Ceramic glazed by turquoise and production process thereof

By using turquoise glazing technology and various glazing methods in ceramics, combined with high-temperature firing, the problems of low porcelain degree and excessive lead content in traditional glazed porcelain are solved, the strength and aesthetics of ceramics are improved, and the product's durability is ensured. Safety and reliability.

CN118724561AInactive Publication Date: 2024-10-01HUBEI WUDANG KILN TECH DEV CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411077784.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-07
Publication Date
2024-10-01
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The low-temperature firing of traditional glazed porcelain results in low porcelain degree, loose texture, easy breakage, and excessive lead content, which poses a health threat.

Method used

Using turquoise glazed ceramics and its production process, through the preparation of fine powder blanks, glazing and high-temperature firing, combined with glazes composed of turquoise, glaze ash, flower milkstone and other ingredients, various glazing methods such as spray glaze and dip glaze are used , and carry out temperature-controlled firing in slow fire, hot fire and rapid fire periods in the kiln.

Benefits of technology

It significantly improves the overall strength and porcelain degree of ceramics, prevents deglazing, reduces lead content, improves the durability and aesthetics of the product, meets health and environmental protection requirements, and broadens the application field.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118724561A_ABST
    Figure CN118724561A_ABST
Patent Text Reader

Abstract

The invention discloses ceramic glazed by turquoise and a production process of the ceramic. The production process comprises the following steps: step 1, preparing a blank; 2, blank making and forming; step 3, glazing; and step 4, firing. According to the ceramic glazed by turquoise and the production process thereof, various raw materials such as copper flowers, tin ash and turquoise are blended in glaze preparation, the unique aesthetic feeling and stability of a glaze surface are ensured, the porcelainization strength of the porcelain is remarkably enhanced through accurate control of multiple temperature levels and prolonged firing of a high-temperature stage, a glaze layer is finer and brighter, and the service life of the porcelain is prolonged. Meanwhile, a natural and smooth slicing effect is formed, the artistic ornamental value of the ceramic is improved, potential harmful substances are reduced by optimizing the process, and the problem of lead content possibly existing in traditional colored glaze ceramic is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of ceramic production, in particular to ceramics using turquoise glaze and a production process thereof. Background Art

[0002] Colored glaze porcelain, also known as Liuli, is a colorful and crystal clear artificial crystal that combines the warmth of ceramics with the splendor of colored glaze. Its production process has a long history and is one of my country's intangible cultural heritage. Colored glaze porcelain uses silicon dioxide as the main raw material, lead oxide as a combustion aid, and various metal oxides as colorants. It is made through high-temperature smelting and complex firing. The production process includes the selection, grinding, molding, glazing, bisque firing and color firing of raw materials. First, the selected clay raw materials are ground to enhance their plasticity. Subsequently, the clay is molded into various shapes of utensils through methods such as wheel making, hand kneading or mold molding. Next, a layer of colored glaze is applied to the surface of the vessel to increase its waterproof effect and aesthetics. Finally, after a high-temperature bisque firing and a low-temperature color firing, a bright and stable glaze color is formed on the surface of the vessel. The value of colored glaze porcelain is not only reflected in its exquisite production process, but also in its unique artistic charm and profound cultural connotation.

[0003] However, the firing temperature of traditional glazed porcelain is usually controlled at around 880 degrees, which belongs to the category of low-temperature firing. Low-temperature firing results in a low degree of vitrification of the ceramics and a relatively loose texture, which makes the pottery easy to break or the glaze fall off during use, affecting the durability and aesthetics of the ceramic products. At the same time, low-temperature firing is difficult to effectively degrade the lead content in the ceramics, and there is a risk of excessive lead content, posing a potential threat to the health of users. In this regard, we proposed a ceramic glazed with turquoise and a production process thereof. Summary of the invention

[0004] The purpose of the present invention is to provide a ceramic glazed with turquoise and a production process thereof, so as to solve the problems in the above-mentioned background technology that the ceramic production has a low degree of vitrification and there is a risk of excessive lead content, which poses a potential threat to the health of users.

