the detection and adjustment efficiency is high, and the accuracy is guaranteed.
[0046] like Figure 6-Figure 8 As shown, a guide groove with a toothed ring 603 is provided on the inner ring wall of the guide ring 601, and an outer ring groove 609 is provided on the outer wall; an inner ring groove 610 is provided on the groove wall of the guide groove; the mounting frame 604 includes a U-shaped frame body slidably arranged on the inner ring of the guide ring 601 and a positioning ball 1 608 extending into the outer ring groove 609; a parallel frame body 605 extending into the guide groove is provided on the U-shaped frame body; an electric control gear 607 meshing with the toothed ring 603 and a positioning ball 2 611 extending into the inner ring groove 610 are provided on the parallel frame body 605.
[0047] It should be further explained that the positioning ball 1 608 and the positioning ball 2 611 are positioned relative to each other.
[0048] The electrically controlled gear 607 rotates along the gear ring 603 after being powered on, and the thickness detecting member 11 / thickness adjusting member 10 can move synchronously therewith. Due to the arrangement of the positioning ball 1 608 and the positioning ball 2 611, the movement process is smooth and stable.
[0049] It should be further explained that multiple groups of mounting frames 604 are arranged on each group of guide components 6; the U-shaped frames of the multiple groups of mounting frames 604 are connected in series through a connecting frame 612. The connecting frame 612 is a semi-circular rod. After the multiple groups of mounting frames 604 are connected in series, the thickness detection member 11 / thickness adjustment member 10 can be synchronously moved at a stable interval and speed, further ensuring the effect of detection and adjustment.
[0050] Embodiment 3
[0051] Based on the first and second embodiments, the specific structure of the positioning component 5 is disclosed in this embodiment, such as Fig. 9 As shown, the positioning assembly 5 includes a positioning rod 501 with rotatable threaded sections 502 at the upper and lower ends, an adjustment sleeve 503 rotatably arranged on the top and bottom of the blow molding cover 3 and threadedly connected to the corresponding threaded sections 502, and a connecting piece 602 detachably arranged on the rod body of the positioning rod 501 and connected to the guide ring 601;
[0052] It should be further explained that the connecting member 602 includes a connecting rod connected to the guide ring 601; a connecting sleeve with a notch is provided at the end of the connecting rod; a connecting block with a mounting hole for the bolt to penetrate is provided on the notch of the connecting sleeve;
[0053] It should be further explained that a support sheet 12 is also welded on the positioning rod 501 to support the connecting sleeve from the bottom.
[0054] When adjusting the height of the guide ring 601, on the one hand, the positioning rod 501 can drive all the guide rings 601 thereon to move up and down by rotating the adjustment sleeve 503, and on the other hand, the nut can be unscrewed and the bolt can be removed to expand the gap of the connecting sleeve, so that the corresponding guide ring 601 can be slid up and down.
[0055] Embodiment 4
[0056] Based on the first, second and third embodiments, the specific structure of the multilayer assembly 9 is disclosed in this embodiment, such as Fig.10 As shown, the multilayer assembly 9 includes three layers of sliding sleeves and decreasing diameter cylinders 901; the cylinder 901 with the largest diameter is located at the center of the annular film blowing die 4; a second thickness detection member 902 is provided on the second layer cylinder 901; and a second thickness adjustment member 903 and a cooling member 904 are provided on the third layer cylinder 901.
[0057] It should be further explained that the detection end of the second thickness detection member 902 is arranged along the outer periphery of the second layer of the cylinder 901, and cooperates with the thickness detection member 11 when working; the thickness detection member 11 and the thickness detection member 2 902 are both non-contact optical detectors. The thickness detection member 11 and the thickness detection member 2 902 respectively emit light waves of different wavelengths to penetrate the plastic film layer, and the reflected light from the upper and lower surfaces of the film is received by the instrument, and the phase difference between the reflected light is enhanced or weakened. The change in phase difference depends on the thickness d and refractive index n of the film. If the optical parameter (n, k) values of the material are known, the film thickness can be deduced.
[0058] It should be further explained that the adjusting end of the second thickness adjusting member 903 is arranged along the outer periphery of the third layer column 901, and cooperates with the thickness detecting member 11 when working; the thickness adjusting member 10 is a negative pressure air extractor; the second thickness adjusting member 903 is a high pressure air blower. Through external air extraction and internal air supply, the effect of external pulling and internal pushing is formed, so that the local thickness of the film can be adjusted.
[0059] It should be further explained that the cooling end of the cooling member 904 is located at the top of the third layer column 901, and cooperates with the cooling component 7 when working; the cooling member 904 is an air cooler, which forms a vortex inside the film bag by sending air upward, thereby accelerating the cooling and shaping of the top film.
