Method of manufacturing extrusion molded product
By using a sensor unit to monitor and adjust the speed of the puller during the manufacturing process of extrusion molded products, the problem of relaxation or over-stretching of core components caused by speed differences is solved, and the molding accuracy and quality of the product are improved.
Patent Information
- Application Number
- CN202410316420.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-03-29
- Filing Date
- 2024-03-20
- Publication Date
- 2024-10-01
AI Technical Summary
When manufacturing extrusion molded products, due to the speed difference between the first puller and the second puller, the core member is relaxed or overstretched, affecting the molding accuracy and quality of the product.
By arranging a sensor unit between the first puller and the second puller, the tension of the core member is monitored, and the drawing speed is adjusted according to the output of the sensor unit so that the tension falls within the normal range and prevents relaxation or excessive pulling. stretch.
It effectively prevents the reduction of molding accuracy and quality of extrusion molded products, ensuring stable manufacturing and high-quality output of products.
Smart Images

Figure CN118721653A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for manufacturing an extrusion molded product such as a weather strip, a decorative strip, and a sealing member mounted on an automobile, a two-wheeled vehicle, an outboard motor, etc. Background Art
[0002] Regarding core members used in extrusion molded products such as weather strips, decorative strips, and sealing parts mounted on automobiles, two-wheelers, outboard engines, etc., the material of these core members has been changed from metal to synthetic resin to achieve weight reduction and recycling, and to solve environmental problems, metal corrosion, and the like.
[0003] In the manufacturing method of the extrusion molded product using such a core member made of synthetic resin, the synthetic resin injected into the first extruder is molded into a core member having a desired shape by using a first mold, and then cooled in a first cooling pool. Then, the first pulling roller receives the core member and sends it to the second mold, and then, in the second mold, a covering portion made of a thermoplastic elastomer, such as a sealing portion or a lip portion, is provided on the outer periphery of the core member. In addition, although not shown, the core member is received by a second puller so as to pass through a second cooling pool (for example, see Japanese Patent No. 6589189 and Japanese Patent No. 6005311).
[0004] Prior art literature
[0005] Patent Document 1: Japanese Patent No. 6589189
[0006] Patent Document 2: Japanese Patent No. 6005311
[0007] However, it is difficult to operate the first puller and the second puller at exactly the same speed simply by setting the speeds of the first puller and the second puller, and there has been a problem that the speed difference between the first puller and the second puller causes a residual portion of the core member made of synthetic resin, thereby forming slack in the core member between the first puller and the second puller, or the speed difference generates excessive tension, causing excessive stretching of the core member and causing defects when a covering portion made of thermoplastic elastomer is provided on the periphery of the core member in the second mold, thereby reducing the quality of the extrusion molded product finally manufactured.
[0008] Specifically, in the case where a core member is molded in a first mold so as to have a desired shape and then a groove is formed in the core member to form an easily bendable extruded molded product as described in Japanese Patent No. 6589189 and Japanese Patent No. 6005311, or in the case where an easily bendable core member having a cross-section that is roughly I-shaped (having a flat plate-like shape) is molded in a first mold, since the core material is easily bendable, the core member is likely to form slack on the core member due to the speed difference between the first and second pullers to produce a residual portion, or excessive tension is generated due to the speed difference, resulting in excessive stretching of the core member. Summary of the invention
[0009] Therefore, the present invention is proposed to solve the above-mentioned problems, and an object of the present invention is to provide a method for manufacturing an extrusion molded product, which method can adjust the pulling speed so that the tension in the core member made of resin between the first puller and the second puller falls within a normal range, and can prevent the molding accuracy of the extrusion molded product from being reduced, the quality of the extrusion molded product from being reduced, etc.
[0010] In order to solve the above-mentioned problems, a method for manufacturing an extrusion molded product according to the present invention includes the following steps: pulling a core member made of resin and molded into a desired shape in a first mold by a first puller; and in a second mold, molding the extrusion molded product by providing a covering portion made of a thermoplastic elastomer on the periphery of the core member pulled by the first puller, and pulling the extrusion molded product by the second puller. A sensor unit for monitoring tension in the core member is provided between the first puller and the second puller, and at least one of the first puller and the second puller adjusts a pulling speed based on the tension in the core member monitored by the sensor unit, so that the tension in the core member between the first puller and the second puller falls within a normal range.
[0011] In the method for manufacturing an extrusion molded product according to the present invention, the sensor unit may include a core component feeding roller and a vertically movable tension applying roller, the core component feeding roller being arranged between a first puller and a second puller, a gap being formed between the core component feeding rollers along the direction in which the core component moves, the vertically movable tension applying roller being arranged between the core component feeding rollers in a manner capable of moving up and down and applying tension to the core component, and the sensor unit can monitor the tension in the core component based on the height of the vertically movable tension applying roller.
[0012] In the method for manufacturing an extrusion molded product according to the present invention, a cutting mechanism unit may be provided between the first mold and the first puller, and the cutting mechanism unit cuts the core member in a manner of forming a groove using a cutting blade. The sensor unit may apply tension to the core member having the groove formed therein by the cutting mechanism unit in a direction in which the core member is easily bent.
