Magnetic powder plant wastewater treatment and resource recovery and utilization method
By using aeration and flocculation technology in the wastewater treatment of magnetic powder plants to recover high-purity iron red, the problem of high content of impurity metal ions in the existing technology is solved, and the feasibility of ferrite and resource utilization efficiency are improved.
Patent Information
- Application Number
- CN202410808994.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-21
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-06-21
AI Technical Summary
Existing technology cannot effectively recover metal ions such as Cu and alkaline earth metals in the wastewater treatment of magnetic powder plants. This results in a high content of impurity metal ions in iron red, which affects its feasibility for ferrite manufacturing and cannot be effectively enriched after wastewater treatment. Impurities in the separation precipitation, such as Cu and Sr, affect its utilization as a raw material for permanent magnet ferrite.
Adjust the pH to neutral by aerating and adding alkali solution in the reaction sedimentation tank, then adding polycarboxylic acid and hydroxide for flocculation, further precipitating and filtering, drying, and crushing to recover iron red, and adjusting the pH value for separation. Alkaline earth metal salts and copper ions reduce the content of impurity metals and improve the purity of ferrite.
It achieves efficient recovery of metal ions such as Cu and alkaline earth metals in the wastewater of the magnetic powder factory, increases the ferrite content of iron red, and reduces the content of impurity metals, so that it can be directly used for bonding or sintering permanent magnet ferrite magnetic powder. The preparation optimizes resource utilization and processing efficiency.
Smart Images

Figure CN118724331A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of wastewater treatment and resource utilization, and in particular to a method for treating wastewater from a magnetic powder factory and recovering and utilizing resources. Background Art
[0002] A large amount of water resources are needed in the production process of magnetic powder plants. Under the current optimized process, most of the water resources can be recycled in production, with less discharge. The purpose of sewage treatment is mainly to meet the sewage discharge requirements and production indicators of recycling. There are still deficiencies in the separation and reuse of solid resources after treatment. At the same time, since the sewage contains a large amount of Fe 3+ In the conventional method, the Fe(OH)3 particles precipitated after adjusting the pH with alkali are too fine, and the filter press treatment efficiency is low.
[0003] In the prior art, CN112299630A discloses a device and method for recovering sodium chloride from wastewater in the preparation of bonded permanent ferrite magnetic powder. The device and method provided by the invention utilize the heat generated in the process of preparing bonded permanent ferrite magnetic powder to crystallize and concentrate the wastewater, and can separate the salt in the wastewater. However, it does not mention a systematic method for treating wastewater in a magnetic powder factory, nor does it propose a method for recovering metals such as Cu.
[0004] CN201410530017.8 discloses a method for treating wastewater produced by manganese zinc ferrite, comprising the following steps: coarsely filtering the wastewater produced by manganese zinc ferrite, adjusting the pH of the wastewater to 6.5-7.5 in a regulating tank, adding a flocculant under stirring in a coagulation sedimentation tank, stirring and mixing, and settling, and the supernatant water is the drainage after reaching the standard. This method is also limited to reaching the standard for wastewater discharge, and other metals cannot be recycled, and the recycling and application of iron red is not mentioned.
[0005] CN110395770A discloses a method for producing red iron oxide using sludge. Although the scheme mentions the resource utilization of red iron oxide, the impurity metal ions therein are not removed. At the same time, a high temperature of 95°C needs to be maintained, which consumes a lot of energy.
[0006] Some other documents also mentioned the scheme of recovering red iron from sewage treatment for permanent magnet production. Although it has certain theoretical feasibility, the ferrite recovered from sewage treatment has mixed components and low purity, and needs to be matched with corresponding purification production lines, which will increase the cost and make it unsuitable for production. The present invention aims to further separate the impurity metal ions in the sludge, further improve the feasibility of recovering red iron for ferrite manufacturing, and at the same time, enrich and separate the impurities such as Cu and Sr contained in the precipitated part under the condition of meeting the sewage discharge standard, so that it can be recovered as a permanent magnet ferrite raw material. Summary of the invention
[0007] The present invention aims to overcome the above-mentioned problems existing in the prior art and provides a method for treating wastewater from a magnetic powder factory and recovering and utilizing resources, which can recover metal ions such as Cu and alkaline earth metals in the wastewater, reduce impurities in the recovered iron red, and increase its ferrite content, so that it can be directly used for the preparation of bonded permanent magnet ferrite powder and sintered permanent magnet ferrite powder, thereby realizing resource utilization.
