A production line for welding seam steel pipes
By using the outer cutting part and the inner scraper mechanism to cut the weld convex material in the seam steel pipe welding processing production line, and using the scratch cutting part to cut the fracture, the problem of solder twist and internal scraper replacement is solved, and the welding strength and efficiency.
Patent Information
- Application Number
- CN202410963807.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-18
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-07-18
AI Technical Summary
The existing seam steel pipe welding processing production line is prone to twist during the cutting process, and the inner scraper is inconvenient to replace, resulting in high defect rate and poor welding effect.
A production line for welding processing with seam steel pipes was designed, using the outer cutting part and the inner scraping mechanism to cut the weld convex material respectively, and the inner scraping mechanism was suspended to fix it, and the fracture was cut through the scratch cutting part, and the convex material of the weld convex material was The segment shape is convenient for falling off, and the installation mechanism does not require prying the steel pipe to replace the inner scraper, which improves the welding strength.
It reduces solder twisting and defective rate, improves welding strength and production efficiency, simplifies the replacement process of internal scrapers, and enhances the welding effect.
Smart Images

Figure CN118492982B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of steel pipe processing, and in particular to a production line for welding seamed steel pipes. Background Art
[0002] Welding is a necessary process for the production of seamless steel pipes. The processing technology generally involves gradually bending the steel plate into a tubular structure, and then using high-frequency welding to weld the seams at the overlapping positions at both ends. After welding, the inner and outer solders need to be cut, and then the cut surfaces need to be fine-machined to remove sharp edges and burrs.
[0003] The existing seam steel pipe welding production line processes the seam steel pipe continuously, and the internal scraper mechanism cuts the solder uninterruptedly. When the seam steel pipe is subsequently cut, the solder inside the seam steel pipe is also cut at the same time. During the cutting process, the solder may be spirally twisted. Since the steel pipe has a long hollow area, it is difficult to remove the cut solder from the seam steel pipe, and the internal scraper may also be damaged. The existing technology has the following technical defects:
[0004] The inner scraper needs to be replaced after being used for a period of time or when it is damaged. In the prior art, it is necessary to use a crowbar to pry open the joint of the seamed steel pipe, and then remove the inner scraper at the leaked position of the pried open part and replace it. Installation and maintenance and replacement are extremely inconvenient, and may also cause local deformation of the steel pipe, thereby producing defective products and failing to meet processing needs. In addition, in the prior art, the stainless steel strip is wound into a seamed steel pipe and then welded, and the weld interface is in vertical contact, and the welding effect needs to be improved.
[0005] Therefore, it is necessary to invent a kind of production line for welding and processing of seam steel pipe to solve the above problems. Summary of the invention
[0006] The object of the present invention is to provide a production line for welding seam steel pipes, which cuts the weld convex materials on the outer and inner sides of the seam steel pipe body after welding through an outer cutting part and an inner scraping mechanism respectively. The mounting mechanism fixes the inner scraping mechanism in a suspended manner, and adjusts the extension length of the three claws so that the inner scraping mechanism cuts the weld convex material. Before that, the running trajectory of the scratching knife of the scratching and cutting part is utilized to make it periodically contact with the weld convex material, and cut out fractures of the weld convex material. When the weld convex material is cut off, the segmented solder is easy to fall off and clean, so as to solve the above-mentioned deficiencies in the technology.
[0007] In order to achieve the above-mentioned purpose, the present invention provides the following technical solutions: a production line for welding a seam steel pipe, comprising a stainless steel pipe making machine, which is used to wind a stainless steel strip into a seam steel pipe body, and the seam steel pipe body passes between the shaping rollers of the stainless steel pipe making machine, the input end of the stainless steel pipe making machine is provided with a mounting frame, and both sides of the mounting frame are provided with a pressing roller part, the output end of the stainless steel pipe making machine is provided with a magnetic coil, and the connecting end of the magnetic coil is connected to the output end of a high-frequency welding machine, and the high-frequency welding machine cooperates with the magnetic coil to weld the seam steel pipe, and the axis of the seam steel pipe body is movably connected with an inner scraping mechanism, and the inner scraping mechanism is assembled with the top two side walls of the stainless steel pipe making machine through the mounting mechanism;
[0008] The production line also includes:
[0009] A trimming part is mounted on the mounting frame and is located between the two pressing roller parts. The trimming part is used to process burrs on the surface of the stainless steel strip. The trimming part cuts inclined sections on both sides of the stainless steel strip, and the inclined sections on both sides of the stainless steel strip are distributed in parallel.
[0010] The outer cutting part is installed at the output end of the stainless steel pipe making machine and is located directly above the seam steel pipe body. The outer cutting part is used to cut the weld convex material on the top of the seam steel pipe body.
[0011] A winding rack is installed on one side of the outer cutting portion and is used to wind and store the weld convex material cutting strip;
[0012] The polishing part is correspondingly installed on the top of the seamed steel pipe body, and the polishing part is used to polish and grind the weld position of the seamed steel pipe body after the weld convex material is cut;
[0013] The inner scraping mechanism comprises a mandrel body, and a groove-shaped rack is provided on the outer top of the mandrel body, a three-jaw chuck is installed on the outer end of the mandrel body, and a sleeve hole matching the mandrel body is provided at the axis of the three-jaw chuck, a collar is provided on one side of the three-jaw chuck and located outside the sleeve hole, and the collar and the three-jaw chuck are fixedly installed by a first bolt, an inner scraper is installed on the supporting jaws located at the top of the three-jaw chuck, and the inner scraper is used to cut the weld convex material inside the seamed steel pipe body, a scratching and cutting part is provided on the outer side of the three-jaw chuck and on the side close to the installation mechanism, and the scratching and cutting part is used to cut a fracture of the weld convex material at the front side of the inner scraper, and support wheels are installed on the two supporting jaws located at the bottom of the three-jaw chuck, and the ends of the inner scraper and the support wheel are both in contact with the inner wall of the seamed steel pipe body;
[0014] The mounting mechanism includes at least two mounting rings, and the core shaft body is slidably connected to the inside of the mounting ring. A notch is opened on the inner top of the mounting ring, and a plate-shaped gear meshing with the grooved rack is rotatably connected to the inner side of the notch. A servo motor is fixedly connected to the outer side of the mounting ring, and the output shaft of the servo motor passes through the mounting ring and is transmission-connected to the plate-shaped gear. Suspensions are fixedly connected to the tops of both sides of the mounting ring, and first electric push rods are fixedly connected to both side walls of the top of the stainless steel pipe making machine, and the output end of the first electric push rod is transmission-connected to the end of the suspension.
