A kind of 2 SO 4 Comprehensive wastewater treatment process
By combining calcium ion denitration and metathesis reaction with multi-component phase diagrams and evaporation crystallization processes, the problem of incomplete separation of NaCl and Na2SO4 was solved, which improved the added value of the product, reduced energy consumption, and achieved efficient utilization of resources.
Patent Information
- Application Number
- CN202411215685.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-02
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-09-02
AI Technical Summary
In existing technologies, wastewater treatment processes in the coal chemical industry suffer from problems such as incomplete separation of NaCl and Na2SO4, high energy consumption, and low product added value, resulting in high costs and low resource utilization.
By introducing a calcium ion denitrification reaction, sulfate ions are converted into calcium sulfate precipitate, forming a brine system mainly composed of sodium chloride. Then, ammonia and carbon dioxide are used for metathesis to convert sodium ions into sodium bicarbonate. Combining a multi-component phase diagram and evaporation crystallization process, products such as NaCl and CaCl2·2H2O are separated.
This method achieves efficient separation of NaCl and Na2SO4, improves the economic value of the product, reduces energy consumption and costs, and makes full use of resources.
Smart Images

Figure CN118724044B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the technical field of wastewater treatment, and specifically to a comprehensive treatment process for wastewater containing NaCl and Na2SO4. Background Art
[0002] In the production process of coal chemical industry, thermal power plant and other industries, a large amount of wastewater is generated, which is mainly composed of sodium sulfate and sodium chloride, and contains impurities such as fluorine, calcium and magnesium. At present, the zero-emission technology of the coal chemical industry is quite mature, but due to cost issues, the sewage treatment problem is still an important factor restricting the development of the industry in the production of coal chemical enterprises. In response to this challenge, the selection of low-cost, superior process and advanced technology sewage treatment methods has become a practical need for coal chemical enterprises, especially in areas with water shortages. It is urgent to reasonably dispose of coal chemical wastewater and achieve efficient utilization. At present, the wastewater treatment process is mainly based on pretreatment + double membrane concentration + evaporation crystallization, but the disadvantage of nanofiltration salt separation is that sodium sulfate and sodium chloride cannot be completely separated, and the membrane concentrated water side is a mixed salt of sodium chloride and sodium sulfate, resulting in low purity of sodium sulfate produced by evaporation crystallization, and low added value of sodium chloride and sodium sulfate products, and market saturation. Summary of the invention
[0003] To this end, an embodiment of the present invention provides a comprehensive treatment process for wastewater containing NaCl and Na2SO4. According to the characteristics of wastewater containing NaCl and Na2SO4 in the industry, the present invention introduces calcium ions for denitration, that is, converts sulfate into calcium sulfate precipitation, and becomes a salt water system mainly composed of sodium chloride. The required calcium ions come from the solution produced by the subsequent process, and the advantage is that no excess dissolved water for dissolving calcium salts is required, and the system scale will not be enlarged, reducing costs; similarly, according to the low solubility and high economic value of sodium bicarbonate, ammonia and carbon dioxide are introduced into the system, and sodium ions are converted into sodium bicarbonate through double decomposition; the double decomposition mother liquor is deaminated by calcium method, and the bicarbonate, carbonate and ammonium ions in the system are removed to obtain a feed liquid containing NaCl and CaCl2, part of which is refluxed to the denitration unit, and the other part is desalted, and the ternary phase diagram of NaCl-CaCl2-H2O is used, and the NaCl reuse and CaCl2.2H2O are obtained through evaporation crystallization and cooling crystallization. Compared with other processes, all materials in the present invention are fully utilized, and the problems of incomplete NaCl / Na2SO4 separation, high energy consumption and low product added value are successfully solved.
