A method for preparing a pneumatic metamaterial supersurface structure
Designing the pneumatic metamaterial metasurface structure through wire material and hot pressing forming technology solves the problem of expensive and time-consuming traditional designs, realizes adaptive design and low-cost production, and ensures breathability and thermal stability.
Patent Information
- Application Number
- CN202411287337.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-09-13
AI Technical Summary
Traditional pneumatic metamaterial metasurface designs are expensive, time-consuming and difficult to adapt to complex environmental needs, and require complex manufacturing techniques to accurately control microstructures, resulting in high manufacturing costs and long design cycles.
The pneumatic metamaterial metasurface structure is designed using wire material. The skeleton layer, dispersion layer, filter layer and protective layer are superimposed in turn by hot pressing forming, and the temperature is slightly lower than the melting point of the wire is heated and applied to the pressure to make each The layers are tightly bonded, avoiding the use of adhesives to maintain breathability.
It realizes simple, fast and low-cost pneumatic metamaterial metasurface structure preparation, adapts to the needs of different application scenarios, ensures breathability and thermal stability of the material, and reduces production costs.
Smart Images

Figure CN118789898B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of pneumatic super surface structures, and in particular to a method for preparing a pneumatic super material super surface structure. Background Art
[0002] Metamaterials are artificial composite structures with extraordinary physical properties. They are made by orderly constructing artificial microstructures with a material size between microscopic particles and macroscopic physical field wavelengths, so that they can obtain extraordinary physical properties that conventional materials do not have. These extraordinary physical properties come from their precise geometric structure and size.
[0003] However, in the design of traditional pneumatic metamaterial metasurfaces, due to the permeable characteristics of the metamaterial metasurface structure, it is necessary to have good air permeability. These functions often rely on the size and arrangement of its microstructure. Precise control of the size and shape of the microstructure often requires complex and sophisticated manufacturing techniques, such as photolithography or electron beam etching, which are expensive and time-consuming, with high manufacturing costs and long design cycles.
[0004] In addition, traditional design methods are usually relatively fixed, which means that the metasurface structure may not achieve the expected effect in complex real environments and it is difficult to adapt to the needs of different application scenarios. Summary of the invention
[0005] Based on this, it is necessary to provide a method for preparing a pneumatic metamaterial supersurface structure that can be adaptively designed according to different application scenarios and is simple to prepare in response to the above technical problems.
[0006] A method for preparing a pneumatic metamaterial supersurface structure, the preparation method comprising designing the structure, the structure design method comprising:
[0007] Determine the performance parameters of the aerodynamic metamaterial metasurface according to the use environment and work requirements;
[0008] Based on the performance parameters, designing the aerodynamic metamaterial metasurface structure;
[0009] The pneumatic metamaterial metasurface structure comprises a skeleton layer, a dispersion layer, a filter layer and a protective layer stacked in sequence; wherein the skeleton layer is designed according to the overall mass flow and pore size of the use environment; the porosity is designed according to the required mass flow, and then the filter layer is designed according to the porosity; the dispersion layer is designed according to the gap between the skeleton layer and the filter layer; the protective layer is designed according to the air permeability requirements and the surface resistance of air flow;
[0010] After the design of the pneumatic metamaterial supersurface structure is completed, corresponding preparation is performed; the preparation method includes:
[0011] Step 301, weave the designed skeleton layer, dispersion layer, filter layer and protection layer into shape, cut them into the same size, and then stack them from bottom to top;
[0012] Step 302, placing the stacked structure into a mold, and pre-pressuring the layers to tightly bond them together;
[0013] Step 303, heating the mold at a temperature slightly lower than the melting point of the metal wire, and then applying pressure to make the tightly bonded structure reach the required thickness of the design;
[0014] Step 304 , after the structure in step 303 is naturally cooled, demolding is performed to obtain the prepared pneumatic metamaterial metasurface structure.
[0015] Compared with the prior art, the method for preparing a pneumatic metamaterial supersurface structure provided by the present invention has the following effects:
[0016] 1. The pneumatic metamaterial metasurface provided by the present invention has a simple structure and good air permeability. It can be adaptively designed according to different usage environments through a structural design method. It has a fast manufacturing speed and low production cost, and is of great industrial production value.
