A forest fire extinguishing agent and preparation method thereof

By surface modification and coating the flame retardant, the water-based forest fire extinguishing agent formed a core-shell structure, the problems of existing fire extinguishing agents being low in efficiency and environmental pollution in forest fires are solved, and efficient and environmentally friendly fire extinguishing effects are achieved The ecological security of Helin District.

CN118286646BActive Publication Date: 2024-11-19BEIJING WEIDE AIKE BIOTECHNOLOGY RESEARCH INSTITUTE CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410409761.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-07
Publication Date
2024-11-19
Estimated Expiration
2044-04-07

AI Technical Summary

Technical Problem

Existing fire extinguishing agents are inefficient when extinguishing forest fires, and commonly used dry powder, foam, and gas fire extinguishing agents are difficult to effectively land in violent airflow. Imported halogen-based fire extinguishing agents release toxic substances at high temperatures, polluting the environment.

Method used

The flame retardant is surface modified by coupling agent, coated with hydrophobic polymer monomer to form a core-shell structure covering, and combined with in-situ polymer polymer polymer polymerization, a highly efficient and environmentally friendly type is prepared Water-based forest fire extinguishing agent can quickly disperse in water. After adding 10-20 times of water to dilute it to achieve a level 2A fire extinguishing effect, and no toxic substances are produced at high temperatures.

Benefits of technology

It achieves an efficient and environmentally friendly forest fire extinguishing effect, simplifies the use method, ensures the ecological security of the forest area, and is easy to obtain raw materials, and is simple in the preparation process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure HDA0004823999420000011
    Figure HDA0004823999420000011
Patent Text Reader

Abstract

The invention discloses a forest fire extinguishing agent and a preparation method thereof, the method comprising the following steps: stirring and mixing a first flame retardant and a coupling agent to obtain a first material; adding a hydrophobic polymer monomer or adding a hydrophobic polymer monomer and an initiator to the first material, stirring to obtain a second material; adding a surfactant to the second material under stirring, heating to obtain a third material; dissolving a hydrophilic polymer in water, adding the third material, heating and stirring after homogenization, and reacting at a constant temperature to obtain a fourth material; cooling the fourth material, adding a flame retardant additive and water, stirring to obtain a forest fire extinguishing agent. The forest fire extinguishing agent of the present invention can be quickly dispersed in water, and the fire extinguishing effect can reach the "2A" high efficiency standard after adding 10-20 times of water dilution, and there is no corrosion to metal, and no toxic substances are produced at high temperature.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of fire extinguishing agents, and in particular relates to a forest fire extinguishing agent and a preparation method thereof. Background Art

[0002] Forest fires occur every year, often causing serious ecological and environmental disasters and significant loss of life and property. There are many types of fire extinguishing agents, but the commonly used dry powder fire extinguishing agents, foam fire extinguishing agents and gas fire extinguishing agents are not suitable for extinguishing forest and grassland fires. Due to the intense air flow in the fire area, it is difficult for the above-mentioned fire extinguishing agents to land on the burning objects.

[0003] Water is the cheapest fire extinguisher, but it is inefficient in extinguishing forest fires. Its function is to reduce the surface temperature of combustibles. Forest fires are characterized by large range, high temperature and fierce fire. It is difficult to extinguish forest fires with a small amount of water.

[0004] At present, my country spends a large amount of foreign exchange every year to import "halon" type halogen-containing forest fire extinguishing agents, but halogen-based fire extinguishing agents release toxic substances at high temperatures, seriously polluting the environment. Summary of the invention

[0005] In view of the deficiencies in the prior art, the present invention provides a forest fire extinguishing agent and a preparation method thereof. The surface of a flame retardant is first modified with a coupling agent, and then the modified flame retardant is coated with a hydrophobic polymer monomer. Under the action of a hydrophilic polymer, in-situ polymerization is performed to form a coating body with a core-shell structure. The diameter of the coating body ranges from several microns to tens of microns, and the coating body can be quickly dispersed and suspended in water. After being diluted with 10-20 times of water, the fire extinguishing effect can reach the 2A level of "National Standard GB17835-2008. Water-based Fire Extinguishing Agent". No toxic substances are produced at high temperatures, and there is no impact on the ecology of the forest area. It is highly efficient and environmentally friendly.

