A method and system for preparing a Schottky diode

By determining the area to be deposited, coating and image feature analysis in the preparation of Schottky diodes, a barrier height mapping relationship is established, which solves the problems of poor production reliability and low yield, and achieves the effects of improving product quality and reducing costs.

CN118213274BActive Publication Date: 2024-10-11NANTONG HUALONG MICROELECTRONICS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410635389.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-05-22
Publication Date
2024-10-11
Estimated Expiration
2044-05-22

AI Technical Summary

Technical Problem

The existing Schottky diode preparation technology has problems such as poor production reliability, low yield, and high cost of scrap parts.

Method used

By determining the area to be deposited on the semiconductor substrate, perform metal coating, collect surface scanning images of the metal film, identify image features, obtain film particle uniformity, structural compactness and grayscale boundary values, and establish film formation quality and Schottky potential The mapping relationship of the barrier height is used to predict the barrier height, and the Schottky diode is prepared when the prediction meets the preset requirements.

Benefits of technology

The product quality of Schottky diodes is improved, the preparation cost is reduced, and the production reliability and yield are enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118213274B_ABST
    Figure CN118213274B_ABST
Patent Text Reader

Abstract

The invention discloses a method and system for preparing a Schottky diode, and relates to the technical field of wind turbine monitoring. The method comprises: determining a to-be-deposited area of ​​a semiconductor substrate; performing metal plating in the to-be-deposited area to obtain a metal film; collecting a surface scanning image of the metal film, performing feature recognition on the surface scanning image, and obtaining the uniformity of film particles, the compactness of the film structure, and the grayscale boundary value of the film; outputting the film forming evaluation quality of the metal film; determining a preset Schottky barrier height according to the use requirements of the Schottky diode; establishing a mapping relationship between a film forming quality sample and a Schottky barrier height sample to predict the film forming evaluation quality, and obtaining a predicted Schottky barrier height; when the predicted Schottky barrier height meets the preset Schottky barrier height, a Schottky diode is prepared on the metal film. The technical effect of improving product quality and reducing preparation costs is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of wind turbine monitoring, and in particular to a method and system for preparing a Schottky diode. Background Art

[0002] Schottky diode is an electronic device with metal-semiconductor contact, which has fast switching characteristics, low on-state voltage and low reverse recovery time. It is widely used in high-frequency rectification, frequency conversion, reverse voltage protection, switching power supply and solar cells.

[0003] The existing Schottky diode preparation technology mostly uses fixed process parameters for processing and preparation. During the preparation process, physical vapor deposition (PVD), chemical vapor deposition (CVD) and other methods are usually used to deposit metal films, and then heat treatment is performed to form a Schottky barrier between the metal and the semiconductor. After the preparation is completed, the Schottky diode is subjected to quality inspection and quality control. The existing preparation technology has technical problems such as poor production reliability, low yield rate and high scrap cost. Summary of the invention

[0004] The present invention provides a method and system for preparing a Schottky diode, so as to solve the technical problems of poor production reliability, low yield rate and high waste cost in the prior art, and achieve the technical effect of improving product quality and reducing preparation cost.

[0005] In a first aspect, the present invention provides a method for preparing a Schottky diode, wherein the method comprises:

[0006] Determining a region to be deposited of a semiconductor substrate, wherein the semiconductor substrate comprises an active region and a drain region, and the region to be deposited is a region between the active region and the drain region;

[0007] Performing metal coating on the area to be deposited to obtain a metal film;

[0008] Collecting a surface scan image of the metal film, performing feature recognition on the surface scan image, and obtaining film particle uniformity, film structure density, and film grayscale boundary value;

[0009] Outputting the film forming evaluation quality of the metal film by using the film particle uniformity, film structure density and film grayscale boundary value;

[0010] According to the use requirements of the Schottky diode, the preset Schottky barrier height is determined;

[0011] Establishing a mapping relationship between film quality samples and Schottky barrier height samples, using the mapping relationship to predict the film evaluation quality, and obtaining a predicted Schottky barrier height;

[0012] When the predicted Schottky barrier height meets the preset Schottky barrier height, a Schottky diode is prepared on the metal film.

[0013] In this method, by identifying the features of the metal film surface scan image, important parameters such as film particle uniformity, film structure density and film grayscale boundary value are obtained, providing basic data for subsequent film evaluation. Using the film characteristic parameters, the film evaluation quality of the metal film is output. This method helps to timely discover the quality problems of the metal film, ensure the quality of Schottky diode preparation, and reduce the waste of materials and costs.

[0014] In this method, a mapping relationship between film quality samples and Schottky barrier height samples is established, and this relationship is used to predict the film quality and obtain the predicted Schottky barrier height. This method can evaluate the performance of Schottky diode finished products in advance.

[0015] In a second aspect, the present invention further provides a system for preparing a Schottky diode, wherein the system comprises:

[0016] A to-be-deposited area positioning component, the to-be-deposited area positioning component is used to determine the to-be-deposited area of ​​the semiconductor substrate, wherein the semiconductor substrate includes an active area and a drain area, and the to-be-deposited area is a region between the active area and the drain area;

[0017] A metal coating component, wherein the metal coating component is used to perform metal coating on the area to be deposited to obtain a metal film;

[0018] A film image acquisition component, wherein the film image acquisition component is used to acquire a surface scan image of the metal film, perform feature recognition on the surface scan image, and obtain film particle uniformity, film structure density, and film grayscale boundary value;

[0019] A film quality assessment component, the film quality assessment component is used to output the film quality assessment of the metal film by using the film particle uniformity, film structure density and film grayscale boundary value;

[0020] A demand conversion component, the demand conversion component is used to determine a preset Schottky barrier height according to the use requirements of the Schottky diode;

[0021] A barrier height prediction component, which is used to establish a mapping relationship between film quality samples and Schottky barrier height samples, and use the mapping relationship to predict the film evaluation quality to obtain a predicted Schottky barrier height;

[0022] A determination preparation component is used to prepare a Schottky diode on the metal film when the predicted Schottky barrier height meets the preset Schottky barrier height.