[0017] 2. Compared with the traditional processing technology that requires the addition of adhesives, the preparation method provided by the present invention does not require the addition of adhesives during the structure forming process, which can ensure that the porosity will not be reduced due to the curing of the adhesive after processing and forming, thereby affecting the air permeability of the aerodynamic metamaterial supersurface. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying any creative work.
[0019] Figure 1 A schematic diagram of a flow chart of a method for designing a pneumatic metamaterial metasurface structure in one embodiment;
[0020] Figure 2 A schematic diagram of a process for preparing a pneumatic metamaterial supersurface structure in an embodiment;
[0021] Figure 3 A schematic diagram of a pneumatic metamaterial metasurface structure in one embodiment;
[0022] Description of reference numerals:
[0023] Skeleton layer 11, dispersion layer 22, filtration layer 33, protection layer 44.
[0024] The purpose, features and advantages of the present invention will be further described with reference to the accompanying drawings in conjunction with the embodiments. DETAILED DESCRIPTION
[0025] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0026] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back, etc.) are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0027] In addition, in the present invention, descriptions such as "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0028] In the present invention, unless otherwise clearly specified and limited, the terms "connection", "fixation", etc. should be understood in a broad sense. For example, "fixation" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, a physical connection, or a wireless communication connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0029] It is understandable that metamaterial research first sprouted in the field of electromagnetism. Due to its unique property of penetration, it has received widespread attention and discussion. The uniqueness of metamaterials comes from their precise geometric structure and size. Based on this, many metamaterial processing methods have emerged, including PCB process, photolithography process, mask printing, electron beam etching process, laser engraving, 3D printing, mechanical ultra-precision machining, etc. Among them, PCB process, photolithography process, mask printing, electron beam etching process, and laser engraving belong to 2D processing technology. This type of processing method usually first processes various flat micro-structures on a plane, and then assembles the various parts into products. However, among these 2D processing technologies, the PCB process has low process accuracy; the photolithography process has high manufacturing cost and long preparation cycle; the structural resolution of mask printing technology will decrease in repeated deposition cycles; most 3D processing technologies cannot achieve multi-material integrated manufacturing, and often require subsequent deposition of metal layers and other processes, which limits the structural design of metamaterials; mechanical ultra-precision machining has the disadvantages of high production cost, complex processing, and low efficiency.
[0030] Based on this, the present application proposes a method for preparing a pneumatic metamaterial supersurface structure. First, the layered structure of the pneumatic metamaterial supersurface is designed. It is mainly made of metal wire material. The metal wire material has good heat resistance and chemical stability, and can maintain stable performance in extreme environments. In addition, it has good ductility, strong plasticity and flexibility, and can accurately control the size, shape and arrangement of each layer according to the weaving requirements. It is low in cost and easy to obtain. When designing each layer, it is designed specifically according to the performance parameters that need to be achieved to adapt to the use environment and work requirements.
[0031] On the other hand, a preparation method is also provided for the pneumatic metamaterial metasurface structure designed in the present invention. The preparation method adopts hot pressing to hot-press the stacked micro-layered wire mesh structure. No adhesive is added during the preparation process, which can ensure that the molded structure can maintain good air permeability and the porosity will not be reduced due to the curing of the adhesive.
[0032] It is worth noting that the aerodynamic metamaterial metasurface structure designed in this application is mainly used for thermal protection of the surface of hypersonic aircraft. By utilizing the active infiltration characteristics of the aerodynamic metamaterial metasurface under high pressure, the infiltrated working gas interacts with the incoming flow, thereby reducing the heat on the surface of the hypersonic aircraft.
[0033] The following will describe the implementation of the present invention in detail with reference to the accompanying drawings in the embodiment diagram of the present invention.
[0034] like Figure 1 and Figure 2 As shown, a method for preparing a pneumatic metamaterial supersurface structure is provided, wherein: Figure 1A schematic diagram of the process of structural design of aerodynamic metamaterial metasurface, wherein the structural design method includes:
[0035] Step 201, determining the performance parameters of the aerodynamic metamaterial metasurface according to the use environment and work requirements.
