A method for on-site removal of existing concrete columns

By detecting and dividing the defects of concrete columns and dismantling them by cutting devices, the problems of low efficiency and waste of resources in traditional methods are solved, and the efficient demolition of concrete columns and effective utilization of resources are achieved, which is suitable for the regeneration needs of different buildings. .

CN118622046BActive Publication Date: 2024-11-12SHANGHAI CONSTRUCTION FOURTH CONSTRUCTION GROUP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411102695.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-11-12
Estimated Expiration
2044-08-13

AI Technical Summary

Technical Problem

The prior art is inefficient and prone to waste of resources when dismantling existing concrete columns, and it is difficult for traditional methods to obtain complete concrete blocks to achieve regeneration.

Method used

Through defect detection and marking partitioning, the critical size of the defect is determined, the concrete column is divided into defect zones and regeneration zones, and the cutting device is used to remove them to obtain renewable segments to achieve effective utilization of resources.

Benefits of technology

It realizes efficient demolition of concrete columns and maximizes resource utilization, ensures the completeness of components and construction efficiency, and is suitable for the recycling needs of different buildings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118622046B_ABST
    Figure CN118622046B_ABST
Patent Text Reader

Abstract

The present invention discloses a method for on-site demolition of existing concrete columns, which belongs to the field of green building demolition technology, and includes: demolition preparation, determining the critical size of defects according to the size characteristics of the existing concrete columns, obtaining the size D of the concrete regeneration segment, wherein the critical size of defects includes the first critical size of defects and the second critical size of defects; defect detection, detecting the defects of the concrete column, marking the defect positions, and marking the second defect and the third defect separately; primary marking, marking the concrete surface according to the positions of the defects marked on the concrete column, and dividing the concrete column into a defect area and a regeneration area; secondary marking, marking the regeneration area according to the size and shape of the concrete regeneration segment, and dividing the regeneration area into a regeneration segment area and an edge area; and finally demolition. The method disclosed by the present invention can be used to dismantle suitable concrete blocks as needed, which is convenient for recycling and reuse of the regenerated concrete columns.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of green building demolition, and in particular relates to an on-site demolition method for an existing concrete column. Background Art

[0002] In the field of modern architecture, with the development of cities and the renewal of building structures, the demand for the demolition of existing concrete columns is increasing. In the past, traditional demolition methods often relied on manual chiseling or blasting. Manual chiseling is inefficient, and although blasting can quickly demolish, it is easy to cause great impact and damage to the surrounding environment and buildings. Although the above demolition method can also quickly demolish concrete columns, most of the concrete columns after demolition are not complete blocks and cannot be used modularly again, which easily leads to waste of resources. Summary of the invention

[0003] In view of this, an object of the present invention is to provide an on-site dismantling method for existing concrete columns, which can be dismantled to obtain suitable concrete blocks as needed, thereby facilitating the recycling and reuse of the regenerated concrete columns.

[0004] In order to achieve the above object, the present invention provides the following technical solutions:

[0005] The present invention discloses a method for on-site removal of existing concrete columns, comprising:

[0006] Demolition preparation, determine the critical size of the defect according to the size characteristics of the existing concrete column, and obtain the size D of the concrete regeneration segment, where the critical size of the defect includes the first critical size of the defect and the second critical size of the defect. There are three sizes of defects, including the first defect, the second defect and the third defect, where 0<first defect<first defect critical size<second defect<second defect critical size<third defect;

[0007] Defect detection: detect defects in concrete columns, mark defect locations, and mark the second and third defects separately;

[0008] One-time marking: according to the position of the defects marked on the concrete column, the concrete column is divided into defect area and regeneration area by marking on the concrete surface;

[0009] Secondary marking: according to the size and shape of the concrete regeneration segment, marking is done in the regeneration area to divide the regeneration area into a regeneration segment area and an edge area;

[0010] Demolition: According to the layout conditions, the existing concrete columns are demolished to obtain concrete recycled segments.