[0013] In the method for manufacturing an extrusion molded product according to the present invention, without stopping, the second puller can pull the extrusion molded product at a pulling speed having an upper limit speed and a lower limit speed based on the tension in the core member monitored by the sensor unit, each of which is within the range of ±12.5% of the pulling speed of the first puller.
[0014] In the method for manufacturing an extrusion molded product according to the present invention, without stopping, the first puller can pull the core member at a pulling speed having an upper limit speed and a lower limit speed based on the tension in the core member monitored by the sensor unit, each of which is within ±12.5% of the pulling speed of the second puller.
[0015] In the method for manufacturing an extrusion molded product according to the present invention, the tension in the core member made of resin is monitored by a sensor unit provided between a first puller and a second puller, and at least one of the first puller and the second puller adjusts its pulling speed so that the tension of the core member falls within a normal range. Therefore, the tension of the core member falls within a normal range between the first puller and the second puller, and the core member does not form slack or excessive stretching. Therefore, an extrusion molded product in which a covering portion made of a thermoplastic elastomer is provided on the periphery of a core member made of resin can be stably manufactured, and problems such as a decrease in molding accuracy of an extrusion molded product using a core member made of resin and a decrease in the quality of the extrusion molded product can be prevented. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 A side view showing one example of the entire manufacturing process in a method of manufacturing an extrusion molded product according to one embodiment of the present invention.
[0017] Figure 2 Shows Figure 1 A schematic diagram of a configuration example of a sensor unit is shown.
[0018] Figure 3A is a cross-sectional view of a core member made of synthetic resin. Figure 1 The first mold is molded so that its cross section is generally inverted U-shaped; Figure 3B is a cross-sectional view of a core member made of synthetic resin. Figure 1 The first mold shown is molded so that its cross-section is generally I-shaped.
[0019] Figure 4 Shows Figure 1 The schematic diagram of the configuration example of the cutting mechanism unit shown in FIG. 1 shows, for example, a state in which the cutting mechanism unit is used to cut the Figure 3A The core member shown, which is generally inverted U-shaped in cross section, has grooves formed therein.
[0020] Figure 5 Shows Figure 1 The schematic diagram of the configuration example of the cutting mechanism unit shown in FIG. 1 shows, for example, a state in which the cutting mechanism unit is used to cut the Figure 3B The core member shown, which is generally I-shaped in cross-section, has grooves formed therein.
[0021] Figure 6 A schematic diagram showing a state in which Figure 1 In the illustrated sensor unit, the vertically movable tension applying roller reaches the upper limit position β due to the tension in the core member exceeding a predetermined range, thereby turning on the upper contact sensor.
[0022] Figure 7 A schematic diagram showing a state in which Figure 1 In the illustrated sensor unit, the vertically movable tension applying roller reaches the lower limit position γ due to the tension in the core member falling below a predetermined range, thereby turning on the lower contact sensor.
[0023] Figure 8 A schematic diagram showing a dimensional tolerance table (ISO 3302-1 Class M) for rubber molded products.
[0024] Fig. 9 A cross-sectional view showing one example of a weathering strip manufactured by a method for manufacturing an extrusion molded product according to one embodiment of the present invention (in which a core member is made of a synthetic resin and has a substantially inverted U-shape in cross section).
[0025] Fig.10 A cross-sectional view showing one example of a weathering strip manufactured by a method for manufacturing an extrusion molded product according to one embodiment of the present invention (in which a core member is made of a synthetic resin and has a substantially I-shaped cross section).
[0026] Fig.11 Shows Figure 1 The diagram is a schematic diagram of a configuration example when a non-contact sensor (for example, an infrared sensor) is used in the sensor unit.
[0027] Fig.12 Shows Figure 1 The diagram shows an example of a configuration when a variable resistance sensor (such as a potentiometer or the like) is used in the sensor unit. DETAILED DESCRIPTION
[0028] The embodiment of the method for manufacturing an extrusion molded product according to the present invention will be described in detail below with reference to the accompanying drawings. It should be noted that the embodiment to be described below is only an example of the present invention. The present invention is not limited to the embodiment, and appropriate changes can also be made within the scope of the technical concept of the present invention.
[0029] Example of a manufacturing process for implementing a method of manufacturing an extrusion molded product according to an embodiment of the present invention
[0030] Figure 1 A schematic diagram showing an example of a manufacturing process for implementing a method of manufacturing an extrusion molded product according to an embodiment of the present invention.
[0031] like Figure 1 As shown, the manufacturing process for implementing the method for manufacturing an extrusion molded product according to an embodiment of the present invention includes a first extruder 11, a first die 12, a first cooling pool 13, a cutting mechanism unit 14, a first puller 15, a sensor unit 16, a heater 17, a second die 18, a second extruder 19, a third extruder 20, a fourth extruder 21, a second cooling pool 22, a second puller 23, a cutter 24, etc.
