Preparation method of high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control

By adopting multi-point temperature data acquisition and analysis in the preparation process of aluminum nitride ceramic heat conduction sheets, and using local variable coefficients and differential reference coefficients for temperature control, the problem of uneven temperature during traditional sintering is solved and the thermal conductivity is improved and preparation quality.

CN118619684BActive Publication Date: 2024-11-15HUNAN XIANGCI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411117952.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-11-15
Estimated Expiration
2044-08-15

AI Technical Summary

Technical Problem

The temperature is uneven during the sintering process of traditional aluminum nitride ceramic heat conduction sheets, resulting in the thermal conductivity not reaching the optimal level, affecting the preparation quality.

Method used

The preparation method based on parameter control is adopted, through ball milling, calcining, molding and hot pressing sintering, combined with multi-point temperature data acquisition and analysis, and the local variable coefficient and differential reference coefficient are used to control the temperature to ensure the temperature uniformity of the sintering process. .

Benefits of technology

The thermal conductivity of aluminum nitride ceramic heat conduction sheets is improved, the impact of temperature data error on preparation performance is reduced, stable parameter control is provided, and the preparation quality is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118619684B_ABST
    Figure CN118619684B_ABST
Patent Text Reader

Abstract

The present application relates to the field of preparation of aluminum nitride ceramic thermal conductive sheets, and specifically to a preparation method of high thermal conductivity aluminum nitride ceramic thermal conductive sheets based on parameter control. The method comprises: ball-milling a number of raw materials, drying and sieving them to obtain an intermediate powder; calcining and sieving the intermediate powder to obtain a mixed powder; secondary mixing the obtained mixed powder with a number of raw materials to obtain a mixed material; vacuum degassing the mixed material to obtain a ceramic slurry, and pressing the ceramic slurry to obtain a ceramic green sheet; applying an insulating powder to the ceramic green sheet and then removing the binder to obtain a vacuum-debinded ceramic green sheet; sintering the vacuum-debinded ceramic green sheet by heating and heat preservation, and then cooling, removing the powder and polishing to obtain a high thermal conductivity aluminum nitride ceramic thermal conductive sheet; during the heat preservation process, the temperature at this time is controlled by the temperature collected at different positions. The present application reduces the influence of temperature data error analysis on the preparation performance of aluminum nitride ceramic thermal conductive sheets and improves the preparation quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of preparation of aluminum nitride ceramic thermally conductive sheets, and specifically to a method for preparing high thermal conductivity aluminum nitride ceramic thermally conductive sheets based on parameter control. Background Art

[0002] Aluminum nitride ceramics have the characteristics of high thermal conductivity, good insulation, low dielectric constant, low dielectric loss, thermal expansion coefficient matching that of silicon, and good chemical stability. They are widely used in semiconductors and vacuum fields, and are also key materials for electronic components such as automotive electronics and aerospace. In order to meet the needs of the power electronics and electronic information industries, the thermal conductivity and insulation capabilities of materials are increasingly required, and aluminum nitride ceramics have high insulation and high heat dissipation properties and are widely used in insulating materials.

[0003] However, with the rapid development of electronic integration and packaging, electronic components and equipment are moving towards miniaturization and micro-miniaturization, which puts higher requirements on the performance of aluminum nitride ceramics. Therefore, it is necessary to further optimize and improve the preparation process of aluminum nitride ceramics to improve the performance of the prepared aluminum nitride ceramics. In the production process of aluminum nitride, in addition to high-quality raw materials, it is also necessary to accurately control the preparation parameters in the preparation process of aluminum nitride. The traditional preparation process of aluminum nitride ceramics includes batching, mixing, drying, molding and sintering. The traditional control accuracy of temperature and time of the sintering process is low. The uneven temperature causes the thermal conductivity of the aluminum nitride ceramic to not reach the optimal level within the set sintering time, affecting the quality of the finally prepared aluminum nitride ceramic thermal conductive sheet. Summary of the invention

[0004] In order to solve the technical problem of poor quality caused by uneven temperature, the present application provides a method for preparing a high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control. The technical solution adopted is as follows:

[0005] The present application proposes a method for preparing a high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control, the method comprising the following steps:

[0006] Aluminum nitride powder, calcium carbonate, lithium nitrate and ethanol are ball-milled and mixed, and then dried and sieved to obtain an intermediate powder;

[0007] The intermediate powder is calcined and sieved in a nitrogen environment to obtain a mixed powder; the mixed powder is mixed with molybdenum disulfide, a solvent, sodium polyacrylate, dimethyl phthalate, and an adhesive by secondary ball milling to obtain a mixed material;

[0008] The mixed material is vacuumed and degassed to obtain a ceramic slurry with a preset viscosity, the ceramic slurry is tape-casted and then cut, and the cut object is pressed to obtain a ceramic green sheet;

[0009] After applying the insulating powder on the ceramic green sheet, the green sheet is placed in a debinding furnace and heated and kept warm to obtain a ceramic green sheet after vacuum debinding;

[0010] The ceramic green sheet after vacuum debinding is placed in a hot pressing sintering furnace, and the heating and heat preservation process is continued to complete the sintering. After the sintering is completed, it is cooled to room temperature and powder is removed and polished to obtain a high thermal conductivity aluminum nitride ceramic thermal conductive sheet;

[0011] During the insulation process, the temperature is controlled as follows:

[0012] Collect all temperatures at different locations;

[0013] All temperatures at different positions are superimposed to obtain a superposition curve, the superposition curve is segmented, and all segments are sorted according to the standard deviation of all data in each segment, the maximum time and minimum time of each segment are used as segmentation points, and the data between the segmentation points are used as temperature superposition subsequences;

[0014] According to the temperature difference of different positions in the interval corresponding to the same temperature superposition subsequence, the local variation coefficient of each position in this interval is obtained;

[0015] The difference reference coefficient of each position is obtained by comparing the local variation coefficients of all intervals corresponding to different positions;

[0016] The sintering temperature is controlled according to the difference reference coefficients at different positions.

