High-density silk-like protein and preparation method thereof

By using the second raw materials of dietary fiber and water in the production of high-density wire-drawn protein, increasing the speed of the extruder and pushing the residual raw materials of high-density wire-drawn protein to eject, the problem of difficult mold cleaning is solved, production efficiency is improved and cleaning is simplified process.

CN118633677BActive Publication Date: 2024-10-29SHANDONG YUWANG ECOLOGY FOOD IND
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411116611.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-10-29
Estimated Expiration
2044-08-15

AI Technical Summary

Technical Problem

In the production process of high-density wire drawing protein, it is difficult to clean the mold, resulting in low production efficiency. Existing methods such as using an electric hammer or impact drill can easily damage the mold, and the residual material is hard and difficult to clean.

Method used

Before the end of production, by adding the second raw material of dietary fiber and water into the hopper, increasing the screw speed and feeding speed of the extruder, and using the high water absorption and dispersion of dietary fiber to push the high-density drawing protein residue The raw materials are ejected from the mold to achieve mold cleaning.

Benefits of technology

It realizes the cleaning of the mold before shutting down at the end of production, avoids blockage of molten high-density drawing protein, and improves the production efficiency of high-density drawing protein. The cleaned mold can be directly used for the next production, simplifying the cleaning process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118633677B_ABST
    Figure CN118633677B_ABST
Patent Text Reader

Abstract

The invention discloses a high-density fibroblast protein and a preparation method thereof, and belongs to the technical field of food processing. After mixing the fibroblast protein raw material, it is sent into an extruder through a hopper. The extruder maintains the set temperature, screw speed and feeding speed, and extrude the fibroblast protein raw material from a mold to obtain a high-density fibroblast protein; before the extruder stops working, stop adding the fibroblast protein raw material into the hopper. When the remaining material level in the hopper reaches the set requirement, the extruder stops heating, and adds a second raw material composed of dietary fiber and water into the hopper; the screw speed and feeding speed of the extruder are increased to increase the internal pressure of the extruder, and then the dietary fiber pushes the residual raw material of the high-density fibroblast protein to be ejected from the mold. The present invention uses dietary fiber to remove the residual molten raw material in the mold, and realizes the cleaning of the mold before stopping the production. The cleaned mold can be directly used for the next production of high-density fibroblast protein, thereby improving the production efficiency of high-density fibroblast protein.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of food processing, and particularly relates to a high-density fibrous protein and a preparation method thereof. Background Art

[0002] The information disclosed in this background technology section is only intended to enhance the understanding of the overall background of the invention, and should not necessarily be regarded as an admission or any form of suggestion that the information constitutes the prior art already known to a person skilled in the art.

[0003] Fiber-drawing protein emerged in the 1970s and has developed rapidly in China since the 21st century. It is made of soy protein isolate, soybean meal, etc. as raw materials, and is subjected to high temperature and high pressure in an extruder and then molded into a mold. When producing high-density fiber-drawing protein, the material is in a molten state under high temperature and high pressure conditions. At this time, the protein molecules undergo conformational reorganization, cool down when passing through the mold, and form filamentous fibers along the flow direction of the material. After flowing out of the mold, high-density fiber-drawing protein is formed. During normal production, although the temperature of the material in the mold drops, it is still high, and the material can pass through the mold smoothly. After the production is stopped, it is necessary to disassemble the mold for cleaning after the temperature and pressure of the extruder drop. At this time, the temperature in the mold drops significantly, and the residual material has become a harder solid, which is difficult to clean. The longer the mold, the more difficult it is to clean. At present, electric hammers or impact drills are usually used to crush the material and then clear it out, which is not only inefficient, but also easy to damage the mold. This seriously restricts the production efficiency of fiber-drawing protein. Therefore, achieving simple cleaning of the mold is of great significance to improving the production efficiency of high-density fiber-drawing protein. Summary of the invention

[0004] In order to overcome the deficiencies in the prior art, an object of the present invention is to provide a high-density fibrous protein and a preparation method thereof. The preparation method of the high-density fibrous protein provided by the present invention can clean the mold before stopping the production, thereby avoiding clogging of the mold by the molten high-density fibrous protein and improving the production efficiency of the high-density fibrous protein.