[0032] The configuration of the manufacturing process is basically the same as the method for manufacturing an extrusion molded product disclosed in the above-mentioned Japanese Patent No. 6589189 and the method for manufacturing an extrusion molded product disclosed in Japanese Patent No. 6005311, except for the sensor unit 16, so only the configuration of the sensor unit 16 will be described in detail. In addition, in the description of the present embodiment, a core member 1 that is roughly inverted U-shaped when viewed in cross section and a core member 1' that is roughly I-shaped (flat plate-like shape) when viewed in cross section will be described as examples of core members. However, the core members 1 and 1' are merely examples, and the present invention is not limited to the core members 1 and 1'. In addition, in Figure 1 In the case where there are unnecessary components in the illustrated configuration, for example, when the heater 17, the third extruder 20, the fourth extruder 21 or the like are not required, it is apparent that they may be omitted as appropriate.
[0033] Configuration of the sensor unit 16
[0034] Figure 2 Shows Figure 1 An example of the configuration of the sensor unit 16 is shown in FIG.
[0035] like Figure 1As shown, the sensor unit 16 is disposed between the first puller 15 and the second puller 23 so as to be located upstream of the heater 17 and the second die 18 (so as to be before the heater 17 and the second die 18), and downstream of the first puller 15 (so as to be after the first puller 15). The sensor unit 16 continuously monitors the tension in the core member 1 in which the grooves 1a have been formed at desired intervals, and sends a control signal to at least one of the first puller 15 and the second puller 23 so that at least one of the first puller 15 and the second puller 23 adjusts its drawing speed so that the tension of the core member 1 between the first puller 15 and the second puller 23 falls within a normal range. Figure 2 As shown, the sensor unit 16 includes core member feeding rollers 16a and 16b, a vertically movable tension applying roller 16c, a vertically movable body 16d, an upper contact sensor 16e, a lower contact sensor 16f, a drawing speed control unit 16g, and the like.
[0036] The core member feeding rollers 16a and 16b are rollers for transversely feeding the core members 1 and 1', and at least a gap equal to or larger than the outer diameter of the vertically movable tension applying roller 16c is formed therebetween in the moving direction of the core members 1 and 1'.
[0037] The vertically movable tension-applying roller 16c is a roller rotatably supported on a vertically movable body 16d, which is configured to be able to move up and down. The roller uses its own weight and the weight of the vertically movable body 16d to apply tension to the core components 1 and 1' between the core component feed rollers 16a and 16b along the direction in which the core components 1 and 1' are easy to bend.
[0038] More specifically, in Figure 4 In the case where the cross section of the core member 1 shown is generally inverted U-shaped and the grooves 1a are formed on both side surfaces of the core member 1, if the grooves 1a are not formed in the core member 1, the core member 1 is not easy to bend in the vertical direction. However, since the grooves 1a are formed in both side surfaces of the core member 1, the core member 1 can be easily bent along the vertical direction. Figure 4 In addition, the core member 1' is made of synthetic resin and is as Figure 5In the case where the cross-section of the core member 1' shown is roughly I-shaped and the two side surfaces of the core member 1' have been formed with grooves 1a', the core member 1' can be easily bent in the vertical direction, which is the thickness direction of the core member 1', regardless of whether the grooves 1a' are present. Therefore, each of the core members 1 and 1' is placed in the sensor unit 16 so that the direction in which the core members 1 and 1' are easy to bend becomes parallel to the vertical direction, and passes through the core member feeding rollers 16a and 16b. Then, by utilizing the weight of the vertically movable tension applying roller 16c between the core member feeding rollers 16a and 16b and the weight of the vertically movable body 16d, tension is applied to the upper surface of each of the core members 1 and 1' from above.
[0039] The vertically movable body 16d is a slider or the like, which supports the vertically movable tension applying roller 16c so that the vertically movable tension applying roller 16c is rotatable, and is provided in the sensor unit 16 via a linear guide (not shown) or the like so as to be movable up and down. It is to be noted that the degree of difficulty with which the core members 1 and 1' can be bent varies depending on the shape, thickness, etc. of the core members 1 and 1', and therefore, it is preferred that a weight or the like be provided on the vertically movable tension applying roller 16c and the vertically movable body 16d in accordance with the tension applied to each of the core members 1 and 1' so as to adjust the tension applied to each of the core members 1 and 1'.
[0040] The upper contact sensor 16e and the lower contact sensor 16f are contact sensors such as switches, which detect whether the vertically movable body 16d is in contact therewith, and the vertically movable body 16d supports the vertically movable tension applying roller 16c that applies tension to the core member 1 passing between the core member feeding rollers 16a and 16b.
[0041] The drawing speed control unit 16g is a control unit that receives a sensor output from the upper contact sensor 16e when the vertically movable body 16d is in contact with the upper contact sensor 16e, receives a sensor output from the lower contact sensor 16f when the vertically movable body 16d is in contact with the lower contact sensor 16f, and outputs a drawing speed adjustment instruction to at least one of the first puller 15 and the second puller 23 to adjust at least one of the first drawing speed of the first puller 15 and the second drawing speed of the second puller 23 so that the tension in the core member 1 between the first puller 15 and the second puller 23 falls within a normal range.
[0042] Method of manufacturing extrusion molded product according to embodiment
[0043] A method of manufacturing an extrusion molded product according to an embodiment of the present invention will now be described, in which method the sensor unit 16 configured in the above-described manner is newly provided in a part of the manufacturing process.
