A production process for corrugated paper

By calculating the characteristic values ​​of the groove width, groove depth and flatness of the corrugated core paper, the processing quality of the core paper is identified, and the problem of high defective rate of corrugated paper processing in the existing technology is solved, and the processing quality and equipment maintenance efficiency of corrugated paper are improved. .

CN118219613BActive Publication Date: 2024-11-19JIANGXI FUSHAN ZHONGPINXIN PACKAGING CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202410060981.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-01-16
Publication Date
2024-11-19
Estimated Expiration
2044-01-16

AI Technical Summary

Technical Problem

The lack of effective identification of the processing quality of corrugated core paper in the prior art, resulting in a high defect rate of corrugated paper processing.

Method used

By dividing the core paper into several core paper subunits according to the V-shaped base, the core paper groove width, groove depth and flat behavior values ​​are obtained, the core paper characteristic value is calculated, the processing quality of the core paper is identified, and the equipment status is performed based on the characteristic value. Monitoring and maintenance management.

Benefits of technology

It realizes accurate identification of core paper processing quality, reduces the defective rate of corrugated paper processing, and promptly maintains it through equipment failure reminders, improving processing quality and yield rate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118219613B_ABST
    Figure CN118219613B_ABST
Patent Text Reader

Abstract

The invention discloses a production process for corrugated paper. After core paper is processed by corrugating rollers to produce UV waveforms, characteristic data of the core paper after being processed by the corrugating rollers is obtained, and a core paper characteristic value is obtained based on the core paper characteristic data. By processing the core paper characteristic value, the processing equipment of the corrugated paper and the state of the core paper are identified, that is, the core paper groove width behavior value is obtained through the groove width of each core paper subunit, the core paper groove depth behavior value is obtained through the groove depth of each core paper subunit, and the core paper flatness behavior value is obtained through the integrated value of each core paper subunit. That is, the core paper groove width behavior value, the core paper groove depth behavior value and the core paper flatness behavior value are processed to obtain the overall processing quality of the core paper, thereby achieving characterization of the core paper state from multiple aspects such as the processing size of the groove of the core paper, the processing depth of the groove and the processing surface flatness of the groove, so that the identification of the core paper processing quality is more accurate, and the defective rate of corrugated paper processing is effectively reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of packaging materials, and in particular to a production process of corrugated paper. Background Art

[0002] Corrugated cardboard is a plate-like material made of face paper, backing paper and core paper processed into corrugated shapes by corrugating rollers. It has the advantages of low cost, light weight, easy processing, high strength, excellent printing adaptability, and convenient storage and transportation. It is widely used.

[0003] For example, patent application number 202211096914.3 discloses a production process for multi-layer corrugated paper. The production process of the present invention includes the following steps: step S1, preparing an impregnation solution with modified nano titanium dioxide added; step S2, preparing a modified polyurethane coating with modified nano zirconium dioxide added; step S3, preparing a modified silicate adhesive with polyvinyl alcohol added; step S4, immersing the corrugated paper core paper, face paper, and bottom paper in the impregnation solution, coating the modified polyurethane coating after drying, and curing at high temperature. After the core paper is processed with a corrugated roller to produce a UV waveform, a modified silicate adhesive is coated on the surface, adhered between the face paper and the bottom paper, and heated and bonded, and cooled to obtain a multi-layer corrugated paperboard.

[0004] It can be seen from the above scheme that in the prior art, the core paper layer plays a very important role in the processing of corrugated paper. Once the processing quality of the core paper layer is poor, the overall quality of the corrugated paper will be poor and the defective rate of the corrugated paper will be high.

[0005] In the prior art, there is a lack of identification of the processing quality of corrugated paper core paper, and the processing quality of corrugated paper cannot be effectively guaranteed. Summary of the invention

[0006] The object of the present invention is to provide a production process for corrugated paper, by dividing the core paper into several core paper sub-units according to a V-shaped bottom, obtaining the core paper groove width behavior value through the groove width of each core paper sub-unit, obtaining the core paper groove depth behavior value through the groove depth of each core paper sub-unit, and obtaining the core paper flatness behavior value through the integration value of each core paper sub-unit, that is, the overall processing quality of the core paper is obtained by processing the core paper groove width behavior value, the core paper groove depth behavior value and the core paper flatness behavior value, thereby achieving characterization of the core paper state from multiple aspects such as the processing size of the core paper groove, the processing depth of the groove, and the processing surface flatness of the groove, so that the identification of the core paper processing quality is more accurate.