[0023] The present invention discloses a method and system for preparing a Schottky diode, including: determining a region to be deposited of a semiconductor substrate, that is, a region between an active region and a drain region; performing metal plating in the region to be deposited to obtain a metal film; collecting a surface scanning image of the metal film, identifying image features, and obtaining film particle uniformity, structural density, and grayscale boundary values; using these features to evaluate the film quality of the metal film; determining a preset Schottky barrier height according to the requirements of the Schottky diode; establishing a mapping relationship between film quality and Schottky barrier height, and predicting the Schottky barrier height; when the predicted Schottky barrier height meets the preset requirements, preparing a Schottky diode on the metal film. The method and system for preparing a Schottky diode disclosed in the present invention solve the technical problems of poor production reliability, low yield, and high scrap cost, and achieve the technical effect of improving product quality and reducing preparation costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 A schematic flow chart of a method for preparing a Schottky diode according to the present invention;

[0025] Figure 2 The present invention is a schematic structural diagram of a system for preparing a Schottky diode.

[0026] Explanation of the reference numerals: deposition area positioning component 11, metal coating component 12, thin film image acquisition component 13, film quality assessment component 14, demand conversion component 15, barrier height prediction component 16, determination and preparation component 17. DETAILED DESCRIPTION

[0027] The technical solution provided in the embodiments of the present invention is to solve the technical problems of poor production reliability, low yield rate and high waste cost in the prior art. The overall idea adopted is as follows:

[0028] First, determine the area to be deposited of the semiconductor substrate, that is, the area between the active area and the drain area; then, perform metal plating on the area to be deposited to obtain a metal film; then, collect a surface scanning image of the metal film, identify image features, and obtain film particle uniformity, structural density and grayscale boundary values; use these features to evaluate the film quality of the metal film; determine the preset Schottky barrier height according to the requirements of the Schottky diode; then, establish a mapping relationship between the film quality and the Schottky barrier height, and predict the Schottky barrier height; finally, when the predicted Schottky barrier height meets the preset requirements, prepare a Schottky diode on the metal film.

[0029] The above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods of the specification to better understand the above technical solution. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments of the present invention. It should be understood that the present invention is not limited to the example embodiments used only to explain the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. In addition, it should be noted that, for the convenience of description, only the parts related to the present invention are shown in the drawings, rather than all of them.

[0030] Embodiment 1

[0031] Figure 1 The present invention is a schematic flow chart of a method for preparing a Schottky diode; the method comprises:

[0032] Determining a region to be deposited of a semiconductor substrate, wherein the semiconductor substrate comprises an active region and a drain region, and the region to be deposited is a region between the active region and the drain region;

[0033] Optionally, first, determine the area to be deposited of the semiconductor substrate, where the Schottky diode material needs to be deposited on the semiconductor substrate. Exemplarily, for a MOS-type Schottky diode, the area to be deposited is located between the active area and the drain area, where the active area and the drain area are specific areas on the semiconductor substrate, the active area is used to construct the PN junction of the diode, and the drain area is used to connect to an external circuit.

[0034] Optionally, the semiconductor substrate includes an n+ layer with a higher doping concentration and an n-drift layer (epitaxial layer) with a lower doping concentration. A method for preparing a Schottky diode of the present invention is based on the semiconductor substrate described above and performs wafer processing based on a deposition process to obtain a target Schottky diode.

[0035] Exemplarily, the area to be deposited of the semiconductor substrate includes an area to be deposited on the front side of the substrate and an area to be deposited on the back side of the substrate; wherein the area to be deposited on the front side of the substrate is used to form a Schottky contact electrode; and the area to be deposited on the back side of the substrate is used to form an ohmic contact electrode.

[0036] Through this process, the area to be deposited between the active area and the drain area on the semiconductor substrate can be accurately determined, laying the foundation for the subsequent preparation of Schottky diodes.

[0037] Performing metal coating on the area to be deposited to obtain a metal film;

[0038] Optionally, a metal film is deposited on the area to be deposited using physical vapor deposition (PVD), chemical vapor deposition (CVD) or other coating techniques. The metal film is a transition layer in the structure combining the Schottky contact electrode or the ohmic contact electrode with the semiconductor substrate, and is used to improve the bonding quality between the semiconductor and the metal.

[0039] For example, using SiC material as a semiconductor substrate can improve the heat dissipation characteristics of the device and reduce the junction temperature of the device. However, SiC has poor wettability, and it is difficult to obtain a smooth film by directly depositing metal on the SiC substrate to obtain a contact electrode. A layer of metal film can be first deposited on the SiC substrate as a nucleation layer for the contact electrode.

[0040] Optionally, the metal film can be a metal, metal oxide or other material with good semiconductor-metal bonding properties, such as aluminum (Al), gold (Au), titanium (Ti), etc. The presence of the metal film (transition layer) helps to make the interface between the metal contact electrode and the semiconductor substrate more closely bonded, reduce interface defects, thereby improving the bonding quality between the metal and the semiconductor, and ensuring the performance and reliability of the target Schottky diode.

