Display panel and preparation method thereof, display device and mask plate
By designing a thinned structure in the packaging part of the display panel, the problem that the packaging part cannot completely fill the evaporated shadow area is solved, and the reliability of the display panel and the protection of the light-emitting device are improved.
Patent Information
- Application Number
- CN202410737868.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-07
- Publication Date
- 2024-10-01
AI Technical Summary
The reliability of existing display panels is low, and the packaging part cannot be completely filled in the evaporation shadow area, resulting in insufficient strength and residual organic glue, which affects the protection and display effect of the light-emitting device.
By pre-designing the thinned encapsulation part when preparing the display panel, and controlling the opening and thickness of the groove, it can better fill the evaporation shadow area, ensuring the strength of the encapsulation part and the protection of the light-emitting device.
The strength of the packaging part in the evaporation shadow area is improved, organic glue residue is avoided, and the reliability of the display panel and the protection of the light-emitting device are improved.
Smart Images

Figure CN118742086A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of display technology, and in particular to a display panel and a method for preparing the same, a display device, and a mask plate. Background Art
[0002] In recent years, benefiting from the rapid development of information technology, display technology has also achieved rapid development. However, the reliability of display products still needs to be further improved. Summary of the invention
[0003] In view of this, the embodiments of the present application provide a display panel and a method for manufacturing the same, a display device, and a mask plate, which solve the problem of low reliability of display products in the prior art.
[0004] In a first aspect, the present application provides a display panel, comprising: a substrate; an isolation structure, located on one side of the substrate, the isolation structure enclosing an isolation opening, the side wall of the isolation structure defining a concave vapor deposition shadow area; a light-emitting device, at least partially located in the isolation opening; and a packaging portion, located on the side of the light-emitting device away from the substrate and filling the vapor deposition shadow area; the packaging portion comprises a continuous portion and a filling portion, the continuous portion comprises a concave-convex sub-portion, the concave-convex sub-portion covers the side wall of the isolation structure close to the isolation opening, the concave-convex sub-portion encloses a groove concave toward the isolation structure, the groove is located in the vapor deposition shadow area, and the filling portion fills the groove; the thickness of the concave-convex sub-portion located at the groove is greater than or equal to 0.1 micrometers and less than or equal to 0.7 micrometers.
[0005] In combination with the first aspect, in some possible implementations, in the thickness direction of the substrate, the opening width of the groove is greater than or equal to 1 micron and less than or equal to 2 microns; preferably, in the direction parallel to the substrate, the depth of the groove is greater than or equal to 1 micron and less than or equal to 2 microns; preferably, in the thickness direction of the substrate, the minimum width of the filling portion is greater than or equal to 1 micron and less than or equal to 2 microns; preferably, in the direction parallel to the substrate, the length of the filling portion is greater than or equal to 1 micron and less than or equal to 2 microns.
[0006] In combination with the first aspect, in some possible implementations, the concave-convex sub-portions extend to the side of the isolation structure facing away from the substrate; preferably, adjacent concave-convex sub-portions are disconnected on the side of the isolation structure facing away from the substrate; preferably, the filling portion extends to the side of the isolation structure facing away from the substrate, and the filling portion covers at least part of the concave-convex sub-portion on the side of the isolation structure facing away from the substrate.
[0007] In combination with the first aspect, in some possible implementations, the isolation structure includes a first part and a second part stacked together, the second part is located on the side of the first part facing away from the substrate, and the orthographic projection of the first part on the substrate is located within the range of the orthographic projection of the second part on the substrate; in the thickness direction of the substrate, the ratio of the opening width of the groove to the height of the first part is greater than or equal to 0.4 and less than or equal to 0.8; preferably, in the thickness direction of the substrate, the height of the first part is greater than or equal to 1.5 microns and less than or equal to 2.5 microns; preferably, the height of the first part is 2 microns.
[0008] In combination with the first aspect, in some possible implementations, the light-emitting device includes a first electrode and a second electrode stacked together, the second electrode being located on a side of the first electrode close to a substrate; the continuous portion also includes a flat sub-portion and a connecting sub-portion, the connecting sub-portion connecting the flat sub-portion and the concave-convex sub-portion, the orthographic projection of the flat sub-portion on the substrate at least partially overlaps with the orthographic projection of the second electrode on the substrate; preferably, the concave-convex sub-portion surrounds the flat sub-portion.
[0009] In combination with the first aspect, in some possible implementations, the thickness of the flat sub-portion is greater than or equal to 0.5 micrometers and less than or equal to 0.7 micrometers.
[0010] In combination with the first aspect, in some possible implementations, the material of the continuous portion includes an inorganic material; preferably, the material of the continuous portion and the filling portion is the same; preferably, the material of the continuous portion includes any one of silicon oxide and silicon nitride.
[0011] In combination with the first aspect, in some possible implementations, the isolation structure includes a first part and a second part stacked together, the second part is located on the side of the first part facing away from the substrate, and the orthographic projection of the first part on the substrate is located within the orthographic projection range of the second part on the substrate; preferably, the isolation structure also includes a third part, located on the side of the first part close to the substrate; preferably, the orthographic projection of the first part on the substrate is located within the orthographic projection range of the third part on the substrate; preferably, the material of the first part includes aluminum or copper or silver; preferably, the material of the second part includes titanium or molybdenum; preferably, the material of the third part includes molybdenum or titanium.
[0012] In combination with the first aspect, in some possible implementations, in the thickness direction of the substrate, the height of the first portion is greater than or equal to 1.5 microns and less than or equal to 2.5 microns; preferably, the height of the first portion is 2 microns.
[0013] In combination with the first aspect, in some possible implementations, the light-emitting device includes a stacked first electrode and a second electrode, and the second electrode is located on a side of the first electrode close to the substrate; preferably, the light-emitting device also includes at least one stacked light-emitting functional layer, which is located between the first electrode and the second electrode; preferably, the display panel also includes a pixel definition layer, which is stacked on a side of the isolation structure close to the substrate; preferably, the pixel definition layer covers an edge area of the second electrode.
[0014] In combination with the first aspect, in some possible implementations, the display panel further includes an organic encapsulation layer, which is located on the side of the encapsulation part facing away from the substrate; preferably, the orthographic projection of the organic encapsulation layer on the substrate covers the orthographic projection of the encapsulation part on the substrate; preferably, the display panel further includes an inorganic encapsulation layer, which is located on the side of the organic encapsulation layer facing away from the substrate; preferably, the orthographic projection of the inorganic encapsulation layer on the substrate covers the orthographic projection of the organic encapsulation layer on the substrate.
[0015] The second aspect of the present application provides another display panel, comprising: a substrate; an isolation structure, located on one side of the substrate, the isolation structure enclosing an isolation opening; the isolation structure comprising a first portion and a second portion stacked together, the second portion being located on a side of the first portion away from the substrate, the orthographic projection of the first portion on the substrate being located within the range of the orthographic projection of the second portion on the substrate; the sidewalls of the first portion and the sidewalls of the second portion enclose and define a concave vapor deposition shadow area; a light-emitting device, at least partially located in the isolation opening; and a packaging portion, located on a side of the light-emitting device away from the substrate and filling the vapor deposition shadow area; the packaging portion comprises a continuous portion and a filling portion, the continuous portion comprising a concave-convex sub-portion, the concave-convex sub-portion covering the sidewall of the isolation structure close to the isolation opening, the concave-convex sub-portion enclosing a groove concave toward the isolation structure, the groove being located in the vapor deposition shadow area, and the filling portion filling the groove; in the thickness direction of the substrate, the ratio of the opening width of the groove to the height of the first portion is greater than or equal to 0.4 and less than or equal to 0.8.
