Semiconductor device and method for manufacturing the same

By setting an etch cutoff layer in a semiconductor device and using specific etching technology, the problem of etching depth control of p-GaN layer is solved, and the stability and electrical performance of the device are improved.

CN118553765BActive Publication Date: 2024-11-29XIAN JIAOTONG LIVERPOOL UNIV
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411035628.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-11-29
Estimated Expiration
2044-07-31

AI Technical Summary

Technical Problem

The prior art cannot accurately control the etching depth of the p-GaN layer, resulting in challenges in process stability and repetition of p-channel devices.

Method used

By setting an etch cut-off layer in the semiconductor device, including the p-AlxGa1-xN layer, the molar ratio of Al ions is 2%≤x≤15%, and using inductively coupled plasma etching technology and wet etching technology, accurate The etching depth is controlled to prevent etching to the first p-type gallium nitride layer.

Benefits of technology

Accurate control of the etching depth of semiconductor devices is achieved, the stability and electrical performance of the device are improved, the thickness controllability of the first p-type gallium nitride layer is ensured, and the functional performance of the device is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118553765B_ABST
    Figure CN118553765B_ABST
Patent Text Reader

Abstract

The present invention discloses a semiconductor device and a preparation method thereof, wherein the semiconductor device comprises a substrate; a barrier layer; a first p-type gallium nitride layer, wherein the first p-type gallium nitride layer and the barrier layer form a hole heterojunction structure; an etching stop layer, which is located on the side of the hole barrier layer away from the substrate, and the etching stop layer comprises a first groove, wherein the first groove penetrates the etching stop layer; a second p-type gallium nitride layer, which is located on the side of the etching stop layer away from the substrate, and the second p-type gallium nitride layer comprises a second groove, wherein the second groove penetrates the second p-type gallium nitride layer, and the second groove overlaps the first groove along the thickness direction of the semiconductor device; a source electrode and a drain electrode are located on the side of the second p-type gallium nitride layer away from the substrate, and the gate electrode overlaps the first groove along the thickness direction of the semiconductor device. By adopting the above means, by setting the etching stop layer, the etching depth of the semiconductor device can be accurately controlled, and etching to the first p-type gallium nitride layer can be prevented, thereby improving the stability and electrical performance of the device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of microelectronic technology, and in particular to a semiconductor device and a preparation method thereof. Background Art

[0002] P-channel GaN devices are particularly important for realizing complementary logic circuits and have broad application prospects. To realize enhanced p-channel GaN devices, the p-GaN layer needs to be etched to a specific thickness to form a depletion region to deplete the two-dimensional hole gas (2DHG) and turn off the device.

[0003] Since the etching depth of the p-GaN layer cannot be accurately controlled, the process stability and repeatability of p-channel devices are greatly challenged. Summary of the invention

[0004] The present invention provides a semiconductor device and a preparation method thereof, which can accurately control the etching depth of the semiconductor device to prevent etching to the first p-type gallium nitride layer, thereby improving the stability and electrical performance of the device.

[0005] In a first aspect, an embodiment of the present invention provides a semiconductor device, including:

[0006] substrate;

[0007] A barrier layer, located on one side of the substrate;

[0008] A first p-type gallium nitride layer, located on a side of the barrier layer away from the substrate, the first p-type gallium nitride layer and the barrier layer forming a hole heterojunction structure;

[0009] an etching stop layer, located at a side of the first p-type gallium nitride layer away from the substrate, the etching stop layer comprising a first groove, and the first groove penetrates the etching stop layer;

[0010] a second p-type gallium nitride layer, located on a side of the etching stop layer away from the substrate, the second p-type gallium nitride layer comprising a second groove, the second groove penetrates the second p-type gallium nitride layer, and along a thickness direction of the semiconductor device, the second groove overlaps the first groove;

[0011] an electrode structure, comprising a source electrode, a gate electrode and a drain electrode; the source electrode and the drain electrode are located on a side of the second p-type gallium nitride layer away from the substrate, and along a thickness direction of the semiconductor device, the gate electrode overlaps with the first groove;

[0012] Wherein, the etching stop layer comprises p-Al x Ga 1-x N layers;

[0013] The molar ratio x of Al ions in the etching stop layer satisfies 2%≤x≤15%.

[0014] Optionally, a thickness L1 of the first p-type gallium nitride layer satisfies 8nm≤L1≤11nm.

[0015] Optionally, the thickness L2 of the etching stop layer satisfies 3nm≤L2≤8nm.

[0016] Optionally, the semiconductor device further includes a polarization enhancement layer, wherein the polarization enhancement layer is located between the barrier layer and the first p-type gallium nitride layer.

[0017] Optionally, the semiconductor device further includes a cap layer, wherein the cap layer is located between the second p-type gallium nitride layer and the source electrode, and between the second p-type gallium nitride layer and the drain electrode;

[0018] The doping concentration of the cap layer is greater than the doping concentration of the second p-type gallium nitride layer.

[0019] Optionally, the gate is at least located in the first groove, and the gate is in contact with the first p-type gallium nitride layer;

[0020] Alternatively, the semiconductor device further includes a gate dielectric layer, and the gate dielectric layer is located between the gate and the first p-type gallium nitride layer.

