Production process of nanocrystalline iron core of electric reactor
By detecting imaging equipment and grayscale histogram analysis, combined with the coating analysis model, the problem of quality detection of nanocrystalline soft magnetic coating and the influence of abnormal surface sub-regions is solved, efficient coating process parameter adjustment is achieved, and the quality of nanocrystalline soft magnetic coating is improved. Uniformity and stability of soft magnetic products.
Patent Information
- Application Number
- CN202410740039.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-07
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-06-07
AI Technical Summary
The existing technology is difficult to quickly detect and adjust the coating quality of nanocrystalline soft magnets, especially in the case of different shapes, sizes and surface properties, and cannot effectively avoid the impact of abnormal surface sub-regions before coating on the coating process, resulting in Failures may occur after coating.
Obtain the grayscale histogram of nanocrystalline soft magnets through detection imaging equipment, calculate the uniformity coefficient and the influence signal of abnormal surface sub-regions, establish a coating analysis model, and adjust process parameters to ensure the uniformity and consistency of the coating effect and adapt to different conditions. Shapes and sizes of nanocrystalline soft magnets.
It improves the uniformity and consistency of nanocrystalline soft magnetic coating, significantly improves the reliability and stability of the product, detects and handles potential problems in a timely manner, avoids adverse effects during the coating process, and enhances the coating quality and product durability. Overall performance.
Smart Images

Figure CN118737675A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of coating processes, and in particular to a production process for a nanocrystalline iron core of a reactor. Background Art
[0002] With the continuous development of power electronics technology, electronic components such as power transformers and inductors have higher and higher requirements for magnetic core materials. Traditional magnetic core materials have deficiencies in magnetic induction intensity, magnetic permeability loss, operating temperature range, etc., and it is difficult to meet the needs of high-performance electronic components. Nanocrystalline iron cores, as a new type of high-performance electronic component material, have the advantages of high saturation magnetic induction intensity, low magnetic permeability loss, wide temperature range and high dimensional stability. Therefore, the research on their production process is of great significance; however, in the production process of nanocrystalline iron cores, the coating process of the curing agent has an important influence on the performance of the iron core.
[0003] However, in the prior art, in the curing agent coating process, it is not possible to quickly detect the coating quality of nanocrystalline soft magnetic materials of different shapes, sizes and surface characteristics, and it is also not possible to use a coating analysis model to accurately calculate the process parameters based on the abnormal surface sub-areas existing before coating to avoid similar abnormalities after coating. Summary of the invention
[0004] The purpose of the present invention is to provide a production process of a nanocrystalline core of a reactor to solve the technical problems in the above background.
[0005] The purpose of the present invention can be achieved through the following technical solutions:
[0006] The present invention provides a production process for a reactor nanocrystalline core, comprising the following steps: raw material preparation, rapid solidification preparation, heat treatment, and curing treatment, wherein the curing treatment comprises the following steps:
[0007] The coating process of the nanocrystalline soft magnetic curing agent subjected to the curing treatment is detected to determine the coating process parameters, and the specific method includes the following steps:
[0008] Step 1: During the coating process, the nanocrystalline soft magnetic material is tested to obtain the test data;
[0009] Among them, the test data include: uniformity coefficient;
[0010] Step 2: Based on the detection data of nanocrystalline soft magnetism, the coating effect is evaluated and a coating effect signal is generated;
[0011] Step 3: Analyze whether the abnormal surface sub-region before nanocrystalline soft magnetic coating will affect the coating process, and generate a signal affecting the coating process;
[0012] The signals affecting the coating process include: signals affecting the coating process and signals not affecting the coating process;
[0013] Step 4: Based on the signal that affects the coating process, the coating process is regulated according to the abnormal surface sub-region before the nanocrystalline soft magnetic coating. The specific process is as follows:
[0014] Based on the signals that affect the coating process, a coating analysis model is established according to the abnormal surface sub-region before coating, the abnormal surface sub-region after coating and the process parameters of the coating process;
[0015] In the subsequent process, the abnormal surface sub-region before coating of the nanocrystalline soft magnetic material to be coated and the grayscale absolute deviation value HP of the abnormal surface sub-region are obtained. 待 , and based on the coating analysis model, obtain the new process parameters GY 新 , where HP 阈 is the grayscale absolute deviation threshold.