[0016] Preferably, the thickness of the concave-convex part located at the groove is greater than or equal to 0.1 micron and less than or equal to 0.7 micron; preferably, in the thickness direction of the substrate, the opening width of the groove is greater than or equal to 1 micron and less than or equal to 2 microns; preferably, in the direction parallel to the substrate, the depth of the groove is greater than or equal to 1 micron and less than or equal to 2 microns; preferably, in the thickness direction of the substrate, the minimum width of the filling part is greater than or equal to 1 micron and less than or equal to 2 microns; preferably, in the direction parallel to the substrate, the length of the filling part is greater than or equal to 1 micron and less than or equal to 2 microns.
[0017] The third aspect of the present application provides a mask plate, comprising: a substrate layer, the substrate layer comprising a first shielding portion, a plurality of hollow portions and a second shielding portion connected in sequence, the plurality of hollow portions are arranged in sequence around the periphery of the first shielding portion, and the second shielding portion surrounds the periphery of the hollow portions; the thickness of the first shielding portion is greater than the thickness of the second shielding portion.
[0018] In combination with the third aspect, in some possible implementations, the ratio of the thickness of the second shielding portion to the thickness of the first shielding portion is greater than or equal to 0.2 and less than or equal to 0.6; preferably, the difference in thickness between the first shielding portion and the second shielding portion is greater than or equal to 50 microns and less than or equal to 100 microns; preferably, the thickness of the first shielding portion is greater than or equal to 100 microns and less than or equal to 200 microns; preferably, the thickness of the first shielding portion is 150 microns; preferably, the thickness of the second shielding portion is greater than or equal to 50 microns and less than or equal to 100 microns.
[0019] In combination with the third aspect, in some possible implementations, the substrate layer also includes a connecting portion, located between adjacent hollow portions, and the connecting portion connects the first shielding portion and the second shielding portion; preferably, in the direction from the first shielding portion to the second shielding portion, the length of the connecting portion is greater than or equal to 10 microns and less than or equal to 30 microns; preferably, the thickness of the connecting portion is the same as the thickness of the first shielding portion; or, the thickness of the connecting portion is the same as the thickness of the second shielding portion; preferably, in the arrangement direction of the multiple hollow portions, the width of the connecting portion is greater than or equal to 5 microns and less than or equal to 10 microns.
[0020] In combination with the third aspect, in some possible implementations, the first shielding portion, the multiple hollow portions and the second shielding portion constitute a repeating unit; the mask plate includes multiple repeating units and a third shielding portion, and the third shielding portion is located between the second shielding portions of adjacent repeating units; preferably, the thickness of the third shielding portion is equal to the thickness of the first shielding portion.
[0021] The fourth aspect of the present application provides a method for preparing a display panel, comprising: preparing an isolation structure and a light-emitting device on a substrate, the isolation structure enclosing an isolation opening, the light-emitting device being at least partially located in the isolation opening, and the sidewall of the isolation structure defining a concave vapor deposition shadow area; the isolation structure comprising a first portion and a second portion stacked together, the second portion being located on a side of the first portion facing away from the substrate, and an orthographic projection of the first portion on the substrate being located within the range of an orthographic projection of the second portion on the substrate; preparing a packaging portion on a side of the light-emitting device facing away from the substrate, the packaging portion filling the vapor deposition shadow area, the packaging portion comprising a continuous portion and a filling portion, the continuous portion comprising a concave-convex sub-portion, the concave-convex sub-portion covering the sidewall of the isolation structure close to the isolation opening, the concave-convex sub-portion enclosing a concave groove toward the isolation structure, the groove being located in the vapor deposition shadow area, and the filling portion filling the groove; wherein the thickness of the concave-convex sub-portion located at the groove is greater than or equal to 0.1 micrometers and less than or equal to 0.7 micrometers; and / or in the thickness direction of the substrate, the ratio of the opening width of the groove to the height of the first portion is greater than or equal to 0.4 and less than or equal to 0.8.
[0022] In combination with the fourth aspect, in some possible implementations, preparing an isolation structure and a light-emitting device on a substrate includes: preparing a second electrode on the substrate; preparing an isolation structure on the substrate; sequentially preparing a light-emitting layer and a first electrode in the isolation opening; preferably, after preparing the second electrode on the substrate and before preparing the isolation structure on the substrate, it also includes: preparing a pixel definition layer on the substrate, the pixel definition layer enclosing a pixel opening, and the pixel opening exposing at least a portion of the second electrode; preferably, preparing a packaging portion on the side of the light-emitting device away from the substrate includes: preparing a continuous portion on the side of the light-emitting device away from the substrate, the continuous portion including a concave-convex sub-portion, a connecting sub-portion and a flat sub-portion connected in sequence, and the flat The orthographic projection of the sub-portion on the substrate at least partially overlaps with the orthographic projection of the second electrode on the substrate, the concave-convex sub-portion covers the side wall of the isolation structure facing the isolation opening, the concave-convex sub-portion encloses a groove concave toward the isolation structure, and the groove is located within the evaporation shadow area of the evaporation shadow space; using the mask plate provided by any embodiment of the present application, a filling portion is prepared on the side of the continuous portion away from the substrate, and the filling portion fills the groove, wherein the orthographic projection of the first blocking portion on the substrate overlaps with the orthographic projection of the pixel opening on the substrate, the orthographic projection of the second blocking portion on the substrate overlaps with the orthographic projection of the isolation structure on the substrate at least partially, and the orthographic projection of the groove on the substrate is located within the orthographic projection range of the hollow portion on the substrate.
[0023] In combination with the fourth aspect, in some possible implementations, the preparation method further includes: sequentially preparing an organic encapsulation layer and an inorganic encapsulation layer on a side of the encapsulation portion facing away from the substrate.
[0024] A fifth aspect of the present application provides a display device, comprising a display panel provided by any of the above embodiments.
[0025] According to the display panel and its preparation method, display device, and mask provided by the embodiment of the present application, by pre-designing the thinned encapsulation part, that is, performing a thinning design on the basis of the conventional encapsulation part, in the process of preparing the display panel, the encapsulation part is prepared based on the thinned thickness, so that the thickness of the concave-convex sub-part covering the side wall of the isolation structure is within the range of 0.1-0.7 microns. In this way, the opening of the groove formed by the concave-convex sub-part covering the side wall of the isolation structure is large enough to better fill the evaporation shadow area, ensure that the encapsulation part fills the evaporation shadow area, and avoid the encapsulation part from forming a groove in the evaporation shadow area, thereby improving the strength of the encapsulation part in the evaporation shadow area, improving the protection of the light-emitting device, avoiding organic glue residue in the evaporation shadow area, and thus improving the reliability of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a schematic diagram of the cross-sectional structure of a display panel in the related art.
[0027] Figure 2aThis is a schematic diagram of the top structure of the display panel provided in the first embodiment of the present application.
[0028] Figure 2b for Figure 2a The cross-sectional structure diagram of the display panel along line A1A2 is shown.
[0029] Figure 3a A schematic diagram of the cross-sectional structure of a display panel provided in the second embodiment of the present application.
[0030] Figure 3b for Figure 3a A partial enlarged view of the S region of the display panel is shown.
