A FC flip-chip welding process used in a PMU chip

Through the FC flip-chip welding process and pulse heating technology, the problem of fixed installation of the chip battery on the mother substrate is solved, a firm connection between the chip and the substrate is achieved, the service life and reliability are improved, and it is suitable for miniaturization and thinning systems.

CN118197937BActive Publication Date: 2024-10-15CHENGDU HANXIN GUOKE INTEGRATION TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410613864.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-05-17
Publication Date
2024-10-15
Estimated Expiration
2044-05-17

AI Technical Summary

Technical Problem

It is difficult to fix the existing chip battery on the mother substrate, which results in reduced service life and reliability. Especially in miniaturized and thin systems, the chip battery is easy to shake or break.

Method used

The FC flip-chip welding process is used to melt the adhesive solution and bumps on the PMU chip through pulse heating to achieve a firm connection between the chip and the substrate. Welding is performed on the silicon nitride ceramic substrate to ensure fixed installation of the chip.

Benefits of technology

It realizes the fixed installation of the chip battery, improves the service life and reliability, ensures the tight patch and welding connection between the chip and the substrate, and enhances the stability of the system.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118197937B_ABST
    Figure CN118197937B_ABST
Patent Text Reader

Abstract

The invention relates to an FC flip-chip welding process adopted by a PMU chip, belongs to the technical field of semiconductor welding, and comprises the following steps: step 1): coplanarity detection; step 2): applying an adhesive solution on a PMU chip and a chip substrate; step 3): performing chip bonding on the PMU chip and the chip substrate; wherein an automatic eutectic chip bonding machine can automatically move up and down, accurately align the bumps on the PMU chip with the openings on the chip substrate, make the PMU chip contact the chip substrate, and drive the automatic eutectic chip bonding machine to move down; step 4): performing FC flip-chip welding on the PMU chip and the chip substrate; wherein, pulse heating is adopted to heat the adhesive solution applied on the PMU chip and the chip substrate, and the bumps on the PMU chip are heated, the bumps on the PMU chip are melted, and the welding connection between the PMU chip and the chip substrate is realized; the beneficial effects of the invention are that the PMU chip can be fixedly mounted on the chip substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of semiconductor welding, and in particular relates to an FC flip-chip welding process adopted by a PMU chip. Background Art

[0002] To date, various devices and terminals (devices or terminals are chip batteries) involving electronic information systems, according to the application, mostly need to be miniaturized and integrated. To date, chip batteries (PMU chips) are usually installed on the mother substrate (chip substrate), and chip batteries can also be installed outside the mother substrate. However, the chip battery packaging to date, whether it is ordinary chip battery packaging or system-level packaging SiP (System in Package), is structurally difficult to install the chip battery on the structure of the mother substrate. Installing the chip battery outside the mother substrate cannot obtain a higher service life and reliability, because the chip battery is not fixed on the mother substrate, and the chip battery is prone to shaking and being accidentally broken by humans, which reduces the service life and reliability of the chip battery.

[0003] According to the safety, reliability and service life requirements of flip chip batteries, the chip battery is an internal chip, and the chip battery packaging process adopts independent packaging to seal the chip battery in the packaging structure. However, how to fix the chip battery on the mother substrate before packaging to meet the fixed installation of the chip battery and improve the service life and reliability of the chip battery is a requirement for miniaturized and thin system terminals. Summary of the invention

[0004] The technical problem to be solved by the present invention is: how to enable a chip battery to be fixedly installed on a mother substrate. The present invention provides an FC flip-chip welding process used for a PMU chip, wherein an adhesive solution coated on the PMU chip and the chip substrate is heated by pulse heating, and the bumps on the PMU chip are heated, so that the bumps on the PMU chip melt, thereby realizing a welding connection between the PMU chip and the chip substrate; the adhesive solution between the chip substrate and the PMU chip is evaporated to secure the patch between the PMU chip and the chip substrate, and a PMU chip of silicon nitride (Si3N4) ceramic is welded on a chip substrate of silicon nitride (Si3N4) ceramic, so that the chip battery can be fixedly installed on the mother substrate.

