An intelligent control system for welding of mining equipment components

By identifying and analyzing connection anomalies and risks in the mine support frame through an intelligent control system, and adjusting the weld layer thickness in conjunction with environmental information, the problems of welding stability and safety of the mine support frame were solved, and efficient and precise welding operations were achieved.

CN118650349BActive Publication Date: 2024-11-12TIBET HUATAILONG MINING DEV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411141603.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-12
Estimated Expiration
2044-08-20

AI Technical Summary

Technical Problem

Existing manual welding methods cannot guarantee the stability and safety of welded components for mine support frames, and the traditional fixed weld layer thickness cannot adapt to the strength requirements of different parts, resulting in low welding efficiency, material waste and increased costs.

Method used

The intelligent control system for welding components of mining equipment is adopted. It uses high-definition cameras to identify the location of connecting components in the laid area, analyzes connection anomalies and risks, and adjusts the weld layer thickness by combining environmental information and historical records, so as to accurately select the welding position and component type.

Benefits of technology

It improves the adaptability and precision of welded connection components, enhances the stability and safety of the mine tunnel support frame, reduces accident risks and material waste, and improves welding quality and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118650349B_ABST
    Figure CN118650349B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of intelligent welding control, and discloses an intelligent control system for welding of mining equipment components, the system comprising a laying area division module, a laid area analysis module, a to-be-laid area analysis module, an environmental information analysis module, a welding operation judgment module, a weld layer thickness correction module, and a data storage library. The present invention obtains the required connection component type not mentioned in the construction plan based on the connection risk situation of each unwelded position in the laid area, and then obtains the actual required connection component type in combination with the required connection component type in the construction plan, thereby increasing the adaptability and accuracy of the selection of welding connection components. At the same time, the present invention analyzes the environmental impact and operation and maintenance abnormalities based on the meteorological environment information of each to-be-welded position and the historical secondary welding records, and then determines whether it is necessary to correct the system default initial weld layer thickness, and can accurately adjust the initial weld layer thickness.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of welding intelligent control and relates to an intelligent control system for welding of mining equipment components. Background Art

[0002] Mining equipment components are an important part of mining equipment, which can be roughly divided into mining equipment, transportation equipment and support equipment. Among them, the support equipment is not only the basis of the equipment structure, but also undertakes multiple functions to ensure the stable operation of the equipment and the safety of the staff. In practice, there are multiple factors inside the mine tunnel, such as harsh environment and high frequency of use, which may cause displacement and deviation of the support frame. Therefore, it is usually necessary to weld the support frame. The existing manual welding method cannot guarantee the stability of the performance of the welding components and the safety of the mine tunnel. Therefore, intelligent control of the welding of the mine support frame is of great significance.

[0003] In practice, welding of mine tunnel support equipment generally includes welding operations on each target connection component corresponding to the support frame.

[0004] The rationality of the connection component type is an important prerequisite for ensuring welding efficiency and mine safety. Traditional mine tunnel support frame welding operations are usually for fixed type connection components. The welding operation method for fixed type connection components does not take into account the actual use of the connection components and the impact of the environment on the connection components, resulting in some connection components that need to be welded being ignored, resulting in the welding operation being unable to meet the actual mine construction needs, lacking flexibility and pertinence, and thus affecting the stability and safety of the support frame after welding.

[0005] In addition, the thickness of the weld layer is an important indicator to ensure the welding quality. Reasonable setting of the weld layer thickness is an important prerequisite for taking into account both welding efficiency and welding quality. The weld layer thickness formed in traditional welding operations is usually fixed. This fixed weld layer thickness cannot provide suitable strength support for all parts, thereby increasing the risk of structural failure. If the weld layer thickness is not selected properly, multiple welding or repairs may be required to achieve the required welding quality, thereby reducing welding efficiency and causing excessive welding materials to be wasted, increasing production costs. Summary of the invention

[0006] In view of this, in order to solve the problems raised in the above background technology, an intelligent control system for welding of mining equipment components is proposed.

[0007] The purpose of the present invention can be achieved through the following technical solutions: an intelligent control system for welding of mining equipment components, including: a laying area division module, used to extract the mine tunnel construction progress book, and then obtain the laid area where the support frame has been laid and the to-be-laid area where the support frame has not been laid from the mine tunnel construction progress book.

[0008] The laid area analysis module is used to use a high-definition camera to collect images of the positions of each connected component in the laid area, and then identify the images to divide the positions of each connected component into welded positions and unwelded positions, thereby analyzing the connection abnormalities of each welded position and the connection risks of the unwelded position, and then locating each position to be welded in the laid area.

[0009] The analysis module for the area to be laid is used to obtain the required welding connection component type from the construction plan, and obtain the actual welding connection component type based on the connection risk situation of each unwelded position in the laid area, and then match it with the connection component type in the area to be laid to obtain each position to be welded in the area to be laid.

