PN junction forming method based on ion implantation, storage medium and integrated circuit device
The PN junction formation method based on ion implantation solves the material damage and doping layer control problems caused by high-temperature treatment in the traditional base diffusion process, achieves precise compensation and repair of the PN junction, and improves product yield and manufacturing quality.
Patent Information
- Application Number
- CN202411068092.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-06
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-08-06
AI Technical Summary
The traditional base region diffusion process requires high-temperature treatment, resulting in material damage, high energy consumption, and difficulty in accurately controlling the doping layer, affecting the uniformity and repeatability of the PN junction and reducing product yield.
Using a PN junction formation method based on ion implantation, B3+ ions are screened through a mass analyzer, and the first and second ion implanters are used for primary and compensation injection respectively. Combined with the annealing process, the concentration and depth of the doped area are accurately controlled. Qualified areas will be compensated for repairs.
It improves the qualification rate and product yield of PN junctions, enhances manufacturing quality, and achieves precise control and uniformity of doped layers.
Smart Images

Figure CN118588542B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of integrated circuit manufacturing, and in particular to a PN junction forming method based on ion implantation, a storage medium and an integrated circuit device. Background Art
[0002] In the manufacturing process of integrated circuit devices such as diodes and triodes, the base diffusion process is involved. The traditional base diffusion method uses solid boron nitride diffusion, and its overall device is as follows Figure 1 As shown, the boron nitride source wafer and the silicon wafer are placed alternately on the V-groove of the quartz boat and kept parallel. With high-purity N2 protection, the impurity vapor is volatilized from the surface of the impurity source. After a series of chemical reactions at high temperature, the impurity atoms diffuse into the wafer to form a PN junction.
[0003] The specific method is: oxygen is passed through at the diffusion temperature (930℃~960℃) for 10~30 minutes to make the surface boron nitride react with oxygen to generate boron trioxide. Then put the positive film and sample film in, and the boron trioxide reacts with silicon at high temperature to produce boron and silicon oxide, and the generated boron will diffuse into the silicon wafer due to the high temperature.
[0004] In the current process, the base re-diffusion process itself requires high-temperature treatment, which can easily lead to material damage and consume a lot of energy. Because the process is manually operated, the solid source saturation time and the speed of pushing and pulling the chip will vary from person to person, making it impossible to accurately control the doping layer. In addition, due to the uniformity between the boron source sheets and the different heat dissipation levels from the furnace mouth to the furnace tail during the diffusion process, the base pre-diffusion block resistance (Ω / □) value cannot be accurately controlled at a specific value every time, and the wet oxygen time of the base re-diffusion cannot be a fixed value every time, resulting in the inability to independently control the junction depth and concentration, which greatly affects the uniformity and repeatability of the manufactured finished product, and the product yield is low. Summary of the invention
[0005] The purpose of the present application is to provide a PN junction formation method based on ion implantation, a storage medium and an integrated circuit device to solve at least one of the above problems.
[0006] In a first aspect of the present application, a method for forming a PN junction based on ion implantation is provided, the method comprising:
[0007] Determine the area to be doped and the standard concentration and depth of doping required on the silicon substrate after photolithography;
[0008] B was screened out from the impurity source B2H6 by mass analyzer 3+ ;
[0009] The B is implanted by a first ion implanter according to the corresponding dose and energy. 3+ implanting into the region to be doped;
[0010] Annealing the doped area to form an initial PN junction;
[0011] Calculating the errors between the actual concentration and actual depth of each doping region in the initial PN junction and the standard concentration and standard depth, and taking the doping region whose error exceeds the error threshold as the region to be compensated;
[0012] The area to be compensated is subjected to B 3+ Inject again;
[0013] To B 3+ The re-implanted region is annealed again to form a PN junction.
[0014] In one embodiment, the B is implanted by a first ion implanter according to a corresponding dose and energy. 3+ Implanting into the region to be doped comprises:
[0015] Determine the injection times and the concentration and dosage of each injection according to the standard concentration and standard depth;
[0016] The first ion implanter implants the doped area according to the determined number, concentration and dosage. 3+ injection.
[0017] In one embodiment, the B is implanted by a first ion implanter according to a corresponding dose and energy. 3+ Implanting into the region to be doped comprises:
[0018] Determining the implantation angle at each position in the region to be doped according to the standard concentration and the standard depth;
[0019] The first ion implanter implants the B at the position in the to-be-doped area according to the corresponding implantation angle, corresponding dose and energy. 3+ implanted into the region to be doped.
[0020] In one embodiment, when the first ion implanter moves relative to the first end of the area to be doped to the second end, the implantation angle gradually increases, and the corresponding implantation angle at the first end is less than 90°, and the implantation angle at the second end is greater than 90°, and the implantation angle is the angle formed by the ion implantation direction and the movement direction of the silicon substrate relative to the first ion implanter.
