Preparation process and preparation device of nano zinc oxide polyethylene fiber fabric

Through the preparation of nano-zinc oxide and polyethylene composite materials, the problem of traditional polyethylene fiber's insufficient high moisture conductivity and perspiration performance is solved, and the high hygroscopicity, air permeability and thermal insulation properties of zinc oxide-polyethylene composite fiber are achieved. Improved thermal management performance and comfort of textile fabrics.

CN118727167APending Publication Date: 2024-10-01SUPIELD TECH (SHANGHAI) CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410947708.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Traditional polyethylene fibers have shortcomings in high moisture conductivity and perspiration performance, especially in sportswear, outdoor clothing and other occasions, resulting in poor use results.

Method used

The composite material of nano-zinc oxide, high-density polyethylene and ultra-high-density polyethylene is used, and the servo motor in the mixing tank drives the rotating shaft and stirring assembly for uniform mixing, and the annular heating tube and temperature sensor are used to accurately control the heating temperature to prepare Zinc oxide-polyethylene composite fiber improves its hygroscopicity, breathability and thermal insulation properties.

Benefits of technology

It improves the hygroscopicity and breathability of zinc oxide-polyethylene composite materials, enhances its antibacterial, deodorant and heat insulation properties, achieves good thermal comfort and comfort, and broadens the application scope of textile fabrics.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118727167A_ABST
    Figure CN118727167A_ABST
Patent Text Reader

Abstract

The invention relates to a preparation device of a nano-zinc oxide polyethylene fiber fabric, and belongs to the technical field of zinc oxide polyethylene processing.The preparation device of the nano-zinc oxide polyethylene fiber fabric comprises a mixing tank, a rotating shaft vertically and rotationally arranged in the mixing tank and a servo motor arranged on the upper side of the mixing tank and used for driving the rotating shaft to rotate; a plurality of stirring assemblies are movably arranged on the outer side of the rotating shaft, a plurality of annular wave grooves matched with one ends of the stirring assemblies are formed in the inner side wall of the mixing tank, and when the rotating shaft drives the stirring assemblies to move, the annular wave grooves drive the stirring assemblies to move along waves; the zinc oxide-polyethylene composite fiber combines the thermal regulation and control capacity of a zinc oxide inorganic material and the excellent performance of a polyethylene fiber fabric, good thermal comfort is achieved, and the perspiration capacity of the composite fiber is greatly enhanced through the two independent floating yarn organizational structures of the outer layer structure of the composite fiber; the double-needle double-column fixed-loop yarn-added weave structure of the inner layer structure is more close-fitting and fine, and the comfort is greatly enhanced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of zinc oxide polyethylene processing, and specifically relates to a preparation process and a preparation device of a nano zinc oxide polyethylene fiber fabric. Background Art

[0002] With the improvement of living standards, people's demand for textiles is no longer limited to keeping warm and covering the body, but they are more pursuing functionality and comfort; especially in the summer environment, whether textiles can provide effective "heat insulation, moisture conduction, and sweat removal" functions has become the focus of consumers' attention; in this context, researchers in the field of textile fibers are constantly seeking innovations to meet the market demand for high-performance textiles.

[0003] In the field of textile fibers, traditional polyethylene fibers are widely used in the textile industry due to their excellent chemical resistance, high strength and wear resistance. However, with the development of technology and consumers' pursuit of comfort, the shortcomings of polyethylene fibers in terms of softness, hygroscopicity and high temperature resistance have gradually become apparent. Especially in situations where high moisture conduction and perspiration wicking performance is required, such as sportswear and outdoor clothing, the limitations of polyethylene fibers are particularly obvious.

[0004] As a multifunctional inorganic material, zinc oxide has excellent antibacterial, anti-odor, and UV protection properties, and has broad application prospects in the textile industry. When zinc oxide is embedded in polyethylene fibers, it can not only improve the fiber's hygroscopicity and air permeability, improve its moisture conduction and perspiration wicking properties, but also give the fiber excellent antibacterial, anti-odor and thermal insulation properties. Polyethylene fibers embedded with zinc oxide, while maintaining the advantages of traditional polyethylene fibers, have brought significant performance improvements to fiber fabrics by improving moisture absorption and perspiration wicking properties and enhancing thermal insulation properties. This new fiber material not only has excellent physical properties, but also has good biocompatibility and environmental protection. The development of zinc oxide-polyethylene fiber fabrics with excellent triple effects is in line with the development trend of modern textiles.

