Shale bedding seam porosity determination method and oil and gas reservoir evaluation method
Through helium porosity testing and low-temperature carbon dioxide adsorption experiments combined with epoxy resin encapsulation methods, the porosity of shale bedding fractures is calculated, which solves the problem that existing technology cannot distinguish the porosity of bedding fractures, and improves shale gas production capacity and Exploration potential assessment, identifying rock reservoir space and fluid saturation.
Patent Information
- Application Number
- CN202310347868.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-03
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2043-04-03
AI Technical Summary
Existing porosity testing methods cannot effectively distinguish between bedding fracture porosity and matrix porosity in shale, and cannot clarify the porosity and proportion of bedding fractures in shale, which affects the calculation of rock storage space, fluid saturation and geological reserves.
Using a combination of helium porosity testing, low-temperature carbon dioxide adsorption experiments, and epoxy resin encapsulation, the shale bedding fracture pores were calculated by obtaining total porosity, matrix micropore porosity, matrix macropore porosity, and matrix fracture porosity. degree, thereby determining the rock storage space and fluid saturation.
It clarifies the enrichment areas of shale gas, improves shale gas production capacity, helps evaluate shale gas exploration potential, and is used to determine rock storage space and geological reserves.
Smart Images

Figure CN118777150A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of geological exploration, and in particular relates to a method for determining the porosity of shale bedding fractures and a method for evaluating oil and gas reservoirs. Background Art
[0002] Shale gas is a type of unconventional natural gas resource with typical self-generation and self-storage characteristics. The bedding in shale is lamellar bedding, or lamellar for short. Bedding fractures in shale are usually called lamellar fractures, which are natural cracks distributed along the lamellar formations during the deposition and diagenesis of mudstone. Lamellar fractures are actually the bedding of mudstone, and lamellar fractures are the specific manifestation of bedding fractures in shale. Lamellar fractures are a type of sedimentary structure developed by mudstone in a weak hydrodynamic environment, formed by the directional arrangement of fine-grained minerals. Horizontal bedding with a thickness of less than 1 cm is usually called lamellar bedding. Lamellar bedding has the habit of rocks easily splitting into thin plates or sheets along parallel planes. Lamination planes are also mechanically weak planes in shale and are the planes in rocks that are most likely to break. Therefore, bedding fractures in shale are mainly distributed along these extremely thin horizontal beddings.
[0003] Bedding fractures are one of the main types of fractures developed in shale. Bedding fractures in shale cores are usually parallel or approximately parallel to the bedding plane, distributed in a discontinuous manner, and are small in scale. According to the analysis of microscopic thin sections and scanning electron microscope observations, the occurrence of bedding fractures in shale is parallel or approximately parallel to its lamination interface. In thin-layer shale sections with dense lamination, bedding fractures are obviously developed, reflecting that the development degree of bedding fractures in shale is closely related to its lamination. Bedding fractures are important storage spaces for free gas in shale. The higher the development degree of bedding fractures, the more conducive it is to the enrichment and high yield of shale gas.
[0004] Porosity is a basic parameter for evaluating rock reservoir properties. Shale porosity can be divided into matrix porosity and microcrack porosity according to the pore type, and microcracks can come from bedding and matrix. Currently, there are many methods for porosity testing, mainly including gas injection porosimetry (GIP), water immersion porosimetry (WIP) and nuclear magnetic resonance (NMR). Summary of the invention
[0005] In order to enrich the shale bedding fracture porosity testing method and apply it to more application scenarios, an embodiment of the present invention provides a shale bedding fracture porosity determination method, including:
[0006] Conduct helium porosity testing on shale samples to obtain total porosity values;
[0007] Conducting a low-temperature carbon dioxide adsorption experiment on the shale sample that has completed the helium porosity test to obtain a matrix micropore porosity value, wherein the matrix micropore pores are matrix pores that are smaller than a preset threshold value;
[0008] The bedding plane of the shale sample that has completed the low-temperature carbon dioxide adsorption experiment is encapsulated with epoxy resin, and a directional mercury injection test is carried out in the vertical bedding direction to obtain the matrix macropore porosity value and matrix fracture porosity value, wherein the matrix macropore porosity is the matrix pore greater than or equal to a preset threshold value;
[0009] The shale bedding fracture porosity value is obtained by subtracting the matrix micropore porosity value, matrix macropore porosity value, and matrix fracture porosity value from the total porosity value.