[0021] In one of the embodiments, when the first ion implanter moves relatively from the first end to the second end of the region to be doped, the dose and energy emitted are kept constant.
[0022] In one of the embodiments, the method further includes: obtaining a historical regional position and a concentration of the region to be compensated; and correcting the injection angle based on the regional position and the concentration to be compensated.
[0023] In one embodiment, the area to be compensated is B 3+ Re-injection, including:
[0024] Determining the compensation dose, compensation energy and implantation distance from the silicon substrate used by the second ion implanter according to the compensation concentration required to be implanted in the area to be compensated;
[0025] The compensation dose and compensation energy B are vertically implanted into the silicon substrate by the second ion implanter at a distance of the compensation area being the implantation distance. 3+ .
[0026] In one embodiment, the step of annealing the doped region comprises:
[0027] The silicon substrate is placed in a predetermined annealing temperature environment, and annealed in a pure oxygen environment for a first time, in a wet oxygen environment for a second time, and in a dry oxygen environment for a second time.
[0028] In a second aspect of the present application, a computer-readable storage medium is provided, on which executable instructions are stored. When the executable instructions are executed by a processor, the processor executes the method described in any one of the embodiments of the present application.
[0029] In a third aspect of the present application, an integrated circuit device is provided, wherein the integrated circuit device comprises a PN junction formed by the method described in any one of the embodiments of the present application.
[0030] Compared with the prior art, the beneficial effects of this application include:
[0031] The PN junction forming method based on ion implantation, the storage medium and the integrated circuit device of the present application determine the area to be compensated by inspecting the actual concentration and actual depth of the area to be doped of the initially formed PN junction, and then performing B 3+ The re-injection and re-annealing treatments make it possible to compensate and repair unqualified PN junction products, thereby improving the qualified rate of the PN junction, and further improving the product yield and product manufacturing quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope of the present application.
[0033] Figure 1 A schematic diagram of the structure of solid boron nitride diffusion in one embodiment;
[0034] Figure 2 is a schematic flow chart of a method for forming a PN junction based on ion implantation in one embodiment;
[0035] Figure 3 is a schematic diagram of a doping region in an embodiment;
[0036] Figure 4 is a schematic diagram of ion implantation in one embodiment;
[0037] Figure 5 is a schematic diagram of ion implantation in another embodiment;
[0038] Figure 6 FIG. 1 is a schematic diagram of a flow chart for calculating the actual concentration of each doping region in an initial PN junction in an embodiment. DETAILED DESCRIPTION
[0039] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0040] All terms (including technical and scientific terms) used in this application have the meanings commonly understood by those skilled in the art, unless otherwise defined. It should be noted that the terms used here should be interpreted as having a meaning consistent with the context of this specification, and should not be interpreted in an idealized or overly rigid manner.
[0041] For example, the terms "first", "second", etc. used in this application can be used to describe various components in this article, but these components are not limited by these terms. These terms are only used to distinguish a first component from another component. For example, without departing from the scope of this application, a first ion implanter can be referred to as a second ion implanter, and similarly, a second ion implanter can be referred to as a first ion implanter. Both the first ion implanter and the second ion implanter are ion implanters, but they are not the same ion implanter.
[0042] For another example, the terms “include”, “comprising”, etc. used in this application indicate the existence of features, steps, operations and / or components, but do not exclude the existence or addition of one or more other features, steps, operations or components.
[0043] In one embodiment, a method for forming a PN junction based on ion implantation is provided. Figure 2 As shown, the method includes:
[0044] Step 202, determining the area to be doped and the standard concentration and standard depth required for doping on the silicon substrate after photolithography.
[0045] In this embodiment, the silicon (Si) substrate is a component of a circuit device that needs to be doped with boron ions to form a PN junction. The circuit device may be a device on an integrated circuit including a diode, a triode, an octal buffer, etc. The area and position of the region that needs to be doped on different devices are different.
[0046] Specifically, before doping, photolithography can be first performed on the silicon substrate. The photolithography process includes one or more of mask preparation, silicon substrate cleaning, photoresist coating, prebaking, mask alignment, exposure, development, postbaking, mapping, etc. The mask is a template for making photolithography patterns, usually a transparent glass sheet coated with photoresist. By using computer-aided design (CAD) software, the desired pattern is made, and then the pattern is transferred to the mask using electron beam exposure or a photolithography machine. Through the cleaning of the silicon substrate, pollutants and unevenness on the surface of the silicon substrate can be removed, providing a suitable surface for photoresist to adhere. Photoresist coating includes uniformly coating the photoresist on the surface of the substrate. Through prebaking, the solvent can be removed and a uniform thin film can be formed. Mask alignment includes accurately aligning the mask and the substrate to ensure that the desired pattern can be correctly transferred to the substrate. Exposure includes using a photolithography machine to irradiate a specific light source (such as ultraviolet light) onto the photoresist through the pattern on the mask, so that the photoresist undergoes a chemical reaction in the pattern area. Development means: immersing the substrate in a developer solution to dissolve the unexposed or exposed parts of the photoresist to form the desired grooves or patterns. Post-baking can further cure the photoresist and remove the remaining solvent. Mapping includes measuring and verifying whether the size and shape of the resulting pattern meet the requirements through tools such as microscopes.