[0005] For example, in the Chinese invention patent with announcement number CN106637467B and titled A boron-containing nano zinc oxide / polyvinyl alcohol composite fiber and a preparation method thereof, the preparation method of the boron-containing nano zinc oxide / polyvinyl alcohol composite fiber comprises the following steps: 1) dissolving polyvinyl alcohol in water, heating and heating, adding boric acid, mixing evenly, then adding nano zinc oxide, adjusting the pH value of the system after mixing evenly, filtering and degassing to obtain a spinning solution; 2) subjecting the spinning solution obtained in step 1) to a boron-containing alkali wet spinning treatment, then neutralizing, wet drawing, washing, and heat treating to obtain a semi-finished fiber, and then washing and drying to obtain the semi-finished fiber. Although the mechanical properties and antibacterial properties of the boron-containing nano zinc oxide / polyvinyl alcohol composite fiber prepared by the above method are improved, it is easy for people to sweat during use, which makes the experience effect not good. In order to make the fiber have a good cooling effect and improve the use effect of the fiber, a preparation process and a preparation device of a nano zinc oxide polyethylene fiber fabric are now needed. Summary of the invention

[0006] The purpose of the present invention is to provide a preparation process and a preparation device of a nano zinc oxide polyethylene fiber fabric with a simple structure and reasonable design in order to solve the above problems.

[0007] The present invention achieves the above-mentioned purpose through the following technical solutions:

[0008] A preparation device for nano zinc oxide polyethylene fiber fabrics comprises a mixing tank, wherein a rotating shaft is vertically rotatably arranged inside the mixing tank and a servo motor is arranged on the upper side of the mixing tank to drive the rotating shaft to rotate, a plurality of stirring components are movably arranged outside the rotating shaft, a plurality of annular wave grooves matching one end of the stirring components are opened on the inner side wall of the mixing tank, and when the rotating shaft drives the stirring components to move, the stirring components are driven to move along the waves through the annular wave grooves.

[0009] As a further optimization solution of the present invention, a plurality of racks are arranged on the outer side of the rotating shaft, a gear is meshed on one side of the plurality of racks, and one end of the stirring assembly is fixedly connected to the gear.

[0010] As a further optimization scheme of the present invention, the stirring assembly includes a rotating rod fixedly arranged on one side of the gear, and a plurality of stirring rods are arranged on the rotating rod. The end of the rotating rod away from the gear is movably inserted into the inner side of the annular wave groove, and a transmission assembly for driving the stirring assembly to move is arranged on the rotating shaft.

[0011] As a further optimization scheme of the present invention, one end of the rotating rod is sleeved with a roller movably arranged inside the annular wave groove, a fixed cylinder is fixedly arranged on the outside of the rotating rod, and a plurality of the stirring rods are fixedly arranged on the outside of the fixed cylinder.

[0012] As a further optimization scheme of the present invention, the transmission assembly includes fixed plates fixedly arranged at both ends of the rotating shaft, a push rod is fixedly arranged between the two fixed plates, a sliding sleeve is provided on the push rod, and a bearing mounted on a fixed cylinder is provided on one side of the sliding sleeve.

[0013] As a further optimization solution of the present invention, a plurality of slide grooves are provided on the outer side of the rotating shaft, and the rack and the gear are both arranged on the inner side of the slide grooves.

[0014] As a further optimization scheme of the present invention, an annular heating pipe is arranged on the inner side of the mixing tank, a temperature sensor is arranged on the bottom of the mixing tank, and a control panel electrically connected to the annular heating pipe and the temperature sensor is arranged on the front side of the mixing tank.

[0015] As a further optimization scheme of the present invention, a feed pipe and a reagent tube are arranged at the top of the mixing tank, a discharge pipe is arranged at the bottom of the mixing tank, an observation window is arranged on one side of the mixing tank, and a plurality of support bases are arranged on the outside of the mixing tank.

