Wafer processing method capable of adjusting wafer warpage by region
By depositing and etching stress films on the wafer substrate, regional stress adjustment is achieved, which solves the problems of complex, time-consuming and high-cost wafer warpage adjustment in the existing technology, and achieves a simple, fast and low-cost solution. Zone adjustment and surface smoothing.
Patent Information
- Application Number
- CN202410815508.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-24
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-06-24
AI Technical Summary
The existing technology involves complex process steps, long processing time, and high costs when adjusting wafer warpage, and cannot achieve partitioned adjustment, making it difficult to adapt to complex warpage conditions.
The warpage of the wafer substrate is measured with an ellipsometer, the first stress film is deposited, and the retention and etching areas are determined according to the warpage condition. The first stress film in the etched area is removed or thinned through the etching process, and then the first stress film is removed. A second stress film is deposited in the etching area, and the stress directions of the first and second stress films are opposite to achieve regional stress adjustment.
It realizes simple adjustment of wafer warpage, completes it in a short time, and low-cost partition adjustment, which can effectively improve complex warpage conditions and ensure wafer surface flatness.
Smart Images

Figure CN118380352B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a wafer processing method capable of adjusting wafer warpage by region. Background Art
[0002] When the wafer is processed on the front side, the stress on the wafer will change, causing the wafer to warp. If the wafer stress warpage is too large, it will make the subsequent process difficult to carry out, the yield will decrease, or affect the product performance. In order to improve the problem of wafer warpage, some existing methods are to coat the back of the wafer, and provide stress opposite to the wafer warpage through coating, so that the wafer stress is neutralized and the warpage meets the requirements. However, as the front processing technology becomes more and more advanced, the warpage of the wafer becomes more complicated, and the warpage in different directions is different, such as the horizontal and vertical warpage is often different. However, the existing technology generally deposits a thin film on the front and back of the wafer through a diffusion machine, and then removes the front film through wet etching or chemical mechanical grinding, leaving the back film, so as to adjust the stress. The method of adjusting the warpage is complicated, the steps are lengthy, the process time is long, and the cost increases; or the wafer is turned over first so that the back is turned to the front, and then a normal PECVD machine is used to deposit a thin film on it, and then the wafer is turned over after the film is coated, so as to adjust the wafer warpage. Therefore, the current method for improving wafer warpage has the problems of complex adjustment mode, long processing time, high process cost, and inability to adjust the wafer warpage in different zones. Summary of the invention
[0003] The purpose of the present application includes providing a wafer processing method and equipment that can adjust the wafer warpage partition. Through the wafer processing method of the present application, it is possible to achieve a significant effect of adjusting the warpage of the wafer partition, so that the method of adjusting the wafer warpage is simple, the processing time is short, and the process cost is low. At the same time, the wafer warpage in complex situations can be improved.
[0004] The embodiments of the present application can be implemented as follows:
[0005] In a first aspect, the present invention provides a wafer processing method capable of adjusting the wafer warpage by region, comprising:
[0006] The warpage of the wafer substrate is obtained by measuring the warpage of the wafer substrate using an ellipsometer, and then a first stress film is deposited on the wafer substrate;
[0007] According to the warpage of the wafer substrate, a reserved area and an etched area are determined on the first stress film, and the first stress film in the etched area is removed or thinned by an etching process;
[0008] A second stress film is deposited in the etched region on the wafer substrate, and the stress directions of the first stress film and the second stress film on the wafer substrate are opposite.
[0009] In an optional embodiment, the step of removing or thinning the first stress film in the etching area by an etching process includes:
[0010] An etching gas is introduced into the etching area, so that the first stress film in the etching area reacts with the etching gas to be removed or thinned.
[0011] In an optional embodiment, the step of introducing an etching gas into the etching area to allow the first stress film in the etching area to react with the etching gas to be removed or thinned includes:
[0012] Partially shielding the wafer substrate using a mask having a shielding area and a non-shielding area, so that the shielding area of the mask shields the reserved area of the first stress film, and the non-shielding area of the mask exposes the etched area of the first stress film;
[0013] The etching gas is supplied from the side of the mask facing away from the wafer substrate toward the wafer substrate.
[0014] In an optional embodiment, the wafer substrate has a central axis perpendicular to itself, and the shielding area and the non-shielding area of the mask are distributed around the central axis of the wafer substrate.