[0031] Figure 4 A schematic diagram of the cross-sectional structure of a display panel provided in the third embodiment of the present application.
[0032] Figure 5 A schematic diagram of the cross-sectional structure of a display panel provided in the fourth embodiment of the present application.
[0033] Figure 6 A schematic diagram of the cross-sectional structure of a display panel provided in the fifth embodiment of the present application.
[0034] Figure 7a A schematic diagram of a partial top view of the structure of a mask plate provided in one embodiment of the present application.
[0035] Figure 7b for Figure 7a The cross-sectional structure diagram of the mask plate along the A1A2 line is shown.
[0036] Figure 7c for Figure 7a A local enlarged view of the N area of the mask shown.
[0037] Figure 8 A flow chart of a method for preparing a display panel provided in one embodiment of the present application.
[0038] Figure 9a-9c For execution Figure 8 Schematic diagram of the structure of the intermediate product obtained during the preparation method shown.
[0039] Fig.10 A schematic diagram of the structure of a display device provided in one embodiment of the present application. DETAILED DESCRIPTION
[0040] As mentioned in the background technology, display technology has achieved rapid development in recent years. For example, the preparation process of light-emitting devices in current display panels does not need to use fine metal masks (FMM). Instead, the isolation structure inside the panel is used to separate adjacent light-emitting devices to achieve the independence of the light-emitting devices. Accordingly, the light-emitting devices use independent packaging technology, which can effectively achieve display diversification.
[0041] Figure 1 FIG. 1 is a schematic diagram of a cross-sectional structure of a display panel in the related art. Figure 1 As shown, a vapor deposition shadow area Q is formed at the side wall of the partition structure 12. The vapor deposition shadow area Q causes the functional layer vapor deposited above the partition structure 12 to be disconnected at the partition structure 12, thereby realizing the independence of the light-emitting device 13. At the same time, the encapsulation part 14 will form a depression 140 in the vapor deposition shadow area Q, and cannot completely fill the vapor deposition shadow area Q. In this case, on the one hand, the strength of the encapsulation part 14 is insufficient, and film separation is prone to occur. On the other hand, the protection ability of the encapsulation part 14 to the light-emitting device 12 is reduced. On the other hand, the organic glue in the depression 140 is not easy to remove cleanly in the subsequent process. Any of the above three aspects may affect the reliability of the packaging.
[0042] Although there is a solution for completely filling the evaporation shadow area Q in the related art, the filling effect is poor, and there are often unfilled voids in the evaporation shadow area Q.
[0043] In view of this, the present application provides a display panel and a method for preparing the same, a display device and a mask plate, by pre-designing a thinned encapsulation part, that is, performing a thinning design on the basis of a conventional encapsulation part, and in the process of preparing the display panel, preparing the encapsulation part based on the thinned thickness, so that the thickness of the concave-convex sub-part covering the side wall of the isolation structure is within the range of 0.1-0.7 microns. In this way, the opening of the recess 140 is large enough to facilitate the subsequent better filling of the evaporation shadow area, ensuring that the encapsulation part fills the evaporation shadow area, and avoiding the encapsulation part from forming a groove in the evaporation shadow area, thereby improving the strength of the encapsulation part in the evaporation shadow area, improving the protection of the light-emitting device, avoiding organic glue residue in the evaporation shadow area, and thus improving the reliability of the display panel.
[0044] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0045] In the accompanying drawings, the sizes of layers and regions may be exaggerated for clarity of illustration. It is understood that when a structure is referred to as being "on or under" another structure, the structure may be directly on or under the other structure, or there may be intermediate structures. The same reference numerals always indicate the same structure. The structures mentioned herein include any of a film layer, an element, a device, a component, and an assembly.
[0046] When a structure is referred to as being “connected” to another structure, the structure may be directly connected to the other structure or indirectly connected to the other structure with one or more intervening structures interposed therebetween.
[0047] Figure 2a This is a schematic diagram of the top structure of the display panel provided in the first embodiment of the present application. Figure 2b for Figure 2a The cross-sectional structure diagram of the display panel along the A1A2 line is shown. Figure 2a and Figure 2b As shown, the display panel includes: a substrate 11, an isolation structure 12, a light-emitting device 13 and a packaging part 14. The isolation structure 12 is located on one side of the substrate 11, and the isolation structure 12 encloses an isolation opening 120. The sidewall of the isolation structure 12 defines a concave vapor deposition shadow area Q. The light-emitting device 13 is at least partially located in the isolation opening 120. The packaging part 14 is located on the side of the light-emitting device 13 away from the substrate 11, and fills the vapor deposition shadow area Q.
[0048] The substrate 11 may be a base substrate or an array substrate. The array substrate refers to a substrate structure having pixel circuits formed on a base substrate.
[0049] In some embodiments, the base substrate may be a glass-based substrate.
[0050] In some embodiments, the base substrate may include an organic resin material such as epoxy, triazine, silicone, or polyimide. For example, the base substrate may be polyimide.
[0051] In some embodiments, the substrate substrate may also include a ceramic material such as silicon nitride, aluminum nitride or aluminum oxide, or include a metal or a metal compound. The light-emitting device 13 may be an organic light-emitting diode (OLED), a micro light-emitting diode (Micro LED), a quantum dot light-emitting diode (QLED), etc. The light-emitting device 13 may be a light-emitting device of various colors, such as a red light-emitting device R, a green light-emitting device G, a blue light-emitting device B, etc. The light-emitting device 13 includes a first electrode 131, at least one light-emitting functional layer 132, and a second electrode 133 stacked in sequence in a direction gradually approaching the substrate 11. Exemplarily, the first electrode 131 is an anode and the second electrode 133 is a cathode. Alternatively, the first electrode 131 is a cathode and the second electrode 133 is an anode.
[0052] At least one light-emitting functional layer 132 includes a light-emitting layer, and may also include at least one of a hole injection layer (HIL), a hole transport layer (HTL), and an electron blocking layer (EBL) located between the anode and the light-emitting layer, and at least one of an electron injection layer (EIL), an electron transport layer (ETL), and a hole blocking layer (HBL) located between the cathode and the light-emitting layer. The light-emitting functional layers 132 of different light-emitting devices 13 are disconnected at the isolation structure 12.
[0053] The sidewall of the isolation structure 12 defines an evaporation shadow region Q, which is a space that cannot be reached by the evaporation material when a film layer is prepared on the isolation structure 12 by the evaporation process. Therefore, the light-emitting functional layer 132 evaporated on the isolation structure 12 cannot reach the evaporation shadow region Q, so that the light-emitting functional layer 132 is disconnected in the evaporation shadow region Q, thereby isolating the adjacent light-emitting devices 13.
[0054] The isolation structure 12 includes a first portion 121 and a second portion 122 stacked together, wherein the first portion 121 is located on the side of the second portion 122 close to the substrate 11, and the orthographic projection of the second portion 122 on the substrate 11 covers the orthographic projection of the first portion 121 on the substrate 11, that is, the orthographic projection of the first portion 121 on the substrate 11 is located within the orthographic projection of the second portion 122 on the substrate 11. The first portion 121 can be designed as an independent film layer, that is, there is no physical interface inside the first portion 121, and each portion is composed of the same material. Alternatively, the first portion 121 can be designed to be composed of at least two stacked film layers. For example, the first portion 121 is formed by stacking two conductive film layers, and the material of the second portion 122 can be an organic material, an inorganic material, or a metal material. In the case where the second portion 122 is a metal material, the material of the second portion 122 can be titanium. Exemplarily, the material of the first portion 121 includes aluminum, copper, or silver. The material of the second portion 122 includes titanium or molybdenum.