[0010] The environmental information analysis module is used to set up mobile detection equipment, which includes a temperature detector, a humidity detector, a gas concentration sensor and a coal dust concentration sensor. The mobile detection equipment is used to collect real-time environmental information of each welding position, and the environmental information includes meteorological environmental information and risk environmental information.

[0011] The welding operation judgment module is used to analyze the construction risk situation of each welding position based on the risk environment information of each welding position, thereby judging whether the welding operation is allowed.

[0012] The weld layer thickness correction module is used to analyze environmental abnormalities and operation and maintenance abnormalities based on the meteorological environment information and historical secondary welding records of each welding position when it is determined that welding operations are allowed, thereby obtaining the weld layer thickness correction requirements of each welding position, and determining whether the system default initial weld layer thickness needs to be corrected. If necessary, the initial weld layer thickness is corrected based on the weld layer thickness correction requirements.

[0013] Data repository for storing mine construction schedules, construction plans, standard weld defect images and historical secondary welding records.

[0014] In a preferred embodiment of the present invention, the analysis of abnormal connection conditions at each welded position is specifically as follows: extracting images of each connection component position in the laid area captured by a high-definition camera, and then extracting images of each welded connection component position therefrom, which are recorded as monitoring images.

[0015] The monitoring images are processed by image processing software to identify the existing abnormal positions, locate the abnormal positions corresponding to each monitoring image, compare the images of each abnormal position with the standard weld defect images stored in the data repository, and then obtain the defect type of each abnormal position.

[0016] The abnormal positions in the monitoring images are classified according to the defect types, and the number of defects corresponding to each defect type in each monitoring image is obtained by statistics. The defect area of ​​each abnormal position is obtained by using image processing software, and then the defect areas of the same defect type are accumulated to obtain the defect area corresponding to each defect type.

[0017] The number of defects corresponding to each defect type in each monitoring image and defect area Substitute into the analysis formula Get the connection anomaly index corresponding to the welded position ,in Indicates the area of ​​the solder layer at the abnormal position. Indicates the defect type number, .

[0018] In a preferred embodiment of the present invention, the connection risk situation of the unwelded position is specifically as follows: extract the image of each connection component position in the laid area collected by a high-definition camera, and then extract the image of each unwelded connection component position therefrom, and record it as the target image.

[0019] The component connection positions in the target image are divided into several monitoring points at equal intervals, and the component spacing corresponding to each monitoring point is obtained using image processing software.

[0020] The component spacing corresponding to each monitoring point is calculated by difference with the preset initial component spacing to obtain the component spacing deviation value, and then the absolute value of each component spacing deviation value is calculated by ratio with the initial component spacing to obtain the component spacing variation degree of each monitoring point.

[0021] The component spacing variation at each monitoring point was compared, and the maximum component spacing variation was selected as the connection risk index of the unwelded position.

[0022] In a preferred embodiment of the present invention, the step of locating each position to be welded in the laid area is as follows: compare the connection abnormality index of each welded position with the preset allowable connection abnormality index; if the connection abnormality index of a welded position is greater than the allowable connection abnormality index, it is judged that the welded position needs to be welded again; if the connection abnormality index of a welded position is less than or equal to the allowable connection abnormality index, it is judged that the welded position does not need to be welded again.

[0023] The connection risk index of each unwelded position is compared with the pre-set allowable connection risk index. If the connection risk index of an unwelded position is greater than the allowable connection risk index, it is judged that the unwelded position needs to be welded. If the connection risk index of an unwelded position is less than or equal to the allowable connection risk index, it is judged that the unwelded position does not need to be welded.

[0024] The welded positions that are judged to need secondary welding and the unwelded positions that need welding are recorded as positions to be welded in the laid area.

[0025] In a preferred embodiment of the present invention, the construction risk situation includes gas concentration risk and coal dust concentration risk, and the specific analysis steps are as follows: extracting the real-time gas concentration and real-time coal dust concentration of each welding position collected by the gas concentration sensor and the coal dust concentration sensor.

[0026] The difference between the real-time gas concentration of each welding position and the preset safe gas concentration threshold is calculated, and then the result of the difference calculation is compared with the safe gas concentration threshold to obtain the gas concentration risk.

[0027] The difference between the real-time coal dust concentration of each welding position and the preset safe coal dust concentration threshold is calculated, and then the result of the difference calculation is compared with the safe coal dust concentration threshold to obtain the coal dust concentration risk.

[0028] In a preferred embodiment of the present invention, the determination of whether the welding operation is allowed is specifically as follows: the gas concentration risk and the coal dust concentration risk are respectively compared with the preset allowable gas concentration risk and the allowable coal dust concentration risk, thereby obtaining a determination result of whether the welding operation is allowed.

