An enhanced trench gate gallium oxide switch device and a method for preparing the same

By adopting a trench gate structure and a high K dielectric alumina current barrier layer in gallium oxide switching devices, combined with the design of Si-low resistance layer and n+ source region, the resistance of gallium oxide devices in high voltage and high frequency applications is solved. The problem of insufficient pressure and control capabilities achieves higher performance and lower costs.

CN118693159BActive Publication Date: 2024-11-15SHENZHEN GANG CHEUNG FAIR ELECTRONICS
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411174000.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-26
Publication Date
2024-11-15
Estimated Expiration
2044-08-26

AI Technical Summary

Technical Problem

The existing gallium oxide switching devices have limited voltage withstandability, high on-resistance and insufficient gate control capabilities in high voltage and high frequency applications, which limit their application potential in high-performance power electronic systems.

Method used

Using enhanced trench gate gallium oxide switching device, the Si-low resistance layer and n+ source are introduced by designing the trench gate structure in the longitudinal device, combining high K dielectric alumina gate dielectric and undoped gallium oxide current barrier layer. The region, optimizes the device structure and manufacturing process, including specific layer thickness and doping concentration design, and uses hydride gas-phase epitaxial method and magnetron sputtering technology for thin film deposition.

Benefits of technology

The device's voltage withstandability and gate control capabilities are significantly improved, on-resistance and leakage current are reduced, performance is improved, and manufacturing costs are reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118693159B_ABST
    Figure CN118693159B_ABST
Patent Text Reader

Abstract

The present invention discloses an enhanced trench gate gallium oxide switch device and a preparation method thereof, which relates to the field of semiconductor technology, including a drain metal, a gate dielectric is arranged in the middle above the drain metal, an n+ substrate is arranged on the outside of the gate dielectric, a current blocking layer is arranged above the n+ substrate, a Si-low-resistance layer is arranged above the current blocking layer, an n+ source region is arranged above the Si-low-resistance layer, a source metal is arranged above the n+ source region, and a gate metal is arranged in a dielectric groove of the gate dielectric. By adopting a vertical bottom-up structural design and combining the trench gate technology, the control ability of the gate is effectively enhanced, and at the same time, by introducing the Si-low-resistance layer below the n+ source region, the on-resistance is significantly reduced; the wide bandgap gallium oxide material of the current blocking layer enables the device to withstand higher voltages and reduce leakage current, which not only improves the performance of the device but also reduces the manufacturing cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to an enhanced trench gate gallium oxide switch device and a preparation method thereof. Background Art

[0002] In the field of power electronics, the performance requirements for switching devices are constantly increasing, especially in high voltage and high frequency applications. Due to the limitations of their physical properties, traditional silicon-based semiconductor devices do not perform well in high voltage and high temperature environments, which limits their application in advanced power conversion and management systems. With the development of technology, gallium oxide (Ga2O3) semiconductor materials are considered to be ideal alternative materials that surpass traditional silicon devices due to their wide energy gap, high electron mobility and excellent thermal stability. However, existing gallium oxide switching devices still have some shortcomings in manufacturing processes and structural design. For example, traditional gallium oxide devices often face problems such as limited voltage resistance, high on-resistance and insufficient gate control capabilities, all of which limit their application potential in high-performance power electronic systems. Summary of the invention

[0003] In view of the deficiencies in the prior art, the present invention provides an enhanced trench-gate gallium oxide switch device and a method for preparing the same to solve the problems raised in the above-mentioned background technology.

[0004] To achieve the above object, the present invention provides the following technical solutions: an enhanced trench gate gallium oxide switch device, comprising a drain metal, the drain metal being located at the bottom of the device, a gate dielectric being arranged in the middle above the drain metal, an n+ substrate being arranged above the drain metal on the outside of the gate dielectric, a current blocking layer being arranged above the n+ substrate and being located outside the gate dielectric, a Si-low resistance layer being arranged above the current blocking layer, an n+ source region being arranged above the Si-low resistance layer and being located outside the gate dielectric, and a source metal being arranged above the n+ source region;

[0005] A gate metal is arranged in the dielectric groove of the gate dielectric, and the gate metal is flush with the height of the n+ source region and the gate dielectric.

