A method and device for repairing cracks in shield segments

By setting seals on the front and back of the shield segments to create a pressure difference, the repair material seeps out and fills the cracks, solving the problems of poor waterproofing and secondary damage in the existing technology and achieving efficient crack repair effects.

CN118582227BActive Publication Date: 2024-10-11JINAN RAILWAY SEGMENT MFG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411037222.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-10-11
Estimated Expiration
2044-07-31

AI Technical Summary

Technical Problem

The existing shield segment crack repair methods have problems such as poor waterproofing effect, secondary damage caused by drilling holes, and difficulty in fully filling the cracks with repair materials.

Method used

The through-crack repair method is adopted. By setting seals on the front and back of the shield segment, a pressure difference is formed to allow the repair material to seep out and fill the crack, avoiding drilling holes, ensuring that the repair material is fully filled and improving compactness.

Benefits of technology

It effectively makes up for the waterproofing deficiency of the surface sealing method, avoids secondary damage, ensures that the repair material fully fills the cracks, and improves the repair effect and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118582227B_ABST
    Figure CN118582227B_ABST
Patent Text Reader

Abstract

The present application provides a method and device for repairing cracks through shield segments, which belongs to the field of shield segment repair. The repair method includes: step 1, determining the position of the cracks through the shield segment; step 2, forming a front sealing cavity on the front of the shield segment and a back sealing cavity on the back; step 3, injecting repair material into the front sealing cavity to form a pressure difference between the front sealing cavity and the back sealing cavity; step 4, when the repair material changes to a non-flowing and plastic state, removing the seal and scraping off the excess repair material. The repair device includes two clamping plates, the two clamping plates are arranged on the two axial butt joint sides of the shield segment to clamp the shield segment, two tightening plates are located on the front and back of the shield segment, and two sealing plates are located on the front and back of the shield segment to form a sealed cavity and are fixed by two tightening fixing components respectively. The above scheme not only avoids secondary damage to the segment, but also has a better repair effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of shield segment repair, and in particular to a shield segment through crack repair method and a repair device. Background Art

[0002] At present, shield construction technology has been widely used in urban subway construction and still occupies a dominant position. Among them, precast concrete shield segments are the most important structural components of shield subway tunnels. They are in a complex underground hydrogeological environment for many years. Therefore, in engineering design, the concrete impermeability grade and durability are usually required to reach P10 or above and 100 years respectively. Various factors in the production and transportation process may cause the segments to crack and produce through cracks. The existing shield segment crack repair methods mainly use surface sealing method, injection method (low-pressure slow injection), pressure grouting method, etc. according to the crack situation. Among them, the surface sealing method has poor waterproof effect and only performs surface sealing. There are still gaps in the cracks inside the segment. During the service of the shield segment, it is easy to cause the damage of the sealing surface under the influence of high water pressure, and then it is easy to cause water leakage. The injection method and pressure grouting method usually inject repair materials into the cracks by drilling holes. The drilling process will not only cause secondary damage to the shield segments around the cracks, but also there is no good sealing around the cracks when injecting the repair materials, resulting in low grouting pressure and the problem of difficulty in filling the entire crack with repair materials. Summary of the invention

[0003] In order to solve the problems existing in the prior art, the present invention designs a shield segment penetration crack repair method and repair device.

[0004] On the one hand, the present invention provides a method for repairing through cracks in a shield segment, comprising the following steps:

[0005] Step 1: Determine the location of the through-crack in the shield segment, and determine the circumferential length and axial length of the through-crack in the shield segment.

[0006] Step 2: Set a front seal at the position of the through-crack corresponding to the front face of the shield segment, and set a back seal at the position of the through-crack corresponding to the back face of the shield segment, so that the front seal and the back seal will fully cover the through-crack, that is, the circumferential length of the front seal and the back seal on the shield segment is greater than the circumferential length of the through-crack, and the axial length of the front seal and the back seal is greater than the axial length of the through-crack; a front sealing cavity is formed between the front seal and the shield segment, and a back sealing cavity is formed between the back seal and the shield segment.

[0007] Step 3: inject the repair material into the front sealing cavity, and form a pressure difference between the front sealing cavity and the back sealing cavity, so that the repair material enters the back sealing cavity through the crack.

[0008] Step 4: When the repair material changes to a non-flowing and plastic state, remove the seal and scrape off the excess repair material on the front and back sides to complete the through crack repair.