[0008] In order to achieve the above object, the present invention adopts the following technical solutions: In a first aspect, the present invention provides a method for treating wastewater from a magnetic powder factory and recovering resources, comprising the following steps: (1) passing the wastewater into a reaction sedimentation tank, aerating it, and adding alkali solution to adjust the pH of the wastewater to neutral, and discharging the supernatant after reaction sedimentation; (2) adding polycarboxylic acid and hydroxide to the bottom flocculent obtained by precipitation in step (1), and then adding a flocculant, stirring and further precipitating to obtain a blue solution A and a flocculent precipitate; filtering the obtained flocculent precipitate, drying, and crushing to obtain recovered iron red; (3) adjusting the pH of the blue solution A to 9-10.5, precipitating a white precipitate and obtaining a blue solution B; filtering the white precipitate to obtain an alkaline earth metal salt; (4) The pH of the blue solution B is adjusted to 11-12 to obtain a blue flocculent precipitate. The remaining solution after filtration is discharged into the reaction sedimentation tank described in step (1) and mixed with the wastewater.
[0009] In step (1) of the present invention, the wastewater is first aerated and an alkali solution is added to adjust the pH of the wastewater to neutral. The main purpose of aeration is to reduce the COD caused by ferrous iron and to have a stirring effect. After the pH is adjusted to neutral, Fe 3+ , Cu 2+ The ions of chromium and alkaline earth metals can form hydroxide precipitation, and the supernatant meets the requirements of the third-level standard of the Integrated Wastewater Discharge Standard GB 8978-1996. 6+ It is the main environmental hazard ion to be monitored. 6+ It has been monitored closely, and the wastewater itself contains Fe 2+ , can Cr 6+ Reduction to Cr 3+ , and the Fe(OH)3 colloids produced during the pH adjustment process have an adsorption effect, and the main metal ions are adsorbed. 6+ The content reaches the discharge standard. The small amount of metal ions contained in the discharged supernatant is mainly Na + , K + Light metals such as smelters can be recycled in production, mainly used as cooling water for products, etc. A large amount of water is consumed during evaporation during cooling.
[0010] After the upper clear liquid is discharged, the bottom floccules cannot be filtered because the Fe(OH)3 is too fine, which makes it impossible to achieve rapid dehydration by filtering or other methods, so further flocculation is required. In step (2) of the present invention, before adding the flocculant, polycarboxylic acid and hydroxide are first added, which can play a coagulant effect and reduce the amount of PAM used. The addition of polycarboxylic acid and hydroxide can dissolve the copper ions and alkaline earth metal ions in the precipitate, and then the flocculant is added for flocculation to obtain a blue solution A containing copper ions and alkaline earth metal ions and a flocculent precipitate whose main component is Fe(OH)3; the recovered iron red obtained after filtering, drying and crushing the flocculent precipitate has a high iron oxide content of more than 98%, and a low content of metal ion impurities such as Cu and alkaline earth metals, and can be directly used in the preparation of low-end bonded permanent magnet ferrite powder and sintered permanent magnet ferrite powder (in low-end products, the iron oxide content is above 98.5). Since Cu in the raw materials when preparing ferrite is less than 1%, the iron oxide content is 0.1% and 0.04% respectively. 2+ The content is very small (<0.05%), so in the prior art, when recovering iron red from wastewater of magnetic powder factories, no attention is paid to Cu 2+ Separation. The present invention has found that before adding polycarboxylic acid and hydroxide, Cu is enriched in the flocculent, and the content can be close to 10wt%. If it is not separated, it will greatly affect the subsequent resource utilization of recovered iron red. In step (1), the upper clear liquid is first discharged, which can reduce the amount of water treatment in subsequent work, prevent excessive dilution of PAM, reduce the precipitation time, and increase the metal ion concentration of the blue solution A. The drying process in step (2) includes decomposing Fe(OH)3 into Fe2O3.
[0011] After the Fe(OH)3 precipitate is recovered, the pH of the blue solution A is adjusted to 9-10.5, and alkaline earth metal salts can be recovered, the main components of which are strontium salts and a very small amount of barium salts or calcium salts. The pH of the obtained blue solution B is then adjusted to 11-12, and the copper ions therein are precipitated and recovered. The remaining liquid finally obtained can enter the reaction sedimentation tank and be mixed with wastewater for further treatment. The pH adjustment in step (3) is critical because it overlaps with the precipitation pH in step (4). If the precipitation pH in step (3) exceeds 10.5, the copper ions will precipitate together with the alkaline earth metal citrate, and they cannot be recovered separately for subsequent use.
[0012] Preferably, after the supernatant is discharged in step (1), the solid content of the bottom flocs obtained is 3.5 wt% to 10 wt%.
[0013] Preferably, the polycarboxylic acid in step (2) is selected from one or more of citric acid, oxalic acid, malic acid, tartaric acid and succinic acid; and the hydroxide is selected from one or both of sodium hydroxide and potassium hydroxide.