[0005] In order to achieve the above object, the present invention is implemented by the following technical solutions:

[0006] An FC flip-chip welding process for a PMU chip includes the following steps:

[0007] Step 1): Coplanarity detection; wherein the PMU chip and the chip substrate are respectively subjected to coplanarity detection, and the PMU chips and chip substrates that do not meet the requirements are screened out;

[0008] Step 2): applying an adhesive solution on the PMU chip and the chip substrate to prepare for bonding between the PMU chip and the chip substrate;

[0009] Step 3): PMU chip and chip substrate are mounted; wherein the automatic eutectic mounter can automatically move up and down, accurately align the bumps on the PMU chip with the openings on the chip substrate, make the PMU chip contact the chip substrate, drive the automatic eutectic mounter to move down, make the PMU chip and the chip substrate fit tightly, and realize the mounting between the PMU chip and the chip substrate;

[0010] Step 4): FC flip-chip welding is performed on the PMU chip and the chip substrate; wherein, pulse heating is used to heat the adhesive solution applied on the PMU chip and the chip substrate, and the bumps on the PMU chip are heated, so that the bumps on the PMU chip melt, thereby achieving a welding connection between the PMU chip and the chip substrate.

[0011] Optionally, in step 1), the coplanarity detection is performed on the outer surface of the PMU chip and the bumps on the PMU chip, and the coplanarity detection is performed on the outer surface of the chip substrate.

[0012] Furthermore, the coplanarity of the entire PMU chip and the entire chip substrate is detected by an online 3D digital microscope station. The coplanarity accuracy of the online 3D digital microscope station is less than 5 μm within the range of 300X~1100X.

[0013] Optionally, in step 3), the surface processing accuracy of the patching location between the PMU chip and the chip substrate is processed to a surface processing accuracy of less than 5 μm.

[0014] Optionally, in step 4), the chip substrate is fixed to a fixed structure, which is a welding pad, and the adhesive solution between the chip substrate and the PMU chip is evaporated, the evaporation temperature of the adhesive solution is 220°C-250°C, the residue of the adhesive solution is <0.2%, and the adhesive solution is halogen-free.

[0015] Furthermore, the pulse heating method is: the bumps on the PMU chip are heated every 60 seconds, and the bump material on the PMU chip is selected as Au. 80 Sn 20 Gold-Tin Alloy or Sn 96.5 Ag 3.5 Tin-silver alloy, gently heats up the bumps on the PMU chip.

[0016] Furthermore, the PMU chip and the chip substrate are placed in an environmentally friendly gas for pulse heating, wherein the environmentally friendly gas is a hydrogen-nitrogen mixed gas, and the ratio of the hydrogen-nitrogen mixed gas is: H2:N2=5%:95%, or the environmentally friendly gas is pure nitrogen.

[0017] Optionally, after step 4), the PMU chip and the chip substrate are gas-phase cleaned and baked.

[0018] Furthermore, after the PMU chip and the chip substrate are gas-phase cleaned and baked, the PMU chip and the chip substrate are subjected to microscopic inspection and X-Ray inspection.

[0019] Beneficial effects of the present invention:

[0020] 1. The present invention adopts pulse heating to heat the adhesive solution coated on the PMU chip and the chip substrate, and heats the bumps on the PMU chip, so that the bumps on the PMU chip melt; the adhesive solution between the chip substrate and the PMU chip is heated and evaporated to make the patch between the PMU chip and the chip substrate firm; the bumps on the PMU chip and the chip substrate are heated to melt the bumps on the PMU chip so that the PMU chip can be fixedly installed on the chip substrate, thereby realizing FC flip-chip welding between the PMU chip and the chip substrate, and the PMU chip can be fixedly installed on the chip substrate.

[0021] 2. The present invention places the PMU chip and the chip substrate in an environmentally friendly gas for pulse heating, wherein the environmentally friendly gas is a hydrogen-nitrogen mixed gas, and the ratio of the hydrogen-nitrogen mixed gas is: H2:N2=5%:95%, or the environmentally friendly gas is pure nitrogen, to ensure that the chip substrate and the PMU chip can be tightly connected through the adhesive solution, and the PMU chip and the chip substrate can be tightly welded. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0023] Figure 1 The process flow chart of FC flip-chip welding of the PMU chip of the present invention;

[0024] Figure 2 A vacuum welding temperature curve diagram of FC flip-chip welding of a PMU chip according to an embodiment of the present invention;

[0025] Figure 3 A vacuum welding temperature curve diagram of FC flip-chip welding of a PMU chip according to another embodiment of the present invention;

[0026] Figure 4 The figure is a flow chart of the sealing process of the PMU chip of the present invention. DETAILED DESCRIPTION

[0027] The embodiments of the present application are described in detail below with reference to the accompanying drawings.

