A process for purifying and concentrating waste sulfuric acid
By using treatment agents and adsorbents in waste sulfuric acid for ultrasonic oscillation and photoelectro-catalytic degradation, combined with pulsed magnetic field treatment, the problems of waste sulfuric acid purification and concentration are solved, and efficient resource recycling and environmental protection are achieved.
Patent Information
- Application Number
- CN202410824019.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-25
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-06-25
AI Technical Summary
The prior art is difficult to effectively purify and enrich waste sulfuric acid, resulting in waste of resources and environmental pollution, especially in the presence of organic impurities, which makes it difficult to meet the needs of industrial production.
Ultrasonic oscillation and photoelectric catalytic degradation under natural light conditions are used to perform ultrasonic oscillation and photoelectric catalytic degradation, combined with pulsed magnetic field treatment and pressurized filtration, and the treatment agent and adsorbent are prepared through hydrothermal reaction and aging treatment to achieve purification and concentration of waste sulfuric acid. .
It improves the concentration and quality of waste sulfuric acid, realizes the recycling and utilization of waste sulfuric acid, saves energy, is green and environmentally friendly, and meets industrial production standards.
Smart Images

Figure BDA0004909910680000111
Abstract
Description
Technical Field
[0001] The invention relates to a purification and concentration process of waste sulfuric acid, belonging to the technical field of industrial waste sulfuric acid reuse. Background Art
[0002] Sulfuric acid is an important industrial raw material and a binary inorganic strong acid that can react with most metals. Concentrated sulfuric acid has strong water absorption and can be used as a dehydrating agent. It has strong corrosiveness and oxidizing properties and is widely used in medicine, fertilizers, detergents, pigments, dyes, explosives, metal smelting and other fields.
[0003] Since the gas usually contains a small amount of methanol, methyl chloride, dimethyl ether, organic matter and other components, when concentrated sulfuric acid is used to dry the gas in industrial production, the organic matter in the gas is oxidized by sulfuric acid and dissolved in the sulfuric acid, making the waste sulfuric acid darker in color. This part of the organic matter dissolved in the acid cannot be separated by conventional methods, resulting in the waste sulfuric acid cannot be recycled, causing serious environmental pollution. In addition, the waste sulfuric acid produced after sulfuric acid treatment in industries such as metal smelting contains heavy metal ions in addition to organic matter. If it is discharged directly, the pollution situation is even more serious.
[0004] At present, waste sulfuric acid is usually treated by alkali neutralization or multiple-effect concentration. The alkali neutralization method has high operating costs, and the solid sulfate waste residue produced still pollutes the environment. The multiple-effect concentration method uses steam as a heat source to concentrate the waste sulfuric acid to a certain concentration for recycling. However, the organic matter contained in the waste sulfuric acid will directly affect the recycling process. The resulting product has low concentration and poor quality, and it is difficult to meet the reuse standard, which limits the recycling of waste sulfuric acid and causes a waste of resources.
[0005] Patent application CN104045063A discloses a method for treating a waste sulfuric acid solution, wherein the waste sulfuric acid solution contains sulfuric acid and ferrous sulfate, and the concentration of sulfuric acid in the waste sulfuric acid solution is not higher than 20% based on the total weight of the waste sulfuric acid solution. The method comprises removing the crystal water in the green vitriol and then calcining it, and first contacting the waste sulfuric acid solution with the waste sulfuric acid solution after the calcination until the sulfuric acid concentration in the waste sulfuric acid solution reaches 45-50%, and then performing solid-liquid separation on the waste sulfuric acid solution, and continuing to contact the obtained filtrate with the waste gas for a second time. The mass concentration of the sulfuric acid solution finally obtained in the patent application is 80%, which is not high enough and still difficult to meet the needs of industrial production. In addition, the method is not applicable to the presence of organic impurities, has a limited scope of application, and is difficult to promote and use on a large scale.
[0006] Patent CN102951617B discloses a waste sulfuric acid purification system and method, which heats the air and directly contacts the waste sulfuric acid, fully exchanges heat to make its temperature reach 150-200°C, and performs stripping treatment on the waste sulfuric acid, so that all volatile organic impurities, most soluble organic impurities, and some oligomers in the waste sulfuric acid are blown out, and the remaining organic impurities in the polymerized state generate a small amount of carbon and increase the molecular weight of the polymer to a solid state dispersed in the sulfuric acid, thereby achieving the purpose of purifying the waste sulfuric acid generated in the process of producing 1,4-butanediol. However, the sulfuric acid obtained by the patented technology has no obvious change in acid color from before treatment. The color of the waste sulfuric acid before treatment is brown, and the sulfuric acid after treatment is black, which does not meet the relevant standards. Summary of the invention
[0007] The purpose of the present invention is to overcome the above-mentioned deficiencies in the prior art and to provide a process for purifying and concentrating waste sulfuric acid.