[0055] In some other embodiments, the cross-sectional shape of the isolation structure 12 may be an inverted trapezoid.
[0056] In one embodiment, the first portion 121 includes a conductive sub-portion. For example, the first portion 121 is a conductive structure as a whole, or a part of the first portion 121 is a conductive structure, that is, the conductive structure is used as its conductive sub-portion. The first electrode 131 of the light emitting device 13 overlaps the conductive sub-portion.
[0057] In one embodiment, the isolation structure 12 further includes a third portion 123, which is located on a side of the first portion 121 close to the substrate 11, and the orthographic projection of the first portion 121 on the substrate 11 is located within the orthographic projection range of the third portion 123 on the substrate 11. Exemplarily, the cross-sectional shape of the isolation structure 12 may be an I-shaped shape. Exemplarily, the material of the first portion 121 is aluminum, and the material of the third portion 123 is molybdenum or titanium.
[0058] The isolation openings 120 and the light-emitting devices 13 may correspond one to one, or may be arranged one to many. For example, part of the isolation openings 120 and the light-emitting devices 13 correspond one to one, and the rest of the isolation openings 120 and the light-emitting devices 13 are arranged one to many. Exemplarily, the red light-emitting device R and the blue light-emitting device B correspond one to one to the isolation openings 120, respectively, that is, one red light-emitting device R is arranged in one isolation opening 120, and one blue light-emitting device B is arranged in one isolation opening 120. The green light-emitting device G and the isolation opening 120 are arranged many to one, that is, multiple green light-emitting devices G are located in the same isolation opening 120, for example, two green light-emitting devices G are located in the same isolation opening 120.
[0059] The packaging portion 14 fills the evaporation shadow area Q, that is, the packaging portion 14 completely fills the evaporation shadow area Q, that is, the packaging portion 14 is a solid structure in the evaporation shadow area Q without holes, grooves, etc.
[0060] like Figure 2b As shown, the display panel may further include a pixel definition layer 15, which is stacked on the side of the isolation structure 12 close to the substrate 11. The pixel definition layer 15 encloses a pixel opening, and the orthographic projection of the pixel opening on the substrate 11 is located within the orthographic projection range of the isolation opening 120 on the substrate 11. Exemplarily, the pixel definition layer 15 covers the edge area of the second electrode 133, and the central area of the second electrode 133 is exposed to the pixel opening and the isolation opening 120.
[0061] According to the display panel provided in this embodiment, the packaging part 14 is provided to fill the evaporation shadow area Q, thereby improving the strength of the packaging part 14 in the evaporation shadow area Q, improving the protection of the light-emitting device 13, and further improving the reliability of the display panel.
[0062] Figure 2a and Figure 2b The packaging part 14 in the embodiment can be an integral structure, that is, the packaging part 14 is formed as a whole at one time; or it can be disassembled into different sub-parts and prepared separately. Among them, for the packaging part 14 with an integral structure, in order to ensure that the packaging part 14 fills the vapor deposition shadow area Q, it is necessary to control the packaging part 14 to meet certain thickness requirements. For the packaging part 14 composed of different sub-parts, the requirements for thickness are relatively broad.
[0063] Figure 3a This is a schematic diagram of the cross-sectional structure of a display panel provided in the second embodiment of the present application. As shown in FIG3 , the display panel and Figure 2b The difference of the display panel shown is that, in this embodiment, the encapsulation portion 14 includes a continuous portion 141 and a filling portion 142. The continuous portion 141 includes a concave-convex sub-portion 1411, which covers the side wall of the isolation structure 12 close to the isolation opening 120, and the concave-convex sub-portion 1411 encloses a groove G that is concave toward the isolation structure 12, and the groove G is located in the vapor deposition shadow area Q. The filling portion 142 fills the groove G.
[0064] In order to facilitate filling the filling part 142 into the groove G, the thickness of the formed continuous part 141 is reduced compared to the thickness of the conventional packaging part, so that the groove G is larger, thereby facilitating the filling of the filling part 142. Therefore, in this embodiment, the thickness D0 of the concave-convex sub-part 1411 located at the groove G is greater than or equal to 0.1 micron and less than or equal to 0.7 micron. Exemplarily, the thickness D0 of the concave-convex sub-part 1411 located at the groove G can be 0.3 micron, 0.4 micron, 0.5 micron or 0.6 micron, etc.
[0065] In one embodiment, the material of the continuous portion 141 includes an inorganic material, such as silicon nitride, silicon oxide, and the like.
[0066] In one embodiment, the continuous portion 141 and the filling portion 142 are made of the same material, such as silicon nitride, silicon oxide, or the like.
[0067] In one embodiment, the material of the continuous portion 141 includes any one of silicon oxide and silicon nitride.
[0068] In this embodiment, the encapsulation part 14 is implemented as a continuous part 141 and a filling part 142. The continuous part 141 is integrally formed, and a groove G is formed in the vapor deposition shadow area Q. In this case, the continuous part 141 can be prepared by a conventional encapsulation process to achieve compatibility with conventional technologies. At the same time, the filling part 142 is used to fill the groove G, so that the encapsulation part 14 fills the vapor deposition shadow area Q. At the same time, the filling part 142 mainly fills the groove G during the filling process, which has little effect on the light-emitting device 13, thereby not affecting the light output of the light-emitting device 13, and ensuring the display effect.
[0069] Figure 3b for Figure 3a The S area of the display panel is shown as a partial enlarged view. Figure 3a and Figure 3b As shown, in the thickness direction of the substrate 11, in the thickness direction of the substrate 11, the ratio of the opening width D1 of the groove to the height D3 of the first part 121 is greater than or equal to 0.4 and less than or equal to 0.8; for example, the ratio between the two can be 0.4, 0.42, 0.5, 0.55, 0.6, 0.67, 0.72, 0.78 or 0.8.
[0070] Exemplarily, the opening width D1 of the groove G is greater than or equal to 1 micron and less than or equal to 2 microns. The opening width D1 can be measured by the width of the narrowest position of the groove G in the thickness direction of the substrate 11. In this case, in the thickness direction of the substrate 11, the minimum width of the filling portion 142 located at the groove G is greater than or equal to 1 micron and less than or equal to 2 microns. For example, the opening width D1 is 1.3 microns, 1.5 microns, 1.7 microns, etc. Correspondingly, the width of the filling portion 142 located at the groove G is 1.3 microns, 1.5 microns, 1.7 microns, etc.
[0071] Exemplary, combined Figure 3a and Figure 3b As shown, in the thickness direction of the substrate 11, the height D3 of the first portion 121 is greater than or equal to 1.5 micrometers and less than or equal to 2.5 micrometers. For example, the height D3 of the first portion 121 is 1.7 micrometers, 2 micrometers, 2.3 micrometers, and so on.
[0072] In one embodiment, in combination Figure 3a and Figure 3bAs shown, in the direction parallel to the substrate 11, the depth D2 of the groove G is greater than or equal to 1 micron and less than or equal to 2 microns. The depth D2 can be measured by the maximum depth of the groove G in the direction parallel to the substrate 11. In this case, in the direction parallel to the substrate 11, the length of the filling portion 142 located at the groove G is greater than or equal to 1 micron and less than or equal to 2 microns. For example, the depth D2 is 1.3 microns, 1.5 microns, 1.7 microns, etc. Correspondingly, the length of the filling portion 142 located at the groove G is 1.3 microns, 1.5 microns, 1.7 microns, etc.