[0004] In order to achieve the above purpose, the embodiment of the present invention provides the following technical solutions:
[0005] The present invention provides a comprehensive treatment process for wastewater containing NaCl and Na2SO4, the process comprising the following steps:
[0006] (1) Desiliconization and defluorination treatment are performed on the raw water to obtain impurity-free effluent;
[0007] (2) The impurity-removing effluent reacts with a feed liquid containing NaCl and CaCl2 to undergo a denitration reaction, and solid-liquid separation is performed to obtain CaSO4.2H2O and a filtrate;
[0008] (3) the filtrate is passed through a cationic resin exchange column and then concentrated to obtain a refined concentrated solution;
[0009] (4) blowing NH3 and CO2 gases into the refined concentrated liquid to carry out an amination-carbonization reaction, and separating the solid from the liquid to obtain NaHCO3 crystals and an amination-carbonization mother liquor;
[0010] (5) adding Ca(OH)2 to the ammoniated carbonization mother liquor to react, and performing solid-liquid separation to obtain a CaCO3 precipitate and a supernatant;
[0011] (6) The supernatant is subjected to ammonia evaporation treatment, and the NH3 evaporated is sent to step (4) for ammonia carbonization reaction. The resulting NaCl and CaCl2-containing liquid is divided into two parts, one part is sent to step (2) for denitration reaction, and the other part is evaporated and crystallized to obtain NaCl crystals and CaCl2.2H2O crystals.
[0012] Furthermore, in step (1), the desiliconization treatment comprises: adding a desiliconization agent to the raw water at a mass ratio of 2-4:1, stirring at 20-40° C. for 10-30 minutes, and then settling for 30-60 minutes, wherein the desiliconization agent comprises sodium aluminate, polyaluminium chloride and magnesium chloride;
[0013] The defluorination treatment comprises: adding Ca 2+ With F - Add CaCl2 at a molar ratio of 0.5~1:1, stir at 20~40℃ for 0.5~1h, and then precipitate for 30~60min; or, add Al 3+ With F - AlCl3 is added in a molar ratio of 1 to 4:1, stirred at 20 to 40°C for 0.5 to 2 hours, and then precipitated for 30 to 60 minutes; or, the effluent after the desiliconization treatment is adsorbed by a resin, wherein the resin includes an aluminum-based resin or a non-aluminum-based defluorination resin.
[0014] Furthermore, in step (2), the Ca in the NaCl and CaCl2 solution is 2+ and remove SO4 from the effluent 2- The molar ratio is 1-1.2:1; the temperature of the denitration reaction is 20-40°C, and the time is 10-30 minutes.
[0015] Furthermore, in step (3), the filler of the cationic resin exchange column has the following functional groups: sulfonic acid group, carboxylic acid group; the concentration includes reverse osmosis and evaporation concentration, the TDS of the concentrated water side of reverse osmosis is ≥60g / L, and the TDS of the liquid after evaporation concentration is ≥300g / L.
[0016] Furthermore, in step (4), the molar ratio of NH3 to CO2 is 1:1.5-2, and the mass ratio of NH3 to NaCl in the refined concentrated solution is 8-16:1, wherein the ammonia is blown in twice, and the ammonia blown in for the first time accounts for 30%-50% of the total ammonia; the ammonia carbonization reaction is carried out in a closed reactor under the following reaction conditions: after reacting at 30-40°C for 0.5-2h, the temperature is lowered to 20-28°C and the reaction is continued for 0.5-2h, and the reactor is protected by CO2 gas to maintain the pressure between 0.1-1MPa; NH4 + The content is 80~150g / L.
[0017] Furthermore, the process also includes: calcining NaHCO3 crystals to obtain soda ash products and carbon dioxide, and the carbon dioxide is sent to step (4) for ammonia carbonization reaction; the calcination temperature is 200-300°C and the time is 20-40 minutes.
[0018] Furthermore, in step (5), Ca(OH)2 reacts with NH4 in the ammonia carbonization mother liquor to form a + The molar ratio is 1-1.5:2, the reaction temperature is 20-50°C, and the reaction time is 0.5-1h.
[0019] Furthermore, the process also includes: calcining the CaCO3 precipitate to obtain calcium oxide and carbon dioxide, the calcium oxide is sent to step (5) for reaction, and the carbon dioxide is sent to step (4) for ammonia carbonization reaction; the calcination temperature is 800~1200℃.
[0020] Furthermore, in step (6), the temperature of the ammonia evaporation treatment is 40-100° C. and the time is 1-3 hours.
[0021] Furthermore, in step (6), another part of the feed liquid is evaporated and crystallized at 70-100°C until the CaCl2 concentration in the feed liquid is 450-600 g / L, and the precipitated NaCl crystals are separated and sent to step (4) for ammonia carbonization reaction, and the remaining mother liquor is cooled to 50-70°C to obtain CaCl2.2H2O crystals.
