Manufacturing method of U-shaped groove

Through the Y-direction opening patterned etching method, field oxygen self-alignment is used to define the sides of the U-shaped trench, which solves the problems of asymmetric sharp corners of semiconductors and uneven bottom of the trench in the existing technology, and achieves symmetrical sharp corners and Flat bottom to prevent leakage.

CN118737833APending Publication Date: 2024-10-01SHANGHAI HUALI INTEGRATED CIRCUIT CORP
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410816276.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-21
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Existing U-shaped trench manufacturing methods have problems such as asymmetry of semiconductor sharp corners and uneven channel bottom, resulting in leakage and shortened channels.

Method used

The Y-direction opening patterned etching method is used to define the Y-direction opening pattern to extend along the Y direction and span multiple active areas. Field oxygen self-alignment is used to define the sides of the U-shaped trench, making the semiconductor sharp corners symmetrical and highly variable. It is small and avoids overlay errors caused by the definition of opening graphics in the X direction.

Benefits of technology

It achieves symmetrical distribution and height control of semiconductor sharp corners, prevents leakage, and improves the flatness of the bottom of the U-shaped trench to avoid channel shortening.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118737833A_ABST
    Figure CN118737833A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a U-shaped groove, which comprises the following steps of: providing a semiconductor substrate on which field oxide is formed, and isolating first active regions which are arranged in parallel by the field oxide in a first region; and opening the first area. Performing Y-direction opening graphical etching, which comprises the following steps of: defining a Y-direction opening graph; the Y-direction opening pattern extends along the Y direction and spans the plurality of first active regions and the field oxide. Etching the semiconductor substrate with the bottom exposed under the definition of the Y-direction opening pattern, and forming a U-shaped groove; and the first side surface and the second side surface of the U-shaped groove are two side surfaces which extend along the X direction and are defined by field oxide self-alignment at two sides of the first active region. According to the invention, the semiconductor sharp corners on the side surfaces, adjacent to the field oxide, of the U-shaped groove are symmetrically distributed and become smaller, so that the height of the semiconductor sharp corners can be controlled, electric leakage caused by too high height of the semiconductor sharp corners can be prevented, the flatness of the bottom surface of the U-shaped groove can be increased, and the channel can be prevented from being shortened.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for manufacturing a semiconductor integrated circuit, and in particular to a method for manufacturing a U-trench. Background Art

[0002] Capacitors are the bottleneck of traditional DRAM development. Semi-floating gate transistors are a potential capacitor-free DRAM that is compatible with standard logic processes and easier to scale down. U-trench can isolate the semi-floating gate Nwell, forming a U-shaped channel at the bottom, which is more conducive to miniaturizing the device area than the traditional profile channel. In addition, the polysilicon gate in the U-trench is used to store charge, and the tunneling effect is used to accelerate the writing of charge.

[0003] In the existing method, in the semi-floating gate process compatible with the memory array (array) and the logic circuit, the development of U-trench needs to first use array photolithography (photo, PH) to open the array area, and then remove the pad (pad) SiN and pad oxide layer (OX) by dry etching, and then sequentially deposit (dep) OX / SIN / OX as a hard mask layer (hard mask). U-trench Y first etches OX with a high selectivity and stops on SiN to form a Y-direction HM pattern. U-trench X then opens the active area (AA) area for X-direction etching, photoresist (PR) protects the shallow trench isolation (STI) area, and etches HM OX / SIN / OX under PR protection, and then etches the Si of the silicon substrate of the active area under the dual protection of HM and PR to form U-trench. Wherein, U-trench Y represents the Y direction of the U-trench, U-trench X represents the X direction of the U-trench, U-trench Y is perpendicular to the length direction of the active area, and U-trench X is parallel to the length direction of the active area.