[0021] In a second aspect, an embodiment of the present invention further provides a method for preparing a semiconductor device, comprising:

[0022] providing a substrate;

[0023] preparing a barrier layer on one side of the substrate;

[0024] Preparing a first p-type gallium nitride layer on a side of the barrier layer away from the substrate, wherein the first p-type gallium nitride layer and the barrier layer form a hole heterojunction structure;

[0025] An etching stop layer is prepared on a side of the first p-type gallium nitride layer away from the substrate; wherein the etching stop layer comprises p-Al x Ga 1-x N layer; the molar ratio x of Al ions in the etching stop layer satisfies 2%≤x≤15%;

[0026] Forming a second p-type gallium nitride layer on a side of the etching stop layer away from the substrate;

[0027] Etching the second p-type gallium nitride layer and the etch stop layer to form a second groove in the second p-type gallium nitride layer and generate an etch stop structure in the etch stop layer;

[0028] Removing the etch stop structure to form a first groove in the etch stop layer, wherein the first groove overlaps with the second groove along a thickness direction of the semiconductor device;

[0029] An electrode structure is prepared, the electrode structure comprising a source, a gate and a drain; the source and the drain are located on a side of the second p-type gallium nitride layer away from the substrate, and along the thickness direction of the semiconductor device, the gate overlaps the first groove.

[0030] Optionally, etching the second p-type gallium nitride layer and the etching stop layer includes:

[0031] The second p-type gallium nitride layer and the etching stop layer are etched using an inductively coupled plasma etching technique; the plasma used in the inductively coupled plasma etching technique includes SF6, and the etching stop layer includes p-Al x Ga 1-x N layer, the etching stop structure comprises AlF3;

[0032] Removing the etch stop structure to form a first groove in the etch stop layer includes:

[0033] The etch stop structure is removed by wet etching technology to form a first groove in the etch stop layer. The solution used in the wet etching technology includes HF / NH4OH or TMAH solution.

[0034] Optionally, after preparing the barrier layer on one side of the substrate, the method further comprises:

[0035] Preparing a polarization enhancement layer on a side of the barrier layer away from the substrate;

[0036] Preparing a first p-type gallium nitride layer on a side of the barrier layer away from the substrate, comprising:

[0037] A first p-type gallium nitride layer is formed on a side of the polarization enhanced layer away from the substrate.

[0038] In the technical solution of the embodiment of the present invention, the first p-type gallium nitride layer and the barrier layer form a hole heterojunction structure, and a two-dimensional hole gas is provided in the hole heterojunction. The etching stop layer is etched through the second groove in the second p-type gallium nitride layer to form an etching stop structure in the etching stop layer, and the etching stop structure is further removed to form the first groove. That is, when etching the semiconductor device, the etching stops at the interface between the etching stop layer and the first p-type gallium nitride layer, so that the etching depth of the semiconductor device can be accurately controlled to prevent etching to the first p-type gallium nitride layer, and ensure that the thickness of the first p-type gallium nitride layer is accurately controllable, thereby improving the stability and electrical performance of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] Figure 1 A schematic top view of a semiconductor device provided by an embodiment of the present invention;

[0040] Figure 2 for Figure 1 A schematic diagram of a first cross-sectional structure of a semiconductor device along a cross-sectional line AA' is provided;

[0041] Figure 3 A schematic diagram of a curve showing changes in etching time and etching depth during a semiconductor device manufacturing process provided by an embodiment of the present invention;

[0042] Figure 4 for Figure 1 A schematic diagram of a second cross-sectional structure of a semiconductor device along a cross-sectional line AA' is provided;

[0043] Figure 5 for Figure 1 A third cross-sectional structural schematic diagram of a semiconductor device along a cross-sectional line AA' is provided;

[0044] Figure 6 A process flow chart of a first semiconductor device manufacturing method provided by an embodiment of the present invention;

[0045] Figure 7 A schematic diagram of a relationship curve between gas pressure and etching rate provided in an embodiment of the present invention;

[0046] Figure 8 A partial physical diagram of a semiconductor device provided by an embodiment of the present invention;

[0047] Fig. 9 for Figure 8 The corresponding enlarged schematic diagram of the aa region;

[0048] Fig.10 A schematic diagram of etching result testing of a semiconductor device provided by an embodiment of the present invention;

[0049] Fig.11 A schematic diagram of test results of an etching cut-off surface in a semiconductor device provided by an embodiment of the present invention;

[0050] Fig.12 A flow chart of the preparation process of a second semiconductor device provided in an embodiment of the present invention. DETAILED DESCRIPTION

[0051] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.

[0052] Figure 1 A schematic top view of a semiconductor device provided by an embodiment of the present invention, Figure 2 for Figure 1 A schematic diagram of a first cross-sectional structure of a semiconductor device along a cross-sectional line AA' is provided, as shown in FIG. Figure 1 and Figure 2 As shown, the semiconductor device includes: a substrate 10; a barrier layer 20, located at one side of the substrate 10; a first p-type gallium nitride layer 30, located at a side of the barrier layer 20 away from the substrate 10, the first p-type gallium nitride layer 30 and the barrier layer 20 forming a hole heterojunction structure; an etching stop layer 40, located at a side of the first p-type gallium nitride layer 30 away from the substrate 10, the etching stop layer 40 includes a first groove 401, the first groove 401 penetrates the etching stop layer 40; a second p-type gallium nitride layer 50, located at a side of the etching stop layer 40 away from the substrate 10, the second p-type gallium nitride layer 50 includes a second groove 501, the second groove 501 penetrates the second p-type gallium nitride layer 50, and along the thickness direction of the semiconductor device (such as Figure 2 ), the second groove 501 overlaps with the first groove 401; the electrode structure 60 includes a source 601, a gate 602 and a drain 603; the source 601 and the drain 603 are located on a side of the second p-type gallium nitride layer 50 away from the substrate 10, and along the thickness direction Z of the semiconductor device, the gate 602 overlaps with the first groove 401.