[0006] To further optimize the technical solution, the device is a vertical device and adopts a trench gate structure.

[0007] To further optimize the technical solution, the gate dielectric is high-K dielectric aluminum oxide, and the gate metal is Al-Au alloy.

[0008] To further optimize the technical solution, the current blocking layer is undoped gallium oxide, and the corresponding withstand voltage level is 1600V~3300V.

[0009] To further optimize the technical solution, the thickness of the drain metal is 800nm, the thickness of the n+ substrate is 1200nm, the thickness of the current blocking layer is 10-20μm, the thickness of the Si-low resistance layer is 600nm, and the thickness of the n+ source region is 200nm.

[0010] To further optimize the technical solution, the bottom thickness of the dielectric groove of the gate dielectric is 30 nm thicker than the thickness of the n+ substrate, and the side wall width of the dielectric groove of the gate dielectric is 20 nm.

[0011] Further optimizing the technical solution, the doping concentration of the n+ substrate is 2×10 18 cm -3 The doping concentration of the Si-low resistance layer is 1×10 17 cm -3 The doping concentration of the n+ source region is 2×10 18 cm -3 .

[0012] A method for preparing an enhanced trench gate gallium oxide switch device is prepared based on the above-mentioned enhanced trench gate gallium oxide switch device, comprising the following specific steps:

[0013] S1. Deposit a protective layer on the β-type gallium oxide material of the n+ substrate, etch a through hole for the gate dielectric, etch gallium oxide along the through hole to form a gate dielectric, the etching depth is 1.2 μm, and then deposit aluminum oxide on the gate dielectric along the through hole, gasify the metal organic matter of aluminum at 1200° C., and then use carrier gas and oxygen to pass into the square gallium oxide material reaction chamber to cause a chemical reaction, and the reaction product is deposited to form an aluminum oxide film;

[0014] S2, growing a current blocking layer on the n+ substrate β-type gallium oxide material by hydride vapor phase epitaxy;

[0015] S3, depositing a barrier layer on the current blocking layer, etching a through hole of the gate dielectric again, and etching gallium oxide along the through hole to form a dielectric groove of the gate dielectric;

[0016] S4, depositing aluminum oxide in the dielectric groove along the through hole in step S3, gasifying the aluminum metal organic matter at 800° C. and then introducing the metal organic matter into the gallium oxide material reaction chamber together with carrier gas and oxygen to cause a chemical reaction, and the reaction product is deposited to form an aluminum oxide film;

[0017] S5, etching a through hole for the gate metal, and using magnetron sputtering along the through hole, in an argon atmosphere, high voltage produces glow discharge on the argon gas, which hits the metal target, causing it to splash and deposit inside the dielectric groove;

[0018] S6, removing the barrier layer formed in step S3, re-depositing a new barrier layer on the gate metal, etching out the Si-low resistance layer area, and implanting Si ions into the Si-low resistance layer with an implantation energy of 70-270kev;

[0019] S7, along the Si-low resistance layer area, Sn ion implantation is performed on the Si-low resistance layer with an implantation energy of 10-70kev to form an n+ source region;

[0020] S8, removing the barrier layer formed in step S3, re-depositing a new barrier layer on the n+ source region, etching out the source metal region, and depositing source metal.

[0021] To further optimize the technical solution, in steps S1 and S4, dry etching is used for etching, the RF power is 600 W, the chamber pressure is 1.5 Pa, the etching gas is sulfur hexafluoride and argon, and the flow ratio of sulfur hexafluoride to argon is 2:1.

