Method for purifying wet-process phosphoric acid by double salt crystallization method

Through the two-stage crystallization process of the double salt crystallization method, the temperature and fluid state are controlled, which solves the problems of phosphoric acid purity and particle size distribution in the single-stage crystallization method, achieves higher purity and narrow particle size distribution, reduces energy consumption, and is suitable for Temperature-sensitive response of fluid viscosity.

CN118723950AActive Publication Date: 2024-10-01QIANNAN NORMAL UNIV FOR NATTIES
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411128196.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-16
Publication Date
2024-10-01
Estimated Expiration
2044-08-16

AI Technical Summary

Technical Problem

When purifying wet phosphoric acid with existing technology, single-stage crystallization can only remove 80% to 90% of impurities, resulting in low purity of phosphoric acid, excessive crystal size distribution and easy agglomeration, making it difficult to control the fluid dynamic state and high energy consumption.

Method used

The double salt crystallization method is adopted, and through a two-stage crystallization process, the first and second stages control the reaction temperature at 25-30°C and 15-20°C respectively. The vacuum forced external circulation crystallizer and the internal and external circulation crystallizer are used to control non-condensation. The gas is extracted to form a fluidized state and adjust the crystal growth, thereby improving the narrowness and purity of the particle size distribution.

Benefits of technology

It achieves higher phosphoric acid purity and narrow particle size distribution, reduces energy consumption, is suitable for the temperature-sensitive reaction of fluid viscosity, and improves production efficiency and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118723950A_ABST
    Figure CN118723950A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of phosphorus, in particular to a method for purifying wet-process phosphoric acid through a double salt crystallization method. The advantage that the average temperature difference of two-stage crystallization is lower than that of single-stage crystallization is utilized, the first-stage reaction temperature is controlled to be 25-30 DEG C, the second-stage reaction temperature is controlled to be 15-20 DEG C, the problem that due to the fact that the single-stage temperature difference is too large, crystal particle size distribution is too large, and caking is prone to occurring is solved, and due to the fact that the hydrodynamic state is easy to control, energy consumption is low, and cost is low. The two-stage crystallization device is particularly suitable for reactants with fluid viscosity sensitive to temperature, and two-stage crystallization is completed by a vacuum forced external circulation crystallizer and a vacuum forced internal and external circulation crystallizer respectively. The analytically pure phosphoric acid is prepared by oxygenolysis of urea phosphate through concentrated nitric acid, the reaction formula is # imgabs0 #, and the method can be divided into two steps of oxygenolysis and concentration which are respectively completed by a circulating fluidized bed reactor and a fluidized bed concentrator.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of phosphorus chemical industry, and in particular to a method for purifying wet-process phosphoric acid by a double salt crystallization method. Background Art

[0002] Phosphoric acid, also known as orthophosphoric acid, is a common inorganic acid. Phosphoric acid is mainly used in pharmaceutical, food, fertilizer and other industries. Phosphoric acid obtained by decomposing phosphate rock with sulfuric acid, nitric acid or hydrochloric acid is collectively referred to as wet-process phosphoric acid, and the method of decomposing phosphate rock with sulfuric acid is the most basic method in the production of wet-process phosphoric acid. Industrially produced wet-process phosphoric acid needs to be further purified. The Chinese invention patent (patent number CN202410454336.9, patent name A method for improving the yield of urea phosphate prepared from wet-process phosphoric acid) discloses a method for improving the yield of urea phosphate prepared from wet-process phosphoric acid, which mixes a crystal promoter with wet-process phosphoric acid and urea for reaction, cools and crystallizes after the reaction, filters, and dries to obtain urea phosphate; or wet-process phosphoric acid is mixed with urea for reaction, and a crystal promoter or a urea phosphate mother liquor containing a crystal promoter is added after the reaction, and urea phosphate is obtained by cooling, crystallizing, filtering, and drying. The crystal promoter is one or a mixture of any proportion of ethylene glycol methyl ether, ethylenediaminetetraacetic acid, and citric acid. The urea phosphate produced by the method of the present invention is a crystalline particle, which meets the industrial urea phosphate standard (GB / T27805-2011), can meet market demand, has a low cost of a crystal promoter, is flexible in adding method, and is very convenient for actual production. The Chinese invention patent (patent number CN202311491148.5, patent name is a process system and process for continuously producing urea phosphate by concentrated acid method of wet phosphoric acid) discloses a process system and process for continuously producing urea phosphate by concentrated acid method of wet phosphoric acid, including a reaction system, a crystallization system, a centrifugal filtration system, a finished product cooling and packaging system and an auxiliary pipeline conveying device connected in sequence; the reaction system includes a reactor, the feed inlet of the reactor is connected to a pre-treated phosphoric acid storage tank and a urea storage tank, and the discharge port of the reactor is connected to a reaction liquid storage tank; the feed inlet of the crystallization system is connected to the reaction liquid storage tank, the crystallization system includes several stages of crystallizers with conical bottoms, and the crystallizer is provided with a cooling jacket; the centrifugal filtration system includes a centrifugal filter, the feed inlet of the centrifugal filter is connected to the discharge port of the crystallization system, the liquid discharge port of the centrifugal filter is connected to the mother liquid storage tank, and the solid discharge port of the centrifugal filter is connected to the finished product cooling and packaging system. The present invention realizes the continuous and stable production of urea phosphate and reduces the labor intensity of employees.