[0016] A preparation process of nano zinc oxide polyethylene fiber fabric comprises the following steps:

[0017] S1: First, high-density polyethylene and ultra-high-density polyethylene are added into a mixing tank through a feed pipe to mix and melt, and then nano zinc oxide is added through a reagent tube to mix with the melted polyethylene, and then paraffin oil is added through a reagent tube to heat and stir, and then the composite mixture is pressed into a film, and a solvent is added to obtain a pure zinc oxide-polyethylene composite material;

[0018] S2: blending and spinning polyethylene and zinc oxide-polyethylene composite materials to obtain polyethylene fibers and zinc oxide-polyethylene composite fibers, respectively;

[0019] S3: Design polyethylene fiber and zinc oxide-polyethylene fiber composite structure to prepare cool fabric

[0020] As a further optimization scheme of the present invention, the particle size of the nano zinc oxide is 0.3-0.8 μm, the mass ratio of the high-density polyethylene, ultra-high-density polyethylene and nano zinc oxide melts is 4:1:2, the mass ratio of the melted polyethylene to the paraffin oil in step S1 is 1:5, the melting temperature of the paraffin oil added in step S1 is 130-180°C, the rotation speed is 100-1200 r / min, and the stirring is 20-30 min, and the solvent is dichloromethane.

[0021] The beneficial effects of the present invention are:

[0022] 1. In the present invention, the servo motor drives the rotating shaft to rotate, so that the push rod on the rotating shaft can be driven to rotate together, and the push rod pushes the fixed cylinder to rotate together with the rotating rod. Since one end of the rotating rod is movably inserted into the annular wave groove, the rotating rod will make wave motion along with the annular wave groove during rotation, and the other end of the rotating rod is meshed with the rack on the rotating shaft through the gear. Therefore, when the rotating rod is in the process of vertical movement, the rotating rod will rotate, and the several stirring rods on the rotating rod can be rotated. Finally, the several stirring rods will rotate while making wave motion, so that the nano zinc oxide, polyethylene and paraffin oil in the mixing tank are evenly mixed, which can improve the mixing effect of nano zinc oxide and polyethylene, and improve the hygroscopicity and air permeability of the subsequently prepared zinc oxide-polyethylene composite material, and on the other hand, it can improve the mixing effect of paraffin oil with nano zinc oxide and polyethylene, improve the heat conduction effect, make the melting effect of nano zinc oxide and polyethylene better, and improve the preparation efficiency.

[0023] 2. In the present invention, the heating area and the melting effect can be increased by setting the annular heating tube on the inner wall of the mixing tank, and the heating and melting temperature can be accurately controlled to 130-180°C through the temperature sensor and the control panel, so that the melting and mixing of nano zinc oxide and polyethylene is more uniform, the hygroscopicity and air permeability of the zinc oxide-polyethylene composite material are improved, and the composite material has excellent antibacterial, deodorizing and heat-insulating properties.

[0024] 3. In the present invention, the zinc oxide-polyethylene composite fiber combines the thermal regulation ability of zinc oxide inorganic materials and the excellent performance of polyethylene fiber fabrics to achieve good thermal comfort. The two independent floating yarn mechanism structures of the outer layer structure greatly enhance its perspiration ability; the double-needle double-column fixed loop and yarn structure of the inner layer structure is more close-fitting and delicate, which greatly enhances the comfort. Nano zinc oxide polyethylene fibers can be used in multiple fields such as textile fabrics and fillers to improve thermal management performance and broaden the wide application of polyethylene in the field of textile fabrics. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 is a schematic diagram of a first internal overall structure of the present invention;

[0026] Figure 2 is a second internal overall structure schematic diagram of the present invention;

[0027] Figure 3 It is a schematic diagram of the partial internal overall structure of the present invention;

[0028] Figure 4 It is a schematic diagram of the overall structure of the present invention when viewed from above;

[0029] Figure 5 It is a schematic diagram of the overall structure of the present invention from a top view;

[0030] Figure 6 The present invention Figure 1 Enlarged view of point A in the middle;

[0031] Figure 7 The present invention Figure 2 Enlarged view of point B in the middle;

[0032] Figure 8 It is a double needle double column fixed loop plus yarn organization diagram;

[0033] Fig. 9 It is an organizational diagram of two independent floating yarn mechanisms.