[0007] The technical problems solved by the present invention are:

[0008] The purpose of the present invention can be achieved by the following technical solutions:

[0009] A production process for corrugated paper comprises the following steps:

[0010] Step 1: Soak the corrugated paper core paper, face paper and base paper in the impregnation liquid;

[0011] Step 2: After taking out and drying, evenly apply modified polyurethane coating on the surface of core paper, face paper and base paper, cure at 105℃ for 1h, and set aside;

[0012] Step 3: After the core paper is processed into UV waveform by corrugating rollers, a modified silicate adhesive is coated on the surface;

[0013] Acquire the core paper feature data after the core paper is processed by the corrugated roller, and obtain the core paper feature value based on the core paper feature data. By processing the core paper feature value, the processing equipment of the corrugated paper and the core paper state are identified;

[0014] Step 4: Glue the core paper between the face paper and the base paper, place at room temperature for 2 hours, heat to 110°C and dry for 12 hours, and obtain a multi-layer corrugated cardboard after cooling.

[0015] As a further solution of the present invention: the core paper characteristic data includes a core paper groove width behavior value, a core paper groove depth behavior value and a core paper flatness behavior value;

[0016] The core paper slot width behavior value is marked as E i;

[0017] The core paper slot depth behavior value is marked as D i;

[0018] The core paper flatness behavior value is marked as Yi;

[0019] That is, through the formula The core paper characteristic value EDY is calculated, wherein a1, a2 and a3 are preset proportional coefficients.

[0020] As a further solution of the present invention: the process of obtaining the core paper slot width behavior value is:

[0021] Divide the core paper into a number of core paper sub-units according to the V-shaped bottom, that is, each V-shaped bottom is a core paper sub-unit;

[0022] Select multiple groove width measurement points along the groove direction of the V-shaped bottom in the core paper subunit, and obtain the groove width value obtained at each groove width measurement point;

[0023] Add up all the slot width values ​​on the core paper sub-unit and take the average to get the slot width value of the core paper sub-unit;

[0024] The groove width values ​​of all core paper sub-units are calculated according to the standard deviation formula to obtain the core paper groove width behavior value.

[0025] As a further solution of the present invention: the process of obtaining the core paper groove depth behavior value is:

[0026] Select multiple groove bottom measuring points along the groove direction of the V-shaped bottom in the core paper subunit, and obtain the groove depth value obtained at each groove bottom measuring point;

[0027] Add up all the groove depth values ​​on the core paper sub-unit and take the average value to obtain the groove depth value of the core paper sub-unit;

[0028] The groove depth values ​​of all core paper sub-units are calculated according to the standard deviation formula to obtain the core paper groove depth behavior value.

[0029] As a further solution of the present invention: the process of obtaining the flat behavior value of the core paper is:

[0030] Divide the core paper sub-unit into a number of micro sub-units along the groove direction;

[0031] The core paper subunit is divided into the first side, the V-shaped bottom and the second side according to the structure;

[0032] Obtaining measurement values ​​of the first side surface, the V-shaped bottom, and the second side surface in the micro-subunit by a level measurement method to obtain a measurement value group;

[0033] Based on the measurement value group, the first side variance value of the core paper subunit, the second side variance value of the core paper subunit, and the V-shaped bottom variance value of the core paper subunit are obtained.

[0034] As a further solution of the present invention: weighting the variance value of the first side of the core paper subunit, the variance value of the second side of the core paper subunit and the variance value of the V-shaped bottom of the core paper subunit to obtain an integrated value of the core paper subunit;

[0035] The integrated values ​​of all core paper sub-units are summed and averaged to obtain the core paper flatness behavior value.

[0036] As a further solution of the present invention: presetting the core paper characteristic value threshold as edy, and comparing the core paper characteristic value EDY with the core paper characteristic value threshold edy;

[0037] When the core paper characteristic value EDY> the core paper characteristic value threshold edy, it means that the core paper corrugated roller processing is normal, and a core paper processing normal signal is generated;

[0038] When the core paper characteristic value EDY is less than the core paper characteristic value threshold edy, it indicates that the core paper corrugated roller processing is abnormal, and an equipment processing verification signal is generated.