[0073] Combination Figure 3a and Figure 3b As shown, the continuous portion 141 also includes a flat sub-portion 1412 and a connecting sub-portion 1413, and the connecting sub-portion 1413 connects the flat sub-portion 1412 and the concave-convex sub-portion 1411. The orthographic projection of the flat sub-portion 1412 on the substrate 11 overlaps at least partially with the orthographic projection of the second electrode 133 on the substrate 11. Exemplarily, the flat sub-portion 1412 is parallel to the second electrode 133. The flat sub-portion 1412 is parallel to the substrate 11. The concave-convex sub-portion 1411 surrounds the flat sub-portion 1412. The concave-convex sub-portion 1411 and the flat sub-portion 1412 are integrally formed. In this embodiment, the thickness D4 of the flat sub-portion 1412 is greater than or equal to 0.5 microns and less than or equal to 0.7 microns. For example, the thickness D4 is 0.55 microns, 0.6 microns, 0.7 microns, etc. The thickness of the flat sub-portion 1412 is the thickness of the thinned continuous portion 141 designed in the related art. The continuous portion 141 is prepared according to the thickness of the flat sub-portion 1412, and the concave-convex sub-portion 1411 that meets the thickness requirement can be obtained. In this embodiment, the thickness of the concave-convex sub-portion is required to be greater than or equal to 0.1 micrometers and less than or equal to 0.7 micrometers.
[0074] Figure 4 FIG. 1 is a schematic diagram of a cross-sectional structure of a display panel provided in the third embodiment of the present application. Figure 4 The display panel and Figure 3a The difference of the display panel shown is that, in this embodiment, the concave-convex sub-portions 1411 extend to the side of the isolation structure 12 away from the substrate 11. Exemplarily, adjacent concave-convex sub-portions 1411 are disconnected at the side of the isolation structure 12 away from the substrate 11.
[0075] In one embodiment, Figure 4 As shown, the filling portion 142 extends to the side of the isolation structure 12 away from the substrate 11, and the filling portion 142 covers at least part of the concave-convex sub-portion 1411 on the side of the isolation structure 12 away from the substrate 11. Exemplarily, on the side of the isolation structure 12 away from the substrate 11, the sidewalls of the concave-convex sub-portion 1411 and the filling portion 143 are flush. In this way, the mask plate used in the preparation process of the concave-convex sub-portion 1411 and the filling portion 143 has openings at corresponding positions, which is convenient for mask plate design.
[0076] In one embodiment, the sidewall of the filling portion 142 close to the isolation opening 120 is a plane. Further, in one embodiment, the plane is parallel to the sidewall of the first portion 121 .
[0077] Figure 5 FIG. 4 is a schematic diagram of a cross-sectional structure of a display panel provided in the fourth embodiment of the present application. Figure 5 The display panel and Figure 4 The difference of the display panel shown is that, in this embodiment, on the side of the isolation structure 12 facing away from the substrate 11 , the filling portion 142 covers the side wall of the concave-convex sub-portion 1411 .
[0078] Figure 6 FIG. 5 is a schematic diagram of a cross-sectional structure of a display panel provided in the fifth embodiment of the present application. Figure 6 The display panel shown is based on the display panel provided in any of the above embodiments. Figure 3a Taking the display panel shown as an example, it also includes an organic encapsulation layer 16, which is located on the side of the encapsulation part 14 away from the substrate 11. Exemplarily, the orthographic projection of the organic encapsulation layer 16 on the substrate 11 covers the orthographic projection of the encapsulation part 14 on the substrate 11.
[0079] In one embodiment, the display panel further includes an inorganic encapsulation layer 17, which is located on the side of the organic encapsulation layer 16 away from the substrate 11. Exemplarily, the orthographic projection of the inorganic encapsulation layer 17 on the substrate 11 covers the orthographic projection of the organic encapsulation layer 16 on the substrate 11. In this way, the encapsulation part 14, the organic encapsulation layer 16 and the inorganic encapsulation layer 17 constitute an encapsulation structure as a whole.
[0080] The present application also provides another display panel. Figure 3a and Figure 3bAs shown, the display panel includes: a substrate 11; an isolation structure 12, located on one side of the substrate 11, the isolation structure 12 encloses an isolation opening 120; the isolation structure 12 includes a first portion 121 and a second portion 122 stacked, the second portion 122 is located on the side of the first portion 121 away from the substrate 11, and the orthographic projection of the first portion 121 on the substrate 11 is located within the orthographic projection range of the second portion 122 on the substrate 11; the side wall of the first portion 121 and the side wall of the second portion 122 enclose and define a concave vapor deposition shadow area Q; the light emitting device 13, at least partially located in the isolation opening 120; and a packaging portion 14, located On the side of the light-emitting device 13 away from the substrate 11, and fills the vapor deposition shadow area Q; the packaging part 14 includes a continuous part 141 and a filling part 142, the continuous part 141 includes a concave-convex sub-part 1411, the concave-convex sub-part 1411 covers the side wall of the isolation structure 12 close to the isolation opening 120, the concave-convex sub-part 1411 encloses a groove G concave toward the isolation structure 12, the groove G is located in the vapor deposition shadow area Q, and the filling part 142 fills the groove G; in the thickness direction of the substrate 11, the ratio of the opening width D1 of the groove G to the height D3 of the first part 121 is greater than or equal to 0.4 and less than or equal to 0.8.
[0081] The display panel provided according to this embodiment and the display panel provided in any of the above embodiments belong to the same inventive concept. The technical details not described in this embodiment can be referred to the above related embodiments and will not be repeated here.
[0082] The present application also provides a mask plate suitable for preparing the display panel provided by any of the above embodiments. Figure 7a A schematic diagram of a partial top view of the structure of a mask plate provided in one embodiment of the present application. Figure 7b for Figure 7a The cross-sectional structure diagram of the mask plate along the A1A2 line is shown. It should be noted that: Figure 7a Only a top view of one repeating unit is shown. Figure 7b A cross-sectional view of multiple repeating units is shown. Figure 7a and Figure 7b As shown, the mask plate includes a substrate layer, and the substrate layer includes a first shielding portion 71, a plurality of hollow portions 72, and a second shielding portion 73 connected in sequence. The plurality of hollow portions 72 are sequentially arranged around the periphery of the first shielding portion 71, that is, the plurality of hollow portions 72 are arranged circumferentially along the first shielding portion 71, and the second shielding portion 73 surrounds the periphery of the hollow portions 72. The thickness of the first shielding portion 71 is greater than the thickness of the second shielding portion 73. In this way, the evaporation shadow area of the second shielding portion 73 is smaller than the evaporation shadow area of the first shielding portion 71. Accordingly, when the mask plate is used to prepare the packaging portion 14 provided in any of the above embodiments, it can be specifically Figure 3a-Figure 6The filling portion 142 in the display panel shown can allow the film-forming material entering from the hollow portion 72 to be deposited more toward the side close to the second shielding portion 73 , thereby ensuring that more film-forming material fills the evaporation shadow area Q.
[0083] The first shielding portion 71 and the second shielding portion 73 both have shielding functions, but the difference is that the thicknesses of the two portions are different. Figure 7c for Figure 7a A partial enlarged view of the mask N area shown. Figure 7a , Figure 7b and Figure 7c As shown, the ratio of the thickness d2 of the second shielding portion 73 to the thickness d1 of the first shielding portion 71 is greater than or equal to 0.2 and less than or equal to 0.6; for example, the ratio between the two can be 0.2, 0.23, 0.25, 0.28, 0.3, 0.35, 0.42, 0.5, 0.55, 0.58 or 0.6.