[0022] The technical solution is further optimized. In step S2, the growth conditions are 900°C, the molar fraction of GaCl is 0.5; the intake speed of O2 is 0.03m / s; the molar fraction of O2 is 0.5; the intake speed of the separation gas N2 is 2.8m / s; and the distance from the n+ substrate to the nozzle is 15cm.

[0023] Compared with the prior art, the present invention provides an enhanced trench gate gallium oxide switch device and a preparation method thereof, which has the following beneficial effects:

[0024] The enhanced trench gate gallium oxide switch device and its preparation method adopt a vertical bottom-up structural design and combine trench gate technology to effectively enhance the control ability of the gate. At the same time, by introducing a Si-low resistance layer under the n+ source region, the on-resistance is significantly reduced; the wide bandgap gallium oxide material of the current blocking layer enables the device to withstand higher voltages while reducing leakage current, which not only improves the performance of the device but also reduces the manufacturing cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A schematic cross-sectional view of an enhanced trench-gate gallium oxide switch device proposed by the present invention;

[0026] Figure 2 A schematic cross-sectional view of a device in step S1 of a method for preparing an enhanced trench-gate gallium oxide switch device proposed in the present invention;

[0027] Figure 3 A schematic cross-sectional view of a device in step S2 of a method for preparing an enhanced trench-gate gallium oxide switch device proposed in the present invention;

[0028] Figure 4 A schematic cross-sectional view of a device in step S3 of a method for preparing an enhanced trench-gate gallium oxide switch device proposed in the present invention;

[0029] Figure 5 A schematic cross-sectional view of a device in step S4 of a method for preparing an enhanced trench-gate gallium oxide switch device proposed by the present invention;

[0030] Figure 6 A schematic cross-sectional view of a device in step S5 of a method for preparing an enhanced trench-gate gallium oxide switch device proposed by the present invention;

[0031] Figure 7 A schematic cross-sectional view of a device in step S6 of a method for preparing an enhanced trench-gate gallium oxide switch device proposed by the present invention;

[0032] Figure 8 A schematic cross-sectional view of a device in step S7 of a method for preparing an enhancement-mode trench-gate gallium oxide switch device proposed by the present invention;

[0033] Fig. 9 It is a schematic cross-sectional view of a device in step S8 in a method for preparing an enhancement-mode trench-gate gallium oxide switch device proposed in the present invention.

[0034] In the figure: 1. drain metal; 2. gate dielectric; 3. n+ substrate; 4. current blocking layer; 5. Si- low resistance layer; 6. n+ source region; 7. source metal; 8. gate metal. DETAILED DESCRIPTION

[0035] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Embodiment 1:

[0036] See also Figure 1 , an enhanced trench gate gallium oxide switching device, the device is a vertical device with the characteristics of high withstand voltage. The device adopts a trench gate structure and the gate has a strong control ability over the device.

[0037] The device includes a drain metal 1, which is located at the bottom of the device, a gate dielectric 2 is arranged in the middle above the drain metal 1, an n+ substrate 3 located above the drain metal 1 is arranged outside the gate dielectric 2, a current blocking layer 4 located outside the gate dielectric 2 is arranged above the n+ substrate 3, a Si-low-resistance layer 5 is arranged above the current blocking layer 4, an n+ source region 6 located outside the gate dielectric 2 is arranged above the Si-low-resistance layer 5, and a source metal 7 is arranged above the n+ source region 6. A gate metal 8 is arranged in the dielectric groove of the gate dielectric 2, and the gate metal 8 is flush with the height of the n+ source region 6 and the gate dielectric 2.

[0038] The gate dielectric 2 is high-K dielectric aluminum oxide, and the gate metal 8 is Al-Au alloy. The gate dielectric 2 is longitudinally distributed throughout the entire thickness range of the device. The gate dielectric 2 distributed in the n+ substrate 3 can withstand the high voltage from the substrate, improve the device gate voltage impact resistance to the drain, and improve the device reliability. The gate dielectric 2 uses high-K dielectric aluminum oxide, which can effectively suppress the gate leakage current of the device, reduce the off-state leakage current of the device, and improve the gate reliability of the device.

