A method for preparing a high-sensitivity resonant differential pressure sensor and a high-sensitivity resonant differential pressure sensor
Through the combination of dry etching and low-pressure chemical vapor deposition, the local packaging of the resonator is realized, solving the problems of poor packaging accuracy and sealing in the prior art, and improving the sensitivity and static pressure resistance of the resonant differential pressure sensor ability.
Patent Information
- Application Number
- CN202410761677.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-13
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-06-13
AI Technical Summary
The sensitivity and range of existing resonant differential pressure sensors are relatively low, mainly because the packaging method is difficult to achieve accuracy control, resulting in static pressure errors and poor packaging sealing, which limits the performance of the sensor.
The SOI sheet is etched by dry method to form resonators and anchors, and the low-pressure chemical vapor deposition method is used to deposit silicon dioxide and polysilicon, so as to realize the local packaging of the resonator through structural design, control the side drilling amount and sealing of the capping layer, and reduce static Pressure error.
The measurement accuracy and static pressure tolerance of the sensor are improved, the sensitivity and range ratio are improved, and the yield and efficiency of the silicon-glass/silicon-silicon bonded packaging solution is solved.
Smart Images

Figure CN118730382B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of resonant differential pressure sensors, and more specifically, to a preparation method of a high-sensitivity resonant differential pressure sensor and a high-sensitivity resonant differential pressure sensor. Background Art
[0002] Resonant MEMS differential pressure sensors use the deformation of the pressure membrane to produce corresponding stress changes in the resonator, thereby changing the frequency of the resonator. Usually, the resonator needs to work in a vacuum environment. A higher vacuum degree will provide the resonator with less damping and a higher Q value, which in turn has higher accuracy and stability. Since the resonator package has a cavity structure, the resonator cannot be located on the surface of the diaphragm, which limits the sensitivity of the sensor, and the sensor's range ratio is much lower than that of a silicon piezoresistive differential pressure sensor.
[0003] Most of the widely used resonator packaging methods currently use wafer bonding processes such as anodic bonding, eutectic bonding, and silicon-silicon bonding. For example, the cited patent technology (CN112611501B) uses silicon glass bonding and getters to achieve the packaging of multiple groups of resonators, and thins the cap to the expected thickness through grinding or etching processes. The cited technology CN116465541A uses a cover structure with an oxide layer to achieve a 3-5um cap, which improves the differential pressure sensitivity of the sensor. In addition, some packaging methods use a thin film deposition process, which has the ability to accurately control the thickness of the film. The cited patent CN103350983A uses multiple sacrificial layers and polysilicon to achieve the packaging of the resonator.
[0004] CN112611501B is difficult to achieve precision control of several microns of the capping layer due to grinding and etching techniques, so its sensitivity is difficult to further improve. CN116465541A multilayer structure (especially amorphous materials) causes the linearity and repeatability of the diaphragm to deteriorate, causing sensor hysteresis error. At the same time, due to the large alignment error and material degassing problems in the bonding process, it is necessary to enlarge the resonator capping size and retain a large getter storage area, so the sensor also has a larger static pressure error, which limits the sensor range ratio. Although the design of multiple resonators is adopted and the error compensation is performed by the algorithm, there are still problems such as large sensor chip size, low bonding yield, and high single-chip bonding cost. Although CN103350983A realizes the packaging of the resonator, there are problems such as large side drilling of the sacrificial layer, large size of the resonant capping, and poor reliability of the packaging seal, which is not conducive to improving the static pressure tolerance and range ratio of the micro differential pressure sensor.
[0005] Therefore, how to provide a preparation method for a highly sensitive resonant differential pressure sensor becomes a technical problem that needs to be solved urgently. Summary of the invention
[0006] The object of the present invention is to provide a method for preparing a high-sensitivity resonant differential pressure sensor and a high-sensitivity resonant differential pressure sensor.