[0010] Furthermore, helium porosity testing is performed on shale samples to obtain total porosity values, including:
[0011] The sample is placed in a gas porosimeter to remove air from the pores of the shale sample, and helium with a preset pressure is applied without applying confining pressure to allow helium to enter the pores of the shale sample;
[0012] After the pressure in the pores of the shale sample reaches equilibrium, the total pore volume and total porosity are calculated using Boyle's law.
[0013] Furthermore, helium porosity testing is performed on shale samples to obtain total porosity values, including:
[0014] Before placing the sample into the gas porosity meter, the target shale is first cut using a waterless wire cutter to obtain a shale sample of a desired shape, and then the shale sample is dried.
[0015] Furthermore, the shale sample of desired shape is a cubic sample.
[0016] Furthermore, matrix pores greater than or equal to 2 nm are matrix macropores, and matrix pores less than 2 nm are matrix micropores.
[0017] Furthermore, a low-temperature carbon dioxide adsorption experiment was conducted on the shale samples that had completed the helium porosity test to obtain the matrix micropore porosity value, including:
[0018] The shale sample that has completed the helium porosity test is placed in a low-temperature adsorption tester for vacuum treatment to remove the helium remaining in the nanopores of the shale sample;
[0019] Conducting a low-temperature carbon dioxide adsorption experiment and setting the carbon dioxide gas pressure so that carbon dioxide gas molecules enter the micropores of the shale sample;
[0020] According to the low-temperature carbon dioxide adsorption experiment, the carbon dioxide adsorption volume of the shale sample under different relative pressure conditions is obtained, and the matrix micropore volume is obtained according to the carbon dioxide adsorption volume using the following formula:
[0021]
[0022] Among them, V sp is the matrix micropore volume, cm 3 ; V 0 is the micropore filling adsorption capacity, cm 3 / g; M is the molar mass of carbon dioxide, g / mol; is the density of carbon dioxide gas under standard conditions, g / cm 3 ; V m is the standard molar volume of gas, L / mol; c is the unit conversion factor.
[0023] Further, the micropore filling adsorption capacity is obtained by the following steps:
[0024] The relative pressure and the carbon dioxide adsorption volume are nonlinearly fitted according to a preset formula using preset software to obtain the micropore filling adsorption capacity. The preset formula is as follows:
[0025]
[0026] Among them, V a is the amount of carbon dioxide adsorbed, cm 3 / g; R is the gas constant; T is the absolute temperature, K; p is the experimental pressure, MPa; p 0 CO at 0℃ 2 The saturated vapor pressure, MPa; β is the characteristic constant; E 0 is the adsorption characteristic energy.
[0027] Furthermore, the step of encapsulating the bedding surface of the shale sample that has completed the low-temperature carbon dioxide adsorption test with epoxy resin comprises:
[0028] The bedding surface of the shale sample that has completed the low-temperature carbon dioxide adsorption test is wrapped with epoxy resin, wherein the upper and lower surfaces of the shale sample parallel to the bedding are not wrapped with epoxy resin;
[0029] The shale samples were dried until the epoxy resin on their surface was fully hardened.
[0030] Furthermore, the directional mercury injection test is carried out in the vertical bedding direction to obtain the matrix macropore porosity value and matrix fracture porosity value, including:
[0031] The shale sample with the epoxy resin on the surface fully hardened is placed in a high-pressure mercury injection instrument, and the mercury injection porosity test is carried out according to the preset parameters;
[0032] After the mercury injection test, the sum of the matrix macropore porosity and matrix fracture porosity of the shale sample can be calculated based on the mercury injection volume;
[0033] On the other hand, the present invention also discloses an oil and gas reservoir evaluation method, which uses the above-mentioned shale layer fracture porosity determination method to determine rock storage space, fluid saturation and geological reserve calculation.
