Mould and eyebrow pencil tube production process using same
By designing a hydraulically controlled mold and utilizing the fluidity differences of injection plastics with different melting points, the two materials are fitted and bonded during the manufacturing process of the eyebrow pencil tube, which solves the problem of low connection strength in the existing technology and improves production efficiency and Energy efficiency.
Patent Information
- Application Number
- CN202410850740.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-10-01
AI Technical Summary
In the manufacturing process of existing eyebrow pencil tubes, the joint strength of the two injection plastics is low, resulting in low production efficiency and energy waste.
Design a mold that uses a hydraulic mechanism to control partitions and protrusions to slide in the cavity. The cavity is divided into a first cavity and a second cavity. Injection plastics with different melting points are injected into different cavities. The difference in fluidity is used to make the two Materials are embedded and bonded to improve connection strength.
The connection strength between the two materials is improved, the process flow is shortened, the time to maintain the cavity temperature is reduced, and energy is saved.
Smart Images

Figure CN118721608A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of eyebrow pencil tube manufacturing, and more specifically, to a mold and an eyebrow pencil tube production process using the mold. Background Art
[0002] In the manufacturing process of eyebrow pencil tubes, injection molding is generally used for production. During the injection molding process, different parts of the eyebrow pencil tube may require different discharge materials, that is, multiple injection moldings are required. Usually, one injection plastic is first injected into the mold cavity, and after it is cooled and solidified, another injection plastic is injected into the mold cavity. The two injection plastics are bonded together and then cooled. However, the connection strength of the two materials on the eyebrow pencil tube produced by this method is low.
[0003] Therefore, a new solution needs to be proposed to solve this problem. Summary of the invention
[0004] In view of the deficiencies in the prior art, the object of the present invention is to provide a mold and a production process for an eyebrow pencil tube using the mold.
[0005] The above technical purpose of the present invention is achieved through the following technical scheme: a mold, including a main body and a cavity located in the main body, the main body is movably connected with a partition, when the partition is raised, the partition divides the cavity into a first cavity and a second cavity, the first cavity is connected to the outside world through a first feed port, and the second cavity is connected to the outside world through a second feed port, and a plurality of protrusions are fixedly connected to one side of the partition close to the first cavity, when the partition is folded, the partition and the protrusions are immersed in the main body, so that the first cavity and the second cavity are connected.
[0006] The present invention is further configured as follows: a hydraulic cavity and a sliding cavity that are interconnected are provided on the main body, the sliding cavity is located between the mold cavity and the hydraulic cavity, a hydraulic mechanism that is connected to the hydraulic cavity is fixedly connected to one side of the main body, and the hydraulic mechanism controls the partition and the protrusion to slide in the sliding cavity through the hydraulic cavity.
[0007] The present invention is further configured such that: the cross-sectional area of the connection between the sliding cavity and the hydraulic cavity is smaller than the cross-sectional area of the partition and the protrusion.
[0008] The present invention is further configured such that: the width of the protrusion at a side away from the partition is greater than the width of the protrusion at a side close to the partition.
[0009] A production process for an eyebrow pencil tube comprises the following steps:
[0010] S1, using a hydraulic mechanism to allow the partition and the protrusion to enter the cavity, dividing the cavity into a first cavity and a second cavity;
[0011] S2, injecting a first injection plastic in a molten state into the first cavity through the first feed port, and keeping the first injection plastic in a molten state;
[0012] S3, injecting a second injection plastic in a molten state into the second cavity through a second feed port, wherein the melting point of the first injection plastic is higher than that of the second injection plastic;
[0013] S4, cooling down so that the first shot plastic is in a semi-molten state while the second shot plastic is still in a molten state;
[0014] S5, the partition and the protrusion are retracted into the sliding cavity by the hydraulic mechanism, and a gap is formed in the first cavity where the protrusion was originally located. Due to the difference in fluidity, the second injection plastic first fills the gap;
[0015] S6, cooling down so that both the first injection plastic and the second injection plastic are in solid state;
[0016] S7. Take out the eyebrow pencil tube.
[0017] The present invention is further configured such that: S3 and S4 are started synchronously, and when the injection of the second injection plastic is completed, the first injection plastic is transformed from a molten state to a semi-molten state.
