Nanofiltration membrane system for efficiently extracting lithium

By designing a nanofiltration membrane system that can efficiently extract lithium and using carbon layers and corrosion-resistant materials, the problem of low lithium extraction efficiency in lithium batteries has been solved, and the rapid extraction and crushing of lithium battery electrolytes has been achieved, thus protecting environmental resources.

CN118767676AInactive Publication Date: 2024-10-15JUNSHAN LIXING (GUANGZHOU) ENVIRONMENTAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310373054.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-04-10
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

It is difficult to efficiently extract lithium from lithium batteries with existing technology, leading to waste of lithium resources and environmental pollution problems.

Method used

A nanofiltration membrane system is designed to efficiently extract lithium, including a storage box, filter element, reverse osmosis element and static box. The surface of the filter element is coated with a carbon layer. Combined with a vibration motor and a crusher, the carbon layer improves the permeability and permeability. efficiency, and use corrosion-resistant materials to protect equipment to achieve effective extraction and crushing of electrolyte.

Benefits of technology

It realizes the rapid extraction and crushing of lithium battery electrolyte, prevents the waste of lithium resources and environmental pollution, and improves the service life of the equipment and the environmental protection effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118767676A_ABST
    Figure CN118767676A_ABST
Patent Text Reader

Abstract

The invention discloses an efficient lithium extraction nanofiltration membrane system which comprises a recovery device, the recovery device is connected with a storage box, the storage box is connected with a filter part, the surface of the filter part is coated with a carbon layer, the filter part is connected with a reverse osmosis part, the reverse osmosis part is connected with a static box, and the static box is connected with a lithium ion battery. The static box is connected with the storage box; the recycling device comprises a water storage tank and a material storage tank, a vibration motor is arranged on the material storage tank, the bottom of the water storage tank is obliquely arranged, a water outlet pipe is arranged on one side of the water storage tank and connected with the storage box, a support is arranged on the water storage tank, a crusher is arranged on the support, and a water outlet pipe is arranged on the other side of the water storage tank. A discharge pipe is arranged at the discharge end of the crusher; according to the nanofiltration membrane system for efficiently extracting lithium, electrolyte can be extracted and prevented from flowing into an ecological system, and the ecological environment is protected.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a nanofiltration membrane system for efficiently extracting lithium. Background Art

[0002] Lithium batteries are a type of battery that uses lithium metal or lithium alloy as positive / negative electrode materials and non-aqueous electrolyte solutions. Battery recycling refers to the collection of used batteries to prevent them from entering the ecosystem and causing harm to the environment.

[0003] Waste batteries contain a large amount of heavy metals, lithium, waste acid and waste alkali; in particular, the extraction of lithium has become a problem that needs to be solved. Therefore, a nanofiltration membrane system for efficient lithium extraction is proposed to solve the above problems. Summary of the invention

[0004] The object of the present invention is to provide a nanofiltration membrane system for efficient lithium extraction to solve the problems raised in the above background technology.

[0005] To achieve the above object, the present invention provides the following technical solution: a nanofiltration membrane system for efficient lithium extraction, comprising a recovery device, the recovery device is connected to a storage box, the storage box is connected to a filter element, the surface of the filter element is coated with a carbon layer, the filter element is connected to a reverse osmosis element, the reverse osmosis element is connected to a static box, and the static box is connected to the storage box; The recovery device comprises a water storage tank and a material storage tank, the material storage tank is provided with a vibration motor, the bottom of the water storage tank is inclined, a water outlet pipe is provided on one side of the water storage tank, the water outlet pipe is connected to the storage box, a bracket is provided on the water storage tank, a crusher is provided on the bracket, and a discharge pipe is provided at the discharge end of the crusher; The water storage tank is also provided with a rotating motor, a receiving plate is provided on the driving end of the rotating motor, a plurality of plate holes are provided on the receiving plate, and a filter is provided under the receiving plate.

[0006] Preferably, the filter element is a nanofiltration membrane, and the carbon layer is graphene oxide.

[0007] Preferably, the bottom surface of the water storage tank is arranged at 45° to the wall surface of the water storage tank.

[0008] Preferably, the pore size of the filter screen is smaller than the pore size of the plate holes.