[0003] Urea phosphate is also called urea phosphate It is a colorless, transparent prismatic crystal with a parallel layer structure. The layers are connected by hydrogen bonds and belong to the orthorhombic system. The relative density is 1.74, the melting point is 117.3℃, it is easily soluble in water and ethanol, and the solubility at 46℃ is 202g / L. It is insoluble in ether, toluene, carbon tetrachloride, etc. The aqueous solution is acidic, and the pH value of 1% aqueous solution is 1.89. Urea phosphate is the product of the reaction of phosphoric acid and urea under certain conditions. Its reaction formula is: .

[0004] The existing technology for preparing wet-process phosphoric acid by purifying urea phosphate adopts a single-stage crystallization process, which has the advantage of a high yield of phosphoric acid, but can only remove 80% to 90% of impurities in phosphoric acid, and the purity of the phosphoric acid is not high. Summary of the invention

[0005] In view of the deficiencies in the prior art, the purpose of the present invention is to provide a method for purifying wet-process phosphoric acid by a double salt crystallization method, comprising the following steps: Step 1, utilizing the advantage of a low average temperature difference at each stage of two-stage crystallization compared to a single-stage crystallization, the first stage controls the reaction temperature to be 25-30°C, and the second stage controls the reaction temperature to be 15-20°C, so as to solve the problem that the single-stage temperature difference is too large, resulting in a large crystal size distribution and easy agglomeration. Since the fluid dynamic state is easy to control and the energy consumption is low, it is particularly suitable for reactions where the fluid viscosity is sensitive to temperature; the two-stage crystallization is completed by a first-stage vacuum forced external circulation crystallizer and a second vacuum forced internal and external circulation crystallizer, respectively. The first-stage vacuum forced external circulation crystallizer comprises a feed pipe, a downcomer, a crystallization reactor, and a feed pipe. reaction chamber, non-condensable gas outlet, circulation pipe, water cooler, slurry outlet, screw pump; 40% extracted wet phosphoric acid and urea solution are mixed and sent into the crystallization reaction chamber through the feed pipe at a molar ratio of 1:1, urea phosphate crystals precipitated from the reaction of phosphoric acid and urea solution form slurry, part of the slurry is pushed by the downcomer at the bottom of the crystallization reaction chamber through the screw pump, the heat generated by the reaction is removed by the water cooler, and then returned to the crystallization reaction chamber through the tangential direction of the circulation pipe, the non-condensable gas generated in the reaction process is promptly extracted by the vacuum pump from the non-condensable gas outlet, the vacuum reaction condition of the crystallization reaction chamber is maintained, and the non-condensable gas is prevented from being trapped during the crystal growth, thereby affecting the lattice arrangement and the state of crystal habit, and the slurry is drawn out from the slurry outlet and sent to the buffer tank for temporary storage.

