Method and system for detecting damage of external anticorrosive coating of horizontal directional drilling crossing pipeline

By combining the internal and external inspection data of the pipeline to evaluate the damage to the external anti-corrosion layer of the pipeline traversed by horizontal directional drilling, the problem of difficulty in detecting damage to the external anti-corrosion layer of HDD pipelines with existing technology is solved, achieving safe operation and extending the service life of the pipeline.

CN118730876APending Publication Date: 2024-10-01PIPECHINA SOUTH CHINA CO
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411012075.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Existing technology is difficult to effectively detect damage to the external anti-corrosion layer of horizontal directional drilling pipelines, especially when the burial depth is large and the formation is complex. Existing external detection methods such as ACVG and DCVG are difficult to apply to HDD pipelines with large burial depths.

Method used

By combining the internal inspection data of the pipeline bidding section and the external inspection data of conventional shallow-buried pipelines, the difference in external corrosion distribution data is determined, the degree of damage to the external anti-corrosion layer of the pipeline penetrated by horizontal directional drilling is evaluated, and the processing module and detection module are used to perform defect detection. Obtain the damage detection results of the outer anti-corrosion layer.

Benefits of technology

It achieves accurate assessment of the damage to the outer anti-corrosion layer of the pipeline penetrated by horizontal directional drilling, ensuring the safe operation of the pipeline and extending its service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118730876A_ABST
    Figure CN118730876A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of oil and gas long-distance pipeline anticorrosion detection, and particularly discloses a horizontal directional drilling crossing pipeline outer anticorrosion layer damage detection method and system.The method comprises the steps that first external corrosion distribution data of a horizontal directional drilling crossing pipeline are determined according to internal detection data of the horizontal directional drilling crossing pipeline on a pipeline section, determining second external corrosion distribution data of the conventional shallow buried pipeline according to the internal detection data of the conventional shallow buried pipeline on the pipeline section; based on the difference between the first external corrosion distribution data and the second external corrosion distribution data, determining the damage degree of an outer anticorrosive coating of the horizontal directional drilling crossing pipeline, and performing defect detection on the horizontal directional drilling crossing pipeline according to the internal detection data and the damage degree of the outer anticorrosive coating of the horizontal directional drilling crossing pipeline. And obtaining a damage detection result of the outer anti-corrosion layer of the horizontal directional drilling crossing pipeline. Safe operation of the pipeline can be guaranteed, and the service life of the pipeline is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Background Art

[0002] Horizontal Directional Drilling (HDD) is an efficient trenchless laying technology for buried pipelines. During the construction of HDD pipelines, the outer anti-corrosion layer is often scratched and worn due to the influence of underground rock layers, and even the metal matrix is ​​exposed. This damage not only affects the long-term operation of the pipeline, but also increases the risk of pipeline corrosion.

[0003] HDD pipelines are buried deep, pass through complex strata, and are usually inaccessible from above. Currently, there is no effective external detection method to evaluate the damage of their anti-corrosion coating. For newly built pipelines, the feeding method can be used to test the average conductivity of the HDD pipeline coating, thereby indirectly evaluating the overall quality of the HDD anti-corrosion layer. However, this method cannot determine whether there is a large area of ​​anti-corrosion layer damage or peeling on the HDD pipeline. For in-service pipelines, existing external detection methods such as ACVG and DCVG technology are difficult to apply to HDD pipelines with larger burial depths.

[0004] Therefore, it is urgent to provide a technical solution to solve the above problems. Summary of the invention

[0005] In order to solve the above technical problems, the present invention provides a method and system for detecting damage of the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed.