[0005] In order to achieve the above object, the technical solution of the present invention is:

[0006] The first aspect of the present invention provides a method for preparing high-density fibrous protein, comprising the following steps:

[0007] After mixing the fibrous protein raw materials, the fibrous protein raw materials are fed into the extruder through the hopper. The extruder maintains the set temperature, screw speed and feeding speed, and extrude the fibrous protein raw materials from the die to obtain high-density fibrous protein;

[0008] Before the extruder stops working, stop adding the fibrous protein raw material into the hopper. When the remaining material level in the hopper reaches the set requirement, the extruder stops heating and adds the second raw material consisting of dietary fiber and water into the hopper; the screw speed and feeding speed of the extruder are increased to increase the internal pressure of the extruder, and then the dietary fiber pushes the residual high-density fibrous protein raw material to be ejected from the mold.

[0009] In some embodiments of the present invention, after the dietary fiber is completely ejected, the extruder stops working, and the mold is disassembled and cleaned.

[0010] When the high-density fibrous protein is produced continuously to the set production days or output, the extruder stops working normally. Before stopping, dietary fiber is used to push out the residual raw materials of the high-density fibrous protein in the mold to clean the mold.

[0011] Under the high temperature and high pressure conditions in the extruder, dietary fiber molecules do not become molten like protein molecules, but are in the form of dispersed fine particles. Dietary fiber has high water absorption. The water content of dietary fiber added to the hopper is high. After increasing the screw speed and feeding speed of the extruder, the internal pressure of the extruder increases under the action of high temperature, pushing the dietary fiber forward with the residual raw materials of high-density fibrous protein. When all the dietary fiber flows out of the mold, the pressure inside the extruder and the mold drops, the material is ejected, and the mold is hollow. There will be no residual material (ie dietary fiber). The mold is easy to clean after disassembly, and it only needs to be simply rinsed with clean water, realizing the residue-free preparation of high-density fibrous protein.

[0012] In some embodiments of the present invention, the dietary fiber is insoluble plant dietary fiber, and the protein content is no higher than 12%.

[0013] Preferably, the dietary fiber may be derived from wheat, rice, beans, vegetables, or fruits. For example, the dietary fiber may be soybean dietary fiber.

[0014] In some embodiments of the present invention, the mass ratio of the dietary fiber to water is 1:(3-5), preferably 1:4. Dietary fiber has high water absorption, and the water content in the dietary fiber cannot be too low or too high. If the water content in the dietary fiber is too low, the material will burn and block the screw of the extruder. If the water content in the dietary fiber is too high, the material is too thin and semi-solid or liquid, and cannot form a dispersed particle state, and cannot flow out of the mold quickly, and cannot achieve the purpose of clearing the residual raw materials of high-density fibrous protein in the mold and the extruder.

[0015] In some embodiments of the present invention, after the dietary fiber and water are mixed, they are left to stand for at least 5 minutes, and after the water is fully absorbed by the dietary fiber, the dietary fiber containing water (ie, the second raw material) is added into the hopper of the extruder.

[0016] In some embodiments of the present invention, a mixer can be used to evenly mix the dietary fiber and water. The mixer can be a horizontal mixer, a vertical mixer, a cone mixer or a ribbon mixer, preferably a horizontal high-speed mixer.

[0017] Wherein, when a mixer is used to mix dietary fiber and water, the rotation speed of the mixer is 150-250 rpm, preferably 200 rpm.

[0018] In some embodiments of the present invention, the fibrous protein raw material includes, by mass percentage, 40%-60% soy protein isolate and 40%-60% low-temperature edible soybean meal.

[0019] In some embodiments of the present invention, the extruder is a single-screw extruder, a twin-screw extruder or a multi-screw extruder, preferably a single-screw extruder or a twin-screw extruder.

[0020] In some embodiments of the present invention, when high-density fibrous protein is produced, the extrusion temperature of the extruder is 130-250°C, preferably 200°C; the screw speed of the extruder is 20-500 rpm, preferably 20-100 rpm; the feeding speed of the extruder is 10-100 rpm, preferably 20-90 rpm.

[0021] In some embodiments of the present invention, when the remaining material level in the hopper is ≤3%, the second raw material is added into the hopper.

[0022] In some embodiments of the present invention, after adding the second raw material into the hopper, the screw speed and the feeding speed of the extruder are increased by 10-400 rpm, preferably 10-100 rpm. After the screw speed and the feeding speed of the extruder are increased, no matter how much they are increased, under the action of high temperature, the internal pressure of the extruder will increase, thereby pushing the dietary fiber forward with the residual raw material of high-density fibrous protein. When the screw speed and the feeding speed of the extruder are increased to a large extent, the extrusion rate of the dietary fiber and the residual raw material of high-density fibrous protein is fast, and when the degree of increase is small, the extrusion rate of the dietary fiber and the residual raw material of high-density fibrous protein is relatively slow. Regardless of the degree of increase, the internal pressure of the extruder can be increased, and the dietary fiber pushes the residual raw material of high-density fibrous protein forward, thereby achieving the purpose of mold cleaning.