[0047] In this embodiment, the region to be doped (i.e., the region to be doped) of the silicon substrate to be doped and the standard concentration and standard depth of doping required in the corresponding region are pre-set according to the process requirements of the integrated circuit device to be manufactured. When it is determined that the integrated circuit device to be manufactured using the silicon substrate is to be used, the corresponding region to be doped and the standard concentration and standard depth of doping required can be determined based on the determined integrated circuit device. The region to be doped can be as follows: Figure 3 The area shown in the figure, for the silicon substrate after lithography, can be determined that the area that needs to be doped is the "doping area" marked in the figure, the standard depth is the depth of the corresponding "doping area" in the figure, and the doping concentration represents the ratio of boron ions to silicon atoms in the doping area, or the number of boron ion atoms doped per unit volume.
[0048] For example, the standard concentration may be a ratio of one thousandth to one billionth, or a doping concentration of 10 14 / cm 3 ~10 18 / cm 3 The doping depth (depth of the PN junction) can be, for example, 0.1 micron to 10 microns.
[0049] Step 204, filter out B from the impurity source B2H6 by a mass analyzer 3+ .
[0050] In this embodiment, the impurity source selected is diborane (B2H6), and the mass analyzer uses an electromagnetic field to separate the impurity source ions, and B2H6 is screened out from the impurity source. 3+ (trivalent boron ion). Specifically, the magnetic field and electric field parameters of the mass analyzer can be adjusted so that B 3+ The ions can be separated from other ions and transported along a specific path to subsequent processing steps.
[0051] Step 206: B is implanted by a first ion implanter according to the corresponding dose and energy. 3+ Implant into the area to be doped.
[0052] In this embodiment, the screened B 3+ The ions are then directed to the first ion implanter. In the first ion implanter, the intensity and direction of the ion beam are precisely controlled according to the predetermined doping dose and energy parameters, so that B 3+ The ions can be uniformly implanted into the area to be doped of the silicon substrate and reach the required standard concentration and standard depth.
[0053] like Figure 4 and Figure 5 As shown in the figure, when boron ions are implanted into the silicon substrate, they collide with silicon atoms to generate energy. When the energy is exhausted, the boron ions will stay at a certain position in the silicon substrate. Boron ions transfer energy to silicon atoms by colliding with silicon atoms, making silicon atoms become new incident particles. The new incident particles will collide with other silicon atoms, forming a chain reaction, thereby completing the doping.
[0054] Among them, the dose injected by the ion implanter determines the concentration of the area to be doped, and the injected energy determines the range of the ions, that is, the depth of the area to be doped. Before the implantation, the relationship between one or more requirements such as the area to be doped, the standard concentration and the standard depth and one or more parameters such as the injected dose, energy, injection angle, and moving speed are preset. Based on this relationship, the dose, energy, and relative position between the first ion implanter and the silicon substrate required for each position can be determined, and the beam density, injection angle, and scanning mode of the first ion implanter can be controlled to ensure the uniformity and depth of doping. For example, the implantation dose is 1.0E14ion / cm 2 、2.0E14ion / cm 2 、2.5E14ion / cm 2 、3.0E14ion / cm 2 、4.0E14ion / cm 2 、5.0E14ion / cm 2 、5.5E14ion / cm 2 、6.0E14ion / cm 2 、7.0E14ion / cm 2 、8.0E14ion / cm 2 、10.0E14ion / cm 2 Equal dose; injection energy is 50Kev, 100Kev, 200Kev, 300Kev, 400Kev, 500Kev and other energies.
[0055] Optionally, during the implantation process, the first ion implanter may move to implant the region to be doped, or the silicon substrate may move, or both the first ion implanter and the silicon substrate may move to implant various positions in the region to be doped.
[0056] In one embodiment, the implanted dose indicates the dose set for the particle implanter when implanting, which may be an average dose or a fixed dose; the implanted energy indicates the energy set for the particle implanter when implanting, which may be an average energy or a fixed energy. When the average energy is used, the implanted energy set at each position remains unchanged; when the fixed dose is used, the implanted dose set at each position remains unchanged.