[0034] Based on the above technical solution, the beneficial effects of the present invention compared with the prior art are as follows:
[0035] The present invention establishes a shale bedding fracture porosity interpretation model, and the inventors found that the total porosity value is equal to the sum of the matrix micropore porosity value, the matrix macropore porosity value, the matrix fracture porosity value and the shale bedding fracture porosity value. A shale bedding fracture porosity determination method proposed in an embodiment of the present invention can measure multiple shale samples in the same layer, and use the obtained total porosity value to subtract the matrix micropore porosity value, the matrix macropore porosity value, and the matrix fracture porosity value to obtain the shale bedding fracture porosity, which is helpful to clarify the shale gas enrichment area and effectively improve the shale gas production capacity. Clarifying the bedding fracture porosity of different areas of the shale gas reservoir is helpful to evaluate the shale gas exploration potential and predict the shale gas favorable area. The obtained bedding fracture porosity is helpful to determine the rock storage space, fluid saturation and geological reserve calculation. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0037] Figure 1 A schematic flow chart of a method for determining shale bedding fracture porosity provided in an embodiment of the present invention;
[0038] Figure 2 This is a flow chart of step S110 in an embodiment of the present invention;
[0039] Figure 3 A shale sample cutting effect diagram provided by an embodiment of the present invention;
[0040] Figure 4 Schematic diagram of the process of step S120 in an embodiment of the present invention;
[0041] Figure 5A graph showing the amount of carbon dioxide adsorbed under different relative pressure conditions provided by an embodiment of the present invention;
[0042] Figure 6 A schematic diagram of a process for epoxy resin encapsulation of a bedding surface of a shale sample that has completed a low-temperature carbon dioxide adsorption test provided in an embodiment of the present invention;
[0043] Figure 7 Schematic diagram of epoxy resin coating on the surface of a shale sample provided in an embodiment of the present invention;
[0044] Figure 8 A schematic diagram of a process for carrying out directional mercury injection testing in a direction perpendicular to bedding to obtain matrix macropore porosity values and matrix fracture porosity values provided in an embodiment of the present invention;
[0045] Fig. 9 This is a mercury injection experiment curve diagram provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0046] In order to better understand the above technical solution, the above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0047] The inventors found that the existing porosity testing method can only obtain the total porosity value of shale, and cannot effectively distinguish the bedding fracture porosity and matrix porosity of shale. It is impossible to clearly define the bedding fracture porosity and proportion in shale, which is not conducive to the calculation of rock storage space, fluid saturation and geological reserves. Therefore, the inventors made the present invention after further research and development.
[0048] Specifically, the inventors divided the shale reservoir space into two categories: matrix pores and microfractures. Based on the above reservoir space division method, the inventors established a shale total porosity composition model. The total pore volume consists of three parts, which can be expressed as:
[0049] V tp =V mp +V mf +V 1f (1)
[0050] Due to the differences in pore size in different experimental tests, the inventors further divided the matrix pores into micropores smaller than 2 nm and matrix pores larger than 2 nm, so the total pore volume can be expressed as:
[0051] V tp =V sp +V bp +V mf +V 1f (2)
[0052] The porosity of shale is the ratio of the pore volume to the volume of the rock itself. Formula (2) can be rewritten as:
[0053]
[0054] Among them, V tp is the total pore volume, cm 3 ; V mp is the matrix pore volume, cm 3 ; V sp is the micropore volume of the mineral matrix, cm 3 ; V bp is the macropore volume of the mineral matrix, cm 3 ; V mf is the matrix pore volume, cm 3 ; V lf is the pore volume of bedding fractures, cm 3 ; is the total porosity of shale, %; is the micropore porosity of the mineral matrix, %; is the macropore porosity of the mineral matrix, %; is the matrix slit porosity, %; is the bedding fracture porosity, %.
[0055] According to the above theoretical deduction, if the total porosity value, matrix micropore porosity value, matrix macropore porosity value and matrix fracture porosity value can be obtained, the shale bedding fracture porosity can be calculated, which is helpful to clarify the shale gas enrichment area and effectively improve the shale gas production capacity.
[0056] In order to better understand the above technical solution, the above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0057] This embodiment provides a method for determining the porosity of shale bedding fractures. Figure 1 As shown, it includes steps S110 to S140, specifically:
[0058] Step S110, performing a helium porosity test on the shale sample to obtain a total porosity value.