[0006] In the first aspect, the present invention provides a method for detecting damage of an outer anti-corrosion layer of a pipeline through horizontal directional drilling, and the technical scheme of the method is as follows:

[0007] Determine first external corrosion distribution data of the pipeline traversed by the horizontal directional drilling according to internal detection data of the pipeline traversed by the horizontal directional drilling on the pipeline section, and determine second external corrosion distribution data of the conventional shallow buried pipeline according to internal detection data of the conventional shallow buried pipeline on the pipeline section;

[0008] Based on the difference between the first external corrosion distribution data and the second external corrosion distribution data, the degree of damage of the outer anti-corrosion layer of the horizontal directional drilling pipeline is determined, and according to the internal detection data of the horizontal directional drilling pipeline and the degree of damage of the outer anti-corrosion layer, the horizontal directional drilling pipeline is subjected to defect detection to obtain the detection result of damage of the outer anti-corrosion layer of the horizontal directional drilling pipeline.

[0009] The beneficial effects of the method for detecting damage of the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed according to the present invention are as follows:

[0010] The method of the present invention evaluates and detects damage defects of the outer anti-corrosion layer of the pipeline passed by the horizontal directional drill through the pipeline through the detection data in the pipeline, which can ensure the safe operation of the pipeline and extend its service life.

[0011] On the basis of the above scheme, the method for detecting damage of the outer anti-corrosion layer of a pipeline through horizontal directional drilling of the present invention can also be improved as follows.

[0012] In an optional manner, the method further includes:

[0013] The internal detection data of the pipeline section is obtained, and the internal detection data of the horizontal directional drilling crossing the pipeline is determined in combination with the pipeline mileage information, pipeline wall thickness information and crossing pipeline width information of the horizontal directional drilling crossing the pipeline.

[0014] In an optional manner, the first external corrosion distribution data includes: the first external metal corrosion quantity ratio and the first maximum corrosion depth of the horizontal directional drilling pipeline; the second external corrosion distribution data includes: the second external metal corrosion quantity ratio and the second maximum corrosion depth of the conventional shallow buried pipeline.

[0015] In an optional manner, based on the difference between the first external corrosion distribution data and the second external corrosion distribution data, the step of determining the degree of damage to the external anti-corrosion layer of the horizontal directional drilling through the pipeline includes:

[0016] Based on a first difference between the first external metal corrosion quantity ratio and the second external metal corrosion quantity ratio and a second difference between the first maximum corrosion depth and the second second maximum corrosion depth, the degree of damage to the external anti-corrosion layer of the horizontal directional drilling pipeline is determined.

[0017] In an optional manner, the external anti-corrosion layer damage detection result includes: the clock direction of external metal corrosion, the defect concentrated distribution area and the external metal corrosion morphology.

[0018] In the second aspect, the present invention provides a system for detecting damage of an outer anti-corrosion layer of a pipeline through horizontal directional drilling, and the technical solution of the system is as follows:

[0019] It includes: a processing module and a detection module;

[0020] The processing module is used to: determine first external corrosion distribution data of the pipeline traversed by the horizontal directional drilling according to the internal detection data of the pipeline traversed by the horizontal directional drilling on the pipeline section, and determine second external corrosion distribution data of the conventional shallow buried pipeline according to the internal detection data of the conventional shallow buried pipeline on the pipeline section;

[0021] The detection module is used to: determine the degree of damage of the outer anti-corrosion layer of the horizontal directional drilling pipeline based on the difference between the first external corrosion distribution data and the second external corrosion distribution data, and perform defect detection on the horizontal directional drilling pipeline based on the internal detection data of the horizontal directional drilling pipeline and the degree of damage of the outer anti-corrosion layer, so as to obtain the detection result of damage of the outer anti-corrosion layer of the horizontal directional drilling pipeline.

[0022] The beneficial effects of the damage detection system for the outer anti-corrosion layer of a horizontal directional drill through a pipeline of the present invention are as follows:

[0023] The system of the present invention evaluates and detects damage defects of the outer anti-corrosion layer of the pipeline passed by the horizontal directional drill through the pipeline through the detection data in the pipeline, which can ensure the safe operation of the pipeline and extend its service life.

[0024] On the basis of the above scheme, the damage detection system of the outer anti-corrosion layer of a horizontal directional drilling pipeline of the present invention can also be improved as follows.