[0017] In the above scheme, aluminum nitride, calcium carbonate, lithium nitrate and other additives are mixed, calcined, formed and hot-pressed to prepare a high thermal conductivity aluminum nitride ceramic thermal conductive sheet. During the preparation process, the stability of the hot-pressing sintering process directly affects the performance of the aluminum nitride ceramic thermal conductive sheet finally prepared. During the hot-pressing sintering process of the aluminum nitride ceramic thermal conductive sheet, the performance of the thermal conductive sheet will vary within a small temperature change difference. Therefore, in order to analyze the temperature data during the hot-pressing sintering process using an automated control method, affected by the heat non-uniformity characteristics of the hot-pressing sintering, multiple temperature data collection points are set and The relative change influence of data at different temperature data collection points is analyzed. For different collection positions, the temperature uniformity of each position is analyzed. Based on the analysis results, the error analysis data of hot pressing sintering parameter control is screened and calculated. The beneficial effect is that it fully considers the problem of large parameter control errors that may be caused by the uneven heat distribution characteristics in the preparation process of aluminum nitride ceramic thermal conductive sheets, reduces the influence of temperature data error analysis on the preparation performance of aluminum nitride ceramic thermal conductive sheets, provides stable parameter control for the preparation of aluminum nitride ceramic thermal conductive sheets, and thus improves the performance of the prepared aluminum nitride ceramic thermal conductive sheets.

[0018] In one embodiment, in the process of obtaining the intermediate powder, the mass fraction interval of the aluminum nitride powder is [85, 87], the mass fraction interval of the calcium carbonate is [5, 7], and the mass fraction interval of the lithium nitrate is [3, 5].

[0019] In one embodiment, the specific method of obtaining the mixed material is:

[0020] The intermediate powder is calcined at 960-1000°C for 40-80 minutes, and the secondary mixing time is 12-18 hours. In the secondary mixing, the amount of molybdenum disulfide added is 30-40% of the mass of the mixed powder; the solvent in the secondary mixing is a mixture of anhydrous ethanol and isopropanol in a mass ratio of 1:1, and the amount of the solvent added is 40-55% of the mass of the mixed powder; in the secondary mixing, the amount of sodium polyacrylate added is 1.5-2.5% of the mass of the mixed powder; in the secondary mixing, the amount of dimethyl phthalate added is 0.5-0.8% of the mass of the mixed powder; in the secondary mixing, the adhesive is composed of polyvinyl butyral resin, ethylene acrylic acid copolymer and linear low-density polyethylene, wherein the mass fraction of the polyvinyl butyral resin is in the range of [20, 28], the mass fraction of the ethylene acrylic acid copolymer is in the range of [2, 2.5], the mass fraction of the linear low-density polyethylene is in the range of [20, 28], and the amount of the adhesive added is 2-3% of the mass of the mixed powder.

[0021] In one embodiment, in the process of obtaining ceramic green sheets, the ceramic slurry obtained after vacuum degassing is 12000-14000 mPa*s; the pressure during pressing in a cold isostatic press is 240-250 MPa, and the holding time is 8-10 min.

[0022] In one embodiment, when obtaining ceramic green sheets, the ceramic green sheets are first stacked and preheated at 130°C for 80 minutes, and then placed in a debinding furnace and heated to 280-320°C at a rate of 1-2°C / min, and kept warm for 2-2.5 hours; secondly, the temperature is increased to 420-460°C at a rate of 4-5°C / min, and kept warm for 1-2 hours, and finally the temperature is increased to 540-560°C at a rate of 3-4°C / min, and kept warm for 1-2 hours.

[0023] In one embodiment, when obtaining a high thermal conductivity aluminum nitride ceramic thermal conductive sheet, the ceramic green sheet after vacuum debinding is heated to 1000-1100°C at a heating rate of 3-4°C / min under a pressure of 40-50Mpa in a nitrogen environment, and after being kept warm for 1-2 hours, the temperature is further raised to 1700-1800°C. While heating, the pressure is increased to 90-100Mpa, and the temperature is kept and pressure is maintained for 5-8 hours.

[0024] In one embodiment, the method for obtaining the temperature superposition subsequence is:

[0025] For each acquisition position, all temperature values ​​are normalized and then fitted to obtain the local temperature curve of each acquisition position, and the normalized temperature values ​​of the local temperature curves of all positions at the same time are added to obtain a superposition curve;

[0026] The superimposed curve is divided into curve segments of preset time length, the standard deviation of the data values ​​of all data points in each curve segment is calculated, all standard deviations are sorted in order from large to small to select a preset number of curve segments, and the maximum time and minimum time of each selected curve segment are used as segmentation points; the superimposed curve is divided by all segmentation points, wherein the data between every two segmentation points is regarded as a temperature superposition subsequence.

[0027] In the above scheme, the time period in which the heat distribution may be uneven is screened out by analyzing the curves of all positions, and the time period in which the heat distribution is uneven is extracted and its characteristics are retained, so as to provide a basis for analyzing each subsequent time period.

[0028] In one embodiment, the method for obtaining the local variation coefficient of each position in the interval corresponding to the same temperature superposition subsequence according to the temperature difference of different positions in the interval is:

[0029] For each temperature superposition subsequence, the acquisition time of all data points corresponding to the temperature superposition subsequence constitutes the interval to be analyzed; the curve segment of the local temperature characteristic curve in the interval to be analyzed is recorded as the curve segment to be analyzed; in the same interval to be analyzed, the difference coefficient between any curve segment to be analyzed and all other curve segments to be analyzed is calculated by the DTW algorithm;

[0030] In the interval to be analyzed, any curve segment to be analyzed is recorded as the target curve segment, and the collinearity between the target curve segment and all other curve segments to be analyzed is used as the relative coefficient of the preparation process of the target curve segment, wherein the collinearity is obtained by the variance inflation factor;

[0031] The local variation coefficient of the target curve segment on the interval to be analyzed is obtained according to the preparation process relative coefficient and all difference coefficients of the target curve segment, wherein the local variation coefficient of the target curve segment is positively correlated with the difference coefficient, and the local variation coefficient is negatively correlated with the preparation process relative coefficient.