[0006] To achieve the above object, the first aspect of the present invention discloses a method for preparing a forest fire extinguishing agent, comprising the following steps:

[0007] (1) stirring and mixing the first flame retardant and the coupling agent to obtain a first material;

[0008] (2) adding a hydrophobic polymer monomer or a hydrophobic polymer monomer and an initiator to the first material, and stirring the mixture to obtain a second material;

[0009] (3) adding a surfactant to the second material under stirring and heating to obtain a third material;

[0010] (4) dissolving the hydrophilic polymer in water and adding the mixture to the third material, homogenizing the mixture, heating and stirring the mixture, and reacting the mixture at a constant temperature to obtain a fourth material;

[0011] (5) Cool the fourth material, add a flame retardant additive and water, and stir evenly to obtain a forest fire extinguishing agent.

[0012] The first flame retardant is at least one of a guanidine salt flame retardant, an ammonium salt flame retardant, and / or a phosphorus-based flame retardant.

[0013] In a preferred embodiment of the present invention, the amount of the guanidine salt flame retardant is 5-30 parts by weight, the amount of the phosphorus flame retardant is 5-35 parts by weight, and the amount of the ammonium salt flame retardant is 5-25 parts by weight.

[0014] The present invention firstly performs surface modification treatment on a plurality of flame retardants with a coupling agent, and then coats the modified flame retardants with a hydrophobic polymer monomer, and in situ polymerizes under the action of a hydrophilic polymer to form a coating body with a core-shell structure, thereby preparing a highly efficient and environmentally friendly water-based forest fire extinguishing agent. The forest fire extinguishing agent can be quickly dispersed in water, and the fire extinguishing effect can reach the "2A" high efficiency standard after adding 10-20 times of water for dilution. The method of use is simple, no toxic substances are generated at high temperature, no impact on the ecology of the forest area, and high efficiency and environmental protection.

[0015] Guanidine salt flame retardants are non-toxic, highly efficient, environmentally friendly, and safe, and are the main agents of forest killers. They have a fast natural degradation rate, and guanidine decomposes into nitrogen, water, and urea-like substances at high temperatures, which can dilute oxygen, quickly reduce the oxygen content in the air, cover and block the burning materials, and extinguish the fire. Ammonium salt flame retardants are non-toxic, highly efficient, environmentally friendly, and safe, and have obvious flame retardant effects. They are the traditional main flame retardant agents.

[0016] The present invention compounds the guanidine salt flame retardant and the ammonium salt flame retardant so that the flame retardants can fully exert the synergistic effect.

[0017] Further, in step (1), the amount of guanidine salt flame retardant is 5-30 parts by weight, and the amount of ammonium salt flame retardant is 5-25 parts by weight. Preferably, the guanidine salt flame retardant is selected from one or more of polymerized guanidine, guanidine carbonate, guanidine nitrate, guanidine acetate, guanidine phosphate, guanidine borate, guanidine sulfate, guanidine oxalate, and guanidine benzoate. More preferably, the guanidine salt flame retardant is selected from one or more of guanidine carbonate, guanidine phosphate, and guanidine borate. The ammonium salt flame retardant is selected from one or more of ammonium sulfate, ammonium carbonate, ammonium phosphate, diammonium phosphate, diammonium bicarbonate, and polyammonium phosphate. More preferably, the ammonium salt flame retardant is selected from one or more of ammonium phosphate, diammonium phosphate, and polyammonium phosphate.

[0018] In a preferred embodiment of the present invention, in step (2), the initiator is added to an oily carrier and then added to the first material. Preferably, the oily carrier is selected from at least one of mineral oil, petroleum ether and paraffin.

[0019] In order to further improve the flame retardant effect, a second flame retardant is further added in step (4), wherein the second flame retardant is a metal hydroxide flame retardant, and the amount used is 2-15 parts by weight.

[0020] Metal hydroxide flame retardants decompose into a large amount of water and metal oxides at high temperatures. Water can rapidly reduce the surface temperature of the burning material, and the metal oxides can cover the surface of the burning material to block the oxidation reaction. The produced metal oxides can not only block the oxidation of the burning material at high temperature, but also eliminate smoke and improve the transparency of the air in the fire area.

[0021] Phosphorus-based flame retardants decompose into phosphoric acid, polymetaphosphoric acid, metaphosphoric acid and other acids with strong dehydration effect when heated. These acids rapidly dehydrate and carbonize the surface of plants, forming a dense phosphorus-containing carbonized layer, blocking the oxidation reaction, absorbing the oxidation heat energy on the surface of the burning object, and isolating from air and heat sources.

[0022] Preferably, the metal hydroxide is selected from one or more of magnesium hydroxide, iron hydroxide, aluminum hydroxide, calcium hydroxide, and zinc oxide. More preferably, the metal hydroxide is selected from one or more of aluminum hydroxide, calcium hydroxide, and magnesium hydroxide.

