Method for manufacturing pattern of metal protective layer on surface of ceramic copper-clad plate
The removal of unnecessary metal layers by ultraviolet laser solves the problems of high precision and cost in the production of metal layer patterns on the surface of traditional ceramic copper-clad laminates, and achieves a high-precision, environmentally friendly and energy-saving process, which is suitable for the preparation of IGBT power modules.
Patent Information
- Application Number
- CN202410996845.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-10-01
AI Technical Summary
The traditional metal layer pattern production process on the surface of ceramic copper-clad laminates has problems such as difficult control of pattern production accuracy, risk of liquid leakage, and high cost, especially in the secondary film and electroless nickel gold processes.
Use ultraviolet laser to directly remove unnecessary metal layers. By setting and adjusting laser process parameters, such as spot size, scanning spacing, filling angle and power factor, combined with CCD visual alignment system, high-precision metal layer removal can be achieved.
The position accuracy is improved, the process steps are reduced, and efficient, environmentally friendly and energy-saving metal layer pattern production is achieved, which is suitable for the preparation of ceramic copper-clad laminates for IGBT power modules.
Abstract
Description
Technical Field
[0001] The invention relates to the field of ceramic copper-clad plate preparation technology, in particular to a method for producing a metal protective layer pattern on the surface of a ceramic copper-clad plate. Background Art
[0002] At present, the surface metal layer pattern production and processing process of copper clad laminates generally adopts secondary film lamination, position exposure, development, and surface metal layer production process. There are many problems in actual production, which are explained below using chemical nickel-gold as an example. For the process of secondary protective film production → exposure → development → chemical nickel-gold plating, there are the following problems: First, the accuracy of graphic production is difficult to control after the secondary film lamination; second, there is a risk of leakage in the graphic grooves; the protective film partially falls off and decomposes during the chemical nickel-gold process, contaminating the gold cylinder solution and causing great losses; film stripping and copper surface treatment after film stripping have a greater impact on the nickel and gold layers. In summary, traditional processes have problems such as high cost and difficult to control position accuracy. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide a method for producing a metal protective layer pattern on the surface of a ceramic copper-clad laminate by directly removing the metal layer in non-required areas by using ultraviolet laser, thereby achieving high-precision surface metal layer pattern production.
[0004] The technical solution adopted by the present invention to solve its technical problem is: a method for producing a metal protective layer pattern on the surface of a ceramic copper-clad plate, comprising the following steps: a. producing a copper-clad plate with a pattern and a nickel-gold layer: first, the copper-clad plate is cleaned, then the pattern is transferred, and finally the copper is etched; the process of the nickel-gold layer includes any one of a nickel-gold plating process, a nickel-gold process, or a nickel-palladium-gold process; b. removing the unnecessary nickel-gold layer by ultraviolet laser: turning on an ultraviolet picosecond laser, and controlling the laser temperature to be constant within 25±2°C; then, filling the area to be processed, dividing it into blocks and converting it into a processing file; then, setting and adjusting the laser spot size to 30-50μm; next, setting the laser Process parameters: scanning spacing 0.02-0.05mm, filling angle 0-45°, progressive angle 90-135°, power factor 50-95%, laser frequency 300-1000KHz, engraving speed 100-2000, engraving times 1-5 times; finally, use the camera's CCD visual alignment system to identify the product positioning mark point alignment, the alignment accuracy of the alignment is controlled within 0.02mm, and start laser processing to remove the nickel-gold layer in the specified area; c. Surface treatment, i.e. cleaning and copper surface anti-oxidation treatment: the cleaning solution is: H2SO4 concentration 6-10%, temperature 20-40℃, spray pressure 1-2kg / cm 2 ; Antioxidant solution concentration 8-15%, temperature 20-40℃, soaking time 30-90s. d. Complete subsequent marking, slicing, inspection and packaging.
[0005] Furthermore, the process flow of nickel-gold plating in step a includes the following steps in sequence: pretreatment, degreasing, microetching, pre-impregnation, nickel plating and gold plating, and a water washing step is provided between each step of the process flow.
[0006] Furthermore, the nickel-gold plating process in step a includes the following steps in sequence: pretreatment, degreasing, microetching, pickling, pre-immersion, activation, post-immersion, nickel plating and gold plating, and a water washing step is provided between each step of the process.
[0007] Furthermore, the nickel-palladium-gold process flow in step a includes the following steps in sequence: pretreatment, degreasing, microetching, pre-immersion, activation, post-immersion, nickel immersion, palladium immersion and gold immersion, and a water washing step is provided between each step of the process flow.
[0008] Furthermore, in step a, copper etching includes the following processes in sequence: board entry, copper etching, compensation etching, film stripping, pickling, ultrasonic immersion, drying and board exit.