[0022] The embodiments of the present invention have the following advantages:
[0023] 1) In the ammoniating and carbonizing process, the present invention improves the conversion rate of sodium bicarbonate crystals to more than 85% by adopting processes such as gradient cooling, blowing ammonia twice, and always maintaining CO2 gas pressurization protection during the reaction process, thereby solving the problem of low utilization rate of sodium chloride, and at the same time improving the particle size of sodium bicarbonate crystals, making it easy to filter and separate, and reducing the introduction of impurities; reducing the tail gas loss during the ammonia blowing process, and also providing more favorable conditions for carbonation.
[0024] 2) The present invention adopts an effective process to convert the mixed bittern mainly composed of Na2SO4 and NaCl into baking soda, calcium sulfate and calcium chloride with high economic value, realizing resource recycling. The impurities in the mixed salt are reasonably removed to ensure the purity of the product. The problem of high cost of coal chemical wastewater treatment and low economic value of products is successfully solved.
[0025] 3) In the present invention, except for a small amount of waste residue generated during the impurity removal process, the gas, liquid and solid products generated in the remaining processes are all recycled, thereby improving the recovery rate of the product, avoiding resource waste and reducing costs.
[0026] 4) In the water-salt system, by using the phase diagram and co-saturation point at various temperatures in the multi-component system, crystalline salts such as sodium bicarbonate, sodium chloride, and calcium chloride were successfully separated through double decomposition, evaporation crystallization, and cooling crystallization processes. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] In order to more clearly illustrate the implementation methods of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for the implementation methods or the description of the prior art. Obviously, the drawings in the following description are only exemplary, and for ordinary technicians in this field, other implementation drawings can be derived from the provided drawings without creative work.
[0028] Figure 1 A process flow chart for comprehensive treatment of wastewater containing NaCl and Na2SO4 provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0029] The following is a description of the implementation of the present invention by specific embodiments. People familiar with the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0030] like Figure 1 The process flow shown:
[0031] 1) Impurity removal system (silicon / fluorine): The raw water is treated for silicon removal. The silicon removal agent can be sodium aluminate, polyaluminium chloride, magnesium chloride, etc. The mass ratio of silicon removal agent to silicon element in raw water is 2~4:1, the reaction temperature is 20~40℃, the reaction time is 10~30min, the precipitation time is 30~60min, solid-liquid separation, and the silicon content in the silicon removal effluent is ≤5mg / L; the silicon removal effluent is treated for fluorine removal. The fluorine removal method can be selected from calcium method, aluminium salt, resin adsorption, among which: ① Calcium method fluorine removal is based on the molar ratio n(Ca 2+ ):n(F - ) = 0.5 ~ 1:1, add CaCl2, react at 20 ~ 40 ℃ for 0.5 ~ 1 h, and precipitate for 30 ~ 60 min; ② Aluminum salt defluorination by molar ratio n (Al 3+ ):n(F - )=1~4:1, add AlCl3, react at 20~40℃ for 0.5~2 h, and precipitate for 30~60 min; ③ Resin adsorption The resin can be aluminum-based resin or non-aluminum-based defluorination resin. In some specific embodiments, the temperature of resin adsorption treatment is 20~30℃, and the water inlet flow rate is 1~4BV / h. The fluorine content in the defluoridation effluent is ≤5mg / L.
[0032] 2) Denitration-Separation Unit: Step 1) The impurity removal effluent is subjected to denitration reaction with the NaCl and CaCl2-containing feed solution. According to the flow rate and sulfate concentration of the impurity removal effluent, the n(Ca 2+ ) and remove impurities in the effluent n(SO4 2- ) molar ratio is 1~1.2:1, calculate the flow rate of NaCl and CaCl2 feed liquid. The temperature of denitration reaction is 20~40℃, the time is 10~30min, and the SO4 in the system after the reaction is completed 2- Content ≤20mg / L, Ca 2+ Content ≤10mg / L; the denitrified liquid enters the separation unit to separate CaSO4.2H2O and filtrate.
