Energy-saving synergist as well as preparation method and application thereof
By using energy-saving synergists prepared from raw materials such as copper nitrate, the boiler combustion efficiency is improved and pollutant emissions are reduced, which solves the problems of short residence time and large pollutant emissions of existing combustion-supporting materials, and improves boiler operation stability and efficiency. .
Patent Information
- Application Number
- CN202410714016.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-04
- Publication Date
- 2024-10-01
AI Technical Summary
Existing boiler combustion-supporting materials cannot stay in the furnace for a long time to participate in the reaction, resulting in low combustion efficiency, increased tail pollutants, shortened catalyst life, high risk of tube explosion, and cannot effectively reduce the generation of nitrogen oxides and sulfides.
It uses energy-saving synergists prepared from raw materials such as copper nitrate, potassium nitrate, sodium nitrate, silicon dioxide, sodium carbonate, ferric oxide and kaolin. Through the redox cycle of metal additives under heating conditions, it absorbs oxygen and prolongs the metal life. and the residence time of oxides, reducing the emissions of sulfur dioxide and nitrogen oxides, and inhibiting boiler coking.
It has improved the thermal efficiency of the boiler, reduced sulfur dioxide and nitrogen oxide emissions, extended the boiler operation interval, and reduced the labor intensity of maintenance. The slag is loose and brittle, and the failure rate of the slag discharge system has been significantly reduced.
Smart Images

Figure CN118725932A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chemical additives, and in particular to an energy-saving synergist and a preparation method and application thereof. Background Art
[0002] At present, for the energy-saving and decoking technology of boiler combustion, most of the existing market is to add acidic combustion-supporting materials into the furnace and spray them on the surface to achieve the combustion-supporting effect. However, since this kind of combustion-supporting material cannot be retained in the furnace to participate in long-term reaction, the amount added is large and needs to be added evenly. The addition ratio is as high as more than 5 / 10,000, and as high as 3 / 1000. The labor intensity of workers is high, the energy-saving and emission-reduction effect is not obvious, and the short-term decoking effect is poor. This kind of combustion-supporting material is basically composed of acidic objects and chlorides. Although it has a certain combustion-supporting effect in a short period of time, it cannot effectively solve the combustion problem for a long time, which will lead to the aggravation of the reducing atmosphere in the furnace, the increase of the generation of ammonium bisulfate at the tail, the reduction of the catalyst life, the aggravation trend of coking after long-term use, and the increase of the probability of pipe explosion. In addition, since this kind of product itself cannot release oxygen, it can only achieve the purpose of combustion-supporting unless it is added continuously, but it cannot reduce the generation of nitrogen oxides and the reduction of sulfides. Summary of the invention
[0003] The purpose of the present invention is to provide an energy-saving synergist and a preparation method and application thereof, so as to overcome the defects in the prior art.
[0004] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions:
[0005] The present invention provides an energy-saving synergist, which is prepared from raw materials containing the following parts by weight:
[0006] 0.5-2 parts of copper nitrate, 1.5-4.5 parts of potassium nitrate, 5-10 parts of sodium nitrate, 1-5 parts of silicon dioxide, 20-30 parts of sodium carbonate, 0.5-2 parts of ferric oxide, 55-65 parts of kaolin, and 0.5-2 parts of water.
[0007] The present invention provides a method for preparing the energy-saving synergist, comprising the following steps:
[0008] The energy-saving synergist is obtained by mixing the raw materials in proportion.
[0009] Preferably, the mixing rate is 150-200 r / min;
[0010] The mixing time is 20 to 30 minutes.
[0011] The invention also provides application of the energy-saving synergist in boiler combustion.