[0059] In one embodiment, step S110 includes step S111 and step S112. Figure 2 As shown:
[0060] Step S111, placing the sample into a gas porosimeter to remove air from the pores of the shale sample, and applying helium at a preset pressure to allow helium to enter the pores of the shale sample without applying confining pressure.
[0061] Specifically, a shale sample from a bedding-rich section is taken, and the bedding distribution should be clearly visible on the surface of the shale sample. The shale sample taken is a full-diameter sample, with a diameter of 10 cm and a length of 5 cm.
[0062] The shale sample was cut using a waterless wire cutter. The sample shape required for cutting was a cube. The length, width and height of the cube sample were all 2 cm. The sample cutting effect was as follows: Figure 3 As shown, the sample shape used in general experiments is cylindrical. In order to use the sample for the subsequent directional mercury injection experiment, the present invention preferably uses a cubic sample.
[0063] After the cubic shale sample is dried, it is placed in a gas porosimeter, and then vacuum is applied to remove the air in the pores of the shale sample. Generally, the vacuuming time is 2 hours. Without applying confining pressure, helium at a certain pressure is applied to allow it to enter the pores of the shale sample.
[0064] Generally, a gas porosity meter can test samples under two conditions: with and without confining pressure. Under confining pressure, the sample is affected by external pressure, the pores are compressed, and the porosity obtained by measurement is not the total porosity, while the porosity obtained without confining pressure is the total porosity value. The total porosity value is required in the present invention, so it is necessary to apply a certain pressure of helium to allow it to enter the pores of the shale sample without confining pressure.
[0065] Step S112: After the pressure in the pores of the shale sample reaches equilibrium, the total pore volume and total porosity are calculated using Boyle's law.
[0066] Specifically, while waiting for the pressure in the pores of the shale sample to reach equilibrium, it is necessary to set the equilibrium condition. Generally, the equilibrium condition is set to a pressure change of less than 1 psi within 10 minutes. After setting the equilibrium condition, the porosity meter equipment will automatically determine whether the pressure in the shale sample has reached equilibrium.
[0067] The porosity meter system analysis software can be used to calculate the pore volume based on Boyle's law and to set the initial gas pressure to allow helium to isothermally expand into the core chamber. The gas continuously diffuses into the pores inside the core.
[0068] In a specific embodiment, the gas pressure is set to 600 psi and the equilibrium time is 1 hour. After the pressure reaches equilibrium, the total pore volume V is calculated using Boyle's law. tp 0.51cm 3 , total porosity It is 6.37%.
[0069] Specifically, shale pores smaller than 2 nm are generally classified as small pores, shale pores between 2 nm and 50 nm are classified as medium pores, and pores larger than 50 nm are classified as large pores. In the present invention, matrix pores larger than or equal to 2 nm are classified as matrix macropores, and matrix pores smaller than 2 nm are classified as matrix micropores.
[0070] Step S120, performing a low-temperature carbon dioxide adsorption experiment on the shale sample that has completed the helium porosity test to obtain a matrix micropore porosity value, wherein the matrix micropore pores are matrix pores that are smaller than a preset threshold.
[0071] In one embodiment, step S120 includes steps S121 to S123. Figure 4 As shown:
[0072] Step S121, placing the shale sample that has completed the helium porosity test into a low-temperature adsorption tester for vacuum treatment to remove the helium remaining in the nanopores of the shale sample.
[0073] Specifically, in the process of vacuuming to remove helium remaining in the nanopores of the shale sample, the vacuuming time is generally set to 2 hours.
[0074] Step S122, conducting a low-temperature carbon dioxide adsorption experiment, and setting the gas pressure of carbon dioxide so that carbon dioxide gas molecules enter the micropores of the shale sample.
[0075] Specifically, during the low-temperature carbon dioxide adsorption experiment, the temperature and the carbon dioxide pressure need to be set. Generally, the experimental temperature is set to 0°C, and the maximum carbon dioxide pressure is set to 1 atmosphere.