[0015] As a preferred embodiment of the present invention, the scratching and cutting portion includes a limit plate, and a short shaft is fixedly connected to one side of the limit plate, a stepper motor is fixedly installed on the end of the support claw located at the top, and an eccentrically arranged jump disk is transmission-connected to the output end of the stepper motor, an annular member is fixedly connected to the outer side of the jump disk, a plug-in plate is provided at the top of the annular member, and a scratching knife is plugged into the outer side of the plug-in plate, and the scratching knife and the plug-in plate are fixedly connected by a second bolt, a bar slide rail is fixedly connected to the bottom end of the annular member, and the short shaft is slidably connected to the bar slide rail.
[0016] As a preferred solution of the present invention, one end of the mandrel body close to the three-jaw chuck is fixedly connected to a pipe head, the other end of the mandrel body is installed with a pressure-bearing pipe, and the outside of the pipe head is connected to at least three high-pressure nozzles, and the high-pressure nozzles are arranged in an inclined annular array;
[0017] A cavity is formed at the axis center of the core shaft body, and the pipe head and the pressure-bearing pipe are both connected to the cavity;
[0018] The core shaft body is composed of multiple core shaft tube segments, and a threaded segment is integrally provided at one end of the core shaft tube segment, and an internal thread groove matching the threaded segment is opened on the inner side of the other end of the core shaft tube segment, an annular groove is opened inside the core shaft body and on one side of the internal thread groove, and a sealing gasket is arranged in the annular groove.
[0019] As a preferred solution of the present invention, the input end of the pressure-bearing pipe is provided with a high-pressure water pump or a high-pressure air pump for cleaning the cutting residue inside the cavity and cooling the seamed steel pipe body.
[0020] As a preferred solution of the present invention, the mounting mechanism is mounted at the opening of the seamed steel pipe body;
[0021] A space area for the core shaft to move is provided inside the stainless steel pipe making machine and located at the installation mechanism;
[0022] The three-jaw chuck is provided with a small bevel gear for adjusting the extension length of the multiple claws;
[0023] The end of the support claw is fixedly mounted with an H-shaped plate by a third bolt, and the inner scraper and the support wheel are both detachably mounted on the H-shaped plate;
[0024] The output shafts of the multiple servo motors rotate synchronously.
[0025] As a preferred embodiment of the present invention, the outer cutting portion includes a transverse plate, a slot is provided on the transverse plate, and a tool rod is inserted into the slot, an outer scraper is detachably installed on the bottom end of the tool rod, and the transverse plate and the tool rod are fixedly connected by a fourth bolt.
[0026] As a preferred solution of the present invention, a first extension frame is fixedly connected to one side of the output end of the stainless steel pipe making machine, a second extension frame is fixedly connected to the other side of the output end of the stainless steel pipe making machine, and a support frame is fixedly connected to the top of the first extension frame;
[0027] The transverse plate and the winding frame are both arranged on the supporting frame, the first extension frame is located on the side of the winding frame away from the outer cutting part, a hydraulic cylinder is fixedly installed on one side of the top of the first extension frame, and a hydraulic mechanism for providing kinetic energy is arranged at the connecting end of the hydraulic cylinder, and the output end of the hydraulic cylinder is fixedly connected to the bottom of the polishing part;
[0028] A sliding rod is fixedly connected to the top of the second extension frame. The sliding rod passes through the polishing portion and is slidably connected to the through hole.
[0029] As a preferred embodiment of the present invention, the production line further comprises a cooling spray system, which sprays cooling liquid at the inner part, outer cutting part, winding frame and polishing part of the stainless steel pipe making machine to cool the winding and welding process of the seamed steel pipe;
[0030] The polishing part is configured as a belt-type pipe polishing machine.
[0031] As a preferred solution of the present invention, both ends of the outer side of the pressing roller are movably connected to limit rings for adapting to stainless steel strips of different widths and performing limit adjustment;
[0032] The trimming part includes two parallel distributed racks, and the racks are fixed on the mounting frame, the racks are fixedly connected with a second electric push rod, the output end of the second electric push rod passes through the racks and is fixedly connected with a trimming plate, and a flat scraping blade is arranged at the corner of the trimming plate;
[0033] A notch is provided on the upper surface of the trimming plate at the bottom, and the depth of the notch is equal to the thickness of the stainless steel belt. Limiting grooves are provided on both sides of the notch, and the first cutting module and the second cutting module are slidably connected inside the two limiting grooves respectively. Threaded rods are threadedly penetrated on both sides of the trimming plate, and the threaded rods penetrate the limiting grooves and are rotatably connected to one of the first cutting module and the second cutting module;
[0034] The first cutter module and the second cutter module are both provided with blades on one side opposite to each other, and the blades on both sides are arranged obliquely and distributed in parallel.
[0035] A method for welding a seamed steel pipe is provided, wherein the above-mentioned production line is used for processing, and the specific steps are as follows:
[0036] Step 1: Take the stainless steel strip from the steel strip coil and feed it into the input end of the stainless steel pipe making machine at a uniform speed. Use the trimming part to deal with the burrs on the surface of the stainless steel strip, and cut inclined and parallel sections on both sides of the stainless steel strip to expand the contact surface.
[0037] Step 2: According to the processing inner and outer diameter size requirements of the seamed steel pipe body, the device is adjusted to achieve the processing of seamed steel pipe bodies of different specifications;
[0038] Step 3: Use multiple pressing wheels and shaping rollers of the stainless steel pipe making machine to gradually roll the stainless steel strip into a seamed steel pipe body, and continuously transport it for continuous processing, and accurately install the outer cutting part and the inner scraping mechanism;
[0039] Step 4: When the seamed steel pipe body is transported to the output end of the stainless steel pipe making machine, a high-frequency welding machine is used in conjunction with a magnetic coil to heat the seamed steel pipe in the final stage of welding, and pressure is applied to close and weld the seamed steel pipe body;
[0040] Step 5: Use the outer cutting part and the inner scraping mechanism to cut the outer and inner weld convex materials of the welded steel pipe body after welding, and on the inner scraping mechanism, the weld convex material is cut into a fracture at the front side of the inner scraper by the scratching and cutting part, so as to cut off the inner weld convex material;
[0041] Step 6: Use a winding rack to wind up and store the weld convex material cutting strip, and use a high-pressure water pump or a high-pressure air pump to clean the cutting residue inside the cavity;
[0042] Step 7: After cutting, the seam steel pipe body is further transported to the polishing department, and the polishing belt of the polishing department is used to polish and grind the weld position on the top of the seam steel pipe body.