[0029] In a preferred embodiment of the present invention, the abnormal environmental situation is analyzed as follows: the temperature and humidity of each position to be welded detected by a temperature detector and a humidity detector are extracted.

[0030] The temperature of each welding position and humidity Substitute into the analysis formula Get the environmental anomaly index corresponding to the welding position ,in Indicates the suitable temperature. Indicates suitable humidity. represents a natural constant, Represent the weights of temperature and humidity respectively.

[0031] In a preferred embodiment of the present invention, the abnormal operation and maintenance situation is analyzed as follows: the temperature and humidity of each position to be welded detected by a temperature detector and a humidity detector are extracted.

[0032] The temperature and humidity corresponding to the historical secondary welding records are matched with the temperature and humidity of each position to be welded, and then the corresponding historical secondary welding records with the same temperature and humidity as each position to be welded are extracted and recorded as target historical secondary welding records. Each target historical secondary welding record corresponds to a type of connection component.

[0033] The connection component type corresponding to each target historical secondary welding record is obtained, and then the connection components of the same type are classified, and the number of historical secondary welding records corresponding to each type of connection components is obtained by counting.

[0034] The historical maintenance number corresponding to each type of connection component is counted, and the number of historical secondary welding records of each type is compared with the corresponding historical maintenance number to obtain the abnormality ratio corresponding to each type of connection component, which is then used as the operation and maintenance abnormality index corresponding to each type of connection component.

[0035] The type of connection component of each position to be welded is extracted, and then matched with the operation and maintenance anomaly index of each type of connection component to obtain the operation and maintenance anomaly index of each position to be welded.

[0036] In a preferred embodiment of the present invention, the step of obtaining the weld thickness correction requirement of each welding position is as follows: the environmental anomaly index and the operation and maintenance anomaly index of each welding position are summed up according to the weight to obtain the weld thickness correction requirement index of each welding position.

[0037] In a preferred embodiment of the present invention, the judgment on whether the system default initial weld layer thickness needs to be corrected is specifically as follows: the weld layer thickness correction requirement index of each welding position to be welded is compared with the pre-set standard weld layer thickness correction requirement index to obtain a judgment result on whether the initial weld layer thickness needs to be corrected.

[0038] Compared with the prior art, the beneficial effects of the present invention are as follows: (1) The present invention obtains the required connection component types not mentioned in the construction plan based on the connection risk conditions of each unwelded position in the paved area, and then obtains the actual required connection component types in combination with the required connection component types in the construction plan. This analysis method can meet the needs of the actual construction environment and construction process, increase the adaptability and accuracy of the selection of welding connection components, enhance the stability and safety of the mine tunnel support frame, and can effectively reduce the risk of accidents caused by incomplete selection of welding connection components.

[0039] (2) The present invention analyzes environmental impacts and operation and maintenance abnormalities based on the meteorological environment information of each welding position and the historical secondary welding records, and then determines whether it is necessary to correct the system's default initial weld layer thickness. This method of determining the type of connection component can accurately adjust the initial weld layer thickness to ensure that the mechanical properties of the welded connection component meet the requirements and that the welding quality is not affected. At the same time, it avoids the occurrence of unnecessary excessive weld layer thickness and reduces material waste. By improving the welding quality, the subsequent maintenance and repair costs caused by welding defects can be reduced. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for describing the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.

[0041] Figure 1 It is a schematic diagram of the connection of each module of the system of the present invention. DETAILED DESCRIPTION

[0042] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0043] See also Figure 1 As shown, the present invention provides an intelligent control system for welding of mining equipment components, the system includes a laying area division module, a laid area analysis module, a to-be-laid area analysis module, an environmental information analysis module, a welding operation judgment module, a weld layer thickness correction module and a data storage library, wherein the laying area division module is respectively connected to the laid area analysis module and the to-be-laid area analysis module, the laid area analysis module and the to-be-laid area analysis module are both connected to the environmental information analysis module, the environmental information analysis module is connected to the welding operation judgment module, the welding operation judgment module is connected to the weld layer thickness correction module, and the data storage library is respectively connected to the laid area analysis module, the to-be-laid area analysis module and the weld layer thickness correction module.

[0044] The laying area division module is used to extract the mine tunnel construction progress book, and then obtain the laid area where the support frame has been laid and the to-be-laid area where the support frame has not been laid from the mine tunnel construction progress book.

[0045] It should be noted that the support frame plays an important role in mine tunnel construction: the support frame plays a vital role in mine tunnel construction. It is a key structure to ensure construction safety and stability. It can bear and disperse the stress during mine tunnel excavation, prevent surrounding rock collapse, provide workers with a safe working environment, and ensure the smooth progress of mine tunnel projects.