[0014] Preferably, the mass ratio of the polycarboxylic acid to the hydroxide added in step (2) is 1.5 to 5:1; the concentration of the added polycarboxylic acid in the bottom flocculent is 0.1 to 4 g / L. If the addition ratio of the polycarboxylic acid to the hydroxide is too small, the pH of the water body after addition is too high, and the salt generated by the reaction of the polycarboxylic acid and the impure metal ions will precipitate prematurely, resulting in a decrease in the purity of the iron hydroxide filter cake, affecting the subsequent utilization of the recovered iron oxide red.
[0015] Preferably, in step (2), the polycarboxylic acid and the hydroxide are added in the form of aqueous solution; when adding, the polycarboxylic acid and the hydroxide are first prepared into a mixed solution, and then added to the bottom floccules; or the polycarboxylic acid solution is first added to the bottom floccules and then the hydroxide solution is added. The present invention has found that the amount of PAM used when the polycarboxylic acid is added first and then the hydroxide is added is less than that when the hydroxide is added first and then the polycarboxylic acid is added, and the amount of PAM used when the polycarboxylic acid is added first can reduce the amount of PAM by about 50wt%.
[0016] Preferably, the flocculant in step (2) is PAM, and the concentration of the added flocculant in the bottom floc is 0.01-0.1 g / L.
[0017] In the second aspect, the present invention provides an application of recycled iron red recovered by the above method in the preparation of bonded permanent magnet ferrite powder, comprising the following steps: adding the recycled iron red at a mass ratio of 1% to 2% into iron red with a purity of more than 98.5%, and then adding BaCO3 to make the molar ratio of Fe and Ba 5.5 to 5.8 to obtain a mixture, and then densifying, balling, pre-calcining, crushing and pulverizing the mixture to obtain bonded permanent magnet ferrite powder.
[0018] Preferably, the densification time is 0.5 to 1.5 hours; the pre-sintering temperature is 1180 to 1230° C., and the pre-sintering time is 60 to 120 minutes; and the average particle size of the obtained bonded permanent magnet ferrite powder is 2.0 to 2.3 μm.
[0019] In the third aspect, the present invention provides an application of recycled iron red obtained by the above method in the preparation of sintered permanent magnet ferrite powder, comprising the following steps: adding the recycled iron red at a mass ratio of 1% to 2% into iron red with a purity of more than 99%, and then adding SrCO3 to make the molar ratio of Fe and Sr 5.3 to 6.0 to obtain a mixture, and then densifying, balling, pre-calcining, crushing and pulverizing the mixture to obtain sintered permanent magnet ferrite powder.
[0020] Preferably, the densification time is 0.5 to 1.5 hours; the pre-sintering temperature is 1240 to 1280° C., and the pre-sintering time is 60 to 120 minutes; and the average particle size of the obtained sintered permanent magnet ferrite powder is 3 to 6 μm.
[0021] The performance of permanent ferrite is greatly affected by the composition of raw materials. In the prior art, the recycled iron red recovered from the wastewater of magnetic powder factory has less ferrite content and more metal impurities. It is easy to cause unqualified products if it is directly used for ferrite preparation without treatment. The recycled iron red recovered by the method of the present invention has high ferrite content and less metal ion impurities such as Cu. It can be directly added to the iron red for preparing bonding or sintering permanent ferrite without affecting the performance of the prepared ferrite.
[0022] Therefore, the present invention has the following beneficial effects: (1) It can further optimize the utilization of wastewater resources in magnetic powder plants and reduce wastewater discharge; (2) The metal ions in the wastewater of the magnetic powder factory can be recovered, further improving the feasibility of recovering iron red for ferrite manufacturing; (3) The treatment efficiency is high, and the additives are environmentally friendly and have no environmental hazards. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 The present invention is a flow chart of wastewater treatment and resource recovery in a magnetic powder factory. DETAILED DESCRIPTION
[0024] The present invention is further described below in conjunction with specific implementation methods.
[0025] In the present invention, unless otherwise specified, all equipment and raw materials can be purchased from the market or are commonly used in the industry. The methods in the following embodiments, unless otherwise specified, are conventional methods in the art.
[0026] The magnetic powder factory wastewater used in the embodiments of the present invention comes from the magnetic powder production wastewater of Zhejiang Ante Magnetic Materials Co., Ltd. The sampling point is the water inlet of the wastewater treatment plant, and the obtained wastewater is untreated.