[0011] Furthermore, during one marking, the defect area and the regeneration area are marked along the axial direction of the concrete column, and by observing the marked position of the concrete column, a plurality of defect-intensive areas with marked defects distributed along the axial direction are obtained; each defect-intensive area is confined to a corresponding defect area.

[0012] Furthermore, when defining the defect-dense area, by observing the density of defect positions in the marked area and then comparing them one by one, the two points located on the outermost side of the dense area are found, and the two circles formed by encircling the two points with the center line of the concrete column as the axis are defined as the boundary lines of the defect area, thereby limiting the defect-dense area to a defect area.

[0013] Furthermore, there are at least N defect marks in the defect-intensive area, and the distance between two adjacent defect marks is less than D / 10, where N≥3, and the remaining defect marks are discrete defects. When the discrete defect belongs to the third defect, it is divided into a separate defect area.

[0014] Further, when the discrete defect belongs to the second defect, it is classified into the regeneration zone.

[0015] Furthermore, for discrete defects whose sizes belong to the second defect, they are repaired before the concrete column is dismantled.

[0016] Furthermore, during the secondary scribing, the edge area is divided to be adjacent to the defect area.

[0017] Furthermore, when dismantling the concrete column, cutting or breaking is adopted.

[0018] Furthermore, the defect position is marked by punching.

[0019] Furthermore, a cutting device is used to dismantle the concrete column. The cutting device includes a cutting rope, a wire feeding wheel for cooperating with the cutting rope, and a motor for driving the wire feeding wheel to rotate. The cutting device also includes a bracket, a hydraulic cylinder, a bottom support, and a sliding drive device. The motor is slidably installed on the bracket, and a sliding drive device for driving the motor to slide along the bracket is installed on the bracket. One side of the bracket is hinged to the bottom support, and a hydraulic cylinder for driving the bracket to flip is installed on the bottom support.

[0020] The beneficial effects of the present invention are:

[0021] The present invention discloses an on-site demolition method for an existing concrete column. Before the existing concrete column is demolished, defect detection and identification are first performed on the existing concrete column. According to the identification result, the intact cutting position and angle are determined to facilitate the subsequent better utilization of the demolished components. This can ensure the best degree of resource conservation while ensuring the completeness of component demolition and use.

[0022] In the device disclosed in the present invention, the first defect critical size and the second defect critical size can be preset as needed to meet the recycling needs of different buildings. When facing more stringent building recycling, a more stringent first defect critical size can be selected. At this time, the size of the first defect critical size is smaller, and there are only small cracks and other defects on the complete recycling segment. The possibility of repeated processing during reuse is small, so the construction efficiency can be guaranteed, and the completeness of the building use can also be guaranteed.

[0023] When faced with semi-prefabricated segmental recycled concrete columns, the requirements for the recycled segments are not so strict. Since they need to be coordinated with cast-in-place, some small cracks are allowed on the recycled segments to maximize the use of resources.

[0024] Other advantages, objectives and features of the present invention will be described in the following description and will be apparent to those skilled in the art to some extent, or those skilled in the art may be taught from the practice of the present invention. The objectives and other advantages of the present invention may be realized and obtained through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to make the purpose, technical solution and beneficial effects of the present invention clearer, the present invention provides the following drawings for illustration:

[0026] Figure 1 It is a construction flow chart of the demolition method of the present invention;

[0027] Figure 2 It is a regional division diagram of the present invention;

[0028] Figure 3 This is a schematic structural diagram of the cutting device of Example 2;

[0029] Figure 4 This is the front view of the cutting device of Example 2.