[0043] In the above technical solution, the technical effects and advantages provided by the present invention are:
[0044] The outer cutting part and the inner scraping mechanism are used to cut the weld convex materials on the outer and inner sides of the welded steel pipe body after welding. The installation mechanism fixes the inner scraping mechanism in a suspended manner, and adjusts the extension length of the three claws so that the inner scraping mechanism cuts the weld convex materials. Before that, the scratching knife of the scratching and cutting part is used to run along the trajectory so that it periodically contacts the weld convex materials and cuts the weld convex materials into fractures. When the weld convex materials are cut off, the segmented solder is easy to fall off and clean, reducing the adverse effects of the spiral distortion of the solder. The installation mechanism is used to output the inner scraping mechanism, and the inner scraper is replaced on the outside, without prying the seam of the welded steel pipe, thereby reducing the defective rate.
[0045] The surface of the stainless steel strip is processed by the trimming part. The burrs are scraped off during the sliding contact between the stainless steel strip and the flat scraper blade. The blades on both sides cut the two sides of the stainless steel strip. The cutting surfaces are parallel bevels. After the bevels on both sides are butted, a high-frequency welding machine is used in conjunction with a magnetic coil to heat the final stage of the welding of the seamed steel pipe, and pressure is applied to close and weld the seamed steel pipe body. The contact area is increased compared to the straight contact, and the seams at both ends are staggered in orientation. The connection strength is significantly enhanced after welding.
[0046] The first cutting knife module and the second cutting knife module are moved by rotating the threaded rods on both sides so that the gap between the first cutting knife module and the second cutting knife module is located in the center of the notch, the stainless steel strip raw material is preset, and the gap between the shaping roller and the pressing roller of the stainless steel pipe making machine is adjusted to meet the processing requirements of the seam steel pipe body with different diameters, and the height of the inner scraper mechanism is adjusted by the installation mechanism so that the core shaft body is located at the axial position of the seam steel pipe body, and the small bevel gear is rotated to transmit the drive mechanism on the inner side of the three-jaw chuck, so that the three claws on the three-jaw chuck are extended or retracted synchronously, and the inner scraper and the support wheel support the three-jaw chuck in a triangle shape to improve the stability of the core shaft body, and the outer cutting part and the polishing part are adjusted to meet the processing needs of the seam steel pipe body with different diameters. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For ordinary technicians in this field, other drawings can also be obtained based on these drawings.
[0048] Figure 1 It is a stereoscopic diagram of the overall structure of the present invention from a first viewing angle;
[0049] Figure 2 It is a stereoscopic diagram of the overall structure of the present invention from a second viewing angle;
[0050] Figure 3It is a third perspective stereogram of the overall structure of the present invention;
[0051] Figure 4 It is a stereoscopic diagram of the overall structure of the present invention from a fourth viewing angle;
[0052] Figure 5 It is the overall structural front view of the present invention;
[0053] Figure 6 It is a rear view of the overall structure of the present invention;
[0054] Figure 7 It is a top view of the overall structure of the present invention;
[0055] Figure 8 This is a diagram showing the effect of the stainless steel strip of the present invention being wound into a seamed steel pipe body;
[0056] Fig. 9 This is a diagram showing the effect of heating the butt weld of the seamed steel pipe body of the present invention;
[0057] Fig.10 A first-view stereoscopic diagram of the connection structure between the inner scraping mechanism and the mounting mechanism of the present invention;
[0058] Fig.11 A second perspective perspective view of the connection structure between the inner scraping mechanism and the mounting mechanism of the present invention;
[0059] Fig.12 It is a front view of the connection structure between the inner scraping mechanism and the mounting mechanism of the present invention;
[0060] Fig.13 It is a cutaway structural stereogram of the connection structure between the inner scraping mechanism and the mounting mechanism of the present invention;
[0061] Fig.14 It is a front cross-sectional view of the connection structure between the inner scraping mechanism and the mounting mechanism of the present invention;
[0062] Fig.15 It is an exploded view from a first perspective of the connection structure between the inner scraping mechanism and the mounting mechanism of the present invention;
[0063] Fig.16 It is an exploded view from a second perspective of the connection structure between the inner scraping mechanism and the mounting mechanism of the present invention;
[0064] Fig.17 It is a three-dimensional diagram of the three-jaw chuck of the present invention;
[0065] Fig.18 is a side view of the trimming portion of the present invention;
[0066] Fig.19 A first-view stereoscopic diagram of the local structure of the trimming portion of the present invention;
[0067] Fig. 20A second perspective stereoscopic view of the local structure of the trimming portion of the present invention;
[0068] Fig.21 It is a three-dimensional diagram of the matching structure of the first cutting module and the second cutting module of the present invention.
[0069] Description of reference numerals:
[0070] Stainless steel pipe making machine-1; mounting frame-2; pressing roller part-3; magnetic coil-4; inner scraping mechanism-5; mounting mechanism-6; trimming part-7; seamed steel pipe body-8; outer cutting part-9; winding frame-10; polishing part-11; scoring and cutting part-12; first extension frame-13; second extension frame-14; supporting frame-15; hydraulic cylinder-16; sliding rod-17;
[0071] Mandrel body-51; grooved rack-52; three-jaw chuck-53; socket hole-54; collar-55; inner scraper-56; support wheel-57; pipe head-58; pressure-bearing pipe-59; high-pressure nozzle-510; mandrel pipe section-511; threaded section-512; annular groove-513; sealing gasket-514; small bevel gear-515; H-shaped plate-516;
[0072] Mounting ring-61; plate gear-62; servo motor-63; suspension-64; first electric push rod-65;
[0073] Rack plate-71; second electric push rod-72; trimming plate-73; notch-74; limit groove-75; first cutter module-76; second cutter module-77; threaded rod-78; blade-79;
[0074] Horizontal plate-91; tool bar-92; external scraper-93;
[0075] Limiting plate-121; short shaft-122; stepping motor-123; jump plate-124; ring-125; plug-in board-126; scratching knife-127; strip slide rail-128. DETAILED DESCRIPTION
[0076] In order to enable those skilled in the art to better understand the technical solution of the present invention, the present invention will be further described in detail below with reference to the accompanying drawings.