[0007] The first aspect of the present invention provides a method for preparing a high-sensitivity resonant differential pressure sensor, comprising: step S1: dry etching an SOI wafer, etching a single crystal silicon device layer of the SOI wafer to form a resonator, an anchor point and an electrode; an electrode is provided on each side of the width of the resonator, and a separation groove extending along the length direction of the resonator is formed between the electrode and the resonator; an anchor point is connected to each end of the length of the resonator, the two anchor points are located on opposite sides of the electrode, and an isolation groove connected to the separation groove is formed between the anchor point and the electrode, the isolation groove includes a first isolation groove connected to the separation groove and a second isolation groove connected to the other end of the first isolation groove, and the groove width of the second isolation groove is greater than that of the first isolation groove;
[0008] Step S2: using a low pressure chemical vapor deposition method, depositing a first layer of silicon dioxide on the surface of the SOI wafer to cover the surface, and allowing the first layer of silicon dioxide to fill the etched isolation grooves;
[0009] Step S3: patterning the first layer of silicon dioxide, and etching a groove on the periphery of the resonator; the etched peripheral area of silicon dioxide needs to cover the second isolation groove of step S1 to ensure that the first isolation groove is not etched;
[0010] Step S4: using low pressure chemical vapor deposition to deposit a first layer of polysilicon on the surface of the first layer of silicon dioxide, the first layer of polysilicon filling the groove etched in step S3 and connected to the electrode;
[0011] Step S5: patterning and etching the first layer of polysilicon directly above the resonator to etch a plurality of groups of release holes distributed along the length direction of the resonator above the resonator, the release holes being connected to the first layer of silicon dioxide deposited in step S2;
[0012] Step S6: using low pressure chemical vapor deposition, depositing a second layer of silicon dioxide on the surface of the first layer of polysilicon, wherein the second layer of silicon dioxide fills the release holes and connects to the first layer of silicon dioxide;
[0013] Step S7: patterning and etching the second layer of silicon dioxide on both sides of the width of the resonator, so as to etch through holes distributed along the length direction of the resonator and penetrating the second layer of silicon dioxide above the resonator and on both sides of the straight line where the plurality of groups of release holes are located;
[0014] Step S8: using low pressure chemical vapor deposition, depositing a second layer of polysilicon on the surface of the second layer of silicon dioxide, the second layer of silicon dioxide being connected to the first layer of polysilicon through the through hole etched in step S7;
[0015] Step S9: patterning and etching the second layer of polysilicon to the second layer of silicon dioxide, leaving a portion of the second layer of polysilicon above the resonator to form a shielding layer above the resonator;
[0016] Step S10: etching the exposed second layer of silicon dioxide, and etching the silicon dioxide around the resonator through the gap between the shielding layer and the first layer of polysilicon and the release hole to release the resonator;
[0017] Step S11: depositing a third layer of polysilicon in a vacuum environment using a low-pressure chemical vapor deposition method to complete the sealing of the resonator.
[0018] Optionally, the preparation method further comprises:
[0019] Step S12: etching multiple layers of polysilicon and silicon dioxide on both sides of the width of the resonator until the upper surface of the SOI wafer is exposed;
[0020] Step S13: performing high temperature annealing.
[0021] Optionally, the preparation method further comprises:
[0022] Step S14: using low pressure chemical vapor deposition to deposit a layer of silicon nitride on the surface of the cover.
[0023] Optionally, the preparation method further comprises:
[0024] Step S15: Dry / wet etching of silicon nitride to expose the single crystal silicon on the surface of the electrode, and evaporating metal on the electrode to form a metal pad.
[0025] Optionally, in step S2, the method of depositing a first layer of silicon dioxide on the surface of the SOI wafer by using a low pressure chemical vapor deposition method, and allowing the first layer of silicon dioxide to fill the etched isolation groove includes:
[0026] A layer of tetraethoxysilane is deposited on the surface of the SOI wafer by low-pressure chemical vapor deposition. The tetraethoxysilane is decomposed into silicon dioxide and then deposited on the surface of the resonator. The thickness of the deposited silicon dioxide is 1um to 2um.
[0027] Optionally, the thickness of the first layer of polysilicon deposited in step S4 is greater than 2 um and less than 5 um.
[0028] Optionally, in step S10 , etching the exposed second silicon dioxide layer, and etching silicon dioxide around the resonator through the gap between the shielding layer and the first polysilicon layer and the release hole to release the resonator includes: etching silicon dioxide using gaseous hydrofluoric acid.
[0029] Optionally, the method of etching the multilayer polysilicon and silicon dioxide in step S12 includes:
[0030] Dry etching and / or wet etching.