[0046] The paved area analysis module is used to use a high-definition camera to collect images of the positions of each connected component in the paved area, and then identify the images to divide the positions of each connected component into welded positions and unwelded positions, thereby analyzing the connection abnormalities of each welded position and the connection risks of the unwelded position, and then locating each position to be welded in the paved area.

[0047] Exemplarily, the connection components may be steel plate-steel plate, steel plate-scaffolding.

[0048] It should be noted that the step of dividing the position of each connecting component into a welded position and an unwelded position is: positioning the image at the connecting part of the connecting component, and then observing whether there is a welding layer at the connecting part; if so, judging the connecting position of the connecting component as a welded position; if not, judging the connecting position of the connecting component as an unwelded position.

[0049] It needs to be explained that the reason for dividing the positions of each connection component into welded positions and unwelded positions is: the construction plan explains the welding requirements for connection components that generally have connection stability problems and are used frequently. However, in practice, due to factors such as differences in mine environment, some of the connection components that are not included may also have stability abnormalities. Therefore, analysis of these connection components can determine whether the corresponding connection components need to be welded.

[0050] It should be added that the connection components corresponding to the unwelded positions are connection components that are determined not to require welding operations during initial welding.

[0051] Preferably, the analysis of abnormal connection conditions at each welded position is specifically as follows: extracting images of each connection component position in the laid area collected by a high-definition camera, and then extracting images of each welded connection component position therefrom, which are recorded as monitoring images.

[0052] The monitoring images are processed by image processing software to identify the existing abnormal positions, locate the abnormal positions corresponding to each monitoring image, compare the images of each abnormal position with the standard weld defect images stored in the data repository, and then obtain the defect type of each abnormal position.

[0053] It should be added that the monitoring image is compared with the normal image to determine whether there is an abnormality, and if so, the abnormal position is located.

[0054] Exemplarily, the defect type may be cracking of the solder layer or peeling of the solder layer.

[0055] The abnormal positions in the monitoring images are classified according to the defect types, and the number of defects corresponding to each defect type in each monitoring image is obtained by statistics. The defect area of ​​each abnormal position is obtained by using image processing software, and then the defect areas of the same defect type are accumulated to obtain the defect area corresponding to each defect type.

[0056] The number of defects corresponding to each defect type in each monitoring image and defect area Substitute into the analysis formula Get the connection anomaly index corresponding to the welded position ,in Indicates the area of ​​the solder layer at the abnormal position. Indicates the defect type number, .

[0057] It should be noted that the reason for selecting the number of defects and the defect area as influencing factors of the connection abnormality index of the welded position is: the strength of the welded connection directly determines the bearing capacity and stability of the structure. The increase in the number of defects and the defect area will weaken the connection strength of the welded joint and reduce the overall performance of the structure. In complex environments such as mines and tunnels, the safety performance of welding is particularly important. The increase in the number of defects and the defect area will increase the risk of failure of the welded joint during use, thereby posing a threat to the life safety of workers and the normal operation of production equipment.

[0058] Preferably, the connection risk situation of the unwelded position is as follows: extract the image of each connection component position in the laid area collected by a high-definition camera, and then extract the image of each unwelded connection component position therefrom, and record it as the target image.

[0059] The component connection positions in the target image are divided into several monitoring points at equal intervals, and the component spacing corresponding to each monitoring point is obtained using image processing software.

[0060] For example, the spacing may be .

[0061] It should be noted that the reason for setting multiple monitoring points is: in practice, the component spacing at the component connection position may not change completely due to partial deformation and deviation of the connected components. Therefore, monitoring multiple sets of data can promptly detect abnormal situations.

[0062] The component spacing corresponding to each monitoring point is calculated by difference with the preset initial component spacing to obtain the component spacing deviation value, and then the absolute value of each component spacing deviation value is calculated by ratio with the initial component spacing to obtain the component spacing variation degree of each monitoring point.

[0063] It should be noted that the reason for the initial spacing between the components in the mine tunnel is to avoid the situation where the components are squeezed due to temperature and other reasons. For example, the initial component spacing is .

[0064] The component spacing variation at each monitoring point was compared, and the maximum component spacing variation was selected as the connection risk index of the unwelded position.

[0065] It should be noted that the reason for selecting the maximum component spacing variation as the connection risk index for unwelded positions is that in welding projects, slight changes in component spacing may have a significant impact on the stability of the overall structure. In particular, when the spacing variation reaches a certain degree, it may cause local stress concentration, deformation, or even failure of the structure. The maximum value usually represents the extreme or most unfavorable situation that may occur. During the welding process, even if most component spacing remains stable, significant changes in spacing at individual locations may also have a significant impact on the safety of the overall structure. Therefore, paying attention to the maximum value helps to identify and respond to these potential extreme risks.

