A component micro-filament connection joint and its morphology control method

By surrounding the multi-strand wires around the periphery of the micro filament pin and using solder body welding technology to form a non-clustered connection joint, the problem of morphology control and diameter control of the micro filament joint in the prior art is solved, and high connection strength and Stability, avoid dummy welding defects, and ensure that the joint diameter is consistent with the base material.

CN118572401BActive Publication Date: 2024-11-05CHONGQING UNIVERSITY OF SCIENCE AND TECHNOLOGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411059564.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-04
Publication Date
2024-11-05
Estimated Expiration
2044-08-04

AI Technical Summary

Technical Problem

The prior art cannot quickly and accurately regulate the shape of the micro-fiber joint joint, and it is particularly difficult to control its diameter to the same state as the diameter of the base material, and traditional methods cannot effectively avoid the problems of dummy welding defects and insufficient solder wetting.

Method used

The wire using multiple strands of wire is surrounded by the outer periphery of the micro wire pin, and a non-clustered connection joint is formed by welding the solder body, and the forming channel and feeding mechanism of the welding tool are used to control the filling of the solder and the pull-down speed of the wire to form a A specific shuttle or cylinder structure ensures that the solder is fully wet and forms a stable connection.

Benefits of technology

The multi-strand wire is in a non-clustered state, forming a micro-wire connection joint with high connection strength and stability. It can quickly and accurately adjust the joint shape and length, ensure that the joint diameter is consistent with the base material, avoid dummy welding defects, and improve welding Forming quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118572401B_ABST
    Figure CN118572401B_ABST
Patent Text Reader

Abstract

The present invention discloses a component micro-filament connection joint and a method for controlling its morphology. The connection joint includes a micro-filament pin, and the micro-filament pin is connected to multiple strands of wires of a conductor by welding with a solder body. The multiple strands of wires of the conductor are axially wrapped around the periphery of the micro-filament pin, and the axis of the micro-filament pin is substantially coincident with the axis of the conductor. The multiple strands of wires themselves and the gaps between the multiple strands of wires and the micro-filament pin are filled with the solder body. The control method steps include: heating the graphite part by a welding power supply, so that the solder in the forming channel melts and fills the gap, and the conductor is pulled down vertically at a preset speed. During this process, the multiple strands of wires and the liquid solder gradually gather until a connection joint of the desired morphology is formed. The present invention provides a brand-new component micro-filament connection joint, which can not only quickly and accurately control the morphology of the micro-filament connection joint, but also facilitates accurate control of the length of the micro-filament connection joint.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of avionics components, and in particular relates to a component micro-filament connection joint and a morphology control method thereof. Background Art

[0002] Most of the pins of components are connected to multiple strands of wires by micro-wires, and the quality of the connection joints is directly related to the service life of the components. The existing document CN106785493B discloses a method for connecting micro-diameter electrode pins and multiple strands of wires, which places the multiple strands of wires in the groove electrode head, places the micro-diameter electrode pins on the multiple strands of wires, adjusts the position of the pressed electrode head, sets the welding pressure parameters of the precision resistance welding machine, presses and shapes the micro-diameter electrode pins and multiple strands of wires, and welds the pressed and shaped micro-diameter electrode pins and multiple strands of wires; wherein the pressed electrode head serves as the upper electrode of the precision resistance welding machine, and the groove electrode head serves as the lower electrode of the precision resistance welding machine. The micro-wire pin connection joint (i.e., connection joint, referred to as micro-wire connection joint or micro-wire welding joint) welded and formed based on this method is shown in the attached figure, the micro-diameter electrode pin wire (i.e., micro-wire pin) is oriented to the end surface of the pressed electrode, and the wires of the multiple strands of wires are almost gathered (i.e., multiple adjacent wires are in direct contact), which needs to be further optimized.

[0003] Another existing document CN116387919A provides a device for connecting sensor heterogeneous material pins, including a solder electromagnetic shrink connector, a heating device, a magnetic collector and a coil. The shrink body is filled with solder, and multiple strands of wire and micro-wire sensor pins are arranged inside. After power is turned on, an electromagnetic pulse is generated to cause the metal electromagnetic shrink sleeve to shrink and plastically deform, allowing the liquid solder to fill the gap between the multiple strands of wire and the micro-wire sensor pin. This scheme uses a heating device to heat and melt the solder to form liquid solder, and the shrink body is plastically contracted through the coil, so that the liquid solder can better infiltrate the gap between the multiple strands of wire and the micro-wire, and complete the connection between the multiple strands of wire and the micro-wire. However, this scheme cannot quickly and accurately control the shape of the micro-wire connection joint. More importantly, in the field of micro-wire connection joint technology, it is a technical difficulty in this field to control the diameter of the micro-wire lead connection joint to be consistent / same as the diameter of the parent material. Summary of the invention

[0004] The present invention aims to provide a component micro-wire connection joint in which the wires of a multi-strand conductor are in a non-gathered state and a morphology control method thereof.