[0032] In the above scheme, in an interval to be analyzed, if there is no heat unevenness feature, the curve segments to be analyzed at other positions have the same change characteristics as the curve segments to be analyzed at the current analysis position, so the calculated variance expansion factor is larger; on the contrary, when the heat is uneven, the calculated variance expansion factor is smaller; at the same time, the relative coefficient of the preparation process is obtained by calculating the difference between the data points at each position and other positions. The larger the difference, the greater the degree of unevenness can be guaranteed; further, the local variation coefficient is obtained by calculating the ratio of the mean of all difference coefficients to the relative coefficient of the preparation process, and the unevenness characteristics can be reflected by analyzing the local feature differences. The larger the local variation coefficient, the greater the degree of unevenness of the heat distribution at that position in the interval to be analyzed.

[0033] In one embodiment, the method of obtaining the difference reference coefficient of each position by comparing the local variation coefficients in all intervals corresponding to different positions is:

[0034] For the local temperature curve at each position, the local variation coefficients of the local temperature curve in all the intervals to be analyzed are combined into a comparison set of local temperature curves; any local temperature curve is recorded as a target characteristic curve, and the difference comparison result between the target characteristic curve and the comparison set of each local temperature curve is used as the comparison coefficient between the target characteristic curve and each local temperature curve;

[0035] The average value of the contrast coefficient between the target characteristic curve and all other local temperature curves is taken as the aluminum nitride preparation process difference value of the target characteristic curve;

[0036] The accumulation of aluminum nitride preparation process difference values ​​of all local temperature curves is taken as the total difference value, and the ratio of the aluminum nitride preparation process difference value of each local temperature curve to the total difference value is taken as the difference reference coefficient of each local temperature curve.

[0037] In the above scheme, after analyzing the heat distribution unevenness of different intervals, all temperatures collected at each position are analyzed for heat unevenness according to the corresponding intervals, and the least affected position is selected to facilitate subsequent temperature control.

[0038] In one embodiment, the method for controlling the sintering temperature according to the difference reference coefficients at different positions is:

[0039] For each selected position, the difference between the temperature value of each selected position at the current moment and the set temperature value is calculated as the temperature difference value, the ratio of the difference reference coefficient of each selected position to the cumulative sum of the difference reference coefficients of all selected positions is used as the reference weight of each selected position, and the cumulative sum of the reference weights and temperature difference values ​​of all selected positions is used as the deviation value;

[0040] The temperature is regulated by a PID control system. The inputs to the PID control system are the set temperature and the deviation value to regulate the current temperature. Each time the temperature is regulated, the deviation value is recalculated to complete the temperature control.

[0041] The beneficial effects of this application are:

[0042] Aluminum nitride ceramic thermal conductive sheet with high thermal conductivity is prepared by mixing, calcining, molding and hot pressing sintering aluminum nitride, calcium carbonate, lithium nitrate and other additive materials. During the preparation process, the stability of the hot pressing sintering process directly affects the performance of the aluminum nitride ceramic thermal conductive sheet finally prepared. During the hot pressing sintering process of the aluminum nitride ceramic thermal conductive sheet, the performance of the thermal conductive sheet will be different within a small temperature change difference. Therefore, the temperature data analysis during the hot pressing sintering process is affected by the heat non-uniformity characteristics of the hot pressing sintering by using an automated control method. Multiple temperature data collection points are set and the relative change influence of the data at different temperature data collection points is analyzed. Based on the analysis results, the error analysis data of the hot pressing sintering parameter control is screened and calculated. The beneficial effect is that the problem of large parameter control error that may be caused by the heat distribution non-uniformity characteristics in the preparation process of the aluminum nitride ceramic thermal conductive sheet is fully considered, the influence of the temperature data error analysis on the preparation performance of the aluminum nitride ceramic thermal conductive sheet is reduced, and stable parameter control is provided for the preparation of the aluminum nitride ceramic thermal conductive sheet, thereby improving the performance of the prepared aluminum nitride ceramic thermal conductive sheet. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] In order to more clearly illustrate the technical solutions and advantages in the embodiments of the present application or the prior art, the drawings required for use in the embodiments or the prior art descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0044] Figure 1 A flow chart of a method for preparing a high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control provided in one embodiment of the present application;

[0045] Figure 2 The present invention is a flow chart of the heat preservation process in the step of preparing a high thermal conductivity aluminum nitride ceramic heat conductive sheet. DETAILED DESCRIPTION

[0046] In order to further explain the technical means and effects adopted by the present application to achieve the predetermined invention purpose, the following is a detailed description of the method for preparing the high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control proposed in the present application, its specific implementation method, structure, characteristics and effects, in combination with the accompanying drawings and preferred embodiments. In the following description, different "one embodiment" or "another embodiment" does not necessarily refer to the same embodiment. In addition, specific features, structures or characteristics in one or more embodiments may be combined in any suitable form.

[0047] Unless defined otherwise, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs.

[0048] Example of a method for preparing a high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control:

[0049] The specific scheme of the method for preparing the high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control provided by the present application is described in detail below in conjunction with the accompanying drawings.

[0050] See also Figure 1 , which shows a flow chart of a method for preparing a high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control provided by an embodiment of the present application, the method comprising the following steps:

[0051] Mix materials to prepare intermediate powders, add material A and material B into a ball mill for ball milling, preset the ball milling dispersion time, and obtain intermediate powders after ball milling through drying and sieving. Material A is a mixed material of aluminum nitride powder, calcium carbonate and lithium nitrate, material B is ethanol, and the mass ratio of material A to material B is 5:3.

[0052] Preferably, in one embodiment of the present application, the ball milling dispersion time is 6 hours, and the mass ratio of aluminum nitride, calcium carbonate and lithium nitrate is 85:5:3.

[0053] Preferably, in one embodiment of the present application, the ball milling dispersion time is 9 hours, and the mass ratio of aluminum nitride, calcium carbonate and lithium nitrate is 86:6:4.

[0054] Preferably, in one embodiment of the present application, the ball milling dispersion time is 12 hours, and the mass ratio of aluminum nitride, calcium carbonate and lithium nitrate is 87:7:5.

