Touch screen sensor and manufacturing method thereof
By adding a metal micro-break anti-fool mechanism and a through-hole structure in the production process of touch screen sensors, the problem of micro-breaks in metal traces is solved, the reliability and life of the product are improved, and the yield rate and user experience are improved.
Patent Information
- Application Number
- CN202410872161.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-01
- Publication Date
- 2024-10-01
AI Technical Summary
Existing touch screen sensors are prone to micro-breaks in metal traces, resulting in poor functionality. Due to their instability and concealment, they may fail before shipment, on the client side, or during use, affecting yield, cost control, and user experience.
During the production process, a metal micro-break prevention mechanism is added. By forming a sandwich structure between the metal wiring layers and setting a through-hole structure on the first ITO layer, a reliable protective layer is formed to avoid micro-breaks and isolation of the metal wiring. Air and water are in contact to prevent oxidation, and exhaust is used to prevent bubbling.
It effectively avoids poor functionality caused by micro-breaks in metal traces, improves product reliability and lifespan, improves yield rate and user experience, and reduces costs.
Smart Images

Figure CN118732884A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of touch technology, and in particular to a touch screen sensor and a manufacturing method thereof. Background Art
[0002] Touch screens are widely used in mobile phones, wearable devices, industrial applications, automotive applications, and other terminal displays. As products become more diverse and thinner, users are demanding higher performance.
[0003] Touchscreen sensors, a key component of touch screens, are functional boards equipped with touchscreen patterns. Currently, touchscreen sensors are prone to minor metal trace breaks. These micro-breaks disrupt the channel, causing poor touchscreen functionality. Due to the unstable, random, and hidden nature of these micro-breaks, products may fail before shipment, at the customer end, or even during market use. Consequently, these failures not only impact product yield and cost control, but also shorten product lifespan and reduce user experience.
[0004] Based on this, how to design a touch screen sensor that can avoid functional defects caused by micro-breaks in metal traces has become an urgent problem to be solved in the industry. Summary of the Invention
[0005] In order to solve at least one problem existing in the prior art, the purpose of this application is to provide a touch screen sensor and a process method thereof. By adding a metal micro-breakage anti-mistake mechanism during the manufacturing process and forming a reliable protective layer for the metal wiring, functional defects caused by metal wiring micro-breakage can be effectively avoided, thereby helping to improve the yield rate, reduce costs, and help extend product life and enhance user experience.
[0006] To achieve the above-mentioned purpose, the present application provides a touch screen sensor, wherein the screen surface includes a touch area and a frame area; the touch screen sensor includes a transparent substrate and the following components formed successively on the transparent substrate:
[0007] The first ITO layer forms a bridge pattern for connecting the X electrodes in the touch area; and forms a routing pattern corresponding to the metal routing in the frame area; wherein the routing pattern is provided with a plurality of through holes;
[0008] The metal wiring layer includes a plurality of pillar structures and a layer structure; wherein the layer structure is located above the wiring pattern of the first ITO layer, and the plurality of pillar structures penetrate and match the plurality of through-hole arrangements;
[0009] A first insulating layer, forming an electrode insulation pattern for insulating the X electrodes from the Y electrodes in the touch area; and forming a wiring insulation pattern on the metal wiring layer in the frame area;
[0010] The second ITO layer includes an independent grid pattern constituting the X electrodes and the Y electrodes, and a border area pattern connecting the trace pattern of the first ITO layer;
[0011] The second insulating layer is at least covered on the second ITO layer.
[0012] Furthermore, a shadow elimination layer is provided on the transparent substrate.
[0013] Furthermore, the wiring insulation pattern of the first insulating layer covers the layer structure of the metal wiring layer on the first ITO layer, so that the first ITO layer, the layer structure of the metal wiring layer and the border area pattern of the second ITO layer define an insulating medium cavity that accommodates the wiring insulation pattern.
[0014] Furthermore, the thickness of the trace insulation pattern of the first insulation layer is in a range of 1.2 μm to 1.6 μm.
[0015] Furthermore, the through hole has a pore size ranging from 2 μm to 10 μm.