[0036] It is understandable that the characteristics that aerodynamic metamaterial metasurfaces need to possess are determined according to their use environment and work requirements. For example, in order to form stable seepage, aerodynamic metamaterial metasurfaces need to have appropriate air permeability; since they may be used in extreme environments for a long time, such as in hypersonic aircraft, they need to withstand extremely high temperatures, so they need to have certain heat resistance and chemical stability; in addition, in order to reduce friction resistance, the texture structure needs to be designed.
[0037] Based on this, the performance parameters of the aerodynamic metamaterial metasurface are determined, and the performance parameters include but are not limited to: the pressure that needs to be withstood in the use environment, mass flow rate, pore size, size, thickness and other parameters.
[0038] Step 202, based on the performance parameters, designing the pneumatic metamaterial metasurface structure; the pneumatic metamaterial metasurface structure includes a skeleton layer, a dispersion layer, a filter layer and a protective layer stacked in sequence; wherein the skeleton layer is designed according to the overall mass flow and pore size of the use environment; the porosity is designed according to the required mass flow, and then the filter layer is designed according to the porosity; the dispersion layer is designed according to the gap between the skeleton layer and the filter layer; the protective layer is designed according to the air permeability requirements and the surface resistance of air flow.
[0039] After completing the design of the pneumatic metamaterial metasurface structure, the pneumatic metamaterial metasurface structure is also prepared accordingly, such as Figure 2 As shown, the preparation method comprises:
[0040] Step 301, weave the designed skeleton layer, dispersion layer, filter layer and protection layer into shape, cut them into the same size, and then stack them up from bottom to top.
[0041] Step 302, placing the stacked structure into a mold, and pre-pressuring the layers to tightly bond them together.
[0042] Step 303, the mold is heated at a temperature slightly lower than the melting point of the metal wire, and then pressure is applied to make the structure reach the required thickness. Specifically, when applying pressure, the mold is vibrated slightly and the pressure is gradually increased. The metal wires will rub against each other due to vibration at the locations where the metal meshes contact each other, causing the local temperature to rise above the melting point. When the structure reaches the required thickness, the vibration and heating are stopped, and the pressure is maintained.
[0043] Step 304 , after the structure in step 303 is naturally cooled, demolding is performed to obtain the prepared pneumatic metamaterial metasurface structure.
[0044] It can be understood that based on the material and designed structure of the metamaterial metasurface, a corresponding preparation method is provided, and each layer of the structure is tightly combined by heating and pressurizing. While ensuring good air permeability, the traditional method of using adhesives for bonding is abandoned, ensuring that the designed porosity will not be reduced due to the curing of the adhesive after processing and molding, and the performance of the metamaterial metasurface can be maintained unaffected, improving the reliability and consistency of the finished product. At the same time, it does not rely on adhesives that may decompose at high temperatures or in specific chemical environments, which can improve the thermal and chemical stability of the material. The processing process is simple, the preparation speed is fast, and the production cost is low.
[0045] See also Figure 3 The pneumatic metamaterial metasurface designed in this application mainly includes a four-layer structure, and the skeleton layer, dispersion layer, filter layer and protective layer are all made of metal wire weaving. Among them, the skeleton layer plays a supporting role as a whole, and its weaving method should be firm and dense. The filter layer is mainly used to limit the airflow velocity and disperse the gas. It can be understood that the pores of the skeleton layer, dispersion layer and protective layer are usually relatively large. Blowing air directly outward will form a local jet, rather than a uniform air film. Adding the filter layer allows the gas to form an air film more uniformly on the surface. The filter layer needs to have a designed porosity and a uniform distribution of pore positions and sizes. The protective layer is set on the top layer, mainly used to protect other layered structures. It should be woven with a lightweight and wear-resistant material, and the overall surface of the woven structure is smooth to reduce the resistance of the incoming flow. The dispersion layer is mainly used to fill the gap between the skeleton layer and the filter layer, increase the contact area, and improve the overall strength and rigidity. Therefore, the diameter and mesh of the warp and weft in the dispersion layer are designed according to the skeleton layer and the filter layer.
[0046] In one embodiment, the skeleton layer is designed according to the overall mass flow and pore size of the use environment, including:
[0047] The diameters of the warp and weft threads in the skeleton layer are determined according to the pressure that needs to be borne in the use environment, and then the weaving method of the skeleton layer is determined according to the overall mass flow rate and the minimum pore size.