[0008] To achieve the above object, the present invention adopts the following technical solutions:
[0009] A process for purifying and concentrating waste sulfuric acid, the specific steps are as follows:
[0010] (1) first adding a treatment agent to waste sulfuric acid, subjecting it to ultrasonic oscillation treatment under natural light conditions, filtering and collecting the filtrate to obtain pretreated sulfuric acid;
[0011] (2) using nitrogen-doped titanium dioxide as an anode, a graphite electrode as a cathode, and a saturated calomel electrode as a reference electrode, the pretreated sulfuric acid is subjected to photoelectrocatalytic degradation under natural light conditions, an adsorbent is added, the mixture is allowed to stand for adsorption, and the filtrate is filtered to obtain purified sulfuric acid;
[0012] (3) finally, the purified sulfuric acid and magnesium sulfate are mixed and stirred, treated with a pulse magnetic field, allowed to stand, and filtered under pressure to obtain a filtrate to obtain concentrated sulfuric acid;
[0013] The treating agent is prepared by the following method: cerium nitrate, zirconium oxynitrate, yttrium-doped molecular sieve, urea and deionized water are mixed evenly, subjected to hydrothermal reaction, filtered to obtain a solid, washed with water, dried, and calcined; the adsorbent is prepared by the following method: hydrogen-type zeolite is mixed with a binder, maleic anhydride grafted polyvinyl alcohol, and deionized water to form a mixture, dried, and subjected to aging treatment.
[0014] Preferably, when preparing the treating agent, the mass ratio of cerium nitrate, yttrium-doped molecular sieve and deionized water is 1:5-6:250-300, and the molar ratio of cerium nitrate, zirconium oxynitrate and urea is 3:2:5-6.
[0015] Preferably, when preparing the treating agent, the process conditions of the hydrothermal reaction are: hydrothermal reaction at 130-140° C. for 6-7 hours.
[0016] Preferably, when preparing the treating agent, the treating agent is washed with deionized water for 2 to 3 times; the drying process conditions are: drying at 70 to 80° C. for 4 to 5 hours; and the calcining process conditions are: calcining at 500 to 600° C. for 2 to 3 hours.
[0017] Preferably, when preparing the treating agent, the yttrium-doped molecular sieve is prepared by the following method, measured in parts by weight: first, 20 to 30 parts of 3-(N-anilino)propyltrimethoxysilane, 500 to 600 parts of sodium aluminate, 0.1 parts of yttrium nitrate, 0.75 parts of tetrapropylammonium bromide, 0.25 parts of hexamethylammonium bromide, 8 to 10 parts of polyethylene glycol 200, 0.2 to 0.3 parts of sodium hydroxide and 4500 to 5000 parts of deionized water are stirred and mixed, heated to 80 to 90° C., stirred and kept warm for 8 to 10 hours, transferred to a hydrothermal crystallization reactor, crystallized at 110 to 112° C. for 80 to 90 hours, filtered to obtain the solid, washed with water 2 to 3 times, dried at 70 to 80° C. for 8 to 10 hours, and calcined at 580 to 600° C. for 5 to 6 hours to obtain the yttrium-doped molecular sieve.
[0018] Preferably, when preparing the adsorbent, the hydrogen-type zeolite is HZSM-5 molecular sieve purchased from Zhuoran Environmental Protection Technology (Dalian) Co., Ltd., with a silicon-aluminum ratio of 350.
[0019] Preferably, when preparing the adsorbent, the maleic anhydride grafted polyvinyl alcohol is prepared by the following method: a dimethyl sulfoxide solution of polyvinyl alcohol with a mass concentration of 3 to 4% is added dropwise to a dimethyl sulfoxide solution of maleic anhydride with a mass concentration of 30 to 40%, the mixture is stirred at 50 to 60°C for 3 to 4 hours, naturally cooled to room temperature, filtered to obtain a precipitate, washed with acetone 2 to 3 times, and dried; wherein the mass ratio of polyvinyl alcohol to maleic anhydride is 1:2.5 to 3.5, and the relative molecular weight of polyvinyl alcohol is 25,000 to 35,000.
[0020] Preferably, when preparing the adsorbent, the mass ratio of hydrogen zeolite, binder, maleic anhydride grafted polyvinyl alcohol, and deionized water is 5-6:3-4:0.2-0.3:3-4; wherein the binder is selected from any one of bentonite, kaolin or montmorillonite.
[0021] Preferably, when preparing the adsorbent, the drying process conditions are: drying at 70-80° C. for 5-6 hours; and the aging process conditions are: aging at 90-100° C. for 6-8 hours.
[0022] Preferably, in step (1), the amount of the treating agent required per liter of waste sulfuric acid is 0.5 to 0.7 g.
[0023] Preferably, in step (1), the process conditions of ultrasonic oscillation treatment are: 300-400W ultrasonic oscillation treatment for 8-10 hours.
[0024] Preferably, in step (2), the nitrogen-doped titanium dioxide is prepared by the following method: tetrabutyl titanate and concentrated ammonia water with a mass concentration of 22-25% are mixed in a volume ratio of 1:9-10 and stirred for 2-3 hours, transferred to a reaction kettle, sealed at 185-195° C. for reaction for 30-34 hours, naturally cooled to room temperature, centrifuged to obtain a precipitate, washed with deionized water, 1 mol / L hydrochloric acid solution, and deionized water in sequence, dried at 70-80° C. for 6-7 hours, and dried to obtain the product.
[0025] Preferably, in step (2), an electrolyte is added before the photoelectrocatalytic degradation, and the process conditions of the photoelectrocatalytic degradation are: an external bias voltage of 1 to 1.2 V and a time of 3 to 4 hours.
[0026] Further preferably, the electrolyte is sodium sulfate, and the ratio of sodium sulfate to waste sulfuric acid is 1g:1L.
[0027] Preferably, in step (2), the amount of adsorbent required per liter of waste sulfuric acid is 6-7 g / L.
[0028] Preferably, in step (2), the static adsorption time is 20 to 22 hours.
[0029] Preferably, in step (3), the mass ratio of purified sulfuric acid to magnesium sulfate is 1:0.2-0.3.