[0016] Furthermore, the area of the through hole on the first ITO layer accounts for 25%-35%.
[0017] The present application also provides a process method for manufacturing a touch screen sensor, which is used to manufacture the touch screen sensor as described above; the method comprises:
[0018] Preparing the first ITO layer in the corresponding areas of the bridge pattern and the wiring pattern on the transparent substrate;
[0019] Preparing the metal wiring layer on the wiring pattern of the first ITO layer;
[0020] Preparing the first insulating layer in the corresponding areas of the electrode insulation pattern and the wiring insulation pattern;
[0021] Preparing the second ITO layer in the corresponding areas of the independent grid pattern and the border area pattern;
[0022] The second insulating layer is formed at least on the second ITO layer.
[0023] Furthermore, at least one of the first ITO layer, the metal wiring layer, the first insulating layer and the second ITO layer is prepared by a method of first scraping and then exposing and developing.
[0024] Furthermore, a second insulating layer covering the screen surface of the touch screen sensor is formed by coating.
[0025] Furthermore, before the step of preparing the first ITO layer, the method further comprises preparing an image elimination layer on the surface of the substrate on which the first ITO layer is to be prepared, by using an evaporation method or a magnetron sputtering method.
[0026] The present application discloses a touch screen sensor and its manufacturing method. By placing a metal routing layer between a first ITO layer and a first insulating layer to form a sandwich structure, a metal micro-breakage prevention mechanism is added during the manufacturing process. This effectively avoids functional defects caused by metal routing micro-breaks, and the metal routing layer is protected by the first ITO layer and the first insulating layer, isolating the metal routing from contact with external air and water, preventing oxidation and improving reliability. Furthermore, the through-hole structure on the first ITO layer ensures full contact between the metal routing layer and the first ITO layer, and further enhances the metal micro-breakage prevention mechanism by venting air and preventing routing anomalies caused by bubbling. Therefore, the touch screen sensor structure helps improve yield, reduce costs, extend product life, and enhance user experience.
[0027] Other features and advantages of the present application will be set forth in the following description, and in part will be apparent from the description, or may be understood by practicing the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The accompanying drawings are used to provide a further understanding of the present application and constitute a part of the specification. Together with the embodiments of the present application, they are used to explain the present application and do not constitute a limitation of the present application. In the accompanying drawings:
[0029] Figure 1 Schematic diagram of the stacked structure of a touch screen sensor according to an embodiment of the present application;
[0030] Figure 2 Schematic diagram of the structure of a touch screen sensor according to an embodiment of the present application;
[0031] Figure 3 Schematic diagram of the regional structure of a touch screen sensor according to an embodiment of the present application;
[0032] Figure 4 Schematic diagram of a first ITO layer pattern according to an embodiment of the present application;
[0033] Figure 5 for Figure 4 A partial enlarged view of point A in the middle;
[0034] Figure 6 is a schematic diagram of a metal routing layer pattern according to an embodiment of the present application;
[0035] Figure 7 is a schematic diagram of a first insulating layer pattern according to an embodiment of the present application;
[0036] Figure 8 Schematic diagram of a second ITO layer pattern according to an embodiment of the present application;
[0037] Figure 9 is a schematic diagram of a second insulating layer pattern according to an embodiment of the present application;
[0038] Figure 10 FIG. 4 is a flow chart of a method for manufacturing a touch screen sensor according to an embodiment of the present application.
[0039] Specifically include the following reference numerals:
[0040] 100-touch screen sensor; 110-touch area; 120-frame area; 130-transparent substrate;
[0041] 10-first ITO layer; 11-bridge pattern; 12-track pattern; 13-through hole;
[0042] 20-metal routing layer; 21-layer structure; 22-pillar structure;
[0043] 30-first insulation layer; 31-electrode insulation pattern; 32-track insulation pattern;
[0044] 40 - second ITO layer; 41 - independent grid pattern; 42 - border area pattern;
[0045] 50-Second insulating layer. DETAILED DESCRIPTION
[0046] The following describes embodiments of the present application in more detail with reference to the accompanying drawings. Although certain embodiments of the present application are shown in the accompanying drawings, it should be understood that the present application can be implemented in various forms and should not be construed as limited to the embodiments described herein. Instead, these embodiments are provided to provide a more thorough and complete understanding of the present application. It should be understood that the drawings and embodiments of the present application are for illustrative purposes only and are not intended to limit the scope of protection of the present application.