[0033] 3) Brine refining-concentration unit: The filtrate separated in step 2) is refined and impurity-removed, and the calcium and magnesium ions in the system are replaced by a cationic resin (weak cationic sodium bed, with sulfonic acid or carboxylic acid group) exchange column. In some specific embodiments, the treatment temperature of the exchange column is 20~30℃, and the water inlet flow rate is 3~5BV / h. The calcium and magnesium content of the effluent is ≤1mg / L. The refined effluent is further subjected to reverse osmosis + evaporation concentration. Reverse osmosis and evaporation concentration are conventional technical means in the art. In some specific embodiments, reverse osmosis is concentrated in two stages, with two sections in each stage; evaporation concentration is concentrated by a multi-effect evaporation crystallization process, and the evaporation temperature is 50~100℃. The TDS (total dissolved solids content, the same below) of the reverse osmosis concentrated water side is ≥60g / L, and the TDS of the slurry after evaporation concentration is ≥300g / L.
[0034] 4) Ammoniated carbonization-separation-calcination: Cool the refined concentrated liquid obtained in step 3) to between 30 and 40°C, then add it to a sealed reactor, and blow in NH3 and CO2 gases, n(NH3):n(CO2)=1:1.5~2, and the mass ratio of NH3 to NaCl in the refined concentrated liquid is 8~16:1, wherein the ammonia is blown in twice, and the ammonia blown in for the first time accounts for 30%~50% of the total ammonia. After maintaining the reaction at 30~40°C for 0.5~2h, cool to 20~28°C and continue the reaction for 0.5~2h. The reaction process is sealed throughout, and the reactor is protected by CO2 gas to maintain the pressure between 0.1~1MPa. After the reaction is completed, the solid and liquid are separated to obtain NaHCO3 crystals and ammoniated carbonization mother liquor, wherein NH4 + The content is 80~150g / L. Furthermore, the NaHCO3 crystals are calcined at 200~300℃ for 20~40min to obtain a soda ash product with a purity of more than 99%. The CO2 gas released during the calcination process is collected and blown into the ammonia carbonization unit.
[0035] 5) Separation unit - ammonia evaporation - calcination - dissolution: Add Ca(OH)2, n(Ca 2 + ): n(NH4 + ) =1~1.5:2, react at 20~50℃ for 0.5~1h, separate and obtain CaCO3 precipitate and supernatant. The supernatant enters the ammonia distillation unit, heated to 40~100℃, and the reaction time is 1~3h. The evaporated ammonia returns to the ammonia carbonization unit to obtain a liquid containing NaCl and CaCl2. Further, the CaCO3 precipitate is calcined at 800~1200℃ to become CaO, and CaO combines with water to become Ca(OH)2 and returns to the separation unit.
[0036] 6) Preparation of calcium chloride: The NaCl and CaCl2-containing liquid obtained in step 5) is divided into two parts, one part of the liquid is returned to the denitration-separation unit in step 2), and the other part of the liquid is evaporated and crystallized at 70-100°C until the CaCl2 concentration in the liquid is 450-600 g / L. The precipitated NaCl crystals are separated and sent to the amination carbonization unit in step 4), and the remaining mother liquor is cooled to 50-70°C to obtain CaCl2.2H2O crystals with a purity of more than 98%. The crystallized mother liquor is cooled and returned to the evaporation crystallization unit.
[0037] Example 1
[0038] The composition of wastewater from a coal chemical enterprise is shown in Table 1.
[0039] Table 1 Coal chemical wastewater test results
[0040]
[0041] This embodiment provides a comprehensive treatment process for wastewater containing NaCl and Na2SO4, comprising the following steps:
[0042] Step 1: Remove silicon from the raw water. Add sodium aluminate to the raw water at a concentration of 68 mg / L. Stir for 20 min at 20 °C. Stop stirring. Let it settle for 30 min. Filter. The silicon content of the effluent is 2 mg / L. Remove fluoride from the filtrate after silicon removal by calcium salt. Add sodium aluminate to the effluent at a molar ratio of Ca 2+ :F - =0.5:1, add CaCl2, stir at 20℃ for 0.5 h, stop stirring, precipitate for 30 min, filter, the fluoride content of the effluent is 4.38 mg / L.
[0043] Step 2: Add NaCl and CaCl2 solution to the impurity removal effluent obtained in step 1, and adjust the concentration of n(Ca 2+ ): n(SO4 2- )=1:1, calculate the flow rate of NaCl and CaCl2 liquid, react at 20℃ for 10min, after the reaction, the SO4 in the system 2- The concentration is 18 mg / L, Ca 2+ The concentration is 10 mg / L; the denitrified liquid enters the separation unit to separate CaSO4.2H2O and filtrate.