[0030] Preferably, in step (3), the mixing and stirring process conditions are: 15000-20000 r / min stirring for 15-20 minutes.
[0031] Preferably, in step (3), the process conditions of the pulsed magnetic field treatment are: pulsed magnetic field intensity 3-4T, pulse width 100-120ms, pulse frequency 30-40Hz, and pulse number 15-20.
[0032] Preferably, in step (3), the standing time is 20 to 30 minutes.
[0033] Preferably, in step (3), the filtration pressure of the pressure filtration is 0.3-0.4 MPa.
[0034] Beneficial effects of the present invention:
[0035] The present invention first adds a treatment agent to waste sulfuric acid, performs ultrasonic oscillation treatment under natural light conditions, filters and collects filtrate to obtain pretreated sulfuric acid; then uses nitrogen-doped titanium dioxide as an anode, a graphite electrode as a cathode, and a saturated calomel electrode as a reference electrode to perform photoelectrocatalytic degradation of the pretreated sulfuric acid under natural light conditions, adds an adsorbent, allows to stand for adsorption, and filters and collects filtrate to obtain purified sulfuric acid; then, the purified sulfuric acid is mixed and stirred with magnesium sulfate, subjected to pulse magnetic field treatment, allowed to stand, and filtered under pressure to collect filtrate to obtain concentrated sulfuric acid. The concentrated sulfuric acid obtained by the present invention has high concentration and good quality, and realizes the recycling of waste sulfuric acid.
[0036] The treatment agent is prepared by the following method: cerium nitrate, zirconium oxynitrate, yttrium-doped molecular sieve, urea and deionized water are uniformly mixed, hydrothermally reacted, filtered to obtain a solid, washed with water, dried, and roasted. The treatment agent of the present invention can achieve the degradation of impurities such as organic matter in waste sulfuric acid. Combined with subsequent photoelectric catalytic degradation, the remaining impurities are further degraded to promote the purification of waste sulfuric acid.
[0037] The adsorbent is prepared by the following method: firstly, sodium silicate and aluminum nitrate are used as raw materials to prepare hydrogen zeolite, and then the hydrogen zeolite is mixed with a binder, maleic anhydride grafted polyvinyl alcohol, and deionized water to form, dry, and age. The adsorbent can have a good adsorption effect under the action of strong acid, adsorb small molecular impurities and heavy metals, etc., to fully purify waste sulfuric acid and improve the quality of sulfuric acid.
[0038] The present invention does not use a multi-effect concentration method for concentration, but uses the water absorption effect of magnesium sulfate, combined with pulse magnetic field treatment and pressure filtration, to achieve full dehydration and increase the sulfuric acid concentration of the product. The concentration step of the present invention saves energy and is green and environmentally friendly. DETAILED DESCRIPTION
[0039] The present invention is further described below in conjunction with embodiments. It should be noted that the following description is only for explaining the present invention and does not limit its contents.
[0040] Embodiment 1:
[0041] A process for purifying and concentrating waste sulfuric acid, the specific steps are as follows:
[0042] (1) first adding a treatment agent to waste sulfuric acid, subjecting it to ultrasonic oscillation treatment under natural light conditions, filtering and collecting the filtrate to obtain pretreated sulfuric acid;
[0043] The amount of treatment agent required for each liter of waste sulfuric acid is 0.5g.
[0044] The process conditions of the ultrasonic oscillation treatment are: 300W ultrasonic oscillation treatment for 8 hours.
[0045] (2) using nitrogen-doped titanium dioxide as an anode, a graphite electrode as a cathode, and a saturated calomel electrode as a reference electrode, the pretreated sulfuric acid is subjected to photoelectrocatalytic degradation under natural light conditions, an adsorbent is added, the mixture is allowed to stand for adsorption, and the filtrate is filtered to obtain purified sulfuric acid;
[0046] The nitrogen-doped titanium dioxide is prepared by the following method: tetrabutyl titanate and concentrated ammonia water with a mass concentration of 22% are mixed in a volume ratio of 1:9 and stirred for 2 hours, transferred to a reactor, sealed and reacted at 185° C. for 30 hours, naturally cooled to room temperature, centrifuged to obtain a precipitate, washed with deionized water, 1 mol / L hydrochloric acid solution, and deionized water in sequence, and dried at 70° C. for 6 hours.
[0047] Electrolyte is added before photoelectrocatalytic degradation, and the process conditions of photoelectrocatalytic degradation are: external bias voltage 1V, time 3 hours. The electrolyte is sodium sulfate, and the ratio of sodium sulfate to waste sulfuric acid is 1g:1L.
[0048] The amount of adsorbent required per liter of waste sulfuric acid is 6 g / L.
[0049] The static adsorption time is 20 hours.
[0050] (3) Finally, the purified sulfuric acid and magnesium sulfate are mixed and stirred, treated with a pulse magnetic field, allowed to stand, and filtered under pressure to obtain the filtrate to obtain concentrated sulfuric acid.
[0051] The mass ratio of purified sulfuric acid to magnesium sulfate is 1:0.2.
[0052] The process conditions for mixing and stirring are: stirring at 15000r / min for 15 minutes.
[0053] The process conditions of the pulse magnetic field treatment are: pulse magnetic field intensity 3T, pulse width 100ms, pulse frequency 30Hz, and 15 pulses.
[0054] The standing time is 20 minutes.
[0055] The filtration pressure of pressure filtration is 0.3MPa.