[0066] Preferably, the step of locating each position to be welded in the laid area is as follows: comparing the connection abnormality index of each welded position with the preset allowable connection abnormality index; if the connection abnormality index of a welded position is greater than the allowable connection abnormality index, it is judged that the welded position needs to be welded again; if the connection abnormality index of a welded position is less than or equal to the allowable connection abnormality index, it is judged that the welded position does not need to be welded again.

[0067] For example, the allowed connection anomaly index is .

[0068] The connection risk index of each unwelded position is compared with the pre-set allowable connection risk index. If the connection risk index of an unwelded position is greater than the allowable connection risk index, it is judged that the unwelded position needs to be welded. If the connection risk index of an unwelded position is less than or equal to the allowable connection risk index, it is judged that the unwelded position does not need to be welded.

[0069] For example, the allowed connection risk index is .

[0070] The welded positions that are judged to need secondary welding and the unwelded positions that need welding are recorded as positions to be welded in the laid area.

[0071] It should be noted that the present invention obtains the required connection component types not mentioned in the construction plan based on the connection risk conditions of each unwelded position in the paved area, and then obtains the actual required connection component types in combination with the required connection component types in the construction plan. This analysis method can meet the needs of the actual construction environment and construction process, increase the adaptability and accuracy of the selection of welding connection components, enhance the stability and safety of the mine tunnel support frame, and can effectively reduce the risk of accidents caused by incomplete selection of welding connection components.

[0072] It should be noted that, for welded positions that require secondary welding, the weld layer of the initial welding needs to be removed and polished before the secondary welding operation is performed.

[0073] The to-be-laid area analysis module is used to obtain the required welding connection component type from the construction plan, and obtain the actual welding connection component type based on the connection risk situation of each unwelded position in the laid area, and then match it with the connection component type in the to-be-laid area to obtain each to-be-welded position in the to-be-laid area.

[0074] It should be added that the actual welding connection component type is obtained as follows: the connection risk index of each unwelded position in the laid area is compared with the pre-set allowable connection risk index. When the connection risk index of an unwelded position is greater than the allowable connection risk index, it is judged that the unwelded position needs to be welded. When the connection risk index of an unwelded position is less than or equal to the allowable connection risk index, it is judged that the unwelded position does not need to be welded.

[0075] For example, the allowed connection risk index is .

[0076] The types of connection components corresponding to the unwelded positions in the laid area that are judged to need welding are extracted, and then the number of unwelded positions that need to be welded of each type of connection component is counted, and the number of unwelded positions of each type of connection component in the laid area is counted, and the ratio of the number of unwelded positions that need to be welded of each type of connection component and the corresponding number of unwelded positions is calculated to obtain the ratio of the required welding quantity.

[0077] The proportion of welding quantity required for each type of connection component is compared with the preset proportion of welding quantity required to meet the standard. If the proportion of welding quantity required for a certain type of connection component is greater than or equal to the proportion of welding quantity required to meet the standard, it is determined that the connection component of this type needs to be welded.

[0078] For example, the proportion of welding quantity that meets the standard is .

[0079] It should be noted that the types of welding connection components required in the construction plan are connection components that are frequently used and prone to stability changes, as evaluated during the planning and construction phase.

[0080] The environmental information analysis module is used to set up mobile detection equipment, which includes a temperature detector, a humidity detector, a gas concentration sensor and a coal dust concentration sensor. The mobile detection equipment is used to collect real-time environmental information of each welding position, and the environmental information includes meteorological environmental information and risk environmental information.

[0081] The welding operation judgment module is used to analyze the construction risk situation of each welding position based on the risk environment information of each welding position, thereby judging whether the welding operation is allowed.

[0082] Preferably, the construction risk conditions include gas concentration risk and coal dust concentration risk, and the specific analysis steps are as follows: extracting the real-time gas concentration and real-time coal dust concentration of each welding position collected by the gas concentration sensor and the coal dust concentration sensor.

[0083] The difference between the real-time gas concentration of each welding position and the preset safe gas concentration threshold is calculated, and then the result of the difference calculation is compared with the safe gas concentration threshold to obtain the gas concentration risk.

[0084] For example, the safe gas concentration threshold is .

[0085] The difference between the real-time coal dust concentration of each welding position and the preset safe coal dust concentration threshold is calculated, and then the result of the difference calculation is compared with the safe coal dust concentration threshold to obtain the coal dust concentration risk.

[0086] For example, the safe coal dust concentration threshold is .