[0023] Preferably, the phosphorus flame retardant is selected from one or more of coated red phosphorus, phosphate, methyl phosphate, ethyl phosphate, butyl phosphate, zinc phosphate, isooctyl phosphate, isopropylated triphenyl phosphate, phenyl phosphate, and dimethyl methyl phosphate. More preferably, the phosphorus flame retardant is selected from one or more of coated red phosphorus, isooctyl phosphate, and isopropylated triphenyl phosphate.

[0024] Further, the coupling agent is selected from one or more of butyl titanate, aluminate, silane coupling agent, phosphate coupling agent, borate coupling agent, and the amount of the coupling agent is 0.1-5.0 parts by weight. The silane coupling agent can be KH550, KH560, KH570 or KH792. More preferably, it is selected from one or more of silane coupling agent and butyl titanate.

[0025] The solvent for dissolving the coupling agent is selected from one or more of ethanol, methanol, butanol, acetone, dimethylformamide, dichloromethane, and chloroform. Preferably, it is selected from one or more of ethanol, acetone, and dichloromethane. The amount of the solvent is 1-10 parts by weight.

[0026] Further, the hydrophobic polymer monomer is selected from one or more of methyl acrylate, ethyl acrylate, butyl acrylate, glycidyl methacrylate, 1,4-butanediol dimethacrylate, methyl methacrylate, ethyl acetoacetate methacrylate, isophorone diisocyanate, and toluene diisocyanate, and the amount of the hydrophobic polymer monomer is 0.5-20 parts by weight; the initiator is selected from one or more of azobisisobutyronitrile, potassium persulfate, ammonium persulfate, and benzoyl peroxide, preferably, one or more of azobisisobutyronitrile and potassium persulfate. The mass ratio of the initiator to the hydrophobic polymer monomer is 0.01%-5.00%. The surfactant is selected from one or more of propylene glycol monolaurate, sorbitan monostearate, polyoxyethylene sorbitan monooleate, sorbitan laurate, sodium lauryl sulfate, sodium dodecylbenzene sulfonate, diethylene glycol fatty acid ester, sorbitan monopalmitate, polyoxypropylene stearate, polyoxyethylene sorbitan trioleate, and sorbitan monooleate polyoxyethylene ether, and the ratio of the surfactant to the hydrophobic polymer monomer is 0.2-50:100; the hydrophilic polymer is selected from one or more of polyvinyl alcohol, polyethylene glycol, acrylamide, N-hydroxymethyl acrylamide, N-hydroxyethyl acrylamide, acrylonitrile, and diethylenetriamine, and the amount of the hydrophilic polymer is 0.1-10 parts by weight.

[0027] In order to make the hydrophobic polymer monomer more evenly coated on the surface of the flame retardant, in step (2), a hydrophobic ester can be selected as a diluent or solvent.

[0028] Furthermore, in step (4), the homogenization time is 1-60 min, preferably 10-30 min; in step (4), the constant temperature heating temperature is 45°C-90°C, preferably 45°C-80°C, and the constant temperature reaction time is 0.5h-8.0h, preferably 1-3h.

[0029] Furthermore, the flame retardant additive is selected from one or more of silicon dioxide nanopowder, ammonium polyphosphate, sodium silicate, silica sol, aluminum hydroxide, and ammonium dihydrogen phosphate. The amount of the flame retardant additive is 1 to 10 parts by weight.

[0030] To achieve the above-mentioned object, the second aspect of the present invention discloses a forest fire extinguishing agent, which is prepared by the preparation method of the first aspect.

[0031] To achieve the above-mentioned object, the third aspect of the present invention discloses a forest fire extinguishing agent, which comprises: a flame retardant component having a core-shell structure, and a carrier;

[0032] In the core-shell structured flame retardant, the core material includes a first flame retardant, the shell material includes a water-absorbing polymer, the first flame retardant is at least one of a guanidine salt flame retardant, an ammonium salt flame retardant, and / or a phosphorus-based flame retardant; preferably, the shell material further includes a second flame retardant, and the second flame retardant is a metal hydroxide flame retardant.

[0033] Furthermore, the carrier is water.

[0034] Furthermore, the carrier is a solution or a mixed solution including water and a flame retardant additive.

[0035] Furthermore, the flame retardant additive is selected from one or more of silicon dioxide nanopowder, ammonium polyphosphate, sodium silicate, silica sol, aluminum hydroxide, and ammonium dihydrogen phosphate.