[0015] In an optional embodiment, the mask includes a frame, the frame includes a frame body and a step portion arranged on the inner side of the frame body, the thickness of the step portion is less than the thickness of the frame body, and the shielding area and the non-shielding area are arranged on the inner side of the step portion; when the mask is used to partially shield the wafer substrate, the edge of the wafer substrate overlaps the step portion of the frame.
[0016] In an optional embodiment, the first stress film and the second stress film exert stresses on the wafer substrate in opposite directions.
[0017] In an optional embodiment, the step of depositing a second stress film in the etched region on the wafer substrate includes:
[0018] Partially shielding the wafer substrate using a mask having a shielding area and a non-shielding area, so that the shielding area of the mask shields the first stress film, and the non-shielding area of the mask exposes the etched area on the wafer substrate;
[0019] A process gas is supplied from a side of the mask facing away from the wafer substrate toward the wafer substrate to deposit a second stress film in a region of the wafer substrate where the first stress film has been removed or thinned.
[0020] In an optional embodiment, the material of the wafer substrate is selected from one of crystalline silicon, silicon oxide, strained silicon, silicon germanium, doped or undoped polysilicon, doped or undoped silicon wafers, patterned or unpatterned wafers, silicon on insulator, carbon-doped silicon oxide, silicon nitride, doped silicon, germanium, gallium arsenide, glass and sapphire.
[0021] In an optional embodiment, the material of the first stress film and / or the second stress film is selected from silicon nitride or amorphous silicon.
[0022] In a second aspect, the present application provides a wafer processing device for adjusting the wafer warpage by region, the wafer processing device comprising:
[0023] A reaction chamber, wherein a support is disposed in the reaction chamber, a mask is detachably mounted on the support, the mask having a shielding area and a non-shielding area, the shielding area can block gas, and the non-shielding area allows gas to pass through, the mask having a first side and a second side opposite to each other, the first side of the mask being used to place a wafer substrate, one of the mask and the support being provided with a positioning groove, and the other being provided with a positioning portion, the positioning groove being plugged and matched with the positioning portion;
[0024] The first gas supply component includes a pipeline and a nozzle. One end of the pipeline is used to connect with the gas source, and the other end extends into the reaction chamber. The nozzle is connected to one end of the pipeline located in the reaction chamber, and the nozzle is spaced opposite to the second side of the mask.
[0025] In an optional embodiment, the mask includes a frame, the frame abuts against the support, the frame includes a frame body and a step portion arranged on the inner side of the frame body, the thickness of the step portion is less than the thickness of the frame body, and the shielding area and the non-shielding area are arranged on the inner side of the step portion; the step portion of the frame is used to support the edge of the wafer substrate.
[0026] The beneficial effects of the embodiments of the present application include, for example:
[0027] The wafer processing method provided by the present application includes: obtaining the warpage of the wafer substrate by measuring the ellipsometer, and then depositing a first stress film on the wafer substrate; determining the reserved area and the etching area on the first stress film according to the warpage condition of the wafer substrate, and removing or thinning the first stress film in the etching area by etching process; depositing the second stress film in the etched area on the wafer substrate, and the first stress film and the second stress film have opposite stress directions on the wafer substrate. The wafer processing method provided by the embodiment of the present application realizes stress adjustment in stages and regions through the process of "first coating-etching-second coating". The method for adjusting the wafer warpage is simple, the processing time is short, the process cost is low, and the wafer warpage in complex situations can be improved. In addition, the second stress film covers the area where the first stress film is etched, so that the entire surface of the wafer substrate is coated with a film, which can ensure the flatness of the wafer surface, and can adjust the warpage that the first stress film cannot adjust, which can better improve the complex warpage of the wafer. The wafer processing equipment provided in the embodiment of the present application can selectively perform etching and deposit the second stress film by providing a detachable mask, and can therefore be used to implement the above-mentioned wafer processing method. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.
[0029] Figure 1 This is a flow chart of a wafer processing method in one embodiment of the present application;
[0030] Figure 2 This is a schematic diagram of a wafer substrate, a mask and a nozzle in an etching process in one embodiment of the present application;
[0031] Figure 3 for Figure 2 A magnified view of the middle part III;
[0032] Figures 4a to 4j Schematic diagram of the distribution of the masked area and the non-masked area in different embodiments of the present application;
[0033] Figure 5 Schematic diagram of the relationship between etching time and the obtained warpage difference;
[0034] Figure 6 This is a cross-sectional view of a wafer processing device in one embodiment of the present application;
[0035] Figure 7 for Figure 6 Enlarged view of part VII in the middle.
