Semiconductor structure and forming method thereof

By cleaning the substrate surface and forming an adsorption layer during the semiconductor manufacturing process, the problem of potential leakage caused by impurities and defects after removal is solved, the device performance and stability are improved, and the risk of leakage is reduced.

CN118866652APending Publication Date: 2024-10-29XINMENG TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410889099.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-03
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

After removal during the semiconductor manufacturing process, impurities and defects remaining on the wafer surface lead to potential leakage risks, especially affecting the performance of dynamic random access memory (DRAM) devices.

Method used

The substrate surface after the removal treatment is cleaned, and an adsorption layer is formed after the cleaning treatment. The adsorption layer material can be an oxide or a high-K dielectric material, formed by atomic layer deposition, covering the entire substrate surface to fix impurities and defects.

Benefits of technology

Effectively eliminate leakage hazards caused by impurities and defects, improve device performance and stability, reduce the probability of leakage, and control process costs and risks at the same time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118866652A_ABST
    Figure CN118866652A_ABST
Patent Text Reader

Abstract

The invention discloses a semiconductor structure and a forming method thereof. The forming method comprises the following steps: forming a substrate; carrying out removal treatment on the substrate; carrying out cleaning treatment on the surface of the substrate subjected to the removal treatment; and forming an adsorption layer on the surface of the cleaned substrate. After the removal treatment, cleaning the surface of the substrate subjected to the removal treatment; and forming an adsorption layer on the surface of the cleaned substrate. The adsorption layer can effectively fix impurities left on the surface of the substrate, can effectively eliminate the hidden danger of electric leakage caused by the impurities, is beneficial to improving the performance of the device, and is beneficial to guaranteeing the stability of the device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a forming method thereof. Background Art

[0002] In the semiconductor manufacturing process, material removal processes such as etching and grinding are often used; the cleaning step after removal can obtain a clean surface to prevent impurities generated during the removal process from affecting the performance of the formed structure.

[0003] Although the cleaning step after the removal treatment can remove a large amount of impurities, impurities will still remain on the surface of the wafer, and the removal treatment itself is also prone to form defects on the surface of the wafer; the presence of impurities and defects will bring leakage risks to the semiconductor structure.

[0004] Especially for dynamic random access memory (DRAM), leakage potential is more harmful and greatly affects the performance of the device. Summary of the invention

[0005] The problem solved by the invention is how to eliminate the hidden danger of leakage caused by impurities and defects.

[0006] In order to solve the above problems, the present invention provides a method for forming a semiconductor structure, comprising:

[0007] forming a substrate; performing a removal process on the substrate; performing a cleaning process on the surface of the substrate that has undergone the removal process; and forming an adsorption layer on the surface of the substrate that has undergone the cleaning process.

[0008] Optionally, in the step of performing a removal treatment on the substrate, the removal treatment includes at least one of a planarization treatment and an etching treatment.

[0009] Optionally, in the step of forming a substrate, the substrate has a silicon surface; in the step of performing a removal treatment on the substrate, the silicon surface of the substrate is removed; in the step of performing a cleaning treatment on the surface of the substrate that has undergone the removal treatment, the silicon surface that has undergone the removal treatment is cleaned; in the step of forming an adsorption layer on the surface of the substrate that has undergone the cleaning treatment, an adsorption layer is formed on the silicon surface that has undergone the cleaning treatment.

[0010] Optionally, in the step of forming an adsorption layer on the surface of the cleaned substrate, the material of the adsorption layer is an oxide.

[0011] Optionally, in the step of forming an adsorption layer on the surface of the substrate after the cleaning treatment, the material of the adsorption layer is a high-K dielectric material.

[0012] Optionally, the material of the adsorption layer includes at least one of hafnium oxide, zirconium oxide, titanium oxide and aluminum oxide.

[0013] Optionally, in the step of forming an adsorption layer on the surface of the cleaned substrate, the formation temperature is in the range of 300°C to 400°C.

[0014] Optionally, in the step of forming an adsorption layer on the surface of the cleaned substrate, the thickness of the adsorption layer is less than 10 nm.

[0015] Optionally, in the step of forming an adsorption layer on the surface of the cleaned substrate, the adsorption layer is formed by atomic layer deposition.