[0004] In the existing method, two pattern etchings are required to define the U-shaped trench. When the X-direction opening pattern is defined in the X-direction etching, i.e., the U-trench X ET, the photolithography process inevitably has an overlay error, i.e., the two side surfaces of the X-direction opening pattern extending along the X-direction and the side surfaces of the corresponding active area are not completely aligned, but have a deviation in the Y-direction, i.e., the overlay in the Y-direction. The overlay variation in the Y-direction will lead to the appearance of asymmetric semiconductor corners such as Si corners. Since the AA profile is close to vertical, a slight change in the overlay in the Y-direction will lead to a sharp change in the height difference of the Si corners on both sides, and the process window will become very small. The side with the higher corner height is prone to leakage between the source and the drain.

[0005] In addition, due to the presence of HM SIN and OX on STI, there is a natural barrier to Si etching, resulting in a high Si corner height in the Y direction, an uneven bottom of the U-trench, and a shortened channel. Summary of the invention

[0006] The technical problem to be solved by the present invention is to provide a method for manufacturing a U-shaped groove, which can make the semiconductor corners on the side of the U-shaped groove adjacent to the field oxygen symmetrically distributed and smaller, thereby achieving control of the height of the semiconductor corners and preventing leakage caused by excessive height of the semiconductor corners, and also increasing the flatness of the bottom surface of the U-shaped groove and preventing the channel from shortening.

[0007] In order to solve the above technical problems, the present invention provides a method for manufacturing a U-shaped groove, comprising the following steps:

[0008] A semiconductor substrate with field oxide formed thereon is provided. In a first region, first active regions are isolated by the field oxide. The first active regions are arranged in parallel. The X direction is the length direction of the first active regions, and the Y direction is perpendicular to the X direction.

[0009] Open the first area.

[0010] The Y-direction opening pattern etching is performed, including the following steps:

[0011] A Y-direction opening pattern is defined; the Y-direction opening pattern extends along the Y-direction and spans across a plurality of the first active regions and the field oxygen between the first active regions, and the Y-direction opening pattern exposes the top surface of the spanned first active region and the top surface of the field oxygen.

[0012] The semiconductor substrate at the first active area exposed at the bottom is etched under the definition of the Y-direction opening pattern to form the U-shaped groove; the first side surface and the second side surface of the U-shaped groove are two side surfaces extending along the X-direction defined by the field oxygen self-alignment on both sides of the first active area, and the semiconductor sharp corners on the first side surface and the second side surface of each U-shaped groove are symmetrical and the height is reduced by utilizing the characteristics defined by the field oxygen self-alignment; the third side surface and the fourth side surface of the U-shaped groove are two side surfaces extending along the Y-direction defined by the Y-direction opening pattern.

[0013] A further improvement is that, in the Y-direction opening patterning etching, while etching the semiconductor substrate of the first active area exposed at the bottom of the Y-direction opening pattern, the field oxygen exposed at the bottom of the Y-direction opening pattern is also partially consumed, and the more the thickness of the field oxygen exposed at the bottom of the Y-direction opening pattern is consumed, the more the height of the semiconductor corner is reduced.

[0014] A further improvement is that the semiconductor substrate comprises a silicon substrate.

[0015] A further improvement is that the field oxide is formed by a shallow trench isolation process.

[0016] A further improvement is that the Y-direction opening pattern includes a photoresist pattern defined by a photolithography process.

[0017] A further improvement is that the Y-direction opening pattern also includes an organic bottom layer pattern located at the bottom of the photoresist pattern; when performing the photolithography process, the organic bottom layer is first coated, and then the photoresist is coated, and then the exposure and development processes of the photolithography process are performed to form the photoresist pattern, and then the organic bottom layer is etched to form the organic bottom layer pattern, and the organic bottom layer pattern and the photoresist pattern together constitute the Y-direction opening pattern.

[0018] A further improvement is that the material of the organic bottom layer includes SOC.

[0019] A further improvement is that the U-shaped trench is a semi-floating gate trench of a semi-floating gate transistor.

[0020] A further improvement is that the first region is a formation region of each of the semi-floating gate transistors, and in the first region, each of the semi-floating gate transistors is arranged in rows and columns to form a storage array.

[0021] A further improvement is that a first conductive type well is formed in the first active region, and the first conductive type well is formed in a surface region of the second conductive type well.