[0009] Preferably, when injecting the repair material in step 3, the injection is stopped until the liquid levels of the repair material in the back sealing cavity and the front sealing cavity are higher than the highest point through the crack.

[0010] Preferably, the following steps may be included between step 3 and step 4:

[0011] The front sealing cavity and the back sealing cavity are evacuated to allow the remaining small bubbles in the through-cracks to escape.

[0012] Preferably, the repair material injected in step 3 is epoxy resin potting glue.

[0013] Preferably, the front sealing cavity is provided with a grouting hole and a first air hole, and the back sealing cavity is provided with a second air hole. In step 3, the repair material is injected into the front sealing cavity through the grouting hole.

[0014] Preferably, in step 3, the grouting hole is connected to valve A and the grouting tube in sequence; the first air hole is connected to valve B and valve C in sequence and then connected to an air compressor, valve D is connected between valve B and valve C and then connected to a vacuum pump, the second air hole is connected to valve E and then connected to a vacuum pump, air is injected into the front sealing cavity through the air compressor, and the back sealing cavity is evacuated to form a pressure difference so that the repair material enters the back sealing cavity through the crack.

[0015] The present application also provides a shield segment penetration crack repair device, specifically comprising:

[0016] Two clamping plates, each having a protrusion matching the groove on the side of the shield segment, the two clamping plates are vertically arranged on the two side surfaces of the shield segment respectively, the two clamping plates are connected by a connecting piece and clamp the shield segment in place; the two side surfaces of the shield segment refer to the splicing surfaces of the shield segment along the axial direction.

[0017] Two sealing plates have sealing strips on their surfaces along their respective edges. One of the sealing plates is sealed against the front side of the shield segment that passes through the crack to form a front sealing cavity, and the other sealing plate is sealed against the back side of the shield segment that passes through the crack to form a back sealing cavity.

[0018] Two tightening and fixing components, each of which is installed on the connecting piece, and the tightening and fixing components are used to tighten the two sealing plates against the front and back sides of the shield segment respectively.

[0019] Preferably, the specific structure of the tightening and fixing component includes:

[0020] Two tightening plates, the tightening plates are fixed on the connecting piece, and the two tightening plates are respectively arranged toward the two sealing plates;

[0021] A first threaded hole, the first threaded hole is arranged on the top plate and the axis thereof is parallel to the two clamping plates;

[0022] The screw rod is rotatably connected with the sealing plate after the screw rod thread passes through the first threaded hole.

[0023] Preferably, each sealing plate is provided with a seat bearing, and one end of the screw rod extends into the axial hole of the seat bearing and rotates with the inner ring of the bearing.

[0024] Preferably, the center of the top tightening plate and the center of the sealing plate are in a straight line, the first threaded hole is arranged at the center of the top tightening plate, and the seat bearing is arranged at the center of the sealing plate.

[0025] The present invention has the following technical effects by adopting the above technical solution:

[0026] ① Sealing cavities covering the through cracks are respectively set on the front and back sides of the shield segment. After the repair material is injected into the front sealing cavity under high pressure, the repair material seeps from the front sealing cavity to the back sealing cavity through the through cracks under the action of pressure difference and fills the through cracks, thereby making up for the shortcomings of the surface sealing method and avoiding drilling on the shield segment and avoiding secondary damage to the through cracks.

[0027] ② During the repair process, timely add the repair material to the front sealing cavity so that the liquid level of the repair material in the front sealing cavity is higher than the highest part of the through-crack, and stop injecting the repair material only after the liquid levels in the front sealing cavity and the back sealing cavity are close, so that the through-crack is fully in the liquid environment formed by the repair material, and the repair material fully fills the through-crack and the small cracks at the edge, thereby improving the density of the repair material in the crack and ensuring the repair effect.

[0028] ③ After stopping the injection of the repair material, the front sealing cavity and the back sealing cavity are evacuated, which can more fully and quickly discharge the residual small bubbles in the small cracks that penetrate the edge of the crack, thereby improving the repair efficiency and effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 This is a three-dimensional diagram of the shield segment after being clamped and fixed by the repair device of the present invention;

[0030] Figure 2 This is the main view of the shield segment;

[0031] Figure 3 is a top view of the upper clamping plate;

[0032] Figure 4 for Figure 3 Sectional view at AA in the middle;

[0033] Figure 5 It is the front view of the tie rod;

[0034] Figure 6 It is a structural diagram of the connection between the top plate and the tie rod;

[0035] Figure 7 This is the front view of the top tightening plate;