[0057] When it is an average dose, the set injection dose at different positions can be fine-tuned based on the average dose. For example, at the position of a certain area to be doped, the corresponding set injection dose can be within the range of the average dose-fine-tuning dose ~ average dose + fine-tuning dose. When it is an average energy, the injection energy at different positions can be fine-tuned based on the average energy. For example, at the position of a certain area to be doped, the corresponding injection energy can be within the range of the average energy-fine-tuning energy ~ average energy + fine-tuning energy. Among them, the fine-tuning energy and fine-tuning dose are pre-set fixed values. The system can set the injection energy and injection dose at each position based on actual experience and / or historical injection results, so that the actual concentration and actual depth of the doped area finally formed reach the standard concentration and standard depth.
[0058] By setting fine-tuning energy and fine-tuning dose, the set injection energy and injection dose at each position can be fine-tuned, which improves the flexibility of ion injection and can be flexibly adjusted according to actual conditions, experience and historical injection results to maximize operational flexibility.
[0059] Step 208, annealing the doped region to form an initial PN junction.
[0060] In this embodiment, ion implantation may cause damage to the crystal lattice, especially when the implantation dose is large, the wafer may change from single crystal to amorphous, so annealing is required to repair the crystal lattice defects. Figure 4 As shown, Figure 4 The left picture shows the state of the chip before annealing. It can be found that some of the lattices have defects. Figure 4 The right picture shows the state after annealing treatment. It can be found that its lattice is repaired.
[0061] Specifically, the annealing time and temperature, as well as the annealing environment, can be controlled to form a processed PN junction so that the leakage current, breakdown voltage, etc. of the obtained silicon wafer meet subsequent requirements.
[0062] In one embodiment, step 208 includes placing the silicon substrate in a predetermined annealing temperature environment, and performing annealing treatment in the order of annealing in a pure oxygen environment for a first time, annealing in a wet oxygen environment for a second time, and annealing in a dry oxygen environment for a second time.
[0063] Among them, the annealing temperature, the first time, the second time, and the third time can be the temperature and time determined according to the process requirements and the area to be doped, the standard concentration, and the standard depth. The time and annealing temperature corresponding to different areas to be doped, standard concentrations, and standard depths may not be the same.
[0064] After obtaining the area to be doped and the standard concentration and depth to be doped, the corresponding annealing temperature, first duration, second duration and third duration can be determined. For example, when the integrated circuit device is an eight-buffer, its process requirement is 250-270Ω / □. Based on this, the area to be doped of the silicon substrate determined is as follows: Figure 3 For the doping region shown, the determined annealing temperature is 1050° C., and the corresponding first duration is 5 minutes, the second duration is 8 minutes, and the third duration is 5 minutes.
[0065] The repair quality of the lattice can be improved by first performing pure oxygen environment annealing, then performing wet oxygen environment annealing, and finally performing dry oxygen environment annealing.
[0066] Step 210, calculating the errors between the actual concentration and actual depth of each doping region in the initial PN junction and the standard concentration and standard depth, and taking the doping region whose error exceeds the error threshold as the region to be compensated.
[0067] In this embodiment, after annealing, the doping area of each silicon substrate that has been doped can be inspected to determine whether the doping area is qualified, and doping compensation can be performed on unqualified silicon substrates. Specifically, the actual concentration and actual depth of the boron ions injected into the area to be doped can be measured, and the error between the actual concentration, actual depth and the standard concentration and standard depth can be measured. When the error exceeds the corresponding error threshold, the corresponding position is used as the corresponding area to be compensated. When the area of the area to be compensated exceeds the preset first area threshold, it is determined that the silicon substrate needs to be compensated.
[0068] The actual concentration and actual depth at each position in the doping region can be directly or indirectly measured by electrochemical capacitance voltage spectroscopy. The first area threshold is a pre-set minimum area suitable for compensation by an ion implanter. The system can pre-set the corresponding error threshold and the first area threshold.
[0069] Specifically, the error includes a first error and a second error. The first error between the actual concentration and the standard concentration at each position in the doping region can be compared, and the second error between the actual depth and the standard depth can be compared. Based on the first error and the second error, it is determined whether compensation is required. The first error reflects the difference between the actual concentration and the standard concentration, and the second error reflects the difference between the actual depth and the standard depth.
[0070] Optionally, the first error = standard concentration - actual concentration; the second error = standard depth - actual depth. The error threshold may also include a first error threshold corresponding to the first error, and a second error threshold corresponding to the second error.
[0071] When the error at any position exceeds the corresponding error threshold, the corresponding position is determined to be the position to be compensated. Alternatively, when both errors exceed the corresponding error threshold, the corresponding position is determined to be the position to be compensated.
[0072] Optionally, for the identified positions to be compensated, the connected positions to be compensated can be grouped together to form a region to be compensated. It can be understood that the positions to be compensated and the regions to be compensated on the same silicon substrate can include multiple ones. When the area of any region to be compensated exceeds the corresponding first area threshold, it is determined that the silicon substrate needs to be ion implanted again, and the following step 212 is executed. Otherwise, no ion implantation is required.