[0025] In an optional manner, the method further includes: an acquisition module; the acquisition module is used to:

[0026] The internal detection data of the pipeline section is obtained, and the internal detection data of the horizontal directional drilling crossing the pipeline is determined in combination with the pipeline mileage information, pipeline wall thickness information and crossing pipeline width information of the horizontal directional drilling crossing the pipeline.

[0027] In an optional manner, the first external corrosion distribution data includes: the first external metal corrosion quantity ratio and the first maximum corrosion depth of the horizontal directional drilling pipeline; the second external corrosion distribution data includes: the second external metal corrosion quantity ratio and the second maximum corrosion depth of the conventional shallow buried pipeline.

[0028] In a third aspect, a technical solution of an electronic device of the present invention is as follows:

[0029] The invention comprises a memory, a processor and a program stored in the memory and running on the processor. When the processor executes the program, the steps of the method for detecting damage of an outer anti-corrosion layer of a pipeline when horizontal directional drilling is passed through are implemented as described in the present invention.

[0030] In a fourth aspect, the present invention provides a computer-readable storage medium having the following technical solution:

[0031] Instructions are stored in the computer-readable storage medium. When the computer-readable storage medium reads the instructions, the computer-readable storage medium executes the steps of the method for detecting damage of the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed according to the present invention.

[0032] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention, it can be implemented according to the contents of the specification. In order to make the above and other purposes, features and advantages of the present invention more obvious and easy to understand, the specific implementation methods of the present invention are listed below. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] The accompanying drawings are only used to illustrate the embodiments and are not to be considered as limiting the present invention. In addition, the same reference symbols are used to represent the same components throughout the accompanying drawings. In the accompanying drawings:

[0034] Figure 1 A schematic flow chart of an embodiment of a method for detecting damage of an outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed according to the present invention;

[0035] Figure 2 It is a structural schematic diagram of an embodiment of a system for detecting damage of an outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed;

[0036] Figure 3 The figure is a schematic structural diagram of an embodiment of an electronic device of the present invention. DETAILED DESCRIPTION

[0037] Exemplary embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present invention are shown in the drawings, it should be understood that the present invention can be implemented in various forms and should not be limited to the embodiments set forth herein.

[0038] Figure 1 A flow chart of an embodiment of a method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed provided by the present invention is shown. The method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed can be executed by an electronic device such as a terminal device or a server. The terminal device can be any fixed or mobile terminal such as a user equipment (UE), a mobile device, a user terminal, a terminal, a cellular phone, a cordless phone, a personal digital assistant (PDA), a handheld device, a computing device, a vehicle-mounted device, a wearable device, etc. The server can be a single server or a server cluster composed of multiple servers. Any electronic device can implement the method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed by a processor calling computer-readable instructions stored in a memory. Figure 1 As shown, the following steps are included:

[0039] S1. Determine first external corrosion distribution data of the pipeline traversed by the horizontal directional drilling according to the internal inspection data of the pipeline traversed by the horizontal directional drilling on the pipeline section, and determine second external corrosion distribution data of the conventional shallow buried pipeline according to the internal inspection data of the conventional shallow buried pipeline on the pipeline section.

[0040] Among them, the pipeline section is the oil and gas long-distance pipeline project section, with a length ranging from tens to hundreds of kilometers. Usually, a pipeline section contains multiple horizontal directional drilling pipelines. Except for the horizontal directional drilling pipelines, the rest are conventional shallow buried pipelines. The internal inspection data includes internal metal corrosion, external metal corrosion, manufacturing defects and weld defects, and can provide the maximum depth, length and width of the defects and location information.