[0030] The markings in the accompanying drawings are as follows: concrete column 1, first defect 2, second defect 3, third defect 4, defect area 5, regeneration segment area 6, edge area 7, cutting rope 8, wire feeding wheel 9, motor 10, bracket 11, hydraulic cylinder 12, bottom support 13, sliding drive device 14, square hoop 15, slide rail 16, clamping wheel 17, sliding shaft 18, telescopic device 19. DETAILED DESCRIPTION

[0031] Embodiment 1, as Figure 1 and 2 As shown, the present invention discloses a method for on-site removal of an existing concrete column. The existing concrete column 1 is cylindrical. The specific removal method includes:

[0032] Demolition preparation, prepare the necessary tools and materials, including measuring tools and protective equipment, ensure the safety of the work area, and clear obstacles around the column. Determine the critical size of the defect based on the dimensional characteristics of the existing concrete column 1, and obtain the size of the concrete regeneration segment D = 1000mm. The critical size of the defect includes the first critical size of 10mm and the second critical size of 25mm. There are three sizes of defects, including the first defect 2, the second defect 3 and the third defect 4, among which 0<first defect 2<first defect critical size<second defect 3<second defect critical size<third defect 4. The above sizes are the maximum sizes of the defects measured in a straight line distance.

[0033] Defect detection, detect the defects of the concrete column 1, mark the defect position, mark the two defect sizes separately, and detect the defects inside the concrete, such as cracks, cavities, looseness, etc., by transmitting and receiving the propagation of ultrasonic waves in the concrete. Parameters such as the propagation speed, amplitude and frequency of ultrasonic waves can be measured to analyze the quality of concrete. The embodiment of the present invention marks the defect position by marking or punching, and marks the two defect sizes separately, which is convenient for subsequent identification.

[0034] One-time marking: according to the positions of the defects marked on the concrete column 1, marking is performed on the concrete surface along the circumference of the concrete column 1 to divide the concrete column 1 into a defect area 5 and a regeneration area. The defect area 5 mainly includes an area with multiple defects, which is subsequently used to generate concrete aggregates, and the regeneration area is subsequently used to generate reusable concrete blocks, which can save resources.

[0035] During the secondary marking, according to the size and shape of the concrete regeneration segment, the regeneration area is marked to divide the regeneration area into a regeneration segment area 6 and an edge area 7. Since the length of the regeneration segment needs to be determined in advance during design, as many regeneration segment areas 6 as possible are accommodated in one regeneration area so that resources can be fully utilized. Although the edge area 7 is also complete, it is a scrap that needs to be discarded, and it can also be used as a surplus when cutting.

[0036] Finally, the existing concrete column 1 is dismantled according to the layout to obtain the concrete regeneration segment. The dismantling method of the embodiment of the invention can be a diamond wire saw, a disk saw or a water knife. If the margin is sufficient, the size needs to be corrected later.

[0037] The present invention adopts the above method during demolition. Before demolishing the existing concrete column 1, defects are first detected and identified. According to the identification results, the intact cutting position and angle are determined to facilitate the subsequent better utilization of the demolished components. This can ensure the best degree of resource conservation while ensuring the completeness of component demolition and use.

[0038] In this embodiment, during one scribing, the defect area 5 and the regeneration area are scribed along the axial direction of the concrete column 1. By observing the marked positions of the concrete column 1, multiple defect-intensive areas with marked defects distributed along the axial direction are obtained; each defect-intensive area is confined to a corresponding defect area 5. That is, the defect area 5 obtained by scribing contains as many defect mark positions as possible. In this way, the defect area 5 and the regeneration area are separated, which facilitates the subsequent removal operation of the cutting equipment.

[0039] In this embodiment, when defining a defect-dense area, the density of defect positions in the marked area is observed and then compared one by one to find the two points located on the outermost side of the dense area. The two points are surrounded by the center line of the concrete column 1 as the axis to form two circles. The two circles are defined as the boundary lines of the defect area 5, thereby limiting the defect-dense area to a defect area 5. By adopting the above method, the defect area 5 can be quickly defined to improve the efficiency of removal.

[0040] In this embodiment, there are at least N defect marks in the defect-dense area, and the distance between two adjacent defect marks is less than D / 10, where N≥3, and the size of N is set as needed. The remaining defect marks are discrete defects. When the size of the discrete defect is larger than the second defect critical size, it is divided into a separate defect area 5. The above method can better isolate the defects and facilitate the reuse of the regeneration area.