[0012] Beneficial effects:
[0013] 1. The present invention provides an energy-saving synergist, which is prepared from the following raw materials in parts by weight: 0.5-2 parts of copper nitrate, 1.5-4.5 parts of potassium nitrate, 5-10 parts of sodium nitrate, 1-5 parts of silicon dioxide, 20-30 parts of sodium carbonate, 0.5-2 parts of ferric oxide, 55-65 parts of kaolin, and 0.5-2 parts of water. During the research and development of this application, full consideration was given to the pain points that need to be solved in current boilers. Alkaline substances are used to prepare the energy-saving synergist. Under heating conditions, metal additives are reduced to metals and then absorb oxygen to become oxides. Carbon is also reduced to metal oxides due to heating. In this way, the metal is always in a redox cycle, switching back and forth between the metal and oxide states to achieve a long-term retention effect.
[0014] 2. The energy-saving synergist provided by the present invention has unique sulfur dioxide emission reduction technology, nitrogen oxide reduction technology and unique decoking and coking suppression technology to prevent boiler coking.
[0015] 3. The preparation method and addition method of the energy-saving synergist provided by the present invention are simple. It can be added from the raw coal bin at a one-time amount of less than 1.5 ten-thousandth of the amount of coal entering the furnace in eight hours. After use, the sulfur dioxide and nitrogen oxides at the furnace outlet can be reduced by more than 10%, the furnace efficiency is increased and the coal-saving effect is reflected, the slag is loose and fragile, the failure rate of the slag discharge system is effectively reduced, and the labor intensity of maintenance personnel is reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 This is a graph showing changes in the #1 boiler load and exhaust gas temperature after the energy-saving synergist of Example 1 is used;
[0017] Figure 2 This is a graph showing the change in the amount of coal fed to boiler #1 after the energy-saving synergist of Example 1 is used;
[0018] Figure 3 This is a diagram showing the coking condition at the bottom of the screen after the energy-saving synergist of Example 1 is used;
[0019] Figure 4 This is a diagram showing the coking condition of the windward surface after the energy-saving synergist of Example 1 is used;
[0020] Figure 5 This is a diagram showing the coking condition of the burner port after the energy-saving synergist of Example 1 is used;
[0021] Figure 6 This is a diagram of the nitrogen oxide and sulfur emissions of boiler #31 after the energy-saving synergist of Example 2 is used;
[0022] Figure 7 This is a diagram showing the change in the desuperheating water flow rate of the #31 boiler reheater after the energy-saving synergist of Example 2 is used;
[0023] Figure 8 This is a diagram of sulfur emission of boiler #32 after using the energy-saving synergist of Example 3;
[0024] Fig. 9 This is a diagram showing the change in the desuperheating water flow rate of the #32 boiler reheater after the energy-saving synergist of Example 3 is used. DETAILED DESCRIPTION
[0025] The present invention provides an energy-saving synergist, which is prepared from raw materials containing the following parts by weight:
[0026] 0.5-2 parts of copper nitrate, 1.5-4.5 parts of potassium nitrate, 5-10 parts of sodium nitrate, 1-5 parts of silicon dioxide, 20-30 parts of sodium carbonate, 0.5-2 parts of ferric oxide, 55-65 parts of kaolin, and 0.5-2 parts of water.
[0027] In the present invention, the mass fraction of the copper nitrate is preferably 0.7 to 1.8 parts, more preferably 0.9 to 1.6 parts, and even more preferably 1 to 1.5 parts.
[0028] In the present invention, the mass fraction of potassium nitrate is preferably 1.8 to 4.2 parts, more preferably 2.1 to 3.9 parts, and even more preferably 2.5 to 3.5 parts.
[0029] In the present invention, the mass fraction of the sodium nitrate is preferably 6 to 9 parts, more preferably 6.5 to 8.5 parts, and even more preferably 7 to 8 parts.
[0030] In the present invention, the mass fraction of the silicon dioxide is preferably 1.5 to 4.5 parts, more preferably 2 to 4 parts, and even more preferably 2.5 to 3.5 parts.
[0031] In the present invention, the mass fraction of the sodium carbonate is preferably 22 to 28 parts, more preferably 23 to 27 parts, and even more preferably 24 to 26 parts.