[0036] Icons: 010-wafer processing equipment; 020-wafer substrate; 100-reaction chamber; 110-support; 111-exhaust hole; 112-positioning groove; 120-exhaust channel; 200-mask; 210-frame; 211-frame body; 212-step part; 213-positioning part; 300-first gas supply component; 310-pipeline; 320-nozzle; 400-second gas supply component. DETAILED DESCRIPTION
[0037] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, rather than all the embodiments. The components of the embodiments of the present application described and shown in the drawings here can be arranged and designed in various different configurations.
[0038] Therefore, the following detailed description of the embodiments of the present application provided in the accompanying drawings is not intended to limit the scope of the present application for which protection is sought, but merely represents selected embodiments of the present application. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.
[0039] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.
[0040] In the description of the present application, it should be noted that if the terms "upper", "lower", "inside", "outside", etc. appear to indicate an orientation or position relationship, it is based on the orientation or position relationship shown in the drawings, or is the orientation or position relationship in which the product of the invention is usually placed when used. It is only for the convenience of describing the present application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application.
[0041] In addition, the terms “first”, “second”, etc., if used, are merely used to distinguish between the descriptions and should not be understood as indicating or implying relative importance.
[0042] It should be noted that, in the absence of conflict, the features in the embodiments of the present application may be combined with each other.
[0043] At present, in order to improve the problem of wafer warpage, some existing practices are to coat the back of the wafer, and provide stress opposite to the wafer warpage through coating, so that the wafer stress is neutralized and the warpage meets the requirements. However, this process of coating the entire back of the wafer can only have a good effect when the wafer warpage is simple (for example, the wafer is warped in the positive direction or reverse direction as a whole). As the front processing technology becomes more and more advanced, the warpage of the wafer becomes more complicated, and the warpage in different directions is different, such as the horizontal and vertical warpage is often different. For example, in the manufacturing process of flash memory chips (NAND) or 3D-IC chips, many layers of film will be plated due to process requirements. The film itself has internal stress. As the number of film layers increases, the stress will be superimposed accordingly, resulting in a large warpage of the wafer substrate, and the next process (such as photolithography or etching process) cannot be carried out, and the warpage in a single direction may also be large. In this case, since the warpage of the traditional whole-surface coating in different directions or different regions is basically the same, it is impossible to achieve differentiated adjustment of the warpage in different directions and different regions of the wafer substrate.
[0044] In order to improve the deficiencies in the above-mentioned prior art, the embodiment of the present application provides a wafer processing method, which realizes the zoning adjustment of the wafer warpage by depositing different stress films in different areas, thereby meeting the wafer warpage adjustment under complex warpage conditions. In addition, the embodiment of the present application also provides a wafer, which is processed by the above-mentioned wafer processing method.
[0045] Figure 1 This is a flow chart of a wafer processing method in one embodiment of the present application. Figure 1 As shown, the wafer processing method provided in the embodiment of the present application includes the following steps.
[0046] In step S100 , the warpage of a wafer substrate is obtained by measuring the warpage of the wafer substrate using an ellipsometer, and then a first stress film is deposited on the wafer substrate.
[0047] In the embodiment of the present application, the warpage of the wafer substrate can be detected by an ellipsometer measuring device. The specific structure and principle of the ellipsometer measuring device can refer to the prior art and will not be described in detail here. Figure 2 , Figure 3 ) is deposited on the front or back side of the wafer substrate 020 to improve the warpage of the wafer substrate 020. In some cases, photolithography, etching and other processes will be performed on the front side of the wafer substrate 020 for the chip to be manufactured, so the first stress film can be deposited on the back side of the wafer substrate 020.
[0048] Optionally, the wafer substrate 020 may be made of the following materials: crystalline silicon (eg Si <100> or Si <111> ), silicon oxide, strained silicon, silicon germanium, doped or undoped polysilicon, doped or undoped silicon wafers and patterned or unpatterned wafers, silicon on insulator (SOI), carbon-doped silicon oxide, silicon nitride, doped silicon, germanium, gallium arsenide, glass or sapphire. The wafer substrate 020 can have various sizes, such as 200 mm or 300 mm diameter wafers, and rectangular or square panels.