[0041] For example, when a discrete defect is far from an adjacent defect-intensive area, if it is confined to the defect area 5, it is easy to cause a large section of the concrete column 1 to be divided into the defect area 5, resulting in a waste of resources. By dividing it into a separate defect area 5, it can be divided, so that resources can be more fully utilized. When there are two discrete defects with a short distance, they can be divided into zones separately, or they can be divided into one zone as a whole. The distance is less than D / 10, and it can be selected according to needs.

[0042] In this embodiment, when the size of the discrete defect is between the first defect critical size and the second defect critical size, it means that the size will not affect the overall performance of the concrete column 1, and it can be used as a regeneration segment, which is divided into a regeneration zone to facilitate subsequent cutting and breaking operations. A regeneration zone is allowed to have at most three discrete defects with a large distance and a size between the first defect critical size and the second defect critical size. When there are other defect distributions, they are generally divided in the same way as the ordinary defect zone 5 to ensure that the safety standards of the regeneration segment are met.

[0043] In this embodiment, for discrete defects whose size belongs to the second defect 3, they are repaired before the concrete column 1 is dismantled, which is not only conducive to the repair and utilization of the regenerated segment, but also can reduce the extension of defects such as cracks during dismantling, and can ensure the integrity of the regenerated segment.

[0044] In this embodiment, during the secondary marking, the edge area 7 is divided to be adjacent to the defective area 5, which is convenient for subsequent one-time removal. The edge area 7 is used as a buffer to avoid damage to the regeneration area caused by misoperation. When the concrete column 1 is removed, cutting or breaking is adopted.

[0045] In this embodiment, the defect position is marked by punching, which is convenient and easy to identify.

[0046] Embodiment 2, as Figure 3 and Figure 4 As shown, the difference between this embodiment and embodiment 1 is that the concrete column 1 in this embodiment is a square column, and the axis of the concrete column 1 is at an angle of 20° with the horizontal plane. The concrete column 1 is dismantled by using a cutting device. When marking, the plane of the marking is as perpendicular to the axis of the concrete column 1 as possible, so that it can be more stable when cutting. In order to adapt to the uniformity of cutting, it is necessary to deviate the cutting device from the corresponding angle before cutting. Specifically, the cutting device disclosed in this embodiment includes a cutting rope 8, a wire feeding wheel 9 for cooperating with the cutting rope 8, and a motor 10 for driving the wire feeding wheel 9 to rotate. The motor 10 drives the wire feeding wheel 9 to rotate, and the two ends of the cutting rope 8 are respectively wound around the wire feeding wheel 9 and the concrete column 1, and the wire feeding wheel 9 drives the cutting rope 8 to transmit to achieve cutting of the concrete column 1.

[0047] The cutting device disclosed in the present invention also includes a bracket 11, a hydraulic cylinder 12, a bottom support 13, and a sliding drive device 14. The motor 10 is slidably mounted on the bracket 11, and the bracket 11 is equipped with a sliding drive device 14 that drives the motor 10 to slide along the bracket 11. The sliding drive device 14 is driven by a gear and a rack, and the rack is fixed on the bracket 11. One side of the bracket 11 is hinged to the bottom support 13, and the bottom support 13 is equipped with a hydraulic cylinder 12 that drives the bracket 11 to flip. The hydraulic cylinder 12 can drive the bracket 11 to deflect around the hinge axis by supporting the bracket 11, thereby realizing free switching of the cutting angle, and can also realize switching during the cutting process, which is convenient and practical.

[0048] In some other embodiments, a tightening mechanism is installed on the concrete column 1. By setting the tightening mechanism, a pre-tightening force can be provided to the cutting rope 8 to prevent the cutting rope 8 from excessively sagging, thereby improving the efficiency and accuracy of cutting. The tightening mechanism includes a square hoop 15, a slide rail 16, a clamping wheel 17, a sliding shaft 18 and a telescopic device 19. A square hoop 15 is installed on the outer side of the concrete column 1. A slide rail 16 is fixed on the square hoop 15. Two sliding shafts 18 are slidably matched on the sliding rail 16 at the same time. A clamping wheel 17 is rotatably matched on the sliding shaft 18. The two sets of sliding shafts 18 are respectively connected to the two ends of the telescopic device 19. The telescopic device 19 drives the sliding shaft 18 to slide, and can drive the two sets of clamping wheels 17 to move closer to or away from each other. When the cutting rope 8 cuts a part of the concrete column 1 and penetrates into it, the limiting distance of the concrete column 1 on the cutting rope 8 changes, and the cutting rope 8 becomes loose and easy to fall. At this time, the two sets of clamping wheels 17 are controlled to be close to each other, which can provide a pre-tightening force for the cutting rope 8, so that the cut end of the cutting rope 8 can be pressed in the cutting seam, thereby improving the cutting efficiency and accuracy.

