Detection method for judging position of crack on surface of hot-rolled round steel
By setting marks on the hot-rolled round steel samples and splitting them for pickling and docking, the location of the cracks on the surface of the hot-rolled round steel can be accurately judged, which solves the problems of inaccurate judgment and heavy workload in the existing technology, and realizes heat transfer. Accurate analysis of surface cracks in rolled round steel.
Patent Information
- Application Number
- CN202410828983.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-25
- Publication Date
- 2024-10-01
AI Technical Summary
It is difficult to accurately determine the location of cracks on the surface of hot-rolled round steel with the existing technology, and existing methods such as pickling the surface of the entire round steel or metallographic inspection of the full-section round steel require a large workload and cannot retain the original characteristics of the cracks.
By setting marks in the round steel sample to be inspected, it is divided into a first section and a second section of the sample. The first section of the sample is pickled to expose the crack location, and then the pickled first section of the sample is Butt it with the unpickled second section sample, determine the surface crack location of the second section sample based on the marks, and conduct metallographic analysis.
This method can accurately find the location of cracks on the surface of hot-rolled round steel, retain the original characteristics of the cracks, and avoid the problems of the entire pickling method being unable to guarantee the characteristics and the heavy workload of full-section metallographic inspection. It is suitable for long-term components that are difficult to identify after surface oxidation. Strip workpiece.
Smart Images

Figure CN118730655A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of hot-rolled round steel surface crack detection, and more specifically, relates to a detection method for determining the position of a hot-rolled round steel surface crack. Background Art
[0002] Whether there are cracks on the surface of hot-rolled round steel is mainly tested by hot upsetting test of hot-rolled round steel. The hot upsetting qualified rate is an important indicator reflecting the surface quality of hot-rolled round steel. How the surface cracks of hot-rolled round steel are generated is usually analyzed by sampling the cracks of the hot upsetting specimen for metallographic analysis, observing the metallographic structure, decarburization layer and inclusions around the cracks, to determine whether it is caused by unreasonable steelmaking or rolling process. However, in the upsetting test after the hot-rolled round steel is heated, the upsetting crack destroys the metallographic structure, decarburization layer and inclusions around the cracks of the specimen after heating. The analysis of the cracks in the upsetting test of hot-rolled round steel often leads to misjudgment of the cause of the cracks, which is not conducive to improving the steelmaking and rolling process. Therefore, it is very important to develop an effective sampling method, that is, to take metallographic samples at the cracks directly on the hot-rolled round steel, for accurately analyzing the causes of the cracks. However, without upsetting, the sample cannot guarantee the accurate location of the surface cracks of the hot-rolled round steel.
[0003] The existing technology is to confirm the surface crack position by pickling the surface of the whole round steel or metallographic inspection of the whole section round steel, but the whole round steel surface pickling method cannot guarantee the original characteristics of the crack, and the full section round steel metallographic inspection method is labor-intensive and cannot be operated. How to determine the surface crack position of hot-rolled round steel has become a technical problem that needs to be solved in this field. Summary of the invention
[0004] The purpose of the present invention is to provide a detection method for determining the position of surface cracks of hot-rolled round steel in view of the deficiencies of the prior art, so as to solve the problem that the prior art cannot accurately determine the position of surface cracks of hot-rolled round steel.
[0005] In order to achieve the above object, the present invention provides a detection method for determining the position of surface cracks of hot-rolled round steel, the method comprising:
[0006] Set marks on the round steel specimens to be tested;
[0007] The round steel sample to be tested is divided into a first section sample and a second section sample, so that at least part of the mark is retained on the surface of the first section sample and the second section sample;
[0008] The first section of the sample is pickled to expose its surface cracks and retain at least a portion of the mark;
[0009] The pickled first section sample and the second section sample are butted together according to the marks, and the position of the surface crack of the second section sample is determined according to the position of the surface crack exposed on the first section sample;
[0010] Based on the location of the cracks on the surface of the second section sample, metallographic analysis was performed on the second section sample.
[0011] The marking of the round steel sample to be tested includes:
[0012] Two marks are set along the axial direction on the middle surface of the round steel sample to be tested, and the two marks are located on the same straight line.
[0013] The distance between the two marks is 20 mm.
[0014] The mark is a concave structure hammered into the surface of the round steel sample to be tested.
[0015] The round steel sample to be tested is cut into the first section and the second section along the marked middle position by cold sawing.
[0016] The first section of the sample was pickled with hydrochloric acid aqueous solution.
[0017] The volume ratio of the hydrochloric acid aqueous solution is 1:1.
[0018] The temperature for surface pickling is 70°C to 80°C.
[0019] The surface pickling time is 30 minutes.
[0020] The surface pickling of the first section sample further comprises:
[0021] Take out the first section of the sample after pickling from the acid tank, rinse it with clean water, and then blow it dry.