[0016] Optionally, in the step of forming an adsorption layer on the surface of the cleaned substrate, the adsorption layer covers the entire surface of the substrate.

[0017] Optionally, the semiconductor structure is a dynamic random access memory.

[0018] Optionally, the step of forming a base includes: providing a substrate; forming a word line within a first surface of the substrate; in the step of performing a removal treatment on the substrate, the removal treatment thins the second surface of the substrate, wherein the second surface is arranged opposite to the first surface; in the step of forming an adsorption layer on the surface of the substrate after the cleaning treatment, the adsorption layer covers the word line exposed on the second surface.

[0019] Optionally, the step of forming a substrate further includes: forming a shielding metal within the first surface of the substrate; in the step of forming an adsorption layer on the surface of the substrate after the cleaning treatment, the adsorption layer also covers the word lines exposed on the second surface.

[0020] Optionally, the step of forming a substrate further includes: forming a storage capacitor on the first surface of the substrate.

[0021] Optionally, the step of forming a storage capacitor on the first surface of the substrate includes: sequentially forming a first electrode layer, a capacitor dielectric layer, and a second electrode layer on the first surface of the substrate.

[0022] Optionally, in the step of sequentially forming a first electrode layer, a capacitor dielectric layer and a second electrode layer on the first surface of the substrate, a material of the capacitor dielectric layer is a high-K dielectric material.

[0023] Optionally, the method further includes: forming a bit line on the second surface of the substrate.

[0024] Accordingly, the present invention further provides a semiconductor structure, comprising:

[0025] A substrate; an adsorption layer, wherein the adsorption layer is located on the surface of the substrate.

[0026] Optionally, the substrate has a silicon surface; and the adsorption layer is located on the silicon surface.

[0027] Optionally, the material of the adsorption layer is oxide.

[0028] Optionally, the material of the adsorption layer is a high-K dielectric material.

[0029] Optionally, the material of the adsorption layer includes at least one of hafnium oxide, zirconium oxide, titanium oxide and aluminum oxide.

[0030] Optionally, the adsorption layer has a thickness of less than 10 nm.

[0031] Optionally, the adsorption layer conformally covers the surface of the substrate.

[0032] Optionally, the adsorption layer covers the entire surface of the substrate.

[0033] Optionally, the semiconductor structure is a dynamic random access memory.

[0034] Optionally, the substrate comprises:

[0035] A substrate; a word line, wherein the word line is located in a first surface of the substrate; and the adsorption layer also covers the word line exposed on a second surface, wherein the second surface is arranged opposite to the first surface.

[0036] Optionally, the base further includes: a shielding metal, wherein the shielding metal is located within the first surface of the substrate; and the adsorption layer also covers the shielding metal exposed on the second surface.

[0037] Optionally, the substrate further includes: a storage capacitor, and the storage capacitor is located on the first surface of the substrate.

[0038] Optionally, the storage capacitor includes: a first electrode layer, a capacitor dielectric layer, and a second electrode layer sequentially located on the first surface.

[0039] Optionally, the material of the capacitor dielectric layer is a high-K dielectric material.

[0040] Optionally, it also includes: a bit line, wherein the bit line is located on the second surface of the substrate.

[0041] Compared with the prior art, the technical solution of the present invention has the following advantages:

[0042] In the technical solution of the present invention, after the removal treatment, the surface of the substrate subjected to the removal treatment is cleaned; an adsorption layer is formed on the surface of the substrate subjected to the cleaning treatment. The adsorption layer can effectively fix the impurities remaining on the surface of the substrate, can effectively eliminate the leakage risk caused by the impurities, is conducive to improving the performance of the device, and is conducive to ensuring the stability of the device.

[0043] In an optional solution of the present invention, the material of the adsorption layer is an oxide. The material of the adsorption layer is set to an oxide, and an oxidation effect needs to be introduced in the process of forming the adsorption layer. The process of forming the adsorption layer can repair the defects on the surface of the substrate, can effectively improve the quality of the surface of the substrate, can effectively eliminate the leakage current caused by the defects, is conducive to improving the performance of the device, and is conducive to ensuring the stability of the device.

[0044] In an optional solution of the present invention, the material of the adsorption layer is set to be a high-K dielectric material. The introduction of the high-K dielectric material can introduce heavy metal elements into the substrate; the heavy metal elements and the substrate material are prone to generate dipoles, which can effectively increase the energy of the conduction band bottom of the substrate material, thereby effectively reducing the probability of leakage.