[0022] The U-shaped trench passes through the first conductive type well and a bottom surface of the U-shaped trench enters into the second conductive type well.

[0023] A further improvement is that the semi-floating gate transistor is an N-type device, the first conductivity type is N-type, and the second conductivity type is P-type; or, the semi-floating gate transistor is a P-type device, the first conductivity type is P-type, and the second conductivity type is N-type.

[0024] Unlike the prior art, which requires forming a hard mask layer, and performing patterned etching on the hard mask layer in the X direction and the Y direction, and defining the formation area of ​​the U-shaped groove by the overlapping area of ​​the hard mask layer in the X direction and the Y direction, the present invention does not need to define an opening pattern in the X direction, but only needs to define an opening pattern in the Y direction. The formation area of ​​the U-shaped groove is directly defined by the overlapping area between the opening pattern in the Y direction and the first active area. In this way, the two side surfaces of the U-shaped groove adjacent to the field oxygen, namely the first side surface and the second side surface, are completely defined by the corresponding field oxygen by self-alignment. Compared with the prior art, in which the first side surface and the second side surface of the U-shaped groove need to be defined by the X-direction opening pattern, the self-alignment definition does not have an alignment problem, so the semiconductor sharp corners on the side surfaces of the U-shaped groove adjacent to the field oxygen can be symmetrically distributed and reduced, thereby achieving the control of the height of the semiconductor sharp corners and preventing leakage caused by the excessive height of the semiconductor sharp corners, and increasing the flatness of the bottom surface of the U-shaped groove and preventing the channel from shortening. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] The present invention is further described in detail below with reference to the accompanying drawings and specific embodiments:

[0026] Figure 1A-1E It is a three-dimensional structure diagram of the device in each step of an existing method for manufacturing a semi-floating gate U-shaped trench;

[0027] Figure 2A It is a schematic cross-sectional structure diagram of the influence of the overlay deviation in the Y direction on the height of the semiconductor corner during the X-direction pattern etching in an existing method for manufacturing a semi-floating gate U-shaped groove;

[0028] Figure 2B It is a cross-sectional structure diagram along the Y direction after a U-shaped groove is formed in an area with good overlay accuracy and an area with poor overlay accuracy in an existing method for manufacturing a semi-floating gate U-shaped groove;

[0029] Figure 2C It is a cross-sectional structure diagram along the X direction after a U-shaped groove is formed in an area with good overlay accuracy and an area with poor overlay accuracy in an existing method for manufacturing a semi-floating gate U-shaped groove;

[0030] Figure 3 is a flow chart of a method for manufacturing a U-shaped groove according to an embodiment of the present invention;

[0031] Figure 4A-4B is a three-dimensional structural diagram of a device in each step of a method for manufacturing a U-shaped groove according to an embodiment of the present invention;

[0032] Figure 4C It is a cross-sectional structural diagram along the Y direction after the U-shaped groove is formed in the manufacturing method of the U-shaped groove of an embodiment of the present invention. DETAILED DESCRIPTION

[0033] The embodiments of the present invention are formed on the basis of analyzing the technical problems of the existing methods. Before introducing the embodiments of the present invention in detail, the existing methods are briefly introduced:

[0034] like Figures 1A to 1E As shown, it is a three-dimensional structure diagram of the device in each step of the existing method for manufacturing a semi-floating gate U-shaped trench; Figure 2A , is a schematic cross-sectional structure diagram of the effect of the Y-direction overlay deviation on the height of the semiconductor corner during X-direction pattern etching in an existing method for manufacturing a semi-floating gate U-shaped groove; Figure 2B As shown, it is a cross-sectional structure diagram along the Y direction after the U-shaped groove is formed in the area with good overlay accuracy and the area with poor overlay accuracy in an existing method for manufacturing a semi-floating gate U-shaped groove; Figure 2C As shown, it is a cross-sectional structure diagram along the X direction after the U-shaped groove is formed in the area with good overlay accuracy and the area with poor overlay accuracy in an existing method for manufacturing a semi-floating gate U-shaped groove; the existing method for manufacturing a semi-floating gate U-shaped groove includes the following steps:

[0035] like Figure 1A As shown, a semiconductor substrate 102 with a field oxide 103 is provided. In a first region 101, the field oxide 103 isolates first active regions, that is, the semiconductor substrate 102 located between the field oxides 103 constitutes each of the first active regions, and the first active regions are arranged in parallel.