[0009] Furthermore, in step b, the wavelength of the ultraviolet picosecond laser is 355 nanometers, the laser constant temperature is 25±2°C, the processing spot size is 30-50μm, the scanning spacing is 0.02-0.05mm, the filling angle is 0-45°, the progressive angle is 90-135°, the power factor is 50%-95%, the laser frequency is 300-1000KHz, the engraving speed is 100-2000, and the engraving times are 1-5 times.
[0010] The beneficial effects of the present invention are as follows: In the traditional process, due to defects in the process flow design, there are many defects such as the difficulty in controlling the accuracy of the pattern production after the secondary film lamination, the risk of leakage in the pattern grooves, and high costs. In this solution, a new design is made for the entire process flow, wherein the entire surface of the copper clad laminate with patterns is first metallized, and then the metal layer is burned by ultraviolet laser to remove unnecessary areas, thereby finally realizing the production of copper surface metal layer patterns. Such a new process flow reduces the steps required for the production process flow, improves the positioning accuracy, and achieves high efficiency, environmental protection, and energy saving. It is particularly suitable for the preparation of ceramic copper clad laminates in IGBT power modules. DETAILED DESCRIPTION
[0011] The method for producing a metal protective layer pattern on the surface of a ceramic copper-clad laminate comprises the following steps: a. producing a copper-clad laminate with a pattern and a nickel-gold layer: first, the copper-clad laminate is cleaned, then the pattern is transferred, and finally the copper is etched; the process of the nickel-gold layer comprises any one of a nickel-gold plating process, a nickel-gold process or a nickel-palladium-gold process; b. removing the unnecessary nickel-gold layer by ultraviolet laser: turning on an ultraviolet picosecond laser, and controlling the laser temperature to be constant within 25±2°C; then, filling the area to be processed, dividing it into blocks and converting it into a processing file; then, setting and adjusting the laser spot size to 30-50μm; next, setting the laser process parameters: scanning The scanning spacing is 0.02-0.05mm, the filling angle is 0-45°, the progressive angle is 90-135°, the power factor is 50-95%, the laser frequency is 300-1000KHz, the engraving speed is 100-2000, and the number of engravings is 1-5 times; finally, the CCD visual alignment system of the camera is used to identify the product positioning mark point alignment, and the alignment accuracy of the alignment is controlled within 0.02mm, and the laser processing is started to remove the nickel-gold layer in the specified area; c. Cleaning and anti-oxidation of the copper surface: the cleaning solution is: H2SO4 concentration 6-10%, temperature 20-40℃, spray pressure 1-2kg / cm 2 ; Antioxidant solution concentration 8-15%, temperature 20-40°C, soaking time 30-90s. d. Complete subsequent scribing, slicing, inspection and packaging. Specifically, in step b, the wavelength of the ultraviolet picosecond laser is 355 nanometers, the laser constant temperature is 25±2°C, the processing spot size is 30-50μm, the scanning spacing is 0.02-0.05mm, the filling angle is 0-45°, the progressive angle is 90-135°, the power factor is 50%-95%, the laser frequency is 300-1000KHz, the engraving speed is 100-2000, and the number of engravings is 1-5 times. Among them, the CCD visual alignment system is a laser constant temperature control, using a temperature-controlled cold water tank constant temperature control, and the temperature fluctuation range is ±1°C.
[0012] The core of this solution is to improve the core of using ultraviolet laser to burn the metal layer, and then directly remove the metal layer in the non-required area, so as to achieve high-precision surface metal layer pattern production. Among them, for the production of copper-clad laminates with patterns and nickel-gold layers, any one of the nickel-gold plating process, nickel-gold process or nickel-palladium-gold process is selected. The copper-clad laminates with patterns produced by these three processes can be well adapted to the ultraviolet laser in the subsequent step b, and then the metal layer in the non-required area can be removed conveniently, greatly improving the production efficiency. Among them, the laser process parameters of the ultraviolet laser need to be set for the copper-clad laminate. The relevant parameter settings are the guarantee to ensure the removal of the metal layer in the non-required area of the copper-clad laminate.
[0013] In the surface treatment of step c, the surface metal protective layer includes silver, nickel, gold, nickel gold, nickel palladium gold, aluminum, titanium, chromium, etc., and its film layer can be produced by electroplating, chemical method, PVD sputtering coating and other processes.
