Anti-crack concrete containing modified polypropylene fiber and preparation method thereof

By using modified polypropylene fiber and other components in underwater concrete, the problem of poor cracking resistance of underwater concrete when used for a long time is solved, and the cracking resistance and service life of the concrete are significantly improved.

CN118851702APending Publication Date: 2024-10-29HUNAN QINGYU CONSTR GRP CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410974045.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

Existing underwater concrete is prone to surface cracking when used for a long time, resulting in an unguaranteed service life and affecting the quality of the concrete.

Method used

Using modified polypropylene fiber, by adding cement, gelling agent, machine-made sand, gravel, water-reducing agent, aggregate, fly ash, mineral powder, admixtures, modified polypropylene fiber, clay, and lime into the concrete , gypsum and volcanic ash and other ingredients, combined with specific proportion design and processing steps, to improve the crack resistance of concrete.

Benefits of technology

It effectively enhances the crack resistance of concrete, avoids surface cracking, extends the service life, and improves the overall performance and use quality of concrete.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses anti-crack concrete containing modified polypropylene fiber and a preparation method, the anti-crack concrete is prepared from the following main components: a strength improving component, a crack resistance improving component and a reinforcing component, and the strength improving component is composed of cement, a gelling agent, machine-made sand, broken stone and a water reducing agent. The strength of the concrete can be enhanced through the cement, the gelling agent, the machine-made sand, the gravel and the water reducing agent, the phenomenon of insufficient strength is avoided, the crack resistance of the concrete can be enhanced through the aggregate, the fly ash, the mineral powder, the additive and the modified polypropylene fiber, the phenomenon of cracking during use is avoided, and the service life of the concrete is prolonged. Through the clay, lime, gypsum and volcanic ash, the overall mixability of the concrete can be better, the phenomenon of dispersion is prevented, and the problems that the overall service life cannot be guaranteed and the use quality of the concrete is affected due to the fact that the surface of the concrete is prone to cracking after long-time use are solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of crack-resistant concrete, in particular to crack-resistant concrete containing modified polypropylene fiber and a preparation method thereof. Background Art

[0002] According to the patents published on the China Patent Network, the patent name is: An underwater concrete and a preparation method thereof, and the patent number is: 202210179966.0. This application relates to the field of building materials, and specifically discloses an underwater concrete and a preparation method thereof; an underwater concrete, comprising the following raw materials in parts by weight: 300-400 parts of medium sand, 600-750 parts of crushed stone, 120-280 parts of cement, 5-15 parts of inorganic polymer flocculant, 5-10 parts of water reducer, 100-250 parts of water, 15-45 parts of mineral admixture, and 10-25 parts of anti-seepage modified polypropylene mesh fiber. The invention discloses a method for preparing underwater concrete, wherein the present invention relates to an underwater concrete having the advantages of effectively improving the anti-seepage performance of underwater concrete; and the anti-seepage modified polypropylene mesh fiber is obtained by surface-modifying the polypropylene mesh fiber with a SY-K expansion fiber anti-cracking waterproofing agent; the preparation method comprises the following steps: mixing the raw materials except water and the anti-seepage modified polypropylene mesh fiber and stirring; then adding the anti-seepage modified polypropylene mesh fiber and stirring; finally adding water and stirring to obtain underwater concrete; the underwater concrete of the present invention has the advantages of effectively improving the anti-seepage performance of underwater concrete; however, the concrete mentioned above has poor anti-cracking performance and its surface is prone to cracking when used for a long time, which results in that the overall service life cannot be guaranteed and affects the quality of concrete.

[0003] Therefore, it is necessary to design and transform concrete to effectively prevent its poor resistance to cracking. Summary of the invention

[0004] In order to solve the problems raised in the above background technology, the purpose of the present invention is to provide a crack-resistant concrete containing modified polypropylene fiber and a preparation method, which has the advantage of containing modified polypropylene fiber to increase crack resistance and solves the problem of poor crack resistance.