[0006] Step 2, the second-stage vacuum forced internal and external circulation crystallizer includes an external circulation pump, an external circulation liquid inlet, an external circulation downcomer, an external circulation cooler, an external circulation reflux pipe, a fluidized crystallization reaction chamber, an internal guide tube, a vacuum port, an internal circulation reflux pipe, an internal circulation cooler, an internal circulation liquid inlet, an internal circulation pump, an internal circulation downcomer, and an elutriation leg. Since the internal guide tube is provided, an internal circulation channel is formed, which greatly improves the internal circulation rate, and the weight density of the slurry can be maintained at a level of 30% to 40%, and the high saturation area can be significantly eliminated. The supersaturation at various locations in the fluidized crystallization reaction chamber is relatively uniform, and the supercooling is less than 1°C, thereby enhancing the production capacity of the vacuum forced internal and external circulation crystallizer. In addition to the internal circulation channel, an external circulation channel is also provided to eliminate excessive fine crystals and elutriate the product particle size, ensuring that a particle size distribution range can be produced. Narrow crystal products, urea phosphate crystal slurry is extracted from the buffer tank and pumped into the inner circulation channel and the outer circulation channel in two ways. The outer circulation channel of the slurry flows down through the outer circulation downcomer at the conical bottom of the fluidized crystallization reaction chamber, is transported by the outer circulation pump, and is taken away from the reaction heat by the outer circulation cooler, and is returned to the fluidized crystallization reaction chamber through the tangent of the outer circulation reflux pipe. The inner circulation channel of the slurry flows down through the inner circulation downcomer at the conical bottom of the fluidized crystallization reaction chamber, is transported by the inner circulation pump, and is taken away from the reaction heat by the inner circulation cooler, and is injected into the inner guide tube through the inner circulation reflux pipe. The slurry fluid in the fluidized crystallization reaction chamber becomes a fluidized state through internal and external circulation. The flow rate of the internal and external circulation channels can be adjusted to control crystal growth, thereby obtaining the required crystal particle size distribution. The non-condensable gas generated during the reaction process is timely extracted by the vacuum pump from the vacuum port, and the slurry is drawn out from the elutriation leg and separated by centrifugal filtration and sent to the mother liquid tank for temporary storage.

[0007] Step 3, preparing analytically pure phosphoric acid by oxidative decomposition of urea phosphate with concentrated nitric acid, the reaction formula is: , which can be divided into two steps, namely, oxidation decomposition and concentration, which are respectively completed by a circulating fluidized bed reactor and a fluidized bed concentrator; the circulating fluidized bed reactor comprises an acid inlet, a mother liquor inlet, a circulating fluidized bed reaction chamber, a cyclone separator, a return liquid pipe, a gas distribution ring pipe, and an intermediate product port. The mixed liquid of urea phosphate and circulating acid is transported by a centrifugal pump and injected into the circulating fluidized bed reaction chamber from the mother liquor inlet, and concentrated nitric acid is injected from the acid inlet. High-purity nitrogen is evenly blown into the circulating fluidized bed reaction chamber from the gas distribution ring pipe to form a bubbling boiling state, thereby improving the mass transfer efficiency of the reactants and taking away the non-condensable gas. At the same time, the reaction temperature is controlled at 55-60°C. The gas flow carrying the acid liquid passes through a cyclone separator to achieve gas-liquid separation. The non-condensable gas is recycled after being washed and absorbed by pure water. The acid liquid absorbed by the pure water washing becomes The source of circulating acid, the acid liquid flows back to the circulating fluidized bed reaction chamber through the return pipe, and the phosphoric acid liquid is pumped to the fluidized bed concentrator through the intermediate product port; the fluidized bed concentrator includes a liquid receiving tank, a finished product port, a steam distribution plate, an infusion port, a fluidized bed concentration chamber, and a separator. Steam is evenly distributed from the steam distribution plate to the fluidized bed concentration chamber, and the liquid flow in the chamber is bubbled and boiled into a fluidized state. The reaction temperature is controlled to be 120°C, and the steam evaporates nitric acid and water away. After gas-liquid separation in the separator, the non-condensable gas is condensed and absorbed and then recycled. The separated acid liquid flow is collected by the liquid receiving tank and becomes the source of circulating acid. The circulating acid is added to the mother liquid tank for recycling. In order to ensure the fluidity of the liquid flow, the mass ratio of the circulating amount of the circulating acid to the reactant is 1:1, and the purified phosphoric acid is drawn out from the finished product port.