[0044] like Figure 1 As shown, in the method for manufacturing an extrusion molded product according to an embodiment of the present invention, the thermoplastic resin injected into the first extruder 11 is molded into a desired shape in the first mold 12, that is, formed into a synthetic resin such as Figure 3A The core member 1 having a substantially inverted U-shaped cross section as shown or made of synthetic resin, such as Figure 3B The core member 1' shown having a generally I-shaped cross section is cooled in a first cooling pool 13 while its shape is controlled by a first cooling sizer 13a so as to correspond to the most suitable shape of an extrusion molded product (e.g., a weather strip, decorative strip or sealing component mounted on an automobile, a two-wheeled vehicle, an outboard engine or the like).
[0045] It should be noted that as the synthetic resin used for the core member 1, for example, an olefin-based resin such as polypropylene having a type A durometer hardness (Shore A) of 85 or more, or a mixed synthetic resin obtained by mixing 20% by weight to 50% by weight of talc or wollastonite powder into the olefin-based resin can be used. However, the present invention is not particularly limited thereto.
[0046] The core members 1 and 1 ′, each of which has been cooled by passing through the first cooling bath 13 and each of which has a desired shape, are pulled by the first puller 15 at a first pulling speed and transferred to the cutting mechanism unit 14 .
[0047] In the cutting mechanism unit 14, grooves are formed in the core members 1 and 1' by a plurality of cutting blades 14a5 of a rotating body 14a4 which is rotated by a rotating shaft 14a3 arranged on both left and right sides of a holder 14a, as shown in FIG. Figure 4 and Figure 5 As shown. The core member 1 is made of synthetic resin and as Figure 4 In the case where the cross section of the core member 1 shown is generally inverted U-shaped, grooves 1a are formed at desired intervals on both left and right sides of the core member 1 in a continuous manner. Figure 5 In the case where the cross section of the core member 1 ′ is shown to be substantially I-shaped, grooves 1 a ′ are formed in a continuous manner at desired intervals on both left and right sides of the core member 1 ′.
[0048] Therefore, the holder 14a of the cutting mechanism unit 14 has a core member passage hole 14a1 formed so as to be aligned with the core member passage hole 14a1. Figure 3AThe cross-sectional shape of the core member 1 shown in FIG. 1 corresponds to the cross-sectional shape of the core member 1 which is substantially inverted U-shaped when viewed in cross section, or corresponds to the cross-sectional shape of the core member 1 as shown in FIG. Figure 3B The cross-sectional shape of the core member 1' shown in FIG. 1 corresponds to the cross-sectional shape of the core member 1' which is substantially I-shaped when viewed in cross section. Figure 4 and Figure 5 As shown, slits 14b and 14b are formed in the retainer 14a, and the slits are respectively located on the left and right sides of the retainer 14a and are offset from each other in the longitudinal direction of the core member 1, that is, displaced from each other. The slits 14b and 14b extend to the core member passage hole 14a1 and allow the rotating body 14a4 and the plurality of cutting blades 14a5 to pass through. It should be noted that in the following reference Figure 6 In the description of the following drawings, although the core member 1 is described as a representative example for the convenience of description, the same applies to the core member 1 ′.
[0049] The core member 1 , on which the grooves 1 a have been formed at desired intervals by the cutting mechanism unit 14 , is pulled by the first puller 15 at a first pulling speed and is transferred to the sensor unit 16 .
[0050] like Figure 2 As shown, in the sensor unit 16, the vertically movable tension applying roller 16c is located between the core member feeding rollers 16a and 16b. The core member 1 passes through the core member feeding roller 16a, the vertically movable tension applying roller 16c, and the core member feeding roller 16b in the sensor unit 16 in sequence, and is transferred to the second mold 18 via the heater 17. In this case, tension is applied to the core member 1 from one side of the upper surface of the core member 1, for example, by utilizing the weight of the vertically movable tension applying roller 16c and the weight of the vertically movable body 16d.
[0051] Here, since the vertically movable body 16d supporting the vertically movable tension applying roller 16c so that the vertically movable tension applying roller 16c can rotate is provided to be movable up and down, when the tension generated in the core member 1 between the first puller 15 and the second puller 23 becomes large, the vertically movable tension applying roller 16c and the vertically movable body 16d move upward. On the contrary, when the tension in the core member 1 becomes small, the vertically movable tension applying roller 16c and the vertically movable body 16d move downward.
[0052] A reference position α, an upper limit position β, and a lower limit position γ are set for the height of the vertically movable tension applying roller 16c, and the vertically movable tension applying roller 16c and the vertically movable body 16d move up and down within this range. The upper contact sensor 16e detects the height of the vertically movable tension applying roller 16c reaching the upper limit position β, and the lower contact sensor 16f detects the height of the vertically movable tension applying roller 16c reaching the lower limit position γ. The pulling speed control unit 16g optimally adjusts the difference between the first pulling speed of the first puller 15 and the second pulling speed of the second puller 23.
[0053] When the tension in the core member 1 between the first puller 15 and the second puller 23 is appropriate
[0054] When the tension in the core member 1 between the first puller 15 and the second puller 23 is appropriate, the weight of the vertically movable tension applying roller 16c, the vertically movable body 16d supporting the vertically movable tension applying roller 16c, and the like are in a balanced state with the tension in the core member 1. Figure 2 As shown, the vertically movable tension applying roller 16c does not move in the vertical direction or moves slightly in the vertical direction, so that the center of the vertically movable tension applying roller 16c is located near the reference position α, and the vertically movable body 16d does not contact the upper contact sensor 16e or the lower contact sensor 16f.