[0023] In some embodiments of the present invention, the mold has a cooling jacket, cooling water is passed into the jacket, and a discharge pipe is contained inside. The discharge pipe can be circular, rectangular, triangular or any other shape, preferably a circular tube.

[0024] In some embodiments of the present invention, a material receiver is provided in front of the mold to collect the ejected material.

[0025] In some embodiments of the present invention, after the mold is disassembled, it can be rinsed clean with clean water.

[0026] The second aspect of the present invention provides a high-density fibrous protein, wherein the high-density fibrous protein is prepared by the preparation method;

[0027] The density of the high-density fibrous protein is 500-600 g / L.

[0028] The beneficial effects of the present invention are:

[0029] The method for preparing high-density drawn protein provided by the present invention can prepare drawn protein with a density of 500-600 g / L, and uses dietary fiber to remove residual molten raw materials in the mold, so that the mold is cleaned before the production is stopped. The cleaned mold can be directly used for the next production of high-density drawn protein, thereby improving the production efficiency of high-density drawn protein. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] The accompanying drawings in the specification, which constitute a part of the present invention, are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute improper limitations on the present invention.

[0031] Figure 1 This is the production process of high-density fibrous protein according to an embodiment of the present invention;

[0032] Figure 2 This is a structural diagram of the production system used in the production process of high-density fibrous protein according to an embodiment of the present invention.

[0033] Among them, 1-horizontal mixer, 2-hopper, 3-extruder, 4-mold cooling water inlet, 5-mold, 6-mold cooling water outlet, 7-discharging port, 8-receiver. DETAILED DESCRIPTION

[0034] In order to enable those skilled in the art to more clearly understand the technical solution of the present invention, the technical solution of the present invention will be described in detail below in conjunction with specific embodiments.

[0035] When producing high-density fibrous protein, the production line needs to be shut down when continuous production reaches a set number of days (such as one week, two weeks, four weeks, etc.), reaches a set production volume, or needs to replace raw materials. After the production is stopped, it is necessary to disassemble the mold 5 for cleaning after the temperature and pressure of the extruder 3 drop. At this time, the temperature in the mold 5 drops significantly, and the residual material has become a harder solid, which is difficult to clean. The longer the mold 5, the more difficult it is to clean. At present, electric hammers or impact drills are usually used to crush the materials and then clear them out, which is not only inefficient, but also easy to damage the mold 5. This seriously restricts the production efficiency of fibrous protein.

[0036] To solve this problem, the present invention provides a method for preparing high-density fibrous protein, which can prepare fibrous protein with a density of 500-600 g / L. Before the production is completed and the machine is shut down, dietary fiber is used to remove the residual molten raw material in the mold 5 to clean the mold 5. The cleaned mold 5 can be directly used for the next production of high-density fibrous protein, thereby improving the production efficiency of high-density fibrous protein.

[0037] The production process of high-density fibrous protein in the following embodiments is as follows Figure 1 As shown. And the following embodiments all adopt Figure 2 The production system shown allows for the production of high-density fibroin. Figure 2 The production system shown includes a horizontal mixer 1 , a hopper 2 , an extruder 3 , a mold 5 , a mold cooling water inlet 4 , a mold cooling water outlet 6 , a discharge port 7 and a material receiver 8 .

[0038] The horizontal mixer 1 is used to mix dietary fiber and water evenly. The material outlet of the horizontal mixer 1 is connected to the hopper 2 through a spiral auger, which is conducive to the mixed dietary fiber (i.e., the second raw material) entering the hopper 2. The hopper 2 is connected to the material inlet of the extruder 3, and the extruder 3 is provided with a feeding screw, a feeding motor, a conveying screw and a screw motor. The feeding motor is used to drive the feeding screw to rotate, and the screw motor is used to drive the conveying screw to rotate. The material outlet of the extruder 3 is connected to the material inlet of the mold 5, and the end of the mold 5 is provided with a discharge port 7 for extruding high-density fibrous protein. A cooling jacket is provided on the side wall of the mold 5, and cooling water for controlling the temperature is passed through the cooling jacket. The cooling jacket is provided with a mold cooling water inlet 4 and a mold cooling water outlet 6. A material receiver 8 is provided in front of the mold 5 (i.e., the discharge port 7 end) to collect the ejected material.