[0005] The present invention adopts the following technical solution.

[0006] A component micro-wire connection joint includes a micro-wire pin, the micro-wire pin is connected to multiple strands of wires of a conductor through solder body welding, the multiple strands of wires of the conductor are axially wrapped around the micro-wire pin, the axis of the micro-wire pin is substantially coincident with the axis of the conductor, and the multiple strands of wires themselves and the gaps between the multiple strands of wires and the micro-wire pin are filled with solder body. The solder body refers to the solder after solder welding.

[0007] As a preferred solution, the connecting joint is a shuttle structure with thin ends and a thick middle; or, the connecting joint is a cylindrical structure.

[0008] As a preferred solution, the multiple strands of the wire are embedded in the solder body and cover the fine wire pin in a "grasping" manner. "Grasping" means that the multiple strands of wire in the solder body are in an expanded posture.

[0009] As a preferred embodiment, the micro-filament pin is in the shape of a flat body, a column or a spiral body.

[0010] As a preferred solution, the number of wire strands of the conductor is not less than 15, the wire diameter is not greater than 60 μm, and the diameter of the micro-wire pin is not greater than 0.5 mm.

[0011] A method for controlling the shape of a micro-wire connection joint of a component as described above, wherein the shape of the connection joint is controlled by means of a welding tool, wherein the welding tool comprises a graphite piece 1 connected to the positive electrode of a welding power source, and a graphite piece 2 connected to the negative electrode of the welding power source, wherein both the graphite piece 1 and the graphite piece 2 are provided with semicircular grooves, and the two semicircular grooves can form a forming channel for accommodating a wire, wherein the diameter of the lower section of the forming channel is equal to the outer diameter of the wire, and the upper section of the forming channel is in a funnel-shaped structure; a cooling support block is provided on the wall below the graphite piece, wherein a through hole on the cooling support block is coaxially arranged with the forming channel, and the diameter of the through hole is equal to the outer diameter of the wire; an actuator for vertically pulling the wire downward is provided below the cooling support block; a wire feeding mechanism, a feeding mechanism and a cutting mechanism are provided above the graphite piece, wherein the wire feeding tube of the wire feeding mechanism is coaxially arranged with the forming channel, and the feeding mechanism is used to add solder and brazing agent into the forming channel;

[0012] The steps of the morphology control method include:

[0013] S1, firstly, stripping off the insulation layer of the wire section to be welded to expose multiple strands of wire, then adjusting the multiple strands of wire to a divergent state, and then chemically cleaning and drying the multiple strands of wire and the micro-wire for standby use;

[0014] S2, placing the wire into the semicircular groove of the first graphite piece or the second graphite piece, and then closing and fixing the first graphite piece and the second graphite piece to form a forming channel, wherein the multiple strands of wire are located at the upper section of the forming channel;

[0015] S3, controlling the operation of the wire feeding mechanism to vertically insert (feed) the front section of the micro-filament downward into the middle of the multi-strand wire;

[0016] S4, controlling the feeding mechanism to add powdered brazing material and brazing flux into the forming channel;

[0017] S5, cutting the microfilament from the top of the forming channel, the microfilament after cutting and located in the forming channel is the microfilament pin; the specific cutting position is determined by a person skilled in the art according to the required microfilament pin length;

[0018] S6, electrically heating the graphite part by means of a welding power source, so that the brazing material in the forming channel melts and fills the gap;

[0019] S7, controlling the actuator to operate and vertically pull the wire downward at a preset speed. During this process, the multiple strands of wire and the liquid solder are gradually gathered together until a connection joint of a desired shape is formed.

[0020] As a preferred solution, in step S7, after the upper end of the micro-filament pin leaves the through hole (that is, after the wire and the micro-filament pin are completely pulled out of the forming channel), the actuator is controlled to pause, and the resulting connection joint is in a cylindrical shape.

[0021] As a preferred solution, in step S7, when the upper end of the micro-filament pin is located in the lower middle area of ​​the upper section of the forming channel, the actuator is controlled to pause, and the connection joint obtained at this time is in the form of a shuttle.