[0005] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a crack-resistant concrete containing modified polypropylene fiber and a preparation method thereof, wherein the main components of the crack-resistant concrete preparation formula are: a strength-enhancing component, a crack-resistance-enhancing component and a reinforcement component.

[0006] As preferred embodiment of the present invention, the strength-enhancing component consists of cement, gelling agent, machine-made sand, crushed stone and water reducing agent, the crack resistance-enhancing component consists of aggregate, fly ash, mineral powder, admixture and modified polypropylene fiber, and the reinforcement component consists of clay, lime, gypsum and volcanic ash.

[0007] As preferred embodiment of the present invention, the contents of the components are: 205 parts of cement, 400 kg / m³ of gelling agent, 760 kg / m³ of machine-made sand, 800 kg / m³ of crushed stone, 8.5 kg / m³ of water reducing agent, 420 parts of aggregate, 64 parts of fly ash, 66 parts of mineral powder, 13 parts of admixture, 28 parts of modified polypropylene fiber, 44 parts of clay, 65 parts of lime, 65 parts of gypsum, and 39 parts of volcanic ash.

[0008] As a preferred embodiment of the present invention, the method comprises the steps of a) raw material preparation; b) mix ratio design; c) stirring treatment; d) pouring treatment; e) vibration treatment; f) curing treatment; and g) quality inspection. Step a) Raw material preparation: First, select high-quality cement that meets the standard requirements to ensure the strength and stability of the cement. Then select well-graded medium-coarse sand and continuously graded gravel with small void ratio, control the mud content and mud block content of the aggregate, and select specially modified polypropylene fibers. These fibers should have good dispersibility, good bond strength with the cement body, and enhanced crack resistance. Step b) Mix design: According to the engineering requirements and raw material properties, the basic mix ratio of cement, water and aggregate is preliminarily determined. Considering the influence of modified polypropylene fiber on the performance of concrete, the mix ratio is appropriately adjusted to ensure that the slump, workability, strength and other properties of concrete meet the requirements. The optimal dosage of modified polypropylene fiber is determined through experiments to achieve the best anti-cracking effect. Generally speaking, the dosage of fiber should be controlled within a certain range. Too much or too little may affect the performance of concrete. Step c) Mixing: dry mix cement, aggregate and other dry materials in a mixer to eliminate caking. After dry mixing, add appropriate amount of water and admixtures for wet mixing. During wet mixing, the mixing time and mixing speed should be controlled to ensure that the concrete mixture is uniform. During or after wet mixing, the modified polypropylene fiber is evenly sprinkled into the mixer, and the mixing is continued to make the fiber fully dispersed and evenly distributed in the concrete. Step d) Casting treatment: transport the mixed modified polypropylene fiber concrete to the casting site in time for casting. During the casting process, attention should be paid to controlling the casting speed and casting height to avoid excessive impact and vibration; Step e) Vibration treatment: Use appropriate vibration methods to vibrate the concrete to improve the density and uniformity of the concrete. During the vibration process, over-vibration or under-vibration should be avoided; Step f) Curing: After pouring, concrete should be cured in time to keep the concrete surface moist and the temperature stable. The curing time should be determined according to factors such as the strength grade of the concrete and climatic conditions; Step g) Quality testing: Perform strength testing on the poured concrete to ensure that the strength of the concrete meets the design requirements. Then test the concrete's crack resistance, including crack strength, crack toughness and other indicators. Then test other properties of the concrete, such as durability, impermeability, etc., as needed.

[0009] As a preferred embodiment of the present invention, the water used in the preparation of the raw materials needs to be clean drinking water or water that meets the standards for concrete mixing water.

[0010] As a preferred embodiment of the present invention, the stirring time during the stirring treatment should be appropriately extended by 1 to 2 minutes to ensure uniform dispersion of the fibers.

[0011] As a preferred embodiment of the present invention, during the stirring process, the various materials need to be added in sequence according to a proportion, and cannot be added all at once.

[0012] As a preferred embodiment of the present invention, during the quality inspection, it is necessary to ensure that surrounding workers are within a safe range to avoid splashing to the workers.