[0009] Preferably, the inner walls of the storage box and the static box are coated with a corrosion-resistant material, the corrosion-resistant material is a modified epoxy resin, and the corrosion-resistant material includes the following raw materials: 50-60 parts of epoxy resin, 10-15 parts of deionized water, 20-30 parts of anhydrous ethanol solvent, 10-15 parts of petroleum resin, 10-16 parts of methyl isobutyl ketone, 15-20 parts of anionic acrylic emulsion, 10-15 parts of defoaming agent, 8-14 parts of antioxidant, 17-25 parts of curing agent, 10-15 parts of polyaniline, 15-20 parts of film-forming aid, 20-25 parts of isooctyl ester, and 3-5 parts of thickener.

[0010] Preferably, the method for preparing the corrosion-resistant material comprises the following steps: S1. Add equal amounts of epoxy resin, petroleum resin, deionized water and methyl isobutyl ketone into a reactor in a batching room and stir for 5-10 minutes; S2, heating the reactor by a heater at a temperature of 150°C-300°C for 40-60 minutes, then cooling naturally to form a mixed solution A, which is taken out for standby use; S3, the mixed solution A is poured into a vacuum stirring dissolver, and then the polyaniline and isooctyl ester of equal amounts are poured into the vacuum stirring dissolver, and the liquid inside is stirred in the vacuum stirring dissolver for 40-60 minutes at a speed of 700-1500 rpm. After the stirring is completed, a mixed solution B is formed and taken out for standby use; S4, pouring the mixed solution B and anhydrous ethanol solvent and anionic acrylic emulsion of equal amounts into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 30-40 minutes at a speed of 800-1000 rpm; S5, adding equal amounts of antioxidant, defoamer, curing agent, film-forming aid, and thickener into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 40-60 minutes at a speed of 1000-1200 rpm to form a mixed solution C; S6. The mixed solution C is stored in a constant temperature box.

[0011] Compared with the prior art, the present invention has the following beneficial effects: The battery is quickly crushed by a crusher to extract the battery electrolyte, and then the electrolyte is extracted through a filter to prevent it from flowing into the ecosystem and protect the ecological environment. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 This is a schematic structural diagram of a nanofiltration membrane system for efficient lithium extraction according to the present invention; Figure 2 This is a schematic diagram of the structure of a recovery device in a nanofiltration membrane system for efficient lithium extraction according to the present invention. Implementation

[0013] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0014] like Figure 1-2 As shown, a nanofiltration membrane system for efficient lithium extraction includes a recovery device 1, the recovery device 1 is connected to a storage box 2 for storing liquid after crushing the battery, the storage box 2 is connected to a filter element 3 (the filter element 3 is a nanofiltration membrane), and the surface of the filter element 3 is coated with a carbon layer (the carbon layer is a graphene oxide material). By providing the carbon layer, the permeability of the nanofiltration membrane is improved, the positive charge repulsion of the nanofiltration is increased while maintaining its permeability, thereby providing stability of the nanofiltration membrane.

[0015] The filter element 3 is connected to a reverse osmosis element 4, the reverse osmosis element 4 is connected to a static box 5, the static box 5 is connected to the storage box 2, the inner walls of the storage box 2 and the static box 5 are coated with corrosion-resistant material, the corrosion-resistant material is a modified epoxy resin, and the corrosion-resistant material can prevent electrolyte corrosion and increase the service life of the static box 5 and the storage box 2; The recycling device 1 includes a water storage tank 11 and a material storage tank 12. The material storage tank 12 is used to store crushed batteries. A vibration motor 121 is provided on the material storage tank 12. The bottom of the water storage tank 11 is tilted, and the bottom surface of the water storage tank 11 is set at 45 degrees with the wall surface of the water storage tank 11, so that the liquid can flow into the static box 5 better; a water outlet pipe 111 is provided on one side of the water storage tank 11, and the water outlet pipe 111 is connected to the storage box 2. A bracket 112 is provided on the water storage tank 11, and a crusher 1121 is provided on the bracket 112. A discharge pipe 11211 is provided at the discharge end of the crusher 1121. The crusher 1121 is used to quickly crush the battery to extract the electrolyte of the battery, and then the electrolyte is extracted through the filter 3 to prevent it from flowing into the ecosystem, thereby protecting the ecological environment; The water storage tank 11 is also provided with a rotating motor 113, and a receiving plate 1131 is provided on the driving end of the rotating motor 113. The receiving plate 1131 is provided with a plurality of plate holes 11311, and a filter screen 1132 is provided below the receiving plate 1131. The aperture of the filter screen 1132 is smaller than the aperture of the plate holes 11311, so as to further filter the crushed battery fragments. When the receiving plate 1131 and the filter screen 1132 store too many impurities, the receiving plate 1131 is rotated by the rotating motor 113, so that the impurities on the receiving plate 1131 and the filter screen 1132 fall into the storage tank 12. If there are still impurities on the filter screen 1132, the vibration motor 121 is started to vibrate the receiving plate 1131, so that the remaining impurities in the filter screen 1132 also fall into the storage tank 12.