[0022] In order to further improve the welding quality of micro-wire connection joints, the speed of the wire moving downward is controlled to 1~2mm / s. If the speed is too fast, it is easy to cause a cold weld defect in the joint because the solder melt cannot fully penetrate into the gap of the wire.

[0023] As a preferred solution, in step S4, the amount of flux added is no more than half of the volume of the upper section of the forming channel. Too little flux added may easily affect the wetting of the solder, while too much flux added may be wasted.

[0024] Beneficial effects: The present invention provides a brand-new component micro-filament connection joint (welding joint), in which the multiple strands of wire are in a non-gathered state, which is essentially different from the structure of the traditional connection joint in which the micro-filament pin is biased to press the electrode end surface, and the micro-filament is covered in a "grabbing" manner and cooperates with the solder filling part to form a specific shuttle structure or column structure, which has the advantages of high connection strength and good stability; by adopting the scheme of the present invention, while ensuring that the solder fully infiltrates the gap of the base material, not only can the shape of the micro-filament connection joint be quickly and accurately controlled, but also the length of the micro-filament connection joint can be accurately controlled, and the position of the protruding part of the joint can also be accurately controlled, and more importantly, the diameter of the micro-filament pin connection joint can be controlled to be consistent / the same as the diameter of the base material (conductor). BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 Schematic diagram of the micro-wire connection joint morphology control process in Example 1, in which: (a) shows the state before the wire is placed in the forming channel; (b) shows the state after the wire is placed in the forming channel and solder is added, the vertically downward hollow arrow shows the direction of vertically pulling the wire downward, and the vertically downward solid arrow shows the direction of vertically adding solder; (c) shows the state at a certain moment in the process of vertically pulling the wire downward; (d) shows the state after the upper end of the micro-wire pin leaves the through hole;

[0026] Figure 2 Schematic diagram of the microfilament connection joint in Example 2. DETAILED DESCRIPTION

[0027] The technical solution of the present invention is described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. It should be noted that the welding method parameters (including welding current, welding voltage, welding time) in the present invention, the specific volume, length, diameter of the forming channel 10, the amount of solder and other parameters are calculated and determined by those skilled in the art according to the specifications of the base material. Example 1

[0028] Combination Figure 1As shown, the shape of the micro-wire connection joint of the component is controlled by means of a welding tool. The welding tool includes a graphite piece 11 connected to the positive electrode of the welding power supply, and a graphite piece 2 12 connected to the negative electrode of the welding power supply. The graphite piece 11 and the graphite piece 2 12 are both provided with semicircular grooves. The two semicircular grooves can form a forming channel 10 for accommodating the wire 3. The diameter of the lower section of the forming channel 10 is equal to the outer diameter of the wire 3 (the lower section of the forming channel 10 is the height interval corresponding to the number 17 in the figure), and the upper section of the forming channel 10 is a funnel-shaped structure (the forming channel 10 The upper section is the height interval corresponding to the number 16 in the figure); a cooling support block 13 is arranged against the wall below the graphite part, and the through hole 14 on the cooling support block 13 is coaxially arranged with the forming channel 10, and the diameter of the through hole 14 is equal to the outer diameter of the wire 3; an actuator for vertically pulling the wire 3 downward is arranged below the cooling support block 13; a wire feeding mechanism, a feeding mechanism and a cutting mechanism 6 are arranged above the graphite part, and the wire feeding tube 8 of the wire feeding mechanism is coaxially arranged with the forming channel 10, and the feeding mechanism is used to add brazing material 7 and brazing agent into the forming channel 10. Among them, the inner diameter of the wire feeding tube 8 of the wire feeding mechanism is only 0.1~0.2mm larger than the diameter of the micro-wire, so as to ensure that the front section 9 of the micro-wire can be vertically fed downward into the forming channel 10; the cutting mechanism 6 is horizontally arranged on the side of the wire feeding tube 8, and when cutting is required, the tool of the cutting mechanism 6 is controlled to move to the target position directly below the wire feeding tube 8 for cutting; the actuator includes a screw lifting mechanism, and a clamp for clamping the wire 3 is provided on the lifting plate of the screw lifting mechanism. When the wire 3 needs to be pulled vertically downward, the clamp is first controlled to rise to the target height and clamp the wire 3, and then the clamp is controlled to move downward at a preset speed, thereby realizing the vertical pulling of the wire 3 at a preset speed.