[0034] In the figure: 1. mixing tank; 2. rotating shaft; 3. annular wave groove; 4. fixed plate; 5. transmission assembly; 501. push rod; 502. sliding sleeve; 503. bearing; 6. sliding groove; 7. rack; 8. stirring assembly; 801. rotating rod; 802. fixing cylinder; 803. stirring rod; 9. feeding pipe; 10. servo motor; 11. reagent tube; 12. discharging pipe; 13. annular heating tube; 14. supporting base; 15. observation window; 16. control panel; 17. gear; 18. roller; 19. temperature sensor. DETAILED DESCRIPTION

[0035] The present application is further described in detail below in conjunction with the accompanying drawings. It is necessary to point out here that the following specific implementation methods are only used to further illustrate the present application and cannot be understood as limiting the scope of protection of the present application. Technical personnel in this field can make some non-essential improvements and adjustments to the present application based on the above application content.

[0036] Example 1: Figure 1 , Figure 2 , Figure 3 , Figure 4 , Figure 5 , Figure 6 , Figure 7As shown, a preparation device for nano zinc oxide polyethylene fiber fabric comprises a mixing tank 1, a feeding pipe 9 and a reagent pipe 11 are arranged at the top of the mixing tank 1, a discharging pipe 12 is arranged at the bottom of the mixing tank 1, and valves (not shown in the figure) are arranged on the feeding pipe 9, the reagent pipe 11 and the discharging pipe 12, a rotating shaft 2 is arranged vertically inside the mixing tank 1, a plurality of racks 7 are arranged on the outside of the rotating shaft 2, and the plurality of racks 7 can be arranged in multiple rows. In this embodiment, two rows are taken, and three in each row are taken as an example. The specific number of rows and the number of each row can be flexibly adjusted according to the production scale, one side of the plurality of racks 7 are meshed with gears 17, a plurality of chutes 6 are provided on the outside of the rotating shaft 2, the racks 7 and the gears 17 are arranged on the inner side of the chutes 6, one end of the stirring assembly 8 is fixedly connected to the gear 17, and a servo motor 10 for driving the rotating shaft 2 to rotate is arranged on the upper side of the mixing tank 1. A plurality of stirring assemblies 8 are movably arranged on the outer side of the shaft 2. The stirring assemblies 8 include a rotating rod 801 fixedly arranged on one side of the gear 17, and a plurality of stirring rods 803 are arranged on the rotating rod 801. One end of the rotating rod 801 away from the gear 17 is movably inserted into the inner side of the annular wave groove 3. One end of the rotating rod 801 is sleeved with a roller 18 movably arranged on the inner side of the annular wave groove 3. The roller 18 allows one end of the rotating rod 801 to move freely inside the annular wave groove 3, so that the rotating rod 801 can make wave motion. A fixed cylinder 802 is fixedly arranged on the outer side of the rotating rod 801, and a plurality of stirring rods 803 are fixedly arranged on the outer side of the fixed cylinder 802. A plurality of annular wave grooves 3 cooperating with one end of the rotating rod 801 are opened on the inner side wall of the mixing tank 1. When the rotating shaft 2 drives the stirring assembly 8 to move, the annular wave groove 3 drives the stirring assembly 8 to move up and down along the waves.

[0037] like Figure 1 , Figure 2 , Figure 6 , Figure 7As shown, fixed plates 4 are fixedly provided at both ends of the rotating shaft 2, a push rod 501 is fixedly provided between the two fixed plates 4, a sliding sleeve 502 is slidably sleeved on the push rod 501, and a bearing 503 with an inner ring fixedly sleeved on a fixed cylinder 802 is fixedly provided on one side of the sliding sleeve 502. When in use, the servo motor 10 drives the rotating shaft 2 to rotate, and then drives the fixed plate 4 and the push rod 501 to rotate together, and the sliding sleeve 502 and the bearing 503 on the push rod 501 push the fixed cylinder 802 and the rotating rod 801 to rotate around the rotating shaft 2. During the rotation of the rotating rod 801, the roller 18 at one end of the rotating rod 801 rolls on the inner side of the annular wave groove 3 on the inner wall of the mixing tank 1. Since the annular wave groove 3 adopts a wavy structure and is closed on the inner wall of the mixing tank 1, the rotating rod 801 can move up and down in waves while rotating around the rotating shaft 2. During the up and down wave movement of the rotating rod 801, the gear 17 at one end of the rotating rod 801 is engaged with the rack 7, so it can also rotate while moving in waves, so that the degree of freedom of the stirring rod 803 on the rotating rod 801 is increased, the mixing effect is improved, and the contact area between the paraffin oil and the polyethylene can be increased, further improving the melting effect.