[0053] Specifically, the first p-type gallium nitride layer 30 and the barrier layer 20 form a hole heterojunction structure, and a two-dimensional hole gas is arranged in the hole heterojunction structure, and the two-dimensional hole gas can be used as a conductive medium in the semiconductor device. Further, an etching stop layer 40 and a second p-type gallium nitride layer 50 are sequentially arranged on the side of the hole heterojunction structure away from the substrate 10, and a second groove 501 can be etched in the second p-type gallium nitride layer 50 through an etching process, and the second groove 501 penetrates the second p-type gallium nitride layer 50, so that the etching stop layer 40 can be etched through the second groove 501 to form an etching stop structure in the etching stop layer. Since the etching stop structure is difficult to volatilize, it can be ensured that the etching process is stopped at the etching stop layer 40 and will not react with the first p-type gallium nitride layer 30 under the etching stop layer 40. Subsequently, the wet etching technology is continued to be used to remove the etching stop structure, that is, the first groove 401 can be etched in the etching stop layer 40. Since the solution used to remove the etching stop structure only reacts with the etching stop structure and does not react with the first p-type gallium nitride layer 30, the first groove 401 penetrates the etching stop layer 40, that is, the first groove 401 is etched to the interface between the etching stop layer 40 and the first p-type gallium nitride layer 30. In this way, by providing the etching stop layer 40, the first groove 401 can be prevented from being etched to the first p-type gallium nitride layer 30, thereby ensuring that the thickness of the first p-type gallium nitride layer is accurately controllable, thereby improving the stability and electrical properties of the semiconductor device.

[0054] Specifically, along the thickness direction Z of the semiconductor device, the second groove 501 overlaps with the first groove 401 , which is beneficial for etching the etching stop layer 40 through the second groove 501 to form the first groove 401 .

[0055] Specifically, the electrode structure 60 includes a source 601, a gate 602, and a drain 603. The source 601 and the drain 603 can form an ohmic contact with the epitaxial structure, respectively, and the gate 602 can form a Schottky contact with the first p-type gallium nitride layer 30. Specifically, the source 601 can be used as an input terminal of the semiconductor device, and the drain 603 can be used as an output terminal of the semiconductor device. It should be noted that Figure 1 The semiconductor device is described as including multiple gates 602 , that is, the semiconductor device is a multi-cell structure. It can be understood that the semiconductor device can also include only one gate 602 , that is, the cell structure is a single cell structure of the source 601 , the gate 602 and the drain 603 .

[0056] Exemplarily, the substrate 10 may be a combination of one or more of gallium nitride, aluminum gallium nitride, indium gallium nitride, aluminum indium gallium nitride, indium phosphide, gallium arsenide, silicon carbide, diamond, sapphire, germanium, silicon, or any other material capable of growing group III nitrides.

[0057] For example, the material of the barrier layer 20 may be CaN or AlCaN.

[0058] It is understandable that the substrate 10 and the barrier layer 20 may also include a stacked nucleation layer, a buffer layer and a channel layer. Exemplarily, the material of the nucleation layer may be AlN, which is located between the substrate and the buffer layer. The nucleation layer affects the parameters such as the crystal quality, surface morphology and electrical properties of the heterojunction material above. The nucleation layer varies with different substrate materials, and mainly plays a role in matching the substrate material and the semiconductor material layer in the heterojunction structure. Exemplarily, the buffer layer is located on one side of the substrate, and the buffer layer may include iron atoms, which is conducive to achieving the high resistance of the buffer layer, ensuring that vertical leakage can be blocked and improving the pinch-off performance of the semiconductor device. The buffer layer can play a role in bonding the semiconductor material layer to be grown next, and can protect the substrate from being invaded by some metal ions. The material of the buffer layer may be a group III nitride material such as AlGaN, GaN or AlGaInN. Exemplarily, the channel layer may be a group III nitride, such as GaN, InGaN or AlInGaN. The channel layer may be undoped or unintentionally doped. The channel layer may also be a multi-layer structure, for example, a combination of superlattice, GaN or AlGaN.

[0059] Optional, continue to refer to Figure 2 , the etching stop layer 40 includes p-Al x Ga 1-x N layer; the molar ratio x of Al ions in the etching stop layer 40 satisfies 2%≤x≤15%.