[0036] Figure 8 for Figure 7 Cross-section at the middle BB;

[0037] Fig. 9 for Figure 6 The main view of the bolt in the middle;

[0038] Fig.10 It is the front view of the front sealing plate;

[0039] Fig.11 It is the front view of the inner fixing plate;

[0040] Fig.12 for Fig.11 Sectional view of CC;

[0041] Fig.13 It is a top view of the bearing with seat;

[0042] Fig.14 It is the front view of the bearing with seat;

[0043] Fig.15 Connection diagram of air compressor, vacuum pump and valve with front sealing plate and back sealing plate;

[0044] Fig.16 This is a state diagram of the grouting of the repair material after the grouting completely covers the crack;

[0045] Fig.17 This is the state diagram after the repair material grouting is completed;

[0046] Fig.18 This is a diagram showing the state after the front sealing plate and the back sealing plate are removed and the repair material is scraped off.

[0047] In the figure, 1, upper clamping plate, 2, lower clamping plate, 3, shield segment, 4, tie rod, 5, front clamping plate, 6, clamping fixing component, 601, screw, 602, first threaded hole, 603, hand wheel, 7, back clamping plate, 8, back sealing plate, 9, front sealing plate, 10, seat bearing, 11, inner fixing plate, 12, protrusion, 13, tie rod hole, 14, second threaded hole, 15, bolt, 16, through hole, 17, grouting hole, 18, sealing strip, 19, first air hole, 20, connecting hole, 21, radial bolt, 22, vacuum pump, 23, valve E, 24, valve D, 25, air compressor, 26, valve C, 27, valve B, 28, valve A, 29, grouting barrel, 30, second air hole, 31, front sealing cavity, 32, back sealing cavity, 33, through crack. DETAILED DESCRIPTION

[0048] In order to clearly illustrate the technical features of the present invention, the present invention is described in detail below through specific implementation methods in conjunction with the accompanying drawings.

[0049] In addition, in the description of the present invention, it should be understood that the terms "center", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0050] like Figure 1-18 As shown, the shield segment penetration crack repair method provided in the present application comprises the following steps:

[0051] Step 1, determine the position of the through crack 33 of the shield segment 3, and determine the circumferential length and axial length of the through crack 33 in the shield segment 3. After determination, the front and back sides of the shield segment 3 can be marked with a marker pen;

[0052] A single shield segment 3 is an arc-shaped sheet structure. During the operation of the shield machine, multiple shield segments are spliced ​​to form an annular tunnel lining. The circumferential direction of the shield segment described in the present application is the same as the circumferential direction of the annular tunnel lining formed by its installation and splicing, and the axial direction is the same as the axial direction of the annular tunnel lining. The front of the shield segment is the inner arc surface facing the tunnel, and the back is the outer arc surface.

[0053] Step 2, set a front seal at the position of the through crack 33 corresponding to the front side of the shield segment 3, and set a back seal at the position of the through crack 33 corresponding to the back side of the shield segment 3, the circumferential length of the front seal and the back seal on the shield segment 3 is greater than the circumferential length of the through crack 33, and the axial length of the front seal and the back seal on the shield segment 3 is greater than the axial length of the through crack 33, to ensure that the front seal and the back seal can completely cover the through crack 33 on the front and back sides, provide conditions for the through crack 33 to be completely immersed in the liquid environment formed by the repair material, form a front sealing cavity 31 between the front seal and the shield segment 3, and form a back sealing cavity 32 between the back seal and the shield segment 3.

[0054] Step 3: Figure 16-17 As shown, repair material is injected into the front sealing cavity 31, and a pressure difference is formed between the front sealing cavity 31 and the back sealing cavity 32, that is, when the pressure in the front sealing cavity 31 is greater than the pressure in the back sealing cavity 32, the repair material enters the back sealing cavity 32 through the through crack 33, and in this process, the repair material is filled into the tiny cracks at the edge of the through crack 33.