[0087] It should be noted that the reasons for choosing gas concentration risk and coal dust concentration risk as influencing factors of construction risk are: 1. Gas (mainly methane) is a common harmful gas in underground projects such as coal mines. As the mining depth of coal mines increases, the gas concentration may gradually increase. When the gas concentration reaches a certain range, it is very likely to explode if it encounters ignition conditions such as open flames and electric sparks, causing great harm to construction personnel and equipment; 2. Coal dust can ignite and produce violent explosions under certain conditions. Coal dust explosions are often related to gas explosions, forming more serious disasters. The power and destructive power of coal dust explosions are equally huge, posing a serious threat to coal mine safety production.

[0088] Preferably, the determination of whether the welding operation is allowed is specifically as follows: the gas concentration risk and the coal dust concentration risk are respectively compared with the preset allowable gas concentration risk and the allowable coal dust concentration risk, thereby obtaining a determination result of whether the welding operation is allowed.

[0089] For example, the allowable gas concentration risk and the allowable coal dust concentration risk are .

[0090] It should be added that when the gas concentration risk is greater than the allowable gas concentration risk or the coal dust concentration risk is greater than the allowable coal dust concentration risk, it is judged that welding operation is not allowed; when the gas concentration risk is less than or equal to the allowable gas concentration risk and the coal dust concentration risk is less than or equal to the allowable coal dust concentration risk, it is judged that welding operation is allowed.

[0091] The weld layer thickness correction module is used to analyze environmental abnormalities and operation and maintenance abnormalities based on the meteorological environment information and historical secondary welding records of each welding position when it is determined that the welding operation is allowed, thereby obtaining the weld layer thickness correction requirements of each welding position, and judging whether it is necessary to correct the system default initial weld layer thickness. If necessary, the initial weld layer thickness is corrected based on the weld layer thickness correction requirements.

[0092] For example, the initial solder layer thickness is .

[0093] It should be noted that the thickness of the weld layer has an impact on the connection components: the thickness of the weld layer directly affects the strength of the welded joint. Generally speaking, the thicker the weld layer, the higher the weld strength, because a thicker weld layer can provide a better material bonding area and stronger metal-to-metal bonding.

[0094] It should be noted that in the actual production process, the thickness of the weld layer should be comprehensively analyzed in combination with the environment in which the connected components are located and the properties of the welding materials.

[0095] Preferably, the abnormal environmental situation is analyzed as follows: extracting the temperature and humidity of each position to be welded detected by a temperature detector and a humidity detector.

[0096] The temperature of each welding position and humidity Substitute into the analysis formula Get the environmental anomaly index corresponding to the welding position ,in Indicates the suitable temperature. Indicates suitable humidity. represents a natural constant, Represent the weights of temperature and humidity respectively.

[0097] It should be noted that the suitable welding temperature and suitable welding humidity refer to the temperature and humidity that are suitable for welding operation and can ensure the welding quality. For example, , .

[0098] For example, .

[0099] It should be noted that temperature and humidity have the following effects on the connection components welded in mine tunnels: 1. When the welding temperature is too high, the organizational structure of the weld metal may change, thereby affecting the hardness, toughness and other mechanical properties of the weld. Excessive temperature may also cause defects such as cracks and pores in the weld, reducing the strength and reliability of the weld. 2. A high humidity environment will cause a large amount of moisture and gas to be adsorbed on the metal surface. These moisture and gases may enter the weld during the welding process, forming defects such as pores and slag inclusions, thereby reducing the quality of the weld.

[0100] Preferably, the abnormal operation and maintenance situation is analyzed as follows: extracting the temperature and humidity of each position to be welded detected by a temperature detector and a humidity detector.

[0101] The temperature and humidity corresponding to the historical secondary welding records are matched with the temperature and humidity of each position to be welded, and then the corresponding historical secondary welding records with the same temperature and humidity as each position to be welded are extracted and recorded as target historical secondary welding records. Each target historical secondary welding record corresponds to a type of connection component.

[0102] The connection component type corresponding to each target historical secondary welding record is obtained, and then the connection components of the same type are classified, and the number of historical secondary welding records corresponding to each type of connection components is obtained by counting.

[0103] The historical maintenance number corresponding to each type of connection component is counted, and the number of historical secondary welding records of each type is compared with the corresponding historical maintenance number to obtain the abnormality ratio corresponding to each type of connection component, which is then used as the operation and maintenance abnormality index corresponding to each type of connection component.

[0104] The type of connection component of each position to be welded is extracted, and then matched with the operation and maintenance anomaly index of each type of connection component to obtain the operation and maintenance anomaly index of each position to be welded.

[0105] Further preferably, the obtaining of the weld layer thickness correction requirement of each welding position is specifically as follows: the environment anomaly index and the operation and maintenance anomaly index of each welding position are summed up according to the weight to obtain the weld layer thickness correction requirement index of each welding position.