[0060] Specifically, the second p-type gallium nitride layer 50 and the etching stop layer 40 are etched by inductively coupled plasma etching technology. The plasma used in the inductively coupled plasma etching technology includes SF6. x Ga 1-x N reacts to generate an etch stop structure AlF3 which is difficult to volatilize. A wet etching technique is adopted to remove the etch stop structure using HF / NH4OH or TMAH solution to form a first groove 401 in the etch stop layer 40. The HF / NH4OH or TMAH solution only reacts with the etch stop structure and does not react with the first p-type gallium nitride layer 30. That is, the first groove 401 can penetrate the etch stop layer 40 without etching the first p-type gallium nitride layer 30, thereby ensuring that the thickness of the first p-type gallium nitride layer is precisely controllable, thereby ensuring the stability and electrical performance of the semiconductor device.

[0061] Specifically, the molar ratio x of Al ions in the etching stop layer 40 satisfies 2%≤x≤15%. Such a moderate molar ratio of Al ions can ensure the current conduction of the semiconductor device on the one hand, and provide a higher selectivity during the etching process on the other hand. For example, the molar ratio of Al ions can be x=5%.

[0062] For example, when x>15%, it indicates that the molar ratio of Al ions is relatively high, which in turn affects the conduction of the current of the semiconductor device.

[0063] For example, when x is less than 2%, it indicates that the molar ratio of Al ions is relatively low and a high selectivity cannot be generated during the etching process.

[0064] It should be noted that Figure 3 A schematic diagram of a curve showing a change in etching time and etching depth during a semiconductor device manufacturing process provided by an embodiment of the present invention is shown in FIG. Figure 3 As shown, when x=5%, when the p-GaN film layer above the etching stop layer 40 is etched, the etching rate is about 1nm / min. When the etching stop layer 40 is etched, the etching rate is about 0.25nm / min, that is, the etching rate ratio is 1:4. It can be seen that by adding the etching stop layer 40, the etching rate can be slowed down, thereby extending the etching time and increasing the etching window time, and the etching can be more accurately stopped at the junction of the etching stop layer 40 and the first p-type gallium nitride layer 30, thereby ensuring that the thickness of the first p-type gallium nitride layer is accurately controllable.

[0065] It should also be noted that a higher molar ratio of Al ions will affect the performance of the P-channel device and the hole heterojunction structure. Therefore, the molar ratio x of Al ions in the etching stop layer 40 satisfies 2%≤x≤15%, which can ensure the performance of the P-channel device on the one hand, and slow down the etching rate and increase the etching window time on the other hand.

[0066] The semiconductor device provided by the embodiment of the present invention etches the etching stop layer through the second groove in the second p-type gallium nitride layer to form an etching stop structure in the etching stop layer. Since the etching stop structure is not easy to volatilize, it can ensure that the etching process is stopped at the etching stop layer and will not react with the first p-type gallium nitride layer under the etching stop layer. Subsequently, the etching stop structure is further removed to form the first groove, and in the process of removing the etching stop structure by wet etching, the solution used only reacts with the etching stop structure and does not react with the first p-type gallium nitride layer, that is, when etching the semiconductor device, the etching stops at the interface between the etching stop layer and the first p-type gallium nitride layer. In this way, the etching depth of the semiconductor device can be accurately controlled to prevent etching to the first p-type gallium nitride layer, and ensure that the thickness of the first p-type gallium nitride layer is accurately controllable, thereby improving the stability and electrical performance of the device.

[0067] Optional, continue to refer to Figure 2 , the thickness L1 of the first p-type gallium nitride layer 30 satisfies 8nm≤L1≤11nm.

[0068] Specifically, L1 satisfies 8nm≤L1≤11nm, so that a depletion region is formed to deplete the two-dimensional hole gas in the channel of the first p-type gallium nitride layer 30, and the device is turned off, that is, the gate control effect of the enhanced semiconductor device can be guaranteed. In addition, the output current of the semiconductor device can also be guaranteed to meet the actual application requirements.

[0069] It can be understood that compared with the technical solution of etching the epitaxial structure in the prior art, due to the instability of the process, the prior art cannot control L1 to satisfy 8nm≤L1≤11nm during the etching process of the semiconductor device, and the first groove 401 is easily etched to the upper surface of the first p-type gallium nitride layer 30. However, in the embodiment of the present invention, an etching stop layer 40 is prepared on the side of the first p-type gallium nitride layer 30 away from the substrate 10, so that the etching stop layer 40 is etched during the etching process, which can effectively control the etching accuracy of the semiconductor device, and can prevent the etching of part of the first p-type gallium nitride layer 30, thereby improving the stability and electrical performance of the semiconductor device.

[0070] Exemplarily, when L1>11 nm, it indicates that the thickness of the first p-type gallium nitride layer 30 is too thick to meet the functional requirements of the enhancement mode semiconductor device.

[0071] Exemplarily, when L1<8 nm, it indicates that the thickness of the first p-type gallium nitride layer 30 is relatively thin, and the output current of the semiconductor device is relatively low, thereby affecting the electrical performance of the device.

[0072] Optional, continue to refer to Figure 2 , the thickness L2 of the etching stop layer 40 satisfies 3nm≤L2≤8nm.