[0032] In the present invention, the mass fraction of the ferric oxide is preferably 0.7 to 1.8 parts, more preferably 0.9 to 1.6 parts, and even more preferably 1 to 1.5 parts.
[0033] In the present invention, the mass fraction of the kaolin is preferably 57 to 63 parts, more preferably 58 to 62 parts, and even more preferably 59 to 61 parts.
[0034] In the present invention, the mass fraction of water is preferably 0.7 to 1.8 parts, more preferably 0.9 to 1.6 parts, and even more preferably 1 to 1.5 parts.
[0035] The present invention also provides a method for preparing the energy-saving synergist, comprising the following steps:
[0036] The energy-saving synergist is obtained by mixing the raw materials in proportion.
[0037] In the present invention, copper nitrate is first diluted with water into a liquid state and then mixed with other raw materials to obtain the energy-saving synergist.
[0038] In the present invention, the mixing rate is preferably 150 to 200 r / min, more preferably 160 to 190 r / min, and further preferably 170 to 180 r / min.
[0039] In the present invention, the mixing time is preferably 20 to 30 minutes, more preferably 22 to 28 minutes, and even more preferably 24 to 26 minutes.
[0040] The invention also provides application of the energy-saving synergist in boiler combustion.
[0041] In the present invention, the energy-saving synergist of the present invention is added once according to the ratio of less than 1.5 ten-thousandth of the mass of the raw coal entering the furnace every 6 to 8 hours. After entering the furnace, it starts to melt at 500°C and starts to gasify at 750°C. After gasification, the metal atoms in the product start oxidation-reduction reaction and release oxygen autonomously. At the same time, they preferentially carry out oxidation-reduction reaction with the metal atoms in the fuel. Within a certain period of time (about eight hours), new oxygen will be continuously generated, thus achieving the purpose of high-temperature retention; the increase in oxygen in the low-nitrogen area will make the fuel more flammable and the ignition point advanced. Due to the oxidation-reduction reaction of the metal atoms in the furnace, the generation of thermal nitrogen and instantaneous nitrogen is reduced, and the increase in oxygen occupies the excess air, which reduces the nitrogen oxides in the furnace; due to easier combustion, the generation of sulfides becomes less, and some sulfides will combine with some components in the energy-saving enhancer to generate new substances that are adsorbed on the slag, so that the sulfur dioxide content in the flue gas in the furnace is reduced, and the purpose of reducing sulfur dioxide emissions is achieved; with the improvement of combustion conditions, the components in the fuel that are prone to coking are reduced, which effectively slows down the coking speed and achieves the purpose of slowing down the coking speed; the slag-improving components in the energy-saving enhancer will effectively penetrate into the coke layer that has been formed, and the special metal oxides will cause the coke layer lattice to become larger and empty, and the abnormally developed needle-shaped dendrite ions will preferentially combine with the sulfides in the coke layer, so that the coke layer is modified to be loose and fall off with an irregular dendrite arrangement.
[0042] The technical solutions provided by the present invention are described in detail below in conjunction with the embodiments, but they should not be construed as limiting the protection scope of the present invention.
[0043] The kaolin in the following examples was selected from Lingshou County Xingyuan Mineral Powder Processing Plant.
[0044] Example 1
[0045] After 0.5 tons of copper nitrate is diluted into liquid with 0.5 tons of water, 1.5 tons of potassium nitrate, 5 tons of sodium nitrate, 1 ton of silicon dioxide, 20 tons of sodium carbonate, 0.5 tons of ferric oxide and 55 tons of kaolin are added and mixed at a speed of 150r / min for 20 minutes to obtain an energy-saving synergist.