[0041] Among them, the first external corrosion distribution data includes: the first external metal corrosion quantity ratio and the first maximum corrosion depth of the horizontal directional drilling pipeline. The second external corrosion distribution data includes: the second external metal corrosion quantity ratio and the second maximum corrosion depth of the conventional shallow buried pipeline. It should be noted that the external metal corrosion quantity ratio is the average number of external metal corrosion per 100 meters of length. For example, taking the horizontal directional drilling pipeline and the conventional shallow buried pipeline in a certain pipeline section as an example, the first external metal corrosion quantity ratio is 0.07 / 100m, the second external metal corrosion quantity ratio is 0.5 / 100m, the first maximum corrosion depth is 12%, and the second maximum corrosion depth is 25%.

[0042] S2. Based on the difference between the first external corrosion distribution data and the second external corrosion distribution data, determine the degree of damage of the external anti-corrosion layer of the horizontal directional drilling pipeline, and perform defect detection on the horizontal directional drilling pipeline according to the internal detection data of the horizontal directional drilling pipeline and the degree of damage of the external anti-corrosion layer, and obtain the detection result of damage of the external anti-corrosion layer of the horizontal directional drilling pipeline.

[0043] In S2, based on the difference between the first external corrosion distribution data and the second external corrosion distribution data, the step of determining the degree of damage to the external anti-corrosion layer of the horizontal directional drilling through the pipeline includes:

[0044] Based on a first difference between the first external metal corrosion quantity ratio and the second external metal corrosion quantity ratio and a second difference between the first maximum corrosion depth and the second maximum corrosion depth, the degree of damage to the external anti-corrosion layer of the horizontal directional drilling traversal pipeline is determined.

[0045] Among them, the degree of damage to the external anti-corrosion layer is determined based on the difference in the external metal corrosion quantity ratio and the maximum corrosion depth between the horizontal directional drilling pipeline and the conventional shallow buried pipeline. In the above example, the degree of damage to the external anti-corrosion layer of the horizontal directional drilling pipeline is better than that of the conventional shallow buried pipeline, and the maximum corrosion depth of the horizontal directional drilling pipeline is less than the maximum corrosion depth of the external anti-corrosion layer of the conventional shallow buried pipeline. The results of the external anti-corrosion layer damage detection include: the clock direction of external metal corrosion, the concentrated distribution area of ​​defects, and the external metal corrosion morphology.

[0046] It should be noted that, taking the horizontal directional drilling crossing a long distance across a large river as an example, based on the internal inspection data of the horizontal directional drilling crossing the pipeline and the degree of damage to the external anti-corrosion layer, the clock direction of the external metal corrosion of the horizontal directional drilling crossing the pipeline, the defect concentration distribution area and the external metal corrosion morphology are analyzed. Determine whether there are scratches and damage patterns on the external anti-corrosion layer, identify the long strip defects of the damaged anti-corrosion layer, and analyze the possible causes of these defects (such as whether the damage to the anti-corrosion layer is caused by scratches caused by external forces during the crossing process). For example, through internal inspection data, it was found that the external corrosion points of a horizontal directional drilling crossing pipeline were concentrated at the clock position of 11:45 and were long strips. It is speculated that this was caused by scratches on the anti-corrosion layer during the backhaul process.

[0047] In an optional manner, the method further includes:

[0048] The internal detection data of the pipeline section is obtained, and the internal detection data of the horizontal directional drilling crossing the pipeline is determined in combination with the pipeline mileage information, pipeline wall thickness information and crossing pipeline width information of the horizontal directional drilling crossing the pipeline.