[0036] Figure 1A It shows that the X direction is parallel to the length direction of the first active region, and the Y direction is perpendicular to the X direction. Please also refer to the cross-sectional structure of the field oxide 103 Figure 2A shown.

[0037] Typically, the semiconductor substrate 102 is a silicon substrate, and the field oxide 103 is formed by a shallow trench isolation process.

[0038] like Figure 1A As shown, the first area 101 is opened.

[0039] Figure 1A In the figure, the first area 101 is located on the right side of the dotted line AA.

[0040] Typically, the left region of the dotted line AA is also covered with a pad layer, such as a SiN pad layer and a silicon oxide pad layer. The pad layer in the first region 101 is removed, thereby opening the first region 101.

[0041] like Figure 1B As shown, a hard mask layer 104 is formed in the first region 101 .

[0042] Typically, the hard mask layer 104 includes a first oxide layer 104a, a second nitride layer 104b, and a third oxide layer 104c stacked in sequence. Figure 2B shown.

[0043] The processes for forming the first oxide layer 104a, the second nitride layer 104b and the third oxide layer 104c are respectively:

[0044] U-trench OX1 dep; U-trench SiNdep; U-trench OX2 dep.

[0045] like Figure 1C As shown, Y-direction opening patterning etching, namely U-trench Y etching (ET) is performed to form a Y-direction opening, and photolithography definition is required before etching.

[0046] U-trench Y ET uses high selectivity to etch OX and stop on SIN. Figure 2B As described above, the third oxide layer 104c is etched and stops on the top surface of the second nitride layer 104b.

[0047] Perform X-direction opening pattern etching, namely U-trench X ET, including:

[0048] An organic bottom layer such as a SOC layer is coated. The organic bottom layer completely fills the Y-direction opening and extends to the top surface of the hard mask layer 104 outside the Y-direction opening. The top surface of the organic bottom layer is flat.

[0049] like Figure 1D As shown, after that, a photoresist is formed and an X-direction opening pattern is defined by photolithography. After that, the semiconductor substrate 102 exposed at the bottom is etched according to the defined X-direction opening pattern to form a U-shaped groove 107, and the exposed semiconductor substrate 102 is located in the region where the X-direction opening pattern and the Y-direction opening pattern overlap, that is, the U-shaped groove 107 is located in the X-direction opening pattern and the Y-direction opening pattern.

[0050] Therefore, the four sides of the U-shaped groove 107 need to be defined by the photolithography process, wherein the two sides adjacent to the field oxide 103, namely the first side and the second side, are defined by the X-direction opening pattern, and the other two sides are defined by the Y-direction opening pattern. Semiconductor corners 107a will be formed at the first side and the second side of the U-shaped groove 107. The height of the semiconductor corner 107a will be affected by the photolithography process of the X-direction opening pattern. Figure 2A As shown, the top surface of the first active area composed of the semiconductor substrate 102 is the bottom structure, which is a fixed structure; when defining the X-direction opening pattern, the X-direction opening pattern needs to be aligned with the first active area at the bottom, but the photolithography process has a certain error, so the X-direction opening pattern cannot be completely aligned with the first active area, and there is a registration deviation between the two, and the registration deviation in different areas may be different. The difference in registration deviation will affect the height of the semiconductor corner 107a, and because the side 102a of the first active area is close to vertical, the registration deviation will have a greater impact on the height of the semiconductor corner 107a. Figure 2A As shown in FIG. 1 , the edges of the X-direction opening pattern corresponding to the two different registration deviations are shown as dashed line BB and dashed line BB, respectively, with a deviation of w1 between the two; the height of the semiconductor corner 107a formed between the two will have a deviation shown as d1.