[0039] In the following examples, when producing high-density fibrous protein, the raw materials of high-density fibrous protein, measured by mass percentage, include: 50% soy protein isolate and 50% low-temperature edible soybean meal.

[0040] Example 1

[0041] A method for preparing high-density fibrous protein comprises the following steps:

[0042] (1) After the high-density fibrous protein raw materials are mixed, they are fed into the extruder 3 through the hopper 2. During the production of high-density fibrous protein, the temperature of the extruder 3 is 200°C, the screw speed is 30 rpm, and the feeding speed is 28 rpm. The high-density fibrous protein raw materials are extruded from the die 5 to obtain high-density fibrous protein.

[0043] (2) Weigh 1 kg of soybean dietary fiber and pour it into a horizontal mixer 1. First, add 2 times the amount of water. After mixing, add 2 times the amount of water again, for a total of 4 kg of water. Turn on the horizontal mixer 1 at a speed of 200 rpm to mix the soybean dietary fiber and water evenly and set aside for later use.

[0044] When the production is continuously continued to the set production days, stop adding high-density fibrous protein raw materials into hopper 2, observe the material level in hopper 2, and when almost no material can be seen in hopper 2 (i.e., the remaining material level in hopper 2 is ≤3%), stop heating in extruder 3, and immediately add the mixed soybean dietary fiber into hopper 2. Close the mold cooling water inlet 4, and at the same time increase the screw speed of extruder 3 to 80 rpm and the feeding speed to 40 rpm. The soybean dietary fiber is heated in the extruder 3, and the temperature and pressure rise rapidly through the high-speed extrusion of the screw. Driven by the screw and its own pressure, the soybean dietary fiber is rapidly pushed forward. After about 10 s, the soybean dietary fiber pushes the residual raw materials of high-density fibrous protein to the discharge port 7, and under the action of the strong pressure difference, it is quickly ejected from the mold 5 and falls into the receiver 8.

[0045] (3) After the soybean dietary fiber is completely ejected, the screw motor and the feeding motor of the extruder 3 are stopped, the mold cooling water outlet 6 is opened, the remaining water in the mold 5 is drained, and the mold 5 is disassembled. After the mold 5 is disassembled, there is no residual material inside, and it is rinsed with clean water and placed aside for use, and the entire production process is completed.

[0046] Example 2

[0047] A method for preparing high-density fibrous protein comprises the following steps:

[0048] (1) After the high-density fibrous protein raw materials are mixed, they are sent into the extruder 3 through the hopper 2. During the production of high-density fibrous protein, the temperature of the extruder 3 is 180°C, the screw speed is 30 rpm, and the feeding speed is 28 rpm. The high-density fibrous protein raw materials are extruded from the die 5 to obtain high-density fibrous protein.

[0049] (2) Weigh 1 kg of soybean dietary fiber and pour it into a horizontal mixer 1. First, add 2 times of water. After mixing, add 3 times of water, for a total of 5 kg of water. Turn on the horizontal mixer 1 at a speed of 200 rpm to mix the soybean dietary fiber and water evenly and set aside for later use.

[0050] When the production is continuously continued for the set number of days, stop adding high-density fibrous protein raw materials into hopper 2, observe the material level in hopper 2, and when almost no material can be seen in hopper 2 (i.e., the remaining material level in hopper 2 is ≤3%), stop heating in extruder 3, and immediately add the mixed soybean dietary fiber into hopper 2. Close the mold cooling water inlet 4, and at the same time increase the screw speed of extruder 3 to 100 rpm, and the feeding speed to 60 rpm. The soybean dietary fiber is heated in the extruder 3, and the temperature and pressure rise rapidly through the high-speed extrusion of the screw. Driven by the screw and its own pressure, the soybean dietary fiber is rapidly pushed forward. After about 7 seconds, the soybean dietary fiber pushes the residual high-density fibrous protein raw materials to the discharge port 7, and under the action of the strong pressure difference, it is quickly ejected from the mold 5 and falls into the receiver 8.

[0051] (3) After the soybean dietary fiber is completely ejected, the screw motor and the feeding motor of the extruder 3 are stopped, the mold cooling water outlet 6 is opened, the remaining water in the mold 5 is drained, and the mold 5 is disassembled. After the mold 5 is disassembled, there is no residual material inside, and it is rinsed with clean water and placed aside for use, and the entire production process is completed.