[0013] Compared with the prior art, the present invention has the following beneficial effects: 1. The present invention can enhance the strength of concrete through cement, gelling agent, machine-made sand, crushed stone and water reducing agent to avoid the phenomenon of insufficient strength; can enhance the crack resistance of concrete through aggregate, fly ash, mineral powder, admixture and modified polypropylene fiber to avoid the phenomenon of cracking during use; can make the overall mixing property of concrete better through clay, lime, gypsum and volcanic ash to prevent the phenomenon of dispersion, and solve the problem that the surface is easy to crack during long-term use, which leads to the overall service life cannot be guaranteed, affecting the use quality of concrete. DETAILED DESCRIPTION

[0014] The technical solutions in the embodiments of the present invention are described clearly and completely. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0015] The invention provides a crack-resistant concrete containing modified polypropylene fiber and a preparation method thereof. The main components of the preparation formula of the crack-resistant concrete are: a strength-enhancing component, a crack-resistance-enhancing component and a reinforcement component.

[0016] The present invention is further configured such that the strength-enhancing component consists of cement, gelling agent, machine-made sand, crushed stone and water reducing agent, the crack resistance-enhancing component consists of aggregate, fly ash, mineral powder, admixture and modified polypropylene fiber, and the reinforcement component consists of clay, lime, gypsum and volcanic ash.

[0017] The present invention is further configured such that the content of each component is: 205 parts of cement, 400 kg / m³ of gelling agent, 760 kg / m³ of machine-made sand, 800 kg / m³ of crushed stone, 8.5 kg / m³ of water reducing agent, 420 parts of aggregate, 64 parts of fly ash, 66 parts of mineral powder, 13 parts of admixture, 28 parts of modified polypropylene fiber, 44 parts of clay, 65 parts of lime, 65 parts of gypsum, and 39 parts of volcanic ash.

[0018] The present invention is further configured to include step a) raw material preparation; step b) mix ratio design; step c) stirring treatment; step d) pouring treatment; step e) vibration treatment; step f) curing treatment; step g) quality inspection; Step a) Raw material preparation: First, select high-quality cement that meets the standard requirements to ensure the strength and stability of the cement. Then select well-graded medium-coarse sand and continuously graded gravel with small void ratio, control the mud content and mud block content of the aggregate, and select specially modified polypropylene fibers. These fibers should have good dispersibility, good bond strength with the cement body, and enhanced crack resistance. Step b) Mix design: According to the engineering requirements and raw material properties, the basic mix ratio of cement, water and aggregate is preliminarily determined. Considering the influence of modified polypropylene fiber on the performance of concrete, the mix ratio is appropriately adjusted to ensure that the slump, workability, strength and other properties of concrete meet the requirements. The optimal dosage of modified polypropylene fiber is determined through experiments to achieve the best anti-cracking effect. Generally speaking, the dosage of fiber should be controlled within a certain range. Too much or too little may affect the performance of concrete. Step c) Mixing: dry mix cement, aggregate and other dry materials in a mixer to eliminate caking. After dry mixing, add appropriate amount of water and admixtures for wet mixing. During wet mixing, the mixing time and mixing speed should be controlled to ensure that the concrete mixture is uniform. During or after wet mixing, the modified polypropylene fiber is evenly sprinkled into the mixer, and the mixing is continued to make the fiber fully dispersed and evenly distributed in the concrete. Step d) Casting treatment: transport the mixed modified polypropylene fiber concrete to the casting site in time for casting. During the casting process, attention should be paid to controlling the casting speed and casting height to avoid excessive impact and vibration; Step e) Vibration treatment: Use appropriate vibration methods to vibrate the concrete to improve the density and uniformity of the concrete. During the vibration process, over-vibration or under-vibration should be avoided; Step f) Curing: After pouring, concrete should be cured in time to keep the concrete surface moist and the temperature stable. The curing time should be determined according to factors such as the strength grade of the concrete and climatic conditions; Step g) Quality testing: Perform strength testing on the poured concrete to ensure that the strength of the concrete meets the design requirements. Then test the concrete's crack resistance, including crack strength, crack toughness and other indicators. Then test other properties of the concrete, such as durability, impermeability, etc., as needed.