[0056] The treating agent is prepared by the following method: cerium nitrate, zirconium oxynitrate, yttrium-doped molecular sieve, urea and deionized water are mixed evenly, subjected to hydrothermal reaction, filtered to obtain a solid, washed twice with deionized water, dried at 70°C for 4 hours, and calcined at 500°C for 2 hours.
[0057] The mass ratio of cerium nitrate, yttrium-doped molecular sieve and deionized water is 1:5:250, and the molar ratio of cerium nitrate, zirconium oxynitrate and urea is 3:2:5. The process conditions of the hydrothermal reaction are: hydrothermal reaction at 130°C for 6 hours. The yttrium-doped molecular sieve is prepared by the following method: first, 2kg 3-(N-anilino)propyltrimethoxysilane, 50kg sodium aluminate, 0.01kg yttrium nitrate, 0.075kg tetrapropylammonium bromide, 0.025kg hexamethylammonium bromide, 0.8kg polyethylene glycol 200, 0.02kg sodium hydroxide and 450kg deionized water are stirred and mixed, heated to 80°C, stirred for 8 hours, transferred to a hydrothermal crystallization reactor, crystallized at 110°C for 80 hours, filtered to obtain the solid, washed with water twice, dried at 70°C for 8 hours, and calcined at 580°C for 5 hours to obtain the yttrium-doped molecular sieve.
[0058] The adsorbent is prepared by the following method: hydrogen zeolite is mixed with a binder (bentonite), maleic anhydride grafted polyvinyl alcohol, and deionized water in a mass ratio of 5:3:0.2:3, dried at 70°C for 5 hours, and aged at 90°C for 6 hours. The hydrogen zeolite is HZSM-5 molecular sieve purchased from Zhuoran Environmental Protection Technology (Dalian) Co., Ltd., with a silicon-aluminum ratio of 350. The maleic anhydride grafted polyvinyl alcohol is prepared by the following method: a dimethyl sulfoxide solution of 3% polyvinyl alcohol by mass concentration is added dropwise to a dimethyl sulfoxide solution of 30% maleic anhydride by mass concentration, stirred at 50°C for 3 hours, cooled naturally to room temperature, filtered to obtain a precipitate, washed twice with acetone, and dried; wherein the mass ratio of polyvinyl alcohol to maleic anhydride is 1:2.5, and the relative molecular weight of polyvinyl alcohol is 30,000.
[0059] Embodiment 2:
[0060] A process for purifying and concentrating waste sulfuric acid, the specific steps are as follows:
[0061] (1) first adding a treatment agent to waste sulfuric acid, subjecting it to ultrasonic oscillation treatment under natural light conditions, filtering and collecting the filtrate to obtain pretreated sulfuric acid;
[0062] The amount of treatment agent required per liter of waste sulfuric acid is 0.7g.
[0063] The process conditions of the ultrasonic oscillation treatment are: 400W ultrasonic oscillation treatment for 10 hours.
[0064] (2) using nitrogen-doped titanium dioxide as an anode, a graphite electrode as a cathode, and a saturated calomel electrode as a reference electrode, the pretreated sulfuric acid is subjected to photoelectrocatalytic degradation under natural light conditions, an adsorbent is added, the mixture is allowed to stand for adsorption, and the filtrate is filtered to obtain purified sulfuric acid;
[0065] The nitrogen-doped titanium dioxide is prepared by the following method: tetrabutyl titanate and concentrated ammonia water with a mass concentration of 25% are mixed and stirred at a volume ratio of 1:10 for 3 hours, transferred to a reactor, sealed and reacted at 195°C for 34 hours, naturally cooled to room temperature, centrifuged to obtain a precipitate, washed with deionized water, 1 mol / L hydrochloric acid solution, and deionized water in sequence, dried at 80°C for 7 hours, and obtained by drying.
[0066] Electrolyte is added before photoelectrocatalytic degradation, and the process conditions of photoelectrocatalytic degradation are: external bias voltage 1.2V, time 4 hours. The electrolyte is sodium sulfate, and the ratio of sodium sulfate to waste sulfuric acid is 1g:1L.
[0067] The amount of adsorbent required per liter of waste sulfuric acid is 7g / L.
[0068] The static adsorption time is 22 hours.
[0069] (3) Finally, the purified sulfuric acid and magnesium sulfate are mixed and stirred, treated with a pulse magnetic field, allowed to stand, and filtered under pressure to obtain the filtrate to obtain concentrated sulfuric acid.
[0070] The mass ratio of purified sulfuric acid to magnesium sulfate is 1:0.3.
[0071] The process conditions for mixing and stirring are: stirring at 20000r / min for 20 minutes.
[0072] The process conditions of the pulse magnetic field treatment are: pulse magnetic field intensity 4T, pulse width 120ms, pulse frequency 40Hz, and 20 pulses.
[0073] The standing time is 30 minutes.
[0074] The filtration pressure of pressure filtration is 0.4MPa.
[0075] The treating agent is prepared by the following method: cerium nitrate, zirconium oxynitrate, yttrium-doped molecular sieve, urea and deionized water are mixed evenly, subjected to hydrothermal reaction, filtered to obtain a solid, washed with deionized water for 3 times, dried at 80°C for 5 hours, and calcined at 600°C for 3 hours.