[0106] For example, the weights of the environment anomaly index and the operation and maintenance anomaly index are .

[0107] It should be noted that the present invention analyzes environmental impacts and operation and maintenance abnormalities based on the meteorological environment information of each welding position and the historical secondary welding records, and then determines whether it is necessary to correct the system's default initial weld layer thickness. This method of determining the type of connection component can accurately adjust the initial weld layer thickness to ensure that the mechanical properties of the welded connection component meet the requirements and that the welding quality is not affected. At the same time, it avoids the occurrence of unnecessary excessive weld layer thickness and reduces material waste. By improving welding quality, the subsequent maintenance and repair costs caused by welding defects can be reduced.

[0108] Preferably, the judgment on whether the system default initial weld layer thickness needs to be corrected is specifically as follows: the weld layer thickness correction requirement index of each welding position to be welded is compared with the preset standard weld layer thickness correction requirement index to obtain a judgment result on whether the initial weld layer thickness needs to be corrected.

[0109] Exemplarily, the required index for correcting the thickness of the welding layer to meet the standard is .

[0110] It should be supplemented that, when the weld layer thickness correction requirement index of a certain welding position to be welded is greater than or equal to the standard weld layer thickness correction requirement index, it is judged that the initial weld layer thickness of the welding position to be welded needs to be corrected; when the weld layer thickness correction requirement index of a certain welding position to be welded is less than the standard weld layer thickness correction requirement index, it is judged that the initial weld layer thickness of the welding position to be welded does not need to be corrected.

[0111] The data repository is used to store mine tunnel construction schedules, construction plans, standard weld defect images and historical secondary welding records.

[0112] The above contents are merely examples and explanations of the concept of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the concept of the invention or exceed the scope defined by the present invention, they shall all fall within the protection scope of the present invention.

Claims

1. An intelligent control system for welding of mining equipment components, characterized in that: include: The laying area division module is used to extract the mine tunnel construction progress book, and then obtain the laid area where the support frame has been laid and the to-be-laid area where the support frame has not been laid from the mine tunnel construction progress book; The laid area analysis module is used to use a high-definition camera to collect images of the positions of each connected component in the laid area, and then identify the images to divide the positions of each connected component into welded positions and unwelded positions, thereby analyzing the connection abnormalities of each welded position and the connection risks of the unwelded position, and then locating each position to be welded in the laid area; The analysis module of the area to be laid is used to obtain the required welding connection component type from the construction plan, and obtain the actual welding connection component type based on the connection risk of each unwelded position in the laid area, and then match it with the connection component type in the area to be laid to obtain each position to be welded in the area to be laid; An environmental information analysis module is used to set up a mobile detection device, which includes a temperature detector, a humidity detector, a gas concentration sensor, and a coal dust concentration sensor. The mobile detection device is used to collect real-time environmental information of each welding position, and the environmental information includes meteorological environmental information and risk environmental information; A welding operation judgment module is used to analyze the construction risk situation of each welding position based on the risk environment information of each welding position, thereby judging whether the welding operation is allowed; The welding layer thickness correction module is used to analyze the abnormal environment and operation and maintenance abnormalities based on the meteorological environment information and historical secondary welding records of each welding position when it is determined that the welding operation is allowed, thereby obtaining the welding layer thickness correction requirements of each welding position, and judging whether the system default initial welding layer thickness needs to be corrected. If necessary, the initial welding layer thickness is corrected based on the welding layer thickness correction requirements; Data repository for storing mine tunnel construction schedules, construction plans, standard weld defect images and historical secondary welding records; The analysis of abnormal connection conditions at each welded position is as follows: Extracting an image of the position of each connection component in the laid area collected by a high-definition camera, and then extracting an image of the position of each welded connection component therefrom, which is recorded as a monitoring image; Use image processing software to process the monitoring images and identify the existing abnormal positions, locate the abnormal positions corresponding to each monitoring image, compare the images of each abnormal position with the standard weld defect images stored in the data repository, and then obtain the defect type of each abnormal position; The abnormal positions in the monitoring images are classified according to the defect types, and the number of defects corresponding to each defect type in each monitoring image is obtained by counting, and the defect area of ​​each abnormal position is obtained by using image processing software, and then the defect areas of the same defect type are accumulated to obtain the defect area corresponding to each defect type; The number of defects corresponding to each defect type in each monitoring image and defect area Substitute into the analysis formula Get the connection anomaly index corresponding to the welded position ,in Indicates the area of ​​the solder layer at the abnormal position. Indicates the defect type number, ; The abnormal environmental situation is analyzed as follows: Extract the temperature and humidity of each position to be welded detected by a temperature detector and a humidity detector; The temperature of each welding position and humidity Substitute into the analysis formula Get the environmental anomaly index corresponding to the welding position ,in Indicates the suitable temperature. Indicates suitable humidity. represents a natural constant, Represent the weights of temperature and humidity respectively.