[0055] It should be noted that as the repair material is injected into the through crack 33 and flows to the back sealing cavity 32 through the through crack 33, the liquid level of the repair material in the front sealing cavity 31 will drop. Moreover, when the repair material in the front sealing cavity 31 flows into the back sealing cavity 32 through the through crack 33, the liquid will preferentially pass through the path with less resistance, while the fine cracks at the edge of the through crack 33 are not easy to penetrate the repair material due to the large resistance to penetration of the repair material. Therefore, in this process, when the liquid level in the front sealing cavity 31 is lower than the highest position of the through crack 33, it is necessary to inject the repair material into the front sealing cavity 31 again, and repeat this operation until the liquid level of the repair material in the front sealing cavity is higher than the highest position of the through crack 33 and the liquid levels on both sides are close, so that the through crack 33 can be completely immersed in the liquid environment formed by the repair material, and the repair material can penetrate into the through crack 33 and the fine cracks at the edge, thereby improving the compactness of the repair material in the through crack 33, improving the bonding strength between the repair material and the crack surface, and ensuring the repair effect;

[0056] Step 4: When the repair material changes to a non-flowing and plastic state, remove the seal and scrape off the excess repair material on the front and back sides to ensure that the front and back sides of the shield segment 3 are flat. The state of the above repair material can be tested in advance to obtain a curve of the viscosity of the repair material changing with time, and the time for the repair material to reach the required state can be determined based on the viscosity change curve.

[0057] Furthermore, the following steps may be included between step 3 and step 4: after the liquid level of the repair material in the front sealing cavity 31 and the liquid level of the repair material in the back sealing cavity 32 reach the highest position higher than the through-crack 33, the front sealing cavity 31 and the back sealing cavity 32 are evacuated. The evacuation can accelerate the overflow of residual small bubbles in the through-crack 33, further improve the compactness of the repair material in the through-crack 33, and improve the repair effect.

[0058] Furthermore, the repair material injected in step 3 is epoxy resin potting glue. Epoxy resin potting glue is an adhesive with high bonding strength and chemical resistance. It can be used in bonded materials such as rocks and concrete and has a good effect on concrete repair.

[0059] Furthermore, in the above step 3, epoxy resin is injected into the front sealing cavity 31 specifically by the following methods and components, that is, a grouting hole 17 and a first air hole 19 are set on the front of the shield segment 3, and the first air hole 19 is located above the grouting hole 17 and above the highest point of the crack. The liquid level of the repair material in the front sealing cavity 31 is higher than the highest position of the through-crack 33 and lower than the position of the first air hole 19.

[0060] In addition, a second air hole 30 is provided on the back of the shield segment 3. The height of the second air hole 30 is also higher than the highest position of the through crack 33, and also higher than the liquid level of the repair material. In step 3, the repair material is injected into the front sealing cavity 31 by connecting the valve A28 and the grouting tube 29 at the grouting hole 17. The valve A28 is used to control the on-off of the pipeline between the grouting tube 29 and the grouting hole 17. When grouting is required, the valve A28 is opened, and when grouting is not required, the valve A28 is closed. Usually, the above-mentioned grouting tube 29 adopts a potting glue injector on the market, which is a conventional structure in the prior art, and its structure is not described in detail here.

[0061] Furthermore, in step 3, the specific implementation method of using the pressure difference to make the repair material flow from the front sealing cavity 31 into the back sealing cavity 32 is as follows: the first air hole 19 is connected to the valve B27 and the valve C26 in sequence, and then connected to the air compressor 25, the valve D24 is connected between the valve B27 and the valve C26, and then connected to the vacuum pump 22, and the second air hole 30 is connected to the valve E23 and then connected to the above-mentioned vacuum pump 22. When the repair material initially enters the front sealing cavity 31 and reaches the required height, the valve A28 and the valve D24 are closed, and the valve B27, the valve C26, and the valve E23 are opened. High-pressure air is injected into the front sealing cavity 31 through the air compressor, and at the same time, the back sealing cavity 32 is evacuated to form a pressure difference so that the repair material enters the back sealing cavity 32 through the crack 33.

[0062] The vacuum pump 22, the air compressor 25 and the valves are all conventional equipment in the prior art.

[0063] The present application also provides a shield segment through crack repair device, which is used in the above shield segment through crack repair method 33. Specifically, the repair device includes two clamping plates, two sealing plates and two top-tightening fixing components 6. For the convenience of description, the above two clamping plates are respectively recorded as upper clamping plate 1 and lower clamping plate 2 in the present application; the above two sealing plates are recorded as front sealing plate 9 and back sealing plate 8.