[0019] The present invention is further configured such that the water used in the preparation of raw materials needs to be clean drinking water or water that meets the standards for concrete mixing water.

[0020] The present invention is further configured such that the stirring time during the stirring process should be appropriately extended by 1 to 2 minutes to ensure uniform dispersion of the fibers.

[0021] The present invention is further configured such that, during the mixing process, each material needs to be added in sequence according to a proportion, and cannot be added all at once.

[0022] The present invention is further configured such that, during quality inspection, it is necessary to ensure that surrounding workers are within a safe range to avoid splashing onto the workers.

[0023] The working principle and use process of the present invention are as follows: first, high-quality cement that meets the standard requirements is selected to ensure the strength and stability of the cement, then medium-coarse sand with good gradation and gravel with continuous gradation and small porosity are selected, the mud content and mud block content of the aggregate are controlled, and polypropylene fibers that have been specially modified are selected. These fibers should have good dispersibility, bond strength with the cement body, and enhanced crack resistance. Then, according to the engineering requirements and the properties of the raw materials, the basic mix ratio of cement, water, and aggregate is preliminarily determined, and the influence of the addition of modified polypropylene fibers on the properties of concrete is considered. The mix ratio is appropriately adjusted to ensure that the slump, workability, strength and other properties of the concrete meet the requirements. The optimal dosage of the modified polypropylene fibers is determined through experiments to achieve the best anti-cracking effect. Generally speaking, the dosage of the fibers should be controlled within a certain range. Too much or too little may affect the properties of the concrete. Then, the cement, aggregate and other dry materials are dry-mixed evenly in a mixer to eliminate the caking phenomenon. After dry mixing evenly, an appropriate amount of water and admixtures are added for wet mixing. The wet mixing process The mixing time and speed should be controlled during the process to ensure that the concrete mixture is uniform. During or after wet mixing, the modified polypropylene fiber should be evenly sprinkled into the mixer, and continued to stir to make the fiber fully dispersed and evenly distributed in the concrete. The mixed modified polypropylene fiber concrete should be transported to the pouring site for pouring in time. During the pouring process, attention should be paid to controlling the pouring speed and pouring height to avoid excessive impact and vibration. Then, a suitable vibration method should be used to vibrate the concrete to improve the density and uniformity of the concrete. Over-vibration or missed vibration should be avoided during the vibration process. After the concrete is poured, it should be cured in time to keep the surface of the concrete moist and the temperature stable. The curing time should be determined according to factors such as the strength grade of the concrete and climatic conditions. Then, the strength of the poured concrete should be tested to ensure that the strength of the concrete meets the design requirements. Then, the crack resistance of the concrete is tested through experiments, including indicators such as crack resistance strength and crack toughness. Other properties of the concrete, such as durability and impermeability, are tested as needed.

[0024] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0025] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A crack-resistant concrete containing modified polypropylene fiber and a preparation method thereof, Features: The main components of the crack-resistant concrete preparation formula are: a strength-enhancing component, a crack-resistance-enhancing component and a reinforcement component.

2. The anti-cracking concrete containing modified polypropylene fiber and the preparation method according to claim 1, Features: The strength-enhancing component consists of cement, gelling agent, machine-made sand, crushed stone and water reducing agent, the crack-resistance-enhancing component consists of aggregate, fly ash, mineral powder, admixture and modified polypropylene fiber, and the reinforcement component consists of clay, lime, gypsum and volcanic ash.

3. The crack-resistant concrete containing modified polypropylene fiber and the preparation method according to claim 2, Features: The contents of the components are: 205 parts of cement, 400 kg / m³ of gelling agent, 760 kg / m³ of machine-made sand, 800 kg / m³ of crushed stone, 8.5 kg / m³ of water reducing agent, 420 parts of aggregate, 64 parts of fly ash, 66 parts of mineral powder, 13 parts of admixture, 28 parts of modified polypropylene fiber, 44 parts of clay, 65 parts of lime, 65 parts of gypsum, and 39 parts of volcanic ash.