[0049] Among them, the pipeline mileage information is the ground mileage information of the pipeline. The ground mileage information is determined by HDD construction drawings and GPS coordinates, and the internal detection data mileage is obtained through the detection report provided by the internal detection tool. The width information of the crossing pipeline is obtained through HDD construction drawings or field survey data. By comparing the ground mileage information with the mileage information in the internal detection data, the specific location of the horizontal directional drilling crossing the pipeline can be determined. The pipe wall thickness information of the horizontal directional drilling crossing pipeline is usually greater than the pipe wall thickness of the conventional shallow buried pipeline. According to the wall thickness change of the horizontal directional drilling crossing pipeline in the crossing area, the possible internal detection data of the horizontal directional drilling crossing pipeline can be further screened. Since there is a significant difference between the crossing pipe width information of the horizontal directional drilling crossing pipeline and the crossing pipe width information of the conventional shallow buried pipeline, combined with the parameters such as the width of the river crossed by the horizontal directional drilling crossing pipeline, the part of the internal detection data of the pipeline section related to the horizontal directional drilling crossing pipeline is finally determined, thereby obtaining the internal detection data of the horizontal directional drilling crossing pipeline.

[0050] The technical solution of this embodiment evaluates and detects damage defects of the outer anti-corrosion layer of the pipeline through which the horizontal directional drill passes through by using the detection data inside the pipeline, which can ensure the safe operation of the pipeline and extend its service life.

[0051] Figure 2 FIG. 2 is a schematic diagram showing a structure of an embodiment of a horizontal directional drilling pipeline outer anti-corrosion layer damage detection system 200 provided by the present invention. Figure 2 As shown, the system 200 includes: a processing module 210 and a detection module 220;

[0052] The processing module 210 is used to: determine the first external corrosion distribution data of the pipeline traversed by the horizontal directional drilling according to the internal detection data of the pipeline traversed by the horizontal directional drilling on the pipeline section, and determine the second external corrosion distribution data of the conventional shallow buried pipeline according to the internal detection data of the conventional shallow buried pipeline on the pipeline section;

[0053] The detection module 220 is used to: determine the degree of damage of the outer anti-corrosion layer of the horizontal directional drilling pipeline based on the difference between the first external corrosion distribution data and the second external corrosion distribution data, and perform defect detection on the horizontal directional drilling pipeline according to the internal detection data of the horizontal directional drilling pipeline and the degree of damage of the outer anti-corrosion layer, so as to obtain the detection result of damage of the outer anti-corrosion layer of the horizontal directional drilling pipeline.

[0054] In an optional manner, the method further includes: an acquisition module; the acquisition module is used to:

[0055] The internal detection data of the pipeline section is obtained, and the internal detection data of the horizontal directional drilling crossing the pipeline is determined in combination with the pipeline mileage information, pipeline wall thickness information and crossing pipeline width information of the horizontal directional drilling crossing the pipeline.

[0056] In an optional manner, the first external corrosion distribution data includes: the first external metal corrosion quantity ratio and the first maximum corrosion depth of the horizontal directional drilling pipeline; the second external corrosion distribution data includes: the second external metal corrosion quantity ratio and the second maximum corrosion depth of the conventional shallow buried pipeline.

[0057] In an optional manner, the step of determining the degree of damage of the outer anti-corrosion layer of the horizontal directional drilling through the pipeline based on the difference between the first external corrosion distribution data and the second external corrosion distribution data in the detection module 220 includes:

[0058] Based on a first difference between the first external metal corrosion quantity ratio and the second external metal corrosion quantity ratio and a second difference between the first maximum corrosion depth and the second second maximum corrosion depth, the degree of damage to the external anti-corrosion layer of the horizontal directional drilling pipeline is determined.

[0059] In an optional manner, the external anti-corrosion layer damage detection result includes: the clock direction of external metal corrosion, the defect concentrated distribution area and the external metal corrosion morphology.

[0060] The technical solution of this embodiment evaluates and detects damage defects of the outer anti-corrosion layer of the pipeline through which the horizontal directional drill passes through by using the detection data inside the pipeline, which can ensure the safe operation of the pipeline and extend its service life.

[0061] The above-mentioned parameters and steps of each module to implement corresponding functions in the horizontal directional drilling through the pipeline outer anti-corrosion layer damage detection system 200 of this embodiment can refer to the parameters and steps in the above embodiment of the horizontal directional drilling through the pipeline outer anti-corrosion layer damage detection method, and will not be repeated here.