[0077] The present invention provides Figure 1-21The production line for welding a seamed steel pipe shown in the figure comprises a stainless steel pipe making machine 1 for winding a stainless steel strip into a seamed steel pipe body 8. The stainless steel pipe making machine 1 can be a stainless steel pipe making machine of Foshan Yuanxinghong Welding Pipe Machinery and Mould Co., Ltd., and the seamed steel pipe body 8 passes between the shaping rollers of the stainless steel pipe making machine 1. The gap between the shaping rollers and the pressing rollers of the stainless steel pipe making machine 1 can be adjusted, so that the seamed steel pipe bodies 8 with different outer diameters can be processed. The input end of the stainless steel pipe making machine 1 is provided with a mounting frame 2, and both sides of the mounting frame 2 are provided with pressing rollers 3, and the stainless steel pipe body 8 is pressed by the pressing rollers 3. The belt is shaped to make it into a flat surface structure. The output end of the stainless steel pipe making machine 1 is provided with a magnetic coil 4, and the connecting end of the magnetic coil 4 is connected to the output end of the high-frequency welding machine. The high-frequency welding machine cooperates with the magnetic coil 4 to weld the seamed steel pipe. In this embodiment, the high-frequency welding machine adopts a JJG-60 high-frequency induction heating machine. The axis of the seamed steel pipe body 8 is movably connected with an inner scraping mechanism 5, and the inner scraping mechanism 5 is assembled with the two side walls of the top of the stainless steel pipe making machine 1 through an installation mechanism 6. The installation mechanism 6 is used to install the inner scraping mechanism 5 and also used to adjust the height of the inner scraping mechanism 5;
[0078] The production line also includes:
[0079] The trimming part 7 is mounted on the mounting frame 2 and is located between the two roller parts 3. The trimming part 7 is used to process the burrs on the surface of the stainless steel strip, and the trimming part 7 cuts inclined sections on both sides of the stainless steel strip, and the inclined sections on both sides of the stainless steel strip are distributed in parallel;
[0080] As an embodiment of the trimming portion 7 in the present invention:
[0081] The trimming part 7 includes two parallelly distributed racks 71, and the racks 71 are fixed on the mounting frame 2. A second electric push rod 72 is fixedly connected to the rack 71. The output end of the second electric push rod 72 passes through the rack 71 and is fixedly connected to a trimming plate 73. Flat scraping blades are arranged at the corners of the trimming plate 73. The flat scraping blades are installed on the opposite side surfaces of the two trimming plates 73 through slots, and are easy to install and replace. The burrs on the surface of the stainless steel belt are scraped off during the sliding contact between the flat scraping blades.
[0082] A notch 74 is provided on the upper surface of the trimming plate 73 at the bottom, and the depth of the notch 74 is equal to the thickness of the stainless steel belt. Limiting grooves 75 are provided on both sides of the notch 74, and the first cutting module 76 and the second cutting module 77 are slidably connected inside the two limiting grooves 75, respectively. Threaded rods 78 are threadedly penetrated on both sides of the trimming plate 73, and the threaded rods 78 penetrate the limiting grooves 75 and are rotatably connected to one of the first cutting module 76 and the second cutting module 77. The threaded rods 78 on both sides are rotated to move the first cutting module 76 and the second cutting module 77, so that the gap between the first cutting module 76 and the second cutting module 77 is located at the center of the notch 74, which can be adjusted according to the pipe diameter processing requirements of the seamed steel pipe body 8;
[0083] The first cutting module 76 and the second cutting module 77 are both provided with blades 79 on the opposite side. The blades 79 on both sides are inclined and distributed in parallel. The blades 79 on both sides can cut both sides of the stainless steel strip, and the cutting surfaces are parallel inclined surfaces. After the inclined surfaces on both sides are butted, the contact area is increased compared with the straight surface contact, and the seams at both ends are staggered in orientation, and the connection strength is significantly enhanced after welding;
[0084] The outer cutting part 9 is installed at the output end of the stainless steel pipe making machine 1 and is located directly above the seamed steel pipe body 8. The outer cutting part 9 is used to cut the weld convex material on the top of the seamed steel pipe body 8.
[0085] As an embodiment of the outer cutting portion 9 in the present invention:
[0086] The outer cutting part 9 includes a transverse plate 91, a bayonet is provided on the transverse plate 91, and a tool rod 92 is inserted in the bayonet. An outer scraper 93 is detachably installed at the bottom end of the tool rod 92. The outer scraper 93 is easy to install and replace, and the outer scraper 93 is located just above the axis of the seamed steel pipe body 8. The transverse plate 91 and the tool rod 92 are fixedly connected by a fourth bolt. According to the processing requirements of the seamed steel pipe body 8 with different outer diameters, the position of the tool rod 92 is adjusted in the bayonet, thereby adjusting the height of the outer scraper 93 to adapt to the processing of the seamed steel pipe body 8, and the fourth bolt is used to fix it after adjustment;
[0087] The winding frame 10 is installed on one side of the outer cutting portion 9 and is used to wind and store the weld convex material cutting strip;
[0088] As an embodiment of the winding frame 10 in the present invention:
[0089] The winding frame 10 includes a winding steel ring, and a shaft is fixedly connected to the axis of the winding steel ring. A first driving motor is fixedly connected inside the support frame 15, and the output shaft of the first driving motor is connected to the shaft. A quick clamping mechanism is provided on the winding steel ring, and the quick clamping mechanism is used to clamp the end of the weld convex material cutting strip. Then, the output shaft of the first driving motor drives the winding steel ring to wind up the weld convex material cutting strip. After winding to a certain length, the weld convex material cutting strip is cut off, and then the storage roll can be removed.