[0027] Embodiment 1: A method for treating wastewater from a magnetic powder plant and recovering resources, the process is as follows Figure 1 As shown in , the following steps are included: (1) The wastewater was passed into a reaction sedimentation tank, aerated, and sodium hydroxide solution was added to adjust the pH of the wastewater to 7. The water body turned into an orange-yellow turbid liquid. After standing for 60 minutes, the stratified wastewater was obtained. The supernatant was tested for Cr 6+ The content meets the discharge standard, the supernatant is discharged, and the bottom flocs are obtained; the solid content of the bottom flocs is measured to be 3.8%, and the composition of the bottom flocs is measured, as shown in Table 1; (2) Dissolve citric acid and sodium hydroxide in water at a mass ratio of 2.4:1 to obtain a sodium citrate aqueous solution; take 100 mL of the bottom flocs obtained in step (1), add the sodium citrate aqueous solution, and then add a flocculant PAM until the flocs agglomerate and a clear solution is precipitated; in the added sodium citrate aqueous solution, the concentration of citric acid in the bottom flocs is 0.38 g / L, and the concentration of the added PAM in the bottom flocs is 0.08 g / L; let stand for 5 minutes, at which time the pH is 7.8, to obtain a blue solution A and a flocculent precipitate; filter the obtained flocculent precipitate, dry it, and crush it to obtain 5.6 g of recovered iron red, and measure its component composition, as shown in Table 2; (3) adding sodium hydroxide solution to adjust the pH of blue solution A to 9, precipitating a white precipitate to obtain blue solution B; filtering and drying the white precipitate to obtain 1.2 g of alkaline earth metal citrate, and measuring its composition, as shown in Table 2; (4) Sodium hydroxide solution was added to adjust the pH of the blue solution B to 11 to obtain a blue flocculent precipitate. The remaining liquid after filtration was discharged into the reaction sedimentation tank described in step (1) and mixed with waste water. The blue flocculent precipitate was dried to obtain 0.65 g of blue filter residue, and its composition was measured, as shown in Table 2.
[0028] Embodiment 2: The difference between Example 2 and Example 1 is that the concentration of citric acid added in step (2) in the bottom floc is 1.92 g / L; the concentration of PAM added in the bottom floc is 0.05 g / L; the rest is the same as in Example 1; the recovered iron red mass is 5.5 g, alkaline earth metal citrate is 1.3 g, and blue filter residue is 0.66 g.
[0029] Embodiment 3: The difference between Example 3 and Example 1 is that the concentration of citric acid added in step (2) in the bottom floc is 3.84 g / L, and the concentration of PAM added in the bottom floc is 0.1 g / L; the rest is the same as in Example 1; the recovered iron red mass is 11 g, alkaline earth metal citrate is 2.74 g, and blue filter residue is 1.31 g.
[0030] Embodiment 4: The difference between Example 4 and Example 1 is that the concentration of PAM added in step (2) in the bottom floc is 0.09 g / L; step (3) adjusts the pH of blue solution A to 10, and the rest is the same as in Example 1; the recovered iron oxide mass is 5.6 g, alkaline earth metal citrate is 1.5 g, and blue filter residue is 0.63 g.
[0031] Embodiment 5: The difference between Example 5 and Example 1 is that step (4) adjusts the pH of blue solution B to 12, and the rest is the same as in Example 1; the recovered iron oxide mass is 5.53 g, alkaline earth metal citrate is 1.32 g, and blue filter residue is 0.67 g.
[0032] Embodiment 6: The difference between Example 6 and Example 1 is that in step (2), a citric acid aqueous solution is first added to the bottom floccules, and then a sodium hydroxide aqueous solution is added, and finally PAM is added, the concentration of the added citric acid in the bottom floccules is 0.19 g / L, the concentration of the sodium hydroxide in the bottom floccules is 0.04 g / L, and the concentration of the PAM in the bottom floccules is 0.07 g / L; after standing, the pH is 5.8, and the precipitate is blue-green; the rest is the same as in Example 1; the mass of recovered iron red is 5.38 g, alkaline earth metal citrate is 1.61 g, and blue filter residue is 0.64 g.
[0033] Embodiment 7: The difference between Example 7 and Example 1 is that in step (2), a citric acid aqueous solution is first added to the bottom floccules, and then a sodium hydroxide aqueous solution is added, and finally PAM is added, the concentration of the added citric acid in the bottom floccules is 0.19 g / L, the concentration of the sodium hydroxide in the bottom floccules is 0.08 g / L, and the concentration of the PAM in the bottom floccules is 0.05 g / L; after standing, the pH is 6.4, and the precipitate is blue-green; the rest is the same as in Example 1; the mass of recovered iron red is 5.42 g, alkaline earth metal citrate is 1.55 g, and blue filter residue is 0.62 g.
[0034] Embodiment 8: The difference between Example 8 and Example 1 is that in step (2), sodium hydroxide aqueous solution is first added to the bottom floccules, then citric acid aqueous solution is added, and finally PAM is added, the concentration of the added citric acid in the bottom floccules is 0.19 g / L, the concentration of sodium hydroxide in the bottom floccules is 0.04 g / L, and the concentration of PAM in the bottom floccules is 0.09 g / L; the pH after standing is 5.8; the rest is the same as in Example 1; the mass of recovered iron red is 5.38 g, alkaline earth metal citrate is 1.61 g, and blue filter residue is 0.64 g.