[0076] Step S123, according to the low-temperature carbon dioxide adsorption experiment, the carbon dioxide adsorption volume of the shale sample under different relative pressure conditions is obtained, and according to the carbon dioxide adsorption volume, the matrix micropore volume is obtained using the following formula:
[0077]
[0078] Among them, V sp is the matrix micropore volume, cm 3 ; V 0 is the micropore filling adsorption capacity, cm 3 / g; M is the molar mass of carbon dioxide, g / mol; Under normal circumstances, the molar mass of carbon dioxide is 44g / mol; is the density of carbon dioxide gas under standard conditions, g / cm 3 ; Normally, the density of carbon dioxide gas under standard conditions is 1.072g / cm 3 ; Vm is the standard molar volume of gas, L / mol; usually, the standard molar volume of gas is 22.4 L / mol; c is the unit conversion factor, usually 1000.
[0079] Specifically, the micropore filling adsorption capacity is obtained by the following steps:
[0080] The relative pressure and the carbon dioxide adsorption amount are nonlinearly fitted according to a preset formula using preset software (such as Origin data processing software) to obtain the micropore filling adsorption capacity. The preset formula is as follows:
[0081]
[0082] Among them, V a is the amount of carbon dioxide adsorbed in the experiment, cm 3 / g; R is the gas constant, which is usually 8.314 J / mol / K; T is the absolute temperature, K; p is the experimental pressure, MPa; p 0 CO at 0℃ 2 The saturated vapor pressure is usually 3.48 MPa; β is the characteristic constant; E 0 is the adsorption characteristic energy.
[0083] In a specific embodiment, the amount of carbon dioxide adsorbed under different relative pressure conditions is measured, such as Figure 5 As shown, through the above method, the micropore filling adsorption capacity V can be obtained. 0 =1.42738cm 3 / g, further, the matrix micropore volume V can be obtained sp =1.42738×0.0018323×8×2.6=0.0544cm 3 , so the matrix micropore porosity is
[0084] Step S130, encapsulating the bedding surface of the shale sample that has completed the low-temperature carbon dioxide adsorption experiment with epoxy resin, and conducting a directional mercury injection test in the direction perpendicular to the bedding to obtain the matrix macropore porosity value and the matrix fracture porosity value, wherein the matrix macropore porosity is the matrix pore greater than or equal to a preset threshold.
[0085] Specifically, the bedding surface of the shale sample that has completed the low-temperature carbon dioxide adsorption test is encapsulated with epoxy resin, including step S131 and step S132, such as Figure 6 As shown:
[0086] Step S131, using epoxy resin to wrap the bedding surface of the shale sample that has completed the low-temperature carbon dioxide adsorption test, wherein the epoxy resin is not wrapped on the upper and lower surfaces of the shale sample parallel to the bedding.
[0087] Specifically, Figure 7 As shown, when coating the surface of shale samples with epoxy resin, attention should be paid to the uniformity, sealing and one-time nature of the coating, that is, the coating epoxy resin should be of uniform thickness, completely sealed and formed in one time, and should not be coated twice. In particular, attention should be paid to the problem of voids at corners.
[0088] Step S132, drying the shale sample until the epoxy resin on the surface is fully hardened.
[0089] Specifically, during the process of drying the shale sample until the epoxy resin on the surface of the shale sample is fully hardened, the hardening treatment condition is drying at a temperature of 60° C. for 24 hours.
[0090] Specifically, a directional mercury injection test is carried out in a direction perpendicular to the bedding to obtain the matrix macropore porosity value and the matrix fracture porosity value, including step S133 and step S134, such as Figure 8 As shown:
[0091] Step S133, placing the shale sample whose epoxy resin on the surface has been fully hardened into a high-pressure mercury injection instrument, and conducting a mercury injection porosity test according to preset parameters.
[0092] Specifically, the upper and lower surfaces of the shale sample cube parallel to the bedding are not wrapped with epoxy resin, and can be used as pre-mercury injection surfaces. After the sample is placed in a high-pressure mercury injection instrument, a mercury injection porosimetry test is carried out. The maximum mercury injection pressure is set to 400 MPa, the number of pressure points is set to 30, and the equilibrium time is set to 2 hours.