[0055] The intermediate powder is calcined to prepare a mixed material, and the intermediate powder is calcined at a preset temperature for a preset time in a nitrogen environment. After the calcination, the mixed powder is sieved to obtain a mixed powder; the mixed powder is added to a ball mill with molybdenum disulfide, a solvent, sodium polyacrylate, dimethyl phthalate, and an adhesive for secondary mixing, and after a preset time, a mixed material is obtained.

[0056] Preferably, in one embodiment of the present application, the intermediate powder is calcined at 960°C for 80 minutes, the secondary mixing time is 12 hours, and in the secondary mixing, the amount of molybdenum disulfide added is 30% of the mass of the mixed powder; the solvent in the secondary mixing is a mixture of anhydrous ethanol and isopropanol in a 1:1 mass ratio, and the amount of the solvent added is 40% of the mass of the mixed powder; in the secondary mixing, the amount of sodium polyacrylate added is 1.5% of the mass of the mixed powder; in the secondary mixing, the amount of dimethyl phthalate added is 0.5% of the mass of the mixed powder; in the secondary mixing, the adhesive is composed of polyvinyl butyral resin, ethylene acrylic acid copolymer and linear low-density polyethylene in a mass ratio of 20:3:2, and the amount of the adhesive added is 2% of the mass of the mixed powder.

[0057] Preferably, in one embodiment of the present application, the intermediate powder is calcined at 980°C for 60 minutes, the secondary mixing time is 15 hours, and in the secondary mixing, the amount of molybdenum disulfide added is 35% of the mass of the mixed powder; the solvent during the secondary mixing is a mixture of anhydrous ethanol and isopropanol in a 1:1 mass ratio, and the amount of the solvent added is 48% of the mass of the mixed powder; in the secondary mixing, the amount of sodium polyacrylate added is 2% of the mass of the mixed powder; in the secondary mixing, the amount of dimethyl phthalate added is 0.7% of the mass of the mixed powder; in the secondary mixing, the adhesive is composed of polyvinyl butyral resin, ethylene acrylic acid copolymer and linear low-density polyethylene in a mass ratio of 23:4:2.5, and the amount of the adhesive added is 2.5% of the mass of the mixed powder.

[0058] Preferably, in one embodiment of the present application, the intermediate powder is calcined at 1000°C for 40 minutes, the secondary mixing time is 18 hours, and in the secondary mixing, the amount of molybdenum disulfide added is 40% of the mass of the mixed powder; the solvent in the secondary mixing is a mixture of anhydrous ethanol and isopropanol in a 1:1 mass ratio, and the amount of the solvent added is 55% of the mass of the mixed powder; in the secondary mixing, the amount of sodium polyacrylate added is 2.5% of the mass of the mixed powder; in the secondary mixing, the amount of dimethyl phthalate added is 0.8% of the mass of the mixed powder; in the secondary mixing, the adhesive is composed of polyvinyl butyral resin, ethylene acrylic acid copolymer and linear low-density polyethylene in a mass ratio of 28:5:3.5, and the amount of the adhesive added is 3% of the mass of the mixed powder.

[0059] Prepare ceramic green sheets, vacuum degas the obtained mixed material in a vacuum degassing machine to obtain a ceramic slurry with a preset viscosity; obtain the obtained ceramic slurry by tape casting to obtain a ceramic green body, and then cut the ceramic green body into a required shape and size with a mold, put the obtained ceramic green body cut with the mold into a cold isostatic press for pressing, and obtain the ceramic green sheet after maintaining the preset pressure for a preset time.

[0060] Preferably, in one embodiment of the present application, the ceramic slurry obtained after vacuum degassing is 12000 mPa*s; the pressure during pressing in a cold isostatic press is 240 MPa, and the holding time is 10 min.

[0061] Preferably, in one embodiment of the present application, the ceramic slurry obtained after vacuum degassing is 13000 mPa*s; the pressure during pressing in a cold isostatic press is 245 MPa, and the holding time is 9 min.

[0062] Preferably, in one embodiment of the present application, the ceramic slurry obtained after vacuum degassing is 14000 mPa*s; the pressure during pressing in a cold isostatic press is 250 MPa, and the holding time is 8 min.

[0063] The debinding step of the ceramic green sheets is to apply a layer of anti-sticking powder on the surface of the obtained ceramic green sheets, stack the ceramic green sheets and treat them at a preset temperature for a preset time, then put them into a debinding furnace, heat them to a preset temperature and keep them warm for a preset time, and repeat the heating and keeping process until the debinding is completed.

[0064] Preferably, in one embodiment of the present application, the ceramic green sheets are stacked and preheated at 130°C for 80 minutes, then placed in a debinding furnace and heated to 280°C at a rate of 1°C / min, then kept warm for 2.5 hours, then heated to 420°C at a rate of 4°C / min, then kept warm for 2 hours, then heated to 540°C at a rate of 3°C / min, and then kept warm for 2 hours.

[0065] Preferably, in one embodiment of the present application, the ceramic green sheets are stacked and preheated at 130°C for 80 minutes, then placed in a debinding furnace and heated to 300°C at a rate of 1.5°C / min, then kept warm for 2.25 hours, then heated to 440°C at a rate of 4.5°C / min, then kept warm for 1.5 hours, then heated to 550°C at a rate of 3.5°C / min, and then kept warm for 1.5 hours.

[0066] Preferably, in one embodiment of the present application, the ceramic green sheets are stacked and preheated at 130°C for 80 minutes, then placed in a debinding furnace and heated to 320°C at a rate of 2°C / min, then kept warm for 2 hours, then heated to 450°C at a rate of 5°C / min, then kept warm for 1 hour, then heated to 560°C at a rate of 4°C / min, and then kept warm for 1 hour.

[0067] To prepare a high thermal conductivity aluminum nitride ceramic thermal conductive sheet, the ceramic green sheet after vacuum debinding is placed in a hot pressing sintering furnace, the temperature is raised to a preset temperature under a preset pressure in a nitrogen environment, and then the temperature is kept at a preset time. After the temperature is raised to the preset temperature, the pressure is increased while the temperature is raised, and then the sintering is completed after the preset time is kept at a preset temperature. After sintering, it is cooled to room temperature and then a powder removal and polishing process is performed to obtain a high thermal conductivity aluminum nitride ceramic thermal conductive sheet.