[0039] Wherein, the current blocking layer 4 is undoped gallium oxide, and the corresponding withstand voltage level is 1600V~3300V.

[0040] In this embodiment, the thickness of the drain metal 1 is 800nm, the thickness of the n+ substrate 3 is 1200nm, the thickness of the current blocking layer 4 is 10-20μm, the thickness of the Si-low resistance layer 5 is 600nm, and the thickness of the n+ source region 6 is 200nm. The bottom thickness of the dielectric groove of the gate dielectric 2 is 30nm higher than the thickness of the n+ substrate 3, and the sidewall width of the dielectric groove of the gate dielectric 2 is 20nm.

[0041] The thickness of the drain metal 1 and the n+ substrate 3 is designed to ensure the support of the drain metal 1 and the n+ substrate 3 during the process preparation to meet the preparation of the thick current blocking layer 4.

[0042] The thickness of the gate dielectric 2 is designed because when the device is turned off, the positive voltage at the drain increases, and there must be a sufficient thickness of the gate dielectric 2 to ensure that the large voltage at the drain does not break through the gate dielectric 2 at the bottom of the device.

[0043] In this embodiment, the doping concentration of the n+ substrate 3 is 2×10 18 cm -3 The doping concentration of the Si-low-resistance layer 5 is 1×10 17 cm -3 The doping concentration of the n+ source region 6 is 2×10 18 cm-3 .

[0044] Since it is difficult to achieve p-type doping in gallium oxide at present and the p-type leakage is large, there is no p-type doping structure inside the device, which can reduce the device manufacturing process cost and reduce the leakage current of the device; since the cost of n+ doping of the device increases sharply with the increase of depth, the device adopts an n+ source region 6 and Si-low resistance layer 5 structure to reduce the on-resistance of the device.

[0045] At the same time, the voltage resistance of the device is achieved by the current blocking layer 4. The wide bandgap gallium oxide of the current blocking layer 4 has smaller leakage and stronger voltage resistance than the pn junction structure constructed by p-type doping. When a positive voltage is applied to the gate, the deep trench gate can realize the formation of a conductive channel for electrons on the left and right sides of the gate from the n+ source region 6 to the Si- low-resistance layer 5 to the drain, thereby realizing low-resistance conduction of the device.

[0046] The n+ source region 6 is used to form an ohmic contact with the source metal 7, but as the depth increases, the cost of n+ doping of gallium oxide increases rapidly, so a Si-low resistance layer 5 is constructed under the n+ source region 6 to reduce the on-resistance of the device at a lower cost. Embodiment 2:

[0047] A method for preparing an enhanced trench gate gallium oxide switch device is prepared based on the enhanced trench gate gallium oxide switch device described in Example 1, and comprises the following specific steps:

[0048] S1, such as Figure 2 As shown, a protective layer is deposited on the β-type gallium oxide material of the n+ substrate 3, a through hole of the gate dielectric 2 is etched, and gallium oxide is etched along the through hole to form the gate dielectric 2, and the etching depth is 1.2μm. Then, aluminum oxide is deposited on the gate dielectric 2 along the through hole, and the metal organic matter of aluminum is gasified at 1200°C (in order to increase the deposition speed of aluminum oxide) and then introduced into the square gallium oxide material reaction chamber together with carrier gas (generally argon gas) and oxygen (the ratio of the metal organic matter of aluminum to oxygen is 1:1), a chemical reaction occurs, and the reaction product is deposited to form an aluminum oxide film;

[0049] S2, such as Figure 3 As shown, a current blocking layer 4 is grown on the n+ substrate 3β-type gallium oxide material by using a hydride vapor phase epitaxy method;