[0062] like Figure 3 As shown, an electronic device 300 of an embodiment of the present invention includes a processor 320, the processor 320 is coupled to a memory 310, and the memory 310 stores at least one computer program 330, and the at least one computer program 330 is loaded and executed by the processor 320, so that the electronic device 300 implements any of the above-mentioned methods for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling passes through. Specifically:

[0063] The electronic device 300 may have relatively large differences due to different configurations or performances, and may include one or more processors 320 (Central Processing Units, CPU) and one or more memories 310, wherein the one or more memories 310 store at least one computer program 330, and the at least one computer program 330 is loaded and executed by the one or more processors 320, so that the electronic device 300 implements any of the horizontal directional drilling through the pipeline outer anti-corrosion layer damage detection methods provided in the above embodiments. Of course, the electronic device 300 may also have components such as a wired or wireless network interface, a keyboard, and an input and output interface for input and output, and the electronic device 300 may also include other components for implementing device functions, which will not be repeated here.

[0064] A computer-readable storage medium according to an embodiment of the present invention stores at least one computer program, and the at least one computer program is loaded and executed by a processor so that a computer implements any of the above-mentioned methods for detecting damage to an outer anti-corrosion layer of a pipeline when drilling horizontally.

[0065] Optionally, the computer-readable storage medium may be a read-only memory (ROM), a random access memory (RAM), a compact disc (CD-ROM), a magnetic tape, a floppy disk, an optical data storage device, and the like.

[0066] In an exemplary embodiment, a computer program product or a computer program is also provided, the computer program product or the computer program including computer instructions, the computer instructions being stored in a computer-readable storage medium. A processor of an electronic device reads the computer instructions from the computer-readable storage medium, and the processor executes the computer instructions, so that the electronic device executes any of the above-mentioned methods for detecting damage to an outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed.

[0067] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application are used to distinguish similar objects and represent the definition of a specific order or sequence. The order of use of similar objects can be interchanged where appropriate, so that the embodiments of the present application described herein can be implemented in an order other than the order shown or described.

[0068] Those skilled in the art know that the present invention can be implemented as a system, method or computer program product. Therefore, the present disclosure can be specifically implemented in the following forms, namely: it can be complete hardware, it can be complete software (including firmware, resident software, microcode, etc.), or it can be a combination of hardware and software, which is generally referred to as "circuit", "module" or "system" herein. In addition, in some embodiments, the present invention can also be implemented in the form of a computer program product in one or more computer-readable media, and the computer-readable medium contains computer-readable program code.

[0069] Any combination of one or more computer-readable media can be used. Computer-readable media can be computer-readable signal media or computer-readable storage media. Computer-readable storage media can be, for example, but not limited to, electrical, magnetic, optical, electromagnetic, infrared, or semiconductor systems, devices or devices, or any combination of the above. More specific examples of computer-readable storage media (a non-exhaustive list) include: an electrical connection with one or more wires, a portable computer disk, a hard disk, a random access memory (RAM), a read-only memory (ROM), an erasable programmable read-only memory (EPROM or flash memory), an optical fiber, a portable compact disk read-only memory (CD-ROM), an optical storage device, a magnetic storage device, or any suitable combination of the above. In the present application, a computer-readable storage medium can be any tangible medium containing or storing a program, which can be used by an instruction execution system, device or device or used in combination with it.

[0070] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present invention.

Claims

1. A method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed, characterized in that: include: Determining first external corrosion distribution data of the pipeline traversed by the horizontal directional drilling according to internal inspection data of the pipeline traversed by the horizontal directional drilling on the pipeline section, and determining second external corrosion distribution data of the conventional shallow buried pipeline according to internal inspection data of the conventional shallow buried pipeline on the pipeline section; Based on the difference between the first external corrosion distribution data and the second external corrosion distribution data, the degree of damage of the external anti-corrosion layer of the horizontal directional drilling pipeline is determined, and according to the internal detection data of the horizontal directional drilling pipeline and the degree of damage of the external anti-corrosion layer, the horizontal directional drilling pipeline is subjected to defect detection to obtain the external anti-corrosion layer damage detection result of the horizontal directional drilling pipeline.