[0090] The polishing part 11 is correspondingly installed on the top of the seamed steel pipe body 8, and the polishing part 11 is used to polish and grind the weld position of the seamed steel pipe body 8 after the weld convex material is cut;
[0091] As an embodiment of the internal scraping mechanism 5 in the present invention:
[0092] The inner scraping mechanism 5 includes a mandrel body 51, and a grooved rack 52 is provided on the outer top of the mandrel body 51, a three-jaw chuck 53 is installed on the outer end of the mandrel body 51, and a sleeve hole 54 matching the mandrel body 51 is provided at the axis of the three-jaw chuck 53, and a collar 55 is provided on one side of the three-jaw chuck 53 and outside the sleeve hole 54 for interference connection, and the collar 55 and the three-jaw chuck 53 are fixedly installed by a first bolt, and a support claw located at the top of the three-jaw chuck 53 is installed. An inner scraper is installed, and the inner scraper 56 is used to cut the weld convex material inside the seam steel pipe body 8. A scratching and cutting part 12 is provided on the outer side of the three-jaw chuck 53 and close to the mounting mechanism 6. The scratching and cutting part 12 is used to cut the weld convex material in front of the inner scraper 56. Support wheels 57 are installed on the two supporting claws at the bottom of the three-jaw chuck 53, and the ends of the inner scraper 56 and the support wheel 57 are both in contact with the inner wall of the seam steel pipe body 8.
[0093] As an embodiment of the scratch cutting portion 12 in the present invention:
[0094] The scoring and cutting part 12 includes a limit plate 121, and a short shaft 122 is fixedly connected to one side of the limit plate 121, a stepper motor 123 is fixedly installed at the end of the support claw at the top, and an eccentrically arranged jump disk 124 is transmission-connected at the output end of the stepper motor 123, and a ring member 125 is fixedly connected to the outer side of the jump disk 124, a plug-in board 126 is arranged at the top of the ring member 125, and a scoring knife 127 is plugged into the outer side of the plug-in board 126, and the scoring knife 127 is fixedly connected to the plug-in board 126 by a second bolt, and the scoring knife 127 is easy to install and replace, and a strip slide rail is fixedly connected to the bottom end of the ring member 125 128, and the short shaft 122 is slidably connected with the bar slide rail 128, and the length of the bar slide rail 128 is relatively long, so that the scoring knife 127 can always cut the inner weld convex material during the adjustment of the length of the claw. Specifically, the output shaft of the stepping motor 123 rotates one circle intermittently, and the transmission jump plate 124 rotates one circle. Due to the eccentric setting, the top of the jump plate 124 jumps, so that the scoring knife 127 can contact the weld convex material when it is at the top. The bar slide rail 128 and the short shaft 122 cooperate to limit the running track of the scoring knife 127 and improve its stability.
[0095] As an embodiment of the mounting mechanism 6 in the present invention:
[0096] The mounting mechanism 6 includes at least two mounting rings 61, and the core shaft body 51 is slidably connected to the inside of the mounting ring 61. A notch is opened on the inner top of the mounting ring 61, and a plate-shaped gear 62 meshing with the groove-shaped rack 52 is rotatably connected to the inner side of the notch. A servo motor 63 is fixedly connected to the outer side of the mounting ring 61, and the output shaft of the servo motor 63 passes through the mounting ring 61 and is transmission-connected to the plate-shaped gear 62. Suspensions 64 are fixedly connected to the tops of both sides of the mounting ring 61, and first electric push rods 65 are fixedly connected to the two side walls of the top of the stainless steel pipe making machine 1, and the output end of the first electric push rod 65 is transmission-connected to the end of the suspension 64.
[0097] Further, in the above technical solution, a pipe head 58 is fixedly connected to one end of the mandrel body 51 close to the three-jaw chuck 53, a pressure-bearing pipe 59 is installed at the other end of the mandrel body 51, and at least three high-pressure nozzles 510 are connected to the outside of the pipe head 58, and the high-pressure nozzles 510 are arranged in an inclined annular array, the high-pressure nozzles 510 and the supporting claws are staggered, and the high-pressure nozzles 510 are inclined toward the inner wall of the seamed steel pipe, so as to facilitate the outward flushing of the inner wall of the seamed steel pipe and the removal of the internal cutting residue;
[0098] A cavity is formed at the axis center of the core shaft body 51, and the pipe head 58 and the pressure-bearing pipe 59 are both connected to the cavity;
[0099] The core shaft body 51 is composed of multiple core shaft tube segments 511, and a threaded segment 512 is integrally provided at one end of the core shaft tube segment 511, and an internal thread groove matching the threaded segment 512 is opened on the inner side of the other end of the core shaft tube segment 511, and an annular groove 513 is opened inside the core shaft body 51 and on one side of the internal thread groove, and a sealing gasket 514 is provided in the annular groove 513. The sealing gasket 514 ensures that the core shaft body 51 composed of multiple core shaft tube segments 511 has good sealing performance, thereby ensuring the pressure inside the core shaft body 51. The number of core shaft tube segments 511 can be selected according to actual use needs, thereby controlling the length of the core shaft body 51.
[0100] Furthermore, in the above technical solution, a high-pressure water pump or a high-pressure air pump is provided at the input end of the pressure-bearing pipe 59, which is used to clean the cutting residues inside the cavity, flush the cutting residues forward, and move the cutting residues to facilitate separation, so as to facilitate discharge in subsequent processing. The seamed steel pipe body 8 is cooled by air cooling or water cooling, which improves the processing efficiency and reduces the defective rate in the processing of the seamed steel pipe.
[0101] Furthermore, in the above technical solution, the mounting mechanism 6 is mounted at the opening of the seamed steel pipe body 8, and the opening of the seamed steel pipe body 8 facilitates the insertion of the plate on the top of the mounting ring 61, thereby realizing the suspended fixation of the core shaft body 51;
[0102] A space area for the core shaft body 51 to move is provided inside the stainless steel pipe making machine 1 and located at the installation mechanism 6, so as to facilitate the installation or removal of the core shaft body 51. When installing and maintaining the internal scraper, there is no need to pry open the seamed steel pipe, thereby reducing damage to the seamed steel pipe and improving the yield rate.