[0041] Collecting a surface scan image of the metal film, performing feature recognition on the surface scan image, and obtaining film particle uniformity, film structure density, and film grayscale boundary value;

[0042] Optionally, a surface scanning image of the metal film is collected, wherein the surface scanning image refers to an image scanned and captured on the surface of the metal film, which is used to analyze the surface characteristics of the film. Exemplarily, an optical microscope, a scanning electron microscope (SEM), an atomic force microscope (AFM), an X-ray fluorescence method or other imaging technology is used to scan the surface of the metal film and capture its image.

[0043] Exemplarily, an X-ray fluorescence spectrometer (XRF) is used to scan the surface of the metal film to collect a surface scan image. When the XRF device emits X-rays, the metal film will emit corresponding fluorescence, which is detected and converted into image data. Specifically, when the X-rays emitted by the X-ray source irradiate the surface of the material, the X-rays interact with the atoms in the material, causing the inner electrons of the atoms to be excited and transition from a low energy level to a high energy level. At this time, the atoms are in an unstable state. In order to return to a stable state, the atoms will release characteristic X-rays, namely fluorescent X-rays. The energy or wavelength of the fluorescent X-rays corresponds to the elements in the film. By measuring the energy or wavelength of the fluorescent X-rays, the type and content of the elements in the film can be determined, and the thickness of the film can be calculated.

[0044] Optionally, by analyzing the particle size and distribution in the XRF image, the uniformity of the particles in the metal film is evaluated and the film particle uniformity is generated; by analyzing the particle gaps and bonding conditions in the XRF image, the structural density of the metal film is evaluated and the film structural density is obtained; by analyzing the grayscale difference between the metal film and the substrate or adjacent layers in the XRF image, the bonding quality between the film and the substrate is evaluated and the film grayscale boundary value is obtained.

[0045] Through the above process, key parameters such as film particle uniformity, film structure density and film grayscale boundary value are extracted based on the collected surface scanning images of the metal film, which helps to evaluate the quality of the metal film and provide guidance for subsequent optimization and improvement.

[0046] Outputting the film forming evaluation quality of the metal film by using the film particle uniformity, film structure density and film grayscale boundary value;

[0047] Optionally, factors affecting the barrier height of the Schottky diode include surface states, interface layers, etc. Specifically, the thickness of the metal film affects the barrier height, and generally a thinner metal film will result in a lower barrier height; the surface roughness affects the contact area between the metal and the semiconductor substrate, and thus affects the barrier height, and the lower the surface roughness, the higher the barrier height.

[0048] Furthermore, when multi-layer metal deposition is performed, if the Ehrlich-Schwoebel (ES) barrier formed by the first thin film is low, the film roughness is not large, the film tends to grow in layers, and the ES barrier increases with the increase of layer height. When the layer height reaches a certain height, the ES barrier will tend to a constant value.

[0049] Among them, the film formation evaluation quality refers to the comprehensive evaluation of the film formation quality of the metal film, and the evaluation indicators include the uniformity, density and bonding quality of the film. Specifically, according to the extracted film particle uniformity, film structure density and film gray boundary value, combined with the preset evaluation criteria and algorithm, the film formation evaluation quality of the metal film is output. Exemplarily, a set of scores or levels is set, and multiple levels contain multiple numerical intervals, corresponding to multiple score values, which are used to evaluate the quality of each feature.

[0050] Through this process, the film quality of the metal film is comprehensively evaluated based on the parameters extracted from the surface scanning image of the metal film, and the results of the film evaluation quality are output to facilitate the subsequent prediction of the Schottky barrier height.

[0051] According to the use requirements of the Schottky diode, the preset Schottky barrier height is determined;

[0052] Optionally, the use requirements of Schottky diodes include the forward voltage drop, leakage current, reverse withstand voltage, etc. of the Schottky diode. Specifically, clarify the functional requirements of the Schottky diode in a specific application scenario. If the application scenario requires high-speed switching, a Schottky diode with a lower barrier height is required. Conversely, if the application requires a higher reverse withstand voltage, a Schottky diode with a higher barrier height is required.

[0053] Furthermore, the barrier height of a Schottky diode decreases as the temperature increases. Therefore, when determining the preset Schottky barrier height, the operating temperature of the application scenario must be considered to facilitate obtaining a Schottky diode with an appropriate barrier height at that temperature.

[0054] Furthermore, the barrier height of a Schottky diode affects its reverse leakage current. If the application scenario requires low leakage current, a Schottky diode with a higher barrier height is required.

[0055] Exemplarily, the method for determining the preset Schottky barrier height includes a theoretical calculation method and a statistical analysis method. Among them, the barrier height theoretical calculation method includes the average bond energy method, the Monte Carlo method, the electrical performance level method, etc.; the statistical analysis method relies on collecting and analyzing a large amount of experimental data to determine the optimal Schottky barrier height.

[0056] Exemplarily, performance data of Schottky diodes with different Schottky barrier heights under the same operating conditions are collected, and then the collected data are processed and analyzed, including calculating various statistics (such as mean, median, standard deviation, etc.), drawing data distribution diagrams (such as histograms, box plots, etc.), and performing various statistical tests (such as t-tests, variance analysis, etc.); then, based on the data processing and analysis, a statistical model, such as a regression model, a decision tree model, etc., is established to find the best Schottky diode performance and determine the predicted Schottky barrier height.

[0057] Optionally, when the use requirement of the Schottky diode is determined, a machine learning method (such as random forest, neural network, etc.) is used to establish a mapping relationship between the use requirement of the Schottky diode and the Schottky barrier height, so as to predict the barrier height and obtain a preset Schottky barrier height.

[0058] Establishing a mapping relationship between film quality samples and Schottky barrier height samples, using the mapping relationship to predict the film evaluation quality, and obtaining a predicted Schottky barrier height;

[0059] Specifically, by analyzing a large amount of experimental data, including film quality samples and corresponding Schottky barrier height samples, the correlation between them is found out, so as to establish a mapping relationship between the film quality samples and the Schottky barrier height samples.