[0008] Compared with the prior art, the present invention has at least the following advantages: First, the two-stage crystallization has the advantages of low average temperature difference between each stage, narrow product particle size distribution, easy control of fluid dynamic state, and low energy consumption compared with single-stage crystallization, and is particularly suitable for reactants whose fluid viscosity is sensitive to temperature; Second, the non-condensable gas is extracted in time to maintain vacuum reaction conditions, so as to prevent the non-condensable gas from being trapped during crystal growth and thus affecting the lattice arrangement and crystal habit state, thereby improving the product purity. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 It is a schematic diagram of the main structure of a method for purifying wet-process phosphoric acid by a double salt crystallization method according to the present invention; Figure 2 A schematic diagram of the structure of a large sample of a method for purifying wet-process phosphoric acid by a double salt crystallization method of the present invention; Figure 3 It is a schematic diagram of the structure of sample B of a method for purifying wet-process phosphoric acid by a double salt crystallization method of the present invention; Figure 4 It is a schematic diagram of the structure of sample C of a method for purifying wet-process phosphoric acid by a double salt crystallization method of the present invention; Figure 5 It is a schematic diagram of the structure of a large sample D of a method for purifying wet-process phosphoric acid by a double salt crystallization method of the present invention; 1-vacuum forced external circulation crystallizer, 2-buffer tank, 3-vacuum forced internal and external circulation crystallizer, 4-vacuum tank, 5-vacuum pump, 6-mother liquor tank, 7-centrifugal pump, 8-circulating fluidized bed reactor, 9-fluidized bed concentrator, 10-feed pipe, 11-down pipe, 12-crystallization reaction chamber, 13-non-condensable gas outlet, 14-circulation pipe, 15-water cooler, 16-crystal slurry outlet, 17-screw pump, 18-external circulation pump, 19-external circulation liquid inlet, 20-external circulation downcomer, 21-external circulation cooler, 22-external circulation reflux pipe, 2 3 - fluidized crystallization reaction chamber, 24 - internal guide tube, 25 - vacuum port, 26 - internal circulation reflux pipe, 27 - internal circulation cooler, 28 - internal circulation liquid inlet, 29 - internal circulation pump, 30 - internal circulation downcomer, 31 - elutriation leg, 32 - acid inlet, 33 - mother liquor inlet, 34 - circulating fluidized bed reaction chamber, 35 - cyclone separator, 36 - return liquid pipe, 37 - gas distribution ring pipe, 38 - intermediate product port, 39 - liquid receiving tank, 40 - finished product port, 41 - steam gas distribution plate, 42 - liquid inlet, 43 - fluidized bed concentration chamber, 44 - separator. DETAILED DESCRIPTION

[0010] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments.

[0011] like Figure 1 , Figure 2 , Figure 3 , Figure 4 , Figure 5As shown, a method for purifying wet-process phosphoric acid by a double salt crystallization method comprises the following steps: Step 1, utilizing the advantage of a lower average temperature difference between each stage of two-stage crystallization than that of a single-stage crystallization, the reaction temperature of the first stage is controlled to be 25-30°C, and the reaction temperature of the second stage is controlled to be 15-20°C, so as to solve the problem that the single-stage temperature difference is too large, resulting in a large crystal size distribution and easy agglomeration. Since the fluid dynamic state is easy to control and the energy consumption is low, it is particularly suitable for reactants whose fluid viscosity is sensitive to temperature. The two-stage crystallization is respectively completed by a vacuum forced external circulation crystallizer 1 and a vacuum forced internal and external circulation crystallizer 3. The first-stage vacuum forced external circulation crystallizer 3 comprises a feed pipe 10, a downcomer 11, a crystallization reaction chamber 12, a non-condensable gas outlet 13, a circulation pipe 14, a water cooler 15, The slurry outlet 16 and the screw pump 17 mix 40% extracted wet-process phosphoric acid and urea solution and send them into the crystallization reaction chamber 12 through the feed pipe 10 at a molar ratio of 1:1. The urea phosphate crystals precipitated by the reaction of phosphoric acid and urea solution form slurry. Part of the slurry is pushed by the downcomer 11 at the bottom of the crystallization reaction chamber 12 through the screw pump 17, and the heat generated by the reaction is removed by the water cooler 15. Then, it returns to the crystallization reaction chamber 12 in the tangential direction of the circulation pipe 14. The non-condensable gas generated during the reaction process is promptly extracted by the vacuum pump 5 through the non-condensable gas outlet 13 to maintain the vacuum reaction condition of the crystallization reaction chamber 12 to prevent the non-condensable gas from being trapped during the crystal growth, thereby affecting the lattice arrangement and the state of crystal habit. The slurry is drawn out from the slurry outlet 16 and sent to the buffer tank 2 for temporary storage.