[0103] The three-jaw chuck 53 is provided with a small bevel gear 515 for adjusting the extension length of multiple claws. The small bevel gear 515 is rotated to drive the driving mechanism inside the three-jaw chuck 53, so that the three claws on the three-jaw chuck 53 are extended or retracted synchronously, thereby meeting the processing needs of seam steel pipes with different inner diameters;
[0104] The end of the claw is fixed with an H-shaped plate 516 by a third bolt, and the inner scraper 56 and the support wheel 57 are both detachably mounted on the H-shaped plate 516, which facilitates the installation and maintenance of the inner scraper 56 and the support wheel 57, and ensures a precise cutting effect;
[0105] The output shafts of the multiple servo motors 63 rotate synchronously, and the plate gear 62 is fixed by the self-locking property of the output shafts of the multiple servo motors 63 when not working, that is, the protruding solder part inside the pipe is cut during the welding process, and the stability of the core shaft body 51 in the internal scraping mechanism 5 can be guaranteed.
[0106] Further, in the above technical solution, a first extension frame 13 is fixedly connected to one side of the output end of the stainless steel pipe making machine 1, a second extension frame 14 is fixedly connected to the other side of the output end of the stainless steel pipe making machine 1, and a support frame 15 is fixedly connected to the top of the first extension frame 13;
[0107] The transverse plate 91 and the winding frame 10 are both arranged on the supporting frame 15, the first extension frame 13 is located on the side of the winding frame 10 away from the outer cutting portion 9, a hydraulic cylinder 16 is fixedly installed on one side of the top of the first extension frame 13, and a hydraulic mechanism for providing kinetic energy is provided at the connecting end of the hydraulic cylinder 16, and the output end of the hydraulic cylinder 16 is fixedly connected to the bottom of the polishing portion 11;
[0108] A sliding rod 17 is fixedly connected to the top of the second extension frame 14. The sliding rod 17 passes through the polishing portion 11 and is slidably connected to the through hole.
[0109] The hydraulic mechanism enables the output end of the hydraulic cylinder 16 to push the polishing part 11 up and down, so that the polishing belt at the bottom of the belt pipe polishing machine contacts the weld and performs grinding and polishing, and the slide rod 17 can ensure the stability of the polishing part 11 in the moving and fixed state.
[0110] Furthermore, in the above technical solution, the production line also includes a cooling spray system, which sprays coolant corresponding to the inside of the stainless steel pipe making machine 1, the outside cutting part 9, the winding frame 10 and the polishing part 11, so as to cool the winding and welding process of the seamed steel pipe;
[0111] The polishing section 11 is configured as a belt-type pipe polishing machine, and the belt-type pipe polishing machine may be a product operated by Guangzhou Longteng Grinding Co., Ltd.
[0112] Furthermore, in the above technical solution, both ends of the outer side of the pressing roller part 3 are movably connected with limit rings for adapting to stainless steel strips of different widths and performing limit adjustment, so that the stainless steel strip enters from the middle position of the pressing roller part 3, thereby better performing precise pipe making in the stainless steel pipe making machine 1.
[0113] A method for welding a seamed steel pipe is provided, wherein the above-mentioned production line is used for processing, and the specific steps are as follows:
[0114] Step 1: The stainless steel strip is taken off from the steel strip coil and fed into the input end of the stainless steel pipe making machine 1 at a uniform speed. The burrs on the surface of the stainless steel strip are processed by the trimming part 7. The burrs are scraped off during the sliding contact between the surface of the stainless steel strip and the flat scraper blade. The strip is adjusted according to the pipe diameter processing requirements of the seamed steel pipe body 8. The threaded rods 78 on both sides are rotated to move the first cutting module 76 and the second cutting module 77, so that the gap between the first cutting module 76 and the second cutting module 77 is located at the center of the notch 74. The blades 79 on both sides cut the two sides of the stainless steel strip, and the cutting surfaces are parallel inclined surfaces. After the inclined surfaces on both sides are butted, the contact area is increased compared with the straight contact, and the seams at both ends are staggered in orientation, and the connection strength is significantly enhanced after welding;
[0115] Step 2: According to the inner and outer diameter size requirements of the seamed steel pipe body 8, the device is adjusted to realize the processing of the seamed steel pipe body 8 of different specifications. Specifically, the gap between the shaping roller and the pressing roller of the stainless steel pipe making machine 1 is adjusted to wind the seamed steel pipe body 8 of different diameters, and the height of the inner scraping mechanism 5 is adjusted to make the mandrel body 51 at the axial center of the seamed steel pipe body 8, and the small bevel gear 515 is rotated to drive the driving mechanism inside the three-jaw chuck 53, so that the three claws on the three-jaw chuck 53 are synchronously extended or retracted, so as to meet the processing needs of the seamed steel pipes with different inner diameters. The inner scraper 56 and the support wheel 57 support the three-jaw chuck 53 in a triangular shape, so as to improve the stability of the mandrel body 51, and the mandrel body 51 coincides with the axis of the seamed steel pipe body 8;
[0116] Step 3: Use multiple pressing wheels and shaping rollers of the stainless steel pipe making machine 1 to gradually roll the stainless steel strip into a seamed steel pipe body 8, and continuously transport it for continuous processing, and accurately install the outer cutting part 9 and the inner scraping mechanism 5;
[0117] Step 4: When the seamed steel pipe body 8 is transported to the output end of the stainless steel pipe making machine 1, a high-frequency welding machine is used in conjunction with a magnetic coil 4 to heat the seamed steel pipe at the final stage of welding, and pressure is applied to close and weld the seamed steel pipe body 8;
[0118] Step 5: Use the outer cutting part 9 and the inner scraping mechanism 5 to cut the outer and inner weld convex materials of the seam steel pipe body 8 after welding, and before the inner scraping mechanism 5 cuts the weld convex material, the output shaft of the stepping motor 123 rotates one circle intermittently, driving the transmission jump plate 124 to rotate one circle. Due to the eccentric setting, the bar slide rail 128 and the short shaft 122 cooperate to limit the running track of the scoring knife 127, so that the top of the jump plate 124 jumps, so that the scoring knife 127 can contact the weld convex material when it is at the top, cut the weld convex material on the front side of the inner scraper 56, and when the inner weld convex material is cut off, the sections of solder are easy to fall off, and the adverse effect of spiral distortion of the solder is reduced;
[0119] Step 6: Use the winding frame 10 to wind and store the weld convex material cutting strip, use the quick clamp mechanism to clamp the end of the weld convex material cutting strip, and then the first drive motor output shaft drives the winding steel ring to wind the weld convex material cutting strip. After winding to a certain length, the weld convex material cutting strip is cut, and then the storage roll can be taken down. Use a high-pressure water pump or a high-pressure air pump to clean the cutting residue inside the cavity, flush the cutting residue forward, and move the cutting residue to make it easy to separate, so as to facilitate discharge in subsequent processing. Use air cooling or water cooling to cool the seamed steel pipe body 8, which improves the processing efficiency and reduces the defective rate in the processing of the seamed steel pipe;
[0120] Step 7: After cutting, the seamed steel pipe body 8 is further transported to the polishing part 11, and the weld position at the top of the seamed steel pipe body 8 is polished and ground by the polishing belt of the polishing part 11, and the weld of the seamed steel pipe body 8 is finely processed.