[0039] As a further solution of the present invention: based on the normal signal of core paper processing;

[0040] The core paper characteristic values ​​of n corrugated paper processing processes are collected in an interval collection method;

[0041] Establish an XY two-dimensional plane coordinate system, with the number of acquisitions as the X-axis and the core paper characteristic value as the Y-axis;

[0042] The n-time collection is arranged in chronological order on the X-axis, and then the core paper characteristic values ​​in the n-time corrugated paper processing process are used as Y values ​​to plot points in the coordinate system, and then the points in the coordinate system are smoothly connected in chronological order to obtain the trend graph of the n-time core paper characteristic values.

[0043] As a further solution of the present invention: if the trend graph of the core paper characteristic value for n times is a linear type inclined upward or a linear type inclined downward as a whole, the core paper characteristic value collected for the last time and the core paper characteristic value collected for the first time are calculated by difference to obtain the core paper characteristic value change rate;

[0044] Then, the core paper characteristic value threshold is calculated by difference with the core paper characteristic value collected last time to obtain the core paper characteristic value capacity;

[0045] The ratio of the core paper characteristic value capacity to the core paper characteristic value change rate is calculated to obtain the core paper processing times margin.

[0046] As a further solution of the present invention: if the trend graph of the characteristic value of the n-time core paper is a fluctuating line as a whole, it means that within the n times of processing of the corrugated paper collected, the processing equipment is in a dynamic constant state.

[0047] Beneficial effects of the present invention:

[0048] (1) The present invention divides the core paper into a plurality of core paper sub-units according to the V-shaped bottom, obtains the core paper groove width behavior value through the groove width of each core paper sub-unit, obtains the core paper groove depth behavior value through the groove depth of each core paper sub-unit, and obtains the core paper flatness behavior value through the integrated value of each core paper sub-unit, that is, the core paper groove width behavior value, the core paper groove depth behavior value and the core paper flatness behavior value are processed to obtain the overall processing quality of the core paper, thereby achieving characterization of the core paper state from multiple aspects such as the processing size of the groove of the core paper, the processing depth of the groove, and the processing surface flatness of the groove, so that the identification of the core paper processing quality is more accurate, and the defective rate of corrugated paper processing is effectively reduced;

[0049] (2) The present invention collects the core paper characteristic values ​​in the corrugated paper processing process in an interval acquisition manner based on the normal signal of core paper processing, and establishes a plane coordinate system to identify the collected core paper characteristic values, that is, by obtaining the core paper characteristic value capacity and the core paper characteristic value change rate, the core paper characteristic value capacity and the core paper characteristic value change rate are calculated to obtain the core paper processing times margin. Based on the core paper processing times margin, the core paper processing equipment is maintained and managed when it is close to the core paper processing times margin, so as to effectively prevent the core paper processing from being scrapped and improve the core paper processing quality and yield rate. BRIEF DESCRIPTION OF THE DRAWINGS

[0050] The present invention will be further described below in conjunction with the accompanying drawings.

[0051] Figure 1 It is a flow chart of a production process of corrugated paper of the present invention;

[0052] Figure 2 The present invention discloses a flow chart of processing core paper characteristic values ​​and core paper characteristic value threshold values ​​in a production process of corrugated paper. DETAILED DESCRIPTION

[0053] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0054] See also Figure 1-Figure 2 As shown, the present invention is a production process of corrugated paper, comprising the following steps:

[0055] Step 1: Soak the corrugated paper core paper, face paper and base paper in the impregnation liquid;

[0056] Step 2: After taking out and drying, evenly apply modified polyurethane coating on the surface of core paper, face paper and base paper, cure at 105℃ for 1h, and set aside;

[0057] Step 3: After the core paper is processed into UV waveform by corrugating rollers, a modified silicate adhesive is coated on the surface;

[0058] Acquire the core paper feature data after the core paper is processed by the corrugated roller, and obtain the core paper feature value based on the core paper feature data. By processing the core paper feature value, the processing equipment of the corrugated paper and the core paper state are identified;

[0059] Step 4: Glue the core paper between the face paper and the base paper, place at room temperature for 2 hours, heat to 110°C and dry for 12 hours, and obtain a multi-layer corrugated cardboard after cooling.