[0035] Comparative Example 1: The difference between Comparative Example 1 and Example 1 is that no sodium citrate solution is added in step (2), the concentration of the added PAM in the bottom floc is 0.2 g / L, the pH after standing is 7, and the precipitate is a colorless and transparent solution; the rest is the same as in Example 1; the mass of recovered iron red is 7.3 g, and there is basically no precipitation in steps (3) and (4) when adjusting the pH of the colorless and transparent solution.
[0036] Comparative Example 2: The difference between Comparative Example 2 and Example 1 is that only citric acid solution is added in step (2), and no sodium hydroxide solution is added; the concentration of the added citric acid in the bottom floc is 0.19 g / L, the concentration of the added PAM in the bottom floc is 0.21 g / L, the pH after standing is 4.8, the precipitate is light yellow turbid, and a colorless transparent solution is obtained after filtration; the rest is the same as in Example 1; the mass of recovered iron red is 7.3 g, and only yellow substance is precipitated in steps (3) and (4) to adjust the pH of the colorless transparent solution.
[0037] Comparative Example 3: The difference between Comparative Example 3 and Example 1 is that only sodium hydroxide solution is added in step (2), and citric acid solution is not added; the concentration of the added sodium hydroxide in the bottom floc is 0.04 g / L, the concentration of the added PAM in the bottom floc is 0.18 g / L, the pH after standing is 8.2, and the precipitate is a colorless transparent solution; the rest is the same as in Example 1; the mass of the recovered iron red is 7.5 g, and there is basically no precipitation in the steps (3) and (4) when adjusting the pH of the colorless transparent solution.
[0038] Comparative Example 4: The difference between Comparative Example 4 and Example 1 is that in step (2), acetic acid solution is used instead of the sodium citrate aqueous solution in Example 1, and the concentration of the added acetic acid in the bottom floc is 0.12 g / L; the rest is the same as in Example 1.
[0039] Comparative Example 5: The difference between Comparative Example 5 and Example 1 is that in step (2), sodium acetate solution is used instead of the sodium citrate aqueous solution in Example 1, and the concentration of the added sodium acetate in the bottom floc is 0.16 g / L; the rest is the same as in Example 1.
[0040] Comparative Example 6: The difference between Comparative Example 6 and Example 1 is that the concentration of citric acid added in step (2) in the bottom floc is 0.19 g / L; the rest is the same as in Example 1; the recovered iron red mass is 6.63 g, alkaline earth metal citrate is 1.03 g, and blue filter residue is 0.45 g.
[0041] Comparative Example 7: The difference between Comparative Example 7 and Example 1 is that in step (3), the pH of the blue solution A is adjusted to 10.8, and the rest is the same as in Example 1.
[0042] Table 1: Mass proportion of metal elements in the bottom floc.
[0043] Table 2: Recovered product composition measurement results.
[0044] Among them, whether the discharged supernatant meets the standards refers to whether it meets the third-level standard requirements of the "Comprehensive Sewage Discharge Standard" GB 8978-1996.
[0045] As can be seen from Table 2, the method of the present invention used in Examples 1 to 8 can effectively separate alkaline earth metal ions such as Cu ions and Sr from the precipitate to obtain recovered iron red with a high Fe content. The order of adding citric acid and sodium hydroxide has a certain influence on the recovery effect: in Examples 1 to 5, citric acid and sodium hydroxide are mixed to prepare sodium citrate aqueous solution and then added, which can obtain a better flocculation effect at a lower PAM addition amount; in Examples 6 and 7, citric acid is added first and then sodium hydroxide, which can reduce the amount of PAM and reduce the processing cost compared with adding sodium hydroxide first and then citric acid in Example 8; but the liquid precipitated by adding acid first is blue-green, which may be due to the reaction of the added acid with iron hydroxide, resulting in the introduction of a small amount of Fe 3+ .