[0028] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense, for example, it can be welding, bolt connection, or riveting; it can be fixed connection, detachable connection, or integral connection; it can be mechanical connection or electrical connection; it can be directly connected or indirectly connected through an intermediate medium, or it can be internal communication between two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0029] Example 1

[0030] like Figure 1 As shown, the present invention provides an FC flip-chip welding process used in a PMU chip, comprising the following steps:

[0031] Step 1): Coplanarity detection; wherein the PMU chip and the chip substrate are respectively subjected to coplanarity detection, and the PMU chips and chip substrates that do not meet the requirements are screened out;

[0032] Step 2): applying an adhesive solution on the PMU chip and the chip substrate to prepare for bonding between the PMU chip and the chip substrate;

[0033] Step 3): PMU chip and chip substrate are mounted; wherein the automatic eutectic mounter can automatically move up and down, accurately align the bumps on the PMU chip with the openings on the chip substrate, make the PMU chip contact the chip substrate, drive the automatic eutectic mounter to move down, make the PMU chip and the chip substrate fit tightly, and realize the mounting between the PMU chip and the chip substrate;

[0034] Step 4): FC flip-chip welding is performed on the PMU chip and the chip substrate; wherein, pulse heating is used to heat the adhesive solution applied on the PMU chip and the chip substrate, and the bumps on the PMU chip are heated, so that the bumps on the PMU chip melt, thereby achieving a welding connection between the PMU chip and the chip substrate.

[0035] Specifically, in step 1), the coplanarity detection is performed on the outer surface of the PMU chip and the bumps on the PMU chip, and the coplanarity detection is performed on the outer surface of the chip substrate.

[0036] The coplanarity of the entire PMU chip and the entire chip substrate is detected by an online 3D digital microscope station. The coplanarity accuracy of the online 3D digital microscope station is less than 5 μm within the range of 300X~1100X.

[0037] In step 3), the surface processing accuracy of the patching location between the PMU chip and the chip substrate is processed to a surface processing accuracy of less than 5 μm, so as to facilitate the bonding or patching between the PMU chip and the chip substrate.

[0038] In step 4), the chip substrate is fixed to a fixed structure, which is a welding pad, and the adhesive solution between the chip substrate and the PMU chip is evaporated. The evaporation temperature of the adhesive solution is 220°C-250°C, the residue of the adhesive solution is <0.2%, and the adhesive solution is halogen-free.

[0039] Furthermore, the pulse heating method is: the bumps on the PMU chip are heated every 60 seconds, and the bump material on the PMU chip is selected as Au. 80 Sn 20 Gold-Tin Alloy or Sn 96.5 Ag 3.5 Tin-silver alloy, gently heats up the bumps on the PMU chip.

[0040] The PMU chip and the chip substrate are placed in an environmentally friendly gas for pulse heating, wherein the environmentally friendly gas is a hydrogen-nitrogen mixed gas, and the ratio of the hydrogen-nitrogen mixed gas is: H2:N2=5%:95%, or the environmentally friendly gas is pure nitrogen, to ensure that the chip substrate and the PMU chip can be tightly connected through the adhesive solution, and the PMU chip and the chip substrate are tightly welded.

[0041] Optionally, after step 4), the PMU chip and the chip substrate are subjected to gas phase cleaning and baking. After the PMU chip and the chip substrate are subjected to gas phase cleaning and baking, the PMU chip and the chip substrate are subjected to microscopic inspection and X-Ray inspection.

[0042] The present invention mainly welds a PMU chip, i.e., a silicon nitride (Si3N4) ceramic chip, onto a silicon nitride (Si3N4) ceramic chip substrate, thereby achieving a tight connection between the chip substrate and the PMU chip through an adhesive solution, as well as a tight welding connection between the PMU chip and the chip substrate.

[0043] Example 2

[0044] Based on Example 1, Figure 2 As shown, the temperature control of the pulse heating method is more accurate and it is easier to ensure the execution of the process; the vacuum protection uses a hydrogen-nitrogen mixture, and the ratio of the mixed gas is: H2: N2 = 5%: 95%, which ensures that the chip substrate and the PMU chip can be tightly connected through the adhesive solution, and the PMU chip and the chip substrate can be tightly welded.

[0045] Process curve such as Figure 2 As shown, the bump material of the PMU chip is Au 80 Sn 20 Gold-tin alloy, Au 80 Sn 20 The liquidus point and solidus point of gold-tin alloy are both 280°C, and the upper limit temperature of the process is set to 290°C. The pulse heating speed is relatively fast. Nine temperature zones are set for heating during the entire welding process to obtain a smooth temperature rise curve, so that the two components have sufficient stress release time to ensure the reliability of product welding. The green curve is the vacuum setting curve.