[0036] Compared with the prior art, the forest fire extinguishing agent of the present invention has a simple preparation method, and the raw materials are easy to obtain, and a polymer forest fire extinguishing agent that can be dispersed in water is prepared. Moreover, the forest fire extinguishing agent optimizes the combination of high-efficiency fire extinguishing agent raw materials, has high fire extinguishing efficiency, and the fire extinguishing effect can reach the 2A level of "National Standard GB17835-2008. Water-based Fire Extinguishing Agent" after adding 10-20 times of water for dilution. The method of use is simple, no toxic substances are produced at high temperature, no impact on the ecology of the forest area, and high efficiency and environmental protection. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 Schematic diagram of the structure of the paper strip used for flame retardant effect test. DETAILED DESCRIPTION

[0038] The present invention provides a forest fire extinguishing agent and a preparation method thereof. In the present invention, unless otherwise specified, all raw materials are commercially available products well known to those skilled in the art.

[0039] Embodiment 1:

[0040] (1) Weigh 150g of guanidine borate powder and 150g of ammonium polyphosphate, and premix them in a sand mill for 1h. Weigh 15g of silane coupling agent kH570, dissolve it in 80ml of dichloromethane, and drip it into the flame retardant under stirring for 30 minutes. Start the sand mill heater, keep the temperature at 45℃, continue stirring for 30 minutes, evaporate and remove the solvent, and obtain the modified first material.

[0041] (2) Weigh 8 g of methyl methacrylate and 8 g of 1,4-butanediol dimethacrylate, stir them evenly and add them to the first material. Further, dissolve 0.2 g of azobisisobutyronitrile in 20 g of mineral oil and add it to the first material. Heat to 40°C and continue stirring for 20 min to obtain the second material.

[0042] (3) Weigh 8 g of sorbitan monooleate polyoxyethylene ether, add it to the second material under stirring, mix well, heat to 50°C, and stir for 20 minutes to obtain the third material.

[0043] (4) Weigh 4 g of N-hydroxyethyl acrylamide, dissolve it in 400 ml (60°C) deionized water, and add it to the third material. After homogenization for 10 minutes, react at a constant temperature of 60°C for 4 hours to obtain the fourth material.

[0044] (5) The fourth material was cooled to 45° C., 50 g of silica sol was added, and the mixture was supplemented with deionized water to 1000 g. After stirring for 10 min, a forest fire extinguishing agent was obtained.

[0045] Embodiment 2:

[0046] (1) Weigh 150g of guanidine carbonate and 100g of ammonium polyphosphate, and premix them in a sand mill for 1 hour. Weigh 25g of silane coupling agent kH550, dissolve it in 100ml of dichloromethane, and drip it into the flame retardant under stirring for 30 minutes. Start the sand mill heater, keep the temperature at 45℃, continue stirring for 30 minutes, evaporate and remove the solvent, and obtain the modified first material.

[0047] (2) Weigh 80 g of glycidyl methacrylate and add it to the first material and mix well. Dissolve 1 g of dibenzoyl peroxide in 20 g of mineral oil and add it to the first material. Heat to 50° C. and continue stirring for 20 min to obtain a second material.

[0048] (3) Weigh 10 g of sodium dodecyl sulfate, add it to the second material under stirring, mix well, heat to 50° C., and stir for 20 min to obtain the third material.

[0049] (4) Weigh 50 g of acrylonitrile, 100 g of aluminum hydroxide, and 5 g of sodium carboxymethyl cellulose, dissolve them in 400 ml (60°C) deionized water, and add them to the third material. After homogenization for 10 min, react at a constant temperature of 60°C for 4 h to obtain the fourth material.

[0050] (5) The fourth material was cooled to room temperature, 40 g of silicon dioxide nanopowder was added, and the mixture was supplemented with deionized water to 1000 g. After stirring for 10 min, a forest fire extinguishing agent was obtained.

[0051] Embodiment 3:

[0052] (1) Weigh 150g of guanidine carbonate and 100g of ammonium polyphosphate, and premix them in a sand mill for 1 hour. Weigh 25g of silane coupling agent kH550, dissolve it in 100ml of dichloromethane, and drip it into the flame retardant under stirring for 30 minutes. Start the sand mill heater, keep the temperature at 45℃, continue stirring for 30 minutes, evaporate and remove the solvent, and obtain the modified first material.

[0053] (2) Weigh 80 g of glycidyl methacrylate and add it to the first material and mix well. Dissolve 1 g of dibenzoyl peroxide in 20 g of mineral oil and add it to the first material. Heat to 50° C. and continue stirring for 20 min to obtain a second material.

[0054] (3) Weigh 10 g of sodium dodecyl sulfate, add it to the second material under stirring, mix well, heat to 50° C., and stir for 20 min to obtain the third material.

[0055] (4) Weigh 50 g of acrylonitrile, 100 g of magnesium hydroxide, and 5 g of sodium carboxymethyl cellulose, dissolve them in 400 ml (60°C) deionized water, and add them to the third material. After homogenization for 10 min, react at a constant temperature of 60°C for 4 h to obtain the fourth material.