[0093] Step S134: After the mercury injection test is completed, the sum of the matrix macropore porosity and the matrix fracture porosity of the shale sample can be calculated according to the mercury injection volume.
[0094] In a specific embodiment, the mercury injection test curve is as follows Fig. 9 As shown in the figure, since the mercury injection direction is perpendicular to the shale bedding plane, the pore volume obtained by the mercury injection test does not include the bedding fracture volume without considering the mercury molecules passing through the bedding interface. In addition, since mercury molecules are large, they still cannot enter the micropores smaller than 2nm under high experimental pressure conditions. Therefore, the sum of the pore volume of the shale sample matrix macropores and the pore volume of the matrix fractures can be obtained by this directional high-pressure mercury injection test, which is 4.64%.
[0095] Step S140, subtracting the matrix micropore porosity value, the matrix macropore porosity value, and the matrix fracture porosity value from the acquired total porosity value to obtain the shale bedding fracture porosity.
[0096] In a specific embodiment, when the total porosity of the shale sample, the matrix micropore porosity, the matrix macropore and microcrack porosity are determined, the shale bedding fracture porosity can be calculated:
[0097]
[0098] in, is the total porosity of shale, %; is the micropore porosity of the mineral matrix, %; is the macropore porosity of the mineral matrix, %; is the matrix slit porosity, %; is the bedding fracture porosity, %.
[0099] By using the above-mentioned shale bedding fracture porosity determination method, rock reservoir space, fluid saturation and geological reserve calculation can be determined.
[0100] The present invention establishes a shale bedding fracture porosity interpretation model, and the total porosity value is equal to the sum of the matrix micropore porosity value, the matrix macropore porosity value, the matrix fracture porosity value and the shale bedding fracture porosity value. A shale bedding fracture porosity determination method proposed in an embodiment of the present invention can measure multiple shale samples in the same layer, and use the obtained total porosity value to subtract the matrix micropore porosity value, the matrix macropore porosity value, and the matrix fracture porosity value to obtain the shale bedding fracture porosity, which is helpful to clarify the shale gas enrichment area and effectively improve the shale gas production capacity. Clarifying the bedding fracture porosity of different areas of the shale gas reservoir is conducive to evaluating the shale gas exploration potential and predicting the shale gas favorable area. The obtained bedding fracture porosity is helpful to determine the rock storage space, fluid saturation and geological reserve calculation.
[0101] In the above detailed description, various features are grouped together in a single embodiment to simplify the disclosure. This method of disclosure should not be interpreted as reflecting an intention that the embodiments of the claimed subject matter require more features than are clearly stated in each claim. On the contrary, as reflected in the appended claims, the invention is in a state of having less than all the features of the disclosed individual embodiments. Therefore, the appended claims are hereby expressly incorporated into the detailed description, with each claim standing on its own as a separate preferred embodiment of the invention.
[0102] The above description includes examples of one or more embodiments. Of course, it is not possible to describe all possible combinations of components or methods for the purpose of describing the above embodiments, but it should be recognized by those skilled in the art that the various embodiments may be further combined and arranged. Therefore, the embodiments described herein are intended to cover all such changes, modifications and variations that fall within the scope of protection of the appended claims. In addition, with respect to the term "comprising" used in the specification or claims, the word is encompassed in a manner similar to the term "including", as explained by "including," used as a transitional word in the claims. In addition, any term "or" used in the specification of the claims is intended to mean "non-exclusive or".
Claims
1. A method for determining the porosity of shale bedding fractures, It is characterized in that The following steps are involved: Conduct helium porosity testing on shale samples to obtain total porosity values; Conducting a low-temperature carbon dioxide adsorption experiment on the shale sample that has completed the helium porosity test to obtain a matrix micropore porosity value, wherein the matrix micropore pores are matrix pores that are smaller than a preset threshold value; The bedding plane of the shale sample that has completed the low-temperature carbon dioxide adsorption experiment is encapsulated with epoxy resin, and a directional mercury injection test is carried out in the vertical bedding direction to obtain the matrix macropore porosity value and matrix fracture porosity value, wherein the matrix macropore porosity is the matrix pore greater than or equal to a preset threshold value; The shale bedding fracture porosity value is obtained by subtracting the matrix micropore porosity value, matrix macropore porosity value, and matrix fracture porosity value from the total porosity value.