[0060] Optionally, the Schottky barrier height is predicted by machine learning or statistical models, where the film quality is the input feature and the Schottky barrier height is the target variable.

[0061] Exemplarily, first, a large amount of paired data of film quality and Schottky barrier height is obtained by experiment or simulation. Then, the acquired data is preprocessed. Such as data cleaning (processing missing values ​​and outliers), standardizing or normalizing data (making it on the same scale), and performing feature selection or feature extraction so that machine learning or statistical models can better understand the data. Next, select one or more suitable regression models, such as linear regression, decision tree, random forest, support vector machine, or deep learning model such as neural network, use the preprocessed data to train the model, and optimize the parameters of the model to minimize the prediction error. After the model training is completed, the model is verified and tested by an independent data set. So as to understand the performance of the model and make necessary adjustments to it. When the verification and test results show that the model is good, it is set as the mapping relationship between the above-mentioned film quality sample and the Schottky barrier height sample, which is used to predict the new film quality sample, thereby obtaining the predicted Schottky barrier height.

[0062] In some embodiments, a mapping relationship between film quality samples and Schottky barrier height samples is established, wherein the mapping relationship expression is as follows:

[0063]

[0064] in, The capacitance of the prepared Schottky diode was characterized by The Schottky barrier height is obtained by curve fitting. is the effective barrier height, is the film quality of the metal thin film, is the dielectric constant of the metal film, is the dielectric constant of vacuum, To prepare the resulting Schottky diode electron charge, V represents the forward voltage drop of the Schottky diode.

[0065] Optionally, the above mapping expression describes the relationship between the capacitance of the Schottky diode and the Schottky barrier height. This model is obtained by Curve fitting is used to obtain the Schottky barrier height. Where V is the forward voltage drop of the Schottky diode, that is, the conduction voltage drop.

[0066] In some embodiments, the mapping relationship is used to predict the film formation evaluation quality, and the method includes:

[0067] Acquiring an error medium of the mapping relationship;

[0068] The mapping relationship is optimized according to the error medium, the optimized mapping relationship is output, and then the film formation evaluation quality is solved to obtain the predicted Schottky barrier height.

[0069] Optionally, an error medium of the mapping relationship is obtained, wherein the error medium refers to the error or uncertainty existing in the mapping relationship in actual application. Specifically, the error or uncertainty of the mapping relationship is identified and quantified by bringing a practical sample in an actual preparation scenario into the existing mapping relationship for error analysis.

[0070] In other words, the error measure is calculated by comparing the model's predictions with the actual observed values. Available error metrics include mean square error (MSE), root mean square error (RMSE), mean absolute error (MAE), etc.

[0071] Optionally, using information of the error medium, by adjusting the parameters or structure of the mapping relationship to make it more consistent with the actual situation, reducing the error or uncertainty, involves adjusting the parameters of the model to minimize the error medium. Exemplarily, the mapping relationship is optimized using methods including gradient descent, Newton's method, stochastic gradient descent, etc.

[0072] Furthermore, the optimized mapping relationship is used to predict the new film evaluation quality. Specifically, the film evaluation quality is input into the optimized mapping relationship, and the predicted Schottky barrier height is calculated. Through this process, the mapping relationship is optimized using the error medium of the mapping relationship, thereby reducing errors or uncertainties and making the mapping relationship more accurate. Then, the film evaluation quality is solved using the optimized mapping relationship to obtain the predicted Schottky barrier height. On the one hand, it helps to ensure the performance and reliability of semiconductor devices, and on the other hand, it facilitates the prediction-based pre-quality control before subsequent preparation processes such as metal deposition and photolithography patterning, thereby achieving the technical effect of reducing preparation costs.

[0073] When the predicted Schottky barrier height meets the preset Schottky barrier height, a Schottky diode is prepared on the metal film.

[0074] When the predicted Schottky barrier height meets the preset Schottky barrier height, it indicates that the current intermediate Schottky diode intermediate state, that is, the quality of the semiconductor substrate-metal film complex is good and can meet the expected use requirements of the Schottky diode, and the Schottky diode can be prepared on the metal film.

[0075] Through the above process, the preparation process of Schottky diodes is made more accurate and controllable. By predicting and optimizing the Schottky barrier height, the quality of the preparation process is controlled based on the film quality of the metal film before preparation, thereby improving the performance and reliability of the diode, increasing the yield rate, and reducing production costs.

[0076] In some embodiments, a Schottky diode is prepared on the metal film, comprising:

[0077] When the film quality is greater than a preset film quality, photolithography is performed on the metal film to obtain a photolithography mask;

[0078] Performing metal deposition on the photolithography mask by using a vapor deposition method to obtain a deposited metal;

[0079] The deposited metal and the semiconductor substrate are thermally combined and controlled by a thermal control module to prepare a Schottky diode.

[0080] Optionally, the metal film is subjected to photolithography to obtain a photolithography mask, wherein the photolithography mask is used to transfer a pattern. Specifically, the shape and size of the diode are defined on the metal film using photolithography technology, and then unnecessary metal parts are removed by etching, leaving a metal pattern constituting a Schottky contact or an ohmic contact, thereby obtaining a Schottky contact electrode or an ohmic contact electrode with specific shape characteristics.

[0081] Optionally, after obtaining the photolithography mask, metal is deposited on the photolithography mask using vapor deposition to convert the atoms or molecules of the deposition material from the gas phase to the solid phase, thereby forming a thin film on the target surface to obtain a deposited metal. The deposited metal forms a Schottky contact electrode in the area to be deposited on the front side of the substrate and an ohmic contact electrode in the area to be deposited on the back side of the substrate.