[0076] The mass ratio of cerium nitrate, yttrium-doped molecular sieve and deionized water is 1:6:300, and the molar ratio of cerium nitrate, zirconium oxynitrate and urea is 3:2:6. The process conditions of the hydrothermal reaction are: hydrothermal reaction at 140°C for 7 hours. The yttrium-doped molecular sieve is prepared by the following method: first, 3kg 3-(N-anilino)propyltrimethoxysilane, 60kg sodium aluminate, 0.01kg yttrium nitrate, 0.075kg tetrapropylammonium bromide, 0.025kg hexamethylammonium bromide, 1kg polyethylene glycol 200, 0.03kg sodium hydroxide and 500kg deionized water are stirred and mixed, heated to 90°C, stirred for 10 hours, transferred to a hydrothermal crystallization reactor, crystallized at 112°C for 90 hours, filtered to obtain the solid, washed with water 3 times, dried at 80°C for 10 hours, and calcined at 600°C for 6 hours to obtain the yttrium-doped molecular sieve.
[0077] The adsorbent is prepared by the following method: hydrogen zeolite is mixed with a binder (kaolin), maleic anhydride grafted polyvinyl alcohol, and deionized water in a mass ratio of 6:4:0.3:4, dried at 80°C for 6 hours, and aged at 100°C for 8 hours. The hydrogen zeolite is HZSM-5 molecular sieve purchased from Zhuoran Environmental Protection Technology (Dalian) Co., Ltd., with a silicon-aluminum ratio of 350. The maleic anhydride grafted polyvinyl alcohol is prepared by the following method: a dimethyl sulfoxide solution of 4% polyvinyl alcohol by mass concentration is added dropwise to a dimethyl sulfoxide solution of 40% maleic anhydride by mass concentration, stirred at 60°C for 4 hours, cooled naturally to room temperature, filtered to obtain a precipitate, washed with acetone 3 times, and dried; wherein the mass ratio of polyvinyl alcohol to maleic anhydride is 1:3.5, and the relative molecular weight of polyvinyl alcohol is 30,000.
[0078] Embodiment 3:
[0079] A process for purifying and concentrating waste sulfuric acid, the specific steps are as follows:
[0080] (1) first adding a treatment agent to waste sulfuric acid, subjecting it to ultrasonic oscillation treatment under natural light conditions, filtering and collecting the filtrate to obtain pretreated sulfuric acid;
[0081] The amount of treatment agent required per liter of waste sulfuric acid is 0.6g.
[0082] The process conditions of the ultrasonic oscillation treatment are: 400W ultrasonic oscillation treatment for 9 hours.
[0083] (2) using nitrogen-doped titanium dioxide as an anode, a graphite electrode as a cathode, and a saturated calomel electrode as a reference electrode, the pretreated sulfuric acid is subjected to photoelectrocatalytic degradation under natural light conditions, an adsorbent is added, the mixture is allowed to stand for adsorption, and the filtrate is filtered to obtain purified sulfuric acid;
[0084] The nitrogen-doped titanium dioxide is prepared by the following method: tetrabutyl titanate and concentrated ammonia water with a mass concentration of 23 are mixed and stirred at a volume ratio of 1:9.5 for 2.5 hours, transferred to a reactor, sealed and reacted at 190° C. for 32 hours, naturally cooled to room temperature, centrifuged to obtain a precipitate, washed with deionized water, 1 mol / L hydrochloric acid solution, and deionized water in sequence, dried at 75° C. for 6.5 hours, and obtained by drying.
[0085] Electrolyte is added before photoelectrocatalytic degradation, and the process conditions of photoelectrocatalytic degradation are: external bias voltage 1.1V, time 3.5 hours. The electrolyte is sodium sulfate, and the ratio of sodium sulfate to waste sulfuric acid is 1g:1L.
[0086] The amount of adsorbent required per liter of waste sulfuric acid is 6.5 g / L.
[0087] The static adsorption time is 21 hours.
[0088] (3) Finally, the purified sulfuric acid and magnesium sulfate are mixed and stirred, treated with a pulse magnetic field, allowed to stand, and filtered under pressure to obtain the filtrate to obtain concentrated sulfuric acid.
[0089] The mass ratio of purified sulfuric acid to magnesium sulfate is 1:0.25.
[0090] The process conditions for mixing and stirring are: stirring at 18000r / min for 18 minutes.
[0091] The process conditions of the pulsed magnetic field treatment are: pulsed magnetic field intensity 3T, pulse width 110ms, pulse frequency 30Hz, and 18 pulses.
[0092] The resting time is 25 minutes.
[0093] The filtration pressure of pressure filtration is 0.4MPa.
[0094] The treating agent is prepared by the following method: cerium nitrate, zirconium oxynitrate, yttrium-doped molecular sieve, urea and deionized water are mixed evenly, subjected to hydrothermal reaction, filtered to obtain a solid, washed with deionized water for 3 times, dried at 75°C for 4.5 hours, and calcined at 550°C for 3 hours.
[0095] The mass ratio of cerium nitrate, yttrium-doped molecular sieve and deionized water is 1:5.5:280, and the molar ratio of cerium nitrate, zirconium oxynitrate and urea is 3:2:5.5. The process conditions of the hydrothermal reaction are: 135°C hydrothermal reaction for 6.5 hours. The yttrium-doped molecular sieve is prepared by the following method: first, 2.5 kg of 3-(N-anilino)propyltrimethoxysilane, 55 kg of sodium aluminate, 0.01 kg of yttrium nitrate, 0.075 kg of tetrapropylammonium bromide, 0.025 kg of hexamethylammonium bromide, 0.9 kg of polyethylene glycol 200, 0.02 kg of sodium hydroxide and 480 kg of deionized water are stirred and mixed, heated to 85° C., stirred and kept warm for 9 hours, transferred to a hydrothermal crystallization reactor, crystallized at 111° C. for 85 hours, filtered and solid was collected, washed with water 3 times, dried at 75° C. for 9 hours, and calcined at 590° C. for 6 hours to obtain the yttrium-doped molecular sieve.