[0121] The above description is only by way of illustration of certain exemplary embodiments of the present invention. It is undoubted that those skilled in the art can modify the described embodiments in various ways without departing from the spirit and scope of the present invention. Therefore, the above drawings and descriptions are illustrative in nature and should not be construed as limiting the scope of protection of the claims of the present invention.
Claims
1. A production line for welding a seamless steel pipe, comprising a stainless steel pipe making machine (1) for winding a stainless steel strip into a seamless steel pipe body (8), wherein the seamless steel pipe body (8) passes between shaping rollers of the stainless steel pipe making machine (1), wherein an input end of the stainless steel pipe making machine (1) is provided with a mounting frame (2), and both sides of the mounting frame (2) are provided with a pressing roller portion (3), and an output end of the stainless steel pipe making machine (1) is provided with a magnetic coil (4), and a connection end of the magnetic coil (4) is connected to an output end of a high-frequency welding machine, and the high-frequency welding machine cooperates with the magnetic coil (4) to perform welding processing on the seamless steel pipe, characterized in that: An inner scraping mechanism (5) is movably connected to the axis of the seamed steel pipe body (8), and the inner scraping mechanism (5) is assembled with the top two side walls of the stainless steel pipe making machine (1) via a mounting mechanism (6); The production line also includes: A trimming section (7) is mounted on the mounting frame (2), and the trimming section (7) is located between the two pressing roller sections (3), and the trimming section (7) is used to process burrs on the surface of the stainless steel strip, and the trimming section (7) cuts inclined sections on both sides of the stainless steel strip, and the inclined sections on both sides of the stainless steel strip are distributed in parallel; An outer cutting part (9) is installed at the output end of the stainless steel pipe making machine (1) and is located directly above the seamed steel pipe body (8). The outer cutting part (9) is used to cut the weld convex material at the top of the seamed steel pipe body (8); A winding frame (10) is installed on one side of the outer cutting portion (9) and is used to wind and store the weld convex material cutting strip; A polishing part (11) is correspondingly mounted on the top of the seamed steel pipe body (8), and the polishing part (11) is used to polish and grind the weld position of the seamed steel pipe body (8) after the weld convex material is cut; The internal scraping mechanism (5) comprises a mandrel body (51), and a groove-shaped rack (52) is provided at the top of the outer side of the mandrel body (51); a three-jaw chuck (53) is installed at the outer end of the mandrel body (51), and a sleeve hole (54) matching the mandrel body (51) is provided at the axis of the three-jaw chuck (53); a collar (55) is provided on one side of the three-jaw chuck (53) and located outside the sleeve hole (54) for interference connection, and the collar (55) and the three-jaw chuck (53) are fixedly installed by a first bolt, and a support claw located at the top of the three-jaw chuck (53) An inner scraper (56) is installed on the inner scraper (56), and the inner scraper (56) is used to cut the weld convex material inside the seam steel pipe body (8). A scratching and cutting part (12) is provided on the outer side of the three-jaw chuck (53) and close to the mounting mechanism (6). The scratching and cutting part (12) is used to cut the weld convex material at the front side of the inner scraper (56). Support wheels (57) are installed on the two supporting claws located at the bottom of the three-jaw chuck (53), and the ends of the inner scraper (56) and the support wheel (57) are both in contact with the inner wall of the seam steel pipe body (8); The mounting mechanism (6) comprises at least two mounting rings (61), and the core shaft body (51) is slidably connected to the inside of the mounting ring (61). A notch is provided on the inner top of the mounting ring (61), and a plate-shaped gear (62) meshing with the groove-shaped rack (52) is rotatably connected to the inner side of the notch. A servo motor (63) is fixedly connected to the outer side of the mounting ring (61), and the output shaft of the servo motor (63) passes through the mounting ring (61) and is transmission-connected to the plate-shaped gear (62). Suspensions (64) are fixedly connected to the tops of both sides of the mounting ring (61), and first electric push rods (65) are fixedly connected to the two side walls of the top of the stainless steel pipe making machine (1), and the output end of the first electric push rod (65) is transmission-connected to the end of the suspension (64).
2. A production line for welding a seamed steel pipe according to claim 1, characterized in that: The scoring and cutting portion (12) comprises a limit plate (121), and a short shaft (122) is fixedly connected to one side of the limit plate (121); a stepping motor (123) is fixedly installed at the end of the support claw located at the top; an eccentrically arranged jump plate (124) is transmission-connected to the output end of the stepping motor (123); an annular member (125) is fixedly connected to the outer side of the jump plate (124); a plug-in plate (126) is arranged at the top end of the annular member (125); a scoring knife (127) is plugged into the outer side of the plug-in plate (126); the scoring knife (127) and the plug-in plate (126) are fixedly connected via a second bolt; a strip slide rail (128) is fixedly connected to the bottom end of the annular member (125); and the short shaft (122) and the strip slide rail (128) are slidably connected.
3. The production line for welding a seamed steel pipe according to claim 1, characterized in that: One end of the mandrel body (51) close to the three-jaw chuck (53) is fixedly connected to a pipe head (58), the other end of the mandrel body (51) is installed with a pressure-bearing pipe (59), and the outside of the pipe head (58) is connected to at least three high-pressure nozzles (510), and the high-pressure nozzles (510) are arranged in an inclined annular array; A cavity is formed at the axis center of the core shaft body (51), and the pipe head (58) and the pressure-bearing pipe (59) are both connected to the cavity; The mandrel body (51) is composed of a plurality of mandrel tube segments (511), and a threaded segment (512) is integrally provided at one end of the mandrel tube segment (511), and an internal threaded groove matching the threaded segment (512) is provided on the inner side of the other end of the mandrel tube segment (511), and an annular groove (513) is provided inside the mandrel body (51) and on one side of the internal threaded groove, and a sealing gasket (514) is provided in the annular groove (513).