2. The method according to claim 1, It is characterized in that The helium porosity test is carried out on the shale sample to obtain the total porosity value, including: The sample is placed in a gas porosimeter to remove air from the pores of the shale sample, and helium with a preset pressure is applied without applying confining pressure to allow helium to enter the pores of the shale sample; After the pressure in the pores of the shale sample reaches equilibrium, the total pore volume and total porosity are calculated using Boyle's law.
3. The method according to claim 1, It is characterized in that The helium porosity test is performed on the shale sample to obtain the total porosity value, and further includes: Before placing the sample into the gas porosity meter, the target shale is first cut using a waterless wire cutter to obtain a shale sample of a desired shape, and then the shale sample is dried.
4. The method according to claim 3, It is characterized in that The shale sample of the desired shape is a cubic sample.
5. The method according to claim 1, It is characterized in that The preset threshold matrix pore size is 2 nm.
6. The method according to claim 1, It is characterized in that The method of conducting a low-temperature carbon dioxide adsorption experiment on the shale sample that has completed the helium porosity test to obtain the matrix micropore porosity value includes: The shale sample that has completed the helium porosity test is placed in a low-temperature adsorption tester for vacuum treatment to remove the helium remaining in the nanopores of the shale sample; Conducting a low-temperature carbon dioxide adsorption experiment and setting the carbon dioxide gas pressure so that carbon dioxide gas molecules enter the micropores of the shale sample; According to the low-temperature carbon dioxide adsorption experiment, the carbon dioxide adsorption volume of the shale sample under different relative pressure conditions is obtained, and the matrix micropore volume is obtained according to the carbon dioxide adsorption volume using the following formula: Among them, V sp is the matrix micropore volume, cm 3 ; V 0 is the micropore filling adsorption capacity, cm 3 / g; M is the molar mass of carbon dioxide, g / mol; is the density of carbon dioxide gas under standard conditions, g / cm 3 ; V m is the standard molar volume of gas, L / mol; c is the unit conversion factor.
7. The method according to claim 6, It is characterized in that The micropore filling adsorption capacity is obtained by the following steps: The relative pressure and the carbon dioxide adsorption volume are nonlinearly fitted according to a preset formula using preset software to obtain the micropore filling adsorption capacity. The preset formula is as follows: Among them, V a is the amount of carbon dioxide adsorbed, cm 3 / g; R is the gas constant; T is the absolute temperature, K; p is the experimental pressure, MPa; p 0 CO at 0℃ 2 The saturated vapor pressure, MPa; β is the characteristic constant; E 0 is the adsorption characteristic energy.
8. The method according to claim 4, It is characterized in that The step of performing epoxy resin encapsulation on the bedding surface of the shale sample that has completed the low-temperature carbon dioxide adsorption test comprises: The bedding surface of the shale sample that has completed the low-temperature carbon dioxide adsorption test is wrapped with epoxy resin, wherein the upper and lower surfaces of the shale sample parallel to the bedding are not wrapped with epoxy resin; The shale samples were dried until the epoxy resin on their surface was fully hardened.
9. The method according to claim 1, It is characterized in that The directional mercury injection test is carried out in the vertical bedding direction to obtain the matrix macropore porosity value and matrix fracture porosity value, including: The shale sample with the epoxy resin on the surface fully hardened is placed in a high-pressure mercury injection instrument, and the mercury injection porosity test is carried out according to the preset parameters; After the mercury injection test, the sum of the matrix macropore porosity and matrix fracture porosity of the shale sample can be calculated based on the mercury injection volume.
10. A method for evaluating oil and gas reservoirs, It is characterized in that The method comprises the method for determining the porosity of shale bedding fractures as described in any one of claims 1 to 9.
Citation Information
Patent Citations
Method for testing clay micro pore porosity in shale gas reservoir
CN106290103A
Shale reservoir hole-fracture characterization method and device
CN109283116A
Shale porosity testing method and application thereof
CN114813506A
Gas sorption analysis of unconventional rock samples
US20120192639A1
Cited By
Method for determining microcosmic characteristic influence factors of shale reservoir
CN121049128A