[0052] Example 3

[0053] A method for preparing high-density fibrous protein, which differs from Example 1 in that: in step (2), the screw speed of the extruder 3 is increased to 130 rpm, the feed speed is increased to 128 rpm, and the remaining steps are consistent with Example 1.

[0054] The soybean dietary fiber is heated in the extruder 3, and the temperature and pressure rise rapidly through the high-speed extrusion of the screw. Driven by the screw and its own pressure, the soybean dietary fiber is rapidly pushed forward. After about 5 seconds, the soybean dietary fiber pushes the residual raw material of the high-density fibrous protein to the discharge port 7, and under the action of the strong pressure difference, it is quickly ejected from the mold 5 and falls into the receiver 8.

[0055] After the mold 5 is disassembled, no residual material is left inside.

[0056] Comparative Example 1

[0057] A method for preparing high-density fibrous protein, which differs from Example 1 in that: in step (2), 1 kg of soybean dietary fiber is weighed and poured into a horizontal mixer 1, 0.5 times of water is first added, and after mixing, 0.5 times of water is added again, and a total of 1 kg of water is added. The remaining steps are consistent with those of Example 1.

[0058] After the mixed soybean dietary fiber is added into the hopper 2, the soybean dietary fiber blocks the screw of the extruder 3 due to its low moisture content, and burns in the extruder 3, making it impossible to clean the mold 5.

[0059] Comparative Example 2

[0060] A method for preparing high-density fibrous protein, which differs from Example 1 in that: in step (2), 1 kg of soybean dietary fiber is weighed and poured into a horizontal mixer 1, 5 times of water is first added, and after mixing, 5 times of water is added again, and a total of 10 kg of water is added. The remaining steps are consistent with Example 1.

[0061] After adding the mixed soybean dietary fiber into the hopper 2, the second raw material after the soybean dietary fiber and water are mixed is in liquid state due to the high moisture content in the soybean dietary fiber, and cannot form a dispersed particle state. After being extruded by the extruder 3, the mold 5 is disassembled and it is found that there is high-density fibrous protein raw material remaining inside, and the inside of the mold 5 cannot be cleaned.

[0062] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for preparing high-density fibrous protein, characterized in that: The following steps are involved: After mixing the fibrous protein raw materials, the fibrous protein raw materials are fed into the extruder through the hopper. The extruder maintains the set temperature, screw speed and feeding speed, and extrude the fibrous protein raw materials from the die to obtain high-density fibrous protein; Before the extruder stops working, stop adding the fibrous protein raw material into the hopper. When the remaining material level in the hopper reaches the set requirement, the extruder stops heating and adds the second raw material consisting of dietary fiber and water into the hopper; the screw speed and feeding speed of the extruder are increased to increase the internal pressure of the extruder, so that the dietary fiber pushes the residual high-density fibrous protein raw material to be ejected from the mold; The dietary fiber is insoluble plant dietary fiber, and the protein content is not higher than 12%; The mass ratio of the dietary fiber to water is 1:(3-5); After the second raw material is added into the hopper, the screw speed and the feed speed of the extruder are increased by 10-400 rpm.

2. The method for preparing high-density fibrous protein according to claim 1, characterized in that: After the dietary fiber is completely ejected, the extruder stops working, and the mold is disassembled and cleaned.

3. The method for preparing high-density fibrous protein according to claim 1, characterized in that: The drawn protein raw material comprises, by mass percentage, 40%-60% of isolated soy protein and 40%-60% of low-temperature edible soybean meal.

4. The method for preparing high-density fibrous protein according to claim 1, characterized in that: The extruder is a single-screw extruder, a twin-screw extruder or a multi-screw extruder.

5. The method for preparing high-density fibrous protein according to claim 1, characterized in that: During the production of high-density fibrous protein, the extrusion temperature of the extruder is 130-250° C., the screw speed of the extruder is 20-500 rpm, and the feeding speed is 10-100 rpm.

6. The method for preparing high-density fibrous protein according to claim 1, characterized in that: When the remaining material level in the hopper is ≤3%, add the second raw material into the hopper.

Citation Information

Patent Citations

  • Spicy-flavored wire-drawing protein and producing method thereof

    CN106562215A

  • Method for enhancing water binding capacity of plant wiredrawing protein

    CN111838399A