[0018] The present invention is further configured such that: the ratio of the melting point of the first injection plastic to the melting point of the second injection plastic is in the range of 1.5 to 2.
[0019] The present invention is further configured such that the ratio of the temperature in S4 to the melting point of the second injection plastic is in the range of 1.2 to 1.4.
[0020] In summary, the present invention has the following beneficial effects: the temperature in the mold cavity is maintained at a first temperature higher than the melting point of the first injection plastic, thereby ensuring the fluidity of the first injection plastic, and further ensuring that the first injection plastic can fill the first cavity; the melting point of the first injection plastic is higher than the melting point of the second injection plastic, thereby ensuring the fluidity of the second injection plastic, and further ensuring that the second injection plastic can fill the second cavity; when the two materials are completely solidified, they are interlocked and bonded to each other at the junction of the first cavity and the second cavity, thereby ensuring the connection strength between the two materials; starting steps S3 and S4 at the same time shortens the process flow, improves work efficiency, reduces the time for maintaining the mold cavity temperature, and saves the energy required to maintain the temperature. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a structural schematic diagram of embodiment 1;
[0022] Figure 2 is a cross-sectional view of embodiment 1;
[0023] Figure 3 It is a schematic diagram of the structure of the partition;
[0024] Figure 4This is a flow chart of Embodiment 2;
[0025] Figure 5 This is a flow chart of Example 3.
[0026] In the figure: 1. main body; 2. partition; 3. first cavity; 4. second cavity; 5. first feed port; 6. second feed port; 7. protrusion; 8. hydraulic cavity; 9. sliding cavity; 10. hydraulic mechanism. DETAILED DESCRIPTION
[0027] The present invention is described in detail below in conjunction with the accompanying drawings and embodiments.
[0028] Embodiment 1: A mold, such as Figure 1 , Figure 2 , Figure 3 As shown, it includes a main body 1 and a cavity located in the main body 1, and a partition 2 is movably connected to the main body 1. When the partition 2 is raised, the partition 2 divides the cavity into a first cavity 3 and a second cavity 4. The first cavity 3 is connected to the outside through a first feed port 5, and the second cavity 4 is connected to the outside through a second feed port 6. A plurality of protrusions 7 are fixedly connected to one side of the partition 2 close to the first cavity 3. When the partition 2 is folded, the partition 2 and the protrusions 7 are immersed in the main body 1, so that the first cavity 3 and the second cavity 4 are connected.
[0029] Specifically, the main body 1 includes an outer shell and an inner core, the cavity is located between the outer shell and the inner core, the two partitions 2 are both located in the outer shell, and the partition 2 is located at the junction of the first cavity 3 and the second cavity 4. The partition 2 is close to the first cavity 3 and has three protrusions 7 integrally formed on one side. When the two partitions 2 are closed, the partition 2 and the protrusions 7 fit the outer side of the inner core and separate the cavity to form the first cavity 3 and the second cavity 4. The movement of the partition 2 is controlled to change whether the first cavity 3 and the second cavity 4 are connected to each other. When the partition 2 is folded, a gap is formed in the first cavity 3 where the protrusions 7 were originally located, thereby increasing the contact area of the materials in the first cavity 3 and the second cavity 4 and improving the connection strength between the two materials.
[0030] like Figure 2 , Figure 3 As shown, a hydraulic cavity 8 and a sliding cavity 9 which are interconnected are provided on the main body 1, and the sliding cavity 9 is located between the mold cavity and the hydraulic cavity 8. A hydraulic mechanism 10 which is connected to the hydraulic cavity 8 is fixedly connected to one side of the main body 1. The hydraulic mechanism 10 controls the partition 2 and the protrusion 7 to slide in the sliding cavity 9 through the hydraulic cavity 8. The cross-sectional area of the connection between the sliding cavity 9 and the hydraulic cavity 8 is smaller than the cross-sectional area of the partition 2 and the protrusion 7, and the width of the protrusion 7 away from the partition 2 is greater than the width of the protrusion 7 close to the partition 2.