[0096] The adsorbent is prepared by the following method: hydrogen zeolite is mixed with a binder (montmorillonite), maleic anhydride grafted polyvinyl alcohol, and deionized water in a mass ratio of 5.5:3.5:0.25:3.5, dried at 75°C for 5.5 hours, and aged at 95°C for 7 hours. The hydrogen zeolite is HZSM-5 molecular sieve purchased from Zhuoran Environmental Protection Technology (Dalian) Co., Ltd., with a silicon-aluminum ratio of 350. The maleic anhydride grafted polyvinyl alcohol is prepared by the following method: a dimethyl sulfoxide solution of polyvinyl alcohol with a mass concentration of 3.5% is added dropwise to a dimethyl sulfoxide solution of maleic anhydride with a mass concentration of 35%, stirred at 55°C for 3.5 hours, cooled naturally to room temperature, filtered to obtain a precipitate, washed with acetone 3 times, and dried; wherein the mass ratio of polyvinyl alcohol to maleic anhydride is 1:3, and the relative molecular weight of polyvinyl alcohol is 30,000.
[0097] Comparative Example 1
[0098] A process for purifying and concentrating waste sulfuric acid, the specific steps are as follows:
[0099] (1) firstly, using nitrogen-doped titanium dioxide as an anode, a graphite electrode as a cathode, and a saturated calomel electrode as a reference electrode, photoelectrocatalytically degrading waste sulfuric acid under natural light conditions, adding an adsorbent, standing for adsorption, filtering and collecting the filtrate to obtain purified sulfuric acid;
[0100] The nitrogen-doped titanium dioxide is prepared by the following method: tetrabutyl titanate and concentrated ammonia water with a mass concentration of 22% are mixed in a volume ratio of 1:9 and stirred for 2 hours, transferred to a reactor, sealed and reacted at 185° C. for 30 hours, naturally cooled to room temperature, centrifuged to obtain a precipitate, washed with deionized water, 1 mol / L hydrochloric acid solution, and deionized water in sequence, and dried at 70° C. for 6 hours.
[0101] Electrolyte is added before photoelectrocatalytic degradation, and the process conditions of photoelectrocatalytic degradation are: external bias voltage 1V, time 3 hours. The electrolyte is sodium sulfate, and the ratio of sodium sulfate to waste sulfuric acid is 1g:1L.
[0102] The amount of adsorbent required per liter of waste sulfuric acid is 6 g / L.
[0103] The static adsorption time is 20 hours.
[0104] (2) The purified sulfuric acid and magnesium sulfate are then mixed and stirred, treated with a pulse magnetic field, allowed to stand, and filtered under pressure to obtain a filtrate to obtain concentrated sulfuric acid.
[0105] The mass ratio of purified sulfuric acid to magnesium sulfate is 1:0.2.
[0106] The process conditions for mixing and stirring are: stirring at 15000r / min for 15 minutes.
[0107] The process conditions of the pulse magnetic field treatment are: pulse magnetic field intensity 3T, pulse width 100ms, pulse frequency 30Hz, and 15 pulses.
[0108] The standing time is 20 minutes.
[0109] The filtration pressure of pressure filtration is 0.3MPa.
[0110] The adsorbent is prepared by the following method: hydrogen zeolite is mixed with a binder (bentonite), maleic anhydride grafted polyvinyl alcohol, and deionized water in a mass ratio of 5:3:0.2:3, dried at 70°C for 5 hours, and aged at 90°C for 6 hours. The hydrogen zeolite is HZSM-5 molecular sieve purchased from Zhuoran Environmental Protection Technology (Dalian) Co., Ltd., with a silicon-aluminum ratio of 350. The maleic anhydride grafted polyvinyl alcohol is prepared by the following method: a dimethyl sulfoxide solution of 3% polyvinyl alcohol by mass concentration is added dropwise to a dimethyl sulfoxide solution of 30% maleic anhydride by mass concentration, stirred at 50°C for 3 hours, cooled naturally to room temperature, filtered to obtain a precipitate, washed twice with acetone, and dried; wherein the mass ratio of polyvinyl alcohol to maleic anhydride is 1:2.5, and the relative molecular weight of polyvinyl alcohol is 30,000.
[0111] Comparative Example 2
[0112] A process for purifying and concentrating waste sulfuric acid, the specific steps are as follows:
[0113] (1) first adding a treatment agent to waste sulfuric acid, subjecting it to ultrasonic oscillation treatment under natural light conditions, filtering and collecting the filtrate to obtain pretreated sulfuric acid;
[0114] The amount of treatment agent required for each liter of waste sulfuric acid is 0.5g.
[0115] The process conditions of the ultrasonic oscillation treatment are: 300W ultrasonic oscillation treatment for 8 hours.
[0116] (2) using nitrogen-doped titanium dioxide as an anode, a graphite electrode as a cathode, and a saturated calomel electrode as a reference electrode, the pretreated sulfuric acid is subjected to photoelectrocatalytic degradation under natural light conditions, an adsorbent is added, the mixture is allowed to stand for adsorption, and the filtrate is filtered to obtain purified sulfuric acid;
[0117] The nitrogen-doped titanium dioxide is prepared by the following method: tetrabutyl titanate and concentrated ammonia water with a mass concentration of 22% are mixed in a volume ratio of 1:9 and stirred for 2 hours, transferred to a reactor, sealed and reacted at 185° C. for 30 hours, naturally cooled to room temperature, centrifuged to obtain a precipitate, washed with deionized water, 1 mol / L hydrochloric acid solution, and deionized water in sequence, and dried at 70° C. for 6 hours.