[0047] As used herein, the term "including" and its variations are open-ended, i.e., "including but not limited to." The term "based on" means "based, at least in part, on." The term "one embodiment" means "at least one embodiment," the term "another embodiment" means "at least one additional embodiment," and the term "some embodiments" means "at least some embodiments." Other terms are defined in the following description.
[0048] It should be noted that the modifications of "one" and "plurality" mentioned in this application are illustrative rather than restrictive. Those skilled in the art will understand that unless the context clearly indicates otherwise, they should be understood as "one or more." "Plurality" should be understood as two or more.
[0049] Hereinafter, embodiments of the present application will be described in detail with reference to the accompanying drawings.
[0050] refer to Figures 1 to 9 As shown, the screen of the touch screen sensor 100 includes a touch area 110 and a frame area 120. In a specific example, the touch area 110 corresponds to the visible area of the display; the frame area 120 corresponds to the frame area 120 outside the visible area of the touch screen sensor 100.
[0051] The touch screen sensor 100 includes a transparent substrate 130 , and a first ITO layer 10 , a metal wiring layer 20 , a first insulating layer 30 , a second ITO layer 40 , and a second insulating layer 50 formed successively on the transparent substrate 130 .
[0052] The first ITO layer 10 forms a bridge pattern 11 for connecting X electrodes in the touch area 110 and a wiring pattern 12 corresponding to the metal wiring in the frame area 120. In addition, a plurality of through holes 13 are formed in the wiring pattern 12.
[0053] The metal wiring layer 20 includes a layer structure 21 and a plurality of pillar structures 22. The layer structure 21 is located above the wiring pattern 12 of the first ITO layer 10; and the plurality of pillar structures 22 penetrate into and match the plurality of through holes 13.
[0054] The first insulating layer 30 forms an electrode insulating pattern 31 for insulating the X electrodes from the Y electrodes in the touch area 110 , and forms a wiring insulating pattern 32 on the metal wiring layer 20 in the frame area 120 .
[0055] The second ITO layer 40 includes an independent grid pattern 41 constituting the X electrode and the Y electrode, and a border pattern 42 connecting the trace pattern 12 of the first ITO layer 10 .
[0056] The second insulating layer 50 is at least covered on the second ITO layer 40. It should be noted that the second insulating layer 50 may only cover the second ITO layer 40 or may cover the entire upper surface of the touch screen sensor 100, which is not specifically limited in this application.
[0057] It should be noted that the X and Y electrodes in the embodiment of the present application are formed by partial patterns of the first ITO layer 10 and the second ITO layer 40, respectively, in the touch area 110. Specifically, the X electrode is formed by connecting the bridge pattern 11 of the first ITO layer 10 to a portion of the independent mesh pattern of the second ITO layer 40; the Y electrode is formed by another portion of the independent mesh pattern of the second ITO layer 40. In this specific example, the X and Y electrodes in the touch area are insulated by the electrode insulation pattern 31 of the first insulation layer 30.
[0058] It is understood that the transparent substrate 130 can be a glass substrate or a transparent substrate made of other materials, and this application does not impose any specific restrictions on this. In addition, this application does not impose any specific restrictions on the specific shape of the ITO grid pattern.
[0059] In the embodiment of the present application, an image elimination layer (not shown in the figure) is further provided on the transparent substrate 130 to optimize the light transmittance and reflectivity of the substrate and achieve a better pattern elimination effect.
[0060] In the embodiment of the present application, the trace insulation pattern 32 of the first insulating layer 30 covers the layer structure 21 of the metal trace layer 20 on the first ITO layer 10, so that the first ITO layer 10, the layer structure 21 of the metal trace layer 20 and the border area pattern 42 of the second ITO layer 40 define an insulating medium cavity that accommodates the trace insulation pattern 32.