[0031] Optionally, the annealing temperature of the high temperature annealing in step S13 is 950° C. to 1050° C.;
[0032] And / or the thickness of the second silicon dioxide layer is 0.5um to 1um.
[0033] The second aspect of the present invention discloses a high-sensitivity resonant differential pressure sensor, comprising a sensor chip, wherein the sensor chip is manufactured by any method for preparing a high-sensitivity resonant differential pressure sensor according to the first aspect of the present invention.
[0034] According to the technical content disclosed in the present invention, the following beneficial effects are achieved:
[0035] The preparation method of the high-sensitivity resonant differential pressure sensor provided by the present invention 1. Vacuum packaging is performed through polycrystalline silicon, which can effectively solve the problems of wafer bonding yield and low wafer bonding packaging efficiency in the vacuum packaging scheme of silicon-glass / silicon-silicon bonding; the thin film deposition thickness is accurately controlled by low-pressure chemical vapor deposition method, and the side drilling amount of the capping layer is controlled through process design and structural design to achieve good sealing of the vacuum cavity, thereby realizing partial packaging of the resonant beam, effectively reducing the static pressure error of the sensor, and improving the measurement accuracy of the sensor.
[0036] When sealing the groove etched in step S1, as the low-pressure chemical vapor deposition (LPCVD) process proceeds, the silicon dioxide deposited on the sidewalls of the slit will gradually become thicker until the entire groove is filled. However, the deposition rate is not ideally consistent everywhere, which will cause voids to exist at the junction of the silicon dioxide deposited on both sides, resulting in sealing failure. The present invention uses a first isolation groove and a second isolation groove with different widths through structural design, so that the width of the groove to be sealed is narrowed from wide, so that a layer of silicon dioxide can be completely covered at the outlet of the first isolation groove, and the micro-voids inside the first isolation groove are sealed. Therefore, a smaller packaging size can be used to achieve a better packaging effect and complete partial packaging.
[0037] Further features and advantages of the present invention will become apparent from the following detailed description of exemplary embodiments of the present invention with reference to the attached drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] The accompanying drawings, which are incorporated in and constitute a part of the specification, illustrate embodiments of the invention and, together with the description, serve to explain the principles of the invention.
[0039] Figure 1 It is a schematic diagram of the structure of the sensor chip of the present invention.
[0040] Figure 2It is a schematic diagram of the first cross-sectional structure of the sensor chip of the present invention.
[0041] Figure 3 It is a cross-sectional view corresponding to each step in the preparation process of the high-sensitivity resonant differential pressure sensor of the present invention.
[0042] Figure 4 It is a schematic diagram of the second cross-sectional structure of the sensor of the present invention.
[0043] Figure 5 It is a schematic diagram of the structure of the local packaging of the sensor chip of the present invention.
[0044] In the figure: 1. pressure sensitive film; 2. resonator; 3. local packaging cover; 4. anchor point; 5. wire; 6. electrode; 61. drive electrode; 62. detection electrode; 71. device layer; 72. buried oxide layer; 73. substrate layer; 81. first isolation groove; 82. second isolation groove; 9. cavity. DETAILED DESCRIPTION
[0045] Various exemplary embodiments of the present invention will now be described in detail with reference to the accompanying drawings. It should be noted that the relative arrangement of components and steps, numerical expressions and numerical values set forth in these embodiments do not limit the scope of the present invention unless otherwise specifically stated.
[0046] The following description of at least one exemplary embodiment is merely illustrative in nature and is in no way intended to limit the invention, its application, or uses.
[0047] Technologies, methods, and equipment known to ordinary technicians in the relevant art may not be discussed in detail, but where appropriate, the technologies, methods, and equipment should be considered part of the specification.
[0048] In all examples shown and discussed herein, any specific values should be interpreted as merely exemplary and not as limiting. Therefore, other examples of the exemplary embodiments may have different values.
[0049] It should be noted that like reference numerals and letters refer to similar items in the following figures, and therefore, once an item is defined in one figure, it need not be further discussed in subsequent figures.