[0029] A method for controlling the shape of a micro-wire pin connection joint of a component is used to control the shape of a connection joint between a plurality of nickel wires (a single wire diameter is about 20 μm) of a conductor and a silver pin (a micro-wire pin 1 has a diameter of about 0.2 mm), and the steps include:

[0030] S1, firstly, the insulation layer of the section to be welded of the wire 3 is stripped off to expose the multiple strands of wire 4, and then the multiple strands of wire 4 are adjusted to a divergent state (the divergent state of the multiple strands of wire 4 is as shown in FIG. Figure 1 The state of the wire 4 in the forming channel 10 in part b is shown, and this divergent state is similar to the funnel-shaped profile), and then the multiple strands of wire 4 and the fine wires are chemically cleaned and dried for use;

[0031] S2, put the wire 3 into the semicircular groove of the graphite piece 11 or the graphite piece 2 12, then close and fix the graphite piece 11 and the graphite piece 2 12, at which time the multi-strand wire 4 is located in the upper section of the forming channel 10, as shown in FIG. Figure 1 As shown in part b;

[0032] S3, controlling the wire feeding mechanism to operate, inserting the front section 9 of the microfilament vertically downward into the middle of the multi-strand wire 4, so that the front section 9 of the microfilament is substantially coaxial with the forming channel 10;

[0033] S4, controlling the feeding mechanism to operate, adding powdered solder 7 and flux into the forming channel 10, wherein the amount of flux added is no more than half of the volume of the upper section of the forming channel 10;

[0034] S5, cutting the micro-filament from the top of the forming channel 10, the micro-filament after cutting and located in the forming channel 10 is the micro-filament pin 1, and the state at this time is as follows Figure 1 b is not shown in the figure;

[0035] S6, heating the graphite part by means of a welding power source, so that the brazing material in the forming channel 10 melts and fills the gap;

[0036] S7, control the actuator to operate, pull the wire 3 vertically downward at a preset speed, and the speed of the wire 3 moving downward is controlled to be 1.2 mm / s. During this process, the multiple strands of wire 4 and the liquid solder are gradually gathered together. The posture of the unformed joint at a certain moment during the downward movement of the wire 3 is as follows Figure 1 As shown in part c, until a connection joint with a desired shape is formed;

[0037] In this step, when the upper end of the micro-filament pin 1 leaves the through hole 14, the actuator is controlled to pause, and the connection joint 18 obtained at this time is in a cylindrical shape, such as Figure 1 As shown in part d. Example 2

[0038] A second method for controlling the shape of a micro-wire pin connection joint of a component, the welding tool used refers to Figure 1 As shown, the connection joint posture of the multi-strand nickel wire (single wire diameter is about 30μm) and the silver pin (the diameter of the micro-wire pin 1 is about 0.1mm) used to control the conductor includes:

[0039] S1, firstly, the insulation layer of the section to be welded of the wire 3 is stripped off to expose the multiple strands of wire 4, and then the multiple strands of wire 4 are adjusted to a divergent state (the divergent state of the multiple strands of wire 4 is as shown in FIG. Figure 1 The state of the wire 4 in the forming channel 10 in part b is shown, and this divergent state is similar to the funnel-shaped profile), and then the multiple strands of wire 4 and the fine wires are chemically cleaned and dried for use;

[0040] S2, put the wire 3 into the semicircular groove of the graphite piece 11 or the graphite piece 2 12, then close and fix the graphite piece 11 and the graphite piece 2 12, at which time the multi-strand wire 4 is located in the upper section of the forming channel 10, as shown in FIG. Figure 1 As shown in part b;

[0041] S3, controlling the wire feeding mechanism to operate, inserting the front section 9 of the microfilament vertically downward into the middle of the multi-strand wire 4, so that the front section 9 of the microfilament is substantially coaxial with the forming channel 10;

[0042] S4, controlling the feeding mechanism to operate, adding powdered solder 7 and flux into the forming channel 10, wherein the amount of flux added is no more than half of the volume of the upper section of the forming channel 10;

[0043] S5, cutting the micro-filament from the top of the forming channel 10, the micro-filament after cutting and located in the forming channel 10 is the micro-filament pin 1, and the state at this time is as follows Figure 1 b is not shown in the figure;

[0044] S6, heating the graphite part by means of a welding power source, so that the brazing material in the forming channel 10 melts and fills the gap;