[0073] Specifically, L2 satisfies 3nm≤L2≤8nm, indicating that the thickness of the etching stop layer 40 is moderate. On the one hand, it can prevent the etching stop layer 40 from being penetrated during the etching process due to the thin thickness of the etching stop layer 40, resulting in the first groove 401 penetrating the etching stop layer 40 and a portion of the first p-type gallium nitride layer 30, thereby affecting the performance of the semiconductor device. On the other hand, it can prevent the etching stop layer 40 from being too thick, resulting in the first groove 401 being unable to penetrate the etching stop layer 40 during the etching process, thereby failing to complete the subsequent preparation of the gate 602.

[0074] Exemplarily, when L2>8 nm, it indicates that the etching stop layer 40 is relatively thick, and the first groove 401 cannot penetrate the etching stop layer 40 during the etching process, and thus the subsequent preparation of the gate 602 cannot be completed.

[0075] For example, when L2 is less than 3 nm, it indicates that the etching stop layer 40 is relatively thin and the etching stop layer 40 is easily etched through during the etching process, causing the first groove 401 to penetrate the etching stop layer 40 and a portion of the first p-type gallium nitride layer 30 , thereby affecting the performance of the semiconductor device.

[0076] Exemplarily, L2=5 nm, which can ensure that the thickness of the etching stop layer 40 is moderate, which simplifies the preparation process on the one hand, and can ensure the performance of the semiconductor device on the other hand.

[0077] Optional, Figure 4 for Figure 1 A second cross-sectional structure schematic diagram of a semiconductor device along the cross-sectional line AA' is provided, as shown in FIG. Figure 4 As shown, the semiconductor device further includes a polarization enhancement layer 70 , and the polarization enhancement layer 70 is located between the barrier layer 20 and the first p-type gallium nitride layer 30 .

[0078] Specifically, by disposing the polarization enhancement layer 70 between the barrier layer 20 and the first p-type gallium nitride layer 30 , the polarization effect can be enhanced, the concentration of the two-dimensional hole gas can be increased, and the saturation current of the semiconductor device can be increased.

[0079] Exemplarily, the material of the polarization enhancement layer 70 may be aluminum nitride, and its thickness may be 3 nm, which can ensure that the thickness of the polarization enhancement layer 70 is moderate on the one hand, and the concentration of the two-dimensional hole gas is moderate on the other hand.

[0080] Optional, continue to refer to Figure 1 and Figure 2 The semiconductor device further includes a cap layer 80 , which is located between the second p-type gallium nitride layer 50 and the source 601 , and between the second p-type gallium nitride layer 50 and the drain 603 ; the doping concentration of the cap layer 80 is greater than the doping concentration of the second p-type gallium nitride layer 50 .

[0081] Specifically, by providing the cap layer 80 , the surface state of the semiconductor device can be reduced, the surface leakage of the subsequent semiconductor device can be reduced, and the current collapse can be suppressed, thereby improving the performance and reliability of the epitaxial structure and the semiconductor device.

[0082] Furthermore, the cap layer 80 may be a heavily doped p-type gallium nitride layer, and the doping concentration of the cap layer 80 is greater than the doping concentration of the second p-type gallium nitride layer 50 , which is beneficial to reducing the Schottky barrier and contact resistance.

[0083] For example, the cap layer 80 may be doped with magnesium ions, and the doping concentration of magnesium ions may be 1×10 20 cm -3 , to achieve heavy doping of the doping medium.

[0084] Optional, Figure 5 for Figure 1 A third cross-sectional structure schematic diagram of a semiconductor device along the cross-sectional line AA' is provided, referring to Figure 2 and Figure 5 As shown, the gate 602 is at least located in the first groove 401 , and the gate 602 contacts the first p-type gallium nitride layer 30 ; or, the semiconductor device further includes a gate dielectric layer 90 , and the gate dielectric layer 90 is located between the gate 602 and the first p-type gallium nitride layer 30 .

[0085] As a feasible implementation method, continue to refer to Figure 1 The gate 602 is located in the first groove 401 and is in contact with the first p-type gallium nitride layer 30 . This manufacturing method is simple.

[0086] As another possible implementation, continue to refer to Figure 5 The gate dielectric layer 90 is prepared between the gate 602 and the first p-type gallium nitride layer by using an atomic layer deposition process or a plasma enhanced atomic layer deposition process, so that a "metal-insulator-semiconductor" structure can be formed, and a better leakage suppression effect of the semiconductor device can be obtained.

[0087] Exemplarily, the material of the gate dielectric layer 90 may be Al 2 O 3 or the like.

[0088] In summary, the semiconductor device provided by the embodiment of the present invention etches the etching stop layer through the second groove in the second p-type gallium nitride layer to form an etching stop structure in the etching stop layer. Since the etching stop structure is difficult to volatilize, it can be ensured that the etching process is stopped at the etching stop layer and will not react with the first p-type gallium nitride layer under the etching stop layer. Subsequently, the wet etching technology is continued to be used to remove the etching stop structure, that is, a first groove can be formed in the etching stop layer. Since the solution used to remove the etching stop structure only reacts with the etching stop structure and does not react with the first p-type gallium nitride layer 30, the first groove penetrates the etching stop layer, that is, when etching the semiconductor device, the etching is stopped at the interface between the etching stop layer and the first p-type gallium nitride layer, preventing etching to the first p-type gallium nitride layer, ensuring that the thickness of the first p-type gallium nitride layer is accurately controllable, and thus improving the stability and electrical performance of the device. In addition, by providing a polarization enhancement layer between the barrier layer and the first p-type gallium nitride layer, the polarization effect can be enhanced, the concentration of the two-dimensional hole gas can be increased, and the saturation current of the semiconductor device can be increased.