[0050] See also Figure 1 The present invention discloses a highly sensitive resonant differential pressure sensor, specifically a resonator partially encapsulated micro differential pressure sensor, including: Figure 1 The sensor chip shown is made of SOI and includes a pressure sensitive film 1, a resonator 2, an anchor point 4, a wire 5, an electrode 6, an insulating layer, a local cover 3 and other structures; it should be noted that SOI includes a device layer 71, a buried oxide layer 72 and a substrate layer 73 arranged in sequence. Figure 1 and Figure 2 The resonator 2 uses a resonant beam with a micro-beam structure, the middle part of the resonant beam is suspended, and the two ends are fixed on the anchor point 4. There is a pair of electrodes 6 on the left and right sides of the resonant beam, specifically, the driving electrode 61 and the detection electrode 62 are placed in parallel on the left and right sides of the resonator 2, and keep a 1um to 2um spacing with the resonator, and form a separation groove with a width of 1um to 2um between the resonator 2 and the electrode, so that the resonator can be moved along the Figure 2 In the direction of the arrow, the resonator 2 vibrates in a plane parallel to the plane where the sensor chip is located, along the direction perpendicular to the length direction of the resonator 2. Figure 5 As shown, the anchor points at both ends of the resonator 2 adopt a "convex" shape structure, the protruding parts are connected to the resonant beam, and the two long sides of the electrode 6 (the sides extending along the length direction of the resonator 2) are respectively kept at a distance of 1um to 2um from the driving electrode 61 and the detection electrode 62 to form a separation groove. An isolation groove interconnected with the separation groove is formed between the anchor point 4 and the wide side of the electrode 6 (the side extending along the width direction of the resonator 2). Based on the "convex" shape structure of the anchor point, the protruding part of the anchor point is closer to the wide side of the electrode 6, and the two sides of the protruding part of the anchor point are farther from the wide side of the electrode 6. Therefore, the isolation groove includes a first isolation groove 81 connecting the separation groove and a second isolation groove 82 connected to the other end of the first isolation groove 81. The groove width of the second isolation groove 82 is greater than that of the first isolation groove 81; specifically, the groove width of the second isolation groove 82 is about 20um. In order to reduce the packaging size, the top of the resonant beam is partially packaged by a polysilicon micro-cap. The polysilicon micro-cap is in close contact with the driving electrode 61, the detection electrode 62, the anchor boss, and the pressure film outside the boss, thereby sealing the space around the resonator 2. In order to achieve good sealing and packaging strength, the first isolation groove 81 is filled with a silicon dioxide insulation layer, and the polysilicon micro-cap is laid flat on the surface of the silicon oxide insulation layer. Finally, a dense layer of silicon nitride is grown on the polysilicon micro-cap to further improve the sealing of the micro-cavity structure.
[0051] Combination Figure 3 The present invention also discloses a method for preparing a high-sensitivity resonant differential pressure sensor, comprising:
[0052] Step S1: using dry etching of the SOI wafer, etching the device layer 71 of the SOI to form a resonator layer structure; specifically: etching the single crystal silicon device layer of the SOI wafer to form a resonator 2, an anchor point 4 and an electrode 6; an electrode 6 is provided on each side of the width of the resonator 2, and a separation groove extending along the length direction of the resonator 2 is formed between the electrode 6 and the resonator 2; an anchor point 4 is connected to each end of the length of the resonator 2, and the two anchor points 4 are located on opposite sides of the electrode 6, and an isolation groove connected to the separation groove is formed between the anchor point 4 and the electrode 6, and the isolation groove includes a first isolation groove 81 connected to the separation groove and a second isolation groove 82 connected to the other end of the first isolation groove 81, and the groove width of the second isolation groove 82 is greater than the first isolation groove 81;
[0053] Step S2: using low-pressure chemical vapor deposition to deposit a first layer of silicon dioxide on the surface of the SOI wafer, and allowing the first layer of silicon dioxide to fill the etched isolation groove; the method is to use low-pressure chemical vapor deposition to deposit a layer of tetraethoxysilane on the surface of the SOI wafer, and the tetraethoxysilane is decomposed into silicon dioxide and then deposited on the surface of the resonator, and the thickness of the deposited silicon dioxide is 1um to 2um.