[0118] Electrolyte is added before photoelectrocatalytic degradation, and the process conditions of photoelectrocatalytic degradation are: external bias voltage 1V, time 3 hours. The electrolyte is sodium sulfate, and the ratio of sodium sulfate to waste sulfuric acid is 1g:1L.
[0119] The amount of adsorbent required per liter of waste sulfuric acid is 6 g / L.
[0120] The static adsorption time is 20 hours.
[0121] (3) Finally, the purified sulfuric acid and magnesium sulfate are mixed and stirred, allowed to stand, and the filtrate is filtered under pressure to obtain concentrated sulfuric acid.
[0122] The mass ratio of purified sulfuric acid to magnesium sulfate is 1:0.2.
[0123] The process conditions for mixing and stirring are: stirring at 15000r / min for 15 minutes.
[0124] The standing time is 20 minutes.
[0125] The filtration pressure of pressure filtration is 0.3MPa.
[0126] The treating agent is prepared by the following method: cerium nitrate, zirconium oxynitrate, yttrium-doped molecular sieve, urea and deionized water are mixed evenly, subjected to hydrothermal reaction, filtered to obtain a solid, washed twice with deionized water, dried at 70°C for 4 hours, and calcined at 500°C for 2 hours.
[0127] The mass ratio of cerium nitrate, yttrium-doped molecular sieve and deionized water is 1:5:250, and the molar ratio of cerium nitrate, zirconium oxynitrate and urea is 3:2:5. The process conditions of the hydrothermal reaction are: hydrothermal reaction at 130°C for 6 hours. The yttrium-doped molecular sieve is prepared by the following method: first, 2kg 3-(N-anilino)propyltrimethoxysilane, 50kg sodium aluminate, 0.01kg yttrium nitrate, 0.075kg tetrapropylammonium bromide, 0.025kg hexamethylammonium bromide, 0.8kg polyethylene glycol 200, 0.02kg sodium hydroxide and 450kg deionized water are stirred and mixed, heated to 80°C, stirred for 8 hours, transferred to a hydrothermal crystallization reactor, crystallized at 110°C for 80 hours, filtered to obtain the solid, washed with water twice, dried at 70°C for 8 hours, and calcined at 580°C for 5 hours to obtain the yttrium-doped molecular sieve.
[0128] The adsorbent is prepared by the following method: hydrogen zeolite is mixed with a binder (bentonite), maleic anhydride grafted polyvinyl alcohol, and deionized water in a mass ratio of 5:3:0.2:3, dried at 70°C for 5 hours, and aged at 90°C for 6 hours. The hydrogen zeolite is HZSM-5 molecular sieve purchased from Zhuoran Environmental Protection Technology (Dalian) Co., Ltd., with a silicon-aluminum ratio of 350. The maleic anhydride grafted polyvinyl alcohol is prepared by the following method: a dimethyl sulfoxide solution of 3% polyvinyl alcohol by mass concentration is added dropwise to a dimethyl sulfoxide solution of 30% maleic anhydride by mass concentration, stirred at 50°C for 3 hours, cooled naturally to room temperature, filtered to obtain a precipitate, washed twice with acetone, and dried; wherein the mass ratio of polyvinyl alcohol to maleic anhydride is 1:2.5, and the relative molecular weight of polyvinyl alcohol is 30,000.
[0129] Test example
[0130] For the sake of comparison, the waste sulfuric acid in Examples 1 to 3 and Comparative Examples 1 and 2 all come from a smelter.
[0131] With reference to GB / T534-2014 "Industrial Sulfuric Acid", the concentrated sulfuric acid obtained in Examples 1 to 3 and Comparative Examples 1 and 2 was subjected to relevant tests, including: sulfuric acid mass fraction, ash mass fraction, heavy metal mass fraction, transparency, chromaticity, etc. The results are shown in Table 1.
[0132] Table 1. Test results of various indicators of concentrated sulfuric acid
[0133]
[0134] As can be seen from Table 1, the concentrated sulfuric acid obtained in Examples 1 to 3 has a high concentration, low ash and heavy metal content, high transparency, and is not darker than the standard color, indicating that the concentrated sulfuric acid is of high quality.
[0135] In comparative example 1, the treatment step of the treatment agent is omitted, and the quality of the concentrated sulfuric acid is significantly deteriorated and the concentration is also reduced; in comparative example 2, the pulse magnetic field treatment is omitted during the concentration, and the concentration is significantly reduced. This shows that the treatment agent treatment, photoelectrocatalytic degradation and adsorption steps of the present invention work synergistically to achieve a better purification effect, and the purification effect will also affect the concentration of the product; in the concentration step, the pulse magnetic field treatment is beneficial to improve the dehydration effect and increase the concentration of concentrated sulfuric acid.
[0136] Although the above describes the specific implementation methods of the present invention, it does not limit the scope of protection of the present invention. Based on the technical solution of the present invention, various modifications or variations that can be made by those skilled in the art without creative work are still within the scope of protection of the present invention.