[0056] (5) The fourth material was cooled to room temperature, 40 g of silicon dioxide nanopowder was added, and the mixture was supplemented with deionized water to 1000 g. After stirring for 10 min, a forest fire extinguishing agent was obtained.

[0057] Embodiment 4:

[0058] (1) Weigh 150g of ammonium polyphosphate with a degree of polymerization n>25 and 50g of guanidine phosphate, place them in a sand mill and stir and premix for 1h. Weigh 15g of silane coupling agent KH550, dissolve it in 85ml of anhydrous ethanol, and drip it into the flame retardant powder under stirring. After 30 minutes, start the sand mill heater, keep the temperature at 60℃, continue stirring for 40 minutes, evaporate and remove the solvent, and obtain the modified first material.

[0059] (2) Weigh 8 g of methyl methacrylate and 4 g of ethyl acetoacetate, add them to the first material and stir evenly, further mix 0.2 g of azobisisobutyronitrile and 30 g of petroleum ether evenly, and further add them to the first material, heat to 40° C., and stir evenly to obtain the second material.

[0060] (3) Weigh 8 g of sorbitan monooleate polyoxyethylene ether, mix and heat to 50°C, add the second material while stirring, and continue stirring for 20 min to obtain the third material.

[0061] (4) Weigh 20 g of diethylenetriamine, 150 g of aluminum hydroxide, and 10 g of sodium carboxymethyl cellulose, dissolve them in 400 ml (60°C) deionized water, and add them to the third material. After homogenization for 30 minutes, react at a constant temperature of 70°C for 3 hours to obtain the fourth material.

[0062] (5) The fourth material was cooled to 45° C., 50 g of diammonium phosphate was added, and the mixture was supplemented with deionized water to 1000 g. After stirring for 10 min, a forest fire extinguishing agent was obtained.

[0063] Embodiment 5:

[0064] (1) Weigh 100g of polyguanidine, 150g of ammonium polyphosphate powder, and 100g of isopropylated triphenyl phosphate, and premix them in a stirring sand mill for 1 hour. Take 15g of silane coupling agent KH550, dissolve it in 80ml of anhydrous ethanol, and drip it into the flame retardant under stirring. After dripping for 30 minutes, start the stirring sand mill heater, keep the temperature at 60℃, continue stirring for 40 minutes, and after evaporating and removing the solvent, obtain the modified first material.

[0065] (2) Weigh 40 g of isophorone diisocyanate, add the first material, stir evenly, then add 10 ml of mineral oil, heat to 40° C., and further stir evenly to obtain the second material.

[0066] (3) Weigh 3 g of sorbitan monopalmitate, mix and heat to 50°C, stir for 10 min, add the second material, and stir evenly to obtain the third material.

[0067] (4) Weigh 20 g of diethylenetriamine and 50 g of aluminum hydroxide, disperse them in 400 ml (60°C) deionized water, add them to the third material, homogenize for 20 min, and react at a constant temperature of 65°C for 2.5 h to obtain the fourth material.

[0068] (6) The sixth material was cooled to 45° C., 50 g of silica sol was added, and the mixture was supplemented with deionized water to 1000 g. After stirring for 10 min, a forest fire extinguishing agent was obtained.

[0069] Comparative Example 1: (Based on Example 1, polyphosphate amine was removed to prove the synergy between phosphate ester and guanidine)

[0070] The step (1) of Example 1 is modified as follows: 300 g of guanidine borate powder and 15 g of silane coupling agent kH570 are weighed, dissolved in 80 ml of dichloromethane, and dripped into the flame retardant under stirring for 30 minutes. The sand mill heater is started, the temperature is kept at 45°C, and stirring is continued for 30 minutes. The solvent is evaporated and removed to obtain the modified first material. The remaining steps remain unchanged.

[0071] Comparative Example 2: (Based on Example 1, guanidine was removed to demonstrate the synergy between phosphate and guanidine)

[0072] The step (1) of Example 1 is modified as follows: 300 g of ammonium polyphosphate and 15 g of silane coupling agent kH570 are weighed, dissolved in 80 ml of dichloromethane, and dripped into the flame retardant under stirring for 30 minutes. The sand mill heater is started, the temperature is kept at 45°C, and stirring is continued for 30 minutes to evaporate and remove the solvent to obtain the modified first material. The remaining steps remain unchanged.