[0005] To achieve the above object, the present invention provides the following technical solution: a ceramic glazed with turquoise and a production process thereof, comprising the following steps: Step 1: Prepare the blank In the first step, the soil and various ores used for making the blanks are put into a ball mill and ground into fine powder; The second step is to sieve and filter the ground powder into fine powder. The third step is to prepare the porcelain blank: the green pine colored glaze porcelain blank is made of fine white clay, fine clay, fine yellow slurry stone powder and fine quartz stone powder, with an acidity of 1.37 degrees, a shrinkage of 8.5% after firing, a moisture content of 26.8% when making the blank, a moisture content of 16.0% when repairing the blank, a shrinkage of 5.2% after drying, and a shrinkage of 8.49% after firing. The type of glaze is green pine colored glaze, and the glazing methods are spraying, dipping, coating, swinging and pouring. The firing temperature is 1150°C -1170°C; The fourth step is to put the prepared flour into the mud pressing equipment for repeated stirring, sedimentation, and squeezing out excess water to make green mud; The fifth step is to put the green mud into a vacuum mud refining device for extrusion and refine it into mud strips for standby use; Step 2: Blank forming The first step is blank making: according to the shape and function requirements, the blank shape of the ceramic is made through throwing, carving, bonding, modeling and coiling; The second step is to trim the blank: the blank is finely trimmed by knife trimming, foot digging and hoop trimming techniques to make it the final finished product; The third step is drying the blanks: place the formed blanks on the drying rack, in a drying room or shed that is not exposed to strong light, sun or rain, to allow them to dehydrate and dry naturally, and then place them in the sun to dry; The fourth step is the first bisque firing: the dried ceramic blank is fired without glazing to become a ceramic blank; Step 3: Glazing The first step is to select the raw materials for the glaze: turquoise, glaze ash, steatite, limestone, frit, silica, boric acid, copper flower, tin ash and saltpeter; Step 2: glaze preparation: the green pine colored glaze is selected from copper flower, tin ash, saltpeter, turquoise, frit, limestone powder, glaze ash, flower milk stone, silicon dioxide and boric acid, with an acidity of 1.97 and a shrinkage of 8.5% after firing. The type of glaze is green pine colored glaze, and the glazing methods are spraying, dipping, coating, swinging and pouring. The firing temperature is 1050°C-1070°C. Step 3, glaze processing: put the glaze powder obtained after the glaze preparation in step 3 into a ball mill, add water and ball mill for 48 hours, and filter through a 120-mesh screen; The fourth step is glazing: before glazing, the repaired blank is first glazed inside and then glazed outside. The glazing methods are divided into pouring glaze, swinging glaze, dipping glaze, blowing glaze and painting glaze; Step 5, Drying: After the glazing process is completed, the blank needs to be placed in the sun to dry naturally to enhance the adhesion of the glaze layer. Then, for the bottom of the blank and the area that does not need to be glazed, the glaze layer is accurately removed on the wheel throwing machine using a glaze repair knife. After the glazing process is completed, the blank can be safely sent to the kiln for high-temperature firing; Step 4: Firing The first step is to load the kiln: load from the back of the firing chamber to the front in sequence. Since the temperature of the firing chamber is inconsistent, in order to make the temperature uniform and the firing more consistent, when loading the kiln, the arrangement of the sagger columns in the front and back parts should be kept symmetrical, and a certain gap should be kept between the sagger columns and in the front, back, left and right. When loading the kiln, the bottom of the kiln is first covered with quartz grains about 20cm thick. At the bottom of each sagger, an empty sagger is buried in the quartz grains, and then the saggers filled with porcelain are piled on top; The second step is kiln firing: the kiln firing process is divided into three stages: slow firing, hot firing, and rapid firing; The third step is firing operation: after the electric kiln firing temperature and firing parameter settings are input, press the power start button to start firing. During the firing process, closely observe the parameter changes on the electric kiln screen to see if they are running normally. If any abnormality is found, check and troubleshoot immediately to ensure the normal operation of the firing parameters. Do not open the kiln immediately after the electric kiln firing operation is completed. Wait until the kiln cools down naturally and drops below 35 degrees before opening the kiln.

[0006] Preferably, in step one, the green pine glazed porcelain blank prepared in the third step has the following mixing ratio parameters based on the absolutely dry state: 40% finely washed white clay, 20% finely washed clay, 18% finely washed yellow slurry stone powder and 22% finely washed quartz stone powder.

[0007] Preferably, in step 2, the first biscuit firing in the fourth step is carried out by an electric kiln firing process.