[0049] Specifically, the wafer substrate 020 can be introduced into the processing chamber by a robot arm, and the deposition gas mixture is supplied to the reaction chamber 100. Several process parameters can be adjusted, such as gas flow, pressure, temperature, etc. After a period of reaction, a layer of high pressure stress film, i.e., the first stress film, is deposited on the surface of the wafer substrate 020. After the deposition reaction is completed, the wafer substrate 020 is transported out of the processing chamber by a robot arm, and the wafer substrate 020 is cooled to room temperature for the next step of processing.
[0050] The reaction gas for depositing the stress film can be silane, ammonia, nitrogen and argon. The gas flow rate of silane is 50-1000sccm, which can be selected as 200sccm; the gas flow rate of ammonia is 0-1000sccm, which can be selected as 600sccm; the gas flow rate of nitrogen is 0-20000sccm, which can be selected as 2000sccm; the gas flow rate of argon is 0-20000sccm, which can be selected as 1000sccm. The reaction pressure is 1.0~10torr, which can be selected as 1.5 torr. The reaction temperature can be selected between 300~550℃, which can be selected as 500℃. The high-frequency power supply power of the reaction is 100~2000W, which can be selected as 750W, and its frequency can be selected from 13.56MHz~21.12MHz, which can be selected as 21.12MHz. The low-frequency power supply power is 100~1000W, which can be selected as 150W, and the low-frequency frequency can be selected as 400KHz.
[0051] Optionally, the material of the first stress film is selected from silicon nitride or amorphous silicon, wherein the silicon nitride may be silicon-rich silicon nitride or nitrogen-rich silicon nitride.
[0052] Step S200 , determining a reserved area and an etched area on the first stress film according to the warpage of the wafer substrate, and removing or thinning the first stress film in the etched area by an etching process.
[0053] In the embodiment of the present application, the warping of the wafer substrate 020 may be complicated. For example, the warping of the wafer substrate 020 in the X direction is positive warping, that is, the two ends in the X direction are bent toward the front direction, and the middle part in the X direction is arched toward the back direction; and the warping of the wafer substrate 020 in the Y direction is reverse warping, that is, the two ends in the Y direction are bent toward the back direction, and the middle part in the Y direction is arched toward the front direction. In this way, the wafer substrate 020 forms a saddle shape. Therefore, it is impossible to effectively improve the warping problem by coating the entire surface to make it flat. In the embodiment of the present application, the warping condition of the wafer substrate 020 is required, and the reserved area and the etching area are determined on the first stress film, and the first stress film is retained in the reserved area, and the first stress film is used to adjust the stress of the area; and the warping type of the etching area is different, which cannot be improved by the first stress film, so the first stress film is not retained in this area.
[0054] Taking the above-mentioned saddle-shaped wafer substrate 020 as an example, if the first stress film is a film providing positive stress, that is, the first stress film can provide stress for improving positive warpage to the wafer substrate 020, then the coverage area of the first stress film should be distributed along the X direction of the wafer substrate 020, rather than distributed at the two ends in the Y direction; if the first stress film is a film providing negative stress, that is, the first stress film can provide stress for improving reverse warpage to the wafer substrate 020, then the coverage area of the first stress film should be distributed along the Y direction of the wafer substrate 020, rather than distributed at the two ends in the X direction.
[0055] In this embodiment, the step of removing or thinning the first stress film in the etching area by etching process includes: introducing etching gas into the etching area, allowing the first stress film in the etching area to react with the etching gas to be removed or thinned. In this embodiment, the process of etching by etching gas is a dry etching process.
[0056] In some cases, the warping directions of the wafer substrate 020 in the X direction and the Y direction are consistent, but the warping degrees may be different. Therefore, it is possible to consider performing incomplete etching in areas with weaker warping, that is, thinning the stress film in the etched area to weaken the adjustment ability of the stress film in these areas.
[0057] Specifically, the specific method of dry etching using etching gas includes:
[0058] Step S210, partially shielding the wafer substrate using a mask having a shielding area and a non-shielding area, so that the shielding area of the mask shields the reserved area of the first stress film, and the non-shielding area of the mask exposes the etched area of the first stress film;
[0059] In step S220, an etching gas is delivered from a side of the mask facing away from the wafer substrate toward the wafer substrate.