[0055] Therefore, in this case, neither the upper contact sensor 16e nor the lower contact sensor 16f outputs a sensor output to the drawing speed control unit 16g, and the drawing speed control unit 16g does not output a drawing speed adjustment instruction to the first puller 15 or the second puller 23, so that the first puller 15 and the second puller 23 pull the core member 1 without changing their drawing speeds.
[0056] When the tension in the core member 1 between the first puller 15 and the second puller 23 exceeds the appropriate range
[0057] (When the tension in the core member 1 between the first puller 15 and the second puller 23 becomes larger than the reference value)
[0058] When the tension in the core member 1 between the first puller 15 and the second puller 23 becomes greater than the reference value, the vertically movable tension applying roller 16c and the vertically movable body 16d supporting the vertically movable tension applying roller 16c move upward, and the position of the center of the vertically movable tension applying roller 16c moves upward from the reference position α. When the tension in the core member 1 exceeds the appropriate range and the position of the center of the vertically movable tension applying roller 16c reaches the upper limit position β, as shown in FIG. Figure 6As shown, the upper end portion of the vertically movable body 16d is in contact with the upper contact sensor 16e.
[0059] Then, the upper contact sensor 16e outputs a sensor output to the pulling speed control unit 16g, and the pulling speed control unit 16g transmits an acceleration command for increasing the first pulling speed to the first puller 15, or transmits a deceleration command for decreasing the second pulling speed to the second puller 23.
[0060] Therefore, at least one of the first pulling speed of the first puller 15 and the second pulling speed of the second puller 23 is adjusted, and the tension in the core member 1 between the first puller 15 and the second puller 23 falls within a normal range. Then, the vertically movable tension applying roller 16c moves downward, and the upper end portion of the vertically movable body 16d moves away from the upper contact sensor 16e and returns to the position close to the upper contact sensor 16e. Figure 2 The pulling speed control unit 16g does not output a speed change instruction to the first puller 15 or the second puller 23.
[0061] When the tension in the core member 1 between the first puller 15 and the second puller 23 is lower than the appropriate range
[0062] (When the tension in the core member 1 between the first puller 15 and the second puller 23 becomes smaller than the reference value)
[0063] When the tension in the core member 1 between the first puller 15 and the second puller 23 becomes smaller than the reference value, the core member 1 is relaxed between the first puller 15 and the second puller 23, and the position of the center of the vertically movable tension applying roller 16c moves downward from the reference position α, as shown in FIG. Figure 7 When the tension in the core member 1 drops below the appropriate range and the position of the center of the vertically movable tension applying roller 16c reaches the lower limit position γ, the lower end portion of the vertically movable body 16d contacts the lower contact sensor 16f.
[0064] Then, the lower contact sensor 16f outputs a sensor output to the drawing speed control unit 16g, and the drawing speed control unit 16g transmits a deceleration instruction for decreasing the first drawing speed to the first puller 15, or transmits an acceleration instruction for increasing the second drawing speed to the second puller 23. Therefore, at least one of the first drawing speed of the first puller 15 and the second drawing speed of the second puller 23 is adjusted, and the tension in the core member 1 between the first puller 15 and the second puller 23 falls within a normal range.
[0065] Therefore, the vertically movable tension applying roller 16c moves upward, and the lower end portion of the vertically movable body 16d moves away from the lower contact sensor 16f and returns to the position as shown in FIG. Figure 2 The pulling speed control unit 16g does not output a speed change instruction to the first puller 15 or the second puller 23.
[0066] Here, when the first puller 15 pulls the core member 1, the operation of the second puller 23 cannot be stopped due to the characteristics of extrusion molding; when the second puller 23 pulls the core member 1, the operation of the first puller 15 cannot be stopped due to the characteristics of extrusion molding. In other words, once the extrusion molded product starts to be manufactured, the first puller 15 and the second puller 23 will continuously pull the core member 1 or the extrusion molded product 10 without stopping. In addition, the change in the pulling speed of the first puller 15 and the second puller 23 affects the quality of the extrusion molded product 10, so each pulling speed cannot be controlled at an infinite speed.
[0067] Figure 8 Shown is a “Dimensional tolerance table for molded rubber products (ISO 3302-1M grade)” which is generally used as a standard for evaluating the molding dimensions of extrusion molded products made of thermoplastic resins.
[0068] exist Figure 8 In the table shown, in the case of size classification of [0 or more and less than 4] and [4 or more and less than 6.3], the tolerance of M4 grade rubber products relative to the reference size (i.e. 4) is ±0.5, that is, the minimum value of the tolerance is 3.5 and the maximum value is 4.5. The acceptable range of variation is (±0.5 / 4)×100=±12.5%.
[0069] The molding accuracy of the extrusion molded product 10 is related to the molding speed, and the increase or decrease of the cross section of the molded product is proportional to the molding speed. Therefore, when the tolerance of the M4 class is set to the maximum variation, it is necessary to control the speed difference between the two pullers 15 and 23 to 12.5% or less without stopping the pulling operation so as to synchronize the pulling speed of the first puller 15 with the pulling speed of the second puller 23.