[0045] S7, controlling the actuator to operate, vertically pulling the wire 3 downward at a preset speed, and the speed of the wire 3 moving downward is controlled to be 2 mm / s. During this process, the multiple strands of wire 4 and the liquid solder are gradually gathered together until a connection joint of a desired shape is formed;

[0046] In this step, when the upper end of the micro-filament pin 1 is located in the middle and lower area of ​​the upper section of the forming channel 10, the actuator is controlled to pause, and the connection joint obtained at this time is in the form of a shuttle, such as Figure 2 shown. Example 3

[0047] A third method for controlling the morphology of a micro-wire pin connection joint of a component, referring to Example 1, the main difference between this method and Example 1 is that the micro-wire pin is a spiral, and the diameter of the spiral is not greater than 0.3 mm. This solution can further improve the connection strength of the connection joint, but its disadvantage compared to Example 1 is that it is not easy to insert the micro-wire pin into the middle area of ​​the multi-strand wire 4.

[0048] The microfilament connection joint obtained by adopting the scheme in the embodiment comprises a microfilament pin 1, wherein the microfilament pin 1 is welded with multiple strands of wire 4 of the conducting wire 3 through a solder body 2, the multiple strands of wire 4 of the conducting wire 3 are axially wrapped around the periphery of the microfilament pin 1, the axis of the microfilament pin 1 is substantially coincident with the axis of the conducting wire 3, and the non-gaps of the multiple strands of wire 4 themselves and the gaps between the multiple strands of wire 4 and the microfilament pin 1 are filled with the solder body 2; the multiple strands of wire 4 of the conducting wire 3 are embedded in the solder body 2 and cover the microfilament pin 1 in a "grasping" manner, and "grasping" means that the multiple strands of wire 4 located in the solder body 2 are in an expanded posture.

[0049] During the implementation, it is only necessary to control the vertical downward pulling of the wire 3 so that the roots of the multiple strands of wire 4 are at different height positions to obtain connection joints with different profiles. When the roots of the multiple strands of wire 4 are located below the through hole 14 and the upper end of the micro-wire pin 1 leaves the through hole 14, the connection joint 18 obtained is as follows Figure 1 The cylindrical shape shown in the middle d part, in this case, the connecting joint 18 is as thick as the conductor 3; when the root of the multi-strand wire 4 is at the initial position ( Figure 1 When the multiple wires 4 are at different heights below the initial position, the obtained connection joint 18 is in the shape of a shuttle, and the lower the multiple wires 4 are, the smaller the diameter and the longer the length of the obtained connection joint 18. Therefore, by controlling the vertical downward pulling of the wire 3, the shape and diameter of the connection joint 18 can be cleverly controlled.

[0050] In the present invention, in the process of vertically pulling down the wire 3, the inner wall of the forming channel 10 will give the multiple strands of wire 4 and the solder melt an extrusion force (the force received by the multiple strands of wire 4 during the process of contraction), so that the solder melt continues to immerse in the gaps between the multiple strands of wire 4 and part of the melt moves upward relative to the fine wire pin 1, and as the multiple strands of wire 4 move to the cooling support block 13, the solder melt will be quickly solidified and formed, thereby achieving welding and shaping of the connecting joint. During the welding process, the force of vertically pulling down the wire 3 mainly acts directly on the insulating layer of the wire 3, and the parent material (multiple strands of wire 4 and fine wire pin 1) will not be subjected to the welding pressure in the traditional brazing method, and the parent material will not become flat and is not easily damaged. The contraction is mainly achieved by the extrusion force received by the multiple strands of wire 4, which promotes the solder melt to flow in the gaps between the multiple strands of wire 4.

[0051] The present invention provides a brand-new component micro-filament pin connection joint, in which the multiple strands of wire are in a non-gathered state, which is essentially different from the structure of the traditional connection joint in which the micro-filament pin is biased to press the electrode end surface, and the micro-filament is covered in a "grabbing" manner and cooperates with the solder filling part to form a specific shuttle structure or column structure, which has the advantages of high connection strength and good stability; by adopting the scheme of the present invention, while ensuring that the solder fully infiltrates the gap of the base material, not only can the shape of the micro-filament connection joint be quickly and accurately controlled, but also the length of the micro-filament connection joint is convenient to accurately control, and the position of the protruding part of the joint can also be accurately controlled, and more importantly, the diameter of the micro-filament pin connection joint can be controlled to be consistent / the same as the diameter of the base material (conductor).