[0045] In an optional solution of the present invention, in the step of forming the adsorption layer, the formation temperature is controlled within the range of 300° C. to 400° C. The temperature for forming the adsorption layer is relatively low, which can effectively reduce the thermal budget in the process of forming the semiconductor structure, can effectively control the process risk, and is conducive to improving device performance, device stability and manufacturing yield. BRIEF DESCRIPTION OF THE DRAWINGS

[0046] Figures 1 to 4 It is a schematic cross-sectional structure diagram of each step of an embodiment of a semiconductor structure of the present invention;

[0047] Figures 5 to 26 It is a schematic structural diagram of each step of another embodiment of the semiconductor structure of the present invention. DETAILED DESCRIPTION

[0048] As can be seen from the background technology, the residual impurities and defects in the prior art may bring about the hidden danger of leakage.

[0049] In order to solve the above technical problem, the present invention provides a method for forming a semiconductor structure, comprising:

[0050] forming a substrate; performing a removal process on the substrate; performing a cleaning process on the surface of the substrate that has undergone the removal process; and forming an adsorption layer on the surface of the substrate that has undergone the cleaning process.

[0051] The technical solution of the present invention is to clean the surface of the substrate after the removal treatment, and form an adsorption layer on the surface of the substrate after the cleaning treatment. The adsorption layer can effectively fix the impurities remaining on the surface of the substrate, effectively eliminate the leakage risk caused by the impurities, and is conducive to improving the performance of the device and ensuring the stability of the device.

[0052] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0053] refer to Figures 1 to 4 , showing a schematic structural diagram of each step of an embodiment of a method for forming a semiconductor structure of the present invention.

[0054] The forming method comprises:

[0055] A substrate 110 is formed; a removal process is performed on the substrate 110; a surface of the substrate 110 after the removal process is cleaned; and an adsorption layer 120 is formed on the surface of the substrate after the cleaned process.

[0056] The technical solution of the semiconductor structure forming method embodiment is described in detail below with reference to the accompanying drawings.

[0057] refer to Figure 1 , forming a substrate 110.

[0058] The substrate 110 is used to provide a process basis and mechanical support. Specifically, the substrate 110 has a layer to be processed 112, and the layer to be processed 112 is used to provide a process basis.

[0059] In some embodiments, in the step of forming the substrate 110, the substrate has a silicon surface 110a. Figure 1 In some of the embodiments shown, the material of the layer to be processed 112 may be silicon, and the surface of the layer to be processed 112 is the silicon surface 110 a .

[0060] In some embodiments, the base 110 further has a substrate 111, the layer to be processed 112 is located on the substrate 111, and the substrate 111 is used to provide mechanical support. For example, the substrate 111 is a silicon substrate, and the material of the substrate 111 is silicon. Specifically, the material of the substrate 111 can be selected from monocrystalline silicon, polycrystalline silicon or amorphous silicon.

[0061] In other embodiments, the material of the substrate may also be selected from silicon, germanium, gallium arsenide or silicon germanium compound; the substrate may also be selected from having an epitaxial layer or a silicon structure on an epitaxial layer; the substrate may also be other semiconductor materials.

[0062] refer to Figure 2 , the substrate 110 is removed.

[0063] The removal process is used to remove a portion of the material of the substrate 110 .

[0064] In some embodiments of the present invention, in the step of performing a removal process on the substrate 110, the removal process includes at least one of a planarization process and an etching process. Figure 2 As shown, in the step of removing the substrate 110, the substrate 110 is planarized and etched in sequence. In other embodiments of the present invention, in the step of removing the substrate, the substrate may be planarized or etched.

[0065] In some embodiments of the present invention, the substrate 110 has a silicon surface 110a; in the step of performing a removal treatment on the substrate 110, the removal treatment is performed on the silicon surface 110a of the substrate 110. That is, the silicon surface 110a of the substrate 110 is the active surface of the removal treatment, and the material removed by the removal treatment is separated from the silicon surface 110a and the substrate 110.