[0016] The corrosion-resistant material includes the following raw materials: 50-60 parts of epoxy resin, 10-15 parts of deionized water, 20-30 parts of anhydrous ethanol solvent, 10-15 parts of petroleum resin, 10-16 parts of methyl isobutyl ketone, 15-20 parts of anionic acrylic emulsion, 10-15 parts of defoaming agent, 8-14 parts of antioxidant, 17-25 parts of curing agent, 10-15 parts of polyaniline, 15-20 parts of film-forming aid, 20-25 parts of isooctyl ester, and 3-5 parts of thickener.

[0017] The method for preparing the corrosion-resistant material comprises the following steps: S1. Add equal amounts of epoxy resin, petroleum resin, deionized water and methyl isobutyl ketone into a reactor in a batching room and stir for 5-10 minutes; S2, heating the reactor by a heater at a temperature of 150°C-300°C for 40-60 minutes, then cooling naturally to form a mixed solution A, which is taken out for standby use; S3, the mixed solution A is poured into a vacuum stirring dissolver, and then the polyaniline and isooctyl ester of equal amounts are poured into the vacuum stirring dissolver, and the liquid inside is stirred in the vacuum stirring dissolver for 40-60 minutes at a speed of 700-1500 rpm. After the stirring is completed, a mixed solution B is formed and taken out for standby use; S4, pouring the mixed solution B and anhydrous ethanol solvent and anionic acrylic emulsion of equal amounts into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 30-40 minutes at a speed of 800-1000 rpm; S5, adding equal amounts of antioxidant, defoamer, curing agent, film-forming aid, and thickener into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 40-60 minutes at a speed of 1000-1200 rpm to form a mixed solution C; S6. The mixed solution C is stored in a constant temperature box. Example

[0018] The corrosion-resistant material includes the following raw materials: 50 parts of epoxy resin, 10 parts of deionized water, 20 parts of anhydrous ethanol solvent, 10 parts of petroleum resin, 10 parts of methyl isobutyl ketone, 15 parts of anionic acrylic emulsion, 10 parts of defoaming agent, 8 parts of antioxidant, 17 parts of curing agent, 10 parts of polyaniline, 15 parts of film-forming aid, 20 parts of isooctyl ester, and 3 parts of thickener.

[0019] The method for preparing the corrosion-resistant material comprises the following steps: S1. Add epoxy resin, petroleum resin, deionized water and methyl isobutyl ketone into the reactor in the batching room and stir for 5 minutes; S2, heating the reactor by a heater at a temperature of 150° C. for 60 minutes, then cooling naturally to form a mixed solution A, which is taken out for later use; S3, the mixed solution A is poured into a vacuum stirring dissolver, and then polyaniline and isooctyl ester are poured into the vacuum stirring dissolver, and the liquid inside is stirred in the vacuum stirring dissolver for 40 minutes at a speed of 1500 rpm. After the stirring is completed, a mixed solution B is formed and taken out for standby use; S4, pouring the mixed solution B and anhydrous ethanol solvent and anionic acrylic emulsion of equal amounts into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 30 minutes at a speed of 1000 rpm; S5, adding equal amounts of antioxidant, defoamer, curing agent, film-forming aid, and thickener into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 40 minutes at a speed of 1200 rpm to form a mixed solution C; S6. The mixed solution C is stored in a constant temperature box. Example

[0020] The corrosion-resistant material includes the following raw materials: 60 parts of epoxy resin, 15 parts of deionized water, 30 parts of anhydrous ethanol solvent, 15 parts of petroleum resin, 16 parts of methyl isobutyl ketone, 20 parts of anionic acrylic emulsion, 15 parts of defoaming agent, 14 parts of antioxidant, 25 parts of curing agent, 15 parts of polyaniline, 20 parts of film-forming aid, 25 parts of isooctyl ester, and 5 parts of thickener.