Claims
1. A process for purifying and concentrating waste sulfuric acid, It is characterized in that The specific steps are as follows: (1) first adding a treatment agent to waste sulfuric acid, subjecting it to ultrasonic oscillation treatment under natural light conditions, filtering and collecting the filtrate to obtain pretreated sulfuric acid; (2) using nitrogen-doped titanium dioxide as an anode, a graphite electrode as a cathode, and a saturated calomel electrode as a reference electrode, the pretreated sulfuric acid is subjected to photoelectrocatalytic degradation under natural light conditions, an adsorbent is added, the mixture is allowed to stand for adsorption, and the filtrate is filtered to obtain purified sulfuric acid; (3) finally, the purified sulfuric acid and magnesium sulfate are mixed and stirred, treated with a pulse magnetic field, allowed to stand, and filtered under pressure to obtain a filtrate to obtain concentrated sulfuric acid; The treating agent is prepared by the following method: cerium nitrate, zirconium oxynitrate, yttrium-doped molecular sieve, urea and deionized water are uniformly mixed, hydrothermally reacted, filtered to obtain a solid, washed with water, dried, and roasted; the adsorbent is prepared by the following method: hydrogen-type zeolite is mixed with a binder, maleic anhydride grafted polyvinyl alcohol, and deionized water to form a mixture, dried, and aged; When preparing the treating agent, the mass ratio of cerium nitrate, yttrium-doped molecular sieve and deionized water is 1:5-6:250-300, and the molar ratio of cerium nitrate, zirconium oxynitrate and urea is 3:2:5-6; the process conditions of hydrothermal reaction are: hydrothermal reaction at 130-140°C for 6-7 hours; washing with deionized water 2-3 times; drying process conditions are: drying at 70-80°C for 4-5 hours; roasting process conditions are: roasting at 500-600°C for 2-3 hours; in parts by weight, the yttrium-doped molecular sieve is prepared by the following method: firstly, 20-30 parts of 3-(N-anilino)propane 1-Hydroxytrimethoxysilane, 500-600 parts of sodium aluminate, 0.1 parts of yttrium nitrate, 0.75 parts of tetrapropylammonium bromide, 0.25 parts of hexamethylammonium bromide, 8-10 parts of polyethylene glycol 200, 0.2-0.3 parts of sodium hydroxide and 4500-5000 parts of deionized water are stirred and mixed, heated to 80-90°C, stirred for 8-10 hours, transferred to a hydrothermal crystallization reactor, crystallized at 110-112°C for 80-90 hours, filtered to obtain a solid, washed with water 2-3 times, dried at 70-80°C for 8-10 hours, and calcined at 580-600°C for 5-6 hours to obtain a yttrium-doped molecular sieve; When preparing the adsorbent, the hydrogen-type zeolite is HZSM-5 molecular sieve; the maleic anhydride grafted polyvinyl alcohol is prepared by the following method: a dimethyl sulfoxide solution of polyvinyl alcohol with a mass concentration of 3-4% is added dropwise to a dimethyl sulfoxide solution of maleic anhydride with a mass concentration of 30-40%, stirred at 50-60°C for 3-4 hours, cooled naturally to room temperature, filtered to obtain a precipitate, washed with acetone 2-3 times, and dried to obtain the adsorbent; wherein the mass ratio of polyvinyl alcohol to maleic anhydride is 1:2.5-3.5, and the relative molecular weight of polyvinyl alcohol is 25,000-35,000; the mass ratio of hydrogen-type zeolite, binder, maleic anhydride grafted polyvinyl alcohol, and deionized water is 5-6:3-4:0.2-0.3:3-4; wherein the binder is selected from any one of bentonite, kaolin or montmorillonite; the drying process conditions are: drying at 70-80°C for 5-6 hours; the aging process conditions are: aging at 90-100°C for 6-8 hours; In step (3), the process conditions of the pulsed magnetic field treatment are: pulsed magnetic field intensity 3-4T, pulse width 100-120ms, pulse frequency 30-40Hz, and pulse number 15-20.
2. A process for purifying and concentrating waste sulfuric acid according to claim 1, It is characterized in that In step (1), the amount of treatment agent required per liter of waste sulfuric acid is 0.5 to 0.7 g; The process conditions of ultrasonic oscillation treatment are: 300-400W ultrasonic oscillation treatment for 8-10 hours.
3. A process for purifying and concentrating waste sulfuric acid according to claim 1, It is characterized in that In step (2), an electrolyte is added before the photoelectrocatalytic degradation. The process conditions of the photoelectrocatalytic degradation are: an external bias voltage of 1 to 1.2 V and a time of 3 to 4 hours.
4. A process for purifying and concentrating waste sulfuric acid according to claim 1, It is characterized in that In step (2), the amount of adsorbent required per liter of waste sulfuric acid is 6 to 7 g / L; The static adsorption time is 20 to 22 hours.
5. A process for purifying and concentrating waste sulfuric acid according to claim 1, It is characterized in that In step (3), the mass ratio of purified sulfuric acid to magnesium sulfate is 1:0.2-0.3; The process conditions for mixing and stirring are: stirring at 15000-20000 r / min for 15-20 minutes; The standing time is 20 to 30 minutes; The filtration pressure of pressure filtration is 0.3~0.4MPa.
Citation Information
Patent Citations
A waste sulfuric acid purification and treatment system and method
CN102951617B
Waste sulfuric acid solution treatment method
CN104045063A
Indoor air purification composite photocatalyst filter membrane and preparation method thereof
CN109364916A
Waste sulfuric acid recovery treatment method
CN114715856A
Recycling treatment method of waste sulfuric acid
CN115784171A