[0054] Specifically, in step S2, a layer of tetraethoxysilane (TEOS) is deposited on the surface by low-pressure chemical vapor deposition. TEOS can be decomposed into silicon dioxide and then deposited on the surface of the resonator. The thickness of the silicon dioxide deposited in this step is required to achieve good step coverage, with a thickness of 1 to 2 um, covering the SOI device layer and the etched first isolation groove 81 and the second isolation groove 82; since the resonant beam maintains a small distance from the electrodes 6 on both sides, there may be the following inside the first isolation groove 81: Figure 4 The void 9 shown is also the main problem that the existing packaging method cannot achieve local packaging. At the same time, because the second isolation groove 82 is wider and has a lower aspect ratio, tetraethoxysilane (TEOS) decomposition can be used to well coat a layer of silicon oxide in the isolation groove 2 and its side, so this special structural design can achieve sealing of the end face of the first isolation groove 81 (although there are a small number of voids 9 inside).
[0055] Step S3: Patterning the first layer of silicon dioxide, etching a groove on the periphery of the resonator, the etched peripheral area of the first layer of silicon dioxide covers the second isolation groove to ensure that the first isolation groove is not etched; thereby defining a sacrificial layer area of the first layer of silicon dioxide to prevent excessive drilling corrosion during the release process of the resonator 2, but at the same time, the sacrificial layer area must ensure that the sealing of the junction between the second isolation groove and the first isolation groove is not destroyed.
[0056] Step S4: Using low pressure chemical vapor deposition, deposit a first layer of polysilicon on the surface of the first layer of silicon dioxide. The first layer of polysilicon fills and fills the grooves etched in step S3 and is connected to the electrode, thereby connecting the SOI device layer, and serves as a silicon oxide barrier layer during the release of step S10, so that the silicon dioxide release can stop laterally and prevent the side drilling from being too large during the release, and is used to control the size of the microcavity. Therefore, the thickness of the deposition should not be too low, and the thickness should be greater than 2um, otherwise the groove cannot be filled, and the polysilicon capping finally formed is not thick enough and the strength is not strong enough. It should not be too thick, generally less than 5um, and the opening formed in step S4 has a large depth-to-width ratio, which is not conducive to release. In order to achieve electrical insulation between the electrodes, the deposited polysilicon should be in an intrinsic high-resistance state or be inversely doped with the SOI device layer to form a depletion layer. The main purpose is to insulate the deposited polysilicon from the single crystal silicon of the device layer to prevent electrical connection between the electrodes through the polysilicon, which would cause a short circuit. The method of electrical insulation is to deposit polysilicon in an intrinsic high-resistance state, that is, undoped polysilicon, which has a relatively high resistivity and is approximately insulating. Alternatively, polysilicon that is anti-doped to the single crystal silicon of the device layer will form a depletion layer between the two, which can also avoid a short circuit.
[0057] Step S5: patterning and etching the first layer of polysilicon directly above the resonator to etch a plurality of groups of release holes (small holes) or groove structures distributed along the length direction of the resonator above the resonator, the release holes or groove structures being connected to the first layer of silicon dioxide deposited in step S2; the release holes (small holes) or groove structures reaching the deposited first layer of silicon dioxide, the repeated release holes or groove structures being evenly distributed along the length direction of the resonant beam, maintaining a certain interval, to ensure that the subsequent HF (hydrogen fluoride) can be evenly released to the entire resonant beam;
[0058] Step S6: using low pressure chemical vapor deposition, depositing a second layer of silicon dioxide on the surface of the first layer of polysilicon, the second layer of silicon dioxide fills the release holes and connects to the first layer of silicon dioxide; the thickness of the second layer of silicon dioxide needs to comprehensively consider the HF release time in step S9 and the blocking effect of polysilicon deposition in step S10, and is generally 0.5um to 1um;
[0059] Step S7: patterning and etching the second layer of silicon dioxide on both sides of the width of the resonator, so as to etch through holes distributed along the length direction of the resonator and penetrating the second layer of silicon dioxide above the resonator and on both sides of the straight line where the multiple groups of release holes are located; specifically, the through holes are small holes etched at equal intervals along the length direction of the resonator above the resonator (on both sides of the release holes formed in step S5), and the small holes are located on one side of the straight line where the release holes are located, and are used to form support points for the shielding layer in step S9;
[0060] Step S8: using low pressure chemical vapor deposition, depositing a second layer of polysilicon on the surface of the second layer of silicon dioxide, wherein the second layer of silicon dioxide is connected or communicated with the first layer of polysilicon through the through hole etched in step S7;
[0061] Step S9: Patterning and etching the second layer of polysilicon to the second layer of silicon dioxide until it stops, leaving a portion of the second layer of polysilicon above the resonator to form a shielding layer above the resonator; the shielding layer needs to reach a certain width, otherwise the polysilicon deposited in step S11 will easily enter the sealed cavity of the resonance beam, causing the resonance beam to fail.