[0082] Furthermore, the thermal control module is used to control the thermal bonding of the deposited metal and the semiconductor substrate to prepare a Schottky diode. In this process, the thermal control module is used to control the temperature of the bonding process to optimize the thermal bonding quality and ensure that a stable Schottky contact is formed between the metal and the semiconductor. Different deposited metal and semiconductor bottom matching types correspond to different bonding temperatures.

[0083] In some implementations, the method further includes:

[0084] Determining a first thermal contact surface and a second thermal contact surface for thermal bonding, wherein the first thermal contact surface is a thermal contact surface between the deposited metal and the photolithography mask, and the second thermal contact surface is a thermal contact surface between the photolithography mask and the semiconductor substrate;

[0085] Performing thermal bonding evaluation on the first thermal contact surface and the second thermal contact surface respectively to obtain a first contact quality and a second contact quality;

[0086] When the first contact quality and the second contact quality both meet the preset contact quality, a Schottky diode is obtained.

[0087] Optionally, before thermal bonding, the thermal contact surface is determined and evaluated to further optimize the preparation process of the Schottky diode and ensure the quality and performance of the Schottky diode.

[0088] Specifically, first, determine the first thermal contact surface and the second thermal contact surface for thermal bonding. The first thermal contact surface is the thermal contact surface between the deposited metal and the photolithography mask, and the second thermal contact surface is the thermal contact surface between the photolithography mask and the semiconductor substrate. In other words, the first thermal contact surface and the second thermal contact surface are the upper and lower contact surfaces of the photolithography mask, and the contact conditions of these two contact surfaces jointly affect the thermal bonding effect. Then, the first thermal contact surface and the second thermal contact surface are thermally bonded and evaluated respectively to obtain the first contact quality and the second contact quality. When both the first contact quality and the second contact quality meet the preset contact quality, the thermal bonding process is performed to obtain the Schottky diode.

[0089] In some implementations, thermal bonding evaluation is performed on the first thermal contact surface and the second thermal contact surface respectively to obtain a first contact quality and a second contact quality, and the method further includes:

[0090] Acquiring real-time thermal bonding control parameters of the thermal control module;

[0091] Determining material information of the semiconductor substrate and material information of the deposited metal;

[0092] determining the ion state type of the first thermal contact surface according to the material information of the semiconductor substrate and the real-time thermal bonding control parameter;

[0093] determining the ion state type of the second thermal contact surface according to the material information of the deposited metal and the real-time thermal bonding control parameter;

[0094] Performing a thermal bonding stability analysis on the ionic state type of the first thermal contact surface, and outputting a first contact quality;

[0095] A thermal bonding stability analysis is performed on the ionic state type of the second thermal contact surface, and a second contact quality is output.

[0096] Optionally, the thermal bonding stability analysis of the first thermal contact surface and the second thermal contact surface is achieved by evaluating the ionic state type of the first thermal contact surface and the second thermal contact surface. The ionic state refers to the interface state existing at the metal-semiconductor contact, which is caused by ionic defects, impurities, surface roughness, etc. These interface states can capture or repel electrons, change the height of the Schottky barrier, and thus affect the flow of current.

[0097] Specifically, the ion state type is divided into two types: donor state and acceptor state. If there is an interface state that captures electrons, it can accept electrons from the valence band, which will increase the height of the Schottky barrier, allowing fewer electrons to cross the barrier, thereby reducing the current. The ion state type corresponding to such an interface state is the acceptor state. Conversely, if there is an interface state that repels electrons, it can donate electrons to the conduction band, which will reduce the height of the Schottky barrier, allowing more electrons to cross the barrier, thereby increasing the current. Exemplary state indicators that affect the ion state type include: surface state density, interface layer capacitance density, surface state intermediate performance level, etc.

[0098] Optionally, the ion state also includes the distribution of ions. According to the particle distribution characteristics of the contact surface, the distribution of ions can be divided into island-like and layer-like. Specifically, in the island-like distribution, the ions are unevenly distributed and gathered in a specific area to form an island-like structure, thereby increasing the roughness of the contact surface and affecting the thermal bonding effect; in the layer-like distribution, the ions are evenly distributed on the entire contact surface to form a layered structure. The contact surface has low roughness and good quality, which is conducive to thermal bonding.

[0099] Furthermore, the higher the substrate temperature and the lower the deposition rate, the lower the surface roughness of the contact surface or the molding surface and the better the surface quality; the smaller the interlayer barrier difference of the multi-layer deposited layers, the lower the roughness of the contact surface or the molding surface. In particular, when the interlayer barrier difference of the multi-layer deposited layers exceeds a certain value, the roughness increases significantly, and the deposition molding tends to change from layered growth to island growth.

[0100] Optionally, real-time thermal bonding control parameters are obtained, including temperature, pressure, time, etc., all of which affect the thermal bonding effect; then, the material information of the semiconductor substrate and the material information of the deposited metal need to be determined. Including the type, purity, lattice structure, etc. of the material, the material information of the semiconductor substrate affects the state of the ions; further, the ion state type of the first thermal contact surface is determined according to the material information of the semiconductor substrate and the real-time thermal bonding control parameters. Similarly, the ion state type of the second thermal contact surface is determined according to the material information of the deposited metal and the real-time thermal bonding control parameters. Then, based on the empirical formula obtained by statistical analysis, the ion state type of the first thermal contact surface is subjected to a thermal bonding stability analysis, and the first contact quality is output. Similarly, the ion state type of the second thermal contact surface is subjected to a thermal bonding stability analysis, and the second contact quality is output. Exemplarily, the above empirical formula involves surface state density, interface layer capacitance density, performance level in surface state, distribution characteristic index of ions, etc.

