Preparation method of sun-screening agent OMC
OMC is synthesized through a one-pot method, using a supported solid catalyst to catalyze the reaction of anisaldehyde, ketene and isooctyl alcohol, which solves the problems of complex and high energy consumption of the existing OMC synthesis process and achieves efficient and economical OMC preparation.
Patent Information
- Application Number
- CN202410912608.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-09
- Publication Date
- 2024-10-01
AI Technical Summary
The existing OMC synthesis process is complex in operation, consumes high energy in solvent use, produces large amounts of wastes, and has high overall production costs.
OMC is synthesized using a one-pot method, using single-atom metal catalysts such as Fe, Zn, Al, Ag, Ni and other supported solid catalysts, through the reaction of anisaldehyde, ketene and isooctyl alcohol, and controlling the reaction conditions at 20-100°C. The pressure is between 500-1200hPa, simplifying the process and performing simple distillation and purification.
Efficient synthesis of OMC is achieved, the process flow is simplified, the yield is improved, and the production cost is reduced.
Smart Images

Figure CN118724720A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of organic synthesis, and in particular relates to a method for preparing a sunscreen agent OMC. Background Art
[0002] Ultraviolet rays are always present in the atmosphere, and their harmful effects on the human body are receiving increasing attention. Currently, 2-ethylhexyl methoxycinnamate (OMC) is the most widely used sunscreen product. It boasts high absorption, is non-irritating to the skin, and is safe. It effectively absorbs ultraviolet rays from sunlight, preventing skin from becoming red, burnt, or tanned. It is also a treatment for photodermatitis.
[0003] At present, there are many methods for the synthesis of isooctyl p-methoxycinnamate OMC at home and abroad, which can be divided into the following four methods according to the main raw materials: p-methoxystyrene method, p-methoxyaniline method, p-methoxyhalobenzene method and p-methoxybenzaldehyde method.
[0004] However, current methods generally have problems such as cumbersome operation, large amounts of wastewater generation, low yield, and high overall production costs. To address the various deficiencies of the above processes, this patent provides an economical synthesis process for isooctyl p-methoxycinnamate that is different from previous literature reports. Summary of the Invention
[0005] The purpose of the present invention is to provide an efficient and economically beneficial OMC preparation method to address the problems in the prior art such as complex synthesis process operation, high energy consumption in solvent application, and large amount of three wastes generated.
[0006] In order to achieve the above-mentioned object of the invention, the technical solution of the present invention is as follows:
[0007] A method for synthesizing isooctyl p-methoxycinnamate is prepared by a one-pot process according to the following reaction scheme:
[0008]
[0009] The synthesis method of the invention comprises: in the presence of a single-atom metal catalyst, anisaldehyde, ketene and isooctyl alcohol are synthesized in one pot to form isooctyl p-methoxycinnamate OMC.
[0010] In the synthesis method of the present invention, the amount of ketene added to the system is 0.8 eq.-1.5 eq. of the amount of anisaldehyde used, preferably 1.0 eq.-1.1 eq.
[0011] In the synthesis method of the present invention, the amount of isooctyl alcohol added to the system is 0.8 eq.-1.5 eq. of the amount of anisaldehyde used, preferably 1.0 eq.-1.1 eq.
[0012] In the synthesis method of the present invention, the single-atom catalyst in the reaction is a supported solid catalyst composed of at least one of active metals Fe, Zn, Al, Ag, Ni, and Pd and a metal-organic framework material, wherein the metal-organic framework material is at least one of MOF-5, HKUST-1, ZIF-67, and ZIF-8; the active metal loading is 1-10 wt%, preferably 2-5 wt%, calculated as the weight of the metal element;
[0013] The amount of the catalyst used is 1 to 5 wt.% of the amount of anisaldehyde used, preferably 1 to 2.5 wt.%.
[0014] The synthesis method of the present invention has the following reaction conditions: a temperature range of 20-100° C., preferably 20-50° C., and a reaction pressure range of 500-1200 hPa, preferably 600-1000 hPa.
[0015] According to the synthesis method of the present invention, after the reaction is completed, simple filtration is directly performed to realize the application of the catalyst, and simple distillation and purification are performed to obtain the target product, isooctyl p-methoxycinnamate OMC.