[0070] Therefore, when the drawing speed control unit 16g of the sensor unit 16 controls the second drawing speed (which is the drawing speed of the second puller 23), the drawing speed control unit 16g controls without stopping the drawing operation so that the upper limit speed of the second drawing speed is 12.5% or less of the first drawing speed (which is the drawing speed of the first puller 15) and the lower limit speed of the second drawing speed is within the range of ±12.5% of the first drawing speed. When the drawing speed control unit 16g of the sensor unit 16 controls the drawing speed of the first puller 15, the drawing speed control unit 16g controls without stopping the drawing operation so that the upper limit speed of the first drawing speed is 12.5% or less of the second drawing speed and the lower limit speed of the first drawing speed is within the range of ±12.5% of the second drawing speed. Furthermore, in the case of synchronizing the pulling speeds by sending instructions to both the first puller 15 and the second puller 23 , the speed difference between the two pullers 15 and 23 is controlled to 12.5% or less without stopping the puller operations of the two pullers 15 and 23 .
[0071] It should be noted that, in the method for manufacturing an extrusion molded product according to an embodiment of the present invention, although control is performed so that the speed difference between the upper limit speed of the pulling speed of the first puller 15 and the upper limit speed of the pulling speed of the second puller 23 is 12.5% or less, and the speed difference between the lower limit speed of the pulling speed of the first puller 15 and the lower limit speed of the pulling speed of the second puller 23 is 12.5% or less, it is more preferable to control the speed difference between the upper limit speeds and the speed difference between the lower limit speeds to 4% or less. When the speed control of 4% or less is performed on both the high speed side and the low speed side, for the manufactured extrusion molded product 10, the variation range of the molding size is reduced compared with the case where the speed difference is 12.5% or less, and the accuracy of the product size can be further improved.
[0072] When the core member 1 passes through the holder 14a, grooves 1a are formed in the core member 1 at desired intervals in a continuous manner by the cutting blades 14a5 rotating on both the left and right sides so as to have a desired shape, after which the core member 1 is heated by the heater 17 as needed and enters the second mold 18, as shown in FIG. Figure 1 Then, using the thermoplastic elastomer extruded from the second extruder 19 to the fourth extruder 21, covering parts such as the body sealing lip portion 2, the hollow sealing portion 3 and the glass sealing lip portion 4 are formed on the outer periphery of the core member 1, thereby extrusion molding as shown. Fig. 9 An extrusion molded product 10 is configured as shown.
[0073] Here, as the synthetic resin used for the core member 1, for example, an olefin-based resin such as polypropylene having a type A durometer hardness (Shore A) of 85 or more, or a mixed synthetic resin obtained by mixing 20% by weight to 50% by weight of talc or wollastonite powder into the olefin-based resin can be used. However, the present invention is not particularly limited thereto.
[0074] Furthermore, as a thermoplastic elastomer for forming covering portions such as the body seal lip portion 2, the hollow seal portion 3, and the glass seal lip portion 4, a thermoplastic elastomer containing an olefin-based resin having a type A durometer hardness (Shore A) of 40 to 80 is used. As a soft thermoplastic elastomer for the hollow seal portion 3, a thermoplastic elastomer containing an olefin-based resin having a type A durometer hardness (Shore A) of 20 to 40 is used.
[0075] The extrusion molded product 10 to which the cover portion has been provided in the second die 18 is transferred to the second cooling pool 22. In the second cooling pool 22, the extrusion molded product 10 passes through the second cooling setter 22a provided in the second cooling pool 22 as needed, and is pulled by the second puller 23. After passing through the second puller 23, the extrusion molded product 10 is cut by the cutter 24 to have a predetermined length.
[0076] Fig. 9 is a schematic diagram showing an example of a cross-sectional view of an extrusion molded product 10 which is a weathering strip manufactured by a method for manufacturing an extrusion molded product according to an embodiment of the present invention, Fig.10 is a schematic diagram showing an example of a cross-sectional view of an extrusion molded product 10 ′ which is a weathering strip manufactured by the method for manufacturing an extrusion molded product according to an embodiment of the present invention.
[0077] exist Fig. 9 In the extrusion molded product 10 shown, Figure 4 The grooves 1a shown are formed on the left and right sides of the core member 1, which is made of synthetic resin and has a substantially inverted U-shaped cross section. Figure 3A In addition, a body seal lip portion 2 made of a thermoplastic elastomer is formed on the outer periphery of the core member 1 by a second extruder 19, and a hollow seal portion 3 made of a soft thermoplastic elastomer is extrusion-molded on the outer side of the body seal lip portion 2 by a third extruder 20. A glass seal lip portion 4 to be mounted on a flange of a vehicle body is formed on the inner side of the core member 1 by a fourth extruder 21.
[0078] exist Fig.10 In the extrusion molded product 10' shown, Figure 5The grooves 1a' shown are formed on the left and right sides of the core member 1', and the core member 1' is made of synthetic resin and has a substantially I-shaped cross section. Figure 3B Furthermore, a cover portion 2' made of a thermoplastic elastomer is formed on the outer periphery of the core member 1'.