[0068] Preferably, in one embodiment of the present application, the ceramic green sheet after vacuum debinding is heated to 1000°C at a heating rate of 3°C / min under a pressure of 40Mpa in a nitrogen environment, and after being kept warm for 2 hours, the temperature is further raised to 1700°C. While heating, the pressure is increased to 90Mpa, and the temperature is kept warm and pressure maintained for 8 hours.

[0069] Preferably, in one embodiment of the present application, the ceramic green sheet after vacuum debinding is heated to 1050°C at a heating rate of 3.5°C / min under a pressure of 45Mpa in a nitrogen environment, and after being kept warm for 1.5 hours, the temperature is further raised to 1750°C. While heating, the pressure is increased to 95Mpa, and the temperature is kept warm and pressure maintained for 7 hours.

[0070] Preferably, in one embodiment of the present application, the ceramic green sheet after vacuum debinding is heated to 1100°C at a heating rate of 4°C / min under a pressure of 50Mpa in a nitrogen environment, and after being kept warm for 1 hour, the temperature is further raised to 1800°C. While heating, the pressure is increased to 100Mpa, and the temperature is kept and the pressure is maintained for 5 hours.

[0071] In the process of preparing high thermal conductivity aluminum nitride ceramic thermal conductive sheet, when the temperature is raised and then kept warm, it is necessary to keep the temperature within a fixed range, so the temperature needs to be controlled. The control process is as follows: Figure 2 As shown, the temperature control process is as follows:

[0072] S1, collect all temperatures at different locations.

[0073] In the hot pressing sintering furnace, the temperature needs to be kept warm during the sintering process. During the insulation process, the temperature accuracy directly affects the thermal conductivity of the finally prepared aluminum nitride ceramic thermal conductive sheet. Since there is uneven heat distribution in the sintering furnace, multiple thermocouples are used to collect the temperatures at different positions of the sintering furnace. The implementer can choose the position according to the appearance and size of the sintering furnace. For each thermocouple, a temperature data is collected every 0.1s. All the temperatures collected from the start of temperature collection to the current time constitute a local temperature sequence.

[0074] Preferably, in one embodiment of the present application, two thermocouples are placed on both sides of the sintering furnace, that is, a total of four thermocouples are placed to measure data.

[0075] At this point, the local temperature series is obtained.

[0076] S2, superimpose all temperatures at different positions, and divide all temperatures into intervals according to the local standard deviation of the superimposed temperatures to obtain a temperature superposition subsequence.

[0077] Generally, during the preparation of aluminum nitride, the performance of aluminum nitride ceramic thermal conductive sheets prepared at different temperatures varies greatly, and the temperature control accuracy during hot pressing and sintering greatly affects the performance of the obtained aluminum nitride ceramic thermal conductive sheet. During the hot pressing and sintering process, using a separate thermocouple to collect the temperature in the furnace for deviation analysis and temperature control will ignore the problem of large deviation analysis errors caused by uneven heat distribution, which will reduce the stability of control during the preparation of aluminum nitride ceramic thermal conductive sheets.

[0078] Furthermore, due to the uneven heat transfer characteristics in the furnace during the sintering of the aluminum nitride ceramic thermal conductive sheet, the temperature changes at different positions during the hot pressing sintering of the aluminum nitride are quite different. Therefore, the intervals can be divided according to the consistency of the temperature changes at different positions during the hot pressing sintering process, and the differences in the uniformity of the temperature changes can be analyzed based on the division of different intervals.

[0079] Specifically, in a sintering furnace, all temperatures collected at each position are sorted in chronological order to obtain a local temperature sequence, and all temperature values ​​in the local temperature sequence are normalized by a linear normalization method, all normalized temperature values ​​are mapped to a two-dimensional rectangular coordinate system to obtain a local temperature curve, and all local temperature curves corresponding to all positions are superimposed to obtain a superposition curve; wherein the superposition method is to add the normalized temperature values ​​corresponding to the same time point at different positions as the superposition value of the time point, and use the curve composed of all superposition values ​​as the superposition curve.

[0080] It should be noted that, in this embodiment, the purpose of linear normalization is only to normalize all temperature values ​​in the local temperature sequence, and the implementer may also use other normalization algorithms for processing, such as maximum and minimum value normalization.

[0081] The intervals are divided according to the peak change difference of the superposition curve, and the time length of the time interval is preset. The first time of the first time interval is the time when sintering starts, and the moving step length of the time interval is the time length of the time interval. The superposition curve is divided into several time intervals, and the time length of the last time interval is determined by the number of elements contained. The standard deviation of the data value corresponding to the data point of the superposition curve in each time interval is calculated, that is, the standard deviation of each time interval, and all standard deviations are sorted from large to small. A preset number of time intervals are selected in order as characteristic time intervals, and the maximum time and minimum time of each characteristic time interval are obtained. These two time points are used as segmentation points, and the superposition curve is segmented through all segmentation points to obtain several temperature superposition subsequences, and the data between every two segmentation points is used as a temperature superposition subsequence.

[0082] Preferably, in one embodiment of the present application, the time length of the time interval is set to 1 minute, that is, the moving step of the time interval is also 1 minute; after sorting the standard deviations of all time intervals from large to small, 30% of the number of all time intervals are selected from large to small as feature time intervals. It should be noted that if 30% of the number of all time intervals is not an integer, it is rounded up.

[0083] Among them, the maximum time and minimum time in the characteristic time interval are used as segmentation points, and the temperature curve segment corresponding to the characteristic time interval can be segmented out, and the temperature curve segment corresponding to the characteristic time interval is recorded as the characteristic curve segment. The larger the standard deviation of the data values ​​of all data points in the characteristic curve segment, the more likely the corresponding characteristic time interval is to be a time period with uneven heat distribution. These characteristic curve segments that may be uneven heat distribution are divided out, and the characteristics of the interval are retained, thereby obtaining the heat distribution of each interval.

[0084] So far, several temperature superposition subsequences have been obtained.

[0085] S3, obtaining the local variation coefficient of each position in the interval according to the temperature difference of different positions in the interval corresponding to the same temperature superposition subsequence.