[0089] Based on the same inventive concept, an embodiment of the present invention further provides a method for preparing a semiconductor device. Figure 6 A process flow chart of the first semiconductor device manufacturing method provided by the present invention, combined with Figure 1 and Figure 6 As shown, the preparation method comprises:

[0090] S101. Provide a substrate.

[0091] Exemplarily, the substrate 10 may be a combination of one or more of gallium nitride, aluminum gallium nitride, indium gallium nitride, aluminum indium gallium nitride, indium phosphide, gallium arsenide, silicon carbide, diamond, sapphire, germanium, silicon, or any other material capable of growing group III nitrides.

[0092] S102, preparing a barrier layer on one side of the substrate.

[0093] For example, the material of the barrier layer 20 may be gallium nitride or aluminum gallium nitride.

[0094] S103 , preparing a first p-type gallium nitride layer on a side of the barrier layer away from the substrate, the first p-type gallium nitride layer and the barrier layer forming a hole heterojunction structure.

[0095] Specifically, a two-dimensional hole gas is provided in the hole heterojunction structure, and the two-dimensional hole gas can be used as a conductive medium in a semiconductor device.

[0096] S104, preparing an etching stop layer on a side of the first p-type gallium nitride layer away from the substrate.

[0097] Specifically, the etching stop layer includes p-Al x Ga 1-x N layer; the molar ratio x of Al ions in the etching stop layer satisfies 2%≤x≤15%.

[0098] S105 , preparing a second p-type gallium nitride layer on a side of the etching stop layer away from the substrate.

[0099] S106 , etching the second p-type gallium nitride layer and the etching stop layer to form a second groove in the second p-type gallium nitride layer, and generating an etching stop structure in the etching stop layer.

[0100] S107 , removing the etching stop structure to form a first groove in the etching stop layer, wherein the first groove overlaps the second groove along a thickness direction of the semiconductor device.

[0101] For details, please refer to Figure 6 , an etching stop layer 40 and a second p-type gallium nitride layer 50 are sequentially prepared on a side of the first p-type gallium nitride layer 30 away from the substrate 10, and the second p-type gallium nitride layer 50 and the etching stop layer 40 can be etched by inductively coupled plasma etching technology; the plasma used in the inductively coupled plasma etching technology may include SF6, and the etching stop layer 40 may include p-Al x Ga 1-xThe N-layer, etch stop structure 402 may include AlF3.

[0102] For example, the second p-type gallium nitride layer 50 is first etched to form a second groove 501, and then the etching stop layer 40 is etched through the second groove 501. Cl2, BCl3 and SF6 plasma can be used in the etching process. x Ga 1-x The N layer reacts to generate a non-volatile etching stop structure AlF3, which can prevent Cl2, BCl3 and SF6 plasma from further etching the first p-type GaN layer 30. The first groove 401 penetrating the etching stop layer 40 can be obtained by removing the etching stop structure AlF3.

[0103] It should be noted that in the process of etching using inductively coupled plasma etching technology, the active power is 200W, which can increase the density of plasma and ion flux, thereby increasing the etching rate and etching selectivity. The RF power is 10W, which can control the ion bombardment intensity and ensure the etching morphology. The volume flow rates of BCl3, SF6 and N2 plasma can be 60sccm, 20sccm and 30sccm respectively. Figure 7 A schematic diagram of the relationship between gas pressure and etching rate provided in an embodiment of the present invention is shown in FIG. Figure 7 As shown, curve a1 shows the change of GaN etching rate with increasing gas pressure, and curve a2 shows the change of bias voltage with increasing gas pressure. When the proportion of gas flow BCl3, SF6 and N2 is 55%, 19% and 26% respectively, and the gas pressure is 30mTorr, the optimized GaN etching rate is 1nm / min, which is convenient for accurately controlling the etching depth of semiconductor devices. On this basis, continue to refer to Figure 3 , a selectivity ratio of about 1:4 is formed between p-GaN and p-AlGaN, which can prolong the etching time and increase the etching window time, so that the etching can be stopped more accurately at the interface between the etching stop layer and the first p-type gallium nitride layer, thereby ensuring that the thickness of the first p-type gallium nitride layer is accurately controllable. 0.05 Ga 0.95 N.

[0104] Specifically, the etching stop structure can be removed by wet etching technology to form the first groove 401 in the etching stop layer 40. The solution used in the wet etching technology includes HF / NH4OH or TMAH solution. In addition, along the thickness direction of the semiconductor device, the first groove 401 overlaps with the second groove 501, so that it is convenient to etch the etching stop layer 40 through the second groove 501. In addition, since the HF / NH4OH or TMAH solution only reacts with the etching stop structure and does not react with the first p-type gallium nitride layer 30, the first groove 401 can be formed by removing the etching stop structure by wet etching technology.