[0022] The present invention provides a detection method for judging the position of surface cracks of hot-rolled round steel, and its beneficial effect is that: the method sets a mark on the round steel sample to be detected, divides the round steel sample to be detected into a first section sample and a second section sample at the mark, the first section sample is pickled, and the second section sample is not pickled, the first section sample after pickling is docked with the second section sample that is not pickled according to the mark, and the position of the surface crack of the second section sample is judged according to the position of the surface crack of the first section sample, so as to accurately prepare a metallographic inspection sample at the crack position, perform metallographic analysis on the surface crack of the hot-rolled round steel, provide technical support for solving product quality problems, and avoid the problem that the whole section round steel surface pickling method cannot guarantee the original characteristics of the crack, and the full section round steel metallographic inspection method has a large workload and cannot be operated. The method is particularly suitable for long strip workpieces whose crack positions are difficult to identify after surface oxidation, and has good versatility and reliability.
[0023] Other features and advantages of the present invention will be described in detail in the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] The above and other objects, features and advantages of the present invention will become more apparent through a more detailed description of exemplary embodiments of the present invention in conjunction with the accompanying drawings, wherein like reference numerals generally represent like components throughout the exemplary embodiments of the present invention.
[0025] Figure 1 A flow chart of a detection method for determining the position of surface cracks of hot-rolled round steel according to an embodiment of the present invention is shown.
[0026] Figure 2 One of the schematic principle diagrams of a detection method for determining the position of surface cracks of hot-rolled round steel according to an embodiment of the present invention is shown.
[0027] Figure 3 A second schematic principle diagram of a detection method for determining the position of surface cracks on hot-rolled round steel according to an embodiment of the present invention is shown.
[0028] Figure 4 A third schematic principle diagram of a detection method for determining the position of surface cracks on hot-rolled round steel according to an embodiment of the present invention is shown.
[0029] Figure 5 A fourth schematic principle diagram of a detection method for determining the position of surface cracks on hot-rolled round steel according to an embodiment of the present invention is shown.
[0030] Figure 6 A fifth schematic principle diagram of a detection method for determining the position of surface cracks on hot-rolled round steel according to an embodiment of the present invention is shown.
[0031] Description of reference numerals:
[0032] 1. Round steel sample to be tested; 2. First section of the sample; 3. Second section of the sample; 4. Surface cracks; 5. Marking. DETAILED DESCRIPTION
[0033] The preferred embodiments of the present invention will be described in more detail below. Although the preferred embodiments of the present invention are described below, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided to make the present invention more thorough and complete, and to fully convey the scope of the present invention to those skilled in the art.
[0034] See also Figure 1-6 The present invention provides a detection method for determining the position of surface cracks of hot-rolled round steel, the method comprising:
[0035] like Figure 2 As shown, a mark 5 is set on the round steel sample 1 to be tested;
[0036] like Figure 3 As shown, the round steel sample 1 to be tested is divided into a first section sample 2 and a second section sample 3, so that at least part of the mark 5 is retained on the surface of the first section sample 2 and the second section sample 3;
[0037] like Figure 4 , 5 As shown, the first section of the sample 2 is pickled to expose its surface cracks 4 and retain at least part of the mark 5;
[0038] like Figure 6 As shown, the pickled first section sample 2 and the second section sample 3 are butted together according to the mark 5, and the position of the surface crack 4 of the second section sample 3 is determined according to the position of the surface crack 4 exposed on the first section sample 2;
[0039] Based on the location of the crack 4 on the surface of the second section sample 3, a metallographic analysis is performed on the second section sample 3.
[0040] Specifically, although the pickling method for the entire round steel surface can expose the surface crack position, it cannot guarantee the original characteristics of the crack. Therefore, in this embodiment, the round steel sample 1 to be tested is divided into two sections, the first section sample 2 is pickled to show the crack position, and the second section sample 3 is not pickled to retain the original characteristics of the crack. After pickling, the two sections are butt-jointed, which can find the crack position and retain the original characteristics of the crack. Mark 5 can ensure the accurate position of the first section sample 2 and the second section sample 3 when they are butt-jointed.
[0041] Further, setting a mark 5 on the round steel sample 1 to be tested includes:
[0042] Two marks 5 are arranged along the axial direction on the middle surface of the round steel sample 1 to be tested, and the two marks 5 are located on the same straight line.
[0043] Specifically, the round steel sample 1 to be tested is segmented according to the center line of the two marks 5. After segmentation, the two marks 5 are respectively located on the surface of the first section sample 2 and the second section sample 3, providing a reference for the docking process after pickling. Optionally, a mark 5 can also be set, and the segmentation is performed at the center of the mark 5. After segmentation, a part of the mark 5 is located on the surface of the first section sample 2, and the other part is located on the surface of the second section sample 3. The shape and size of the mark 5 are not limited, as long as it can provide a reference for the docking process.