[0044] Step 3: The filtrate separated in step 2 is refined and impurity-removed, and the calcium and magnesium ions in the system are replaced by a cation exchange resin with a sulfonic acid functional group. The treatment temperature is 25°C, the inlet flow rate is 3BV / h, and the outlet calcium and magnesium concentration is 0.2mg / L. Then reverse osmosis + evaporation concentration is performed. The TDS of the reverse osmosis concentrated water side is 65g / L, and the TDS of the feed liquid after evaporation concentration is 320g / L.
[0045] Step 4: Cool the refined concentrated solution obtained in step 3 to 30°C, then add it into a sealed reactor, and blow in NH3 and CO2 gases, n(NH3):n(CO2)=1:1.5, and the mass ratio of NH3 to NaCl in the refined concentrated solution is 8:1, wherein ammonia is blown in twice, and the first blown ammonia accounts for 30%. After maintaining the reaction time at 30°C for 2h, cool it to 20°C and continue the reaction for 2h. The reaction process is sealed throughout, and the reactor is protected by CO2 gas, and the pressure is maintained at 0.1MPa. Filter to obtain sodium bicarbonate crystals and NH4 +The content of the ammoniated carbonization mother liquor is 85g / L. The conversion rate of sodium ions into sodium bicarbonate crystals is 86%. The sodium bicarbonate crystals are calcined at 200℃ for 40min to obtain Na2CO3 with a purity of 99.25%. The CO2 gas released during the calcination process is collected and blown into the ammoniated carbonization unit.
[0046] Step 5: Add Ca(OH)2 to the ammoniated carbonization mother liquor obtained in step 4 to control n(Ca 2+ ): n(NH4 + )=1.2:2, stirred at 20℃ for 0.5h, and separated to obtain CaCO3 precipitate and supernatant. CaCO3 precipitate is calcined at 1000℃ to become CaO, and CaO is combined with water to become Ca(OH)2 and returned to the separation unit; the supernatant of the separation unit enters the ammonia distillation unit, heated to 40℃, the reaction time is 3h, and the evaporated ammonia gas returns to the ammonia carbonization unit to obtain a feed liquid containing NaCl and CaCl2.
[0047] Step 6: The NaCl and CaCl2-containing feed liquid separated in step 5 is divided into two parts, one part of the feed liquid is returned to step 2 for denitration reaction, and the other part of the feed liquid is evaporated and crystallized at 70°C until the CaCl2 concentration in the feed liquid is 550g / L. The precipitated NaCl crystals are separated and sent to the ammonia carbonization unit. The remaining mother liquor is cooled to 60°C to obtain CaCl2.2H2O crystals with a purity of more than 98%. The cooled crystallized mother liquor is returned to the evaporation crystallization unit.
[0048] Example 2
[0049] The composition of wastewater from a thermal power plant is shown in Table 2.
[0050] Table 2 Test results of wastewater from thermal power plants
[0051]
[0052] This embodiment provides a comprehensive treatment process for wastewater containing NaCl and Na2SO4, comprising the following steps:
[0053] Step 1: Remove silicon from the raw water. Add polyaluminium chloride to the raw water at a concentration of 124 mg / L. Stir for 20 min at 30 °C, stop stirring, settle for 45 min, filter, and the silicon content of the effluent is 1 mg / L. Remove fluorine from the filtrate after silicon removal by aluminium salt. Add polyaluminium chloride to the effluent at a molar ratio of Al 3+ : F - =1:1, add AlCl3, stir at 30℃ for 1 h, stop stirring, precipitate for 30 minutes, filter, the fluorine content of the effluent is 3.2 mg / L.
[0054] Step 2: Add NaCl and CaCl2 solution to the impurity removal effluent obtained in step 1, and adjust the concentration of n(Ca 2+ ): n(SO4 2- )=1.05:1, calculate the flow rate of NaCl and CaCl2 liquid, react at 30℃ for 20min, and after the reaction, the SO4 in the system 2- The content is 5mg / L, Ca 2+ The content is 4 mg / L; the denitrified liquid enters the separation unit to separate CaSO4.2H2O and filtrate.