[0008] Preferably, in step three, the processing method of the turquoise is to process it through hand selection, crushing, ball milling, screening and washing processes before glazing, the processing method of the glaze ash is to put the burned lime into water, cool it in water and naturally divide it into small pieces, and then stack these small pieces of lime alternately with ferns after they are completely dried, and then calcine them. The ash obtained after the calcination is the glaze ash, the processing method of the steatite is to crush the dolomite ore, wash it and set it aside, and the frit, silica, boric acid, copper flower, tin ash and saltpeter are all purchased as finished raw materials for preparation and use.

[0009] Preferably, in step three, the green pine glass glaze prepared by the second step glaze has the following proportions based on the absolute dry state: 4.05% copper flower, 3.20% tin ash, 6.04% saltpeter, 29.27% ​​turquoise, 11.47% frit, 8.27% limestone powder, 12.36% glaze ash, 11.40% steatite, 8.60% silicon dioxide and 5.34% boric acid.

[0010] Preferably, in step three, the method of pouring glaze in the fourth step of glaze processing is to set a wooden board on the glaze basin, place the ceramic body securely on the wooden board, and then use tools to evenly pour the glaze slurry on the surface of the ceramic body. For extra-large ceramics, it is recommended that two people work together to improve efficiency. After the first glazing, it is necessary to wait for the glaze layer to dry naturally, and then pour the glaze for the second time to ensure that the glaze layer is evenly covered and the thickness is consistent.

[0011] Preferably, in step three, the method of shaking the glaze in the fourth step of glaze processing is to use a spoon with a handle to accurately measure the glaze slurry, gently pour it into the interior of the ceramic body, and then slowly and evenly shake it to make the glaze slurry evenly spread and adhere to the inner wall of the ceramic body. After the glaze slurry is evenly distributed, pour out the excess glaze slurry.

[0012] Preferably, in step three, the glaze dipping method in the fourth step of glaze processing is to hold the ceramic body and completely immerse it in the glaze slurry to ensure uniform adhesion of the glaze slurry. After the first dipping, wait until it is semi-dry and then repeat this step to enhance the thickness and uniformity of the glaze layer.

[0013] Preferably, in step three, the glaze blowing processing method in the fourth step of glaze processing is to place the glaze slurry in a glaze spraying tool and spray it evenly on the surface of the ceramic body by air pressure to achieve uniform coverage of the glaze layer.

[0014] Preferably, in step three, the glaze coating method in the fourth step of glaze processing is to use a brush tool, dip an appropriate amount of glaze slurry, and finely apply it on the surface of the ceramic body. It is suitable for situations where the color and distribution of the glaze layer need to be precisely controlled.

[0015] Compared with the prior art, the present invention has the following beneficial effects: Turquoise, silicon dioxide and frit mineral glazes are added to the present invention. Due to its high melting point, turquoise can be stably integrated into the glaze layer during the firing process, thereby enhancing the bonding strength between the glaze surface and the body, thereby significantly improving the overall strength of the ceramic. This increase in strength not only makes the turquoise glazed porcelain more durable in daily use, but also broadens its application areas, and is particularly suitable for scenes that need to withstand greater mechanical stresses, such as art ornaments, architectural decorations, etc.

[0016] The present invention achieves a significant improvement in the degree of vitrification of the glaze surface through glaze formulation and innovative firing technology. During the firing process, the chemical components in the glaze undergo complex physical and chemical changes at high temperatures to form a dense and uniform glaze layer that is tightly combined with the body, effectively preventing the occurrence of deglazing. This optimization not only improves the aesthetics of the product, but also ensures its stability and reliability in long-term use.

[0017] The present invention successfully solves the problem of excessive lead content by introducing environmentally friendly raw materials and strictly controlling the lead content in the glaze. This not only meets the requirements of modern society for health and environmental protection, but also provides the possibility for the application of green pine colored glaze porcelain in a wider range of fields, such as home decoration, dining utensils, etc., providing consumers with a safer and healthier choice.