[0064] The shield segment 3 is Figure 2 In the state shown, the upper clamping plate 1 and the lower clamping plate 2 respectively have a protrusion 12 matching the groove on the side of the shield segment 3, the upper clamping plate 1 is vertically arranged on the upper side of the shield segment 3, and the lower clamping plate 2 is vertically arranged on the lower side of the shield segment 3. The upper clamping plate 1 and the lower clamping plate 2 are square plates and are arranged in parallel up and down. Four tie rod holes 13 are correspondingly arranged at the four corners of the upper clamping plate 1, and four tie rod holes 13 are also arranged at the four corners of the lower clamping plate 2. The tie rod holes 13 of the upper clamping plate 1 are aligned with the tie rod holes 13 of the lower clamping plate 2. The upper clamping plate 1 and the lower clamping plate 2 are connected by inserting a connecting piece into the tie rod holes 13 of the upper clamping plate 1 and the tie rod holes 13 of the lower clamping plate 2. The connecting piece includes a tie rod 4 and a bolt. The end of the tie rod 4 is threaded. After the bolt is tightened, the upper clamping plate 1 and the lower clamping plate 2 are connected, and the shield segment 3 is clamped and fixed.

[0065] The front sealing plate 9 and the back sealing plate 8 are arc-shaped plates. The sealing member in the repair method is the sealing plate here. One of the surfaces of the front sealing plate 9 and the back sealing plate 8 has a sealing strip 18 along the edge of each. The front sealing plate 9 abuts against the front of the shield segment 3 to squeeze and deform the sealing strip 18, thereby forming a front sealing cavity 31 covering the through crack 33 between the front sealing plate 9 and the front of the shield segment; similarly, a back sealing cavity 32 covering the through crack 33 is formed between the back sealing plate 8 and the back of the shield segment 3. Specifically, a groove can be made on the sealing plate, and a solid silicone sealing strip can be embedded in the groove. The sealing plate can be made of a transparent acrylic plate to facilitate observation of the liquid level.

[0066] The front sealing plate 9 and the back sealing plate 8 are pressed and fixed on the shield segment 3 by two top fixing components 6. Firstly, the structure is simple, and secondly, the installation and disassembly are convenient, the overall volume is small, and it is convenient to carry.

[0067] Furthermore, the specific structure of each of the above-mentioned tightening and fixing components 6 includes two tightening plates, a first threaded hole 602 and a screw rod 601 .

[0068] The above two top tightening plates are recorded as the front top tightening plate 5 and the back top tightening plate 7; the front top tightening plate 5 and the back top tightening plate 7 are in the shape of square flat plates, the front top tightening plate 5 is arranged on the front of the shield segment 3 and is located between the upper clamping plate 1 and the lower clamping plate 2, and is perpendicular to the upper clamping plate 1 and the lower clamping plate 2 at the same time, and the two ends of the front top tightening plate 5 have through holes 16, when the tie rod 4 is connected to the upper clamping plate 1 and the lower clamping plate 2, the tie rod 4 simultaneously passes through the through hole 16 of the top tightening plate, and a second threaded hole 14 is arranged in a direction perpendicular to the through hole 16, and a bolt 15 is passed through the second threaded hole 14, and the top tightening plate is fixed to the tie rod 4 by means of the bolt 15. The connection and fixing method of the back top tightening plate 7 is the same as that of the front top tightening plate 5, which will not be repeated here.

[0069] The central axis of the first threaded hole 602 is parallel to the upper clamping plate 1 and the lower clamping plate 2. One end of the screw 601 is threaded through the first threaded hole 602 and is rotatably connected to the front sealing plate 9 or the back sealing plate 8. The other end can be connected to a handwheel 603. By turning the handwheel 603, the screw 601 is rotated, and the screw 601 is rotated to tighten the front sealing plate 9 or the back sealing plate 8. Alternatively, the other end of the screw 601 can also be directly turned with a wrench or pliers.

[0070] Furthermore, the rotational connection between the screw 601 and the front sealing plate 9 or the back sealing plate 8 can be achieved in the following manner, that is, a seat bearing 10 is respectively provided on the two sealing plates, and the base of the seat bearing 10 has a connecting hole 20, which is connected to an inner fixing plate 11 by screws, and the inner fixing plate 11 and the sealing plate are bonded by Kraft AB glue, so that the seat bearing 10 can be fixed on the sealing plate, and one end of the screw 601 extends into the axial hole of the seat bearing 10 and is connected to the inner ring of the bearing by tightening it with a radial bolt 21 so that the screw 601 rotates with the inner ring of the bearing.

[0071] Furthermore, in order to improve the overall stability, especially for the force balance of the front clamping plate 5, the back clamping plate 7, the front sealing plate 9, and the back sealing plate 8, the center of the clamping plate and the center of the sealing plate are in a straight line, the first threaded hole 602 is arranged at the center of the clamping plate, and the seat bearing 10 is arranged at the center of the sealing plate.