[0055] Step 3: The filtrate separated in step 2 is refined and impurity-removed, and the calcium and magnesium ions in the system are replaced by a cation exchange resin with a carboxyl functional group. The treatment temperature is 25°C, the water inlet flow rate is 4BV / h, and the effluent calcium and magnesium content is 0.5mg / L. Then reverse osmosis + evaporation concentration is performed. The TDS of the reverse osmosis concentrated water side is 63g / L, and the TDS of the feed liquid after evaporation concentration is 300g / L.
[0056] Step 4: The refined concentrated solution obtained in step 3 is cooled to 35°C, then added to a sealed reactor, and NH3 and CO2 gases are blown in, n(NH3):n(CO2)=1:1.8, and the mass ratio of NH3 to NaCl in the refined concentrated solution is 12:1, wherein ammonia is blown in twice, and the first blown ammonia accounts for 40%. After maintaining the reaction time at 35°C for 1h, the temperature is lowered to 25°C and the reaction is continued for 1h. The reaction process is sealed throughout, and the reactor is protected by CO2 gas, and the pressure is maintained at 0.5MPa. Filter to obtain sodium bicarbonate crystals and NH4 + The content of ammoniated carbonization mother liquor is 126g / L. The conversion rate of sodium ions into sodium bicarbonate crystals is 91%. The sodium bicarbonate crystals are calcined at 250℃ for 30min to obtain Na2CO3 with a purity of 99.48%. The CO2 gas released during the calcination process is collected and blown into the ammoniated carbonization unit.
[0057] Step 5: Add Ca(OH)2 to the ammoniated carbonization mother liquor obtained in step 4 to control n(Ca 2+ ): n(NH4 + )=1.2:2, stirred at 30℃ for 0.8h, and separated to obtain CaCO3 precipitate and supernatant. CaCO3 precipitate is calcined at 800℃ to become CaO, and CaO is combined with water to become Ca(OH)2 and returned to the separation unit; the supernatant of the separation unit enters the ammonia distillation unit, heated to 80℃, the reaction time is 2h, and the evaporated ammonia gas returns to the ammonia carbonization unit to obtain a feed liquid containing NaCl and CaCl2.
[0058] Step 6: The NaCl and CaCl2-containing liquid separated in step 5 is divided into two parts, one part of the liquid is returned to step 2 for denitration reaction, and the other part of the liquid is evaporated and crystallized at 90°C to a CaCl2 concentration of 450g / L. The precipitated NaCl crystals are separated and sent to the ammonia carbonization unit. The remaining mother liquor is cooled to 50°C to obtain CaCl2.2H2O crystals with a purity of more than 98%. The cooled crystallization mother liquor is returned to the evaporation crystallization unit.
[0059] Example 3
[0060] The composition of the wastewater from a coal chemical enterprise is shown in Table 3.
[0061] Table 3 Coal chemical wastewater test results
[0062]
[0063] This embodiment provides a comprehensive treatment process for wastewater containing NaCl and Na2SO4, comprising the following steps:
[0064] Step 1: Remove silicon from the raw water. Add magnesium chloride to the raw water at a concentration of 90 mg / L, stir at 40°C for 30 minutes, stop stirring, settle for 60 minutes, filter, and the silicon content of the effluent is 4 mg / L; remove fluorine from the filtrate after silicon removal by resin adsorption. The resin is aluminum-based resin, the adsorption temperature is 30°C, the water inlet flow rate is 3BV / h, and the fluorine content of the effluent is 0.5 mg / L.
[0065] Step 2: Add NaCl and CaCl2 solution to the impurity removal effluent obtained in step 1, and adjust the concentration of n(Ca 2+ ): n(SO4 2- )=1.1:1, calculate the flow rate of NaCl and CaCl2 liquid, react at 40℃ for 30min, and after the reaction, the SO4 in the system 2- The content is 15mg / L, Ca 2+ The content is 8 mg / L; the denitrified liquid enters the separation unit to separate CaSO4.2H2O and filtrate.
[0066] Step 3: The filtrate separated in step 2 is refined and impurity-removed, and the calcium and magnesium ions in the system are replaced by a cation exchange resin with a sulfonic acid functional group. The treatment temperature is 25°C, the water inlet flow rate is 5BV / h, and the calcium and magnesium content of the effluent is 0.8mg / L. Then reverse osmosis + evaporation concentration is performed. The TDS of the reverse osmosis concentrated water side is 68g / L, and the TDS of the feed liquid after evaporation concentration is 350g / L.