[0079] In the case where a thermoplastic elastomer or a synthetic resin of a different material is further added to the extrusion molded products 10 and 10', similarly to Figure 1 A fifth extruder, a sixth extruder, and so on are added in the manner of the second extruder 19 , the third extruder 20 , and the fourth extruder 21 shown in FIG. 1 , and co-extrusion molding is performed in the second die 18 .
[0080] Abstract of a method for manufacturing an extrusion molded product according to an embodiment of the present invention
[0081] As described above, in the method for manufacturing an extrusion molded product according to the present invention, the sensor unit 16 for monitoring the tension in the core member 1 is arranged between the first puller 15 and the second puller 23, and the sensor unit 16 adjusts at least one of the pulling speed of the first puller 15 and the pulling speed of the second puller 23 according to the tension in the core member 1 monitored by the sensor unit 16, so that the tension in the core member 1 between the first puller 15 and the second puller 23 falls within a normal range.
[0082] Therefore, the tension in the core member 1 between the first puller 15 and the second puller 23 falls within a normal range, and the core member 1 does not form slack or the core member 1 does not overstretch. Therefore, even if the extrusion molded products 10 and 10' in which the covering parts such as the body sealing lip part, the glass sealing lip part and the hollow sealing part are formed on the core members 1 and 1' by the second extruder 19, the third extruder 20, the fourth extruder 21 and the like are manufactured in the second die 18, the extrusion molded products 10 and 10' each having good quality and constant molding accuracy can be stably manufactured.
[0083] In a method for manufacturing an extrusion molded product according to an embodiment of the present invention, a sensor unit 16 includes: core component feeding rollers 16a and 16b, which are arranged between a first puller 15 and a second puller 23, and a gap is formed between the core component feeding rollers along the direction in which the core component 1 moves; and a vertically movable tension applying roller 16c, which is arranged between the core component feeding rollers 16a and 16b so as to be able to move up and down and apply tension to each core component 1 and 1', and the sensor unit 16 monitors the tension in each core component 1 and 1' according to the height of the vertically movable tension applying roller 16c.
[0084] Therefore, this simple configuration enables the sensor unit 16 to apply tension to the core members 1 and 1 ′, thereby stably manufacturing the extrusion molded products 10 and 10 ′ with good quality and constant molding accuracy without increasing the manufacturing cost.
[0085] In a method for manufacturing an extrusion molded product according to an embodiment of the present invention, a cutting mechanism unit 14 for cutting core components 1 and 1' to form grooves 1a and 1a' using a cutting blade 14a5 is arranged between a first mold 12 and a first puller 15, and a sensor unit 16 applies tension to the core components 1 and 1' in which grooves 1a and 1a' have been formed by the cutting mechanism unit 14 along a direction in which the core components 1 and 1' are easy to bend.
[0086] Therefore, when the core members 1 and 1' are easy to bend due to the grooves 1a and 1a' formed therein, the tension speed can be adjusted by applying tension to the core members 1 and 1' in the direction in which the core members 1 and 1' are easy to bend, so that the tension of each core member 1 and 1' falls within the normal range. In this way, the tension of each core member 1 and 1' can be adjusted to fall within a larger normal range, so that the extrusion molded products 10 and 10' with better quality and more constant molding accuracy can be stably produced.
[0087] In the method of manufacturing an extrusion molded product according to an embodiment of the present invention, the sensor unit 16 includes: an upper contact sensor 16e, which is disposed above the vertically movable tension applying roller 16c and detects the distance between the vertically movable tension applying roller 16c and the upper contact sensor; and a lower contact sensor 16f, which is disposed below the vertically movable tension applying roller 16c and detects the distance between the vertically movable tension applying roller 16c and the lower contact sensor, and the sensor unit 16 monitors the tension in the core member 1 according to the detection outputs of the upper contact sensor 16e and the lower contact sensor 16f. The drawing speed control unit 16g issues an instruction to at least one of the first puller 15 and the second puller 23 to eliminate the speed difference between the first puller 15 and the second puller 23 according to the sensor outputs of the upper contact sensor 16e and the lower contact sensor 16f.
[0088] Therefore, the tension applied to each core member 1 and 1' reaching the upper limit position β or the lower limit position γ can be detected by a simple configuration between the first puller 15 and the second puller 23, so that the extrusion molded products 10 and 10' with good quality and constant molding accuracy can be stably manufactured without increasing the manufacturing cost.
[0089] In the method for manufacturing an extrusion molded product according to an embodiment of the present invention, without stopping, the second puller 23 performs a drawing operation at a drawing speed having an upper limit speed and a lower limit speed according to the tension of each of the core members 1 and 1' monitored by the sensor unit 16, and the upper limit speed and the lower limit speed are respectively within the range of ±12.5% of the drawing speed of the first puller 15, or without stopping, the first puller 15 performs a drawing operation at a drawing speed with an upper limit speed of 12.5% or less of the drawing speed of the second puller 23 and a lower limit speed within the range of ±12.5% of the drawing speed of the second puller 23.
[0090] Therefore, even if there is a speed difference (variation) between the first puller 15 and the second puller 23, the acceptable variation range is within the range of (±0.5 / 4)×100=±12.5%, and the tolerance of the M4 grade rubber product relative to the reference size (i.e., 4) is ±0.5, that is, the minimum value of the tolerance is 3.5 and the maximum value is 4.5. Therefore, from this point of view, the extrusion molded products 10 and 10' also have good quality and stable molding accuracy.