[0051] like Figure 2B As shown, region 101a represents a region with good overlay accuracy, and region 101b represents a region with poor overlay accuracy. It can be seen that in region 101a, the height uniformity of the semiconductor corners 107a is good, and the apex positions of the semiconductor corners 107a are basically located on the same dotted line DD. From region 101b, it can be seen that the heights of the semiconductor corners 107a at various locations are quite different, as shown by dotted lines DD1 and DD2.

[0052] When the height difference of the semiconductor corners 107 a is large, a higher semiconductor corner 107 a may be formed. The higher semiconductor corner 107 a is prone to source-drain leakage.

[0053] like Figure 2C As shown, a first conductive type well 1022 and a second conductive type well 1021 are formed on the semiconductor substrate 102, and the U-shaped groove 107 needs to pass through the first conductive type well 1022 to achieve the isolation of the source and drain regions. It can be seen that in the region 101a, the U-shaped groove 107 passes through the first conductive type well 1022, that is, passes through the interface between the first conductive type well 1022 and the second conductive type well 1021, that is, the interface corresponding to the dotted line EE. However, in the region 101b, in some regions, the bottom of the U-shaped groove 107 does not pass through the dotted line EE, so source-drain leakage will occur.

[0054] like Figure 3 FIG. 2 is a flow chart of a method for manufacturing a U-shaped groove 204 according to an embodiment of the present invention; FIG. 4A to FIG. 4B As shown, it is a three-dimensional structure diagram of the device in each step of the manufacturing method of the U-shaped groove 204 of the embodiment of the present invention; Figure 4C , which is a cross-sectional structure diagram along the Y direction after the U-shaped groove 204 is formed according to the manufacturing method of the U-shaped groove 204 of the embodiment of the present invention; the manufacturing method of the U-shaped groove 204 of the embodiment of the present invention comprises the following steps:

[0055] Step S101: Figure 4A As shown, a semiconductor substrate 202 with a field oxide 203 is provided. In a first region 201, the field oxide 203 isolates first active regions. The first active regions are arranged in parallel. The X direction is the length direction of the first active regions, and the Y direction is perpendicular to the X direction.

[0056] Please refer to the cross-sectional structure of the field oxide 203 Figure 4C shown.

[0057] In the embodiment of the present invention, the semiconductor substrate 202 includes a silicon substrate.

[0058] The field oxide 203 is formed by a shallow trench isolation process.

[0059] Step S102: Figure 4A As shown, the first area 201 is opened.

[0060] The first area 201 is located on the right side of the dotted line AA.

[0061] In some embodiments, the left region of the dotted line AA is also covered with a pad layer, such as a SiN pad layer and a silicon oxide pad layer. The pad layer in the first region 201 is removed, thereby opening the first region 201 .

[0062] Step S103: Figure 4B As shown, the Y-direction opening pattern etching is performed, that is, U-trench Y PH / ET, PH represents photolithography, which is used for pattern definition; ET represents etching; and includes the following sub-steps:

[0063] Step S1031, defining a Y-direction opening pattern; the Y-direction opening pattern extends along the Y-direction and spans across multiple first active regions and the field oxide 203 between the first active regions, and the Y-direction opening pattern exposes the top surface of the first active region spanned and the top surface of the field oxide 203.

[0064] In the embodiment of the present invention, the Y-direction opening pattern includes a photoresist pattern defined by a photolithography process.

[0065] In some preferred embodiments, the Y-direction opening pattern also includes an organic bottom layer pattern located at the bottom of the photoresist pattern; when performing the photolithography process, the organic bottom layer is first coated, and then the photoresist is coated, and then the exposure and development processes of the photolithography process are performed to form the photoresist pattern, and then the organic bottom layer is etched to form the organic bottom layer pattern, and the organic bottom layer pattern and the photoresist pattern together constitute the Y-direction opening pattern.

[0066] Preferably, the material of the organic bottom layer includes SOC.