[0067] Step 4: The refined concentrated solution obtained in step 3 is cooled to 40°C, then added to a sealed reactor, and NH3 and CO2 gases are blown in, n(NH3):n(CO2)=1:2, and the mass ratio of NH3 to NaCl in the refined concentrated solution is 16:1, wherein ammonia is blown in twice, and the ammonia gas blown in for the first time accounts for 50%. After maintaining the reaction time at 40°C for 0.5h, the temperature is lowered to 28°C and the reaction is continued for 0.5h. The reaction process is sealed throughout, and the reactor is protected by CO2 gas, and the pressure is maintained at 1MPa. Filter to obtain sodium bicarbonate crystals and NH4 + The content of the ammoniated carbonization mother liquor is 148g / L. The conversion rate of sodium ions into sodium bicarbonate is 95%. The sodium bicarbonate crystals are calcined at a temperature of 300°C for 20 minutes to obtain Na2CO3 with a purity of 99.56%. The CO2 gas released during the calcination process is collected and blown into the ammoniated carbonization unit.
[0068] Step 5: Add Ca(OH)2 to the mother liquor after the reaction in step 4 to control n(Ca 2+ ): n(NH4 + )=1.5:2, stirred at 35℃ for 1h, and separated to obtain CaCO3 precipitate and supernatant. CaCO3 precipitate is calcined at 1100℃ to become CaO, and CaO is combined with water to become Ca(OH)2 and returned to the separation unit; the supernatant of the separation unit enters the ammonia distillation unit, heated to 100℃, the reaction time is 1h, and the evaporated ammonia returns to the ammonia carbonization unit to obtain a feed liquid containing NaCl and CaCl2.
[0069] Step 6: The NaCl and CaCl2-containing feed solution separated in step 5 is divided into two parts, one part of the feed solution is returned to step 2 for denitration reaction, and the other part of the feed solution is evaporated and crystallized at 100°C until the CaCl2 concentration in the feed solution is 700g / L. The precipitated NaCl crystals are separated and sent to the ammonia carbonization unit. The remaining mother liquor is cooled to 70°C to obtain CaCl2.2H2O crystals with a purity of more than 98%. The cooled crystallized mother liquor is returned to the evaporation crystallization unit.
[0070] Although the present invention has been described in detail above by general description and specific embodiments, it is obvious to those skilled in the art that some modifications or improvements can be made to the present invention. Therefore, these modifications or improvements made without departing from the spirit of the present invention all belong to the scope of protection claimed by the present invention.
Claims
1. A mixture containing NaCl and Na 2 SO 4 Comprehensive wastewater treatment process, It is characterized in that The process comprises the following steps: (1) Desiliconization and defluorination treatment are performed on the raw water to obtain impurity-free effluent; (2) The impurity-removing effluent contains NaCl and CaCl 2 The feed liquid undergoes denitrification reaction, solid-liquid separation, and obtains CaSO 4 .2H 2 O and filtrate; (3) the filtrate is passed through a cationic resin exchange column and then concentrated to obtain a refined concentrated solution; (4) Bubbling NH into the refined concentrated solution 3 and CO 2 The gas undergoes ammoniating and carbonizing reaction, and solid-liquid separation is performed to obtain NaHCO 3 Crystals and ammoniated carbonized mother liquor; (5) Adding Ca(OH) to the ammoniated carbonization mother liquor 2 Reaction, solid-liquid separation, and CaCO 3 sediment and supernatant; (6) The supernatant is subjected to ammonia evaporation treatment, and the NH 3 Go to step (4) for ammonia carbonization reaction, and the obtained product contains NaCl and CaCl 2 The feed liquid is divided into two parts, one part goes to step (2) for denitrification reaction, and the other part is evaporated and crystallized to obtain NaCl crystals and CaCl 2 ·2H 2 O crystal; In step (4), NH 3 and CO 2 The molar ratio of NH 3 The mass ratio of ammonia to NaCl in the refined concentrate is 8-16:1, wherein ammonia is bubbled in twice, and the first ammonia accounts for 30%-50% of the total ammonia; The amination and carbonization reaction is carried out in a closed reactor under the following reaction conditions: after reacting at 30-40°C for 0.5-2h, the temperature is lowered to 20-28°C and the reaction is continued for 0.5-2h, and the CO in the reactor is 2 Gas protection, maintaining pressure between 0.1~1MPa; The NH 4 + The content is 80~150g / L.