[0046] Effect test:
[0047] According to the operating conditions of six high-pressure pulverized coal boilers in a power workshop of a company in Ningxia, combined with the boiler maintenance plan, boiler #1 was selected. The energy-saving synergist obtained in this embodiment was poured into the agent storage box at 01:00, 09:00 and 17:00 every day. The outlet valve of the agent box was opened during the coal loading of the coal bunker of boiler #1, and the agent was evenly added to each operating coal bunker. The trial process was divided into three stages. In the first stage (8 days), 5 bags (25 kg per bag) were added to each batch of coal. In the second stage (8 days), 4 bags were added to each batch of coal. In the third stage (9 days), 3 bags were added to each batch of coal. Data were recorded during the period to observe the coking amount and coking state at the burner mouth and the furnace bottom.
[0048] (1) After adding energy-saving enhancer, the changes of boiler load and exhaust gas temperature of #1 are shown in Table 1 and Figure 1 shown.
[0049] Table 1 Changes in boiler load and exhaust gas temperature of #1
[0050] project Before use After use Change value Boiler load (t / h) 420~430 430~440 10 Exhaust temperature1(℃) 174 161 13 Exhaust temperature 2(℃) 144 128 16
[0051] From Table 1 and Figure 1 It can be seen that after adding the energy-saving synergist of this embodiment, the original soot blowing frequency remains unchanged, the boiler load increases by 10t / h, the energy-saving synergist acts on the heating surface of the boiler, the coking situation of the heating surface in the furnace shows a trend of easing, the amount of coke dropped from the bottom of the furnace is more than that of other operating furnaces, the water-cooled wall absorbs more heat, and the exhaust temperature decreases by 13-16°C. Taking the average of exhaust temperature 1 and exhaust temperature 2, the average exhaust temperature of the boiler before using the energy-saving synergist is 159°C, and the corresponding boiler efficiency is calculated to be 90.75%; after using the energy-saving synergist, the exhaust temperature drops to 144.5°C, and the corresponding boiler efficiency is calculated to be 91.48%, and the boiler thermal efficiency is increased by 0.73%.
[0052] (2) After adding energy-saving synergist, the change of coal feed of boiler #1 is shown in Table 2 and Figure 2 shown.
[0053] Table 2 Changes in coal supply to boiler #1
[0054] project Before use After use Boiler load (t / h) 358~453 378~460 Coal feeding amount (t / h) 56.5 55.9 Fuel coal consumption (t / ton steam) 0.136 0.132
[0055] From Table 2 and Figure 2It can be seen that after using the energy-saving synergist obtained in this embodiment, the amount of coal fed to the boiler under the same load is reduced by 0.6 t / h compared with before use, and the unit consumption of fuel coal is reduced by 0.004 t / ton of steam, which corresponds to the improvement of the boiler's heat absorption efficiency after the exhaust gas temperature is reduced. It can be seen that the energy-saving synergist of this application has certain effects in saving coal.
[0056] (3) After adding the energy-saving enhancer and after the shutdown of furnace #1, the coking condition at the bottom of the screen is as follows Figure 3 shown.
[0057] from Figure 3 It can be seen that there is coking at the bottom of the screens. There are a total of 14 screens, and there are two bridging cokings between screens 7-8 and 8-9. The bridging coking amount at the bottom of the screens is less than 30%. There is coking to varying degrees at the bottom of the remaining screens, but no bridging phenomenon has formed. The traces of reagent penetration can be clearly seen in the coking cross-section layer. The on-site inspection shows that the coking is loose and easy to clean, and there is no black hard hanging coke.
[0058] After adding energy-saving enhancer, and after the No. 1 furnace is shut down, the coking situation above the windward side is as follows: Figure 4 shown.
[0059] from Figure 4 It can be seen that the coke above the windward side is in the shape of pine needles, and traces of reagent penetration can be clearly seen in the coke cross-section layer. The pine needle-shaped coke on the surface is easy to clean, and the original coke at the contact surface between the root and the pipe wall is relatively hard.
[0060] After adding the energy-saving synergist, and after the #1 furnace was shut down, the coking condition at the burner port was as follows: Figure 5 shown.
[0061] from Figure 5 It can be seen that there is a small amount of coking at the burner port, and there is no large piece of coking at the burner port at each corner. The overall coking situation is better than that of other operating furnaces.