[0016] As a further solution of the present invention: the process of obtaining the uniformity coefficient is:
[0017] After the nanocrystalline soft magnetic material is coated with a curing agent, a detection imaging device is used to obtain a grayscale histogram of the nanocrystalline soft magnetic material, and based on the grayscale value, the nanocrystalline soft magnetic surface is divided into multiple regions to obtain surface sub-regions; according to the grayscale values of all surface sub-regions, the grayscale characterization average ratio and the grayscale uniform value are calculated, the grayscale characterization average ratio and the grayscale uniform value are summed and calculated, and the uniformity coefficient is output.
[0018] As a further solution of the present invention: the process of obtaining the grayscale characterization average ratio is:
[0019] Obtain the grayscale values and area ratios of all surface sub-regions, multiply the grayscale values by the area ratios of the corresponding surface sub-regions, and output the grayscale representation values of each surface sub-region; then average the grayscale representation values of all surface sub-regions and output the grayscale representation mean; calculate the ratio of the grayscale representation mean to the standard grayscale representation mean and output the grayscale representation mean ratio;
[0020] The process of obtaining the area ratio is as follows: obtaining the area of the surface sub-region, calculating the ratio of the surface sub-region area to the total area of the nanocrystalline soft magnetic surface, and outputting the area ratio.
[0021] As a further solution of the present invention: the process of obtaining the grayscale uniform value is:
[0022] The grayscale value is calculated to be different from the standard grayscale value, and the grayscale deviation value is output. The absolute value of the grayscale deviation value is marked as the grayscale absolute deviation value. The grayscale absolute deviation value is compared with the grayscale absolute deviation threshold. When the grayscale absolute deviation value is greater than the grayscale absolute deviation threshold, a grayscale abnormality signal is generated, and the surface sub-region corresponding to the grayscale abnormality signal is marked as an abnormal surface sub-region. The grayscale difference value and the grayscale deviation total parameter are obtained, and the grayscale difference value is multiplied by the grayscale deviation total parameter to output the grayscale uniform value.
[0023] As a further solution of the present invention: the grayscale difference acquisition process is:
[0024] Based on all surface sub-regions, the difference between the maximum grayscale deviation value and the minimum grayscale deviation value in all surface sub-regions is calculated, and the grayscale difference is output.
[0025] As a further solution of the present invention: the process of obtaining the total grayscale deviation parameter is as follows:
[0026] Based on the abnormal surface sub-region, the grayscale absolute deviation value of each surface sub-region is obtained, and the grayscale absolute deviation value is multiplied by the area ratio of the corresponding surface sub-region to output the grayscale deviation parameter of each abnormal surface sub-region; all grayscale deviation parameters are summed up and the total grayscale deviation parameter is output.
[0027] As a further solution of the present invention: the specific process of generating the coating effect signal is:
[0028] The coating effect signal includes: coating qualified signal and coating unqualified signal;
[0029] Compare and analyze the uniformity coefficient with the uniformity coefficient threshold;
[0030] If the uniformity coefficient is ≥ the uniformity coefficient threshold, a coating failure signal is generated;
[0031] If the uniformity coefficient is less than the uniformity coefficient threshold, a coating qualified signal is generated.
[0032] As a further solution of the present invention: the specific process of generating the signal affecting the coating process is:
[0033] Before the nanocrystalline soft magnetic material is coated with a curing agent, an abnormal surface sub-region before the nanocrystalline soft magnetic material is coated is obtained; the abnormal surface sub-region before coating and the abnormal surface sub-region after coating are analyzed to obtain an abnormal overlap area ratio, and the abnormal overlap area ratio is compared with the abnormal overlap area ratio;
[0034] If the abnormal overlap area ratio is less than the abnormal overlap area, a signal affecting the coating process is generated;
[0035] If the abnormal overlap area ratio ≥ the abnormal overlap area, a signal affecting the coating process is generated.