2. The method according to claim 1 containing NaCl and Na 2 SO 4 Comprehensive wastewater treatment process, It is characterized in that In step (1), The desiliconization treatment comprises: adding a desiliconization agent to raw water at a mass ratio of 2-4:1 between the desiliconization agent and the silicon element, stirring for 10-30 minutes at 20-40° C., and then settling for 30-60 minutes, wherein the desiliconization agent comprises sodium aluminate, polyaluminum chloride, and magnesium chloride; The defluorination treatment comprises: adding Ca 2+ With F - Add CaCl at a molar ratio of 0.5~1:1 2 , stir at 20~40℃ for 0.5~1h, and then precipitate for 30~60min; or, add Al 3+ With F - Add AlCl at a molar ratio of 1~4:1 3 , stirring at 20-40°C for 0.5-2h, and then settling for 30-60min; or, the effluent after the desiliconization treatment is adsorbed by a resin, wherein the resin includes an aluminum-based resin or a non-aluminum-based defluorination resin.
3. The method according to claim 1 containing NaCl and Na 2 SO 4 Comprehensive wastewater treatment process, It is characterized in that In step (2), the 2 Ca in the feed solution 2+ SO 4 2- The molar ratio is 1-1.2:1; the temperature of the denitration reaction is 20-40°C, and the time is 10-30 minutes.
4. The method according to claim 1 containing NaCl and Na 2 SO 4 Comprehensive wastewater treatment process, It is characterized in that In step (3), The filler of the cationic resin exchange column has the following functional groups: sulfonic acid group, carboxylic acid group; The concentration includes reverse osmosis and evaporation concentration, the TDS of the concentrated water side of reverse osmosis is ≥60g / L, and the TDS of the feed liquid after evaporation concentration is ≥300g / L.
5. The method according to claim 1 containing NaCl and Na 2 SO 4 Comprehensive wastewater treatment process, It is characterized in that The process also includes: treating NaHCO 3 The crystals are calcined to obtain soda ash product and carbon dioxide, and the carbon dioxide is sent to step (4) for ammonia carbonization reaction; The calcination temperature is 200-300° C. and the calcination time is 20-40 min.
6. The method according to claim 1 containing NaCl and Na 2 SO 4 Comprehensive wastewater treatment process, It is characterized in that In step (5), Ca(OH) 2 With the NH 4 + The molar ratio is 1-1.5:2, the reaction temperature is 20-50°C, and the reaction time is 0.5-1h.
7. The method according to claim 1 containing NaCl and Na 2 SO 4 Comprehensive wastewater treatment process, It is characterized in that The process also includes: 3 The precipitate is calcined to obtain calcium oxide and carbon dioxide, the calcium oxide is sent to step (5) for reaction, and the carbon dioxide is sent to step (4) for ammonia carbonization reaction; The calcination temperature is 800-1200°C.
8. The method according to claim 1 containing NaCl and Na 2 SO 4 Comprehensive wastewater treatment process, It is characterized in that In step (6), the temperature of the ammonia evaporation treatment is 40-100° C. and the time is 1-3 hours.
9. The method according to claim 1 containing NaCl and Na 2 SO 4 Comprehensive wastewater treatment process, It is characterized in that In step (6), another portion of the feed solution is evaporated and crystallized at 70-100°C until CaCl 2 The concentration is 450-600 g / L. The precipitated NaCl crystals are separated and sent to step (4) for ammonia carbonization reaction. The remaining mother liquor is cooled to 50-70 °C to obtain CaCl 2 ·2H 2 O crystal.
Citation Information
Patent Citations
Salt, alkali and calcium combined cycle production technology by the use of well mineral salt
CN102205979A
Technology for combined production of sodium carbonate and ammonium chloride through sodium sulfate type brine thermal cycle method
CN105000579A
Method for producing sodium carbonate with salt-containing wastewater and CO2
CN106673019A
Method for preparation of sodium bicarbonate and ammonium sulfate from chemical strong brine
CN106865571A
Method for removal of ammonia nitrogen from waste water
KR1020050006517A