[0046] Example 3

[0047] Based on Example 1, Figure 3 As shown, the temperature control using pulse heating is more accurate and easier to ensure process execution; according to the characteristics of the bumps or solder of the PMU chip, a vacuum formic acid process is used, and 99.99% nitrogen is used as the protective gas to ensure that the chip substrate and the PMU chip can be tightly connected through the adhesive solution, as well as the tight welding connection between the PMU chip and the chip substrate.

[0048] Process curve such as Figure 3 As shown, the bump material of the PMU chip is Sn 96.5 Ag 3.5 The liquidus point and solidus point of tin-silver alloy are both 221°C, and the upper limit of the process temperature is set to 228°C. The pulse heating speed is fast, and 10 temperature zones are set for heating during the entire welding process to obtain a smooth temperature rise curve, so that the two components have sufficient stress release time to ensure the reliability of product welding. The green curve is the vacuum setting curve.

[0049] Example 4

[0050] like Figure 4 As shown, the parallel seam welding process is used for sealing between the PMU chip and the chip substrate. The parallel seam welding process is a very mature sealing process, which requires the air inside the chip to be removed so that the PMU chip can obtain a higher service life and reliability.

[0051] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any person skilled in the art can easily think of changes or substitutions within the technical scope of the present invention, which should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.

Claims

1. An FC flip-chip soldering process used in a PMU chip, characterized in that: The steps include: Step 1): Coplanarity detection; wherein the PMU chip and the chip substrate are respectively subjected to coplanarity detection, and the PMU chips and chip substrates that do not meet the requirements are screened out; Step 2): applying an adhesive solution on the PMU chip and the chip substrate to prepare for bonding between the PMU chip and the chip substrate; Step 3): PMU chip and chip substrate are mounted; wherein the automatic eutectic mounter can automatically move up and down, accurately align the bumps on the PMU chip with the openings on the chip substrate, make the PMU chip contact the chip substrate, drive the automatic eutectic mounter to move down, make the PMU chip and the chip substrate fit tightly, and realize the mounting between the PMU chip and the chip substrate; Step 4): FC flip-chip welding is performed on the PMU chip and the chip substrate; wherein, the adhesive solution applied on the PMU chip and the chip substrate is heated by pulse heating, and the bumps on the PMU chip are heated, so that the bumps on the PMU chip melt, thereby achieving a welding connection between the PMU chip and the chip substrate; Wherein, in the step 4), the chip substrate is fixed to a fixed structure, the fixed structure is a welding pad, and the adhesive solution between the chip substrate and the PMU chip is evaporated, the evaporation temperature of the adhesive solution is 220° C.-250° C., the residue of the adhesive solution is <0.2%, and the adhesive solution is halogen-free; The pulse heating method is: the bumps on the PMU chip are heated every 60 seconds, and the bump material on the PMU chip is selected as Au. 80 Sn 20 Gold-Tin Alloy or Sn 96.5 Ag 3.5 Tin-silver alloy, heating the bumps on the PMU chip; The PMU chip and the chip substrate are placed in an environmentally friendly gas for pulse heating, wherein the environmentally friendly gas is a hydrogen-nitrogen mixed gas, the ratio of the hydrogen-nitrogen mixed gas is: H2:N2=5%:95%, or the environmentally friendly gas is pure nitrogen.

2. The FC flip-chip welding process used in a PMU chip according to claim 1, characterized in that: In the step 1), the coplanarity detection is performed on the outer surface of the PMU chip and the bumps on the PMU chip, and the coplanarity detection is performed on the outer surface of the chip substrate.

3. The FC flip-chip welding process used in a PMU chip according to claim 2, characterized in that: The coplanarity of the entire PMU chip and the entire chip substrate is detected by an online 3D digital microscope station. The coplanarity accuracy of the online 3D digital microscope station is less than 5 μm within the range of 300X~1100X.

4. The FC flip-chip welding process used for a PMU chip according to claim 1, characterized in that: In the step 3), the surface processing accuracy of the patch between the PMU chip and the chip substrate is processed to a surface processing accuracy of less than 5 μm.

5. The FC flip-chip welding process used for a PMU chip according to claim 1, characterized in that: After step 4), the PMU chip and chip substrate are gas-phase cleaned and baked.

6. The FC flip-chip welding process used for a PMU chip according to claim 5, characterized in that: After the PMU chip and the chip substrate are gas-phase cleaned and baked, the PMU chip and the chip substrate are subjected to microscopic inspection and X-Ray inspection.