[0016] The beneficial effects of the present invention are:
[0017] The invention adopts a one-pot method to synthesize isooctyl p-methoxycinnamate, has a simple synthesis process, and can maintain a relatively high yield. DETAILED DESCRIPTION
[0018] In order to further illustrate the present invention in detail, several specific implementation cases are given below, but the present invention is not limited to these embodiments.
[0019] Example 1
[0020] (1) Preparation of hydrated catalyst: Weigh 20.8g of zinc chloride and 100g of MOF-5, add 150mL of 10% dilute hydrochloric acid solution as solvent, stir at room temperature for 2 hours, filter out the solvent, activate and dry at 50℃ to obtain a solid catalyst with a Zn loading of 10%. Weigh 10.0g of the prepared solid catalyst and place it in a tube furnace. Heat it to 700℃ in an argon atmosphere for high-temperature carbonization for 3h at a heating rate of 5℃ / min. Then cool it naturally to room temperature and take out the obtained black carbide. Add the black carbide to 150mL of 2.5mol / L hydrofluoric acid and stir and etch it for 3h. Then centrifuge and wash it with water twice. Place the product in a vacuum drying oven and dry it at 100℃ to obtain a Zn single atom catalyst.
[0021] In a glove box, a Zn single-atom catalyst (1.36 g, 1%) and anisaldehyde (136.15 g, 1.0 mol) were added to a 1L autoclave. Stirring was started at room temperature (25°C), the speed was controlled at 400 rpm, and a diaphragm pump was started to maintain the pressure in the autoclave at 800 hPa. Finally, the ketene feed valve was opened to allow ketene (42.88 g, 1.02 mol) to slowly enter the autoclave over a 0.5 hour period. The ketene feed and diaphragm pump were then turned off. Isooctyl alcohol (136.74 g, 1.05 mol) was added to the autoclave using a horizontal flow pump for 0.5 hour. The reaction was stirred and reacted for 2 hours. The reaction liquid was sampled through a bottom tube in the autoclave and analyzed by GC, confirming complete conversion of the anisaldehyde. The catalyst was filtered out and purified by distillation to obtain 277.61 g of pure isooctyl p-methoxycinnamate (OMC) in a 95.6% yield.
[0022] NMR data of 2-ethylhexyl methoxycinnamate OMC:
[0023] 1 HNMR (400MHz, CDCl3): δ7.62 (d, J=6.2Hz, 2H), 7.48 (d, J=16.0Hz, 1H), 6.96 (d, J=6.2Hz, 2H), 6.31 (d, J=16.0Hz, 1H), 4.54 (dd, J=13.2 Hz, 7.6Hz, 1H), 4.25 (dd, J=13.2Hz, 7.6Hz, 1H), 3.83 (s, 3H), 2.07 (tq, J=7.6Hz, 6.8Hz, 1H), 1.22-1.50 (m, 8H), 0.90 (t, J=7.2Hz, 6H). 13 CNMR (100MHz, CDCl3): δ166.5,159.8,145.1,130.2,127.3,116.2,114.2,67.0 55.8,39.7,30.8,29.3,23.7,23.0,14.1,11.6.
[0024] Example 2
[0025] (1) Preparation of hydrated catalyst: Weigh 14.52 g of ferric chloride and 100 g of ZIF-67, use 150 mL of 10% dilute hydrochloric acid solution as solvent, stir at room temperature for 2 hours, filter out the solvent, activate and dry at 50°C to obtain a solid catalyst with an iron loading of 5%. Weigh 10.0 g of the prepared solid catalyst and place it in a tube furnace. Heat it to 700°C in an argon atmosphere for high-temperature carbonization for 3 hours at a heating rate of 5°C / min. Then cool it naturally to room temperature and take out to obtain a black carbide. Add the black carbide to 150 mL of 2.5 mol / L hydrofluoric acid and stir and etch it for 3 hours. Then centrifuge and wash it with water twice. Place the product in a vacuum drying oven and dry it at 100°C to obtain an Fe single-atom catalyst.