[0073] Comparative Example 3: (Based on Example 1, aluminum hydroxide was added to the capsule core flame retardant composition to prove that adding aluminum hydroxide to the capsule core has no synergistic effect)

[0074] (1) Weigh 150g of guanidine borate powder, 150g of ammonium polyphosphate, and 100g of aluminum hydroxide, and premix them in a sand mill for 1 hour. Weigh 15g of silane coupling agent kH570, dissolve it in 80ml of dichloromethane, and drip it into the flame retardant under stirring for 30 minutes. Start the sand mill heater, keep the temperature at 45℃, continue stirring for 30 minutes, evaporate and remove the solvent, and obtain the modified first material.

[0075] (2) Weigh 8 g of methyl methacrylate and 8 g of 1,4-butanediol dimethacrylate, stir them evenly and add them to the first material. Further, dissolve 0.2 g of azobisisobutyronitrile in 20 g of mineral oil and add it to the first material. Heat to 40°C and continue stirring for 20 min to obtain the second material.

[0076] (3) Weigh 8 g of sorbitan monooleate polyoxyethylene ether, add it to the second material under stirring, mix well, heat to 50°C, and stir for 20 minutes to obtain the third material.

[0077] (4) Weigh 4 g of N-hydroxyethyl acrylamide, dissolve it in 400 ml (60°C) deionized water, and add it to the third material. After homogenization for 10 minutes, react at a constant temperature of 60°C for 4 hours to obtain the fourth material.

[0078] (5) The fourth material was cooled to 45° C., 50 g of silica sol was added, and the mixture was supplemented with deionized water to 1000 g. After stirring for 10 min, a forest fire extinguishing agent was obtained.

[0079] Comparative Example 4: (Based on Example 1, aluminum hydroxide was added to the capsule shell to prove that adding aluminum hydroxide to the capsule shell has a synergistic effect)

[0080] (1) Weigh 150g of guanidine borate powder and 150g of ammonium polyphosphate, and premix them in a sand mill for 1h. Weigh 15g of silane coupling agent kH570, dissolve it in 80ml of dichloromethane, and drip it into the flame retardant under stirring for 30 minutes. Start the sand mill heater, keep the temperature at 45℃, continue stirring for 30 minutes, evaporate and remove the solvent, and obtain the modified first material.

[0081] (2) Weigh 8 g of methyl methacrylate and 8 g of 1,4-butanediol dimethacrylate, stir them evenly and add them to the first material. Further, dissolve 0.2 g of azobisisobutyronitrile in 20 g of mineral oil and add it to the first material. Heat to 40°C and continue stirring for 20 min to obtain the second material.

[0082] (3) Weigh 8 g of sorbitan monooleate polyoxyethylene ether, add it to the second material under stirring, mix well, heat to 50°C, and stir for 20 minutes to obtain the third material.

[0083] (4) Weigh 4 g of N-hydroxyethyl acrylamide, 100 g of aluminum hydroxide, and 5 g of carboxymethyl cellulose, dissolve them in 400 ml (60°C) deionized water, and add them to the third material. After homogenization for 10 min, react at a constant temperature of 60°C for 4 h to obtain the fourth material.

[0084] (5) The fourth material was cooled to 45° C., 50 g of silica sol was added, and the mixture was supplemented with deionized water to 1000 g. After stirring for 10 min, a forest fire extinguishing agent was obtained.

[0085] Comparative Example 5: (Based on Example 2, based on step (2), the component added with mineral oil was removed, which proved that the flame retardant had a poor dispersion effect and precipitation occurred during the later storage process)

[0086] (1) Weigh 150g of guanidine carbonate and 100g of ammonium polyphosphate, and premix them in a sand mill for 1 hour. Weigh 25g of silane coupling agent kH550, dissolve it in 100ml of dichloromethane, and drip it into the flame retardant under stirring for 30 minutes. Start the sand mill heater, keep the temperature at 45℃, continue stirring for 30 minutes, evaporate and remove the solvent, and obtain the modified first material.

[0087] (2) Weigh 80 g of glycidyl methacrylate and 1 g of dibenzoyl oxide, mix them evenly, add them to the first material and mix them evenly, heat to 50° C., and continue stirring for 20 min to obtain the second material.

[0088] (3) Weigh 10 g of sodium dodecyl sulfate, add it to the second material under stirring, mix well, heat to 50° C., and stir for 20 min to obtain the third material.

[0089] (4) Weigh 50 g of acrylonitrile, 100 g of aluminum hydroxide, and 5 g of sodium carboxymethyl cellulose, dissolve them in 400 ml (60°C) deionized water, and add them to the third material. After homogenization for 10 min, react at a constant temperature of 60°C for 4 h to obtain the fourth material.

[0090] (5) The fourth material was cooled to room temperature, 40 g of silicon dioxide nanopowder was added, and the mixture was supplemented with deionized water to 1000 g. After stirring for 10 min, a forest fire extinguishing agent was obtained.