[0084] The thickness difference Δd between the first shielding portion 71 and the second shielding portion 73 is greater than or equal to 50 micrometers and less than or equal to 100 micrometers. For example, the thickness difference Δd is 70 micrometers, 80 micrometers, or 90 micrometers.
[0085] In one embodiment, the thickness d1 of the first shielding portion 71 is greater than or equal to 100 micrometers and less than or equal to 200 micrometers. For example, the thickness d1 is 130 micrometers, 150 micrometers, 180 micrometers, and so on.
[0086] In one embodiment, the thickness d2 of the second shielding portion 73 is greater than or equal to 50 micrometers and less than or equal to 100 micrometers. For example, the thickness d2 is 70 micrometers, 80 micrometers, 90 micrometers, etc.
[0087] In one embodiment, the substrate layer further includes a connecting portion 75, which is located between adjacent hollow portions 72, and the connecting portion 75 connects the first shielding portion 71 and the second shielding portion 72. Exemplarily, in the direction from the first shielding portion 71 to the second shielding portion 72, the length L of the connecting portion 75 is greater than or equal to 10 microns and less than or equal to 30 microns, for example, the length L can be 10 microns, 12 microns, 15 microns, 17 microns, 19 microns, 20 microns, 22 microns, 26 microns, 28 microns or 30 microns. The thickness d3 of the connecting portion 75 can be the same as the thickness d1 of the first shielding portion 71, or the same as the thickness d2 of the second shielding portion 72. Exemplarily, in the arrangement direction of the plurality of hollow portions 72, the width W of the connecting portion 75 is greater than or equal to 5 microns and less than or equal to 10 microns, for example, the width W can be 5 microns, 6 microns, 8 microns, 8.5 microns, 9.2 microns or 10 microns.
[0088] like Figure 7aAs shown, the first shielding portion 71, the plurality of hollow portions 72 and the second shielding portion 73 constitute a repeating unit 70. The one repeating unit can be used to prepare a filling portion 142 of a packaging portion 14. When the display panel includes a plurality of packaging portions 14, the corresponding mask plate includes a plurality of repeating units 70. In this case, the substrate layer also includes a third shielding portion 74, which is located between adjacent repeating units 70, specifically between the second shielding portions 73 of adjacent repeating units 70. The thickness of the third shielding portion 74 is equal to the thickness of the first shielding portion 71.
[0089] The mask plate provided in this embodiment can be used to prepare the display panel provided in any of the above embodiments. Moreover, the difference between the mask plate and the mask plate used in the conventional encapsulation part preparation process is that the conventional mask plate is half-engraved to obtain the second shielding part 73, which is a minor change and easy to implement.
[0090] The present application also provides a method for preparing a display panel. Figure 8 A flow chart of a method for preparing a display panel provided in one embodiment of the present application. Figure 9a-9c For execution Figure 8 The schematic diagram of the structure of the intermediate product obtained during the preparation method shown in FIG. Figure 8 As shown, the preparation method 800 includes:
[0091] Step S810, see Figure 9a , an isolation structure 12 and a light emitting device 13 are prepared on a substrate 11. The isolation structure 12 encloses an isolation opening 120. The light emitting device 13 is at least partially located in the isolation opening 120, and the sidewall of the isolation structure 12 defines a concave vapor deposition shadow area Q. The isolation structure includes a first portion and a second portion stacked together, the second portion is located on a side of the first portion away from the substrate, and the orthographic projection of the first portion on the substrate is located within the orthographic projection range of the second portion on the substrate.
[0092] Step S820, see Figure 9b and Fig.9c , a packaging part 14 is prepared on the side of the light-emitting device 13 away from the substrate 11. The packaging part 14 covers the surface of the light-emitting device 13 away from the substrate 11, and fills the vapor deposition shadow area Q. The packaging part 14 includes a continuous part 141 and a filling part 142. The continuous part 141 includes a concave-convex sub-part 1411. The concave-convex sub-part 1411 covers the side wall of the isolation structure 12 close to the isolation opening 120. The concave-convex sub-part 1411 encloses a groove G concave toward the isolation structure 12. The groove G is located in the vapor deposition shadow area Q, and the filling part 142 fills the groove G. Wherein, the thickness D0 of the concave-convex sub-part 1411 located at the groove G is greater than or equal to 0.1 micrometers and less than or equal to 0.7 micrometers; and / or in the thickness direction of the substrate 11, the ratio of the opening width D1 of the groove G to the height D3 of the first part 121 is greater than or equal to 0.4 and less than or equal to 0.8.
[0093] In one embodiment, step S820 may use an evaporation process to prepare an encapsulation material layer, and the thickness of the encapsulation material layer is sufficient to fill the evaporation shadow area Q. The encapsulation material layer is patterned to obtain the encapsulation portion 14. In this case, in one embodiment, the preparation method 800 may further include thinning the encapsulation portion 14, for example, thinning the encapsulation portion 14 on the side of the light-emitting device 13 away from the substrate 11, and then further filling the evaporation shadow area Q.
[0094] According to the method for preparing a display panel provided in this embodiment, by preparing a packaging part 14 that fills the vapor deposition shadow area Q, the strength of the packaging part 14 in the vapor deposition shadow area Q is improved, the protection of the light-emitting device 13 is improved, and the reliability of the display panel is improved.
[0095] In one embodiment, step S810 specifically includes: first, preparing the second electrode 133 on the substrate 11 ; second, preparing the isolation structure 12 on the substrate 11 ; and then, sequentially preparing the light-emitting layer and the first electrode 131 in the isolation opening 120 .
[0096] Furthermore, in one embodiment, after preparing the second electrode 133 on the substrate 11 and before preparing the isolation structure 12 on the substrate 11, the preparation method 800 also includes: preparing a pixel definition layer 15 on the substrate 11, the pixel definition layer 15 enclosing a pixel opening, and the pixel opening exposes at least a portion of the second electrode 133.
[0097] In this case, step S820 specifically includes:
[0098] First, see Figure 9b , a continuous portion 141 is prepared on the side of the light emitting device 13 away from the substrate 11 . Specifically, the continuous portion 141 may be obtained by evaporating the entire packaging material layer and then patterning the packaging material layer.
[0099] The continuous portion 141 includes a concave-convex sub-portion 1411, a connecting sub-portion 1413 and a flat sub-portion 1412 connected in sequence. The orthographic projection of the flat sub-portion 1412 on the substrate 11 at least partially overlaps with the orthographic projection of the second electrode 133 on the substrate 11. The concave-convex sub-portion 1411 covers the side wall of the isolation structure 12 facing the isolation opening 120, and the concave-convex sub-portion 1411 encloses a groove G that is concave toward the isolation structure 12, and the groove G is located in the vapor deposition shadow area Q.
[0100] The continuous portion 141 is thinner than the conventional packaging portion, thereby forming a larger groove G, which is convenient for the subsequent filling of the filling portion 142. In this case, the deposition rate of the continuous portion 141 is faster, thereby improving the productivity.
[0101] Second, see Fig.9c ,use Figure 7a In the mask shown, a filling portion 142 is prepared on the side of the continuous portion 141 facing away from the substrate 11 , and the filling portion 142 at least fills the groove G.