[0026] In a glove box, a single-atom Fe catalyst (3.40 g, 2.5%) and anisaldehyde (136.15 g, 1.0 mol) were added to a 1L autoclave at 50°C with stirring at 400 rpm. A diaphragm pump was used to maintain the pressure in the autoclave at 700 hPa. Finally, the ketene feed valve was opened to allow ketene (44.14 g, 1.05 mol) to slowly enter the autoclave over a 0.5 hour period. The ketene feed and diaphragm pump were then turned off. Isooctyl alcohol (143.25 g, 1.10 mol) was then added to the autoclave using a horizontal flow pump for 0.5 hour. The reaction was stirred and continued for 2 hours. The reaction solution was sampled through a bottom tube in the autoclave and analyzed by GC, confirming complete conversion of the anisaldehyde. The catalyst was filtered out and purified by distillation to obtain 282.26 g of pure isooctyl p-methoxycinnamate (OMC) in a 97.2% yield.
[0027] Example 3
[0028] (1) Preparation of hydrated catalyst: Weigh 2.15 g of silver oxide, 100 g of ZIF-67, and 150 mL of 10% dilute hydrochloric acid solution as solvent, stir at room temperature for 2 hours, filter out the solvent, activate and dry at 50°C to obtain a solid catalyst with a silver loading of 2%. Weigh 10.0 g of the prepared solid catalyst and place it in a tube furnace. Heat it to 700°C in an argon atmosphere for high-temperature carbonization for 3 hours at a heating rate of 5°C / min. Then cool it naturally to room temperature and take out to obtain a black carbide. Add the black carbide to 150 mL of 2.5 mol / L hydrofluoric acid and stir and etch it for 3 hours. Then centrifuge and wash it with water twice. Place the product in a vacuum drying oven and dry it at 100°C to obtain a Ag single-atom catalyst.
[0029] In a glove box, Ag single-atom catalyst (2.04 g, 1.5%) and anisaldehyde (136.15 g, 1.0 mol) were added to a 1L autoclave at 40°C with stirring at 400 rpm. A diaphragm pump was operated to maintain the autoclave pressure at 900 hPa. Finally, the ketene feed valve was opened to allow ketene (46.24 g, 1.10 mol) to slowly enter the autoclave over a 0.5 hour period. The ketene feed and diaphragm pump were then turned off. Isooctyl alcohol (143.25 g, 1.10 mol) was then added to the autoclave using a horizontal flow pump for 0.5 hour. The reaction was stirred and continued for 2 hours. The reaction liquid was sampled through a bottom tube in the autoclave and analyzed by GC, confirming complete conversion of the anisaldehyde. The catalyst was filtered out and purified by distillation to obtain 285.16 g of pure isooctyl p-methoxycinnamate (OMC) in a 98.2% yield.
Claims
1. A method for synthesizing isooctyl p-methoxycinnamate, characterized in that: The method comprises: in the presence of a single-atom metal catalyst, anisaldehyde, ketene and isooctyl alcohol are used to synthesize isooctyl p-methoxycinnamate in a one-pot method.
2. The synthesis method according to claim 1, characterized in that: The amount of ketene added to the system is 0.8 eq.-1.5 eq. of anisaldehyde, preferably 1.0 eq. eq.-1.1 eq.
3. The synthesis method according to claim 1, characterized in that: The amount of isooctyl alcohol added to the system is 0.8 eq.-1.5 eq. of the amount of anisaldehyde used, preferably 1.0 eq. eq.-1.1 eq.
4. The synthesis method according to claim 1, characterized in that: The single-atom metal catalyst is a supported solid catalyst composed of at least one of active metals Fe, Zn, Al, Ag, Ni, and Pd and a metal organic framework material, wherein the metal organic framework material is at least one of MOF-5, HKUST-1, ZIF-67, and ZIF-8.
5. The synthesis method according to claim 4, characterized in that: The loading amount of the active metal is 1-10 wt %, preferably 2-5 wt %, based on the mass of the metal element.
6. The synthesis method according to claim 1, 4 or 5, characterized in that: The amount of the catalyst used is 1 to 5 wt.% of the amount of anisaldehyde used, preferably 1 to 2.5 wt.%.
7. The synthesis method according to any one of claims 1 to 6, characterized in that: The reaction temperature is 20-100°C, preferably 20-50°C.
8. The synthesis method according to any one of claims 1 to 7, characterized in that: The reaction pressure is 500-1200 hPa, preferably 600-1000 hPa.