[0036] As a further solution of the present invention: the process of obtaining the abnormal overlap area ratio is:
[0037] Based on the abnormal surface sub-region before coating and the abnormal surface sub-region after coating of the nanocrystalline soft magnetic material, the abnormal overlap area is obtained; the abnormal overlap area ratio YMB is obtained by calculation.
[0038] As a further solution of the present invention: the establishment process of the coating analysis model is:
[0039] Based on multiple unqualified coated nanocrystalline soft magnetic materials, modeling data of each unqualified coated nanocrystalline soft magnetic material is obtained respectively; a coating analysis model is preset; the modeling data of all unqualified coated nanocrystalline soft magnetic materials are substituted into the preset coating analysis model, a1, a2 and a3 are calculated and obtained, and the coating analysis model is obtained.
[0040] Beneficial effects of the present invention:
[0041] (1) The present invention obtains the grayscale histogram of nanocrystalline soft magnetic material by detecting imaging equipment, and calculates the uniformity coefficient; compares and analyzes the uniformity coefficient with a preset uniformity coefficient threshold, thereby evaluating the coating effect and generating a coating effect signal; ensures the uniformity and consistency of the surface coating of the nanocrystalline soft magnetic material, and improves the reliability and stability of the product; uses image processing technology and grayscale histogram analysis, so as to adapt to the coating quality detection of nanocrystalline soft magnetic materials with different shapes, sizes and surface characteristics;
[0042] (2) The present invention uses detection imaging equipment to obtain abnormal surface sub-regions during the nanocrystalline soft magnetic coating process and before and after coating, and by calculating the abnormal overlap area ratio, it is determined whether the abnormal surface sub-region before coating has an impact on the coating process, and a corresponding signal affecting the coating process is generated; through precise detection and evaluation steps, the uniformity and consistency of the nanocrystalline soft magnetic coating are effectively guaranteed, thereby significantly improving the overall performance and stability of the product. More importantly, through the identification and analysis of the abnormal surface sub-region before coating, potential coating problems can be discovered in time, and corresponding treatment measures can be taken before coating, thereby effectively avoiding the adverse effects of these problems on the coating process, and further improving the coating quality and product reliability;
[0043] (3) The present invention establishes a coating analysis model by conducting an in-depth analysis of the abnormal surface sub-regions before and after coating and combining the coating process parameters (such as coating pressure); the model can predict the abnormalities that may occur after coating and adjust the coating process parameters accordingly; specifically, when an abnormal surface sub-region is detected before coating, the coating analysis model is used to accurately calculate how to adjust the process parameters to avoid similar abnormalities after coating; the present invention not only improves the accuracy and controllability of the coating process, but also significantly enhances the quality and stability of the nanocrystalline soft magnetic coating products, providing strong technical support for the production of high-quality nanocrystalline soft magnetic products. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] The present invention will be further described below in conjunction with the accompanying drawings.
[0045] Figure 1 is a flowchart of Embodiment 2 of the present invention;
[0046] Figure 2 is a flowchart of Embodiment 3 of the present invention;
[0047] Figure 3 is a flowchart of Embodiment 4 of the present invention;
[0048] Figure 4 It is a system block diagram of embodiment 5 of the present invention. DETAILED DESCRIPTION
[0049] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0050] Embodiment 1:
[0051] A production process for a reactor nanocrystalline core according to an embodiment of the present invention comprises the following steps:
[0052] A1: Raw material preparation:
[0053] Select iron-based alloy raw materials and adjust the chemical composition of the raw materials according to the required nanocrystalline core performance requirements;
[0054] A2: Rapid solidification preparation:
[0055] The raw materials are heated to a molten state, and nanocrystalline soft magnetic materials are prepared by rapid solidification technology (such as spray molding and melt spinning); in this process, the cooling rate and solidification conditions are controlled to form nanoscale grains during the solidification process;
[0056] A3: Heat treatment:
[0057] The prepared nanocrystalline soft magnetic material is subjected to heat treatment to optimize its magnetic properties and structure;
[0058] A4: Curing treatment:
[0059] A diluted curing agent is prepared, coated on the heat-treated nanocrystalline soft magnetic material, and dried to obtain a nanocrystalline iron core.