[0061] That is to say, the first ITO layer 10 and the second ITO layer 40 are conductors, which wrap the metal wiring layer 20, and the metal wiring layer 20 is also provided with an insulating medium cavity filled with the first insulating layer 30, thereby preventing the metal wiring layer 20 from being damaged by static electricity, further improving the reliability of the touch function.
[0062] Preferably, the thickness of the trace insulation pattern 32 of the first insulation layer 30 is in the range of 1.2 μm to 1.6 μm, so as to take into account the anti-static effect, material saving and space layout.
[0063] In the embodiment of the present application, the aperture range of the through hole 13 is preferably 2 μm-10 μm; further, the area of the through hole 13 on the first ITO layer 10 is preferably 25%-35%, so as to take into account both conductivity and through hole coverage.
[0064] It should be noted that in the drawings, the sizes of layers, regions, and components, as well as their relative sizes, may be exaggerated for clarity. The same or similar reference numerals throughout represent the same or similar components or components with the same or similar functions.
[0065] It should be noted that the terms "upper", "lower", "inside", "outside", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it should not be understood as a limitation on this application.
[0066] According to the touch screen sensor provided by the embodiment of the present application, by disposing the metal routing layer between the first ITO layer and the first insulating layer to form a sandwich structure, a metal micro-breakage prevention mechanism is added during the manufacturing process. This can effectively avoid functional defects caused by metal routing micro-breaks, and the metal routing layer is protected by the first ITO layer and the first insulating layer, isolating the metal routing from contact with external air and water, preventing oxidation, and improving reliability. In addition, the through-hole structure on the first ITO layer, on the one hand, allows the metal routing layer to fully contact the first ITO layer; on the other hand, the through-hole structure can also act as an exhaust, preventing bubbling from causing routing abnormalities, thereby further strengthening the metal micro-breakage prevention mechanism. As a result, this touch screen sensor structure helps to improve the yield rate, reduce costs, and is conducive to extending product life and improving user experience.
[0067] The present application also provides a process method for manufacturing a touch screen sensor, which is used to manufacture the touch screen sensor in the above embodiment. Figure 10 As shown, the process method includes the following steps:
[0068] In step 601, a first ITO layer 10 is prepared on the transparent substrate 130 in the corresponding areas of the bridge pattern 11 and the trace pattern 12. Figure 4-Figure 5 shown.
[0069] In step 602, a metal wiring layer 20 is prepared on the wiring pattern 12 of the first ITO layer 10, such as Figure 6 shown.
[0070] In step 603, a first insulating layer 30 is formed in the corresponding areas of the electrode insulating pattern 31 and the wiring insulating pattern 32. Figure 7 shown.
[0071] In step 604, a second ITO layer 40 is prepared in the corresponding areas of the independent grid pattern 41 and the border area pattern 42. Figure 8 shown.
[0072] In step 605, a second insulating layer 50 is prepared at least on the second ITO layer 40. Preferably, the second insulating layer 50 covering the screen surface of the touch screen sensor 100 is formed by coating. Figure 9 shown.
[0073] It should be noted that the second insulating layer covering the entire screen surface can be prepared by coating methods such as scraping and spraying, or by other applicable methods, and this application does not impose any specific restrictions on this.
[0074] In the embodiment of the present application, at least one of the first ITO layer, the metal trace layer, the first insulating layer, and the second ITO layer can be formed by a method of first scraping, then exposing and developing. It is understood that the first ITO layer, the metal trace layer, the first insulating layer, and the second ITO layer can also be formed using other applicable methods, and this application does not impose specific limitations on this.
[0075] Furthermore, before the step of preparing the first ITO layer, the method further comprises preparing an image elimination layer on the surface of the substrate where the first ITO layer is to be prepared, by using an evaporation method or a magnetron sputtering method.
[0076] It should be noted that the explanation of the touch screen sensor in the above embodiment is also applicable to the manufacturing method of the touch screen sensor in the above embodiment, and will not be repeated here.
[0077] In summary, the touch screen sensor and its fabrication method according to the embodiments of the present application sequentially fabricate a first ITO layer, a metal trace layer, a first insulating layer, a second ITO layer, and a second insulating layer, and provide multiple through-hole structures in the trace pattern of the first ITO layer. This adds a metal micro-breakage prevention mechanism during the fabrication process and forms a reliable protective layer for the metal traces. This effectively prevents functional defects caused by metal trace micro-breaks, thereby improving product yields, reducing costs, extending product life, and enhancing the user experience.