[0101] The above steps provide a path to evaluate the thermal bonding effect based on the ionic state type to provide more accurate and reliable predictions, which in turn helps to optimize the thermal bonding process and improve the quality and performance of Schottky diodes.

[0102] In some embodiments, when any one of the first contact quality and the second contact quality does not meet a preset contact quality, the method includes:

[0103] Obtaining thermal bonding control parameters of the thermal control module, including thermal bonding temperature, thermal bonding time and thermal bonding pressure;

[0104] A control variable training sample group is set according to the thermal bonding temperature, the thermal bonding time and the thermal bonding pressure, and the identified contact quality identification information corresponding to the control variable training sample group is obtained;

[0105] Performing training according to the control variable training sample group and the identified contact quality identification information to obtain a contact quality two-way propagation model;

[0106] When any of the first contact quality and the second contact quality does not meet the preset contact quality, back propagation optimization is performed according to the contact quality bidirectional propagation model, and the thermal bonding control parameters obtained by optimization are output.

[0107] Optionally, when either the first contact quality or the second contact quality does not meet the preset contact quality, the thermal bonding control parameters are optimized and adjusted to compensate for the defects of the first contact quality or the second contact quality, ensure the thermal bonding effect, improve the yield rate, and reduce scrap.

[0108] Optionally, a thermal bonding control parameter optimization strategy is formed based on machine learning, a contact quality bidirectional propagation model is obtained, and the thermal bonding control parameters obtained by optimization are output. Specifically, a back propagation method is used to train a neural network, and the error between the predicted result and the actual result is calculated, and the error is back propagated to the network to adjust the parameters of the model.

[0109] Exemplarily, first, the thermal bonding control parameters of the thermal control module are obtained. The thermal bonding control parameters are real-time thermal bonding process parameters, including the temperature, duration and pressure of thermal bonding, which are important factors affecting the thermal bonding process; then, according to the temperature, duration and pressure of thermal bonding, a set of training samples of control variables are set, and at the same time, the identification information of the contact quality corresponding to these samples is obtained. Exemplarily, the identification information of the contact quality can be the contact quality obtained by experiment, or it can be the contact quality calculated by simulating the thermal bonding process using a physical model or a mathematical model, or the contact quality associated and stored in the historical thermal bonding quality inspection data; then, the control variable training sample group and the identification information of the contact quality are used for training to obtain a contact quality bidirectional propagation model. The contact quality bidirectional propagation model is a neural network model using a back-propagation algorithm, including forward propagation and back-propagation.

[0110] Specifically, when any of the first contact quality and the second contact quality does not meet the preset contact quality, a two-way propagation model of the contact quality is used to perform back propagation optimization, and according to the error between the predicted result and the actual result, the parameters of the model are adjusted to reduce the error.

[0111] Exemplarily, in the forward propagation stage, the input data (including thermal bonding temperature, thermal bonding time and thermal bonding pressure) is processed by the contact quality bidirectional propagation model through each layer of neurons to generate output (i.e., predicted contact quality). In the reverse propagation stage, the output of the network is compared with the expected output (identified contact quality identification information) to calculate the error. Then, the calculated error is pushed back to the network, and the parameters of the network are adjusted to reduce the error during the next forward propagation.

[0112] Through the above method steps, the parameters of thermal bonding can be adjusted in real time to adapt to different surface qualities, compensate for surface quality defects, ensure thermal bonding effects, improve yield rate, and reduce scrap.

[0113] In summary, the method for preparing a Schottky diode provided by the present invention has the following technical effects:

[0114] By determining the area to be deposited on the semiconductor substrate, including the area between the active area and the drain area; performing metal plating in the area to be deposited to form a metal film; collecting a surface scanning image of the metal film, analyzing the uniformity, density and boundary value of the film; using the analysis results to evaluate the quality of the metal film; determining the preset Schottky barrier height according to the use requirements of the diode; establishing a mapping relationship between the film quality and the Schottky barrier height, predicting the Schottky barrier height; and preparing a Schottky diode when the predicted Schottky barrier height meets the preset value. This achieves the technical effect of improving product quality and reducing preparation costs.

[0115] Embodiment 2

[0116] Figure 2 Schematic diagram of the structure of a Schottky diode manufacturing system of the present invention. Figure 1 The schematic flow chart of the method for preparing a Schottky diode of the present invention can be as follows: Figure 2 The structure shown is implemented.

[0117] Based on the same concept as the method for preparing a Schottky diode in the embodiment, the present invention also provides a system for preparing a Schottky diode, including:

[0118] The to-be-deposited area positioning component 11 is used to determine the to-be-deposited area of ​​the semiconductor substrate, wherein the semiconductor substrate includes an active area and a drain area, and the to-be-deposited area is the area between the active area and the drain area;

[0119] A metal coating component 12, used for performing metal coating on the area to be deposited to obtain a metal film;

[0120] The film image acquisition component 13 is used to acquire the surface scanning image of the metal film, perform feature recognition on the surface scanning image, and obtain the uniformity of film particles, the density of film structure and the grayscale boundary value of the film;

[0121] The film quality evaluation component 14 is used to output the film quality evaluation of the metal film by using the film particle uniformity, film structure density and film grayscale boundary value;

[0122] The demand conversion component 15 is used to determine the preset Schottky barrier height according to the use requirements of the Schottky diode;

[0123] The barrier height prediction component 16 is used to establish a mapping relationship between the film quality samples and the Schottky barrier height samples, and use the mapping relationship to predict the film evaluation quality to obtain the predicted Schottky barrier height;

[0124] The determination preparation component 17 is used to prepare a Schottky diode on the metal film when the predicted Schottky barrier height meets the preset Schottky barrier height.