Claims

1. A method for controlling the morphology of a micro-filament connection joint of a component, characterized in that: The shape of the connection joint is controlled by means of a welding tool, the welding tool comprising a graphite piece (11) connected to the positive pole of a power source, and a graphite piece (12) connected to the negative pole of the power source, wherein both the graphite piece (11) and the graphite piece (12) are provided with semicircular grooves, and the two semicircular grooves can form a forming channel (10) for accommodating a wire (3), wherein the diameter of the lower section of the forming channel (10) is equal to the outer diameter of the wire (3), and the upper section of the forming channel (10) is in a funnel-shaped structure; a cooling support block (13) is provided on the wall below the graphite piece, and a through hole (14) on the cooling support block (13) is coaxially arranged with the forming channel (10), and the diameter of the through hole (14) is equal to the outer diameter of the wire (3); An actuator for vertically pulling down the wire (3) is provided below the cooling support block (13); a wire feeding mechanism, a feeding mechanism and a cutting mechanism (6) are provided above the graphite member, a wire feeding tube (8) of the wire feeding mechanism being coaxially arranged with the forming channel (10), and the feeding mechanism being used to add brazing material (7) and brazing flux into the forming channel (10); The steps of the morphology control method include: S1, firstly peel off the insulation layer of the section to be welded of the conductor (3) to expose the multiple strands of wire (4), then adjust the multiple strands of wire (4) to a divergent state, and then chemically clean and dry the multiple strands of wire (4) and the micro-wires for later use; S2, placing the wire (3) into the semicircular groove of the first graphite piece (11) or the second graphite piece (12), and then closing and fixing the first graphite piece (11) and the second graphite piece (12), at which time the multiple strands of wire (4) are located in the upper section of the forming channel (10); S3, controlling the operation of the wire feeding mechanism to vertically insert the front section of the micro-filament (9) into the middle of the multi-strand wire (4); S4, controlling the feeding mechanism to operate and adding powdered brazing material (7) and brazing flux into the forming channel (10); S5, cutting the microfilament from the top of the forming channel (10), and the microfilament located in the forming channel (10) after cutting is the microfilament pin (1); S6, heating the graphite part by applying electricity through a welding power source, so that the brazing material in the forming channel (10) melts and fills the gap; S7, controlling the actuator to operate and vertically pull the wire (3) downward at a preset speed. During this process, the multiple strands of wire (4) and the liquid solder are gradually gathered together until a connection joint of a desired shape is formed; The obtained connection joint comprises a microfilament pin (1), the microfilament pin (1) is welded to a plurality of strands of wire (4) of a conducting wire (3) through a solder body (2), the plurality of strands of wire (4) of the conducting wire (3) are axially wrapped around the periphery of the microfilament pin (1), the axis of the microfilament pin (1) and the axis of the conducting wire (3) are substantially coincident, and the plurality of strands of wire (4) themselves and the gaps between the plurality of strands of wire (4) and the microfilament pin (1) are filled with the solder body (2).

2. The morphology control method according to claim 1, characterized in that: In step S7, when the upper end of the micro-filament pin (1) leaves the through hole (14), the actuator is controlled to pause, and the connection joint obtained at this time is in a cylindrical shape.

3. The morphology control method according to claim 2, characterized in that: In step S7, when the upper end of the microfilament pin (1) is located in the middle and lower area of ​​the upper section of the forming channel (10), the actuator is controlled to pause, and the connection joint obtained at this time is in the form of a shuttle.

4. The morphology control method according to claim 2 or 3, characterized in that: The speed of the wire (3) moving downward is controlled to be 1-2 mm / s.

5. The morphology control method according to claim 4, characterized in that: In step S4, the amount of flux added is no more than half of the volume of the upper section of the forming channel (10).

6. The morphology control method according to claim 1, characterized in that: The connecting joint is in the form of a shuttle body with thin ends and a thick middle; or, the connecting joint is in the form of a cylindrical structure.

7. The morphology control method according to claim 1, characterized in that: The multiple strands of wire (4) of the conductor (3) are embedded in the solder body (2) and cover the fine wire pin (1) in a "grasping" manner. "Grasping" means that the multiple strands of wire (4) located in the solder body (2) are in an expanded posture.

8. The morphology control method according to claim 1, characterized in that: The micro-filament pin (1) is in the form of a flat body, a columnar body or a spiral body.

9. The morphology control method according to claim 1, characterized in that: The number of strands of the wire (4) of the conductor (3) is not less than 15, the diameter of the wire is not greater than 60 μm, and the diameter of the micro-wire pin (1) is not greater than 0.5 mm.