[0060] Embodiment 2:
[0061] Based on Example 1, please refer to Figure 1 As shown, a production process of a reactor nanocrystalline core according to an embodiment of the present invention further includes:
[0062] Step 1: During the curing agent coating process, the nanocrystalline soft magnetic material is tested to obtain the test data;
[0063] Among them, the test data include: uniformity coefficient;
[0064] In some embodiments, after the nanocrystalline soft magnetic material is coated with a curing agent, a detection imaging device is used to obtain a grayscale histogram of the nanocrystalline soft magnetic material, and based on the grayscale value, the nanocrystalline soft magnetic surface is divided into multiple regions to obtain surface sub-regions (using methods such as threshold segmentation or regional growth in image processing technology, combined with the grayscale value in the grayscale histogram, the nanocrystalline soft magnetic surface is divided into multiple surface sub-regions, so that the grayscale value in each surface sub-region is consistent, and the image processing technology here is all existing technology and will not be repeated here); according to the grayscale values of all surface sub-regions, the grayscale characterization average ratio and the grayscale uniform value are calculated, the grayscale characterization average ratio and the grayscale uniform value are summed and calculated, and the uniformity coefficient is output;
[0065] Exemplarily, the process of obtaining the grayscale representation average ratio is:
[0066] Obtain the grayscale values and area ratios of all surface sub-regions, multiply the grayscale values by the area ratios of the corresponding surface sub-regions, and output the grayscale representation values of each surface sub-region; then average the grayscale representation values of all surface sub-regions and output the grayscale representation mean; calculate the ratio of the grayscale representation mean to the standard grayscale representation mean and output the grayscale representation mean ratio;
[0067] Among them, the standard grayscale characterization mean value is: the grayscale characterization mean value preset by the process during the coating process of nanocrystalline soft magnetic;
[0068] Furthermore, the process of obtaining the area ratio is as follows: obtaining the area of the surface sub-region, calculating the ratio of the surface sub-region area to the total area of the nanocrystalline soft magnetic surface, and outputting the area ratio;
[0069] The process of obtaining the grayscale average value is:
[0070] Calculate the difference between the grayscale value and the standard grayscale value, output the grayscale deviation value, and mark the absolute value of the grayscale deviation value as the grayscale absolute deviation value, compare the grayscale absolute deviation value with the grayscale absolute deviation threshold, and when the grayscale absolute deviation value is greater than the grayscale absolute deviation threshold, generate a grayscale abnormal signal, and mark the surface sub-region corresponding to the grayscale abnormal signal as an abnormal surface sub-region; obtain the grayscale difference value and the grayscale deviation total parameter, calculate the product of the grayscale difference value and the grayscale deviation total parameter, and output the grayscale average value;
[0071] When the grayscale absolute deviation value is greater than the grayscale absolute deviation threshold, a grayscale normal signal is generated;
[0072] Among them, the standard gray value is: the gray value preset by the process during the coating process of nanocrystalline soft magnetic;
[0073] Furthermore, the grayscale difference acquisition process is:
[0074] Based on all surface sub-regions, the maximum value of the grayscale deviation value and the minimum value of the grayscale deviation value in all surface sub-regions are calculated to output the grayscale difference;
[0075] The process of obtaining the total grayscale deviation parameters is as follows:
[0076] Based on the abnormal surface sub-regions, the grayscale absolute deviation value of each surface sub-region is obtained, and the grayscale absolute deviation value is multiplied by the area ratio of the corresponding surface sub-region to output the grayscale deviation parameter of each abnormal surface sub-region; all grayscale deviation parameters are summed up and the total grayscale deviation parameter is output;
[0077] Step 2: Based on the detection data of nanocrystalline soft magnetism, the coating effect is evaluated and a coating effect signal is generated;
[0078] Wherein, the coating effect signal includes: coating qualified signal and coating unqualified signal;
[0079] Compare and analyze the uniformity coefficient with the uniformity coefficient threshold;
[0080] If the uniformity coefficient is ≥ the uniformity coefficient threshold, it means that the coating effect is not ideal, the coating of the nanocrystalline soft magnetic surface is not uniform, or the coating effect is far from the ideal coating effect, and a coating failure signal is generated;
[0081] If the uniformity coefficient is less than the uniformity coefficient threshold, it means that the coating effect is good, the nanocrystalline soft magnetic surface is coated evenly, and the coating effect is close to the ideal coating effect, and a coating qualified signal is generated;