[0073] Step 212: perform B on the area to be compensated. 3+ Inject again.
[0074] In this embodiment, the identified area to be compensated may be subjected to B 3+ Inject again to optimize the PN junction and improve the product qualification rate.
[0075] Optionally, for B 3+ By injecting again, the compensation concentration and compensation depth of each position that needs to be doped again can be determined by the above difference, and then the compensation dose and compensation energy required according to the compensation concentration and compensation depth. 3+ , use the corresponding ion implanter to carry out B to the corresponding position according to the corresponding compensation energy and compensation dose 3+ Inject again.
[0076] Optionally, the ion implanter used may be a second ion implanter different from the first ion implanter. Step 212 includes: determining the compensation dose, compensation energy and implantation distance from the silicon substrate used by the second ion implanter according to the compensation concentration required to be implanted in the area to be compensated; and vertically implanting the compensation dose and compensation energy B into the silicon substrate by the second ion implanter at a distance from the area to be compensated of the implantation distance. 3+ .
[0077] Because B 3+ The energy and dose required for the second implantation are usually much smaller than the energy and dose of the first B3+ implantation. Therefore, a second ion implanter that can produce a smaller dose can be used to perform B3+ implantation. 3+ Inject again. And in the first B 3+ During implantation, the first ion implanter can process each silicon substrate in batches, thereby improving the operation efficiency. After the batch processing is completed, not all silicon substrates need to be processed by B. 3+ Re-injection and B3+ The compensation concentration and compensation depth required for each silicon substrate to be implanted again are not necessarily the same. Therefore, it is necessary to perform personalized treatment for each silicon substrate that needs doping compensation. At this time, the second ion implanter can be used to perform B 3+ By using a second ion implanter, according to the area of the area to be compensated and one or more parameters of the compensation depth and compensation concentration, the intensity and direction of the ion beam of the second ion implanter, as well as the implantation distance between the second ion implanter and the silicon substrate are determined, so that B 3+ Ions can be injected into corresponding positions as required, so that the doped area after re-injection can reach the required standard concentration and standard depth.
[0078] Furthermore, for the injection angle of the area to be compensated, the injection can be performed in a vertical manner, and a suitable injection angle can be determined according to the compensation concentration and compensation depth corresponding to each position in the area to be compensated, and the area to be compensated can be injected according to the corresponding injection angle. 3+ Inject again.
[0079] In one embodiment, the area of a single region of the region to be compensated is detected, and when the area of the single region does not exceed a preset second area threshold, B is injected vertically into the corresponding single region of the region to be compensated. 3+ When the area of a single region exceeds the second area threshold, the corresponding injection angle is calculated according to the compensation concentration and compensation depth at each position in the single region of the area to be compensated, and the single region is injected according to the injection angle. 3+ Inject again.
[0080] The second area threshold is a preset value that is larger than the first area threshold. When the area of the area to be compensated is too small, there is no need to consider adjusting the injection angle, and B can be directly injected vertically. 3+ Inject again, and when the area exceeds the second area threshold, the injection angle can be adjusted so that according to the adjusted injection angle and the set appropriate distance, the required compensation dose and compensation energy can be accurately injected into the area to be compensated.
[0081] Step 214, for B 3+ The re-implanted region is annealed again to form a PN junction.
[0082] In this embodiment, similar to step 208, for the re-annealing treatment, the corresponding annealing time and temperature parameters can be determined according to the area to be compensated, the compensation concentration, and the compensation depth, and annealing is performed according to the determined environment and temperature parameters to restore the lattice and form a PN junction.
[0083] The PN junction formation method based on boron ion base injection in the present application determines the area to be compensated by inspecting the actual concentration and actual depth of the area to be doped of the initially formed PN junction, and performs B injection on the area to be compensated. 3+ The re-injection and re-annealing treatments make it possible to compensate and repair unqualified PN junction products, thereby improving the qualified rate of the PN junction, and further improving the product yield and product manufacturing quality.
[0084] In one embodiment, step 206 includes: determining the number of implantations and the concentration and dose of each implantation according to the standard concentration and the standard depth; performing B implantation on the to-be-doped region according to the determined number of implantations, concentration and dose by a first ion implanter; 3+ injection.
[0085] Specifically, the system can obtain the previous PN junction formation record information, and based on the record information, calculate the first average error size under different doping area areas, standard concentrations and standard depths under different scanning (injection) times, and determine the number of times the first average error is the smallest under various doping area areas, standard concentrations and standard depths, forming a correlation between the doping area area, standard concentration and standard depth and the injection times. When one injection is completed, one injection is completed for all positions in the area to be doped.