[0060] In this embodiment, the back side of the wafer substrate 020 is partially shielded by the mask 200, the shielding area is a solid structure, which can prevent the etching gas from reaching the reserved area of the first stress film, and the non-shielding area is a window, which can allow the etching gas to reach the etching area of the first stress film, and the first stress film in the area is etched, thereby removing or thinning the first stress film in the area. The material of the mask 200 can be selected from aluminum oxide or aluminum nitride.
[0061] The etching gas includes nitrogen trifluoride, which may be nitrogen trifluoride alone, or a combination of nitrogen trifluoride and argon. The flow rate of nitrogen trifluoride is 1000-10000 sccm, such as 3000 sccm; the flow rate of argon is 2000-20000 sccm, such as 7000 sccm. The reaction pressure is 1-10 torr.
[0062] Specifically, the wafer substrate 020 coated with the first stress film is transferred to the etching chamber by a robot arm for etching reaction. The shape of the mask 200 can be selected according to the specific division method of the reserved area and the etching area of the first stress film. The mask 200 blocks the back side of the wafer substrate 020, and the mask 200 contacts the base. Figure 2 This is a schematic diagram of a wafer substrate 020, a mask 200, and a showerhead 320 in an etching process in one embodiment of the present application; Figure 3 for Figure 2 The enlarged view of part III in the figure. Figure 2 and Figure 3 As shown, in this embodiment, the mask 200 can be supported on the back of the wafer substrate 020, and the nozzle 320 is used to deliver the etching gas to the back of the wafer substrate 020. Optionally, the mask 200 includes a frame 210, and the frame 210 includes a frame body 211 and a step portion 212 arranged inside the frame body 211, the thickness of the step portion 212 is less than the thickness of the frame body 211, and the shielding area and the non-shielding area are arranged inside the step portion 212; when the mask 200 is used to partially shield the wafer substrate 020, the edge of the wafer substrate 020 overlaps the step portion 212 of the frame 210. In this way, the wafer can be well positioned by the mask 200 to ensure that the etching area of the first stress film can be accurately etched. Optionally, the dimensions of the step portion 212 of the mask 200 are: an outer diameter of 300.5-301.5 mm, an inner diameter of 295-299 mm; or, an outer diameter of 200.5-201.5 mm, an inner diameter of 195-199 mm.
[0063] In the embodiment of the present application, the distribution of the shielding area and the non-shielding area of the mask 200 may be diverse. For example, the wafer substrate 020 has a central axis perpendicular to itself, and the shielding area and the non-shielding area of the mask 200 are distributed around the central axis of the wafer substrate 020. Figures 4a to 4j Schematic diagram of the distribution of the shielding area and the non-shielding area of the mask 200 in different embodiments of the present application. The figure takes a circular mask 200 as an example (applicable to a circular wafer substrate 020), the shaded part is the shielding area, and the non-shaded area is the non-shielding area. Taking the improvement of saddle-shaped warpage as an example, you can choose Figure 4a The shape of the mask 200 shown in the figure is that the shielding area is distributed in the X direction (horizontal direction in the figure), and the non-shielding area is distributed in the Y direction (vertical direction in the figure). In this way, the first stress film obtained after the etching process is distributed in the X direction of the wafer substrate 020. It should be understood that when facing other different warping conditions, different masks 200 can be selected to shield the wafer substrate 020, so as to etch and obtain first stress films with different distributions. Therefore, the shielding area and non-shielding area on the mask 200 can be diverse, such as the shielding area in Figure 4b In the middle, it is semicircular. Figure 4c to Figure 4g The distribution is rotationally symmetrical. Figure 4h to Figure 4j It should be understood that when the reserved area and the etching area of the first stress film are complexly distributed, there may be a situation where one mask 200 cannot meet the shielding requirements. In this case, two or more masks 200 can be overlapped and combined to obtain a new pattern to better meet the etching requirements.
[0064] After the wafer substrate 020 is placed in the etching chamber, an etching gas is introduced to etch or thin the first stress film corresponding to the non-shielded area, and the first stress film corresponding to the shielded area is retained. Different etching times can be selected according to the actual warpage difference target, and the film in the non-shielded area can be partially or completely etched.