[0031] Specifically, the hydraulic cavity 8 is located in the housing, the partition 2 and the protrusion 7 are both in the sliding cavity 9 and isolate the sliding cavity 9 from the cavity, the hydraulic mechanism 10 includes a hydraulic interface for connecting the hydraulic press, the hydraulic mechanism 10 transmits the pressure to the sliding cavity 9 through the hydraulic cavity 8, and then controls the movement of the partition 2 and the protrusion 7, the cross-sectional area of the connection between the sliding cavity 9 and the hydraulic cavity 8 is small, and the partition 2 and the protrusion 7 are prevented from entering the hydraulic cavity 8, the thickness of the protrusion 7 and the partition 2 is equal to the depth of the sliding cavity 9, and the depth of the sliding cavity 9 is greater than the depth of the cavity, that is, when the partition 2 and the protrusion When the mold cavity is divided into the first cavity 3 and the second cavity 4, the partition 2 and the protrusion 7 are still partially located in the sliding cavity 9, which prevents the partition 2 and the protrusion 7 from being separated from the sliding cavity 9, causing the hydraulic cavity 8 to be connected with the mold cavity through the sliding cavity 9, thereby ensuring the control of the partition 2 and the protrusion 7 by the hydraulic mechanism 10. The cross-section of the protrusion 7 is triangular, the tip of the triangle is connected to the partition 2, and the long side of the triangle is located on the side of the protrusion 7 away from the partition 2, that is, after the material in the second cavity 4 solidifies, it also presents a triangular structure embedded in the first cavity 3, further improving the connection strength between the two materials.
[0032] Embodiment 2: A production process of an eyebrow pencil tube, such as Figure 4 As shown, the following steps are included:
[0033] S1, using the hydraulic mechanism 10 to make the partition 2 and the protrusion 7 enter the cavity, dividing the cavity into a first cavity 3 and a second cavity 4;
[0034] S2, injecting a first injection plastic in a molten state into the first cavity 3 through the first feed port 5, and keeping the first injection plastic in a molten state;
[0035] S3, injecting a second injection plastic in a molten state into the second cavity 4 through the second feed port 6, wherein the melting point of the first injection plastic is higher than that of the second injection plastic;
[0036] S4, cooling down so that the first shot plastic is in a semi-molten state while the second shot plastic is still in a molten state;
[0037] S5, the partition 2 and the protrusion 7 are retracted into the sliding cavity 9 by the hydraulic mechanism 10, and a gap is formed in the first cavity 3 where the protrusion 7 was originally located. Due to the difference in fluidity, the second injection plastic first fills the gap;
[0038] S6, cooling down so that both the first injection plastic and the second injection plastic are in solid state;
[0039] S7. Take out the eyebrow pencil tube.
[0040] The ratio of the melting point of the first shot plastic to the melting point of the second shot plastic is in the range of 1.5 to 2, and the ratio of the temperature in S4 to the melting point of the second shot plastic is in the range of 1.2 to 1.4.
[0041] Specifically, the first injection plastic is PTFE, and the second injection plastic is HDPE. PTFE has good corrosion resistance and a melting point of 327°C. HDPE has good strength and a melting point of 130°C to 135°C. First, the hydraulic mechanism 10 applies pressure to the partition 2 and the protrusion 7 to separate the cavity. Then, the first injection plastic is injected into the first cavity 3 through the first feed port 5, and the temperature in the cavity is maintained at a first temperature higher than the melting point of the first injection plastic to ensure the fluidity of the first injection plastic, thereby ensuring that the first injection plastic can fill the cavity. The first cavity 3 is filled with the second injection plastic, and then the second injection plastic is injected into the second cavity 4 through the second feed port 6. The melting point of the first injection plastic is higher than that of the second injection plastic, so the first temperature is also higher than the melting point of the second injection plastic, which ensures the fluidity of the second injection plastic, and further ensures that the second injection plastic can fill the second cavity 4. The temperature in the cavity is lowered to the second temperature, which is higher than the melting point of the second injection plastic and lower than the melting point of the first injection plastic. That is, when the temperature drops to the second temperature, the second injection plastic is still in a molten state with good fluidity, while the first injection plastic is in a semi-molten state. In the molten state, the fluidity is greatly reduced. The partition 2 and the protrusion 7 are controlled by the hydraulic mechanism 10 to retract into the sliding cavity 9, that is, a gap appears at the original position of the partition 2 and the protrusion 7, and the second injection plastic is continuously injected. Because the fluidity of the second injection plastic is greater than the fluidity of the first injection plastic at this time, the second injection plastic first fills this part of the gap. After the temperature is briefly raised to near the melting point of the first injection plastic, it is cooled for the second time to a third temperature. The third temperature is lower than the melting point of the second injection plastic. The short heating makes the first injection plastic tend to the molten state, so that the second injection plastic and the first injection plastic are better integrated without destroying the distribution structure of the two. When the temperature is lowered to the third temperature, the two materials are completely solidified and are embedded and bonded to each other at the junction of the first cavity 3 and the second cavity 4, ensuring the connection strength between the two materials. The ratio of the melting point of the first injection plastic to the second injection plastic is small, which avoids the thermal decomposition of the second injection plastic at the first temperature. At the same time, the difference between the second temperature in S4 and the melting point of the first injection plastic is small, which ensures the bonding strength of the first injection plastic in the semi-molten state and the second injection plastic in the molten state.