[0082] The technical solution of the embodiment of the present invention is mainly as follows: by detecting an imaging device, a grayscale histogram of nanocrystalline soft magnetism is obtained, and the grayscale histogram reflects the grayscale distribution of the coating surface; based on the grayscale value in the grayscale histogram, the coating surface is divided into a plurality of surface sub-regions, which is helpful for a more detailed analysis of the coating; for each surface sub-region, its grayscale characterization value is calculated, and then the grayscale characterization mean of all surface sub-regions is calculated, and the grayscale characterization mean is compared with the standard grayscale characterization mean to obtain the grayscale characterization mean ratio; at the same time, by calculating the grayscale absolute deviation value of each surface sub-region, And compare it with the grayscale absolute deviation threshold, mark the abnormal surface sub-area, and calculate the grayscale uniformity value; finally, sum the grayscale characterization average ratio and the grayscale uniformity value to obtain the uniformity coefficient; compare and analyze the calculated uniformity coefficient with the preset uniformity coefficient threshold to evaluate the coating effect and generate a coating effect signal; ensure the uniformity and consistency of the nanocrystalline soft magnetic surface coating and improve the reliability and stability of the product; use image processing technology and grayscale histogram analysis to adapt to the coating quality detection of nanocrystalline soft magnetic with different shapes, sizes and surface characteristics;
[0083] Embodiment three:
[0084] Based on the first and second embodiments, please refer to Figure 2 As shown, a production process of a reactor nanocrystalline core according to an embodiment of the present invention further includes:
[0085] Step 3: Analyze whether the abnormal surface sub-region before nanocrystalline soft magnetic coating will affect the coating process, and generate a signal affecting the coating process;
[0086] The signals affecting the coating process include: signals affecting the coating process and signals not affecting the coating process;
[0087] In some embodiments, before the nanocrystalline soft magnetic material is coated with a curing agent, an abnormal surface sub-region before the nanocrystalline soft magnetic material is coated is obtained; the abnormal surface sub-region before coating and the abnormal surface sub-region after coating are analyzed to obtain an abnormal overlap area ratio, and the abnormal overlap area ratio is compared with the abnormal overlap area ratio;
[0088] If the abnormal overlap area ratio is less than the abnormal overlap area, it means that the overlap between the abnormal surface sub-region before coating and the abnormal surface sub-region after coating is low, and the abnormal surface sub-region before nanocrystalline soft magnetic coating will not affect the coating process, that is, a signal affecting the coating process is generated;
[0089] If the abnormal overlap area ratio is ≥ the abnormal overlap area, it means that the overlap between the abnormal surface sub-region before coating and the abnormal surface sub-region after coating is low, and the abnormal surface sub-region before nanocrystalline soft magnetic coating will not affect the coating process, that is, a signal that affects the coating process is generated;
[0090] Exemplarily, the process of obtaining the abnormal overlap area ratio is as follows:
[0091] Based on the abnormal surface sub-region before coating and the abnormal surface sub-region after coating of the nanocrystalline soft magnetic material, the abnormal overlap area is obtained (the abnormal overlap area is: the area of the overlap area between the abnormal surface sub-region before coating and the abnormal surface sub-region after coating); by the formula: The abnormal overlap area ratio YMB is calculated, where YM is the abnormal overlap area, and YMZ is the abnormal total area (the abnormal total area is: the total area of the abnormal surface sub-area before coating and the abnormal surface sub-area after coating);
[0092] It should be explained that the method for obtaining the abnormal surface sub-region before coating has the same steps as the method for obtaining the abnormal surface sub-region after coating; in the method for obtaining the abnormal surface sub-region before coating and the method for obtaining the abnormal surface sub-region after coating, the numerical values of some standard values and thresholds are inconsistent; for example, in the method for obtaining the abnormal surface sub-region before coating, the standard grayscale characterization mean is the grayscale characterization mean of the nanocrystalline soft magnetic material in the ideal state before the coating process;
[0093] The technical solution of the embodiment of the present invention is mainly as follows: by detecting imaging equipment, the abnormal surface sub-areas of the nanocrystalline soft magnetic coating are obtained respectively during and before and after coating, and by calculating the abnormal overlap area ratio, it is determined whether the abnormal surface sub-areas before coating have an impact on the coating process, and a corresponding signal affecting the coating process is generated; through precise detection and evaluation steps, the uniformity and consistency of the nanocrystalline soft magnetic coating are effectively guaranteed, thereby significantly improving the overall performance and stability of the product, and more importantly, through the identification and analysis of the abnormal surface sub-areas before coating, potential coating problems can be discovered in time, and corresponding treatment measures can be taken before coating, thereby effectively avoiding the adverse effects of these problems on the coating process, and further improving the coating quality and product reliability.