[0065] Figure 5 Figure 2 is a schematic diagram showing the relationship between etching time and the obtained warpage difference. Figure 5 As shown, the difference in the warpage increases gradually with the increase in etching time. When all the stress films in the etching area are etched away, the difference in the warpage stops increasing and tends to be stable.
[0066] Step S300 , depositing a second stress film in the etched region on the wafer substrate, wherein the stress directions of the first stress film and the second stress film on the wafer substrate are opposite.
[0067] In the embodiment of the present application, the etched area on the wafer substrate 020 is not covered with the first stress film or the first stress film is thinned. In the case where the area is not covered with the first stress film, the stress is adjusted by depositing the second stress film in the area where the first stress film has been removed or thinned. In the case where the first stress film in the etching area is thinned, although the first stress film in the etching area also has a warpage adjustment function, it may still have room for further adjustment, so the second stress film may be deposited for further adjustment. Alternatively, after the etching process, the warpage adjustment of the wafer substrate 020 has been completed (at this time, the first stress film in the etching area is thinned or completely removed). In this case, in order to make the wafer surface have better flatness, the second stress film may not have the warpage adjustment ability, and only play a "filling" role.
[0068] Optionally, the material of the second stress film may be selected from silicon nitride or amorphous silicon, wherein the silicon nitride may be silicon-rich silicon nitride or nitrogen-rich silicon nitride.
[0069] In the embodiment of the present application, step S300 may specifically include:
[0070] Step S310, partially shielding the wafer substrate using a mask having a shielding area and a non-shielding area, so that the shielding area of the mask shields the first stress film, and the non-shielding area of the mask exposes the area on the wafer substrate where the first stress film has been removed;
[0071] In step S320 , a process gas is delivered from a side of the mask facing away from the wafer substrate toward the wafer substrate to deposit a second stress film in the region of the wafer substrate where the first stress film has been removed or thinned.
[0072] The mask 200 used in step S300 and the mask 200 used in step S200 may be the same mask or different masks. If the mask 200 in step S200 and step S300 is the same mask, the installation direction of the mask 200 or the placement direction of the wafer substrate 020 should be adjusted so that the shielding area of the mask 200 in step S200 and the non-shielding area of the mask 200 in step S300 correspond to the same area of the wafer substrate 020, and the non-shielding area of the mask 200 in step S200 and the shielding area of the mask 200 in step S300 correspond to the same area of the wafer substrate 020. Of course, step S300 and step S200 may use the first mask and the second mask respectively, and the shielding area and the non-shielding area of the first mask and the second mask are opposite.
[0073] Optionally, the second stress film may cover all the etching regions, or may only cover a portion of the etching regions, which should be determined according to the warping condition of the wafer substrate 020 corresponding to the etching regions.
[0074] Optionally, the first stress film and the second stress film have opposite stress directions on the wafer substrate 020. In some cases, the reason why some areas on the wafer substrate 020 are not covered with the first stress film is that the stress direction or stress type provided by the first stress film does not match the warping mode of the wafer substrate 020 in the area, that is, the warping of the area cannot be improved, so it is necessary to cover the stress film with the opposite stress direction. For example, the saddle-shaped wafer substrate 020 is positively warped along the X direction and reversely warped along the Y direction. Then it is necessary to distribute the positive stress film along the X direction on the back of the wafer substrate 020, and cover the negative stress film in the Y direction.
[0075] In other optional embodiments, the stress directions of the first stress film and the second stress film on the wafer substrate 020 may be the same, while the first stress film and the second stress film have different regulating forces on the warpage.
[0076] In another embodiment, one of the first stress film and the second stress film may not have the warping adjustment function, and its function of covering the wafer substrate 020 is to make the surface of the wafer substrate 020 smoother, avoiding the formation of steps due to one area being covered with the film while the other area is not covered with the film.
[0077] Through the above-mentioned wafer processing method, the wafer substrate 020 can be finely zoned and adjusted through two stress films, so that the complex warped wafer substrate 020 can be improved, so that the wafer substrate 020 is flat during the next process to meet the subsequent exposure, etching and other process conditions with high requirements for warping. It should be understood that the improvement of the warping of the wafer substrate 020 includes adjusting it to be as flat as possible, and also includes adjusting it to the required warping shape to cope with subsequent processing. The following table shows the adjustment of the warping in the X and Y directions of the wafer in an embodiment of the present application and the prior art.