[0018] The present invention adopts various glazing methods such as spraying glaze, dipping glaze, coating glaze, swinging glaze, pouring glaze, etc., and can flexibly select the most suitable glazing method according to the different needs and designs of the products to ensure that the glaze layer is uniform and beautiful. At the same time, during the firing process, through precise temperature control technology, the temperature and firing time of each temperature step are strictly controlled to ensure the stable change of the glaze layer at high temperature, further improving the quality and consistency of the product. This diversified glazing method and precise temperature control technology are important innovations in the production process of Green Pine Colored Glaze Porcelain, and are also the key to its ability to stand out among many ceramic products. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic diagram of the overall process of the present invention; Figure 2 It is a schematic diagram of the process of blank forming of the present invention; Figure 3 It is a schematic diagram of the glazing process of the present invention; Figure 4 It is a schematic diagram of the sintering process of the present invention; Figure 5 A schematic diagram of a blank prepared for the porcelain blank of the present invention; Figure 6 A schematic diagram of a glaze formula prepared for the glaze of the present invention; Figure 7 It is a schematic diagram of the electric kiln temperature steps and firing parameters for the first biscuit firing of the present invention; Figure 8 It is a schematic diagram of specific temperature steps and firing parameters of the electric kiln during firing of the present invention. DETAILED DESCRIPTION

[0020] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0021] See also Figure 1-8 The present invention provides an embodiment: a ceramic glazed with turquoise and a production process thereof, comprising the following steps: Step 1: Prepare the blank In the first step, the soil and various ores used for making the blanks are put into a ball mill and ground into fine powder; The second step is to sieve and filter the ground powder into fine powder. The third step is to prepare the porcelain blank: the green pine colored glaze porcelain blank is made of fine white clay, fine clay, fine yellow slurry stone powder and fine quartz stone powder, with an acidity of 1.37 degrees, a shrinkage of 8.5% after firing, a moisture content of 26.8% when making the blank, a moisture content of 16.0% when repairing the blank, a shrinkage of 5.2% after drying, and a shrinkage of 8.49% after firing. The type of glaze is green pine colored glaze, and the glazing methods are spraying, dipping, coating, swinging and pouring. The firing temperature is 1150°C -1170°C; The fourth step is to put the prepared flour into the mud pressing equipment for repeated stirring, sedimentation, and squeezing out excess water to make green mud; The fifth step is to put the green mud into a vacuum mud refining device for extrusion and refine it into mud strips for standby use; Step 2: Blank forming The first step is blank making: according to the shape and function requirements, the blank shape of the ceramic is made through throwing, carving, bonding, modeling and coiling; The second step is to trim the blank: the blank is finely trimmed by knife trimming, foot digging and hoop trimming techniques to make it the final finished product; The third step is drying the blanks: place the formed blanks on the drying rack, in a drying room or shed that is not exposed to strong light, sun or rain, to allow them to dehydrate and dry naturally, and then place them in the sun to dry; The fourth step is the first bisque firing: the dried ceramic blank is fired without glazing to become a ceramic blank; Step 3: Glazing The first step is to select the raw materials for the glaze: turquoise, glaze ash, steatite, limestone, frit, silica, boric acid, copper flower, tin ash and saltpeter; Step 2: glaze preparation: the green pine colored glaze is selected from copper flower, tin ash, saltpeter, turquoise, frit, limestone powder, glaze ash, flower milk stone, silicon dioxide and boric acid, with an acidity of 1.97 and a shrinkage of 8.5% after firing. The type of glaze is green pine colored glaze, and the glazing methods are spraying, dipping, coating, swinging and pouring. The firing temperature is 1050°C-1070°C. Step 3, glaze processing: put the glaze powder obtained after the glaze preparation in step 3 into a ball mill, add water and ball mill for 48 hours, and filter through a 120-mesh screen; The fourth step is glazing: before glazing, the repaired blank is first glazed inside and then glazed outside. The glazing methods are divided into pouring glaze, swinging glaze, dipping glaze, blowing glaze and painting glaze; Step 5, Drying: After the glazing process is completed, the blank needs to be placed in the sun to dry naturally to enhance the adhesion of the glaze layer. Then, for the bottom of the blank and the area that does not need to be glazed, the glaze layer is accurately removed on the wheel throwing machine using a glaze repair knife. After the glazing process is completed, the blank can be safely sent to the kiln for high-temperature firing; Step 4: Firing The first step is to load the kiln: load from the back of the firing chamber to the front in sequence. Since the temperature of the firing chamber is inconsistent, in order to make the temperature uniform and the firing more consistent, when loading the kiln, the arrangement of the sagger columns in the front and back parts should be kept symmetrical, and a certain gap should be kept between the sagger columns and in the front, back, left and right. When loading the kiln, the bottom of the kiln is first covered with quartz grains about 20cm thick. At the bottom of each sagger, an empty sagger is buried in the quartz grains, and then the saggers filled with porcelain are piled on top; The second step is kiln firing: the kiln firing process is divided into three stages: slow firing, hot firing, and rapid firing; The third step is firing operation: after the electric kiln firing temperature and firing parameter settings are input, press the power start button to start firing. During the firing process, closely observe the parameter changes on the electric kiln screen to see if they are running normally. If any abnormality is found, check and troubleshoot immediately to ensure the normal operation of the firing parameters. Do not open the kiln immediately after the electric kiln firing operation is completed. Wait until the kiln cools down naturally and drops below 35 degrees before opening the kiln.