[0067] Step S1032: Figure 4B As shown, the semiconductor substrate 202 at the first active area exposed at the bottom is etched under the definition of the Y-direction opening pattern to form the U-shaped groove 204; the first side surface and the second side surface of the U-shaped groove 204 are two side surfaces extending along the X-direction defined by the self-alignment of the field oxide 203 on both sides of the first active area, and the semiconductor corners 204a on the first side surface and the second side surface of each of the U-shaped grooves 204 are symmetrical and their heights are reduced by utilizing the self-alignment definition feature of the field oxide 203; the third side surface and the fourth side surface of the U-shaped groove 204 are two side surfaces extending along the Y-direction defined by the Y-direction opening pattern.

[0068] Please refer to the cross-sectional structure after step S1032 is completed. Figure 4C As shown, Figure 4C The two sides shown in FIG. 1 are the first side and the second side of the U-shaped groove 204. It can be seen that the top of each semiconductor corner 204a is located near the dotted line FF, so the semiconductor corner 204a has good symmetry and its height is smaller than that defined by photolithography.

[0069] During the Y-direction opening patterning etching, while etching the semiconductor substrate 202 of the first active area exposed at the bottom of the Y-direction opening pattern, the field oxygen 203 exposed at the bottom of the Y-direction opening pattern is also partially consumed. The more the thickness of the field oxygen 203 exposed at the bottom of the Y-direction opening pattern is consumed, the more the height of the semiconductor corner 204a is reduced.

[0070] like Figure 4CAs shown in the figure, the dotted line HH represents the top surface position of the field oxygen 203 in the area outside the Y-direction opening pattern, and the dotted line GG represents the top surface position of the field oxygen 203 in the Y-direction opening pattern area. The position of the dotted line GG is lower than the position of the dotted line HH. This is because the field oxygen 203 in the Y-direction opening pattern area will be consumed; at the same time, after the top surface position of the field oxygen 203 in the Y-direction opening pattern area becomes lower, the height of the semiconductor corner 204a can be further reduced.

[0071] In the embodiment of the present invention, the U-shaped trench 204 is a semi-floating gate trench of a semi-floating gate transistor.

[0072] The first region 201 is a region where the semi-floating gate transistors are formed. In the first region 201 , the semi-floating gate transistors are arranged in rows and columns to form a storage array.

[0073] The first active region is formed with a first conductivity type well formed in a surface region of the second conductivity type well.

[0074] The U-shaped trench 204 passes through the first conductive type well and the bottom surface of the U-shaped trench 204 enters into the second conductive type well.

[0075] In the embodiment of the present invention, the semi-floating gate transistor is an N-type device, the first conductivity type is N-type, and the second conductivity type is P-type. In other embodiments, the semi-floating gate transistor can also be a P-type device, the first conductivity type is P-type, and the second conductivity type is N-type.

[0076] After forming the U-shaped trench 204, the semi-floating gate transistor can be formed by the same method as in the prior art. For example:

[0077] A floating gate dielectric layer is formed, where the floating gate dielectric layer covers the inner surface of the U-shaped trench 204 and extends to the surface of the first conductive type well outside the U-shaped trench 204 .

[0078] A floating gate dielectric window penetrating through the floating gate dielectric layer is formed in the top region of the first conductive type well on the drain region side outside the U-shaped trench 204 .

[0079] A polysilicon floating gate is formed, which completely fills the U-shaped groove 204 and extends to the outside of the U-shaped groove 204. The polysilicon floating gate also completely fills the floating gate dielectric window and contacts the first conductive type well to form a PN junction. In this way, the polysilicon floating gate has a semi-floating gate structure.

[0080] Then a control gate is formed, which is located on the top of the polysilicon floating gate and separated by an inter-gate dielectric layer. The control gate is also located on the surface of the first conductive type well outside the floating gate dielectric window and separated by a corresponding gate dielectric layer.

[0081] A source region and a drain region heavily doped with the first conductivity type are self-alignedly formed on both sides of a gate structure formed by superposition of a polysilicon floating gate and a control gate.