[0091] Specifically, the molding accuracy of each of the extrusion molded products 10 and 10' is related to the molding speed, and the increase or decrease of the cross section of the molded product is proportional to the molding speed. When the tolerance (±0.5) of the M4 level is set as the maximum variation, although it is necessary to control the speed difference between the two pullers 15 and 23 to 12.5% or less so that the pulling speed of the first puller 15 is synchronized with the pulling speed of the second puller 23, the extrusion molded products 10 and 10', both of which have good quality and constant molding accuracy, can be stably manufactured.
[0092] It is to be noted that, in the description of the above-mentioned embodiment, although the sensor unit 16 detects that the vertically movable tension applying roller 16c applying tension to the core member 1 reaches the upper limit position β when the upper end portion of the vertically movable body 16d contacts the upper contact sensor 16e, and the sensor unit 16 detects that the vertically movable tension applying roller 16c reaches the lower limit position γ when the lower end portion of the vertically movable body 16d contacts the lower contact sensor 16f, as shown in FIG. Figure 2 , Figure 6 and Figure 7 As shown, the present invention is not limited thereto. Fig.11 As shown, the upper end portion and the lower end portion of the vertically movable body 16d can be detected by the upper optical (non-contact) sensor 16g and the lower optical (non-contact) sensor 16h, respectively. Fig.12As shown, for example, a blade 16i1 of a potentiometer 16i which is a variable resistance sensor may be attached to the vertically movable body 16d, and the potentiometer 16i may detect that the vertically movable tension applying roller 16c reaches the upper limit position β and the lower limit position γ.
[0093] Furthermore, in the description of the above embodiment, although the groove 1a is formed in the core member 1 by the cutting mechanism unit 14, and the groove 1a' is formed in the core member 1' by the cutting mechanism unit 14, the present invention is not limited thereto. The present invention is also applicable to molding an extrusion molded product without forming any groove on the core member. For example, Figure 3B The core member 1' shown in a cross section that is roughly I-shaped (flat plate-like shape) has flexibility in one direction (the thickness direction of the core member). Therefore, there is a case where the groove 1a' is not required. In this case, the application mode of the present invention is to use the core member 1' without forming the groove 1a'. In the case where no groove is formed in the core member, the cutting mechanism unit 14 can be omitted. Alternatively, the cutting mechanism unit 14 can also be set as described above, allowing the core member to pass through the cutting mechanism unit 14 without causing the rotating body 14a4 to rotate, so that the core member pops out of the retainer 14a, and the cutting blade 14a5 does not form any groove in the core member.
Claims
1. A method for producing an extrusion molded product, the method comprising: A drawing step of drawing a core member made of resin and molded into a desired shape in a first mold by a first puller; as well as a molding step of molding an extrusion molded product in a second mold by providing a cover portion made of a thermoplastic elastomer on the outer periphery of the core member that has been pulled by the first puller, and pulling the extrusion molded product by the second puller, A sensor unit for monitoring the tension in the core member is provided between the first puller and the second puller, and at least one of the first puller and the second puller adjusts a pulling speed based on the tension in the core member monitored by the sensor unit, so that the tension in the core member between the first puller and the second puller falls within a normal range.
2. The method for producing an extrusion molded product according to claim 1, The sensor unit includes a core component feeding roller and a vertically movable tension applying roller, wherein the core component feeding roller is arranged between the first puller and the second puller, and a gap is formed between the core component feeding rollers along the direction of movement of the core component. The vertically movable tension applying roller is arranged between the core component feeding rollers in a manner that can move up and down and applies tension to the core component. The sensor unit monitors the tension in the core component based on the height of the vertically movable tension applying roller.
3. The method for producing an extrusion molded product according to claim 2, wherein a cutting mechanism unit is provided between the first die and the first puller, the cutting mechanism unit cutting the core member by a cutting blade in a manner of forming a groove, and The sensor unit applies tension to the core member in which the groove has been formed by the cutting mechanism unit in a direction in which the core member is easily bent.
4. A method for producing an extrusion molded product according to any one of claims 1 to 3, wherein the second puller pulls the extruded molded product at a pulling speed having an upper limit speed and a lower limit speed based on the tension in the core member monitored by the sensor unit, and each of the upper limit speed and the lower limit speed is within a range of ±12.5% of the pulling speed of the first puller without stopping.
5. A method for producing an extrusion molded product according to any one of claims 1 to 3, The first puller pulls the core member at a pulling speed having an upper limit speed and a lower limit speed based on the tension in the core member monitored by the sensor unit, and each of the upper limit speed and the lower limit speed is within ±12.5% of the pulling speed of the second puller without stopping.
Citation Information
Patent Citations
Film tension control method in film production
CN101195454A
Method for producing an extrusion molded product for automobiles
CN108215236A
Novel high-speed intermittent traction tension control method
CN111908231A
Fastener tape supply unit of fastener stringer continuous manufacturing apparatus
CN1827007A
Banc et procede d'etirage de tubes avec mandrin de calibrage interieur
FR2471228A1