[0086] In the hot pressing sintering process of aluminum nitride, the temperature of all positions is integrated and superimposed, and then the area is divided. After superposition, if the temperature changes greatly in a certain time interval, it is considered that the temperature is uneven in this time interval. The temperature superposition subsequence obtained above retains the time interval with large differences, and the temperature changes of different acquisition positions in different time intervals are different. According to the interval division results, the relative change relationship of the temperature at each position is further analyzed to determine the local variation coefficient of each divided interval in the preparation process of aluminum nitride. The local variation coefficient reflects the regional relative difference characteristics of the sintering temperature of aluminum nitride ceramic thermal conductive sheet.

[0087] Specifically, for each temperature superposition subsequence, the interval formed by the acquisition time of all data points corresponding to the temperature superposition subsequence is recorded as the interval to be analyzed. The curve segment of any local temperature curve in the interval to be analyzed is recorded as the curve segment to be analyzed; in the same interval to be analyzed, the difference coefficient between any curve segment to be analyzed and all other curve segments to be analyzed is calculated. The difference coefficient reflects the relative temperature fluctuation difference of the curve segment to be analyzed.

[0088] Preferably, in one embodiment of the present application, the dtw values ​​of the two curve segments to be analyzed are calculated by the dtw algorithm, and the dtw values ​​are used as the difference coefficients of the two curve segments to be analyzed.

[0089] In the interval to be analyzed, any curve segment to be analyzed is recorded as the target curve segment, and the collinearity difference between the target curve segment and all other curve segments to be analyzed is used as the relative coefficient of the preparation process; the collinearity between the target curve segment and all other curve segments to be analyzed can be obtained through the variance inflation factor, and the collinearity between the target curve segment and all other curve segments to be analyzed is used as the relative coefficient of the preparation process of the target curve segment.

[0090] Taking the target curve segment as an example, the input of the variance inflation factor is all the data points in the target curve segment, the data used for analysis is all the data points of the remaining curve segments to be analyzed, and the output is the collinearity of the target curve segment and the remaining curve segments to be analyzed.

[0091] The local variation coefficient of the target curve segment on the interval to be analyzed is obtained according to the preparation process relative coefficient of the target curve segment and all the difference coefficients.

[0092] There is a positive correlation between the local variation coefficient of the target curve segment and the difference coefficient between the target curve segment and all other curve segments to be analyzed, and there is a negative correlation between the local variation coefficient of the target curve segment and the relative coefficient of the preparation process of the target curve segment.

[0093] Preferably, in one embodiment of the present application, the ratio of the mean of the difference coefficients between the target curve segment and all other curve segments to be analyzed to the relative coefficient of the preparation process of the target curve segment is used as the local variation coefficient of the target curve segment.

[0094] Preferably, in one embodiment of the present application, the difference between the mean of the difference coefficients between the target curve segment and all other curve segments to be analyzed and the relative coefficient of the preparation process of the target curve segment is used as the local variation coefficient of the target curve segment.

[0095] It should be noted that positive correlation means that when one variable increases, the other variable also increases, and the two variables change in the same direction. When one variable changes from large to small or from small to large, the other variable also changes from large to small or from small to large. The specific relationship can be a multiplication relationship, an addition relationship, or the idempotence of an exponential function, which is determined by actual application and is not specifically limited in this application.

[0096] It should be noted that negative correlation means that as one variable increases, the other variable decreases accordingly, and the two variables change in opposite directions. When one variable changes from large to small or from small to large, the other variable also changes from small to large or from large to small. The specific relationship can be a ratio relationship, a subtraction relationship, etc., which is determined by actual application, and this application does not impose any special restrictions.

[0097] In an interval to be analyzed, if there is no heat unevenness feature, the curve segments to be analyzed at other positions have the same change characteristics as the curve segments to be analyzed at the current analysis position, so the calculated variance expansion factor is larger; on the contrary, when the heat is uneven, the calculated variance expansion factor is smaller; at the same time, the relative coefficient of the preparation process is obtained by calculating the difference between the data points at each position and other positions. The larger the difference, the greater the degree of unevenness can be guaranteed; further, the local variation coefficient is obtained by calculating the ratio of the mean of all difference coefficients to the relative coefficient of the preparation process. The unevenness characteristics can be reflected by analyzing the local feature differences. The larger the local variation coefficient, the greater the degree of unevenness of the heat distribution at that position in the interval to be analyzed.

[0098] At this point, the local variation coefficient of the local temperature curve at each position in an interval to be analyzed is obtained.

[0099] S4, obtaining a difference reference coefficient for each position by comparing the local variation coefficients on all intervals corresponding to different positions.

[0100] Normally, the temperature data obtained during the hot pressing and sintering process of aluminum nitride ceramic thermal conductive sheet will not have local area differences, that is, the changes in temperature collected at different positions should be similar. However, the presence of non-uniform heat change characteristics will lead to differences in the changes in temperature collected at different positions. The collected temperature data cannot accurately reflect the temperature error in the furnace, which in turn affects the temperature control accuracy, resulting in unstable temperature change linearity of the hot pressing and sintering temperature, affecting the performance of the prepared aluminum nitride ceramic thermal conductive sheet.

[0101] Therefore, the degree to which the temperature data obtained at each location collection point is affected by the characteristics of heat distribution non-uniformity can be further reflected by comparing the differences in local change characteristics of different intervals to be analyzed. Therefore, the difference value of the aluminum nitride preparation process is calculated based on the relative difference in the local change coefficients of different location collection points in the interval to be analyzed.

[0102] Specifically, for the local temperature curve at each position, a set consisting of local variation coefficients of the local temperature curve in all intervals to be analyzed is used as a comparison set of the local temperature curves; any local temperature curve is recorded as a target characteristic curve, and a difference comparison result between the target characteristic curve and the comparison set of each local temperature curve is used as a comparison coefficient between the target characteristic curve and each local temperature curve.

[0103] Preferably, in one embodiment of the present application, the difference comparison result of the comparison set of the target characteristic curve and the local temperature curve is represented by the Jaccard coefficient between the two sets.