[0062] Step S10: Use gaseous hydrofluoric acid to etch the exposed second layer of silicon dioxide, and etch the silicon dioxide around the resonator through the gap between the shielding layer and the first layer of polysilicon and the release hole to release the resonator, until the silicon dioxide layer on the side and below the resonator 2 is completely etched. In this step, since the first layer of polysilicon is connected to the SOI layer, it can effectively prevent the first layer of silicon oxide from excessive side drilling, effectively control the side drilling amount, realize the microcavity structure, and help improve the high static pressure tolerance of the sensor;
[0063] Step S11: Deposit the third layer of polysilicon in a near-vacuum environment using low-pressure chemical vapor deposition to seal the resonator. The thickness of the third layer of polysilicon can seal the holes exposed after the silicon dioxide is etched, thus completing the sealing of the resonator 2. It should be noted that the shielding layer is used to prevent the third layer of polysilicon from entering the resonator microcavity and causing structural failure, and in order to achieve vacuum, it is necessary to deposit under vacuum conditions, using H 2 The oxidizing gas in the deposition furnace tube is exhausted, and then pure SiH 4 The polysilicon is deposited by using a gas, so that the reaction product gas is only H 2 .
[0064] Step S12: etching the multilayer polysilicon and silicon dioxide on both sides of the width of the resonator by dry etching and / or wet etching until the upper surface of the SOI wafer is exposed, that is, until the silicon of the SOI device layer is exposed;
[0065] Step S13: high temperature annealing. The annealing temperature of the high temperature annealing is 950°C to 1050°C, preferably 1000°C, so that the residual H in the resonator sealed cavity is 2 Diffusion overflow, reaching high vacuum, annealing time is selected according to the actual need for vacuum. Generally, the longer the time, the higher the vacuum;
[0066] Step S14: using low pressure chemical vapor deposition to deposit a layer of silicon nitride on the surface of the cover to protect the interface and improve the sealing performance of the film;
[0067] Step S15: Dry / wet etching of silicon nitride to expose the single crystal silicon on the surface of the electrode, and evaporating metal on the electrode to form a metal pad.
[0068] It should be noted that in the entire process, polysilicon can be alternately deposited to form thicker polysilicon, providing sufficient structural strength to prevent the vacuum chamber from rupturing and failing under the action of atmospheric pressure.
[0069] according to Figure 4 , Figure 5 Explanation of local encapsulation and its sealing: When the preparation method of the high-sensitivity resonant differential pressure sensor provided by the present invention seals the groove etched in step S1, as the low-pressure chemical vapor deposition (LPCVD) process proceeds, the silicon dioxide deposited on the sidewalls of the slit will gradually become thicker until the entire groove is filled. However, it should be noted that the deposition rate is not ideally consistent everywhere, which will result in voids at the junction of the silicon dioxide deposited on both sides, resulting in sealing failure. Figure 5 As shown, the present invention adopts a first isolation groove 81 and a second isolation groove 82 with different widths through structural design, so that the width of the groove to be sealed is narrowed from wide, so that a layer of silicon dioxide can be completely covered at the outlet of the first isolation groove 81, and the micro-voids inside the first isolation groove 81 are sealed. Therefore, a smaller packaging size can be used to achieve a better packaging effect, and partial packaging can be completed, such as Figure 4 shown.
[0070] In addition, in some embodiments, if the length of the resonant beam is small, a first gaseous hydrofluoric acid etching of the oxide at the bottom of the resonator can be performed between step S1 and step S2 to release the resonator, which also falls within the scope of the present invention. The shapes of the small holes etched in step S5 and step S7 can be different, generally circular holes or square holes, as long as they meet the pattern array arranged with equal spacing, they fall within the scope of the present invention.