2. The intelligent control system for welding of mining equipment components according to claim 1, characterized in that: The connection risk of the unwelded position is specifically analyzed as follows: Extracting an image of the position of each connection component in the laid area collected by a high-definition camera, and then extracting an image of the position of each unwelded connection component therefrom, and recording it as a target image; The component connection positions in the target image are divided into several monitoring points at equal intervals, and the component spacing corresponding to each monitoring point is obtained using image processing software; The component spacing corresponding to each monitoring point is calculated by difference with the preset initial component spacing to obtain the component spacing deviation value, and then the absolute value of each component spacing deviation value is calculated by ratio with the initial component spacing to obtain the component spacing variation degree of each monitoring point; The component spacing variation at each monitoring point was compared, and the maximum component spacing variation was selected as the connection risk index of the unwelded position.

3. The intelligent control system for welding of mining equipment components according to claim 2, characterized in that: The steps of locating each position to be welded in the laid area are as follows: The connection abnormality index of each welded position is compared with the preset allowable connection abnormality index. If the connection abnormality index of a welded position is greater than the allowable connection abnormality index, it is determined that the welded position needs to be welded again. If the connection abnormality index of a welded position is less than or equal to the allowable connection abnormality index, it is determined that the welded position does not need to be welded again. The connection risk index of each unwelded position is compared with the preset allowable connection risk index. If the connection risk index of an unwelded position is greater than the allowable connection risk index, it is determined that the unwelded position needs to be welded. If the connection risk index of an unwelded position is less than or equal to the allowable connection risk index, it is determined that the unwelded position does not need to be welded. The welded positions that are judged to need secondary welding and the unwelded positions that need welding are recorded as positions to be welded in the laid area.

4. The intelligent control system for welding of mining equipment components according to claim 1, characterized in that: The construction risk conditions include gas concentration risk and coal dust concentration risk. The specific analysis steps are as follows: Extracting the real-time gas concentration and real-time coal dust concentration of each welding position collected by the gas concentration sensor and the coal dust concentration sensor; The real-time gas concentration of each welding position is calculated by difference with the preset safe gas concentration threshold, and then the result of the difference calculation is calculated by ratio with the safe gas concentration threshold to obtain the gas concentration risk degree; The difference between the real-time coal dust concentration of each welding position and the preset safe coal dust concentration threshold is calculated, and then the result of the difference calculation is compared with the safe coal dust concentration threshold to obtain the coal dust concentration risk.

5. The intelligent control system for welding of mining equipment components according to claim 4, characterized in that: The determination of whether the welding operation is allowed is specifically as follows: The gas concentration risk and the coal dust concentration risk are respectively compared with the preset allowable gas concentration risk and the allowable coal dust concentration risk, thereby obtaining a judgment result on whether the welding operation is allowed.

6. The intelligent control system for welding of mining equipment components according to claim 1, characterized in that: The abnormal operation and maintenance situation is analyzed as follows: Extract the temperature and humidity of each position to be welded detected by a temperature detector and a humidity detector; Match the temperature and humidity corresponding to the historical secondary welding records with the temperature and humidity of each position to be welded, and then extract the corresponding historical secondary welding records with the same temperature and humidity as each position to be welded, and record them as target historical secondary welding records, each target historical secondary welding record corresponds to a type of connection component; Obtain the connection component type corresponding to each target historical secondary welding record, and then classify them according to the same connection component type, and obtain the number of historical secondary welding records corresponding to each type of connection component by counting; The historical maintenance number corresponding to each type of connection component is counted, and the number of historical secondary welding records of each type is compared with the corresponding historical maintenance number to obtain the abnormal proportion corresponding to each type of connection component, which is then used as the operation and maintenance abnormality index corresponding to each type of connection component; The type of connection component of each position to be welded is extracted, and then matched with the operation and maintenance abnormality index of each type of connection component to obtain the operation and maintenance abnormality index of each position to be welded.

7. The intelligent control system for welding of mining equipment components according to claim 6, characterized in that: The requirements for obtaining the thickness correction of the weld layer at each position to be welded are as follows: The environmental anomaly index and the operation and maintenance anomaly index of each welding position are summed up according to the weight to obtain the welding layer thickness correction requirement index of each welding position.

8. The intelligent control system for welding of mining equipment components according to claim 7, characterized in that: The determination of whether the system default initial welding layer thickness needs to be corrected is as follows: The weld layer thickness correction requirement index of each to-be-welded position is compared with the preset standard weld layer thickness correction requirement index to obtain a judgment result on whether the initial weld layer thickness needs to be corrected.