[0044] Furthermore, the distance between the two marks 5 is 20 mm. Specifically, if the distance between the two marks 5 is too large, the docking will be inaccurate; if the distance between the two marks 5 is too close, the marks 5 will be damaged during cutting; practice has proved that the distance between the two marks 5 of 20 mm can ensure accurate docking and ensure that the marks 5 are not damaged during cutting.
[0045] Furthermore, the mark (5) is a concave structure hammered on the surface of the round steel sample (1) to be tested. In this embodiment, the two marks 5 are "1", which are hammered on the surface of the round steel sample 1 to be tested by a hammering machine. The "1"-shaped mark 5 is linear, which can ensure the accuracy of the docking position during docking. The hammering machine is a commonly used equipment in the workshop, and the "1" hammering mark is also commonly used in the workshop, which is easy to implement.
[0046] Furthermore, the round steel sample 1 to be tested is sawn along the middle position of the mark 5 into the first section sample 2 and the second section sample 3 by cold sawing. Specifically, practice has proved that the cold sawing method does not affect the material properties of the round steel sample 1 to be tested, and can retain the original characteristics of the crack.
[0047] Furthermore, the first section sample 2 was pickled with a hydrochloric acid aqueous solution.
[0048] Specifically, the pickling method can be hot pickling or cold pickling. Hot pickling can be used for hot-rolled round steel with a thicker surface oxide layer, and cold pickling can be used for workpieces with a shallower oxide layer.
[0049] Furthermore, the volume ratio of hydrochloric acid to water is 1:1.
[0050] Furthermore, the surface pickling temperature is 70°C to 80°C.
[0051] Furthermore, the surface pickling time is 30 minutes.
[0052] Furthermore, the surface pickling of the first section sample 2 further includes:
[0053] The first section of sample 2 after pickling is taken out from the acid tank, first rinsed with clean water, and then blown dry with high-pressure argon gas.
[0054] The embodiments of the present invention have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those skilled in the art without departing from the scope and spirit of the described embodiments.
Claims
1. A method for determining the location of surface cracks on hot-rolled round steel, characterized in that: The method includes: Setting a mark (5) on the round steel sample (1) to be tested; The round steel sample (1) to be tested is divided into a first sample section (2) and a second sample section (3), so that at least a portion of the mark (5) is retained on the surface of both the first sample section (2) and the second sample section (3); The first section of the sample (2) is pickled to expose the surface cracks (4) and retain at least a portion of the mark (5); The first section sample (2) and the second section sample (3) after pickling are butted together according to the mark (5), and the position of the surface crack (4) of the second section sample (3) is determined based on the position of the surface crack (4) exposed on the first section sample (2); Based on the position of the crack (4) on the surface of the second section sample (3), a metallographic analysis test is performed on the second section sample (3).
2. A method for determining the location of surface cracks on hot-rolled round steel according to claim 1, characterized in that: The marking (5) for the round steel sample (1) to be tested comprises: Two marks (5) are arranged along the axial direction on the middle surface of the round steel sample (1) to be tested, and the two marks (5) are located on the same straight line.
3. A method for determining the location of surface cracks on hot-rolled round steel according to claim 2, characterized in that: The distance between the two marks (5) is 20 mm.
4. A method for determining the location of surface cracks on hot-rolled round steel according to claim 2 or 3, characterized in that: The mark (5) is a recessed structure hammered into the surface of the round steel sample (1) to be tested.
5. A method for determining the location of surface cracks on hot-rolled round steel according to claim 1, characterized in that: The round steel sample (1) to be tested is sawn along the middle position of the mark (5) into a first section sample (2) and a second section sample (3) by cold sawing.
6. A method for determining the location of surface cracks on hot-rolled round steel according to claim 1, characterized in that: The first section sample (2) was pickled with a hydrochloric acid aqueous solution.
7. A method for determining the location of surface cracks on hot-rolled round steel according to claim 6, characterized in that: The volume ratio of the hydrochloric acid aqueous solution is 1:
1.
8. A method for determining the location of surface cracks on hot-rolled round steel according to claim 7, characterized in that: The temperature for surface pickling is 70°C to 80°C.
9. A method for determining the location of surface cracks on hot-rolled round steel according to claim 8, characterized in that: The surface pickling time is 30 minutes.
10. A method for determining the location of surface cracks on hot-rolled round steel according to claim 6, characterized in that: The surface pickling of the first section sample (2) further comprises: The first section of sample (2) after pickling is taken out from the acid tank, rinsed with clean water, and then blown dry.
Citation Information
Cited By
Metallographic inspection characteristic structure position positioning device and method
CN122109088A
Method for detecting surface crack defect of round steel covered by oxide scale
CN122671457A
Round steel central area micro-defect positioning and analysis sample preparation method
CN122709494A