[0104] The greater the difference between the target characteristic curve and the local temperature curve, the greater the contrast coefficient. The average of the contrast coefficients between the target characteristic curve and all other local temperature curves is taken as the aluminum nitride preparation process difference value of the target characteristic curve.

[0105] The greater the difference value of the aluminum nitride preparation process, the greater the difference between each local temperature curve and the other local temperature curves, and the more likely the curve is to be affected by the uneven heat distribution, that is, the collection point is greatly affected by the uneven characteristics of hot pressing sintering.

[0106] Furthermore, the aluminum nitride preparation process difference value obtained through the above calculation reflects the relative influence of each position collection point on the control of sintering temperature stability during the hot pressing sintering process. The more uneven the heat distribution is, the weaker the control ability of temperature stability is. Therefore, the difference reference coefficient is obtained through the aluminum nitride preparation process difference value, and the collection points at different positions in the sintering furnace are screened through the difference reference coefficient to obtain the position least affected by the heat unevenness.

[0107] The aluminum nitride preparation process difference values ​​corresponding to all local temperature curves are accumulated as the total difference value, and the ratio of the aluminum nitride preparation process difference value of each local temperature curve to the total difference value is used as the difference reference coefficient of each local temperature curve.

[0108] At this point, the difference reference coefficient of each local temperature curve is obtained.

[0109] S5, controlling the sintering temperature according to the difference reference coefficients at different positions.

[0110] Normally, the temperature of hot pressing sintering during the preparation of aluminum nitride ceramic thermal conductive sheets is controlled by obtaining real-time temperature data through a single data acquisition device and then adjusting the parameters. This control method is easily affected by the heat unevenness characteristics during the hot pressing sintering process. Therefore, multiple temperature acquisition devices are set up, and the heat distribution uniformity of each position is obtained through the above analysis of all positions, and based on the heat distribution uniformity of different positions, the positions with more uniform distribution are screened out, and the temperature is controlled accordingly.

[0111] Specifically, the difference reference coefficients corresponding to all positions are sorted from small to large. Since the smaller the difference reference coefficient, the less the temperature of the position is affected by the uneven heat distribution characteristics, a preset number of positions with the smallest difference reference coefficients are selected as the calculation objects of the negative feedback difference of parameter control.

[0112] Preferably, in one embodiment of the present application, two positions with the smallest difference reference coefficients are selected.

[0113] This embodiment uses a PID control system to regulate the temperature. The inputs in the PID control system are a set temperature and a deviation value. The deviation value in traditional PID control is the difference between the current temperature value and the set temperature value. In this application, temperatures at multiple locations are collected, which results in multiple temperature values ​​at the current moment, and locations that are severely affected by uneven heat distribution need to be excluded.

[0114] At the current moment, the deviation value is obtained according to the temperature values ​​of a preset number of positions with the smallest difference reference coefficient.

[0115] Preferably, in one embodiment of the present application, the two positions with the smallest difference reference coefficients correspond to a temperature value, respectively, recorded as the first temperature and the second temperature, and the difference reference coefficients corresponding to the corresponding positions are recorded as the first reference coefficient and the second reference coefficient, respectively; the absolute value of the difference between the first temperature and the set temperature is taken as the first temperature difference, the sum of the first reference coefficient and the second reference coefficient is recorded as the total reference coefficient, and the ratio of the first reference coefficient to the total reference coefficient is taken as the first reference weight; the absolute value of the difference between the second temperature and the set temperature is taken as the second temperature difference, the ratio of the second reference coefficient to the total reference coefficient is taken as the second reference weight, the product of the first reference coefficient and the first temperature difference is recorded as the first product, the product of the second reference coefficient and the second temperature difference is recorded as the second product, and the sum of the first product and the second product is the deviation value.

[0116] The parameter setting process of the PID controller can be obtained by using a parameter setting method such as a trial and error method or a decay curve method. PID control is a well-known technology and is not described in detail in this application. Thus, the current temperature is adjusted to the set temperature through the deviation value through the proportion, integration, and differentiation of the PID control. The deviation value is recalculated each time the temperature value is adjusted to complete the temperature control.

[0117] It should be noted that the above-described embodiments are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. These modifications or replacements do not deviate the essence of the corresponding technical solutions from the scope of the technical solutions of the embodiments of the present application, and should all be included in the protection scope of the present application.

[0118] The various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referenced to each other, and each embodiment focuses on the differences from other embodiments.