[0014] This embodiment takes nickel-gold as an example for the production of the surface metal layer. Among them, the copper-clad laminate can be an AMB, DBC copper-clad laminate or an aluminum-clad laminate. The copper-clad laminate with graphics is a copper-clad laminate that has completed the graphics production and has alignment mark points. The production process of the copper-clad laminate with graphics is: copper-clad laminate cleaning → graphics transfer → copper etching, and AMB products also need to be etched for solder layer. Graphic transfer is to complete the graphic transfer production using the following process: protective film production → exposure → development. Copper etching is to use horizontal wet etching equipment for copper etching and film stripping, and its process is: board entry → copper etching → compensation etching → film stripping → pickling → ultrasonic immersion → drying → board exit. There are multi-level water washing treatments between each link. Solder layer etching is to use vertical wet etching equipment for solder layer etching, and its process is: board entry → degreasing → A solder layer etching → B solder layer etching → C solder layer etching → air drying → board exit; there are multi-level water washing treatments between each link. Among them, the preparation of patterned copper clad laminates is film pasting → exposure → development → copper etching → film stripping → solder layer etching → metallization treatment of the entire board surface.
[0015] The nickel-gold is usually made by three processes: nickel-plated gold, nickel-plated gold or nickel-palladium gold, and the corresponding processes are as follows: nickel-plated gold: pretreatment → degreasing → micro-etching → pre-dip → nickel-plating → gold-plating. Nickel-plated gold: pretreatment → degreasing → micro-etching → pickling → pre-dip → activation → post-dip → nickel-plated → gold-plated. Nickel-palladium gold: pretreatment → degreasing → micro-etching → pre-dip → activation → post-dip → nickel-plated → palladium-plated → gold-plated.
[0016] Among them, in step a, copper etching includes the following processes in sequence: board entry, copper etching, compensation etching, film stripping, pickling, ultrasonic immersion, drying and board exit.
Claims
1. A method for producing a metal protective layer pattern on the surface of a ceramic copper-clad laminate, characterized in that: The steps include: a. Production of copper-clad laminate with patterns and nickel-gold layer: first, the copper-clad laminate is cleaned, then the pattern is transferred, and finally the copper is etched; the process of the nickel-gold layer includes any one of nickel-gold plating process, nickel-gold process or nickel-palladium-gold process; b. Remove the unnecessary nickel-gold layer with ultraviolet laser: turn on the ultraviolet picosecond laser, and control the laser temperature to be constant within 25±2℃; then, fill the area to be processed, divide it into blocks and convert it into a processing file; then, set and adjust the laser spot size to 30-50μm; next, set the laser process parameters: scanning spacing 0.02-0.05mm, filling angle 0-45°, progressive angle 90-135°, power factor 50-95%, laser frequency 300-1000KHz, engraving speed 100-2000, engraving times 1-5 times; finally, use the camera's CCD visual alignment system to identify the product positioning mark point alignment, the alignment accuracy of the alignment is controlled within 0.02mm, and start laser processing to remove the nickel-gold layer in the specified area; c. Surface treatment, i.e. cleaning and anti-oxidation treatment of copper surface: the cleaning solution is: H2SO4 concentration 6-10%, temperature 20-40℃, spray pressure 1-2kg / cm 2 ; Antioxidant solution concentration 8-15%, temperature 20-40℃, soaking time 30-90s; d. Complete subsequent marking, slicing, inspection and packaging.
2. The method for producing a metal protective layer pattern on the surface of a ceramic copper-clad laminate according to claim 1, characterized in that: The process flow of nickel-gold plating in step a includes the following steps in sequence: pretreatment, degreasing, microetching, pre-dipping, nickel plating and gold plating, and a water washing step is provided between each step of the process flow.
3. The method for producing a metal protective layer pattern on the surface of a ceramic copper-clad laminate according to claim 1, characterized in that: The nickel-gold plating process in step a includes the following steps in sequence: pretreatment, degreasing, microetching, pickling, pre-immersion, activation, post-immersion, nickel plating and gold plating, and a water washing step is provided between each step of the process.
4. The method for producing a metal protective layer pattern on the surface of a ceramic copper-clad laminate according to claim 1, characterized in that: The nickel-palladium-gold process flow in step a includes the following steps in sequence: pretreatment, degreasing, microetching, pre-immersion, activation, post-immersion, nickel immersion, palladium immersion and gold immersion, and a water washing step is provided between each step of the process flow.
5. The method for producing a metal protective layer pattern on the surface of a ceramic copper-clad laminate according to any one of claims 1 to 4, characterized in that: In step a, copper etching includes the following processes in sequence: board entry, copper etching, compensation etching, film stripping, pickling, ultrasonic immersion, drying and board exit.
6. The method for producing a metal protective layer pattern on the surface of a ceramic copper-clad laminate according to any one of claims 1 to 4, characterized in that: In step b, the wavelength of the ultraviolet picosecond laser is 355 nanometers, the laser constant temperature is 25±2°C, the processing spot size is 30-50μm, the scanning spacing is 0.02-0.05mm, the filling angle is 0-45°, the progressive angle is 90-135°, the power factor is 50%-95%, the laser frequency is 300-1000KHz, the engraving speed is 100-2000, and the engraving times are 1-5 times.
Citation Information
Cited By
Ceramic copper-clad plate pattern manufacturing method
CN120376421A