Bi-component silane modified polyether sealant and preparation method thereof
Through the two-component silane-modified polyether sealant process, ultra-low moisture content reinforcing fillers and a small amount of water removal agent are used to simplify moisture control and solve the problems of long production cycle and difficult moisture content control of silane-modified polyether sealant. problem, achieving efficient moisture management and improved sealing performance.
Patent Information
- Application Number
- CN202410845374.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-27
- Publication Date
- 2024-10-01
AI Technical Summary
It is difficult to control the moisture content of existing silane-modified polyether sealants during production, storage and transportation, which results in long production cycles, high energy consumption, large carbon emissions, and is unfavorable to highly reactive resins, affecting the long-term stable storage and deep curing of the sealant. speed.
Using a two-component silane-modified polyether sealant process, the process is simplified through the combination of ultra-low moisture content reinforcing filler and a small amount of water removal agent, avoiding vacuum high-temperature dehydration, and using stirring and dispersion at room temperature to achieve effective moisture content Control to ensure long-term stable storage and fast deep curing of the sealant.
It shortens the production cycle, improves production efficiency, reduces energy consumption and carbon emissions, maintains the good adhesion and waterproof sealing effect of the sealant, and reduces the release of odor and VOC.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure SMS_3