[0046] In Comparative Example 1, no citric acid and sodium hydroxide are added for coagulant aid, and a larger amount of PAM is required to effectively flocculate and obtain iron hydroxide precipitation, and Cu ions and alkaline earth metal ions cannot be separated from the iron hydroxide precipitation, resulting in more metal impurities in the recovered iron red, affecting its subsequent utilization. In Comparative Example 2, only citric acid is added without sodium hydroxide, and in Comparative Example 3, only sodium hydroxide is added without citric acid, both of which require a higher amount of PAM, and Cu ions and alkaline earth metal ions cannot be separated from the iron hydroxide precipitation. In Comparative Examples 4 and 5, acetic acid or sodium acetate is used instead of citric acid and sodium hydroxide as coagulants, which cannot achieve the coagulant effect, and iron hydroxide cannot be flocculated and precipitated at the same PAM dosage; Cu ions and alkaline earth metal ions cannot be separated from the iron hydroxide precipitation. In Comparative Example 6, too little citric acid is added, and the dissolution performance of Cu ions and alkaline earth metal ions is poor, and the recovered iron red obtained has more impurities. In Comparative Example 7, the pH of the blue solution A is adjusted too high, and the copper ions will be precipitated together with the alkaline earth metal ions, and the two cannot be separated, which affects the subsequent utilization of the recovered product.
[0047] Application Example 1: An application of recycled iron oxide obtained by the above method in the preparation of sintered permanent magnet ferrite powder comprises the following steps: adding the recycled iron oxide obtained in Example 1 into iron oxide with a purity of more than 99% at a ratio of 1% by mass, adding SrCO3 so that the molar ratio of Fe to Sr is 5.9 to obtain a mixture, and then subjecting the mixture to densification, balling, pre-calcination, crushing and pulverization to obtain sintered permanent magnet ferrite powder with an average particle size of 4.21 μm; the densification time is 1.0 h, the pre-calcination temperature is 1240°C, and the pre-calcination time is 90 min.
[0048] Application Example 2: The invention discloses an application of recycled iron oxide obtained by the above method in preparing sintered permanent magnet ferrite powder, comprising the following steps: adding the recycled iron oxide obtained in Example 1 into iron oxide with a purity of more than 99% at a ratio of 2% by mass, adding SrCO3 so that the molar ratio of Fe to Sr is 5.9 to obtain a mixture, and then subjecting the mixture to densification, balling, pre-calcination, crushing and pulverization to obtain sintered permanent magnet ferrite powder with an average particle size of 4.50 μm; the densification time is 1.0 h, the pre-calcination temperature is 1240°C, and the pre-calcination time is 90 min.
[0049] Comparative application example 1: A method for preparing sintered permanent magnet ferrite powder comprises the following steps: adding SrCO3 to iron red with a purity of more than 99% to make the molar ratio of Fe to Sr be 5.9 to obtain a mixture, and then subjecting the mixture to densification, balling, pre-sintering, crushing and pulverizing to obtain sintered permanent magnet ferrite powder with an average particle size of 4.43 μm; the densification time is 1.0 h, the pre-sintering temperature is 1240° C., and the pre-sintering time is 90 min.
[0050] Comparative application example 2: The recycled iron oxide obtained in Comparative Example 1 is added to iron oxide with a purity of more than 99% at a mass ratio of 1%, SrCO3 is added to make the molar ratio of Fe and Sr be 5.9, and a mixture is obtained. The mixture is then subjected to densification, balling, pre-calcination, crushing and pulverization to obtain sintered permanent magnet ferrite powder with an average particle size of 4.26μm; the densification time is 1.0h, the pre-calcination temperature is 1240℃, and the pre-calcination time is 90min.
[0051] Comparative application example 3: The recycled iron oxide obtained in Example 1 is added to iron oxide with a purity of more than 99% in a ratio of 3% by mass, SrCO3 is added to make the molar ratio of Fe and Sr be 5.9 to obtain a mixture, and then the mixture is subjected to densification, balling, pre-calcination, crushing and pulverization to obtain sintered permanent magnet ferrite powder with an average particle size of 4.34μm; the densification time is 1.0h, the pre-calcination temperature is 1240℃, and the pre-calcination time is 90min.
[0052] The performance of the sintered permanent magnet ferrite powder obtained in the corresponding application examples 1 to 2 and the comparative application examples 1 to 3 was tested, and the results are shown in Table 3. The test method is: 1.2wt% CaCO3, 0.15wt% HBO3 and 0.25wt% SiO2 were added to the sintered permanent magnet ferrite powder obtained in each application example and the comparative application example, and then the slurry was obtained by ball milling for 10 hours, and the average particle size of the slurry magnetic powder particles was 0.85μm. The slurry was pressed and formed under a magnetic field of 8000Oe, sintered at 1260℃ for 1.5h, and then the magnetic properties were tested in a magnetometer.