[0082] Unlike the prior art, which requires forming a hard mask layer, and performing patterning etching on the hard mask layer in the X direction and the Y direction, and defining the formation area of ​​the U-shaped groove 204 by the overlapping area of ​​the hard mask layer in the X direction and the Y direction, the embodiment of the present invention does not need to define an opening pattern in the X direction, but only needs to define an opening pattern in the Y direction. The formation area of ​​the U-shaped groove 204 is directly defined by the overlapping area between the opening pattern in the Y direction and the first active area. In this way, the two side surfaces of the U-shaped groove 204 adjacent to the field oxide 203, namely the first side surface and the second side surface It is completely defined by the corresponding field oxide 203 in self-alignment. Compared with the prior art in which the first side and the second side of the U-shaped groove 204 need to be defined by an X-direction opening pattern, the self-alignment definition does not have an alignment problem. Therefore, the semiconductor corners 204a on the sides of the U-shaped groove 204 adjacent to the field oxide 203 can be symmetrically distributed and become smaller, thereby achieving control of the height of the semiconductor corners 204a and preventing leakage caused by the excessive height of the semiconductor corners 204a, and increasing the flatness of the bottom surface of the U-shaped groove 204 and preventing the channel from shortening.

[0083] The embodiment of the present invention eliminates the influence of the overlay of the U-trench X in the Y direction on the asymmetry of the semiconductor corners, such as the Si corners, and reduces the risk of leakage.

[0084] The embodiment of the present invention reduces the height of the U-trench sharp corner and improves the bottom profile of the U-trench.

[0085] U-trench X etching is used in the existing U-trench process. During the U-trench X etching process, the deterioration of the overlay in the Y direction will lead to the appearance of asymmetric Si corners. Since the AA profile is close to vertical, a slight change in the overlay in the Y direction will cause a sharp change in the height difference of the Si corners on both sides. The process window is very small, and leakage occurs between the source and the drain on the side with the high corner height. Since HM SIN and OX exist on STI, they have a natural blocking effect on Si etching, resulting in a high height of the Si corner in the Y direction, an uneven bottom of the U-trench, and a shortened channel. In view of the problems existing in these prior arts, the process of the embodiment of the present invention is optimized and improved, including:

[0086] After etching to open the array region, ie, the memory cell region 201, U-trench X PH and ET are not performed to avoid the influence of overlay in the Y direction.

[0087] Directly perform U-trench Y ET. Since there is no HM obstruction in the Y direction, self-aligned etching will be carried out downward along the contour of AA to form a symmetrical Si sharp corner. In addition, since STIOX is also consumed during etching, the obstruction to etching is weakened, the Si sharp corner is also smaller, and the bottom of the trench is flatter.

[0088] Therefore, the embodiment of the present invention eliminates the influence of the overlay of the U-trench X on the asymmetry of the Si corner in the Y direction, thereby reducing the leakage risk.

[0089] In the U-trench X-etching process of the existing method, the overlay in the Y direction deteriorates, which leads to the appearance of asymmetric Si corners. Since the AA profile is close to vertical, a slight change in the overlay in the Y direction will lead to a sharp change in the height difference of the Si corners on both sides. The process stability is very poor, and leakage occurs between the source and the drain on the side with the higher corner height.

[0090] In the embodiment of the present invention, U-trench X is canceled or skipped and U-trench Y ET is directly performed. There is no HM blocking in the Y direction, and self-aligned etching is performed downward along the contour of AA to form a symmetrical Si sharp corner, thereby reducing the risk of single-side leakage.

[0091] In addition, after reducing the height of the U-trench corner, the bottom profile of the U-trench can also be improved. The existing process has HMSIN and OX as well as a complete STI. Since the AA profile is not completely vertical, during the etching process, HM and STI will form a certain barrier to etching, resulting in a high Si corner, an uneven trench bottom, and a shorter channel. The process of the embodiment of the present invention does not deposit (dep) HM and directly etches Si. During the etching process, STIOX is also consumed, and the barrier to etching will also be weakened, the Si corner becomes smaller, and the trench bottom is flatter.