[0078]
[0079] As shown in the above table, the prior art adopts the back-side overall coating process for adjustment, so the difference in warpage in the two directions is only 5. The technology of this embodiment can adopt differential adjustment in the two directions, so that the difference in warpage in the two directions is 363, thereby achieving a large difference in the warpage of the wafer substrate 020 in different directions.
[0080] Figure 6 This is a cross-sectional view of a wafer processing device 010 in one embodiment of the present application; Figure 7 for Figure 6 The enlarged view of the local VII in the middle. Figure 6 and Figure 7As shown, the embodiment of the present application further provides a wafer processing device 010, which can be used to implement the above-mentioned wafer processing method. The wafer processing device 010 includes:
[0081] A reaction chamber 100 is provided in the reaction chamber 100, a support 110 is detachably mounted on the support 110, the mask 200 has a shielding area and a non-shielding area, the shielding area can block gas, and the non-shielding area allows gas to pass through, the mask 200 has a first side and a second side opposite to each other, and the first side of the mask 200 is used to place a wafer substrate 020;
[0082] The first gas supply component 300 includes a pipeline 310 and a nozzle 320. One end of the pipeline 310 is used to connect to the gas source, and the other end extends into the reaction chamber 100. The nozzle 320 is connected to one end of the pipeline 310 located in the reaction chamber 100, and the nozzle 320 is spaced opposite to the second side of the mask 200.
[0083] In this embodiment, the pipeline 310 of the first gas supply assembly 300 extends from the bottom of the reaction chamber 100 into the reaction chamber 100 and is connected to the nozzle 320. The support 110 is an annular support, so the middle of the support 110 can provide gas for upward and downward circulation, and the nozzle 320 is arranged in the support 110. The lower end of the support 110 is detachably connected to the reaction chamber 100, and the upper end is detachably connected to the mask 200.
[0084] Optionally, one of the frame 210 and the support 110 of the mask 200 is provided with a positioning portion 213, and the other is provided with a positioning groove 112, and the positioning portion 213 is plugged and matched with the positioning groove 112 to achieve the assembly of the mask 200 and the support 110. Specifically in this embodiment, the positioning portion 213 can be provided on the lower side of the frame 210 of the mask 200, and the positioning groove 112 is provided on the upper end of the support 110. After the mask 200 is placed on the support 110, the positioning portion 213 is plugged and matched with the positioning groove 112, so as to position the mask 200. Of course, the support 110 and the mask 200 can also be connected by screws. In this embodiment, the first gas supply component 300 can provide etching gas or process gas to the back side of the wafer substrate 020 on the mask 200 to achieve local etching and local deposition of thin film.
[0085] In this embodiment, a plurality of exhaust holes 111 are provided on the support 110, and the exhaust holes 111 extend transversely to connect the inner side and the outer side of the support 110, and the plurality of exhaust holes 111 are arranged at intervals around the circumference of the support 110. An exhaust channel 120 is provided on the side wall of the reaction chamber 100 to communicate with the outside. Excess reaction gas can be transported to the outside of the reaction chamber 100 through the exhaust holes 111 and the exhaust channel 120, thereby ensuring the stability of the gas pressure.
[0086] In this embodiment, the wafer processing equipment 010 further includes a second gas supply assembly 400, which is disposed above the support 110 and the mask 200 and can provide gas to the front side of the wafer substrate 020 on the mask 200. The structure of the second gas supply assembly 400 can be similar to the first gas supply assembly 300. When the stress film on the back side of the wafer substrate 020 is etched in different regions, the second gas supply assembly 400 can be used to provide non-reactive gas to the front side of the wafer substrate 020, in order to prevent the front side of the wafer substrate 020 from contacting with the etching gas and causing defects on the front side of the wafer substrate 020.