[0053] Table 3: Performance test results of sintered permanent ferrite. project Br(Gs) Hcb(Oe) Hcj(Oe) HBmax(MGOe) Application Example 1 4216 2856 2882 4.24 Application Example 2 4196 2906 2956 4.24 Comparative application example 1 4220 2911 2821 4.24 Comparative Application Example 2 3938 2929 3041 4.23 Comparative Application Example 3 4085 2976 3015 4.24
[0054] As can be seen from Table 3, the remanence Br of the sintered permanent magnet ferrite to which the recycled iron oxide obtained in Example 1 of the present invention is added in Application Examples 1 and Application Examples 2 is not much different from the permanent magnet ferrite in Comparative Application Example 1 without adding recycled iron oxide, and has the advantage of slightly higher Hcj. However, the Br of the permanent magnet ferrite made from the recycled iron oxide obtained in Comparative Example 1 in Comparative Application Example 2 is significantly lower than that in Comparative Application Example 1, which is caused by the presence of impurity elements. Although Comparative Application Example 2 has a higher Hcj, the requirements for Hcj in practical applications are not as strict as Br, so adding the recycled iron oxide obtained in Comparative Example 1 may cause the product to be unqualified. It can be seen from Comparative Application Example 3 that the addition of excessive recycled iron oxide obtained by the present invention will also cause a decrease in the remanence Br. In the product corresponding to this formula, the performance of Comparative Application Example 3 is already near the lower limit.
[0055] Application Example 3: The invention discloses an application of recycled iron oxide obtained by the above method in preparing bonded permanent magnet ferrite powder, comprising the following steps: adding the recycled iron oxide obtained in Example 1 into iron oxide with a purity of more than 98.5% at a ratio of 1% by mass, adding BaCO3 so that the molar ratio of Fe to Ba is 5.68 to obtain a mixture, and then subjecting the mixture to densification, balling, pre-calcination, crushing and pulverization to obtain bonded permanent magnet ferrite powder with an average particle size of 2.2 μm; the densification time is 1.0 h, the pre-calcination temperature is 1200° C., and the pre-calcination time is 90 min.
[0056] Application example 4: The invention discloses an application of recycled iron oxide obtained by the above method in preparing bonded permanent magnet ferrite powder, comprising the following steps: adding the recycled iron oxide obtained in Example 1 into iron oxide with a purity of more than 98.5% at a ratio of 2% by mass, adding BaCO3 so that the molar ratio of Fe to Ba is 5.68 to obtain a mixture, and then subjecting the mixture to densification, balling, pre-calcination, crushing and pulverization to obtain bonded permanent magnet ferrite powder with an average particle size of 2.15 μm; the densification time is 1.0 h, the pre-calcination temperature is 1200° C., and the pre-calcination time is 90 min.
[0057] Comparative application example 4: A method for preparing bonded permanent magnet ferrite powder comprises the following steps: adding BaCO3 to iron red with a purity of more than 98.5% to make the molar ratio of Fe to Ba be 5.68 to obtain a mixture, and then subjecting the mixture to densification, balling, pre-sintering, crushing and pulverizing to obtain bonded permanent magnet ferrite powder with an average particle size of 2.20 μm; the densification time is 1.0 h, the pre-sintering temperature is 1200° C., and the pre-sintering time is 90 min.
[0058] Comparative application example 5: The recycled iron oxide obtained in Comparative Example 1 is added to iron oxide with a purity of more than 98.5% at a mass ratio of 1%, and BaCO3 is added to make the molar ratio of Fe and Ba be 5.68 to obtain a mixture. The mixture is then subjected to densification, balling, pre-calcination, crushing and pulverization to obtain bonded permanent magnet ferrite powder with an average particle size of 2.19μm; the densification time is 1.0h, the pre-calcination temperature is 1200℃, and the pre-calcination time is 90min.
[0059] Comparative application example 6: The recycled iron oxide obtained in Example 1 is added to iron oxide with a purity of more than 98.5% in a ratio of 3% by mass, and BaCO3 is added so that the molar ratio of Fe and Ba is 5.68 to obtain a mixture. The mixture is then subjected to densification, balling, pre-calcination, crushing and pulverization to obtain bonded permanent magnet ferrite powder with an average particle size of 2.16μm; the densification time is 1.0h, the pre-calcination temperature is 1200℃, and the pre-calcination time is 90min.
[0060] The performance of the bonded permanent magnet ferrite powder obtained in Examples 3 to 4 and Comparative Application Examples 4 to 6 was tested, and the results are shown in Table 4. The test method is: take 20g of magnetic powder, add 1.5g of water, mix well, apply 30MPa pressure under a hydraulic press to press into a 20mm cylindrical magnetic block, and test the magnetic properties of the bonded magnet by a magnetometer.
[0061] Table 4: Bonded permanent ferrite performance test results. project Br(Gs) Hcb(Oe) Hcj(Oe) HBmax(MGOe) Application Example 3 1610 1501 2376 0.49 Application Example 4 1597 1569 2423 0.49 Comparative Application Example 4 1632 1456 2335 0.49 Comparative Application Example 5 1449 1586 2500 0.49 Comparative Application Example 6 1522 1623 2503 0.48
[0062] It can be seen from Table 4 that when the recycled iron oxide red recovered in the embodiments of the present invention and the comparative examples is used for preparing bonded permanent magnet ferrite, it follows a similar rule as when it is used for preparing sintered permanent magnet ferrite.