[0012] Step 2, the second-stage vacuum forced internal and external circulation crystallizer 3 includes an external circulation pump 18, an external circulation liquid inlet 19, an external circulation downcomer 20, an external circulation cooler 21, an external circulation reflux pipe 22, a fluidized crystallization reaction chamber 23, an internal guide tube 24, a vacuum port 25, an internal circulation reflux pipe 26, an internal circulation cooler 27, an internal circulation liquid inlet 28, an internal circulation pump 29, an internal circulation downcomer 30, and an elutriation leg 31. Since the internal guide tube 24 is provided, an internal circulation channel is formed, and the internal circulation rate is very high, which can keep the weight density of the slurry at a level of 30% to 40%, and can significantly eliminate the high saturation area. The supersaturation at various locations in the fluidized crystallization reaction chamber 23 is relatively uniform, and the supercooling degree is less than 1°C, thereby enhancing the production capacity of the vacuum forced internal and external circulation crystallizer 3. In addition to the internal circulation channel, an external circulation channel is also provided to eliminate excessive fine crystals and elutriate the product particle size, ensuring that a narrow particle size distribution range can be produced. The crystal product, urea phosphate crystal slurry is extracted from the buffer tank 2 and pumped to the inner circulation channel and the outer circulation channel in two ways. The outer circulation channel of the crystal slurry is the outer circulation downcomer 20 through the conical bottom of the fluidized crystallization reaction chamber 23, and is transported by the outer circulation pump 18, and the reaction heat is taken away by the outer circulation cooler 21, and the reaction heat is returned to the fluidized crystallization reaction chamber 23 by the tangent of the outer circulation reflux pipe 22. The inner circulation channel of the crystal slurry is the inner circulation downcomer 30 through the conical bottom of the fluidized crystallization reaction chamber 23, and is transported by the inner circulation pump 29, and the reaction heat is taken away by the inner circulation cooler 27, and is injected into the inner guide tube 24 through the inner circulation reflux pipe 26. The crystal slurry fluid in the fluidized crystallization reaction chamber 23 becomes a fluidized state through the inner and outer circulations, and the flow rate of the inner and outer circulation channels can be adjusted to control the crystal growth, so as to obtain the desired crystal particle size distribution. The non-condensable gas generated in the reaction process is timely extracted by the vacuum pump 5 through the vacuum port 25, and the crystal slurry is drawn out from the elutriation leg 31 and separated by centrifugal filtration and sent to the mother liquid tank 6 for temporary storage.

[0013] Step 3: Prepare analytically pure phosphoric acid by oxidative decomposition of urea phosphate with concentrated nitric acid. The reaction formula is: , which can be divided into two steps, namely, oxidation decomposition and concentration, which are respectively completed by a circulating fluidized bed reactor 8 and a fluidized bed concentrator 9: the circulating fluidized bed reactor 8 comprises an acid inlet 32, a mother liquor inlet 33, a circulating fluidized bed reaction chamber 34, a cyclone separator 35, a liquid return pipe 36, a gas distribution ring pipe 37, and an intermediate product port 38. The mixed liquid of urea phosphate and circulating acid is transported by a centrifugal pump 7 and injected into the circulating fluidized bed reaction chamber 34 from the mother liquor inlet 33. Concentrated nitric acid is injected from the acid inlet 32. High-purity nitrogen is evenly blown into the circulating fluidized bed reaction chamber 34 from the gas distribution ring pipe 37 to form a bubbling boiling state, thereby improving the mass transfer efficiency of the reactants and taking away the non-condensable gas. At the same time, the reaction temperature is controlled at 55-60°C. The gas flow carrying the acid solution passes through the cyclone separator 35 to achieve gas-liquid separation. The non-condensable gas is recycled after being washed and absorbed by pure water. The acid solution absorbed by the pure water washing becomes As the source of circulating acid, the acid liquid flows back to the circulating fluidized bed reaction chamber 34 through the return pipe 36, and the phosphoric acid liquid is pumped to the fluidized bed concentrator 9 through the intermediate product port 38; the fluidized bed concentrator 9 includes a liquid receiving tank 39, a finished product port 40, a steam distribution plate 41, an infusion port 42, a fluidized bed concentration chamber 43, and a separator 44. Steam is evenly distributed from the steam distribution plate 41 to the fluidized bed concentration chamber 43, and the liquid flow in the chamber is bubbled and boiled into a fluidized state. The reaction temperature is controlled to be 120°C, and the steam evaporates nitric acid and water away. After gas-liquid separation in the separator 44, the non-condensable gas is condensed and absorbed and then recycled. The separated acid liquid flow is collected by the liquid receiving tank 39 as the source of circulating acid, and the circulating acid is added to the mother liquid tank 6 for recycling. To ensure the fluidity of the liquid flow, the mass ratio of the circulating amount of the circulating acid to the reactant is 1:1. The purified phosphoric acid is drawn out from the finished product port 40.