[0092] The present invention has been described in detail above through specific embodiments, but these do not constitute limitations of the present invention. Without departing from the principle of the present invention, those skilled in the art may also make many variations and improvements, which should also be considered as the protection scope of the present invention.

Claims

1. A method for manufacturing a U-shaped groove, characterized in that: The steps include: Providing a semiconductor substrate with field oxide formed thereon, wherein in a first region, first active regions are isolated by the field oxide, the first active regions are arranged in parallel, an X direction is a length direction of the first active regions, and a Y direction is perpendicular to the X direction; Open the first area; Performing Y-direction opening patterning etching includes the following steps: A Y-direction opening pattern is defined; the Y-direction opening pattern extends along the Y-direction and spans across a plurality of the first active regions and the field oxides between the first active regions, and the Y-direction opening pattern exposes the top surface of the spanned first active region and the top surface of the field oxide; Etching the semiconductor substrate at the first active area exposed at the bottom under the definition of the Y-direction opening pattern to form the U-shaped groove; The first side surface and the second side surface of the U-shaped groove are two side surfaces extending along the X direction and defined by the field oxygen self-alignment on both sides of the first active area. The characteristics defined by the field oxygen self-alignment are utilized to make the semiconductor sharp corners on the first side surface and the second side surface of each U-shaped groove symmetrical and the height smaller; the third side surface and the fourth side surface of the U-shaped groove are two side surfaces extending along the Y direction and defined by the Y-direction opening pattern.

2. The method for manufacturing a U-shaped groove according to claim 1, characterized in that: During the Y-direction opening patterning etching, while etching the semiconductor substrate of the first active area exposed at the bottom of the Y-direction opening pattern, the field oxygen exposed at the bottom of the Y-direction opening pattern is also partially consumed. The more the thickness of the field oxygen exposed at the bottom of the Y-direction opening pattern is consumed, the more the height of the semiconductor corner is reduced.

3. The method for manufacturing a U-shaped groove according to claim 1, wherein: The semiconductor substrate includes a silicon substrate.

4. The method for manufacturing a U-shaped groove according to claim 1, wherein: The field oxide is formed by a shallow trench isolation process.

5. The method for manufacturing a U-shaped groove according to claim 1, wherein: The Y-direction opening pattern includes a photoresist pattern defined by a photolithography process.

6. The method for manufacturing a U-shaped groove according to claim 5, characterized in that: The Y-direction opening pattern also includes an organic bottom layer pattern located at the bottom of the photoresist pattern; when performing the photolithography process, the organic bottom layer is first coated, and then the photoresist is coated, and then the exposure and development processes of the photolithography process are performed to form the photoresist pattern, and then the organic bottom layer is etched to form the organic bottom layer pattern, and the organic bottom layer pattern and the photoresist pattern together constitute the Y-direction opening pattern.

7. The method for manufacturing a U-shaped groove according to claim 6, characterized in that: The material of the organic bottom layer includes SOC.

8. The method for manufacturing a U-shaped groove according to claim 1, wherein: The U-shaped trench is a semi-floating gate trench of a semi-floating gate transistor.

9. The method for manufacturing a U-shaped groove according to claim 8, characterized in that: The first region is a formation region of the semi-floating gate transistors. In the first region, the semi-floating gate transistors are arranged in rows and columns to form a memory array.

10. The method for manufacturing a U-shaped groove according to claim 8, characterized in that: The first active region is formed with a first conductivity type well, the first conductivity type well being formed in a surface region of the second conductivity type well; The U-shaped trench passes through the first conductive type well and a bottom surface of the U-shaped trench enters into the second conductive type well.

11. The method for manufacturing a U-shaped groove according to claim 10, characterized in that: The semi-floating gate transistor is an N-type device, the first conductivity type is N-type, and the second conductivity type is P-type; or, the semi-floating gate transistor is a P-type device, the first conductivity type is P-type, and the second conductivity type is N-type.

Citation Information

Cited By

  • Semiconductor structure and preparation method thereof