[0078] It should be understood that although the steps in the flowcharts of the accompanying drawings are shown in sequence as indicated by the arrows, these steps are not necessarily executed in the order indicated by the arrows. Unless otherwise specified herein, there is no strict order restriction on the execution of these steps, and these steps can be executed in other orders. Moreover, at least a portion of the steps in the flowcharts may include multiple sub-steps or multiple stages, and these sub-steps or stages are not necessarily executed at the same time, but can be executed at different times. The execution order of these sub-steps or stages is not necessarily sequential, but can be executed in turn or alternately with other steps or at least a portion of the sub-steps or stages of other steps.
[0079] Those skilled in the art will understand that the above are merely preferred embodiments of the present application and are not intended to limit the present application. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein with equivalents. Any modifications, equivalent replacements, improvements, etc. made within the spirit and principles of the present application shall be included within the scope of protection of the present application.
Claims
1. A touch screen sensor, characterized in that: The screen surface of the touch screen sensor includes a touch area and a frame area; the touch screen sensor includes a transparent substrate and the following components formed successively on the transparent substrate: The first ITO layer forms a bridge pattern for connecting the X electrodes in the touch area; forms a routing pattern corresponding to the metal routing in the frame area; wherein a plurality of through holes are provided on the routing pattern; A metal wiring layer, comprising a plurality of pillar structures and a layer structure; wherein the layer structure is located above the wiring pattern of the first ITO layer, and the plurality of pillar structures penetrate into and match the plurality of through-hole settings; A first insulating layer, forming an electrode insulating pattern for insulating the X electrode from the Y electrode in the touch control area; and forming a wiring insulating pattern on the metal wiring layer in the frame area; A second ITO layer includes an independent grid pattern constituting an X electrode and a Y electrode, and a border area pattern connecting the routing pattern of the first ITO layer; The second insulating layer is at least covered on the second ITO layer.
2. The touch screen sensor according to claim 1, characterized in that: The transparent substrate is also provided with an image elimination layer.
3. The touch screen sensor according to claim 1, characterized in that: The wiring insulation pattern of the first insulation layer covers the layer structure of the metal wiring layer on the first ITO layer, so that the first ITO layer, the layer structure of the metal wiring layer and the border area pattern of the second ITO layer define an insulating medium cavity accommodating the wiring insulation pattern.
4. The touch screen sensor according to claim 3, characterized in that: The thickness of the wiring insulation pattern of the first insulation layer is in the range of 1.2 μm to 1.6 μm.
5. The touch screen sensor according to claim 1, characterized in that: The through hole has a pore size ranging from 2 μm to 10 μm.
6. The touch screen sensor according to claim 5, characterized in that: The area of the through hole on the first ITO layer accounts for 25%-35%.
7. A process method for manufacturing a touch screen sensor, characterized in that: Used to manufacture a touch screen sensor as described in any one of claims 1-6; the method comprises: Preparing the first ITO layer in the corresponding areas of the bridge pattern and the wiring pattern on the transparent substrate; Preparing the metal wiring layer on the wiring pattern of the first ITO layer; Preparing the first insulating layer in the corresponding areas of the electrode insulating pattern and the wiring insulating pattern; Preparing the second ITO layer in the corresponding areas of the independent grid pattern and the border area pattern; The second insulating layer is formed at least on the second ITO layer.
8. The method according to claim 7, characterized in that At least one of the first ITO layer, the metal wiring layer, the first insulating layer and the second ITO layer is prepared by a method of first scraping and then exposing and developing.
9. The method according to claim 7, characterized in that: A second insulating layer covering the screen surface of the touch screen sensor is formed by coating.
10. The method according to any one of claims 7 to 9, characterized in that: Before the step of preparing the first ITO layer, the method further comprises: On the surface of the substrate where the first ITO layer is to be formed, an evaporation method or a magnetron sputtering method is used to form an erasing layer.