[0091] Test 1 Flame retardant effect test of guanidine salt flame retardants

[0092] Test preparation: Cut the newsprint into the following size: a rectangle of 180mm long and 33.33mm wide, and cut it into an isosceles trapezoid of 30mm high along the diagonal line at the long side of 150mm. Figure 1 shown.

[0093] After the paper strips are prepared, they are placed in a constant temperature drying oven at 40°C and dried for 4 hours for later use.

[0094] Guanidine flame retardant was dissolved in deionized water to form a solution with a content of 5wt%. The test paper strip with the drug-soaked area was immersed in the solution for 10 seconds, taken out and hung indoors, dried for 48 hours, and then put into an oven at 40℃ for 4 hours to obtain a test paper strip with the trapezoidal area as a blank drug-free control area.

[0095] Light a candle, aim the trapezoidal non-combustible area at the candle flame, and light the test paper strip. Accurately measure the area of ​​the unburned area and calculate the flame retardant rate. The guanidine flame retardant rate is shown in Table 1 below:

[0096] Table 1 Flame retardant efficiency of guanidine flame retardants

[0097]

[0098] Test 2: Flame retardant effect test of forest fire extinguishing agent

[0099] After the forest fire extinguishing agents prepared in Examples 1-5 and Comparative Examples 1-5 were diluted with 20 times of water, 10 test paper strips with the same drug-immersion area as Test 1 were respectively immersed in the diluted forest fire extinguishing agent for 10 seconds, taken out and hung indoors, dried for 48 hours, and then put into an oven at 40°C for 4 hours to obtain test paper strips with the trapezoidal area as a blank drug-free control area.

[0100] Light a candle, aim the trapezoidal drug-free area at the candle flame, and light the test paper strip. Accurately measure the area of ​​the unburned area, and calculate the flame retardancy of the forest fire extinguishing agents prepared in Examples 1-5 and Comparative Examples 1-5. The test results are shown in Table 2.

[0101] Table 2 Different proportions of flame retardants and their flame retardant effects

[0102]

[0103] Further stability tests were conducted, and the forest fire extinguishing agents of Examples 1-5 and Comparative Examples 1-5 were stored in a warehouse at a day and night temperature of 15-30°C for 2 months. After storage, the different forest fire extinguishing agents were observed to see whether they were stratified and precipitated. Among them, the forest fire extinguishing agent of Comparative Example 5 had obvious large-scale deposits at the bottom of the storage container, and Example 5 had powdery deposits. The remaining examples and comparative examples had good stability and no obvious deposits occurred.

[0104] Test 3 Fire extinguishing effect test

[0105] Preparation

[0106] A: Wood strips, specifications: square cross section, side length 40mm, wood strip length 500mm. Number of wood strips: 72. Water content of wood strips <10%.

[0107] B: Wood strips stacking, the wood strips are placed on metal brackets, with a total height of 400mm, 8 strips per layer, and a total of 9 layers.

[0108] C: The igniter is 1500ml of No. 120 solvent oil, which is placed in a square metal tray with a side length smaller than the side length of the woodpile. Add 30mm deep water into the metal tray. Ignite the solvent oil, and remove the metal tray after it is completely burned.

[0109] D: After the wood pile is ignited, it burns freely. When the mass power is reduced to 53% of the original mass, the pre-combustion ends.

[0110] E: Use a 6.6L fire extinguisher filled with a forest fire extinguishing agent diluted 20 times with water. Open the spray valve 1.8 meters away from the woodpile to spray and extinguish the fire. Move closer to the woodpile while spraying, and spray the fire extinguishing agent from the top, bottom, and sides.

[0111] Five identical wood piles were set up, and the forest fire extinguishing agents of the above embodiments 1-5 were used to carry out fire extinguishing tests on each wood pile. The experimental results are as follows: after the forest fire extinguishing agent was sprayed, the flames of the five wood piles were extinguished, and there was no re-ignition within 10 minutes.

[0112] According to national standards, it achieves 2A fire extinguishing effect.

[0113] Toxicity test

[0114] The forest fire extinguishing agents of the above examples 1-5 were subjected to toxicity tests, and the specific method was as follows: zebrafish were normally fed with the forest fire extinguishing agents diluted 20 times with water for 96 hours, and none of them died. Conclusion: The toxicity was zero.

[0115] Freezing point test results: reached -19--20℃.

[0116] Corrosion rate test results: corrosion rate <0.9mdd.