[0050] The growth conditions are 900°C, the molar fraction of GaCl is 0.5; the gas inlet velocity of O2 is 0.03 m / s; the molar fraction of O2 is 0.5; the gas inlet velocity of the separation gas N2 is 2.8 m / s; the distance between the n+ substrate 3 and the nozzle is 15 cm;

[0051] S3, such as Figure 4As shown, a barrier layer is deposited on the current blocking layer 4, a through hole of the gate dielectric 2 is etched again, and gallium oxide is etched along the through hole to form a dielectric groove of the gate dielectric 2;

[0052] S4, such as Figure 5 As shown, aluminum oxide is deposited in the dielectric groove along the through hole in step S3, and the aluminum metal organic matter is gasified at 800° C. and then introduced into the square gallium oxide material reaction chamber together with carrier gas and oxygen to cause a chemical reaction, and the reaction product is deposited to form an aluminum oxide film;

[0053] S5, such as Figure 6 As shown, a through hole of the gate metal 8 is etched, and magnetron sputtering is used along the through hole. In an argon atmosphere, high pressure generates glow discharge on the argon gas, which hits the metal target material, causing it to splash and deposit inside the dielectric groove;

[0054] S6, such as Figure 7 As shown, the barrier layer formed in step S3 is removed, a new barrier layer is re-deposited on the gate metal 8, the Si-low-resistance layer 5 region is etched out, and Si-low-resistance layer 5 is implanted with Si ions, with an implantation energy of 70-270kev;

[0055] S7, such as Figure 8 As shown, along the Si-low-resistance layer 5 region, Sn ions are implanted above the Si-low-resistance layer 5 with an implantation energy of 10-70kev to form an n+ source region 6;

[0056] S8, such as Fig. 9 As shown, the barrier layer formed in step S3 is removed, a new barrier layer is re-deposited on the n+ source region 6, the source metal 7 region is etched out, and the source metal 7 is deposited.

[0057] In this embodiment, dry etching is used for etching, the radio frequency power is 600 W, the chamber pressure is 1.5 Pa, the etching gas is sulfur hexafluoride and argon, and the flow ratio of sulfur hexafluoride to argon is 2:1.

[0058] The beneficial effects of the present invention are:

[0059] The enhanced trench gate gallium oxide switch device and its preparation method adopt a vertical bottom-up structural design and combine trench gate technology to effectively enhance the control ability of the gate. At the same time, by introducing a Si-low resistance layer under the n+ source region, the on-resistance is significantly reduced; the wide bandgap gallium oxide material of the current blocking layer enables the device to withstand higher voltages while reducing leakage current, which not only improves the performance of the device but also reduces the manufacturing cost.

[0060] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.

[0061] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. An enhanced trench gate gallium oxide switching device, characterized in that: The device comprises a drain metal, wherein the drain metal is located at the bottom of the device, a gate dielectric is arranged in the middle above the drain metal, an n+ substrate located above the drain metal is arranged outside the gate dielectric, a current blocking layer located outside the gate dielectric is arranged above the n+ substrate, a Si-low-resistance layer is arranged above the current blocking layer, an n+ source region located outside the gate dielectric is arranged above the Si-low-resistance layer, and a source metal is arranged above the n+ source region; A gate metal is disposed in the dielectric groove of the gate dielectric, and the gate metal is flush with the height of the n+ source region and the gate dielectric; The method for preparing the device comprises the following specific steps: S1. Deposit a protective layer on the β-type gallium oxide material of the n+ substrate, etch a through hole for the gate dielectric, etch gallium oxide along the through hole to form a gate dielectric, the etching depth is 1.2 μm, and then deposit aluminum oxide on the gate dielectric along the through hole, gasify the metal organic matter of aluminum at 1200° C., and then use carrier gas and oxygen to pass into the square gallium oxide material reaction chamber to cause a chemical reaction, and the reaction product is deposited to form an aluminum oxide film; S2, growing a current blocking layer on the n+ substrate β-type gallium oxide material by hydride vapor phase epitaxy; S3, depositing a barrier layer on the current blocking layer, etching a through hole of the gate dielectric again, and etching gallium oxide along the through hole to form a dielectric groove of the gate dielectric; S4, depositing aluminum oxide in the dielectric groove along the through hole in step S3, gasifying the aluminum metal organic matter at 800° C. and then introducing the metal organic matter into the gallium oxide material reaction chamber together with carrier gas and oxygen to cause a chemical reaction, and the reaction product is deposited to form an aluminum oxide film; S5, etching a through hole for the gate metal, and using magnetron sputtering along the through hole, in an argon atmosphere, high voltage produces glow discharge on the argon gas, which hits the metal target, causing it to splash and deposit inside the dielectric groove; S6, removing the barrier layer formed in step S3, re-depositing a new barrier layer on the gate metal, etching out the Si-low resistance layer area, and implanting Si ions into the Si-low resistance layer with an implantation energy of 70-270kev; S7, along the Si-low resistance layer area, Sn ion implantation is performed on the Si-low resistance layer with an implantation energy of 10-70kev to form an n+ source region; S8, removing the barrier layer formed in step S3, re-depositing a new barrier layer on the n+ source region, etching out the source metal region, and depositing source metal.