[0066] Specifically, Figure 2 As shown, the base 110 has a layer to be processed 112 located on the substrate 111; in the step of performing a removal treatment on the base 110, the surface of the layer to be processed 112 is subjected to the removal treatment; illustratively, the step of performing a removal treatment on the base 110 includes: performing a planarization treatment on the surface of the layer to be processed 112; and etching the surface of the layer to be processed 112 after the planarization treatment.

[0067] It should be noted that if Figure 2 In some of the embodiments shown, the removal treatment is performed on the surface of the layer to be processed 112 to completely remove the layer to be processed 112 and expose the surface of the substrate 111. In other embodiments of the present invention, the removal treatment is performed on the surface of the layer to be processed 112 to remove part of the material of the layer to be processed and reduce the thickness of the layer to be processed, but the layer to be processed is not completely removed and the substrate surface is not exposed.

[0068] like Figure 2 As shown, after the removal treatment, there are a large number of impurities (such as Figure 2 As shown in the figure, there are impurities 112a in the substrate, as well as defects generated during the removal process, and the surface quality of the substrate after the removal process is poor.

[0069] refer to Figure 3 , the surface of the substrate that has undergone the removal treatment is cleaned.

[0070] The cleaning process is used to remove impurities on the surface of the substrate that has undergone the removal process.

[0071] In some exemplary embodiments, the cleaning process may be a DSP process cleaning process or a SPM process cleaning process.

[0072] In some embodiments, the substrate 110 has a silicon surface 110a, and the removal treatment is performed on the silicon surface 110a of the substrate 110. Therefore, in the step of cleaning the substrate surface after the removal treatment, the silicon surface 110a after the removal treatment is cleaned.

[0073] Specifically, Figure 3 As shown, the base 110 has a layer to be treated 112 located on the substrate 111; the removal treatment treats the surface of the layer to be treated 112; in the step of cleaning the surface of the base after the removal treatment, the surface of the layer to be treated 112 after the removal treatment is cleaned.

[0074] like Figure 3 As shown, although the cleaning treatment can remove most of the impurities on the surface of the substrate that has been removed, and the cleaning solution of the cleaning treatment can repair a small amount of defects on the surface of the substrate that has been removed; however, the cleaning treatment cannot completely remove the impurities remaining on the surface of the substrate that has been removed, nor can it completely repair the defects on the surface of the substrate that has been removed; after the cleaning treatment, there are still impurities and defects remaining on the surface of the substrate that has been removed, and the remaining impurities and defects will cause leakage hazards to the formed semiconductor structure.

[0075] refer to Figure 4 , an adsorption layer 120 is formed on the surface of the substrate after the cleaning treatment.

[0076] The adsorption layer 120 is used to absorb and fix impurities remaining on the surface of the substrate after the cleaning process.

[0077] The adsorption layer 120 can effectively absorb and fix impurities remaining on the surface of the substrate, can effectively isolate defects remaining on the surface of the substrate, can effectively eliminate the leakage risk caused by impurities, and is beneficial to improving device performance and ensuring device stability.

[0078] In some embodiments, the substrate 110 has a silicon surface 110a, the removal treatment is performed on the silicon surface 110a of the substrate 110, and the cleaning treatment is performed on the silicon surface 110a that has undergone the removal treatment; therefore, in the step of forming an adsorption layer 120 on the surface of the substrate that has undergone the cleaning treatment, an adsorption layer 120 is formed on the silicon surface 110a that has undergone the cleaning treatment.

[0079] In some embodiments of the present invention, in the step of forming the adsorption layer 120 on the surface of the substrate after the cleaning treatment, the formation temperature is in the range of 300° C. to 400° C. The formation temperature in the step of forming the adsorption layer 120 on the surface of the substrate after the cleaning treatment is controlled. The formation temperature is appropriate, which can effectively reduce the thermal budget in the process of forming the semiconductor structure, can effectively control the process risk, and is conducive to ensuring the performance stability and reliability of the formed semiconductor structure, and is conducive to improving the yield of the formed semiconductor structure.

[0080] In some embodiments of the present invention, in the step of forming the adsorption layer 120 on the surface of the substrate after the cleaning treatment, the material of the adsorption layer 120 is oxide. In the process of forming the adsorption layer 120 made of oxide material, oxidation needs to be introduced. The introduction of oxidation can repair the defects on the surface of the substrate, effectively improve the quality of the surface of the substrate, effectively eliminate the leakage current caused by the defects, and is conducive to improving the performance of the device and ensuring the stability of the device.