[0038] Embodiment 2: Based on embodiment 1, further improvement is made in that Figure 3 , Figure 4 , Figure 5 As shown, an annular heating tube 13 is arranged on the inner side of the mixing tank 1, and the annular heating tube 13 can increase the heating area, so that the heating effect is better, and in order to further increase the heating area, the annular heating tube 13 can also adopt a wavy structure with the same shape as the annular wave groove 3, and a plurality of them can be arranged, and a temperature sensor 19 is arranged on the bottom of the mixing tank 1, and a control panel 16 electrically connected to the annular heating tube 13 and the temperature sensor 19 is arranged on the front side of the mixing tank 1, and the servo motor 10 is electrically connected to the control panel 16. When in use, the temperature inside the mixing tank 1 and the stirring rate can be adjusted through the control panel 16, so that the melted nano zinc oxide and polyethylene are mixed more evenly, thereby improving the uniformity of the composite fiber.

[0039] Embodiment 3: A process for preparing nano zinc oxide polyethylene fiber fabric, comprising the following steps:

[0040] S1: First, high-density polyethylene (HDPE, molecular weight 1.0×10 5 , melt index 2.2g / 10min) and ultra-high density polyethylene (UHMW, molecular weight 1.15×10 6) Add the mixture into the mixing tank 1 through the feed pipe 9 in a mass ratio of 4:1, mix and melt, then add 2 parts of nano zinc oxide with a particle size of 0.3-0.8 μm through the reagent tube 11 and mix with the melted polyethylene, then add paraffin oil through the reagent tube 11, heat and stir, the mass ratio of polyethylene to paraffin oil is 1:5, so that the melting temperature is 130-180°C, the rotation speed is 100-1200r / min, stir for 20-30min, then, press the composite mixture into a film at 80-120°C, add dichloromethane solvent for purification, and finally wash and dry to obtain a pure zinc oxide-polyethylene (ZnO-PE) composite material;

[0041] When in use, adding paraffin oil can make polyethylene and nano zinc oxide melt faster and improve the mixing effect of the two. Paraffin oil has a higher boiling point and can evenly conduct heat to polyethylene and nano zinc oxide, thereby improving the melting efficiency of the two.

[0042] S2: Blending and spinning polyethylene and zinc oxide-polyethylene composite materials to obtain polyethylene (PE) fibers and zinc oxide-polyethylene (ZnO-PE) composite fibers, respectively;

[0043] The specific steps include:

[0044] 1. Pretreatment of zinc oxide-polyethylene composite fiber:

[0045] a. Grind the ZnO-PE composite material to a powder with an average particle size of less than 20 μm; dry at 50°C for 4 hours, then heat to 100°C and keep warm for 4 hours to fully dry the composite powder to a moisture content of less than 100 ppm.

[0046] b. Select antioxidant 1010 as the additive.

[0047] The chemical name of antioxidant 1010 is: pentaerythritol tetrakis[β-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate], white crystalline powder, and its chemical properties are stable.

[0048] 2. Melt spinning of zinc oxide-polyethylene composite materials:

[0049] The dried powder is added into a spinning machine for melt spinning.

[0050] Specifically, the ZnO-PE nanocomposite material and the antioxidant 1010 are mixed and extruded by a twin-screw extruder at a heating rate of 5-10°C / min to 120-130°C, and then post-cooled, stretched and wound to obtain ZnO-PE fibers.

[0051] The process parameters for spinning zinc oxide-polyethylene composite fibers are as follows:

[0052]

[0053] The above preparation process and spinning process parameters are variable according to actual conditions, and the temperature variation range is ±5°C.