[0022] Further, in step 1, the green pine colored glaze porcelain blank prepared in the third step is prepared with the following proportion parameters based on the absolutely dry state: 40% fine white clay, 20% fine clay, 18% fine yellow slurry stone powder and 22% fine quartz stone powder. The blank type of the third step is as follows: the medium blank is taken as an example, see the attached Figure 5 The precise ratio of each raw material can give full play to their respective advantages and characteristics. The white clay provides a delicate texture, the clay enhances the plasticity of the body, the yellow slurry stone powder gives a natural change in color and texture, and the quartz stone powder improves the hardness and heat resistance of the body, together ensuring the high quality and unique beauty of the green pine glazed porcelain products.

[0023] Furthermore, in step two, the first bisque firing in the fourth step is carried out using an electric kiln firing process. The electric kiln can provide a stable and controllable firing environment, avoiding temperature fluctuations caused by uneven fuel combustion in traditional wood kilns or coal kilns, thereby ensuring the consistency of the bisque firing process and the uniform shrinkage of the ceramic body, laying a good foundation for subsequent glazing and final firing.

[0024] Furthermore, in step three, the processing method of turquoise is to process the turquoise by hand selection, crushing, ball milling, screening and washing before glazing; the processing method of glaze ash is to put the burned lime into water, cool it in water and naturally divide it into small pieces, and then stack them alternately with ferns after the small pieces of lime are completely dried, and then calcine them. The ash obtained after the calcination is the glaze ash; the processing method of steatite is to crush the dolomite ore, wash it and set it aside; the frit, silicon dioxide, boric acid, copper flower, tin ash and saltpeter are all purchased as finished raw materials for preparation and use; The stone is processed by hand selection, crushing and other processes to remove impurities and refine the particles, so that the mineral components in the turquoise can be better integrated into the glaze layer, giving the glaze a unique color and luster. In the preparation process of glaze ash, the alternating stacking and calcination of lime and fern promotes the full decomposition of lime and the ashification of fern, enhances the activity and adhesion of glaze ash, and makes the glaze layer more firm and lustrous. The direct use of finished raw materials such as frit and silica simplifies the production process, ensures the purity and stability of the raw materials, and is beneficial to the consistency and controllability of glaze performance.

[0025] Further, in step 3, the proportion of the green pine colored glaze prepared in the second step glaze in the absolutely dry state is: 4.05% copper flower, 3.20% tin ash, 6.04% saltpeter, 29.27% ​​turquoise, 11.47% frit, 8.27% limestone powder, 12.36% glaze ash, 11.40% steatite, 8.60% silicon dioxide and 5.34% boric acid. The glaze formula of the second step glaze is shown in the attached Figure 6 The addition of copper flowers and tin ash gives the glaze rich metallic luster and color changes, enhancing the artistic expression. The adjustment of saltpeter makes the glaze slurry more fluid and the glaze layer smoother and more delicate. Turquoise, as the core ingredient, not only adds color layers, but also gives the glaze layer a unique texture and texture. The frit, limestone powder and glaze ash together improve the hardness, wear resistance and adhesion of the glaze layer. The introduction of steatite further enriches the mineral composition of the glaze and enhances the overall beauty. The appropriate ratio of silica and boric acid ensures the stability and uniformity of the glaze at high temperatures.