[0060] It should be further explained that the multilayer assembly 9 also includes multiple sets of driving cylinders and a rotary motor 1. The driving cylinders are respectively arranged in the column 901 to drive the three-layer structure to expand and contract, and adjust the positions of the thickness detection member 2 902, the thickness adjustment member 2 903 and the cooling member 904. The rotary motor 1 is arranged at the center of the annular film blowing die 4 to drive the three-layer structure to rotate synchronously and adjust the angles of the thickness detection member 2 902, the thickness adjustment member 2 903 and the cooling member 904. The above-mentioned three-layer structure can shrink in a non-working state, and then stretch out after the bag-like structure of the film is formed, so as to reduce its interference with the film forming, and also ensure the adjustment of the thickness detection member 2 902, the thickness adjustment member 2 903 and the cooling member 904 during the film forming process.
[0061] Embodiment 5
[0062] Based on the first embodiment, the second embodiment, the third embodiment and the fourth embodiment, the specific structure of the cooling assembly 7 is disclosed in this embodiment, such as Fig.11 As shown, the cooling assembly 7 is arranged in two groups in a mirror image, each group includes a gathering plate 701 rotatably arranged on the positioning rod 501; the gathering plates 701 on both sides constitute a gathering structure with an adjustable gathering angle, and a cooling rack 702 is arranged at the bottom of the gathering plate 701, and a gathering roller 703 is arranged at the top.
[0063] It should be further explained that a second driving motor for driving the gathering plate 701 to rotate is disposed on the positioning rod 501 .
[0064] It should be further explained that the air outlet ends of the cooling rack 702 and the cooling member 904 are opposite to each other; the cooling rack 702 is a tile structure, which supports and conducts heat to the film by contacting with the film, and on the other hand, the film in the supporting area contacts with the air outlet of the cooling member 904, and the contact angle and position can be adjusted by rotating the gathering plate 701. While the film is supported, the inside is cooled by the air outlet of the cooling member 904, and the outside is cooled by contact with the cooling rack 702, so the temperature drops quickly and the molding effect is good.
[0065] It should be further explained that a heating layer is provided on the gathering roller 703. When the film thickness is detected to be too thin, the two sets of gathering rollers 703 are used to clamp and heat the film at the too thin position so that the position is bonded to achieve the effect of marking and sealing without shutting down the equipment, which is convenient for subsequent processing by the staff.
[0066] Embodiment 6
[0067] Based on the polyethylene antistatic film blow molding device in the above embodiment, this embodiment further proposes a polyethylene antistatic film blow molding method, the steps are as follows:
[0068] S1, the film is blown out from the film blowing die 4 in a bag shape;
[0069] S2, the three-layer column 901 extends layer by layer and extends into the film bag;
[0070] S3, the thickness detection member 11 moves in a circular trajectory around the film blowing die head 4, emitting and receiving detection light from the outside of the film to detect the film thickness; the thickness detection member 2 902 rotates and rises to be opposite to the thickness detection member 11, emitting and receiving detection light from the inside of the film to detect the film thickness;
[0071] S4, the control system obtains the film thickness detection data and determines whether it meets the standard;
[0072] S5. After receiving the thickness adjustment instruction, the thickness adjustment member 10 moves in a circular trajectory around the film blowing die head 4, and draws air from the outside of the film to generate a pulling force; the thickness adjustment member 2 903 rotates and rises to be opposite to the thickness adjustment member 10, and blows air from the inside of the film to generate a thrust, and locally adjusts the thickness of the film whose thickness exceeds the set threshold;
[0073] S6. After the adjustment is completed, the film moves upward;
[0074] S7, the cooling rack 702 rotates to gather the film;
[0075] S8, the cooling rack 702 is attached to the outside of the film, and the cooling member 904 blows air from the inside of the film toward the cooling rack 702 to cool the film into shape;
[0076] S9, after the film is extruded and exhausted, it flows out from the film outlet member 8 to the winding end of the winding device;
[0077] S10, when the film thickness is detected to be too thin, the two sets of gathering rollers 703 clamp and heat the film at the too thin position so that the position is bonded.
[0078] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited thereto, and various changes can be made within the knowledge scope of technicians in the relevant technical field without departing from the purpose of the present invention.