[0062] Example 2
[0063] After 2 tons of copper nitrate is diluted into liquid with 2 tons of water, 4.5 tons of potassium nitrate, 10 tons of sodium nitrate, 5 tons of silicon dioxide, 30 tons of sodium carbonate, 2 tons of ferric oxide and 65 tons of kaolin are added and mixed at a speed of 200 r / min for 30 minutes to obtain an energy-saving synergist.
[0064] Effect test:
[0065] According to the boiler operating conditions of a workshop of a company in Sichuan, combined with the boiler maintenance plan, boiler #31 was selected, and the energy-saving synergist obtained in this embodiment was poured into the coal mill inlet at 07:00, 15:00, and 23:00 every day. During this period, data was recorded and the coking amount and coking state at the burner port and the furnace bottom were observed.
[0066] (1) After adding the energy-saving enhancer, the load and temperature changes of boiler #31 are shown in Table 3.
[0067] Table 3#31 boiler load and temperature changes
[0068] project Before use After use Change value Boiler load (MW) 288~290 294 4 Furnace turning chamber temperature (℃) 550.3 / 522.6 531.7 / 518.8 18.6 / 3.8 Low smoke temperature (℃) 389 376 13 Exhaust temperature (℃) 143.7 136.1 7.6
[0069] It can be seen from Table 3 that after adding the energy-saving synergist of this embodiment, the original sootblowing frequency is kept unchanged, the boiler load is increased by 4MW, the energy-saving synergist acts on the heating surface of the boiler, the coking situation on the heating surface of the furnace shows a trend of alleviation, the amount of coke falling from the bottom of the furnace is too much, the coke is loose and easy to break, the heat absorption of the water-cooled wall is increased, and the exhaust gas temperature is reduced by 7.6°C.
[0070] (2) After adding energy-saving enhancer, the nitrogen oxide and sulfur emissions of boiler #31 are as follows Figure 6 shown.
[0071] from Figure 6 It can be seen that the sulfur dioxide concentration of the flue gas at the inlet of the #31 furnace desulfurization system changes regularly and periodically with the time of adding the synergist. Before use, the sulfur dioxide concentration of the flue gas at the desulfurization inlet was 1467.75 mg / Nm 3 After using the energy-saving synergist obtained in this example, the average sulfur dioxide concentration of the flue gas at the desulfurization inlet was 1337.3 mg / Nm 3 , the sulfur dioxide concentration in the flue gas at the desulfurization inlet tends to decrease steadily. At the same time, after adding the synergist, the nitrogen oxides decreased by 6%.
[0072] (3) After adding energy-saving enhancer, the change of cooling water flow rate of boiler #31 reheater is as follows Figure 7 shown.
[0073] from Figure 7 It can be seen that during the period when the energy-saving synergist obtained in this embodiment was added to the boiler cooling water, the boiler cooling water volume decreased significantly, from 54t / h of reheater cooling water volume before addition to 35t / h, a decrease of 19t / h.
[0074] Example 3
[0075] After 1 ton of copper nitrate is diluted into liquid with 1 ton of water, 3 tons of potassium nitrate, 8 tons of sodium nitrate, 3 tons of silicon dioxide, 25 tons of sodium carbonate, 1 ton of ferric oxide and 59 tons of kaolin are added and mixed at a speed of 180 r / min for 25 minutes to obtain an energy-saving synergist.
[0076] Effect test:
[0077] According to the boiler operating conditions of a workshop of a company in Sichuan, combined with the boiler maintenance plan, boiler #32 was selected, and the energy-saving synergist obtained in this embodiment was poured into the coal mill inlet at 07:00, 15:00, and 23:00 every day. During this period, data was recorded and the coking amount and coking state at the burner port, water-cooled wall and furnace bottom were observed.
[0078] (1) After adding energy-saving enhancer, the changes in boiler load and temperature are shown in Table 4.