[0087] When the wafer processing equipment 010 of the embodiment of the present application is used for wafer processing, the mask 200 to be used can be determined according to the warpage of the wafer substrate 020. After the mask 200 is installed in place, the wafer substrate 020 with the first stress film deposited on the entire surface is placed on the mask 200, and then the etching gas is introduced by the first gas supply component 300 for local etching to remove or thin the first stress film in some areas. After the etching process is completed, the mask 200 can be replaced (or the relative position of the wafer substrate 020 and the mask 200 can be adjusted), and then the second stress film is deposited in the etching area by the first gas supply component 300, so as to complete the adjustment of the wafer warpage and make the back of the wafer flat. It can be understood that the steps of depositing the second stress film and etching the first stress film can be performed in the same wafer processing equipment 010, or in two different wafer processing equipment 010.
[0088] In summary, the wafer processing method provided by the present application includes: obtaining the warpage of the wafer substrate 020 by measuring the device of the ellipsometer, and then depositing the first stress film on the wafer substrate 020; determining the reserved area and the etching area on the first stress film according to the warpage condition of the wafer substrate 020, removing or thinning the first stress film in the etching area by the etching process; depositing the second stress film in the etched area on the wafer substrate 020. The wafer processing method provided by the embodiment of the present application realizes the stress adjustment in stages and regions through the process of "first coating-etching-second coating", and the stress direction of the second stress film is opposite to that of the first stress film, which can adjust the warpage that the first stress film cannot adjust, thereby improving the wafer with complex warpage. The wafer processing equipment 010 provided by the embodiment of the present application can selectively etch and deposit the second stress film by setting a detachable mask 200, so it can be used to realize the above-mentioned wafer processing method.
[0089] The above are only specific implementations of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed in the present application should be included in the protection scope of the present application. Therefore, the protection scope of the present application shall be based on the protection scope of the claims.
Claims
1. A wafer processing method capable of adjusting wafer warpage by region, characterized in that: include: The warpage of the wafer substrate is obtained by measuring the warpage of the wafer substrate using an ellipsometer, and then a first stress film is deposited on the wafer substrate; Determining a reserved area and an etched area on the first stress film according to the warpage of the wafer substrate, and removing or thinning the first stress film in the etched area by an etching process; Depositing a second stress film in the etched area on the wafer substrate, wherein the first stress film and the second stress film exert stresses on the wafer substrate in opposite directions; The step of removing or thinning the first stress film in the etching area by an etching process comprises: Partially shielding the wafer substrate using a mask having a shielding area and a non-shielding area, so that the shielding area of the mask shields the reserved area of the first stress film, and the non-shielding area of the mask exposes the etched area of the first stress film; Delivering an etching gas from a side of the mask away from the wafer substrate toward the wafer substrate, so that the first stress film in the etching area reacts with the etching gas to be removed or thinned; The step of depositing a second stress film in the etched area on the wafer substrate comprises: Partially shielding the wafer substrate using a mask having a shielding area and a non-shielding area, so that the shielding area of the mask shields the first stress film, and the non-shielding area of the mask exposes the etched area on the wafer substrate; delivering a process gas from a side of the mask facing away from the wafer substrate toward the wafer substrate to deposit the second stress film in a region of the wafer substrate where the first stress film has been removed or thinned; The steps of depositing the second stress film and etching the first stress film are performed in the same wafer processing equipment and use the same mask.
2. The wafer processing method capable of adjusting wafer warpage by region according to claim 1, characterized in that: The wafer substrate has a central axis perpendicular to itself, and the shielding area and the non-shielding area of the mask are distributed around the central axis of the wafer substrate.
3. The wafer processing method capable of adjusting wafer warpage by region according to claim 1, characterized in that: The mask includes a frame, which includes a frame body and a step portion arranged on the inner side of the frame body, the thickness of the step portion is less than the thickness of the frame body, and the shielding area and the non-shielding area are arranged on the inner side of the step portion; when the mask is used to partially shield the wafer substrate, the edge of the wafer substrate overlaps the step portion of the frame.
4. The wafer processing method capable of adjusting wafer warpage by region according to any one of claims 1 to 3, characterized in that: The material of the wafer substrate is selected from one of crystalline silicon, silicon oxide, strained silicon, silicon germanium, doped or undoped polysilicon, doped or undoped silicon wafers, patterned or unpatterned wafers, silicon on insulator, carbon-doped silicon oxide, silicon nitride, doped silicon, germanium, gallium arsenide, glass and sapphire.
5. The wafer processing method capable of adjusting wafer warpage by region according to any one of claims 1 to 3, characterized in that: The material of the first stress film and / or the second stress film is selected from silicon nitride or amorphous silicon.