[0026] Furthermore, in step three, the method of pouring glaze in the fourth step of glaze processing is to set a wooden board on the glaze basin, place the ceramic body securely on the wooden board, and then use tools to evenly pour the glaze slurry on the surface of the ceramic body. For extra-large ceramics, it is recommended that two people work together to improve efficiency. After the first glazing, it is necessary to wait for the glaze layer to dry naturally, and then pour the glaze for the second time to ensure that the glaze layer is evenly covered and the thickness is consistent. The glazing method ensures smooth and uniform glazing by setting a wooden board to stabilize the body, which is suitable for large and complex-shaped ceramic bodies.

[0027] Further, in step three, the glaze swinging method in the fourth step of glaze processing is to use a spoon with a handle to accurately measure the glaze slurry, gently pour it into the interior of the ceramic body, and then slowly and evenly shake it to make the glaze slurry evenly spread and adhere to the inner wall of the ceramic body. After the glaze slurry is evenly distributed, pour out the excess glaze slurry. The glaze swinging method makes the glaze slurry evenly spread on the inner wall of the body by shaking, which is suitable for hollow or deep cavity ceramics to ensure full coverage of the glaze layer.

[0028] Furthermore, in step three, the glaze dipping method in the fourth step of glaze processing is to hold the ceramic body and completely immerse it in the glaze slurry to ensure that the glaze slurry is evenly attached. After the first glazing, wait until it is semi-dry and then repeat this step to enhance the thickness and uniformity of the glaze layer. The glazing dipping method makes the glaze layer thicker and more uniform by completely immersing it in the glaze slurry, which is suitable for works that require a thick glaze layer.

[0029] Furthermore, in step three, the glaze blowing method in the fourth step of glaze processing is to place the glaze slurry in a glaze spraying tool, and spray it evenly on the surface of the ceramic body through air pressure to achieve uniform coverage of the glaze layer. The glaze blowing method uses air pressure to spray the glaze slurry, which is suitable for large areas or occasions that require rapid glazing, thereby improving production efficiency.

[0030] Furthermore, in step three, the glaze coating method in the fourth step of glaze processing is to use a brush tool, dip an appropriate amount of glaze slurry, and finely apply it on the surface of the ceramic body. It is suitable for situations where the color and distribution of the glaze layer need to be precisely controlled. The glazing method controls the color and distribution of the glaze layer by fine application, which is suitable for artistic ceramic creations that have extremely high requirements for glaze layer effects.

[0031] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and scope of the equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.

Claims

1. A ceramic glazed with turquoise and its production process, characterized in that: The following steps are involved: Step 1: Prepare the blank In the first step, the soil and various ores used for making the blanks are put into a ball mill and ground into fine powder; The second step is to sieve and filter the ground powder into fine powder. The third step is to prepare the porcelain blank: the green pine colored glaze porcelain blank is made of finely washed white clay, finely washed clay, finely washed yellow slurry stone powder and finely washed quartz stone powder; The fourth step is to put the prepared flour into the mud pressing equipment for repeated stirring, sedimentation, and squeezing out excess water to make green mud; The fifth step is to put the green mud into a vacuum mud refining device for extrusion and refine it into mud strips for standby use; Step 2: Blank forming The first step is blank making: according to the shape and function requirements, the blank shape of the ceramic is made through throwing, carving, bonding, modeling and coiling; The second step is to trim the blank: the blank is finely trimmed by knife trimming, foot digging and hoop trimming techniques to make it the final finished product; The third step is drying the blanks: place the formed blanks on the drying rack, in a drying room or shed that is not exposed to strong light, sun or rain, to allow them to dehydrate and dry naturally, and then place them in the sun to dry; The fourth step is the first bisque firing: the dried ceramic blank is fired without glazing to become a ceramic blank; Step 3: Glazing The first step is to select the raw materials for the glaze: turquoise, glaze ash, steatite, limestone, frit, silica, boric acid, copper flower, tin ash and saltpeter; The second step is to prepare the glaze: the green pine colored glaze is made of copper flower, tin ash, saltpeter, turquoise, frit, limestone powder, glaze ash, flower milk stone, silicon dioxide and boric acid; Step 3, glaze processing: put the glaze powder obtained after the glaze preparation in step 3 into a ball mill, add water and ball mill for 48 hours, and filter through a 120-mesh screen; The fourth step is glazing: before glazing, first apply glaze to the repaired blank, then glaze the outside; Step 5, Drying: After the glazing process is completed, the blank needs to be placed in the sun to dry naturally. Then, for the bottom of the blank and the area that does not need to be glazed, a glaze repair knife is used to accurately remove the glaze layer on the wheel throwing machine. After the glazing process is completed, the blank can be safely sent to the kiln for high-temperature firing; Step 4: Firing The first step is to load the kiln: load from the back of the firing chamber to the front in sequence. When loading the kiln, the arrangement of the sagger columns in the front and back parts should be kept symmetrical. There should be gaps between the sagger columns and in the front, back, left and right. When loading the kiln, first lay quartz grains about 20cm thick on the bottom of the kiln. At the bottom of each sagger, bury an empty sagger in the quartz grains, and then pile the saggers filled with porcelain on the top. The second step is kiln firing: the kiln firing process is divided into three stages: slow firing, hot firing, and rapid firing; The third step is firing operation: after the electric kiln firing temperature and firing parameter settings are entered, press the power start button to start firing. During the firing process, closely observe the parameter changes on the electric kiln screen to see if they are running normally. If any abnormality is found, check and troubleshoot immediately to ensure the normal operation of the firing parameters. After the electric kiln firing operation is completed, wait for the temperature to drop below 35 degrees before opening the kiln.