[0094] Embodiment 4:
[0095] Based on the first, second and third embodiments, please refer to Figure 3 As shown, a production process of a reactor nanocrystalline core according to an embodiment of the present invention further includes:
[0096] Step 4: Based on the signal that affects the coating process, the coating process is regulated according to the abnormal surface sub-region before the nanocrystalline soft magnetic coating;
[0097] In some embodiments, based on the signal that affects the coating process, a coating analysis model is established according to the abnormal surface sub-region before coating, the abnormal surface sub-region after coating and the process parameters of the coating process, so as to facilitate the subsequent process, based on the coating analysis model and the abnormal surface sub-region before coating, to adjust the process parameters and prevent the generation of the abnormal surface sub-region after coating;
[0098] Among them, process parameters include but are not limited to: coating pressure;
[0099] Exemplarily, the process of establishing the coating analysis model is as follows:
[0100] Based on multiple unqualified coated nanocrystalline soft magnetic materials (unqualified coated nanocrystalline soft magnetic materials are: generated unqualified coating signals, corresponding to the coated nanocrystalline soft magnetic materials), the modeling data of each unqualified coated nanocrystalline soft magnetic material are obtained respectively (the modeling data include: the grayscale absolute deviation value of the abnormal surface sub-region before coating, the grayscale absolute deviation value of the abnormal surface sub-region after coating, and the process parameters when coating the abnormal surface sub-region); the preset coating analysis model is: HP 后 =a1×HP 前 +a2×GY+a3, where a1 and a2 are preset proportional factors, a3 is a constant, HP 后 is the absolute deviation of the grayscale of the abnormal surface sub-region after coating, HP 前 is the grayscale absolute deviation value of the abnormal surface sub-region before coating, GY is the process parameter when coating the abnormal surface sub-region; substitute the modeling data of all unqualified nanocrystalline soft magnetic coatings into the preset coating analysis model, calculate a1, a2 and a3, and obtain the coating analysis model HP 后 =a1×HP 前 +a2×GY+a3;
[0101] In the subsequent process, based on the coating analysis model and the abnormal surface sub-area before coating, the specific method for adjusting the process parameters is as follows:
[0102] In the subsequent process, the abnormal surface sub-region before coating of the nanocrystalline soft magnetic material to be coated and the grayscale absolute deviation value HP of the abnormal surface sub-region are obtained. 待 , and based on the coating analysis model, the formula is obtained: GY 新 =(HP 阈 -a1×HP 待 -a3)÷a2, calculate and obtain the new process parameter GY 新 (New process parameters GY 新 is: the process parameters for preventing the abnormal surface sub-region of the nanocrystalline soft magnetic material to be coated after coating), where HP 阈 is the grayscale absolute deviation threshold;
[0103] The technical solution of the embodiment of the present invention is mainly as follows: during the coating process, an in-depth analysis of the abnormal surface sub-areas before and after coating is performed, and in combination with the coating process parameters (such as coating pressure), a coating analysis model is established; the model can predict the abnormalities that may occur after coating, and adjust the coating process parameters accordingly; specifically, when an abnormal surface sub-area is detected before coating, the coating analysis model is used to accurately calculate how to adjust the process parameters to avoid similar abnormalities after coating; the present invention not only improves the accuracy and controllability of the coating process, but also significantly enhances the quality and stability of nanocrystalline soft magnetic coated products, providing strong technical support for the production of high-quality nanocrystalline soft magnetic products.