[0060] In step 3, the core paper characteristic data includes a core paper groove width behavior value, a core paper groove depth behavior value, and a core paper flatness behavior value;

[0061] The process of obtaining the core paper slot width behavior value is as follows:

[0062] Divide the core paper into a number of core paper sub-units according to the V-shaped bottom, that is, each V-shaped bottom is a core paper sub-unit;

[0063] Select multiple groove width measurement points along the groove direction of the V-shaped bottom in the core paper subunit, and obtain the groove width value obtained at each groove width measurement point;

[0064] Add up all the slot width values ​​on the core paper sub-unit and take the average to get the slot width value of the core paper sub-unit;

[0065] Integrate the groove width values ​​of all core paper sub-units to obtain a groove width value group of the core paper sub-unit;

[0066] The core paper slot width behavior value is obtained by calculating the slot width value group of the core paper sub-unit according to the standard deviation formula;

[0067] In this embodiment, three groove width measurement points are selected, one of which is set at the middle position of the core paper subunit along the groove direction, and the other two groove width measurement points are respectively set at both ends of the core paper subunit;

[0068] The process of obtaining the core paper slot depth behavior value is as follows:

[0069] Select multiple groove bottom measuring points along the groove direction of the V-shaped bottom in the core paper subunit, and obtain the groove depth value obtained at each groove bottom measuring point;

[0070] Add up all the groove depth values ​​on the core paper sub-unit and take the average value to obtain the groove depth value of the core paper sub-unit;

[0071] Integrate the groove depth values ​​of all core paper sub-units to obtain a groove depth value group of the core paper sub-unit;

[0072] The groove depth value group of the core paper sub-unit is calculated according to the standard deviation formula to obtain the core paper groove depth behavior value;

[0073] In this embodiment, three groove depth measurement points are selected, one of which is set at the middle position of the core paper subunit along the groove direction, and the other two groove depth measurement points are respectively set at both ends of the core paper subunit;

[0074] The process of obtaining the core paper flatness behavior value is as follows:

[0075] Divide the core paper sub-unit into a number of micro sub-units along the groove direction;

[0076] The core paper subunit is divided into the first side, the V-shaped bottom and the second side according to the structure;

[0077] Obtaining measurement values ​​of the first side surface, the V-shaped bottom, and the second side surface in the micro-subunit by means of a level measurement method;

[0078] Taking the first micro-subunit as a reference, obtain the measurement value of the first side surface, the measurement value of the V-shaped bottom, and the measurement value of the second side surface of each subsequent micro-subunit by means of a level measurement method;

[0079] The measured values ​​of the first side surface of all the micro sub-units are calculated according to the variance calculation formula to obtain the variance value of the first side surface of the core paper sub-unit;

[0080] The measured values ​​of the second side surface of all the micro sub-units are calculated according to the variance calculation formula to obtain the variance value of the second side surface of the core paper sub-unit;

[0081] The measured values ​​of the V-shaped bottom of all the micro sub-units are calculated according to the variance calculation formula to obtain the variance value of the V-shaped bottom of the core paper sub-unit;

[0082] The first side variance value of the core paper subunit, the second side variance value of the core paper subunit and the V-shaped bottom variance value of the core paper subunit are weighted to obtain an integrated value of the core paper subunit;

[0083] In a specific embodiment, the variance value of the first side of the core paper subunit is recorded as D1, the variance value of the second side of the core paper subunit is recorded as D2, and the variance value of the V-shaped bottom of the core paper subunit is recorded as D3. The weight proportion of the variance value D1 of the first side of the core paper subunit is n1, the weight proportion of the variance value D2 of the second side of the core paper subunit is n2, and the weight proportion of the variance value of the V-shaped bottom of the core paper subunit is n3;

[0084] The integrated value D of the core paper subunit is calculated according to the formula D=D1*n1+D2*n2+D3*n3, where n1, n2, and n3 are all greater than 0; and n1+n2+n3=1;

[0085] Then the integrated values ​​of all the core paper sub-units are summed and averaged to obtain the core paper flatness behavior value;

[0086] The core paper slot width behavior value is marked as E i;

[0087] The core paper slot depth behavior value is marked as D i;

[0088] The core paper flatness behavior value is marked as Yi;

[0089] That is, through the formula The core paper characteristic value EDY is calculated, wherein a1, a2 and a3 are preset proportional coefficients;

[0090] The core paper characteristic value threshold is preset as edy, and the core paper characteristic value EDY is compared with the core paper characteristic value threshold edy;

[0091] When the core paper characteristic value EDY> the core paper characteristic value threshold edy, it means that the core paper corrugated roller processing is normal, and a core paper processing normal signal is generated;

[0092] When the core paper characteristic value EDY is less than the core paper characteristic value threshold edy, it indicates that the core paper corrugated roller processing is abnormal, and an equipment processing verification signal is generated.