Claims

1. A method for purifying wet-process phosphoric acid by a double salt crystallization method, characterized in that: The steps include: Step 1, the first-stage vacuum forced external circulation crystallizer (1) comprises a feed pipe (10), a downcomer (11), a crystallization reaction chamber (12), a non-condensable gas outlet (13), a circulation pipe (14), a water cooler (15), a slurry outlet (16), and a screw pump (17); 40% extracted wet-process phosphoric acid and urea solution are mixed in a molar ratio of 1:1 and fed into a crystallization reaction chamber (12) through a feed pipe (10). Phosphoric acid and urea solution react to form urea phosphate crystals to form slurry. Part of the slurry is pushed through a downcomer (11) at the bottom of the crystallization reaction chamber (12) via a screw pump (17). Heat generated by the reaction is removed by a water cooler (15). The slurry then returns to the crystallization reaction chamber (12) in a tangential direction through a circulation pipe (14). The slurry is drawn out from a slurry outlet (16) and fed into a buffer tank (2) for temporary storage. Step 2, the second stage vacuum forced internal and external circulation crystallizer (3) comprises an external circulation pump (18), an external circulation liquid inlet (19), an external circulation downcomer (20), an external circulation cooler (21), an external circulation reflux pipe (22), a fluidized crystallization reaction chamber (23), an internal guide tube (24), a vacuum port (25), an internal circulation reflux pipe (26), an internal circulation cooler (27), an internal circulation liquid inlet (28), an internal circulation pump (29), an internal circulation downcomer (30), and an elutriation leg (31); The urea phosphate slurry is extracted from the buffer tank (2) and pumped into an inner circulation channel and an outer circulation channel in two ways, wherein the outer circulation channel of the slurry flows down through the outer circulation downcomer (20) at the conical bottom of the fluidized crystallization reaction chamber (23), is transported by the outer circulation pump (18), is transported through the outer circulation cooler (21) to remove the reaction heat, and returns to the fluidized crystallization reaction chamber (23) tangentially through the outer circulation reflux pipe (22); The inner circulation channel of the slurry flows down through the inner circulation downcomer (30) at the conical bottom of the fluidized crystallization reaction chamber (23), is transported by the inner circulation pump (29), and is transported through the inner circulation cooler (27) to remove the reaction heat, and is injected into the inner guide tube (24) through the inner circulation reflux pipe (26). The non-condensable gas generated during the reaction is promptly extracted by the vacuum pump (5) through the vacuum port (25). The slurry is drawn out from the elutriation leg (31), separated by centrifugal filtration, and sent to the mother liquid tank (6) for temporary storage. Step 3, the circulating fluidized bed reactor (8) includes an acid inlet (32), a mother liquor inlet (33), a circulating fluidized bed reaction chamber (34), a cyclone separator (35), a liquid return pipe (36), a gas distribution ring pipe (37), and an intermediate product port (38); The mixed liquid of urea phosphate and circulating acid is transported by a centrifugal pump (7) and injected into the circulating fluidized bed reaction chamber (34) through the mother liquid inlet (33). Concentrated nitric acid is injected through the acid inlet (32). High-purity nitrogen is evenly blown into the circulating fluidized bed reaction chamber (34) from the gas distribution ring pipe (37) to form a bubbling boiling state, thereby improving the mass transfer efficiency of the reactants and taking away the non-condensable gas. At the same time, the reaction temperature is controlled at 55 to 60° C. The acid liquid flows back to the circulating fluidized bed reaction chamber (34) through the return liquid pipe (36), and the phosphoric acid liquid is pumped to the fluidized bed concentrator through the intermediate product port (38); The fluidized bed concentrator comprises a liquid receiving tank (39), a finished product port (40), a steam distribution plate (41), a liquid infusion port (42), a fluidized bed concentration chamber (43), and a separator (44). Steam is uniformly distributed from the steam distribution plate (41) to the fluidized bed concentration chamber (43), and the liquid flow in the chamber is bubbled and boiled into a fluidized state. The reaction temperature is controlled to be 120° C. The purified phosphoric acid is drawn out from the finished product port.