[0102] Among them, the orthographic projection of the first blocking portion 71 of the mask plate on the substrate 11 overlaps with the orthographic projection of the pixel opening on the substrate 11, the orthographic projection of the second blocking portion 72 on the substrate 11 and the orthographic projection of the isolation structure 12 on the substrate 11 at least partially overlap, and the orthographic projection of the groove G on the substrate 11 is located within the orthographic projection range of the hollow portion 72 on the substrate 11.
[0103] According to the method for manufacturing the display panel provided in this embodiment, the packaging portion 14 is separated into two parts (ie, the continuous portion 141 and the filling portion 142 ) for manufacturing, which is easy to implement in terms of process.
[0104] In one embodiment, the method for preparing a display panel according to an embodiment of the present application further includes: referring to Figure 6 , an organic encapsulation layer 16 and an inorganic encapsulation layer 17 are sequentially prepared on the side of the encapsulation portion 14 facing away from the substrate 11 .
[0105] It should be noted that the method for preparing the display panel provided according to the embodiment of the present application and the display panel provided in any of the above embodiments belong to the same inventive concept. The technical details not described in the preparation method embodiment can be found in the display panel embodiment and will not be repeated here.
[0106] The present application also provides a display device. Fig.10 This is a schematic diagram of the structure of a display device provided in one embodiment of the present application. Fig.10 As shown, the display device includes the display panel 100 provided by any one of the above embodiments.
[0107] A display device is a product with an image display function. For example, a display device can be used to display static images, such as pictures or photos. A display device can also be used to display dynamic images, such as videos.
[0108] The display device can be a laptop computer, a mobile phone, a handheld or portable computer, a camera, a camcorder, a vehicle-mounted intelligent central control screen, a calculator, a smart watch, a GPS navigator, an electronic photo, an electronic billboard or sign, a projector, etc.
[0109] In addition, the display device may also have functions such as taking photos, recording videos, fingerprint recognition, and face recognition. Accordingly, the display device also includes at least one functional module for realizing the above functions, such as an under-screen camera, an under-screen fingerprint recognition sensor, and the like.
[0110] The basic principles of the present application are described above in conjunction with specific embodiments. However, it should be noted that the advantages, strengths, effects, etc. mentioned in the present application are only examples and not limitations, and it cannot be considered that these advantages, strengths, effects, etc. are required by each embodiment of the present application. In addition, the specific details disclosed above are only for the purpose of illustration and ease of understanding, not for limitation, and the above details do not limit the present application to being implemented by adopting the above specific details.
[0111] The above description has been given for the purpose of illustration and description. In addition, this description is not intended to limit the embodiments of the present application to the forms disclosed herein. Although multiple example aspects and embodiments have been discussed above, those skilled in the art will recognize certain variations, modifications, changes, additions and sub-combinations thereof.
Claims
1. A display panel, characterized in that: include: substrate; An isolation structure, located on one side of the substrate, the isolation structure encloses an isolation opening, and a side wall of the isolation structure defines a concave evaporation shadow area; a light emitting device, at least partially located in the isolation opening; as well as A packaging portion is located on the side of the light-emitting device away from the substrate and fills the vapor deposition shadow area; the packaging portion includes a continuous portion and a filling portion, the continuous portion includes a concave-convex sub-portion, the concave-convex sub-portion covers the side wall of the isolation structure close to the isolation opening, the concave-convex sub-portion encloses a groove concave toward the isolation structure, the groove is located in the vapor deposition shadow area, and the filling portion fills the groove; the thickness of the concave-convex sub-portion located at the groove is greater than or equal to 0.1 microns and less than or equal to 0.7 microns.
2. The display panel according to claim 1, characterized in that: In the thickness direction of the substrate, the opening width of the groove is greater than or equal to 1 micron and less than or equal to 2 microns; Preferably, in a direction parallel to the substrate, the depth of the groove is greater than or equal to 1 micron and less than or equal to 2 microns; Preferably, in the thickness direction of the substrate, the width of the filling portion located at the groove is greater than or equal to 1 micron and less than or equal to 2 microns; Preferably, in a direction parallel to the substrate, a length of the filling portion located at the groove is greater than or equal to 1 micrometer and less than or equal to 2 micrometers.
3. The display panel according to claim 1, characterized in that: The concave-convex sub-portion extends to a side of the isolation structure away from the substrate; Preferably, adjacent concave-convex sub-parts are disconnected at a side of the isolation structure away from the substrate; Preferably, the filling portion extends to a side of the isolation structure away from the substrate, and the filling portion covers at least a portion of the concave-convex sub-portion on a side of the isolation structure away from the substrate.
4. The display panel according to claim 1, characterized in that: The isolation structure comprises a first portion and a second portion stacked together, the second portion is located on a side of the first portion away from the substrate, and an orthographic projection of the first portion on the substrate is located within the orthographic projection range of the second portion on the substrate; in a thickness direction of the substrate, a ratio of an opening width of the groove to a height of the first portion is greater than or equal to 0.4 and less than or equal to 0.8; Preferably, in the thickness direction of the substrate, the height of the first portion is greater than or equal to 1.5 microns and less than or equal to 2.5 microns; Preferably, the height of the first portion is 2 microns.
5. The display panel according to claim 1, characterized in that: The light emitting device comprises a first electrode and a second electrode stacked together, wherein the second electrode is located on a side of the first electrode close to the substrate; the continuous portion further comprises a flat sub-portion and a connecting sub-portion, wherein the connecting sub-portion connects the flat sub-portion and the concave-convex sub-portion, and an orthographic projection of the flat sub-portion on the substrate at least partially overlaps with an orthographic projection of the second electrode on the substrate; Preferably, the concave-convex sub-portion surrounds the flat sub-portion.
6. The display panel according to claim 5, characterized in that: The thickness of the flat sub-portion is greater than or equal to 0.5 micrometers and less than or equal to 0.7 micrometers.
7. The display panel according to claim 1, characterized in that: The material of the continuous portion includes an inorganic material; Preferably, the continuous portion and the filling portion are made of the same material; Preferably, the material of the continuous portion includes at least one of silicon oxide and silicon nitride.
8. The display panel according to claim 1, characterized in that: The isolation structure comprises a first portion and a second portion stacked together, the second portion is located on a side of the first portion away from the substrate, and an orthographic projection of the first portion on the substrate is within the range of an orthographic projection of the second portion on the substrate; Preferably, the isolation structure further comprises a third portion, which is located on a side of the first portion close to the substrate; Preferably, the orthographic projection of the first portion on the substrate is located within the orthographic projection range of the third portion on the substrate; Preferably, the material of the first part includes aluminum or copper or silver; Preferably, the material of the second part includes titanium or molybdenum; Preferably, the material of the third part includes molybdenum or titanium.
9. The display panel according to claim 1, characterized in that: The light emitting device comprises a first electrode and a second electrode stacked together, wherein the second electrode is located on a side of the first electrode close to the substrate; Preferably, the light emitting device further comprises at least one stacked light emitting functional layer located between the first electrode and the second electrode; Preferably, the display panel further comprises a pixel definition layer stacked on a side of the isolation structure close to the substrate; Preferably, the pixel definition layer covers an edge region of the second electrode.