Claims

1. Preparation method of high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control, It is characterized in that The method comprises the following steps: Aluminum nitride powder, calcium carbonate, lithium nitrate and ethanol are ball-milled and mixed, and then dried and sieved to obtain an intermediate powder; The intermediate powder is calcined and sieved in a nitrogen environment to obtain a mixed powder; the mixed powder is mixed with molybdenum disulfide, a solvent, sodium polyacrylate, dimethyl phthalate, and an adhesive by secondary ball milling to obtain a mixed material; The mixed material is vacuumed and degassed to obtain a ceramic slurry with a preset viscosity, the ceramic slurry is tape-casted and then cut, and the cut object is pressed to obtain a ceramic green sheet; After applying the insulating powder on the ceramic green sheet, the green sheet is placed in a debinding furnace and heated and kept warm to obtain a ceramic green sheet after vacuum debinding; The ceramic green sheet after vacuum debinding is placed in a hot pressing sintering furnace, and the heating and heat preservation process is continued to complete the sintering. After the sintering is completed, it is cooled to room temperature and powder is removed and polished to obtain a high thermal conductivity aluminum nitride ceramic thermal conductive sheet; During the insulation process, the temperature is controlled as follows: Collect all temperatures at different locations; All temperatures at different positions are superimposed to obtain a superposition curve, the superposition curve is segmented, and all segments are sorted according to the standard deviation of all data in each segment, a preset number of time intervals are selected in descending order of standard deviation as characteristic time intervals, the maximum time and minimum time of each characteristic time interval are obtained, the maximum time and minimum time of each segment are used as segmentation points, and the data between the segmentation points are used as temperature superposition subsequences; According to the temperature difference of different positions in the interval corresponding to the same temperature superposition subsequence, the local variation coefficient of each position in this interval is obtained; For each temperature superposition subsequence, the acquisition time of all data points corresponding to the temperature superposition subsequence constitutes the interval to be analyzed; the curve segment of the local temperature characteristic curve in the interval to be analyzed is recorded as the curve segment to be analyzed; in the same interval to be analyzed, the difference coefficient between any curve segment to be analyzed and all other curve segments to be analyzed is calculated by the DTW algorithm; In the interval to be analyzed, any curve segment to be analyzed is recorded as the target curve segment, and the collinearity between the target curve segment and all other curve segments to be analyzed is used as the relative coefficient of the preparation process of the target curve segment, wherein the collinearity is obtained by the variance inflation factor; Obtaining a local variation coefficient of the target curve segment on the interval to be analyzed according to the preparation process relative coefficient and all difference coefficients of the target curve segment, wherein the local variation coefficient of the target curve segment is positively correlated with the difference coefficient, and the local variation coefficient is negatively correlated with the preparation process relative coefficient; The difference reference coefficient of each position is obtained by comparing the local variation coefficients of all intervals corresponding to different positions; For the local temperature curve at each position, the local variation coefficients of the local temperature curve in all the intervals to be analyzed are combined into a comparison set of local temperature curves; any local temperature curve is recorded as a target characteristic curve, and the difference comparison result between the target characteristic curve and the comparison set of each local temperature curve is used as the comparison coefficient between the target characteristic curve and each local temperature curve; The average value of the contrast coefficient between the target characteristic curve and all other local temperature curves is taken as the aluminum nitride preparation process difference value of the target characteristic curve; The sum of the aluminum nitride preparation process difference values ​​of all local temperature curves is taken as the total difference value, and the ratio of the aluminum nitride preparation process difference value of each local temperature curve to the total difference value is taken as the difference reference coefficient of each local temperature curve; The sintering temperature is controlled according to the difference reference coefficients at different positions; Sort the difference reference coefficients corresponding to all positions from small to large, and select a preset number of positions with the smallest difference reference coefficients as the selected positions for parameter control; For each selected position, the difference between the temperature value of each selected position at the current moment and the set temperature value is calculated as the temperature difference value, the ratio of the difference reference coefficient of each selected position to the cumulative sum of the difference reference coefficients of all selected positions is used as the reference weight of each selected position, and the cumulative sum of the reference weights and temperature difference values ​​of all selected positions is used as the deviation value; The temperature is regulated by a PID control system. The inputs to the PID control system are the set temperature and the deviation value to regulate the current temperature. Each time the temperature is regulated, the deviation value is recalculated to complete the temperature control.

2. The method for preparing the high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control according to claim 1, It is characterized in that In the process of obtaining the intermediate powder, the mass fraction range of aluminum nitride powder is [85, 87], the mass fraction range of calcium carbonate is [5, 7], and the mass fraction range of lithium nitrate is [3, 5].

3. The method for preparing the high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control according to claim 1, It is characterized in that The specific method for obtaining the mixed material is: The intermediate powder is calcined at 960-1000°C for 40-80 minutes, and the secondary mixing time is 12-18 hours. In the secondary mixing, the amount of molybdenum disulfide added is 30-40% of the mass of the mixed powder; the solvent in the secondary mixing is a mixture of anhydrous ethanol and isopropanol in a mass ratio of 1:1, and the amount of the solvent added is 40-55% of the mass of the mixed powder; in the secondary mixing, the amount of sodium polyacrylate added is 1.5-2.5% of the mass of the mixed powder; in the secondary mixing, the amount of dimethyl phthalate added is 0.5-0.8% of the mass of the mixed powder; in the secondary mixing, the adhesive is composed of polyvinyl butyral resin, ethylene acrylic acid copolymer and linear low-density polyethylene, wherein the mass fraction of the polyvinyl butyral resin is in the range of [20, 28], the mass fraction of the ethylene acrylic acid copolymer is in the range of [2, 2.5], the mass fraction of the linear low-density polyethylene is in the range of [20, 28], and the amount of the adhesive added is 2-3% of the mass of the mixed powder.

4. The method for preparing a high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control according to claim 1, It is characterized in that In the process of obtaining ceramic green sheets, the ceramic slurry obtained after vacuum degassing is 12000-14000mPa*s; the pressure during pressing in the cold isostatic press is 240-250MPa, and the holding time is 8-10min.

5. The method for preparing a high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control according to claim 1, It is characterized in that When obtaining ceramic green sheets, first stack the ceramic green sheets and preheat them at 130°C for 80 minutes, then place them in a debinding furnace and heat them to 280-320°C at a rate of 1-2°C / min, and keep them warm for 2-2.5 hours; secondly, heat them to 420-460°C at a rate of 4-5°C / min, and keep them warm for 1-2 hours, and finally heat them to 540-560°C at a rate of 3-4°C / min, and keep them warm for 1-2 hours.

6. The method for preparing a high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control according to claim 1, It is characterized in that When obtaining a high thermal conductivity aluminum nitride ceramic thermal conductive sheet, the ceramic green sheet after vacuum debinding is heated to 1000-1100°C at a heating rate of 3-4°C / min under a pressure of 40-50Mpa in a nitrogen environment, and after keeping warm for 1-2 hours, the temperature is further raised to 1700-1800°C. While heating, the pressure is increased to 90-100Mpa, and the temperature and pressure are kept warm and maintained for 5-8 hours.

7. The method for preparing a high thermal conductivity aluminum nitride ceramic thermal conductive sheet based on parameter control according to claim 1, It is characterized in that The method for obtaining the temperature superposition subsequence is: For each acquisition position, all temperature values ​​are normalized and then fitted to obtain the local temperature curve of each acquisition position, and the normalized temperature values ​​of the local temperature curves of all positions at the same time are added to obtain a superposition curve; The superimposed curve is divided into curve segments of preset time length, the standard deviation of the data values ​​of all data points in each curve segment is calculated, all standard deviations are sorted in descending order to select a preset number of curve segments, and the maximum time and minimum time of each selected curve segment are used as the segmentation points; The superposition curve is divided at all division points, wherein the data between every two division points is a temperature superposition subsequence.