2. The method for purifying wet-process phosphoric acid by a double salt crystallization method according to claim 1, characterized in that: The first stage reaction temperature is controlled at 25-30°C, the second stage reaction temperature is controlled at 15-20°C, and the two stages of crystallization are completed by a vacuum forced external circulation crystallizer and a vacuum forced internal and external circulation crystallizer respectively.

3. The method for purifying wet-process phosphoric acid by a double salt crystallization method according to claim 1, characterized in that the reaction The non-condensable gas generated during the process is promptly extracted by the vacuum pump from the non-condensable gas outlet, so as to maintain the vacuum reaction conditions of the crystallization reaction chamber (12) and prevent the non-condensable gas from being trapped during the crystal growth period, thereby affecting the lattice arrangement and the state of the crystal habit.

4. The method for purifying wet-process phosphoric acid by a double salt crystallization method according to claim 1, characterized in that: The inner guide tube (24) forms an inner circulation channel, and its inner circulation rate keeps the weight density of the slurry at a level of 30% to 40%, and significantly eliminates the high saturation area. The supersaturation at various locations in the fluidized crystallization reaction chamber (23) is relatively uniform, and the supercooling is less than 1°C.

5. The method for purifying wet-process phosphoric acid by a double salt crystallization method according to claim 1, characterized in that: The outer circulation channel is used to eliminate excess fine crystals and to adjust the particle size of the product.

6. The method for purifying wet-process phosphoric acid by a double salt crystallization method according to claim 1, characterized in that: The slurry fluid in the fluidized crystallization reaction chamber (23) becomes fluidized through internal and external circulation, and the flow rate of the internal and external circulation channels can be adjusted to control crystal growth, thereby obtaining the desired crystal particle size distribution.

7. The method for purifying wet-process phosphoric acid by double salt crystallization according to any one of claims 1 to 6, characterized in that: Analytical pure phosphoric acid is prepared by oxidative decomposition of urea phosphate with concentrated nitric acid. The reaction formula is: , which can be divided into two steps: oxidation decomposition and concentration. The oxidation decomposition step is completed by a circulating fluidized bed reactor, and the concentration step is completed by a fluidized bed concentrator.

8. The method for purifying wet-process phosphoric acid by a double salt crystallization method according to claim 1, characterized in that: The gas flow carrying the acid liquid passes through the cyclone separator (25) to achieve gas-liquid separation, and the non-condensable gas is washed and absorbed by pure water and then recycled. The acid liquid absorbed by the pure water washing becomes the source of circulating acid.

9. The method for purifying wet-process phosphoric acid by a double salt crystallization method according to claim 1, characterized in that: The steam evaporates the nitric acid and water and separates the gas and liquid in the separator. The non-condensable gas is condensed and absorbed before recycling. The separated acid liquid is collected in the receiving tank and becomes the source of circulating acid. The circulating acid is added to the mother liquid tank for recycling. To ensure the fluidity of the liquid flow, the mass ratio of the circulating acid to the reactant is 1:1.

Citation Information

Patent Citations

  • Method for preparing large-granule industrial-grade urea phosphate product through continuous reaction crystallization of wet-process phosphoric acid

    CN110451513A

  • Process for prodn. of phosphoric acid by crystallisation of phosphoric acid hemihydrate

    CN1344226A

  • Process for production of phosphoric acid by crystallization of phosphoric acid hemihydrate

    US6814949B1