Claims
1. A method for treating wastewater from a magnetic powder factory and recovering resources, characterized in that: The steps include: (1) The wastewater is passed into a reaction sedimentation tank, aerated, and alkali solution is added to adjust the pH of the wastewater to neutral. After reaction sedimentation, the supernatant is discharged; (2) adding polycarboxylic acid and hydroxide to the bottom flocculent obtained by precipitation in step (1), and then adding a flocculant, stirring and further precipitating to obtain a blue solution A and a flocculent precipitate; filtering, drying, and crushing the obtained flocculent precipitate to obtain recovered iron red; (3) The pH of the blue solution A is adjusted to 9-10.5, a white precipitate is precipitated and a blue solution B is obtained; the white precipitate is filtered to obtain an alkaline earth metal salt; (4) The pH of the blue solution B is adjusted to 11-12 to obtain a blue flocculent precipitate. The remaining solution after filtration is discharged into the reaction sedimentation tank described in step (1) and mixed with the wastewater.
2. The method for treating wastewater and recovering resources from a magnetic powder factory according to claim 1, characterized in that: After the supernatant is discharged in step (1), the solid content of the bottom flocculent obtained is 3.5wt%~10wt%.
3. The method for treating wastewater and recovering resources from a magnetic powder factory according to claim 1, characterized in that: The polycarboxylic acid in step (2) is selected from one or more of citric acid, oxalic acid, malic acid, tartaric acid, and succinic acid; and the hydroxide is selected from one or both of sodium hydroxide and potassium hydroxide.
4. The method for treating wastewater from a magnetic powder factory and recovering resources according to claim 1 or 3, characterized in that: The mass ratio of the polycarboxylic acid to the hydroxide added in step (2) is 1.5-5:1; the concentration of the added polycarboxylic acid in the bottom flocculent is 0.1-4 g / L.
5. The method for treating wastewater from a magnetic powder factory and recovering resources according to claim 1 or 3, characterized in that: In step (2), the polycarboxylic acid and the hydroxide are added in the form of aqueous solution; when adding, the polycarboxylic acid and the hydroxide are first prepared into a mixed solution, and then added to the bottom flocculent material; Alternatively, the polycarboxylic acid solution is first added to the bottom floccules and then the hydroxide solution is added.
6. The method for treating wastewater and recovering resources from a magnetic powder factory according to claim 1, characterized in that: The flocculant in step (2) is PAM, and the concentration of the added flocculant in the bottom floc is 0.01-0.1 g / L.
7. An application of recycled iron oxide red obtained by the method according to any one of claims 1 to 6 in preparing bonded permanent ferrite magnetic powder, characterized in that: The following steps are involved: The recycled iron oxide is added into iron oxide with a purity of more than 98.5% at a mass ratio of 1% to 2%, and BaCO3 is added to make the molar ratio of Fe and Ba 5.5 to 5.8 to obtain a mixture. The mixture is then densified, pelletized, pre-sintered, crushed and pulverized to obtain bonded permanent magnet ferrite powder.
8. The use according to claim 7, characterized in that: The densification time is 0.5~1.5h; the pre-sintering temperature is 1180~1230℃, and the pre-sintering time is 60~120min; the average particle size of the obtained bonded permanent magnet ferrite powder is 2.0~2.3μm.
9. An application of recycled iron oxide red obtained by the method according to any one of claims 1 to 6 in preparing sintered permanent magnet ferrite powder, characterized in that: The following steps are involved: The recycled iron oxide is added into the iron oxide with a purity of more than 99% at a mass ratio of 1% to 2%, and then SrCO3 is added to make the molar ratio of Fe and Sr be 5.3 to 6.0 to obtain a mixture, and then the mixture is densified, pelletized, pre-sintered, crushed and pulverized to obtain sintered permanent magnet ferrite powder.
10. The use according to claim 9, characterized in that: The densification time is 0.5~1.5h; the pre-sintering temperature is 1240~1280℃, and the pre-sintering time is 60~120min; the average particle size of the sintered permanent magnet ferrite powder is 3~6μm.
Citation Information
Patent Citations
Method for separating rare earth, iron, copper, cobalt and tungsten from alloy
CN101186969A
Treatment method for electroless copper plating wastewater
CN110451688A
Method for comprehensively recovering valuable metals from neodymium iron boron waste acid leaching residues in sulfuric acid system
CN114875241A
Prepn of doped magnetic ferrite material
CN1486958A
Method for processing of technological waste from the processing of copper ore and concentrates containing iron
EP3260560A1