2. The method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed according to claim 1, characterized in that: Also includes: The internal detection data of the pipeline section is obtained, and the internal detection data of the horizontal directional drilling crossing the pipeline is determined in combination with the pipeline mileage information, pipeline wall thickness information and crossing pipeline width information of the horizontal directional drilling crossing the pipeline.

3. The method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed according to claim 1, characterized in that: The first external corrosion distribution data includes: the first external metal corrosion quantity ratio and the first maximum corrosion depth of the horizontal directional drilling pipeline; the second external corrosion distribution data includes: the second external metal corrosion quantity ratio and the second maximum corrosion depth of the conventional shallow buried pipeline.

4. The method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed according to claim 3, characterized in that: The step of determining the degree of damage to the outer anti-corrosion layer of the pipeline traversed by the horizontal directional drilling based on the difference between the first outer corrosion distribution data and the second outer corrosion distribution data comprises: Based on a first difference between the first external metal corrosion quantity ratio and the second external metal corrosion quantity ratio and a second difference between the first maximum corrosion depth and the second second maximum corrosion depth, the degree of damage to the external anti-corrosion layer of the horizontal directional drilling traversal pipeline is determined.

5. The method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed according to any one of claims 1 to 4, characterized in that: The damage detection results of the external anti-corrosion layer include: the clock direction of the external metal corrosion, the defect concentrated distribution area and the external metal corrosion morphology.

6. A horizontal directional drilling pipeline outer anti-corrosion layer damage detection system, characterized in that: include: Processing module and detection module; The processing module is configured to determine first external corrosion distribution data of the pipeline traversed by the horizontal directional drilling according to internal inspection data of the pipeline traversed by the horizontal directional drilling on the pipeline section, and determine second external corrosion distribution data of the conventional shallow buried pipeline according to internal inspection data of the conventional shallow buried pipeline on the pipeline section; The detection module is used to: determine the degree of damage of the outer anti-corrosion layer of the horizontal directional drilling traversal pipeline based on the difference between the first external corrosion distribution data and the second external corrosion distribution data, and perform defect detection on the horizontal directional drilling traversal pipeline based on the internal detection data of the horizontal directional drilling traversal pipeline and the degree of damage of the outer anti-corrosion layer, and obtain the detection result of damage of the outer anti-corrosion layer of the horizontal directional drilling traversal pipeline.

7. The horizontal directional drilling pipeline outer anti-corrosion layer damage detection system according to claim 6 is characterized in that: Also includes: Acquisition module; the acquisition module is used to: The internal detection data of the pipeline section is obtained, and the internal detection data of the horizontal directional drilling crossing the pipeline is determined in combination with the pipeline mileage information, pipeline wall thickness information and crossing pipeline width information of the horizontal directional drilling crossing the pipeline.

8. The horizontal directional drilling pipeline outer anti-corrosion layer damage detection system according to claim 6 is characterized in that: The first external corrosion distribution data includes: the first external metal corrosion quantity ratio and the first maximum corrosion depth of the horizontal directional drilling pipeline; the second external corrosion distribution data includes: the second external metal corrosion quantity ratio and the second maximum corrosion depth of the conventional shallow buried pipeline.

9. An electronic device, characterized in that: The electronic device includes a processor, which is coupled to a memory. The memory stores at least one computer program, and the at least one computer program is loaded and executed by the processor so that the electronic device can implement the method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed as described in any one of claims 1 to 5.

10. A computer-readable storage medium, characterized in that The computer-readable storage medium stores at least one computer program, which is loaded and executed by the processor so that the computer-readable storage medium implements the method for detecting damage to the outer anti-corrosion layer of a pipeline when horizontal directional drilling is performed as described in any one of claims 1 to 5.