[0079] Table 4#32 boiler load and temperature changes
[0080] project Before use After use Change value Boiler load (MW) 288~290 295 5 Exhaust temperature1(℃) 162 153 9 Exhaust temperature 2(℃) 156 145 11
[0081] It can be seen from Table 4 that after adding the energy-saving synergist of this embodiment, the original sootblowing frequency is kept unchanged, the boiler load is increased by 5MW, the energy-saving synergist acts on the heating surface of the boiler, the coking situation on the heating surface in the furnace shows a trend of alleviation, the amount of coke falling from the bottom of the furnace is too much, the heat absorption of the water-cooled wall increases, and the exhaust gas temperature is reduced by 9-11°C.
[0082] (2) After adding energy-saving enhancer, the sulfur emission of boiler is as follows Figure 8 shown.
[0083] from Figure 8 It can be seen that the sulfur dioxide concentration of the flue gas at the inlet of the #32 furnace desulfurization system changes regularly and periodically with the time of adding energy-saving synergist. Before use, the sulfur dioxide concentration of the flue gas at the desulfurization inlet was 4500mg / Nm 3 After using the energy-saving synergist obtained in this example, the average flue gas sulfur dioxide concentration at the desulfurization inlet is 3557 mg / Nm 3 , the original flue gas sulfur dioxide concentration decreased by 21%. After using the energy-saving synergist, nitrogen oxides decreased by 10%, and the sulfur dioxide concentration at the inlet of the desulfurized flue gas tended to decrease.
[0084] (3) After adding energy-saving enhancer, the change of cooling water flow rate of #32 boiler reheater is as follows Fig. 9 shown.
[0085] from Fig. 9 It can be seen that during the addition of energy-saving and efficiency-enhancing agents, the amount of boiler cooling water decreased significantly and the emergency cooling water was not turned on again.
[0086] It can be seen from the above embodiments that the present invention provides an energy-saving synergist, which is prepared from the following raw materials in parts by weight: 0.5-2 parts of copper nitrate, 1.5-4.5 parts of potassium nitrate, 5-10 parts of sodium nitrate, 1-5 parts of silicon dioxide, 20-30 parts of sodium carbonate, 0.5-2 parts of ferric oxide, 55-65 parts of kaolin, and 0.5-2 parts of water. During the research and development of this application, the pain points that need to be solved in the current boilers are fully considered. The energy-saving synergist is prepared using alkaline substances. Under heating conditions, the metal additives are reduced to metals to absorb oxygen and become oxides, and the carbon is also reduced to metals to absorb oxygen and become oxides. The metal is heated and reduced to metal oxide, so that the metal is always in a redox cycle, switching back and forth between the metal and oxide states to achieve a long-term retention effect, and the thermal efficiency of the boiler is also improved accordingly; the energy-saving synergist provided by the present invention has a unique sulfur dioxide emission reduction technology, a nitrogen oxide reduction technology and a unique decoking and coking suppression technology to prevent boiler coking. After use, the sulfur dioxide and nitrogen oxides at the furnace outlet can be reduced by more than 10%, the furnace efficiency is increased, the coal-saving effect is reflected, the slag is loose and fragile, the failure rate of the slag discharge system is effectively reduced, and the labor intensity of the maintenance personnel is reduced.
[0087] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. An energy-saving synergist, characterized in that: Prepared from the following raw materials in parts by weight: 0.5-2 parts of copper nitrate, 1.5-4.5 parts of potassium nitrate, 5-10 parts of sodium nitrate, 1-5 parts of silicon dioxide, 20-30 parts of sodium carbonate, 0.5-2 parts of ferric oxide, 55-65 parts of kaolin, and 0.5-2 parts of water.
2. The method for preparing an energy-saving synergist according to claim 1, characterized in that: It includes the following steps: The energy-saving synergist is obtained by mixing the raw materials in proportion.
3. The method for preparing an energy-saving synergist according to claim 2, characterized in that: The mixing rate is 150-200 r / min; The mixing time is 20 to 30 minutes.