Claims
1. A method for blow molding a polyethylene antistatic film, the device comprising an extrusion structure (1), a film blowing structure (2) and a blow molding cover (3) covering a film blowing die head (4) connected in sequence, characterized in that: Also includes: A film discharge member (8) located at the top of the blow molding cover (3) and opposite to the film blowing die head (4); A height-adjustable positioning component (5) located in the blow molding cover (3) and arranged between the film blowing die head (4) and the film discharge member (8); A guide assembly (6) disposed at the lower end of the positioning assembly (5); A thickness detection component (11) is driven by a guide component (6) to move in a circular trajectory around a film blowing die head (4), and based on the different light reflection properties of films of different thicknesses, a detection light is emitted and received from the outside of the film to detect the thickness of the film; A thickness adjusting member (10) is driven by a guide assembly (6) to move in a circular trajectory around a film blowing die head (4), and based on the principle that the film is deformed by the force exerted by the fluid, a pulling force is generated from the outside of the film to adjust the thickness of the film; A cooling component (7) is disposed at the upper end of the positioning component (5) and cools the film from the outside by forming a gathering structure; and a multilayer component (9) disposed at the bottom of the blow molding cover (3) and capable of lifting and rotating; the multilayer component (9) is provided with a second thickness detection component (902) for emitting and receiving detection light from inside the film to detect the thickness of the film, a second thickness adjustment component (903) for generating thrust from inside the film, and a cooling component (904) for supplying air from inside the film for cooling; The guide assembly (6) comprises a guide ring (601) connected to the height positioning assembly (5) and located above the film blowing die head (4); a mounting frame (604) is provided on the guide ring (601) and moves along a circular trajectory along the inner ring of the guide ring (601); a thickness detection member 1 (11) and a thickness adjustment member 1 (10) are both provided on the mounting frame (604); The positioning assembly (5) comprises a positioning rod (501) with rotatable threaded sections (502) at the upper and lower ends, an adjustment sleeve (503) rotatably arranged on the top and bottom of the blow molding cover (3) and threadably connected to the corresponding threaded sections (502), and a connecting piece (602) detachably arranged on the rod body of the positioning rod (501) and connected to the guide ring (601); The multilayer assembly (9) comprises three layers of sliding sleeve-connected cylinders (901) with decreasing diameters; the cylinder (901) with the largest diameter is located at the center of the annular film blowing die (4); a second thickness detection component (902) is provided on the second layer cylinder (901); and a second thickness adjustment component (903) and a cooling component (904) are provided on the third layer cylinder (901); The detection end of the second thickness detection member (902) is arranged along the outer periphery of the second layer column (901), and cooperates with the first thickness detection member (11) when in operation; the adjustment end of the second thickness adjustment member (903) is arranged along the outer periphery of the third layer column (901), and cooperates with the first thickness adjustment member (10) when in operation; the cooling end of the cooling member (904) is located at the top of the third layer column (901), and cooperates with the cooling assembly (7) when in operation; The cooling components (7) are arranged in two groups in a mirror image, each group comprising a gathering plate (701) rotatably arranged on a positioning rod (501); the gathering plates (701) on both sides form a gathering structure with an adjustable gathering angle, and a cooling rack (702) is arranged at the bottom of the gathering plate (701), and a gathering roller (703) with a heating layer is arranged at the top; The air outlet ends of the cooling rack (702) and the cooling element (904) are opposite to each other; The steps are as follows: S1, the film is blown out from the film blowing die (4) in a bag shape; S2, the multilayer assembly (9) is stretched layer by layer and extends into the film bag; S3, the thickness detection member 1 (11) moves in a circular trajectory around the film blowing die head (4), emitting and receiving detection light from the outside of the film to detect the thickness of the film; the thickness detection member 2 (902) rotates and rises and falls to a position opposite to the thickness detection member 1 (11), emitting and receiving detection light from the inside of the film to detect the thickness of the film; S4, the control system obtains the film thickness detection data and determines whether it meets the standard; S5. After receiving the thickness adjustment instruction, the thickness adjustment member 1 (10) moves in a circular trajectory around the film blowing die head (4), extracting air from the outside of the film to generate a pulling force; the thickness adjustment member 2 (903) rotates and rises and falls to a position opposite to the thickness adjustment member 1 (10), blowing air from the inside of the film to generate a thrust, and locally adjusting the thickness of the film whose thickness exceeds the set threshold; S6, after the adjustment is completed, the film moves upward to the outside and the cooling assembly (7), while the inside contacts the air outlet of the cooling member (904) to be cooled and formed; S7, the film flows out from the film outlet member (8) to the reeling end of the reeling device.
2. A polyethylene antistatic film blow molding method according to claim 1, characterized in that: A guide groove with a toothed ring (603) is provided on the inner ring wall of the guide ring (601), and an outer ring groove (609) is provided on the outer wall; an inner ring groove (610) is provided on the groove wall of the guide groove; The mounting frame (604) comprises a U-shaped frame body slidably arranged on the inner ring of the guide ring (601) and a first positioning ball (608) extending into the outer ring groove (609); a parallel frame body (605) extending into the guide groove is arranged on the U-shaped frame body; an electric control gear (607) meshing with the gear ring (603) and a second positioning ball (611) extending into the inner ring groove (610) are arranged on the parallel frame body (605).
3. A polyethylene antistatic film blow molding method according to claim 2, characterized in that: A plurality of mounting frames (604) are arranged on each set of guide components (6); the U-shaped frames of the plurality of mounting frames (604) are connected in series via a connecting frame (612).
4. A polyethylene antistatic film blow molding method according to claim 1, characterized in that: The film discharge member (8) comprises a film discharge sleeve (801) which penetrates the top of the blow molding cover (3) and is open at both ends, and a film straightening roller group (802) which is rotatably arranged on the inner wall of the film discharge sleeve (801).
Citation Information
Cited By
Anti-wrinkle plastic film forming equipment
CN119526744A