[0042] Embodiment 3: A production process of an eyebrow pencil tube, such as Figure 5 As shown, the difference from the second embodiment is that S3 and S4 start synchronously, and when the injection of the second injection material is completed, the first injection material completes the transformation from the molten state to the semi-molten state.
[0043] Specifically, the first temperature reduction has begun when the second shot of plastic is injected, that is, the second shot of plastic does not have to withstand the first temperature, so that the melting point of the second shot of plastic can be smaller than that of the first shot of plastic, that is, the melting point difference range between the two materials is increased, and there are more material choices. At the same time, the two steps are started at the same time, which shortens the process flow, improves work efficiency, reduces the time for maintaining the cavity temperature, and saves the energy required to maintain the temperature.
[0044] The above is only a preferred embodiment of the present invention, and the protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.
Claims
1. A mold, characterized in that: It includes a main body and a cavity located in the main body, and a partition is movably connected to the main body. When the partition is raised, the partition divides the cavity into a first cavity and a second cavity. The first cavity is connected to the outside through a first feed port, and the second cavity is connected to the outside through a second feed port. A plurality of protrusions are fixedly connected to one side of the partition close to the first cavity. When the partition is folded, the partition and the protrusions are immersed in the main body, so that the first cavity and the second cavity are connected.
2. The mold according to claim 1, characterized in that: The main body is provided with a hydraulic cavity and a sliding cavity which are interconnected. The sliding cavity is located between the mold cavity and the hydraulic cavity. A hydraulic mechanism which is connected to the hydraulic cavity is fixedly connected to one side of the main body. The hydraulic mechanism controls the partition and the protrusion to slide in the sliding cavity through the hydraulic cavity.
3. The mold according to claim 2, characterized in that: The cross-sectional area of the connection between the sliding cavity and the hydraulic cavity is smaller than the cross-sectional area of the partition and the protrusion.
4. The mold according to claim 3, characterized in that: The width of the protrusion at a side away from the partition is greater than the width of the protrusion at a side close to the partition.
5. A production process for an eyebrow pencil tube, characterized in that: The following steps are involved: S1, using a hydraulic mechanism to allow the partition and the protrusion to enter the cavity, dividing the cavity into a first cavity and a second cavity; S2, injecting a first injection plastic in a molten state into the first cavity through the first feed port, and keeping the first injection plastic in a molten state; S3, injecting a second injection plastic in a molten state into the second cavity through a second feed port, wherein the melting point of the first injection plastic is higher than that of the second injection plastic; S4, cooling down so that the first shot plastic is in a semi-molten state while the second shot plastic is still in a molten state; S5, the partition and the protrusion are retracted into the sliding cavity by the hydraulic mechanism, and a gap is formed in the first cavity where the protrusion was originally located. Due to the difference in fluidity, the second injection plastic first fills the gap; S6, cooling down so that both the first injection plastic and the second injection plastic are in solid state; S7. Take out the eyebrow pencil tube.
6. The eyebrow pencil tube production process according to claim 5, characterized in that: S3 and S4 are started synchronously, and when the injection of the second injection plastic is completed, the first injection plastic is transformed from a molten state to a semi-molten state.
7. The eyebrow pencil tube production process according to claim 5, characterized in that: The ratio of the melting point of the first injection plastic to the melting point of the second injection plastic is in the range of 1.5 to 2.
8. The eyebrow pencil tube production process according to claim 7, characterized in that: The ratio of the temperature in S4 to the melting point of the second shot plastic is in the range of 1.2 to 1.4.