2. The enhancement-mode trench-gate gallium oxide switch device according to claim 1, characterized in that: The device is a vertical device and adopts a trench gate structure.

3. The enhancement-mode trench-gate gallium oxide switch device according to claim 1, characterized in that: The gate dielectric is high-K dielectric aluminum oxide, and the gate metal is Al-Au alloy.

4. The enhancement-mode trench-gate gallium oxide switch device according to claim 1, characterized in that: The current blocking layer is undoped gallium oxide, and the corresponding withstand voltage level is 1600V~3300V.

5. The enhancement-mode trench-gate gallium oxide switch device according to claim 1, characterized in that: The thickness of the drain metal is 800nm, the thickness of the n+ substrate is 1200nm, the thickness of the current blocking layer is 10-20μm, the thickness of the Si-low resistance layer is 600nm, and the thickness of the n+ source region is 200nm.

6. The enhancement-mode trench-gate gallium oxide switch device according to claim 1, characterized in that: The bottom thickness of the dielectric groove of the gate dielectric is 30 nm thicker than the thickness of the n+ substrate, and the side wall width of the dielectric groove of the gate dielectric is 20 nm.

7. The enhancement-mode trench-gate gallium oxide switch device according to claim 1, characterized in that: The doping concentration of the n+ substrate is 2×10 18 cm -3 The doping concentration of the Si-low resistance layer is 1×10 17 cm -3 The doping concentration of the n+ source region is 2×10 18 cm -3 .

8. The enhancement-mode trench-gate gallium oxide switch device according to claim 1, characterized in that: In the steps S1 and S4, dry etching is used for etching, the radio frequency power is 600 W, the chamber pressure is 1.5 Pa, the etching gas is sulfur hexafluoride and argon, and the flow ratio of sulfur hexafluoride to argon is 2:

1.

9. The enhancement-mode trench-gate gallium oxide switch device according to claim 1, characterized in that: In step S2, the growth conditions are 900°C, the molar fraction of GaCl is 0.5; the intake speed of O2 is 0.03m / s; the molar fraction of O2 is 0.5; the intake speed of the separation gas N2 is 2.8m / s; and the distance from the n+ substrate to the nozzle is 15cm.

Citation Information

Patent Citations

  • Longitudinal power device for low-ratio on-resistance employing groove structure with high dielectric constant

    CN102779836A

  • Broad-band gap semiconductor vertical double diffusion metal oxide semiconductor field effect transistor having composite dielectric layer and manufacturing method thereof

    CN107437566A

  • Gallium oxide transistor and preparation method

    CN116722042A

  • Ga2O3 SEMICONDUCTOR ELEMENT

    US20140217405A1

  • Vertical gallium oxide transistor and preparation method therefor

    WO2024050865A1