[0049] Finally, it should be noted that the above preferred embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail through the above preferred embodiments, those skilled in the art should understand that various changes can be made in form and details without departing from the scope defined by the claims of the present invention.

Claims

1. A method for on-site removal of existing concrete columns. It is characterized in that include: Demolition preparation, determine the critical size of the defect according to the size characteristics of the existing concrete column, and obtain the size D of the concrete regeneration segment, where the critical size of the defect includes the first critical size of the defect and the second critical size of the defect. There are three sizes of defects, including the first defect, the second defect and the third defect, where 0<first defect<first defect critical size<second defect<second defect critical size<third defect; Defect detection: detect defects in concrete columns, mark defect locations, and mark the second and third defects separately; One-time marking: according to the position of the defects marked on the concrete column, the concrete column is divided into defect area and regeneration area by marking on the concrete surface; Secondary marking: according to the size and shape of the concrete regeneration segment, marking is done in the regeneration area to divide the regeneration area into a regeneration segment area and an edge area; Demolition: According to the layout conditions, the existing concrete columns are demolished to obtain concrete recycled segments.

2. A method for on-site removal of existing concrete columns according to claim 1, It is characterized in that During one marking process, the defect area and the regeneration area are marked along the axial direction of the concrete column. By observing the marked position of the concrete column, multiple defect-intensive areas with marked defects distributed along the axial direction are obtained; each defect-intensive area is confined to a corresponding defect area.

3. A method for on-site removal of existing concrete columns according to claim 2, It is characterized in that When defining a defect-dense area, the density of defect positions in the marked area is observed and then compared one by one to find the two outermost points in the dense area. The two points are surrounded by the center line of the concrete column as the axis to form two circles. The two circles are defined as the boundary lines of the defect area, thereby limiting the defect-dense area to a defect area.

4. A method for on-site removal of existing concrete columns according to claim 3, It is characterized in that There are at least N defect marks in the defect-intensive area, and the distance between two adjacent defect marks is less than D / 10, where N≥3. The remaining defect marks are discrete defects. When a discrete defect belongs to the third defect, it is divided into a separate defect area.

5. A method for on-site removal of existing concrete columns according to claim 4, It is characterized in that When the discrete defect belongs to the second defect, it is classified in the regeneration zone.

6. A method for on-site removal of existing concrete columns according to claim 5, It is characterized in that For discrete defects whose size belongs to the second defect, they shall be repaired before the concrete column is demolished.

7. A method for on-site removal of existing concrete columns according to claim 6, It is characterized in that During the secondary scribing, the edge area is divided to be adjacent to the defect area.

8. The method for on-site removal of existing concrete columns according to claim 3, It is characterized in that When dismantling concrete columns, cutting or breaking is used.

9. The method for on-site removal of existing concrete columns according to claim 8, It is characterized in that The defect location is marked by punching.

10. A method for on-site removal of existing concrete columns according to any one of claims 1 to 9, It is characterized in that A cutting device is used to dismantle concrete columns. The cutting device includes a cutting rope, a wire feeding wheel for cooperating with the cutting rope, and a motor for driving the wire feeding wheel to rotate. The cutting device also includes a bracket, a hydraulic cylinder, a bottom support, and a sliding drive device. The motor is slidably installed on the bracket, and a sliding drive device for driving the motor to slide along the bracket is installed on the bracket. One side of the bracket is hinged to the bottom support, and a hydraulic cylinder for driving the bracket to flip is installed on the bottom support.