[0072] The above specific implementation manner cannot be used as a limitation on the protection scope of the present invention. For those skilled in the art, any substitution, improvement or change made to the implementation manner of the present invention falls within the protection scope of the present invention.

[0073] The matters not described in detail in the present invention are all known technologies to those skilled in the art.

Claims

1. A method for repairing through-cracks in shield segments, characterized in that: The steps include: Step 1, determining the position of the through-crack of the shield segment, and determining the circumferential length and axial length of the through-crack in the shield segment; Step 2, a front seal is arranged at a position of the front side of the shield segment corresponding to the through-crack, and a back seal is arranged at a position of the back side of the shield segment corresponding to the through-crack, the circumferential length of the front seal and the back seal is greater than the circumferential length of the through-crack, the axial length of the front seal and the back seal on the shield segment is greater than the axial length of the through-crack, the front seal and the back seal are sealing plates respectively, the surfaces of the two sealing plates have sealing strips along their respective edges, the front seal is in sealing contact with the front side of the shield segment around the through-crack to form a front sealing cavity, and the back seal is in sealing contact with the back side of the shield segment around the through-crack to form a back sealing cavity; Step 3, injecting a repair material into the front sealing cavity, and forming a pressure difference between the front sealing cavity and the back sealing cavity, so that the repair material enters the back sealing cavity through the crack; Step 4: When the repair material changes to a non-flowing and plastic state, remove the seal and scrape off the excess repair material on the front and back sides to complete the through crack repair.

2. A method for repairing through cracks in a shield segment according to claim 1, characterized in that: When injecting the repair material in step 3, the injection is stopped until the liquid levels of the repair material in the back sealing cavity and the front sealing cavity are higher than the highest point of the through-crack.

3. A method for repairing through cracks in a shield segment according to claim 1, characterized in that: The following steps are included between step 3 and step 4: The front sealing cavity and the back sealing cavity are evacuated to allow the remaining small bubbles in the through-cracks to escape.

4. A shield segment through crack repair method according to claim 1, characterized in that: The repair material injected in step 3 is epoxy resin potting glue.

5. A method for repairing through cracks in a shield segment according to claim 3, characterized in that: The front sealing cavity is provided with a grouting hole and a first air hole, and the back sealing cavity is provided with a second air hole. In step 3, the repair material is injected into the front sealing cavity through the grouting hole, and the first air hole and the second air hole are used to extract residual small bubbles.

6. A method for repairing through-cracks in a shield segment according to claim 5, characterized in that: In step 3, the grouting holes are connected to valve A and the grouting tube in sequence; the first air hole is connected to valve B and valve C in sequence and then connected to an air compressor, valve D is connected between valve B and valve C and then connected to a vacuum pump, the second air hole is connected to valve E and then connected to the vacuum pump, air is injected into the front sealing cavity through the air compressor, and the back sealing cavity is evacuated to form a pressure difference so that the repair material enters the back sealing cavity through the crack.

7. A repairing device for use in the method for repairing through-cracks in shield segments according to any one of claims 1 to 6, characterized in that: The method comprises two sealing plates, and further comprises: Two clamping plates, each of which has a protrusion matching the groove on the side of the shield segment, and each of which is vertically arranged on two side surfaces of the shield segment, and each of which is connected by a connecting piece to clamp and fix the shield segment; Two tightening and fixing components are installed on the connecting piece, and are used to tighten the two sealing plates against the front and back sides of the shield segment respectively.

8. The repair device according to claim 7, characterized in that: The top tightening and fixing component comprises: Two tightening plates, the tightening plates are fixed on the connecting piece, and the two tightening plates are respectively arranged toward the two sealing plates; A first threaded hole, wherein the first threaded hole is disposed on the top plate and the axis thereof is parallel to the two clamping plates; A screw rod is rotatably connected to the sealing plate after the screw rod threads through the first threaded hole.

9. The repair device according to claim 8, characterized in that: Each of the sealing plates is provided with a seat bearing, and one end of the screw rod extends into the axial hole of the seat bearing and rotates along with the inner ring of the bearing.

10. The repair device according to claim 9, characterized in that: The center of the top tightening plate and the center of the sealing plate are in a straight line, the first threaded hole is arranged at the center of the top tightening plate, and the seat bearing is arranged at the center of the sealing plate.