[0093] Based on equipment processing verification signal

[0094] Obtain the core paper characteristic values ​​of the core paper in the production processes of multiple consecutive corrugated papers after the current corrugated paper. If the core paper characteristic values ​​of the core paper in the production processes of multiple consecutive corrugated papers are all less than the core paper characteristic value threshold, a corrugated paper processing equipment fault signal is obtained;

[0095] Based on the fault signals of corrugated paper processing equipment, repair the core paper processing equipment;

[0096] If the core paper characteristic value of the core paper in multiple consecutive corrugated paper production processes is less than or less than the core paper characteristic value threshold, a corrugated paper verification signal is obtained;

[0097] Based on the corrugated paper verification signal, the process of obtaining the core paper in step two or step one is inspected.

[0098] Based on normal signal of core paper processing

[0099] The core paper characteristic value of the mth corrugated paper processing process is obtained in an interval collection manner, that is, in a 20n+1 manner, where n is the number of collections, and n is 0, 1, 2, 3...n;

[0100] Establish an XY two-dimensional plane coordinate system, with the number of acquisitions as the X-axis and the core paper characteristic value as the Y-axis;

[0101] The n-time collection is set on the X-axis in chronological order, and then the core paper characteristic values ​​in the n-time corrugated paper processing process are used as Y values ​​to plot points in the coordinate system, and then the points in the coordinate system are smoothly connected in chronological order to obtain the trend graph of the n-time core paper characteristic values;

[0102] If the core paper characteristic value trend graph for n times is an upward sloping line or a downward sloping line as a whole, the core paper characteristic value collected for the last time and the core paper characteristic value collected for the first time are calculated by difference to obtain the core paper characteristic value change rate;

[0103] Then, the core paper characteristic value threshold is calculated by difference with the core paper characteristic value collected last time to obtain the core paper characteristic value capacity;

[0104] The core paper characteristic value capacity and the core paper characteristic value change rate are calculated to obtain the core paper processing times margin;

[0105] Based on the allowance of core paper processing times, the core paper processing equipment is maintained and managed when it is close to the allowance of core paper processing times, effectively preventing the core paper processing from being scrapped;

[0106] If the trend graph of the characteristic values ​​of the n-time core paper is a fluctuating line as a whole, it means that the processing equipment is in a dynamic constant state within the n times of processing of the corrugated paper collected.

[0107] Working principle: The core paper is divided into several core paper sub-units according to the V-shaped bottom, and the core paper groove width behavior value is obtained through the groove width of each core paper sub-unit, the core paper groove depth behavior value is obtained through the groove depth of each core paper sub-unit, and the core paper flatness behavior value is obtained through the integrated value of each core paper sub-unit. That is, the core paper groove width behavior value, the core paper groove depth behavior value and the core paper flatness behavior value are processed to obtain the overall processing quality of the core paper, so as to characterize the core paper state from multiple aspects such as the processing size of the core paper groove, the processing depth of the groove, and the processing surface flatness of the groove, so as to make the identification of the core paper processing quality more accurate and effectively reduce the defective rate of corrugated paper processing;

[0108] At the same time, based on the equipment processing verification signal, the core paper characteristic value of the core paper in the production process of multiple consecutive corrugated papers after the current corrugated paper is identified. If the core paper characteristic value of the core paper in the production process of multiple consecutive corrugated papers is less than the core paper characteristic value threshold, a corrugated paper processing equipment fault signal is obtained to remind personnel to repair the core paper processing equipment.

[0109] If the core paper characteristic value of the core paper in multiple consecutive corrugated paper production processes is less than or lower than the core paper characteristic value threshold, a corrugated paper verification signal is obtained to identify the core paper obtained in step two or step one.

[0110] The above is a detailed description of an embodiment of the present invention, but the content is only a preferred embodiment of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made within the scope of the present invention should still fall within the scope of the patent coverage of the present invention.