[0054] 3. Pretreatment of polyethylene fiber:

[0055] The mass ratio of high-density polyethylene to ultra-high-density polyethylene is 10:1-3, to obtain a mixed powder;

[0056] The average particle size of the mixed powder is less than 20 μm. After drying at 60° C. for 4 hours, the temperature is raised to 100° C. and kept at this temperature for 4 hours, and the mixed powder is fully dried so that the moisture content of the composite powder is less than 100 ppm.

[0057] Antioxidant 1010 was selected as the additive.

[0058] The chemical name of antioxidant 1010 is: pentaerythritol tetrakis[β-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate], white crystalline powder, and its chemical properties are stable.

[0059] 4. Melt spinning of polyethylene composite materials:

[0060] The dried powder is added into a spinning machine for melt spinning.

[0061] Specifically, the mixed powder is added into a melt spinning machine and spun at 130-180°C and 80-100rpm for 20-30min. The obtained melt is extruded at a spiral speed of 5-8rpm and wound at a speed of 6-10m / min to obtain a molten extrudate, which is then cooled and stretched to obtain PE fiber.

[0062] The process parameters for polyethylene fiber spinning are as follows:

[0063]

[0064]

[0065] The above preparation process and spinning process parameters are variable according to actual conditions, and the temperature variation range is ±5°C.

[0066] S3: Design a composite structure of polyethylene fiber and zinc oxide-polyethylene fiber to prepare a cool fabric.

[0067] The 100-400μm polyethylene fiber is used as the inner layer fabric and the 200-400μm zinc oxide-polyethylene fiber is used as the outer layer fabric. All the veils of the inner layer fabric are PE fiber filaments. The loom adopts a double-needle double-column fixed loop plus yarn structure and is reciprocatedly woven (such as Figure 8The outer fabric is all ZnO-PE fiber filaments, which are woven back and forth on a loom with two independent floating yarn structures (as shown in Fig. 9 As shown in the figure), the inner and outer layers are connected by weaving polyethylene fibers to finally produce a cool fabric.

[0068] Zinc oxide-polyethylene composite fiber combines the thermal regulation ability of zinc oxide inorganic materials and the excellent performance of polyethylene fiber fabrics, achieving good thermal comfort. The two independent floating yarn mechanism structure of its outer layer structure greatly enhances its perspiration ability; the double-needle double-column fixed loop and yarn structure of the inner layer structure is more close-fitting and delicate, greatly enhancing comfort. Nano zinc oxide polyethylene fiber can be used in textile fabrics, fillings and other fields to improve thermal management performance and broaden the wide application of polyethylene in the field of textile fabrics.

[0069] The woven lining is as follows:

[0070]

[0071] The woven outer layer is as follows:

[0072]

[0073] The nano zinc oxide polyethylene fiber three-in-one cool sweat-wicking fabric prepared according to the above method has the advantages of low thermal radiation, low thermal conductivity, and low thermal humidity. Its unique fiber structure can quickly dissipate heat and absorb moisture to keep the skin dry. At the same time, good air permeability effectively prevents damp heat and brings lasting coolness. This fabric is not only comfortable and breathable, but also has antibacterial properties, making it an ideal choice for summer clothing.

[0074] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention.

Claims

1. A device for preparing nano zinc oxide polyethylene fiber fabric, comprising a mixing tank (1), characterized in that: The mixing tank (1) is provided with a rotating shaft (2) and a servo motor (10) arranged on the upper side of the mixing tank (1) for driving the rotating shaft (2) to rotate. A plurality of stirring components (8) are movably arranged on the outer side of the rotating shaft (2). The inner side wall of the mixing tank (1) is provided with a plurality of annular wave grooves (3) which cooperate with one end of the stirring components (8). When the rotating shaft (2) drives the stirring components (8) to move, the annular wave grooves (3) drive the stirring components (8) to move along the waves.

2. The device for preparing a nano zinc oxide polyethylene fiber fabric according to claim 1, characterized in that: A plurality of racks (7) are arranged on the outer side of the rotating shaft (2), one side of each of the racks (7) is meshed with a gear (17), and one end of the stirring assembly (8) is fixedly connected to the gear (17).