[0105] Specifically, Figure 8 A partial physical diagram of a semiconductor device provided by an embodiment of the present invention, Fig. 9 for Figure 8 The corresponding enlarged schematic diagram of the aa region is shown in Figure 8 and Fig. 9 As shown, the etching is precisely stopped at the interface between the etching stop layer 40 and the first p-type gallium nitride layer 30, that is, at the position of the first groove after etching, and the remaining thickness of the first p-type gallium nitride layer 30 is about 11 nm, so that the first p-type gallium nitride layer 30 is not etched, thereby ensuring that the thickness of the first p-type gallium nitride layer is precisely controllable.

[0106] Specifically, Fig.10 A schematic diagram of an etching result test of a semiconductor device provided by an embodiment of the present invention, such as Fig.10 As shown, the overall depth of the first groove and the second groove may be 63.7 nm, the length of the first groove may be 5 μm, and the width may be 3 μm. Fig.11 A schematic diagram of test results of etching cut-off surface in a semiconductor device provided by an embodiment of the present invention, such as Fig.11 As shown, the etching stop surface can be understood as the etching stop to the junction between the etching stop layer and the first p-type gallium nitride layer. According to the atomic force microscope test, the root mean square roughness of the etching stop surface is 0.554nm, which means that the interface after etching has good flatness and low roughness.

[0107] By setting the etching stop layer 40, an etching stop structure is formed in the etching stop layer in the subsequent etching process. Since the etching stop structure is not easy to volatilize, it can be ensured that the etching process is stopped at the etching stop layer and will not react with the first p-type gallium nitride layer under the etching stop layer. The etching stop structure is subsequently removed by wet etching technology, that is, a first groove can be formed in the etching stop layer. Since the solution used to remove the etching stop structure only reacts with the etching stop structure and does not react with the first p-type gallium nitride layer 30, the first groove penetrates the etching stop layer, that is, when etching the semiconductor device, the etching is stopped at the interface between the etching stop layer and the first p-type gallium nitride layer, preventing etching to the first p-type gallium nitride layer, ensuring that the thickness of the first p-type gallium nitride layer is precisely controllable, which is conducive to ensuring the stability and electrical performance of the semiconductor device.

[0108] Furthermore, a cap layer 80 may be formed on the upper surface of the second p-type gallium nitride layer 50 . The material of the cap layer 80 may be heavily doped p-type gallium nitride, which is beneficial to reducing the Schottky barrier and contact resistance.

[0109] S108, preparing an electrode structure, the electrode structure comprising a source, a gate and a drain; the source and the drain are located on a side of the second p-type gallium nitride layer away from the substrate, and along a thickness direction of the semiconductor device, the gate overlaps the first groove.

[0110] Specifically, a metal stack is deposited by electron beam evaporation, and a source 601 and a drain 603 are formed on a side of the second p-type gallium nitride layer 50 away from the substrate 10 by rapid annealing. A metal stack is directly deposited by electron beam evaporation to form a gate 602 in the second groove 501, and the gate 602 is located on a side of the first p-type gallium nitride layer 30 away from the substrate 10.

[0111] The method for preparing a semiconductor device provided by an embodiment of the present invention provides an etching stop layer, and prepares a second groove in the second p-type gallium nitride layer through an etching process, and then etches the etching stop layer through the second groove to generate an etching stop structure. Since the etching stop structure is difficult to volatilize, it can be ensured that the etching process is stopped at the etching stop layer and will not react with the first p-type gallium nitride layer under the etching stop layer. The solution used to subsequently remove the etching stop structure only reacts with the etching stop structure and does not react with the first p-type gallium nitride layer. The etching stop structure can be removed by a wet etching process to form a first groove, and the first groove penetrates the etching stop layer, so that the first groove can be prevented from penetrating part of the first p-type gallium nitride layer, thereby ensuring the reliability and electrical performance of the semiconductor device.

[0112] Optional, Fig.12 A process flow chart of a second semiconductor device manufacturing method according to an embodiment of the present invention is provided. Fig.12Based on the above embodiments, the operations after the barrier layer is prepared on one side of the substrate are described in detail. Fig.12 As shown, the preparation method comprises:

[0113] S201, providing a substrate.

[0114] S202, preparing a barrier layer on one side of the substrate.

[0115] S203 , preparing a polarization enhancement layer on a side of the barrier layer away from the substrate.

[0116] Specifically, a polarization enhancement layer 70 is formed on the upper surface of the barrier layer 20, so as to enhance the polarization effect, increase the concentration of the two-dimensional hole gas, and thus increase the saturation current of the semiconductor device. Exemplarily, the polarization enhancement layer 70 may be an aluminum nitride layer.

[0117] S204 , preparing a first p-type gallium nitride layer on a side of the polarization enhanced layer away from the substrate, the first p-type gallium nitride layer and the barrier layer forming a hole heterojunction structure.

[0118] Specifically, a first p-type gallium nitride layer 30 is formed on the upper surface of the polarization enhanced layer 70 . A two-dimensional hole gas is formed between the first p-type gallium nitride layer 30 and the barrier layer 20 .

[0119] S205 , preparing an etching stop layer on a side of the first p-type gallium nitride layer away from the substrate.

[0120] S206 , preparing a second p-type gallium nitride layer on a side of the etching stop layer away from the substrate.

[0121] S207 , etching the second p-type gallium nitride layer and the etching stop layer to form a second groove in the second p-type gallium nitride layer, and generating an etching stop structure in the etching stop layer.