[0048] Specifically, the skeleton layer is composed of warp threads and weft threads, and the diameter of the warp threads is larger than the diameter of the weft threads. During weaving, a number of warp threads are arranged in parallel and at intervals, and each weft thread is interlaced in the warp threads to form a high-density mesh structure.
[0049] It can be understood that the skeleton layer is the main supporting structure and mainly plays a supporting role. Therefore, under the premise of ensuring air permeability, its weaving method should be mainly firm and dense. The metal mesh structure of the skeleton layer should not affect the actual use effect of the filter layer. The use of a denser weaving method can improve the pressure resistance of the skeleton layer, but an overly dense weaving form will lead to a reduction in the flow area and affect the overall mass flow rate. Therefore, an overly dense weaving form cannot be used to increase the strength of the skeleton. Therefore, the maximum allowable mass flow rate of a single-layer skeleton layer must be greater than the maximum mass flow rate of the filter layer. There is usually an air chamber under the skeleton layer. The pore size of the skeleton layer is smaller than the pore size of the filter layer, which will affect the gas flow and cause the gas to fail to flow out of the super surface according to the design conditions.
[0050] It is worth noting that the number of skeleton layers is set to be more than one layer according to the required thickness of the overall structure.
[0051] In one embodiment, the porosity is designed according to the required mass flow rate, and the expression of the porosity is:
[0052] ;
[0053] ;
[0054] In the formula, represents the porosity, Indicates the area that needs to be circulated; represents mass flow rate; Indicates the density of the circulating medium; Indicates flow rate; Indicates the coverage area.
[0055] In one embodiment, the filter layer is designed according to the porosity, including:
[0056] Determine the volume of each weft thread as: ; The number of weft threads is: .
[0057] The total volume of the weft yarn in the net is:
[0058] ;
[0059] Then calculate the total volume of the weft and warp in the filter layer:
[0060] ;
[0061] Determine the volume of the filter layer as: ;in, .
[0062] The diameter and mesh number of the weft and warp in the filter layer are determined according to the porosity. The expression is:
[0063] ;
[0064] In the formula, Indicates the warp diameter; Indicates the diameter of the weft wire; Indicates length and width.
[0065] It can be understood that the specifications of the filter layer are: warp mesh number × weft mesh number, warp diameter ( )×weft diameter( ), length and width are The weaving method of the filter layer is as follows: the weft is a straight line, and through the action of the reed and the warp, the weft is bent and deformed to form a filter layer. The weaving method formed by the weft, the reed and the warp is a conventional weaving method, which will not be described here.
[0066] The filter layer is mainly woven with metal wires. During weaving, the bending deformation of the weft wire is compensated by the extension of the metal wire. Based on this, the volume of each weft wire is obtained, and then the number of weft wires is obtained based on the number of weft wire meshes. In addition, during the weaving process, the warp wires are straight and not bent (the amount of wear and thinning of the warp wires due to weaving tension is very small and can be ignored here), so the calculation of the warp wire volume is the same as that of the weft wire. Based on this, the volume of all metal wires in the filter layer is calculated. Finally, the diameter and mesh number of the weft wires and warp wires in the filter layer are determined by the porosity, and the filter layer is woven.
[0067] In one of the embodiments, a protective layer is designed.
[0068] The protective layer is woven with a light and wear-resistant material, such as titanium alloy wire, aluminum alloy wire, copper wire, etc., preferably titanium alloy wire. During the weaving process, the maximum bending angle of the wire is limited. The bending angle is determined according to the actual situation to make the overall surface of the woven metal wire mesh smooth and have a small regular weaving structure. Preferably, the maximum bending angle of the weft is limited to less than 90°. Such a surface is not only very breathable but also can reduce the resistance of air flowing through its surface.
[0069] In one embodiment, a dispersion layer is designed.
[0070] It is understandable that the metal wire mesh of the skeleton layer has many protrusions on the surface and cannot be well combined with the filter layer, so a dispersion layer needs to be designed. The dispersion layer needs to reasonably select the wire diameter and mesh number according to the skeleton layer and the filter layer to fill the gap between the skeleton layer and the filter layer, increase the contact area, and improve the overall strength and rigidity.