[0104] Embodiment five:
[0105] Based on the first, second, third and fourth embodiments, please refer to Figure 4 As shown, the coating process of the nanocrystalline soft magnetic curing agent subjected to the curing treatment is detected and the coating process parameters are determined, which is performed by the coating control system, and the coating control system includes:
[0106] Data acquisition module: used to detect nanocrystalline soft magnetic materials and obtain test data during the coating process;
[0107] Coating evaluation module: Based on the detection data of nanocrystalline soft magnetism, the coating effect is evaluated and a coating effect signal is generated;
[0108] Impact analysis module: used to analyze whether the abnormal surface sub-region before nanocrystalline soft magnetic coating will affect the coating process, and generate a signal affecting the coating process;
[0109] Coating control module: Based on the signal that affects the coating process, the coating process is regulated according to the abnormal surface sub-area before nanocrystalline soft magnetic coating.
[0110] The above thresholds are set for the convenience of comparison. The thresholds depend on the amount of sample data and the number of bases set by technicians in this field for each set of sample data.
[0111] The above is a detailed description of an embodiment of the present invention, but the content is only a preferred embodiment of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made within the scope of the present invention should still fall within the scope of the patent coverage of the present invention.
Claims
1. A production process for a reactor nanocrystalline core, comprising the following steps: Raw material preparation, rapid solidification preparation, heat treatment, and curing treatment, characterized in that the curing treatment includes the following steps: The coating process of the nanocrystalline soft magnetic curing agent subjected to the curing treatment is detected to determine the coating process parameters, and the specific method includes the following steps: Step 1: During the coating process, the nanocrystalline soft magnetic material is tested to obtain the test data; Among them, the test data include: uniformity coefficient; Step 2: Based on the detection data of nanocrystalline soft magnetism, the coating effect is evaluated and a coating effect signal is generated; Step 3: Analyze whether the abnormal surface sub-region before nanocrystalline soft magnetic coating will affect the coating process, and generate a signal affecting the coating process; The signals affecting the coating process include: signals affecting the coating process and signals not affecting the coating process; Step 4: Based on the signal that affects the coating process, the coating process is regulated according to the abnormal surface sub-region before the nanocrystalline soft magnetic coating. The specific process is as follows: Based on the signals that affect the coating process, a coating analysis model is established according to the abnormal surface sub-region before coating, the abnormal surface sub-region after coating and the process parameters of the coating process; In the subsequent process, the abnormal surface sub-region before coating of the nanocrystalline soft magnetic material to be coated and the grayscale absolute deviation value HP of the abnormal surface sub-region are obtained. 待 , and based on the coating analysis model, obtain the new process parameters GY 新 , where HP 阈 is the grayscale absolute deviation threshold.
2. The production process of a reactor nanocrystalline core according to claim 1, characterized in that: The process of obtaining the uniformity coefficient is as follows: After the nanocrystalline soft magnetic material is coated with a curing agent, a grayscale histogram of the nanocrystalline soft magnetic material is obtained by using a detection imaging device, and based on the grayscale value, the surface of the nanocrystalline soft magnetic material is divided into multiple regions to obtain surface sub-regions; According to the grayscale values of all surface sub-areas, the grayscale characterization average ratio and the grayscale uniform value are calculated, the grayscale characterization average ratio and the grayscale uniform value are summed up, and the uniformity coefficient is output.
3. The production process of a reactor nanocrystalline core according to claim 2, characterized in that: The process of obtaining the grayscale characterization average ratio is as follows: Obtaining the grayscale values and area ratios of all surface sub-regions, respectively multiplying the grayscale values by the area ratios of the corresponding surface sub-regions, and outputting the grayscale representation values of each surface sub-region; Then, the grayscale representation values of all surface sub-areas are averaged and the grayscale representation mean is output; the grayscale representation mean is ratioed with the standard grayscale representation mean and the grayscale representation mean ratio is output; The process of obtaining the area ratio is as follows: obtaining the area of the surface sub-region, calculating the ratio of the surface sub-region area to the total area of the nanocrystalline soft magnetic surface, and outputting the area ratio.