4. A production line for welding a seamed steel pipe according to claim 3, characterized in that: The input end of the pressure-bearing pipe (59) is provided with a high-pressure water pump or a high-pressure air pump, which is used to clean the cutting residue inside the cavity and to cool the seamed steel pipe body (8).
5. The production line for welding a seamed steel pipe according to claim 1, characterized in that: The mounting mechanism (6) is mounted at the opening of the seamed steel pipe body (8); A space area for the core shaft (51) to move is provided inside the stainless steel pipe making machine (1) and located at the mounting mechanism (6); The three-jaw chuck (53) is provided with a small bevel gear (515) for adjusting the extension length of the plurality of claws; An H-shaped plate (516) is fixedly mounted on the end of the support claw via a third bolt, and the inner scraper (56) and the support wheel (57) are both detachably mounted on the H-shaped plate (516); The output shafts of the plurality of servo motors (63) rotate synchronously.
6. The production line for welding a seamed steel pipe according to claim 1, characterized in that: The outer cutting portion (9) comprises a transverse plate (91), a bayonet is provided on the transverse plate (91), a tool rod (92) is inserted into the bayonet, an outer scraper (93) is detachably mounted on the bottom end of the tool rod (92), and the transverse plate (91) and the tool rod (92) are fixedly connected by a fourth bolt.
7. A production line for welding a seamed steel pipe according to claim 6, characterized in that: A first extension frame (13) is fixedly connected to one side of the output end of the stainless steel pipe making machine (1), a second extension frame (14) is fixedly connected to the other side of the output end of the stainless steel pipe making machine (1), and a support frame (15) is fixedly connected to the top of the first extension frame (13); The transverse plate (91) and the winding frame (10) are both arranged on the support frame (15); the first extension frame (13) is located on a side of the winding frame (10) away from the outer cutting portion (9); a hydraulic cylinder (16) is fixedly mounted on one side of the top of the first extension frame (13); a hydraulic mechanism for providing kinetic energy is provided at a connection end of the hydraulic cylinder (16); and an output end of the hydraulic cylinder (16) is fixedly connected to the bottom of the polishing portion (11); A sliding rod (17) is fixedly connected to the top of the second extension frame (14); the sliding rod (17) passes through the polishing portion (11) and is slidably connected to the through hole.
8. The production line for welding a seamed steel pipe according to claim 7, characterized in that: The production line also includes a cooling spray system, which sprays cooling liquid at the inner and outer cutting parts (9), the winding frame (10) and the polishing part (11) of the stainless steel pipe making machine (1) to cool the seam steel pipe during the winding and welding process; The polishing part (11) is configured as a belt-type pipe polishing machine.
9. The production line for welding a seamless steel pipe according to claim 1, characterized in that: Both ends of the outer side of the pressing roller part (3) are movably connected to limit rings for adapting to stainless steel strips of different widths and performing limit adjustment; The trimming section (7) comprises two parallel distributed racks (71), and the racks (71) are fixed on the mounting frame (2); a second electric push rod (72) is fixedly connected to the rack (71); an output end of the second electric push rod (72) passes through the rack (71) and is fixedly connected to a trimming plate (73); and flat scraping blades are provided at the corners of the trimming plate (73); A notch (74) is provided on the upper surface of the trimming plate (73) at the bottom, and the depth of the notch (74) is equal to the thickness of the stainless steel strip. Limiting grooves (75) are provided on both sides of the notch (74), and a first cutting module (76) and a second cutting module (77) are slidably connected inside the two limiting grooves (75), respectively. A threaded rod (78) is threadedly penetrated on both sides of the trimming plate (73), and the threaded rod (78) penetrates the limiting groove (75) and is rotatably connected to one of the first cutting module (76) and the second cutting module (77); The first cutting module (76) and the second cutting module (77) are each provided with a cutting blade (79) on one side opposite to the other, the cutting blades (79) on both sides are arranged obliquely, and the cutting blades (79) on both sides are distributed in parallel.
10. A method for welding a seamed steel pipe, using the production line according to any one of claims 1 to 9 for processing, characterized in that: The specific steps are as follows: Step 1: The stainless steel strip is taken off the steel strip coil and fed into the input end of the stainless steel pipe making machine (1) at a uniform speed, the burrs on the surface of the stainless steel strip are processed by a trimming section (7), and inclined and parallel sections are cut on both sides of the stainless steel strip to expand the contact surface; Step 2: adjusting the device according to the inner and outer diameter dimension requirements of the seamed steel pipe body (8) to be processed, thereby realizing the processing of seamed steel pipe bodies (8) of different specifications; Step 3: using a plurality of pressing wheels and shaping rollers of a stainless steel pipe making machine (1) to gradually press and roll the stainless steel strip into a seamed steel pipe body (8), and continuously conveying and processing the strip for accurate installation of the outer cutting portion (9) and the inner scraping mechanism (5); Step 4: When the seamed steel pipe body (8) is transported to the output end of the stainless steel pipe making machine (1), a high-frequency welding machine is used in conjunction with a magnetic coil (4) to heat the seamed steel pipe at the final stage of welding, and pressure is applied to close and weld the seamed steel pipe body (8); Step 5: using the outer cutting portion (9) and the inner scraping mechanism (5) to respectively cut the outer and inner weld convex materials of the welded steel pipe body (8) after welding, and on the inner scraping mechanism (5), the scoring and cutting portion (12) is used to cut the weld convex material in front of the inner scraper (56) to facilitate cutting off the inner weld convex material; Step 6: Using a reel (10) to reel in the weld convex material cutting strip, and using a high-pressure water pump or a high-pressure air pump to clean the cutting residue inside the cavity; Step 7: After cutting, the seamed steel pipe body (8) is further transported to the polishing section (11), and the welding seam position at the top of the seamed steel pipe body (8) is polished and ground using the polishing belt of the polishing section (11).