[0122] S208, removing the etching stop structure to form a first groove in the etching stop layer, along the semiconductor device

[0123] S209, preparing an electrode structure, the electrode structure comprising a source, a gate and a drain; the source and the drain are located on a side of the second p-type gallium nitride layer away from the substrate, and along a thickness direction of the semiconductor device, the gate overlaps the first groove.

[0124] The method for preparing a semiconductor device provided by an embodiment of the present invention can enhance the polarization effect and increase the concentration of two-dimensional hole gas by setting a polarization enhancement layer between the barrier layer and the first p-type gallium nitride layer, thereby increasing the saturation current of the semiconductor device.

[0125] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.

Claims

1. A semiconductor device, characterized in that: include: substrate; A barrier layer, located on one side of the substrate; A first p-type gallium nitride layer, located on a side of the barrier layer away from the substrate, the first p-type gallium nitride layer and the barrier layer forming a hole heterojunction structure; an etching stop layer, located at a side of the first p-type gallium nitride layer away from the substrate, the etching stop layer comprising a first groove, and the first groove penetrates the etching stop layer; a second p-type gallium nitride layer, located on a side of the etching stop layer away from the substrate, the second p-type gallium nitride layer comprising a second groove, the second groove penetrates the second p-type gallium nitride layer, and along a thickness direction of the semiconductor device, the second groove overlaps the first groove; an electrode structure, comprising a source electrode, a gate electrode and a drain electrode; the source electrode and the drain electrode are located on a side of the second p-type gallium nitride layer away from the substrate, and along a thickness direction of the semiconductor device, the gate electrode overlaps with the first groove; Wherein, the etching stop layer comprises p-Al x Ga 1-x N layers; The molar ratio x of Al ions in the etching stop layer satisfies 2%≤x≤15%.

2. The semiconductor device according to claim 1, wherein: The thickness L1 of the first p-type gallium nitride layer satisfies 8nm≤L1≤11nm.

3. The semiconductor device according to claim 1, wherein: The thickness L2 of the etching stop layer satisfies 3nm≤L2≤8nm.

4. The semiconductor device according to claim 1, wherein: The semiconductor device further includes a polarization enhancement layer located between the barrier layer and the first p-type gallium nitride layer.

5. The semiconductor device according to claim 1, wherein: The semiconductor device further includes a cap layer, wherein the cap layer is located between the second p-type gallium nitride layer and the source electrode, and between the second p-type gallium nitride layer and the drain electrode; The doping concentration of the cap layer is greater than the doping concentration of the second p-type gallium nitride layer.

6. The semiconductor device according to claim 1, wherein: The gate is at least located in the first groove, and the gate is in contact with the first p-type gallium nitride layer; Alternatively, the semiconductor device further includes a gate dielectric layer, and the gate dielectric layer is located between the gate and the first p-type gallium nitride layer.

7. A method for preparing a semiconductor device, characterized in that: include: providing a substrate; preparing a barrier layer on one side of the substrate; Prepare a first p-type gallium nitride layer on a side of the barrier layer away from the substrate, wherein the first p-type gallium nitride layer and the barrier layer form a hole heterojunction structure; An etching stop layer is prepared on a side of the first p-type gallium nitride layer away from the substrate; wherein the etching stop layer comprises p-Al x Ga 1-x N layer; the molar ratio x of Al ions in the etching stop layer satisfies 2%≤x≤15%; Forming a second p-type gallium nitride layer on a side of the etching stop layer away from the substrate; Etching the second p-type gallium nitride layer and the etch stop layer to form a second groove in the second p-type gallium nitride layer and generate an etch stop structure in the etch stop layer; Removing the etch stop structure to form a first groove in the etch stop layer, wherein the first groove overlaps with the second groove along a thickness direction of the semiconductor device; An electrode structure is prepared, the electrode structure comprising a source, a gate and a drain; the source and the drain are located on a side of the second p-type gallium nitride layer away from the substrate, and along the thickness direction of the semiconductor device, the gate overlaps the first groove.

8. The preparation method according to claim 7, characterized in that: Etching the second p-type gallium nitride layer and the etching stop layer, comprising: The second p-type gallium nitride layer and the etching stop layer are etched using an inductively coupled plasma etching technique; the plasma used in the inductively coupled plasma etching technique includes SF6, and the etching stop layer includes p-Al x Ga 1-x N layer, the etching stop structure comprises AlF3; Removing the etch stop structure to form a first groove in the etch stop layer includes: The etch stop structure is removed by wet etching technology to form a first groove in the etch stop layer. The solution used in the wet etching technology includes HF / NH4OH or TMAH solution.

9. The preparation method according to claim 7, characterized in that: After preparing the barrier layer on one side of the substrate, the method further comprises: Preparing a polarization enhancement layer on a side of the barrier layer away from the substrate; Preparing a first p-type gallium nitride layer on a side of the barrier layer away from the substrate, comprising: A first p-type gallium nitride layer is formed on a side of the polarization enhanced layer away from the substrate.

Citation Information

Patent Citations

  • Method for manufacturing threshold voltage controllable GaN-based enhanced device based on real-time monitoring open gate structure parameter

    CN107248531A

  • Enhanced p-channel field effect transistor for improving threshold voltage

    CN116344581A

  • Insulated gate e-mode transistors

    US20090146185A1