4. The production process of a reactor nanocrystalline core according to claim 2, characterized in that: The process of obtaining the grayscale average value is as follows: The grayscale value is calculated to be different from the standard grayscale value, and the grayscale deviation value is output. The absolute value of the grayscale deviation value is marked as the grayscale absolute deviation value. The grayscale absolute deviation value is compared with the grayscale absolute deviation threshold. When the grayscale absolute deviation value is greater than the grayscale absolute deviation threshold, a grayscale abnormality signal is generated, and the surface sub-region corresponding to the grayscale abnormality signal is marked as an abnormal surface sub-region. The grayscale difference value and the grayscale deviation total parameter are obtained, and the grayscale difference value is multiplied by the grayscale deviation total parameter to output the grayscale uniform value.
5. The production process of a reactor nanocrystalline core according to claim 4, characterized in that: The grayscale difference acquisition process is as follows: Based on all surface sub-regions, the difference between the maximum grayscale deviation value and the minimum grayscale deviation value in all surface sub-regions is calculated, and the grayscale difference is output.
6. The production process of a reactor nanocrystalline core according to claim 4, characterized in that: The process of obtaining the total grayscale deviation parameter is as follows: Based on the abnormal surface sub-region, the grayscale absolute deviation value of each surface sub-region is obtained, and the grayscale absolute deviation value is multiplied by the area ratio of the corresponding surface sub-region to output the grayscale deviation parameter of each abnormal surface sub-region; all grayscale deviation parameters are summed up and the total grayscale deviation parameter is output.
7. The production process of a reactor nanocrystalline core according to claim 2, characterized in that: The specific process of generating the coating effect signal is as follows: The coating effect signal includes: coating qualified signal and coating unqualified signal; Compare and analyze the uniformity coefficient with the uniformity coefficient threshold; If the uniformity coefficient is ≥ the uniformity coefficient threshold, a coating failure signal is generated; If the uniformity coefficient is less than the uniformity coefficient threshold, a coating qualified signal is generated.
8. The production process of a reactor nanocrystalline core according to claim 1, characterized in that: The specific process of generating the signal affecting the coating process is as follows: Before the nanocrystalline soft magnetic material is coated with a curing agent, an abnormal surface sub-region before the nanocrystalline soft magnetic material is coated is obtained; the abnormal surface sub-region before coating and the abnormal surface sub-region after coating are analyzed to obtain an abnormal overlap area ratio, and the abnormal overlap area ratio is compared with the abnormal overlap area ratio; If the abnormal overlap area ratio is less than the abnormal overlap area, a signal affecting the coating process is generated; If the abnormal overlap area ratio ≥ the abnormal overlap area, a signal affecting the coating process is generated.
9. The production process of a reactor nanocrystalline core according to claim 8, characterized in that: The process of obtaining the abnormal overlap area ratio is as follows: Based on the abnormal surface sub-region before coating and the abnormal surface sub-region after coating of nanocrystalline soft magnetism, the abnormal overlap area is obtained; the abnormal overlap area ratio YMB is obtained by calculation, where YM is the abnormal overlap area and YMZ is the abnormal total area.
10. The production process of a reactor nanocrystalline core according to claim 1, characterized in that: The establishment process of the coating analysis model is as follows: Based on a plurality of unqualified coated nanocrystalline soft magnetic materials, respectively obtaining modeling data of each unqualified coated nanocrystalline soft magnetic material; A coating analysis model is preset; modeling data of all nanocrystalline soft magnetic materials with unqualified coating are substituted into the preset coating analysis model, a1, a2 and a3 are calculated and obtained, and a coating analysis model is obtained.
Citation Information
Patent Citations
Preparation method of nanocrystalline magnetic powder cores
CN102744403A
Coating quality online prediction method and system and computer readable storage medium
CN111444617A
Coating machine control method and coating machine system
CN117930750A
Monitoring system for thin film processing based on Internet of Things
CN118080280A
Coating for soft magnetic alloy core and its spraying process
CN1986488A
Cited By
Process for vacuum freeze drying of Tibetan medicinal materials
CN121383578A
A process for vacuum freeze-drying Tibetan medicinal materials
CN121383578B