[0086] Furthermore, the second average error formed by using different doses and energies for the same number of scans and the same process requirements of the doping region area, standard concentration and standard depth is queried from the recorded information, and the dose and energy corresponding to the injection with the smallest second average error are associated with the doping region area, standard concentration and standard depth.
[0087] Based on the two associations, the number of implantations corresponding to the area to be doped, the standard concentration, and the standard depth in step 202, as well as the concentration and dosage in each implantation can be determined.
[0088] For example, the number of implantations is determined to be 3, the energy of the first implantation is 50 KeV, and the dose is 2E14 ion / cm 2 The energy of the second injection is 100KeV and the dose is 2E14 ion / cm 2 The third injection energy is 50KeV and the dose is 2E14 ion / cm 2 Similarly, the energy of each implantation may be the fixed energy or average energy mentioned above, and the dose of each implantation may be the fixed dose or average dose mentioned above.
[0089] In this embodiment, the number of scans (injections) required, as well as the energy and dose required for each scan, can be set based on the standard concentration and standard depth, so that after the corresponding number of scans, the actual depth and actual concentration reached are as close to the standard depth and standard concentration as possible.
[0090] In one embodiment, step 206 further includes: determining an implantation angle at each position in the to-be-doped region according to the standard concentration and the standard depth; implanting B at the position in the to-be-doped region according to the corresponding implantation angle, the corresponding dose and the energy by the first ion implanter; 3+ Implant into the area to be doped.
[0091] In this embodiment, in addition to the influence of the implantation energy and implantation dose on the doping concentration and the doping depth, the positional relationship between the ion implanter and the region to be doped will also affect the doping concentration and the doping depth.
[0092] Specifically, the positional relationship includes the distance between the ion implanter and the region to be doped and the implantation angle. The implantation angle is the angle formed by the ion implantation direction and the movement direction of the silicon substrate relative to the first ion implanter. Figure 5 As shown, the X direction represents the implantation direction of the ion implanter, and the Y direction represents the movement direction of the silicon substrate relative to the ion implanter. The angle A formed by the two is the implantation angle.
[0093] Optionally, during one implantation process, the distance between the ion implanter and the silicon substrate and the implantation direction can be fixed values or adjustable values. For example, the distance can be a fixed distance, and the implantation direction can be fixed to 90°, that is, the implantation reverse direction is perpendicular to the scanning direction. Or the distance is a fixed distance, and the implantation direction is an adjustable direction, and changes with the scanning position.
[0094] Since the injected boron ions will collide with silicon atoms, in order to improve the consistency and uniformity of the injection concentration and injection depth, and prevent the boron ions from extending laterally to the non-doped area at the edge of the doped area, the angle of the incident direction can be adjusted so that the incident direction does not remain perpendicular to the relative movement of the silicon substrate at all positions.
[0095] Specifically, when the first ion implanter moves relatively from the first end to the second end of the region to be doped, the implantation angle gradually increases, and the corresponding implantation angle at the first end is less than 90°, and the implantation angle at the second end is greater than 90°.
[0096] Among them, a deflection angle can be set so that when it is at the edge position of the area to be doped, the injection angle = 90°-deflection angle, or the injection angle = 90°+deflection angle. The size of the deflection angle can be any suitable value such as 1°~10°. Specifically, the deflection angle can be determined according to one or more parameters such as the area to be doped, the standard concentration and the standard depth, for example, the determined deflection angle can be 3°, 4°, 5°, 6° and other values. When the first end of the area to be doped moves to the second end, the injection angle at the first end position = 90°-deflection angle, the injection angle at the second end position = 90°+deflection angle, and the injection angle at the middle position between the first end and the second end = 90°. During the movement process, the change speed of the injection angle is adjusted according to the movement speed, for example, when the relative movement from the first end to the first relative distance reaches the first relative distance, the change value of the injection angle is just equal to the deflection angle, and the injection angle at the position under the first relative distance = 90°. After the injection angle is kept at 90° and the second relative distance is continuously moved, the injection angle begins to increase until it reaches the position corresponding to the second end, and the injection angle = 90° + deflection angle, wherein the distance between the position corresponding to the second relative distance and the position corresponding to the second end = the first relative distance. The first relative distance does not exceed half of the distance between the first end and the second end of the region to be doped, and its size can be a preset fixed value, or a value determined according to one or more parameters such as the deflection angle, the moving speed, the region to be doped, the standard concentration and the standard depth. Among them, the injection angle can be adjusted by adjusting the injection direction of the ion implanter and / or adjusting the direction of the silicon substrate. For example, during the relative movement of the ion implanter and the silicon substrate, the injection direction of the ion implanter is kept unchanged, and only the direction and height of the silicon substrate are adjusted to adjust the injection angle. For example, in the relationship between the ion implanter and the silicon substrate in the upper and lower positions, one end of the silicon substrate can be raised or lowered by a certain distance to adjust the injection direction.