4. A method for preparing crack-resistant concrete containing modified polypropylene fiber according to any one of claims 1 to 3, Features: The method comprises the steps of a) raw material preparation; b) mix ratio design; c) mixing treatment; d) pouring treatment; e) vibration treatment; f) curing treatment; and g) quality inspection. Step a) Raw material preparation: First, select high-quality cement that meets the standard requirements to ensure the strength and stability of the cement. Then select well-graded medium-coarse sand and continuously graded gravel with small void ratio, control the mud content and mud block content of the aggregate, and select specially modified polypropylene fibers. These fibers should have good dispersibility, good bond strength with the cement body, and enhanced crack resistance. Step b) Mix design: According to the engineering requirements and raw material properties, the basic mix ratio of cement, water and aggregate is preliminarily determined. Considering the influence of modified polypropylene fiber on the performance of concrete, the mix ratio is appropriately adjusted to ensure that the slump, workability, strength and other properties of concrete meet the requirements. The optimal dosage of modified polypropylene fiber is determined through experiments to achieve the best anti-cracking effect. Generally speaking, the dosage of fiber should be controlled within a certain range. Too much or too little may affect the performance of concrete. Step c) Mixing: dry mix cement, aggregate and other dry materials in a mixer to eliminate caking. After dry mixing, add appropriate amount of water and admixtures for wet mixing. During wet mixing, the mixing time and mixing speed should be controlled to ensure that the concrete mixture is uniform. During or after wet mixing, the modified polypropylene fiber is evenly sprinkled into the mixer, and the mixing is continued to make the fiber fully dispersed and evenly distributed in the concrete. Step d) Casting treatment: transport the mixed modified polypropylene fiber concrete to the casting site in time for casting. During the casting process, attention should be paid to controlling the casting speed and casting height to avoid excessive impact and vibration; Step e) Vibration treatment: Use appropriate vibration methods to vibrate the concrete to improve the density and uniformity of the concrete. During the vibration process, over-vibration or under-vibration should be avoided; Step f) Curing: After pouring, concrete should be cured in time to keep the concrete surface moist and the temperature stable. The curing time should be determined according to factors such as the strength grade of the concrete and climatic conditions; Step g) Quality testing: Perform strength testing on the poured concrete to ensure that the strength of the concrete meets the design requirements. Then test the concrete's crack resistance, including crack strength, crack toughness and other indicators. Then test other properties of the concrete, such as durability, impermeability, etc., as needed.

5. The crack-resistant concrete containing modified polypropylene fiber and the preparation method according to claim 4, Features: The water used in the preparation of the raw materials needs to be clean drinking water or water that meets the standards for concrete mixing water.

6. The crack-resistant concrete containing modified polypropylene fiber and the preparation method according to claim 4, Features: The stirring time during the stirring treatment should be appropriately extended by 1 to 2 minutes to ensure uniform dispersion of the fibers.

7. The crack-resistant concrete containing modified polypropylene fiber and the preparation method thereof according to claim 4, Features: During the mixing process, the various materials need to be added in sequence according to the proportion, and cannot be added all at once.

8. The crack-resistant concrete containing modified polypropylene fiber and the preparation method according to claim 4, Features: During the quality inspection, it is necessary to ensure that surrounding workers are within a safe range to avoid splashing onto the workers.

Citation Information

Patent Citations

  • Novel method for pouring steel fiber composite concrete member

    CN102786262A

  • Expansive anti-crack fiber concrete and preparation method therefor

    CN105601199A

  • Preparation method of high-impermeability concrete

    CN110734257A

  • High-strength corrosion-resistant concrete and preparation method of prefabricated part of high-strength corrosion-resistant concrete

    CN114436573A

  • Cementitious composites having wood-like properties and methods of manufacture