Claims

1. A process for producing corrugated paper, characterized in that: The following steps are involved: Step 1: Soak the corrugated paper core paper, face paper and base paper in the impregnation liquid; Step 2: After taking out and drying, evenly apply modified polyurethane coating on the surface of core paper, face paper and base paper, cure at 105℃ for 1h, and set aside; Step 3: After the core paper is processed into UV waveform by corrugating rollers, a modified silicate adhesive is coated on the surface; Acquire the core paper feature data after the core paper is processed by the corrugated roller, and obtain the core paper feature value based on the core paper feature data. By processing the core paper feature value, the processing equipment of the corrugated paper and the core paper state are identified; Step 4: adhere the core paper between the face paper and the base paper, place at room temperature for 2 hours, heat to 110°C and dry for 12 hours, and obtain a multi-layer corrugated paperboard after cooling; In step 3, the core paper characteristic data includes a core paper groove width behavior value, a core paper groove depth behavior value, and a core paper flatness behavior value; The core paper slot width behavior value is marked as Ei; The core paper slot depth behavior value is marked as Di; The core paper flatness behavior value is marked as Yi; That is, through the formula The core paper characteristic value EDY is calculated, wherein a1, a2 and a3 are preset proportional coefficients; The process of obtaining the core paper slot width behavior value is as follows: Divide the core paper into a number of core paper sub-units according to the V-shaped bottom, that is, each V-shaped bottom is a core paper sub-unit; Select multiple groove width measurement points along the groove direction of the V-shaped bottom in the core paper subunit, and obtain the groove width value obtained at each groove width measurement point; Add up all the slot width values ​​on the core paper sub-unit and take the average to get the slot width value of the core paper sub-unit; The groove width values ​​of all core paper sub-units are calculated according to the standard deviation formula to obtain the core paper groove width behavior value; The process of obtaining the core paper slot depth behavior value is as follows: Select multiple groove bottom measuring points along the groove direction of the V-shaped bottom in the core paper subunit, and obtain the groove depth value obtained at each groove bottom measuring point; Add up all the groove depth values ​​on the core paper sub-unit and take the average value to obtain the groove depth value of the core paper sub-unit; The groove depth values ​​of all core paper sub-units are calculated according to the standard deviation formula to obtain the core paper groove depth behavior value; The process of obtaining the core paper flatness behavior value is as follows: Divide the core paper sub-unit into a number of micro sub-units along the groove direction; The core paper subunit is divided into the first side, the V-shaped bottom and the second side according to the structure; Obtaining measurement values ​​of the first side surface, the V-shaped bottom, and the second side surface in the micro-subunit by a level measurement method to obtain a measurement value group; Based on the measurement value group, obtain the first side variance value of the core paper subunit, the second side variance value of the core paper subunit, and the V-shaped bottom variance value of the core paper subunit; The first side variance value of the core paper subunit, the second side variance value of the core paper subunit and the V-shaped bottom variance value of the core paper subunit are weighted to obtain an integrated value of the core paper subunit; The integrated values ​​of all core paper sub-units are summed and averaged to obtain the core paper flatness behavior value; The core paper characteristic value threshold is preset as edy, and the core paper characteristic value EDY is compared with the core paper characteristic value threshold edy; When the core paper characteristic value EDY> the core paper characteristic value threshold edy, it means that the core paper corrugated roller processing is normal, and a core paper processing normal signal is generated; When the core paper characteristic value EDY is less than the core paper characteristic value threshold edy, it indicates that the core paper corrugated roller processing is abnormal, and an equipment processing verification signal is generated; Based on normal signal of core paper processing; The core paper characteristic values ​​of n corrugated paper processing processes are collected in an interval collection method; Establish an XY two-dimensional plane coordinate system, with the number of acquisitions as the X-axis and the core paper characteristic value as the Y-axis; The n-time collection is set on the X-axis in chronological order, and then the core paper characteristic values ​​in the n-time corrugated paper processing process are used as Y values ​​to plot points in the coordinate system, and then the points in the coordinate system are smoothly connected in chronological order to obtain the trend graph of the n-time core paper characteristic values; If the core paper characteristic value trend graph for n times is an upward sloping line or a downward sloping line as a whole, the core paper characteristic value collected for the last time and the core paper characteristic value collected for the first time are calculated by difference to obtain the core paper characteristic value change rate; Then, the core paper characteristic value threshold is calculated by difference with the core paper characteristic value collected last time to obtain the core paper characteristic value capacity; The core paper characteristic value capacity and the core paper characteristic value change rate are calculated to obtain the core paper processing times margin; If the trend graph of the characteristic values ​​of the n-time core paper is a fluctuating line as a whole, it means that the processing equipment is in a dynamic constant state within the n times of processing of the corrugated paper collected.

Citation Information

Patent Citations

  • Production process of multi-layer corrugated board

    CN116080153A

  • Corrugated paper rib line defect degree evaluation method based on image processing

    CN116912256A

  • Multi-layer absorbent cores and methods of manufacture

    US20220241119A1

  • Measurement of variation in flute profile height

    US4800286A

  • Laser-based measurement apparatus and method for the on-line measurement of multiple corrugated board characteristics

    US5581353A