3. The device for preparing a nano zinc oxide polyethylene fiber fabric according to claim 3, characterized in that: The stirring assembly (8) comprises a rotating rod (801) fixedly arranged on one side of the gear (17), a plurality of stirring rods (803) being arranged on the rotating rod (801), one end of the rotating rod (801) away from the gear (17) being movably inserted into the inner side of the annular wave groove (3), and a transmission assembly (5) for driving the stirring assembly (8) to move is arranged on the rotating shaft (2).

4. The device for preparing a nano zinc oxide polyethylene fiber fabric according to claim 3, characterized in that: One end of the rotating rod (801) is sleeved with a roller (18) movably arranged inside the annular wave groove (3); a fixed cylinder (802) is fixedly arranged outside the rotating rod (801); and a plurality of stirring rods (803) are fixedly arranged outside the fixed cylinder (802).

5. The device for preparing nano zinc oxide polyethylene fiber fabric according to claim 4, characterized in that: The transmission assembly (5) comprises fixed plates (4) fixedly arranged at both ends of the rotating shaft (2), a push rod (501) fixedly arranged between the two fixed plates (4), a sliding sleeve (502) slidingly sleeved on the push rod (501), and a bearing (503) sleeved on the fixed cylinder (802) is arranged on one side of the sliding sleeve (502).

6. The device for preparing a nano zinc oxide polyethylene fiber fabric according to claim 2, characterized in that: A plurality of slide grooves (6) are provided on the outer side of the rotating shaft (2), and the rack (7) and the gear (17) are both arranged on the inner side of the slide grooves (6).

7. The device for preparing nano zinc oxide polyethylene fiber fabric according to claim 6, characterized in that: An annular heating pipe (13) is arranged on the inner side of the mixing tank (1), a temperature sensor (19) is arranged on the bottom of the mixing tank (1), and a control panel (16) electrically connected to the annular heating pipe (13) and the temperature sensor (19) is arranged on the front side of the mixing tank (1).

8. The device for preparing nano zinc oxide polyethylene fiber fabric according to claim 7, characterized in that: The top of the mixing tank (1) is provided with a feed pipe (9) and a reagent pipe (11), the bottom of the mixing tank (1) is provided with a discharge pipe (12), one side of the mixing tank (1) is provided with an observation window (15), and the outer side of the mixing tank (1) is provided with a plurality of support bases (14).

9. A process for preparing nano zinc oxide polyethylene fiber fabric using the preparation device according to any one of claims 1 to 8, characterized in that: The following steps are involved: S1: firstly, adding high-density polyethylene and ultra-high-density polyethylene into a mixing tank (1) through a feed pipe (9) to mix and melt, then adding nano zinc oxide and the melted polyethylene through a reagent pipe (11) to mix, then adding paraffin oil through the reagent pipe (11) to heat and stir, then, pressing the composite mixture into a film, adding a solvent, and obtaining a pure zinc oxide-polyethylene composite material; S2: blending and spinning polyethylene and zinc oxide-polyethylene composite materials to obtain polyethylene fibers and zinc oxide-polyethylene composite fibers, respectively; S3: Design a composite structure of polyethylene fiber and zinc oxide-polyethylene fiber to prepare a cool fabric.

10. The process for preparing the nano zinc oxide polyethylene fiber fabric according to claim 9, characterized in that: The particle size of the nano zinc oxide is 0.3-0.8 μm, the mass ratio of the high-density polyethylene, ultra-high-density polyethylene and nano zinc oxide melts is 4:1:2, the mass ratio of the melted polyethylene to the paraffin oil in step S1 is 1:5, the melting temperature of the paraffin oil added in step S1 is 130-180° C., the rotation speed is 100-1200 r / min, and the stirring is 20-30 min, and the solvent is dichloromethane.

Citation Information

Patent Citations

  • Anti bacterial anti mite fiber and preparation method thereof

    CN106498531A

  • Organic silicon flame-retardant sealant and preparation method thereof

    CN112625643A

  • Ultra-high molecular weight polyethylene fiber as well as preparation method and application thereof

    CN113151912A

  • Electrophoresis wastewater comprehensive treatment device

    CN218795257U

  • Herbicide filling device

    CN221165950U