[0021] The method for preparing the corrosion-resistant material comprises the following steps: S1. Add epoxy resin, petroleum resin, deionized water and methyl isobutyl ketone into the reactor in the batching room and stir for 10 minutes; S2, heating the reactor by a heater at a temperature of 300° C. for 40 minutes, then cooling naturally to form a mixed solution A, which is taken out for standby use; S3, the mixed solution A is poured into a vacuum stirring dissolver, and then the polyaniline and isooctyl ester of equal amounts are poured into the vacuum stirring dissolver, and the liquid inside is stirred in the vacuum stirring dissolver for 60 minutes at a speed of 700 rpm. After the stirring is completed, a mixed solution B is formed and taken out for standby use; S4, pouring the mixed solution B and anhydrous ethanol solvent and anionic acrylic emulsion of equal amounts into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 40 minutes at a speed of 800 rpm; S5, adding equal amounts of antioxidant, defoamer, curing agent, film-forming aid, and thickener into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 60 minutes at a speed of 1000 rpm to form a mixed solution C; S6. The mixed solution C is stored in a constant temperature box.

[0022] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A nanofiltration membrane system for efficient lithium extraction, characterized in that: It includes a recovery device, the recovery device is connected to a storage box, the storage box is connected to a filter element, the surface of the filter element is coated with a carbon layer, the filter element is connected to a reverse osmosis element, the reverse osmosis element is connected to a static box, and the static box is connected to the storage box; The recovery device comprises a water storage tank and a material storage tank, the material storage tank is provided with a vibration motor, the bottom of the water storage tank is inclined, a water outlet pipe is provided on one side of the water storage tank, the water outlet pipe is connected to the storage box, a bracket is provided on the water storage tank, a crusher is provided on the bracket, and a discharge pipe is provided at the discharge end of the crusher; The water storage tank is also provided with a rotating motor, a receiving plate is provided on the driving end of the rotating motor, a plurality of plate holes are provided on the receiving plate, and a filter is provided under the receiving plate.

2. A nanofiltration membrane system for efficient lithium extraction according to claim 1, characterized in that: The filter element is a nanofiltration membrane, and the carbon layer is graphene oxide.

3. The nanofiltration membrane system for efficient lithium extraction according to claim 1, characterized in that: The bottom surface of the water storage tank is arranged at 45 degrees to the wall surface of the water storage tank.

4. The nanofiltration membrane system for efficient lithium extraction according to claim 1, characterized in that: The pore size of the filter screen is smaller than the pore size of the plate holes.

5. The nanofiltration membrane system for efficient lithium extraction according to claim 1, characterized in that: The inner walls of the storage box and the static box are coated with corrosion-resistant material, which is a modified epoxy resin. The corrosion-resistant material includes the following raw materials: 50-60 parts of epoxy resin, 10-15 parts of deionized water, 20-30 parts of anhydrous ethanol solvent, 10-15 parts of petroleum resin, 10-16 parts of methyl isobutyl ketone, 15-20 parts of anionic acrylic emulsion, 10-15 parts of defoaming agent, 8-14 parts of antioxidant, 17-25 parts of curing agent, 10-15 parts of polyaniline, 15-20 parts of film-forming aid, 20-25 parts of isooctyl ester, and 3-5 parts of thickener.

6. A nanofiltration membrane system for efficient lithium extraction according to claim 5, characterized in that: The method for preparing the corrosion-resistant material comprises the following steps: S1. Add equal amounts of epoxy resin, petroleum resin, deionized water and methyl isobutyl ketone into a reactor in a batching room and stir for 5-10 minutes; S2, heating the reactor by a heater at a temperature of 150°C-300°C for 40-60 minutes, then cooling naturally to form a mixed solution A, which is taken out for standby use; S3, the mixed solution A is poured into a vacuum stirring dissolver, and then the polyaniline and isooctyl ester of equal amounts are poured into the vacuum stirring dissolver, and the liquid inside is stirred in the vacuum stirring dissolver for 40-60 minutes at a speed of 700-1500 rpm. After the stirring is completed, a mixed solution B is formed and taken out for standby use; S4, pouring the mixed solution B and anhydrous ethanol solvent and anionic acrylic emulsion of equal amounts into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 30-40 minutes at a speed of 800-1000 rpm; S5, adding equal amounts of antioxidant, defoamer, curing agent, film-forming aid, and thickener into a vacuum spiral stirring and differentiation machine, stirring and differentiating for 40-60 minutes at a speed of 1000-1200 rpm to form a mixed solution C; S6. The mixed solution C is stored in a constant temperature box.