[0097] In one embodiment, when the first ion implanter moves relatively from the first end of the region to be doped to the second end, the dose and energy emitted remain constant. During one such relative movement, the dose emitted is set to be a fixed dose, and the energy emitted is set to be a fixed energy.
[0098] In this embodiment, during the implantation process, the distance and angle between the ion implanter and the silicon substrate can also be adjusted. By only adjusting the distance and angle while keeping the set dose and energy unchanged, the actual concentration and actual depth in the area to be doped can be made closer to the standard concentration and standard depth, thereby improving the product yield.
[0099] In one embodiment, the method further includes: obtaining the historical regional position and concentration of the region to be compensated; and correcting the injection angle based on the regional position and the concentration to be compensated.
[0100] In this embodiment, the system can also optimize the implantation angle at the corresponding position according to the historical compensation area and the concentration to be compensated, so that the subsequent silicon substrate is implanted according to the optimized implantation angle to avoid the generation of B 3+ Re-injection and re-annealing further improve the operating efficiency of the product.
[0101] In one embodiment, Figure 6 As shown, the actual concentration of each doping region in the initial PN junction is calculated, including:
[0102] Step 602, obtaining the initial doping concentration at each position, and using the initial doping concentration as the current doping concentration.
[0103] In this embodiment, the standard concentration at each position in the region to be doped can be used as the initial doping concentration, and the initial doping concentration at each position outside the region to be doped can be set to 0. Based on the initial doping concentration, the doping concentration is iteratively updated, and the actual concentration at the corresponding position is calculated through multiple iterative updates.
[0104] Specifically, remember the location r The initial doping concentration N 0 (r) The calculated doping concentration after the i-th iteration is N i (r) .
[0105] Step 604, determining the doping basis function and superposition coefficient at the corresponding position.
[0106] Step 606, calculating the doping concentration change value based on the basis function and the superposition coefficient.
[0107] Among them, the basic function can be set f k (r) = δ(rr k ) , δ is the Dirac-delta function. There are multiple superposition coefficients, record the first k The superposition coefficient is a k For each set current doping concentration, the system can calculate the corresponding basic function through the data measured by the corresponding concentration measurement equipment f k (r)and superposition coefficient a k .
[0108] The doping concentration change value can be expressed as the linear superposition of the basic function and the superposition coefficient. Calculate the change in doping concentration N c (r) , K is the total number of superposition coefficients.
[0109] Specifically, the capacitance-voltage data at different positions of the silicon substrate measured by the experiment are obtained in advance. , where i=1, 2, 3...M, represents the number of measurements; V i Indicates the i The potential of the probe during the first measurement, P i Indicates i The differential capacitance of the probe under measurement.
[0110] Based on the current doping concentration, the capacitance-voltage data at different positions on the silicon substrate is measured by the measuring equipment. Based on this data, the internal B 3+ The exact position of , and combined with , Through the inversion algorithm, the basis function and superposition coefficient can be calculated, and based on this, the actual concentration at each location can be obtained.
[0111] Among them, the doping sensitivity function corresponding to the measuring device is preset or calculated, and the doping sensitivity function is a function of the internal position r of the device, which is used to reflect the sensitivity of the differential capacitance to the doping changes at different positions. Based on this doping sensitivity function, the formula Calculates the scalar product , where Ω represents B 3+ In the doping region on the silicon substrate, the doping region is determined, and this formula represents the basic function for the entire doping region. f k (r k ) And doping sensitivity function The product of is the definite integral, f k (r k ) represents the basis function under the kth superposition coefficient. Combined with the formula Calculate the superposition coefficient ak , and then use the formula Get the doping concentration change value N c (r) .
[0112] Step 608, iterating the current doping concentration based on the doping concentration change value, and updating the current doping concentration.
[0113] in, N i+1 (r) = N i (r)+N c (r) . The doping concentration can be changed by N c (r) and the doping concentration at the current iteration N i (r) The value obtained by superposition is N i+1 (r) As the new current doping concentration (ie, the doping concentration used in the next iteration), and determine whether to continue iteration.
[0114] Step 610 , checking whether the iteration termination condition is met, if so, executing step 612 , otherwise, returning to executing step 604 .
[0115] In this embodiment, it is possible to detect whether the calculated current doping concentration converges. When it converges, the iteration can be terminated, or it is detected whether the current number of iterations reaches the iteration number threshold. If so, the iteration can also be terminated. If it does not converge, or does not reach the iteration number threshold, i=i+1, and returns to step 604 to continue iterating according to the updated current doping concentration.
[0116] Step 612: Using the latest current doping concentration as the actual concentration at the corresponding position.
[0117] After the concentration at each position is determined, the doping depth can be determined based on the concentration. For example, when a position with a doping concentration of 0 is determined, the corresponding actual depth can be calculated based on the distance between the position and the silicon substrate.