10. The display panel according to claim 1, characterized in that: It also includes an organic encapsulation layer, which is located on a side of the encapsulation portion away from the substrate; Preferably, the orthographic projection of the organic encapsulation layer on the substrate covers the orthographic projection of the encapsulation part on the substrate; Preferably, the display panel further comprises an inorganic encapsulation layer, which is located on a side of the organic encapsulation layer away from the substrate; Preferably, the orthographic projection of the inorganic encapsulation layer on the substrate covers the orthographic projection of the organic encapsulation layer on the substrate.
11. A display panel, characterized in that: include: substrate; An isolation structure, located on one side of the substrate, the isolation structure encloses an isolation opening; The isolation structure comprises a first portion and a second portion stacked together, the second portion is located on a side of the first portion away from the substrate, and the orthographic projection of the first portion on the substrate is located within the orthographic projection range of the second portion on the substrate; the side wall of the first portion and the side wall of the second portion enclose and define a concave evaporation shadow area; a light emitting device, at least partially located in the isolation opening; as well as A packaging portion is located on the side of the light-emitting device away from the substrate and fills the vapor deposition shadow area; the packaging portion includes a continuous portion and a filling portion, the continuous portion includes a concave-convex sub-portion, the concave-convex sub-portion covers the side wall of the isolation structure close to the isolation opening, the concave-convex sub-portion encloses a groove concave toward the isolation structure, the groove is located in the vapor deposition shadow area, and the filling portion fills the groove; in the thickness direction of the substrate, the ratio of the opening width of the groove to the height of the first portion is greater than or equal to 0.4 and less than or equal to 0.
8.
12. The display panel according to claim 11, characterized in that: The thickness of the concavo-convex sub-portion located at the groove is greater than or equal to 0.1 micrometer and less than or equal to 0.7 micrometer; Preferably, in the thickness direction of the substrate, the height of the first portion is greater than or equal to 1.5 microns and less than or equal to 2.5 microns; Preferably, in the thickness direction of the substrate, the opening width of the groove is greater than or equal to 1 micron and less than or equal to 2 microns; Preferably, in a direction parallel to the substrate, the depth of the groove is greater than or equal to 1 micron and less than or equal to 2 microns; Preferably, in the thickness direction of the substrate, the minimum width of the filling portion located at the groove is greater than or equal to 1 micron and less than or equal to 2 microns; Preferably, in a direction parallel to the substrate, a length of the filling portion located at the groove is greater than or equal to 1 micrometer and less than or equal to 2 micrometers.
13. A mask plate, characterized in that: include: The substrate layer includes a first shielding portion, a plurality of hollow portions and a second shielding portion. The plurality of hollow portions are sequentially arranged around the periphery of the first shielding portion, and the second shielding portion surrounds the periphery of the hollow portions. The thickness of the first shielding portion is greater than the thickness of the second shielding portion.
14. The mask plate according to claim 13, characterized in that: A ratio of a thickness of the second shielding portion to a thickness of the first shielding portion is greater than or equal to 0.2 and less than or equal to 0.6; Preferably, the difference in thickness between the first shielding portion and the second shielding portion is greater than or equal to 50 microns and less than or equal to 100 microns; Preferably, the thickness of the first shielding portion is greater than or equal to 100 microns and less than or equal to 200 microns; Preferably, the thickness of the first shielding portion is 150 microns; Preferably, the thickness of the second shielding portion is greater than or equal to 50 micrometers and less than or equal to 100 micrometers.
15. The mask plate according to claim 13, characterized in that: The base material layer further includes a connecting portion, which is located between adjacent hollow portions, and the connecting portion connects the first shielding portion and the second shielding portion; Preferably, in the direction from the first shielding portion to the second shielding portion, the length of the connecting portion is greater than or equal to 10 microns and less than or equal to 30 microns; Preferably, the thickness of the connecting portion is the same as the thickness of the first shielding portion, or the thickness of the connecting portion is the same as the thickness of the second shielding portion; Preferably, in the arrangement direction of the plurality of hollow portions, the width of the connecting portion is greater than or equal to 5 microns and less than or equal to 10 microns.
16. The mask plate according to claim 13, characterized in that: The first shielding portion, the plurality of hollow portions surrounding the first shielding portion, and the second shielding portion constitute a repeating unit; the mask plate comprises a plurality of repeating units and a third shielding portion, and the third shielding portion is located between the second shielding portions of adjacent repeating units; Preferably, the thickness of the third shielding portion is equal to the thickness of the first shielding portion.
17. A method for preparing a display panel, characterized in that: include: An isolation structure and a light-emitting device are prepared on a substrate, wherein the isolation structure encloses an isolation opening, the light-emitting device is at least partially located in the isolation opening, and a side wall of the isolation structure defines a concave vapor deposition shadow area; A packaging part is prepared on the side of the light-emitting device away from the substrate, the packaging part fills the vapor deposition shadow area, the packaging part includes a continuous part and a filling part, the continuous part includes a concave-convex sub-part, the concave-convex sub-part covers the side wall of the isolation structure close to the isolation opening, the concave-convex sub-part encloses a groove concave toward the isolation structure, the groove is located in the vapor deposition shadow area, and the filling part fills the groove; Wherein, the thickness of the concavo-convex part located at the groove is greater than or equal to 0.1 micrometer and less than or equal to 0.7 micrometer; and / or, The isolation structure includes a first portion and a second portion stacked together, the second portion is located on a side of the first portion away from the substrate, and the orthographic projection of the first portion on the substrate is within the orthographic projection range of the second portion on the substrate; In a thickness direction of the substrate, a ratio of an opening width of the groove to a height of the first portion is greater than or equal to 0.4 and less than or equal to 0.
8.
18. The preparation method according to claim 17, characterized in that: The step of preparing the isolation structure and the light-emitting device on the substrate comprises: preparing a second electrode on the substrate; preparing an isolation structure on the substrate; Sequentially preparing a light-emitting layer and a first electrode in the isolation opening; Preferably, after preparing the second electrode on the substrate and before preparing the isolation structure on the substrate, the method further includes: Preparing a pixel definition layer on the substrate, wherein the pixel definition layer encloses a pixel opening, and the pixel opening exposes at least a portion of the second electrode; Preferably, preparing the encapsulation portion on the side of the light emitting device away from the substrate comprises: A continuous portion is prepared on a side of the light-emitting device away from the substrate, the continuous portion comprising a concave-convex sub-portion, a connecting sub-portion and a flat sub-portion connected in sequence, the orthographic projection of the flat sub-portion on the substrate at least partially overlaps with the orthographic projection of the second electrode on the substrate, the concave-convex sub-portion covers the side wall of the isolation structure facing the isolation opening, the concave-convex sub-portion encloses a groove concave toward the isolation structure, and the groove is located in the vapor deposition shadow area; A mask plate according to any one of claims 13 to 16 is used, and a filling portion is prepared on the side of the continuous portion facing away from the substrate, and the filling portion fills the groove, wherein the orthographic projection of the first blocking portion on the substrate overlaps with the orthographic projection of the pixel opening on the substrate, the orthographic projection of the second blocking portion on the substrate and the orthographic projection of the isolation structure on the substrate at least partially overlap, and the orthographic projection of the groove on the substrate is within the range of the orthographic projection of the hollow portion on the substrate.
19. The preparation method according to claim 17, characterized in that: Also includes: An organic encapsulation layer and an inorganic encapsulation layer are sequentially prepared on a side of the encapsulation portion away from the substrate.
20. A display device, characterized in that: A display panel comprising any one of claims 1-12.
Citation Information
Cited By
Display panel, preparation method thereof and display device
CN120603453A
Display panel, preparation method thereof and display device
CN120603453B