[0071] The LPCVD process described in this solution can also be replaced by an epitaxial process. The packaging method can also be combined with a wafer bonding process to achieve the packaging and preparation of absolute pressure sensors, gauge pressure sensors, etc.
[0072] In summary, the present invention has the following beneficial effects:
[0073] (1) By using polysilicon for packaging, the resonator package size can be effectively controlled, the thickness of the capping layer can be thinner and more accurately controlled, which can further reduce the chip area, have a higher single wafer yield, and improve the sensitivity of the pressure sensor chip;
[0074] (2) High efficiency of single packaging, which can realize multiple wafer processing;
[0075] (3) The support and shielding structure can avoid the problems of resonator adhesion and excess deposition caused by polysilicon sealing, and achieve precise control of the resonator frequency;
[0076] (4) In step S11, silicon epitaxy and SiH 4 As process gas, avoid the problem of low vacuum caused by residual non-escapable gas.
[0077] (5) In step S3 and step S4, the lateral self-stop structure of the release is realized by opening silicon oxide windows and depositing polysilicon, which can prevent the first layer of silicon dioxide from being over-drilled during the release process in step S10, causing the upper cover to collapse and rupture, thereby improving the static pressure tolerance of the differential pressure sensor and having a higher range ratio.
[0078] (6) Using local packaging and reducing the package size can significantly reduce static pressure errors and improve sensor performance.
[0079] (7) Vacuum packaging of polysilicon can effectively solve the problems of low wafer bonding yield and low wafer bonding packaging efficiency in vacuum packaging solutions of silicon-glass / silicon-silicon bonding;
[0080] (8) The thickness of thin film deposition is precisely controlled by low-pressure chemical vapor deposition, and the side drilling amount of the capping layer is controlled by process design and structural design to achieve good sealing of the vacuum cavity, thereby achieving partial encapsulation of the resonant beam, effectively reducing the static pressure error of the sensor and improving the measurement accuracy of the sensor;
[0081] (9) This scheme can be used not only for vacuum packaging of micro differential pressure sensors, but also for resonator packaging of absolute pressure sensors. Based on the aforementioned process scheme, a vacuum reference cavity is formed by bonding packaging on the other side of the chip or by depositing a thick polysilicon epitaxial layer through an epitaxial process, thereby forming an absolute pressure sensor.
[0082] Please note that the technical features of the above embodiments can be combined arbitrarily. In order to make the description concise, all possible combinations of the technical features in the above embodiments are not described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification. The above embodiments only express several implementation methods of the present application, and their descriptions are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that for ordinary technicians in this field, without departing from the concept of the present application, several variations and improvements can be made, which all belong to the scope of protection of the present application. Therefore, the scope of protection of the patent in this application shall be based on the attached claims.
[0083] The above are preferred embodiments of the present invention. It should be pointed out that, for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principles of the present invention. These improvements and modifications should also be regarded as within the scope of protection of the present invention.
Claims
1. A method for preparing a highly sensitive resonant differential pressure sensor, characterized in that: include: Step S1: dry-etching an SOI wafer, etching a single crystal silicon device layer of the SOI wafer to form a resonator, an anchor point and an electrode; one electrode is disposed on each of the two width sides of the resonator, and a separation groove extending along the length direction of the resonator is formed between the electrode and the resonator; one anchor point is connected to each of the two length ends of the resonator, and the two anchor points are located on opposite sides of the electrode, and an isolation groove interconnected with the separation groove is formed between the anchor point and the electrode, and the isolation groove includes a first isolation groove interconnected with the separation groove and a second isolation groove connected to the other end of the first isolation groove, and the groove width of the second isolation groove is greater than that of the first isolation groove; Step S2: using a low pressure chemical vapor deposition method, depositing a first layer of silicon dioxide on the surface of the SOI wafer, and allowing the first layer of silicon dioxide to fill the etched isolation groove; Step S3: patterning the first silicon dioxide layer, etching a groove on the periphery of the resonator, and the etched periphery of the first silicon dioxide layer covers the second isolation groove; Step S4: depositing a first layer of