[0071] It can be understood that through the design method provided by the present invention, the metamaterial metasurface can be designed specifically according to environmental conditions. By adopting the metal wire weaving method, the various performance parameters of the metamaterial metasurface can be well controlled, thereby meeting the requirements for air permeability and permeability under different conditions.
[0072] It should be understood that although Figure 1 , Figure 2 The steps in the flowchart are shown in sequence as indicated by the arrows, but these steps are not necessarily executed in the order indicated by the arrows. Unless otherwise specified in this document, there is no strict order restriction for the execution of these steps, and these steps can be executed in other orders. Moreover, Figure 1 , Figure 2 At least part of the steps may include multiple sub-steps or multiple stages. These sub-steps or stages are not necessarily executed at the same time, but can be executed at different times. The execution order of these sub-steps or stages is not necessarily sequential, but can be executed in turn or alternately with other steps or at least part of the sub-steps or stages of other steps.
[0073] The technical features of the above embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0074] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the invention. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the attached claims.
Claims
1. A method for preparing a pneumatic metamaterial supersurface structure, characterized in that: The preparation method includes designing the structure, and the structure design method includes: Determine the performance parameters of the aerodynamic metamaterial metasurface according to the use environment and work requirements; Based on the performance parameters, designing the aerodynamic metamaterial metasurface structure; The pneumatic metamaterial metasurface structure comprises a skeleton layer, a dispersion layer, a filter layer and a protective layer stacked in sequence; wherein the skeleton layer is designed according to the overall mass flow and pore size of the use environment; the porosity is designed according to the required mass flow, and then the filter layer is designed according to the porosity; the dispersion layer is designed according to the gap between the skeleton layer and the filter layer; the protective layer is designed according to the air permeability requirements and the surface resistance of air flow; The skeleton layer is designed according to the overall mass flow and pore size of the use environment, including: The diameters of the warp and weft in the skeleton layer are determined according to the pressure that the use environment needs to withstand, and then the weaving method of the skeleton layer is determined according to the overall mass flow rate and the minimum pore size; The porosity is designed according to the required mass flow rate, and the expression of the porosity is: ; ; In the formula, represents the porosity, Indicates the area that needs to be circulated; represents mass flow rate; Indicates the density of the circulating medium; Indicates flow rate; Indicates the coverage area; Designing a filter layer according to the porosity includes: Determine the volume of each weft thread as: ; The number of weft threads is: ; The total volume of the weft yarn in the net is: ; Then calculate the total volume of the weft and warp in the filter layer: ; Determine the volume of the filter layer as: ;in, ; The diameter and mesh number of the weft and warp in the filter layer are determined according to the porosity, and the expression is: ; In the formula, Indicates the warp diameter; Indicates the diameter of the weft wire; Indicates length and width; After the design of the pneumatic metamaterial supersurface structure is completed, corresponding preparation is performed; the preparation method includes: Step 301, weave the designed skeleton layer, dispersion layer, filter layer and protection layer into shape, cut them into the same size, and then stack them from bottom to top; Step 302, placing the stacked structure into a mold, and pre-pressuring the layers to tightly bond them together; Step 303, heating the mold at a temperature slightly lower than the melting point of the metal wire, and then applying pressure to make the structure reach the required thickness; Step 304, after the structure in step 303 is naturally cooled, demoulding is performed to obtain the prepared pneumatic metamaterial metasurface structure; The skeleton layer, the dispersion layer, the filter layer and the protection layer are all made by weaving metal wires.
2. The method for preparing the pneumatic metamaterial supersurface structure according to claim 1, characterized in that: The skeleton layer is composed of warp and weft, and the diameter of the warp is greater than the diameter of the weft; During weaving, a plurality of the warp threads are arranged in parallel and at intervals, and the weft threads are interlaced and interwoven among the warp threads to form a high-density mesh structure.
3. The method for preparing the pneumatic metamaterial supersurface structure according to claim 1 or 2, characterized in that: The protective layer limits the maximum bending angle of the wire during the weaving process.
4. The method for preparing the pneumatic metamaterial supersurface structure according to claim 3, characterized in that: The protective layer is made of a lightweight and wear-resistant material.