[0125] The barrier height prediction component 16 includes a mapping characterization unit for establishing a mapping relationship between film quality samples and Schottky barrier height samples, wherein the mapping relationship expression is as follows:

[0126]

[0127] in, The capacitance of the prepared Schottky diode was characterized by The Schottky barrier height is obtained by curve fitting. is the effective barrier height, is the film quality of the metal thin film, is the dielectric constant of the metal film, is the dielectric constant of vacuum, To prepare the resulting Schottky diode electron charge, V represents the forward voltage drop of the Schottky diode.

[0128] In some implementations, the barrier height prediction component 16 further includes:

[0129] A mapping error acquisition unit, used to acquire an error medium of the mapping relationship;

[0130] A mapping optimization unit is used to optimize the mapping relationship according to the error medium, output the optimized mapping relationship, and then solve the film formation evaluation quality to obtain the predicted Schottky barrier height.

[0131] Further, the identification preparation component 17 includes:

[0132] A photolithography unit, used for performing photolithography on the metal film to obtain a photolithography mask when the film quality is greater than a preset film quality;

[0133] A metal deposition unit, used for performing metal deposition on the photolithography mask by using a vapor deposition method to obtain a deposited metal;

[0134] The thermal bonding unit is used to control the thermal bonding of the deposited metal and the semiconductor substrate through a thermal control module to prepare a Schottky diode.

[0135] In some implementations, the thermal bonding unit in the determination preparation component 17 includes:

[0136] A contact surface positioning unit, used to determine a first thermal contact surface and a second thermal contact surface for thermal bonding, wherein the first thermal contact surface is a thermal contact surface between the deposited metal and the photolithography mask, and the second thermal contact surface is a thermal contact surface between the photolithography mask and the semiconductor substrate;

[0137] a bonding quality evaluation unit, configured to respectively perform thermal bonding evaluation on the first thermal contact surface and the second thermal contact surface to obtain a first contact quality and a second contact quality;

[0138] The standard combining unit is used to obtain a Schottky diode when the first contact quality and the second contact quality both meet the preset contact quality.

[0139] Further, the bonding quality evaluation unit in the thermal bonding unit includes:

[0140] A combination parameter extraction unit, used to obtain real-time thermal combination control parameters of the thermal control module;

[0141] A material information acquisition unit, used to determine the material information of the semiconductor substrate and the material information of the deposited metal;

[0142] A first ion state unit, used to determine the ion state type of the first thermal contact surface according to the material information of the semiconductor substrate and the real-time thermal bonding control parameter;

[0143] A second ion state unit, used to determine the ion state type of the second thermal contact surface according to the material information of the deposited metal and the real-time thermal bonding control parameter;

[0144] A first stability analysis unit, used for performing a thermal bonding stability analysis on the ion state type of the first thermal contact surface and outputting a first contact quality;

[0145] The second stability analysis unit is used to perform a thermal bonding stability analysis on the ion state type of the second thermal contact surface and output a second contact quality.

[0146] Furthermore, the thermal bonding unit also includes a feedback parameter adjustment unit, which is used to:

[0147] When any one of the first contact mass and the second contact mass does not meet the preset contact mass, obtaining thermal bonding control parameters of the thermal control module, including thermal bonding temperature, thermal bonding time and thermal bonding pressure;

[0148] A control variable training sample group is set according to the thermal bonding temperature, the thermal bonding time and the thermal bonding pressure, and the identified contact quality identification information corresponding to the control variable training sample group is obtained;

[0149] Performing training according to the control variable training sample group and the identified contact quality identification information to obtain a contact quality two-way propagation model;

[0150] When any of the first contact quality and the second contact quality does not meet the preset contact quality, back propagation optimization is performed according to the contact quality bidirectional propagation model, and the thermal bonding control parameters obtained by optimization are output.

[0151] It should be understood that the embodiments mentioned in this specification focus on their differences from other embodiments. The specific embodiments in the aforementioned embodiment 1 are also applicable to the preparation system of a Schottky diode described in embodiment 2. For the sake of brevity of the specification, no further elaboration is given here.

[0152] It should be understood that the embodiments disclosed in the present invention and the above description can enable those skilled in the art to use the present invention to implement the present invention. At the same time, the present invention is not limited to the above-mentioned embodiments. It should be understood that those skilled in the art can still modify the technical solutions recorded in the above-mentioned embodiments, or replace some of the technical features therein by equivalents; and these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present invention, and should be included in the protection scope of the present invention.