polysilicon on the surface of the first layer of silicon dioxide by low pressure chemical vapor deposition, wherein the first layer of polysilicon fills the groove etched in step S3 and is connected to the electrode; Step S5: patterning and etching the first layer of polysilicon directly above the resonator to etch a plurality of groups of release holes distributed along the length direction of the resonator above the resonator, wherein the release holes are connected to the first layer of silicon dioxide deposited in step S2; Step S6: using low pressure chemical vapor deposition to deposit a second layer of silicon dioxide on the surface of the first layer of polysilicon, wherein the second layer of silicon dioxide fills the release holes and connects to the first layer of silicon dioxide; Step S7: patterning and etching the second layer of silicon dioxide on both sides of the width of the resonator, so as to etch through holes distributed along the length direction of the resonator and penetrating the second layer of silicon dioxide above the resonator and on both sides of the straight line where the plurality of groups of release holes are located; Step S8: depositing a second layer of polysilicon on the surface of the second layer of silicon dioxide by low pressure chemical vapor deposition, wherein the second layer of silicon dioxide is connected to the first layer of polysilicon through the through hole etched in the step S7; Step S9: patterning and etching the second layer of polysilicon to the second layer of silicon dioxide, leaving a portion of the second layer of polysilicon above the resonator to form a shielding layer above the resonator; Step S10: etching the exposed second silicon dioxide layer, and etching the silicon dioxide around the resonator through the gap between the shielding layer and the first polysilicon layer and the release hole to release the resonator; Step S11: depositing a third layer of polysilicon in a vacuum environment using a low-pressure chemical vapor deposition method to complete the sealing of the resonator.
2. The method for preparing a highly sensitive resonant differential pressure sensor according to claim 1, characterized in that: The preparation method further comprises: Step S12: etching multiple layers of polysilicon and silicon dioxide on both sides of the width of the resonator until the upper surface of the SOI wafer is exposed; Step S13: performing high temperature annealing.
3. The method for preparing a highly sensitive resonant differential pressure sensor according to claim 2, characterized in that: The preparation method further comprises: Step S14: using low pressure chemical vapor deposition to deposit a layer of silicon nitride on the surface of the cover.
4. The method for preparing a highly sensitive resonant differential pressure sensor according to claim 3, characterized in that: The preparation method further comprises: Step S15: etching silicon nitride by dry / wet etching to expose the single crystal silicon on the surface of the electrode, and evaporating metal on the electrode to form a metal pad.
5. The method for preparing a high-sensitivity resonant differential pressure sensor according to any one of claims 1 to 4, characterized in that: In the step S2, the method of depositing a first layer of silicon dioxide on the surface of the SOI wafer by using a low pressure chemical vapor deposition method, and allowing the first layer of silicon dioxide to fill the etched isolation groove includes: A layer of tetraethoxysilane is deposited on the surface of the SOI wafer by using a low-pressure chemical vapor deposition method. The tetraethoxysilane is decomposed into silicon dioxide and then deposited on the surface of the resonator. The thickness of the deposited silicon dioxide is 1um to 2um.
6. The method for preparing a high-sensitivity resonant differential pressure sensor according to any one of claims 1 to 4, characterized in that: The thickness of the first layer of polysilicon deposited in step S4 is greater than 2 um and less than 5 um.
7. The method for preparing a high-sensitivity resonant differential pressure sensor according to any one of claims 1 to 4, characterized in that: In the step S10 , etching the exposed second silicon dioxide layer, and etching the silicon dioxide around the resonator through the gap between the shielding layer and the first polysilicon layer and the release hole to release the resonator includes: etching silicon dioxide using gaseous hydrofluoric acid.
8. The method for preparing a highly sensitive resonant differential pressure sensor according to any one of claims 2 to 4, characterized in that The method of etching the multilayer polysilicon and silicon dioxide in step S12 includes: Dry etching and / or wet etching.
9. The method for preparing a high-sensitivity resonant differential pressure sensor according to any one of claims 2 to 4, characterized in that: In step S13, the annealing temperature of the high temperature annealing is 950° C. to 1050° C.; And / or the thickness of the second silicon dioxide layer is 0.5 um to 1 um.
10. A highly sensitive resonant differential pressure sensor, comprising a sensor chip, characterized in that: The sensor chip is manufactured by the preparation method of the high-sensitivity resonant differential pressure sensor according to any one of claims 1 to 9.