2. The ceramics with turquoise glaze and the production process thereof according to claim 1 are characterized in that: In step one, the green pine glazed porcelain blank prepared in the third step has the following mixing ratio parameters based on the absolutely dry state: 40% finely washed white clay, 20% finely washed clay, 18% finely washed yellow slurry stone powder and 22% finely washed quartz stone powder.

3. The ceramics with turquoise glaze and the production process thereof according to claim 1 are characterized in that: In step 2, the first biscuit firing in the fourth step is performed by an electric kiln firing process.

4. The ceramics with turquoise glaze and the production process thereof according to claim 1 are characterized in that: In step three, the processing method of the turquoise is to process it through hand selection, crushing, ball milling, screening and washing processes before glazing. The processing method of the glaze ash is to put the hot lime into water, cool it in water and naturally divide it into small pieces. After these small pieces of lime are completely dried, they are stacked alternately with ferns, and then calcined. The ash obtained after the calcination is glaze ash. The processing method of the steatite is to crush the dolomite ore, wash it and set it aside. The frit, silica, boric acid, copper flower, tin ash and saltpeter are all purchased finished raw materials for preparation and use.

5. The ceramics with turquoise glaze and the production process thereof according to claim 1 are characterized in that: In step three, the green pine glass glaze prepared in the second step of glaze has the following proportions based on the absolute dry state: 4.05% copper flower, 3.20% tin ash, 6.04% saltpeter, 29.27% ​​turquoise, 11.47% frit, 8.27% limestone powder, 12.36% glaze ash, 11.40% steatite, 8.60% silica and 5.34% boric acid.

6. The ceramics with turquoise glaze and the production process thereof according to claim 1 are characterized in that: In step three, the glazing methods of the fourth step of glazing processing are divided into pouring glaze, swinging glaze, dipping glaze, blowing glaze and coating glaze. The glazing is to set a wooden board on the glaze basin, place the ceramic body securely on the wooden board, and then use tools to evenly pour the glaze slurry on the surface of the ceramic body. After the first glazing, it is necessary to wait for the glaze layer to dry naturally before pouring the glaze for the second time.

7. The ceramics with turquoise glaze and the production process thereof according to claim 6 are characterized in that: The glaze shaking method is to measure the glaze slurry with a spoon with a handle, gently pour it into the interior of the ceramic body, and then slowly and evenly shake it to make the glaze slurry evenly spread and adhere to the inner wall of the ceramic body. After the glaze slurry is evenly distributed, pour out the excess glaze slurry.

8. The ceramics with turquoise glaze and the production process thereof according to claim 6 are characterized in that: The glazing step is to hold the ceramic body and completely immerse it in the glaze slurry to ensure that the glaze slurry is evenly attached. After the first glazing step, wait until it is semi-dry and then repeat this step.

9. The ceramics with turquoise glaze and the production process thereof according to claim 6, characterized in that: The glaze blowing is to place the glaze slurry in a glaze spraying tool and spray it evenly on the surface of the ceramic body through air pressure to achieve uniform coverage of the glaze layer.