[0117] The method of using the forest fire extinguishing agent of the present invention is:

[0118] Dilute 10-20 times with water and spray. First, use a seaplane to spray a 50-100m wide fire-retardant isolation belt 500m away from the downwind area of ​​the fire area. After the fire barrier is established, spray the fire extinguishing agent on the crown fire to extinguish the crown fire and finally extinguish the ground fire. In addition to using seaplanes, fire-fighting machinery can also use ground-based fire-fighting fire trucks, fire-fighting armored vehicles, and small spraying devices carried by humans.

[0119] The specific embodiments of the present invention are merely explanations of the present invention and are not limitations of the present invention. After reading this specification, those skilled in the art may make modifications to the embodiments without any creative contribution as needed. However, such modifications are protected by the patent law as long as they are within the scope of the claims of the present invention.

Claims

1. A method for preparing a forest fire extinguishing agent, characterized in that: The following steps are involved: (1) stirring and mixing a first flame retardant and a coupling agent to obtain a first material; the first flame retardant is a guanidine salt flame retardant and ammonium polyphosphate, the amount of the guanidine salt flame retardant is 5-30 parts by weight, the amount of the ammonium polyphosphate is 5-25 parts by weight, and the amount of the coupling agent is 0.1-5.0 parts by weight; (2) adding a hydrophobic polymer monomer and an initiator dissolved in an oily carrier to the first material, stirring evenly, to obtain a second material; the amount of the hydrophobic polymer monomer is 0.5-20 parts by weight, and the mass ratio of the initiator to the hydrophobic polymer monomer is 0.01%-5.00%; (3) adding a surfactant to the second material under stirring and heating to obtain a third material; the ratio of the surfactant to the hydrophobic polymer monomer is 0.2-50:100; (4) dissolving a hydrophilic polymer in water and adding the mixture to the third material, homogenizing the mixture, heating and stirring the mixture, and reacting the mixture at a constant temperature to obtain a fourth material; the amount of the hydrophilic polymer used is 0.1-10 parts by weight; (5) Cooling the fourth material, adding a flame retardant additive and water, and stirring evenly to obtain a forest fire extinguishing agent, wherein the flame retardant additive is selected from one or more of silicon dioxide nanopowder, ammonium polyphosphate, sodium silicate, silica sol, aluminum hydroxide, and ammonium dihydrogen phosphate, and the amount of the flame retardant additive is 1 to 10 parts by weight.

2. The method for preparing a forest fire extinguishing agent according to claim 1, characterized in that: In step (2), the oily carrier is selected from at least one of mineral oil, petroleum ether and paraffin.

3. The method for preparing a forest fire extinguishing agent according to claim 1, characterized in that: In step (4), a second flame retardant is further added, wherein the second flame retardant is a metal hydroxide flame retardant, and the amount used is 2-15 parts by weight.

4. The method for preparing a forest fire extinguishing agent according to claim 3, characterized in that: The hydroxide flame retardant is an aluminum hydroxide flame retardant.

5. The method for preparing a forest fire extinguishing agent according to claim 1, characterized in that: The coupling agent is selected from one or more of butyl orthotitanate, aluminate, silane coupling agent, phosphate coupling agent, and borate coupling agent.

6. The method for preparing a forest fire extinguishing agent according to claim 1, characterized in that: The hydrophobic polymer monomer is selected from one or more of methyl acrylate, ethyl acrylate, polybutyl acrylate, glycidyl acrylate, 1,4-butanediol dimethacrylate, methyl methacrylate, ethyl acetoacetate methacrylate, isophorone diisocyanate, and toluene diisocyanate; the surfactant is selected from one or more of propylene glycol monolaurate, sorbitan monostearate, polyoxyethylene sorbitan monooleate, sorbitan laurate, sodium lauryl sulfate, sodium dodecylbenzene sulfonate, diethylene glycol fatty acid ester, sorbitan monopalmitate, polyoxypropylene stearate, polyoxyethylene sorbitan trioleate, and sorbitan monooleate polyoxyethylene ether; the hydrophilic polymer is selected from one or more of polyvinyl alcohol, polyethylene glycol, acrylamide, N-hydroxymethyl acrylamide, N-hydroxyethyl acrylamide, acrylonitrile, and diethylenetriamine.

7. The method for preparing a forest fire extinguishing agent according to claim 1, characterized in that: In step (4), the homogenization time is 1-60 min; in step (4), the heating temperature of the isothermal reaction is 45° C.-90° C., and the isothermal reaction time is 0.5 h-8.0 h.

8. A forest fire extinguishing agent, characterized in that: The forest fire extinguishing agent is prepared by the preparation method according to any one of claims 1 to 7.

Citation Information

Cited By

  • Fire extinguishing agent special for forest grassland

    CN120459587A