Claims

1. A method for preparing a Schottky diode, characterized in that: The method comprises: Determining a region to be deposited of a semiconductor substrate, wherein the semiconductor substrate comprises an active region and a drain region, and the region to be deposited is a region between the active region and the drain region; Performing metal coating on the area to be deposited to obtain a metal film; Collecting a surface scan image of the metal film, performing feature recognition on the surface scan image, and obtaining film particle uniformity, film structure density, and film grayscale boundary value; Outputting the film forming evaluation quality of the metal film by using the film particle uniformity, film structure density and film grayscale boundary value; According to the use requirements of the Schottky diode, the preset Schottky barrier height is determined; Establishing a mapping relationship between film quality samples and Schottky barrier height samples, using the mapping relationship to predict the film evaluation quality, and obtaining a predicted Schottky barrier height; When the predicted Schottky barrier height meets the preset Schottky barrier height, a Schottky diode is prepared on the metal film; A Schottky diode is prepared on the metal film, comprising: When the film quality is greater than a preset film quality, photolithography is performed on the metal film to obtain a photolithography mask; Performing metal deposition on the photolithography mask by using a vapor deposition method to obtain a deposited metal; Controlling the thermal bonding of the deposited metal and the semiconductor substrate by a thermal control module to prepare a Schottky diode; A mapping relationship between film quality samples and Schottky barrier height samples is established, wherein the mapping relationship expression is as follows: ; in, The capacitance of the prepared Schottky diode was characterized by The Schottky barrier height is obtained by curve fitting. is the effective barrier height, A is the film quality of the metal film, is the dielectric constant of the metal film, is the dielectric constant of vacuum, To prepare the resulting Schottky diode electron charge, is the space charge density of the prepared Schottky diode, V represents the forward voltage drop of the prepared Schottky diode; The mapping relationship is used to predict the film formation evaluation quality, and the method includes: Acquire an error medium of the mapping relationship; The mapping relationship is optimized according to the error medium, the optimized mapping relationship is output, and then the film formation evaluation quality is solved to obtain the predicted Schottky barrier height.

2. The method according to claim 1, characterized in that The method further comprises: Determining a first thermal contact surface and a second thermal contact surface for thermal bonding, wherein the first thermal contact surface is a thermal contact surface between the deposited metal and the photolithography mask, and the second thermal contact surface is a thermal contact surface between the photolithography mask and the semiconductor substrate; Performing thermal bonding evaluation on the first thermal contact surface and the second thermal contact surface respectively to obtain a first contact quality and a second contact quality; When the first contact quality and the second contact quality both meet the preset contact quality, a Schottky diode is obtained.

3. The method according to claim 2, characterized in that When any one of the first contact quality and the second contact quality does not meet the preset contact quality, the method includes: Obtaining thermal bonding control parameters of the thermal control module, including thermal bonding temperature, thermal bonding time and thermal bonding pressure; A control variable training sample group is set according to the thermal bonding temperature, the thermal bonding time and the thermal bonding pressure, and the identified contact quality identification information corresponding to the control variable training sample group is obtained; Performing training according to the control variable training sample group and the identified contact quality identification information to obtain a contact quality two-way propagation model; When any of the first contact quality and the second contact quality does not meet the preset contact quality, back propagation optimization is performed according to the contact quality bidirectional propagation model, and the thermal bonding control parameters obtained by optimization are output.

4. The method according to claim 3, characterized in that Performing thermal bonding evaluation on the first thermal contact surface and the second thermal contact surface respectively to obtain a first contact quality and a second contact quality, the method further comprising: Acquiring real-time thermal bonding control parameters of the thermal control module; Determining material information of the semiconductor substrate and material information of the deposited metal; determining the ion state type of the first thermal contact surface according to the material information of the semiconductor substrate and the real-time thermal bonding control parameter; determining the ion state type of the second thermal contact surface according to the material information of the deposited metal and the real-time thermal bonding control parameter; Performing a thermal bonding stability analysis on the ionic state type of the first thermal contact surface, and outputting a first contact quality; A thermal bonding stability analysis is performed on the ionic state type of the second thermal contact surface, and a second contact quality is output.

5. A system for preparing a Schottky diode, characterized in that: The system is used to execute the method according to any one of claims 1 to 4, and the system comprises: A to-be-deposited area positioning component, the to-be-deposited area positioning component is used to determine the to-be-deposited area of ​​the semiconductor substrate, wherein the semiconductor substrate includes an active area and a drain area, and the to-be-deposited area is a region between the active area and the drain area; A metal coating component, wherein the metal coating component is used to perform metal coating on the area to be deposited to obtain a metal film; A film image acquisition component, wherein the film image acquisition component is used to acquire a surface scan image of the metal film, perform feature recognition on the surface scan image, and obtain film particle uniformity, film structure density, and film grayscale boundary value; A film quality assessment component, the film quality assessment component is used to output the film quality assessment of the metal film by using the film particle uniformity, film structure density and film grayscale boundary value; A demand conversion component, the demand conversion component is used to determine a preset Schottky barrier height according to the use requirements of the Schottky diode; A barrier height prediction component, which is used to establish a mapping relationship between film quality samples and Schottky barrier height samples, and use the mapping relationship to predict the film evaluation quality to obtain a predicted Schottky barrier height; A determination and preparation component, wherein the determination and preparation component is used to prepare a Schottky diode on the metal film when the predicted Schottky barrier height meets the preset Schottky barrier height; The discriminant preparation components include: A photolithography unit, used for performing photolithography on the metal film to obtain a photolithography mask when the film quality is greater than a preset film quality; A metal deposition unit, used for performing metal deposition on the photolithography mask by using a vapor deposition method to obtain a deposited metal; A thermal bonding unit, used for controlling the thermal bonding of the deposited metal and the semiconductor substrate through a thermal control module to prepare a Schottky diode; The barrier height prediction component includes a mapping characterization unit, which is used to establish a mapping relationship between a film quality sample and a Schottky barrier height sample, wherein the mapping relationship expression is as follows: ; Among them, C represents the capacitance of the prepared Schottky diode. The Schottky barrier height is obtained by curve fitting. is the effective barrier height, A is the film quality of the metal film, is the dielectric constant of the metal film, is the dielectric constant of vacuum, To prepare the resulting Schottky diode electron charge, is the space charge density of the prepared Schottky diode, V represents the forward voltage drop of the prepared Schottky diode; The barrier height prediction components include: A mapping error acquisition unit, used to acquire an error medium of the mapping relationship; A mapping optimization unit is used to optimize the mapping relationship according to the error medium, output the optimized mapping relationship, and then solve the film formation evaluation quality to obtain the predicted Schottky barrier height.