[0118] In one embodiment, a computer-readable storage medium is provided, on which executable instructions are stored. When the instructions are executed by a processor, the processor executes the steps in the above-mentioned method embodiments.
[0119] In one embodiment, an integrated circuit device is also provided, the integrated circuit device comprising the PN junction formed by the above methods. For example, the integrated circuit device may be a device on an integrated circuit such as a diode, a triode, an octal buffer, etc.
[0120] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present application.
[0121] In addition, those skilled in the art will appreciate that, although some embodiments herein include certain features included in other embodiments but not other features, the combination of features of different embodiments is meant to be within the scope of the present application and form different embodiments. For example, in the above claims, any one of the claimed embodiments may be used in any combination. The information disclosed in this background technology section is intended only to deepen the understanding of the overall background technology of the present application and should not be regarded as an admission or in any form of implication that the information constitutes prior art known to those skilled in the art.
Claims
1. A PN junction forming method based on ion implantation, characterized in that: The method comprises: Determine the area to be doped and the standard concentration and depth of doping required on the silicon substrate after photolithography; B was screened out from the impurity source B2H6 by mass analyzer 3+ ; The B is implanted by a first ion implanter according to the corresponding dose and energy. 3+ implanting into the region to be doped; Annealing the doped area to form an initial PN junction; Calculating the errors between the actual concentration and actual depth of each doping region in the initial PN junction and the standard concentration and standard depth, and taking the doping region whose error exceeds the error threshold and whose area exceeds the first area threshold as the region to be compensated; The area to be compensated is subjected to B 3+ The method further comprises: determining, according to the compensation concentration and compensation depth required to be implanted in the area to be compensated, a compensation dose, a compensation energy and an implantation distance from the silicon substrate used by a second ion implanter for each single area in the area to be compensated, detecting the area of the single area, and for a single area whose area does not exceed a preset second area threshold, vertically implanting a compensation dose and a compensation energy B into the silicon substrate by the second ion implanter at a distance from the single area that does not exceed the preset second area threshold as a corresponding implantation distance. 3+ , for a single region whose area exceeds a preset second area threshold, a corresponding implantation angle is calculated according to the compensation concentration and the compensation depth at each position in the region to be compensated, and the second ion implanter is used to implant a dose of a corresponding compensation dose into the silicon substrate at a corresponding implantation angle and an energy of a corresponding compensation energy at a distance of a corresponding implantation distance from the single region exceeding the preset second area threshold. 3+ , the second area threshold is greater than the first area threshold, and the emission dose of the second ion implanter is less than the emission dose of the first ion implanter; To B 3+ The re-implanted region is annealed again to form a PN junction.
2. The method according to claim 1, characterized in that: The B is implanted by a first ion implanter according to the corresponding dose and energy. 3+ Implanting into the region to be doped comprises: Determine the injection times and the concentration and dosage of each injection according to the standard concentration and standard depth; The first ion implanter implants the doped area according to the determined number, concentration and dosage. 3+ injection.
3. The method according to claim 2, characterized in that The B is implanted by a first ion implanter according to the corresponding dose and energy. 3+ Implanting into the region to be doped comprises: Determining the implantation angle at each position in the region to be doped according to the standard concentration and the standard depth; The first ion implanter implants the B at the position in the to-be-doped area according to the corresponding implantation angle, corresponding dose and energy. 3+ implanted into the region to be doped.
4. The method according to claim 3, characterized in that When the first ion implanter moves relative to the first end of the area to be doped to the second end, the implantation angle gradually increases, and the corresponding implantation angle at the first end is less than 90°, and the implantation angle at the second end is greater than 90°. The implantation angle is the angle formed by the ion implantation direction and the movement direction of the silicon substrate relative to the first ion implanter.
5. The method according to claim 4, characterized in that When the first ion implanter moves relatively from the first end to the second end of the region to be doped, the dose and energy emitted are kept constant.
6. The method according to claim 4, characterized in that The method further comprises: Obtain the regional location and concentration of the historical area to be compensated; The implantation angle is corrected based on the position of the region and the concentration to be compensated.
7. The method according to any one of claims 1 to 6, characterized in that The step of annealing the doped region comprises: The silicon substrate is placed in a predetermined annealing temperature environment, and annealed in a pure oxygen environment for a first time, in a wet oxygen environment for a second time, and in a dry oxygen environment for a second time.
8. A computer-readable storage medium, characterized in that: The computer-readable storage medium stores executable instructions, and when the executable instructions are executed by a processor, the processor is enabled to perform the method according to any one of claims 1 to 7.
9. An integrated circuit device, characterized in that: The integrated circuit device comprises a PN junction formed by the method according to any one of claims 1 to 7.
Citation Information
Patent Citations
Fabrication of semiconductor device
JP2000058472A