[0081] In some embodiments, in the step of forming an adsorption layer 120 on the surface of the substrate after the cleaning treatment, the material of the adsorption layer 120 is a high-K dielectric material. The formation of the high-K dielectric material adsorption layer 120 can introduce heavy metal elements into the adsorption layer 120; heavy metal elements can easily form dipoles with the elements of the substrate material, thereby effectively improving the energy of the bottom of the conduction band and effectively reducing the probability of leakage. Exemplarily, the high-K dielectric material is a dielectric material with a dielectric constant greater than 20. For example, the material of the adsorption layer 120 includes: at least one of hafnium oxide, zirconium oxide, titanium oxide and aluminum oxide.

[0082] In some embodiments of the present invention, in the step of forming the adsorption layer 120 on the surface of the cleaned substrate, the thickness of the adsorption layer 120 is less than 10 nm. The thickness of the adsorption layer 120 is appropriate, which can eliminate the leakage risk while controlling the process cost and process time.

[0083] In some embodiments of the present invention, in the step of forming the adsorption layer 120 on the surface of the substrate after the cleaning process, the adsorption layer 120 is formed by atomic layer deposition. The adsorption layer 120 formed by the atomic layer deposition method can conformally cover the surface of the substrate after the cleaning process, and the material film layer has high quality, which can better ensure the elimination of leakage hazards.

[0084] In some embodiments of the present invention, in the step of forming the adsorption layer 120 on the surface of the cleaned substrate, the adsorption layer 120 covers the entire surface of the substrate. When the adsorption layer 120 covers the entire surface of the substrate, the impurities and defects remaining on the surface of the substrate can be absorbed, fixed and isolated by the adsorption layer 120 as much as possible, thereby ensuring the elimination effect of the leakage hazard as much as possible.

[0085] refer to Figures 5 to 26 , showing a schematic structural diagram of each step of another embodiment of the semiconductor structure forming method of the present invention.

[0086] The present invention will not repeat the same points as the above embodiments. In some embodiments of the present invention, the semiconductor structure is a dynamic random access memory (DRAM). Dynamic random access memory is a volatile memory. Dynamic random access memory includes: a plurality of memory cells, the memory cells include: a transistor and a capacitor controlled by the transistor, and each memory cell is electrically connected to each other through a word line and a bit line.

[0087] In some embodiments of the present invention, Figures 5 to 16 As shown, the steps of forming the base 210 include: providing a substrate 211; forming a word line WL (eg, Fig.13 and Fig.14 In addition, in some embodiments, the step of forming the base 210 further includes: forming a shielding metal RM (such as Fig.11 and Fig.14 shown).

[0088] refer to Figure 5 and Figure 6 The steps of forming the base 210 include: first providing a substrate 211; Figure 6 yes Figure 5 Schematic diagram of the cross-sectional structure along line A1A2.

[0089] Specifically, the substrate 211 is a silicon substrate, and the material of the substrate 211 is silicon. Specifically, the material of the substrate 211 can be selected from single crystal silicon, polycrystalline silicon or amorphous silicon. In other embodiments, the material of the substrate can also be selected from silicon, germanium, gallium arsenide or silicon germanium compound; the substrate can also be selected from having an epitaxial layer or a silicon structure on an epitaxial layer; the substrate can also be other semiconductor materials.

[0090] like Figure 5 and Figure 6 As shown, the base 210 further includes an isolation structure 212 , and the isolation structure 212 is located in the first surface 211 a of the substrate 211 .

[0091] Specifically, in a plane parallel to the first surface 211a, the isolation structure 212 is in the shape of a long strip extending along the first direction x. Figure 5As shown, the substrate 210 has a plurality of isolation structures 212, and the plurality of isolation structures 212 are separated from each other, and an active region (not shown in the figure) is formed between adjacent isolation structures 212. Moreover, the plurality of isolation structures 212 are arranged in parallel along a second direction y, wherein the second direction y and the first direction x are both parallel to the first surface 211a, and the second direction y and the first direction x are perpendicular to each other.

[0092] For example, the material of the isolation structure 212 is silicon oxide. In other embodiments of the present invention, the isolation structure 212 may also be a low-K dielectric material or an ultra-low-K dielectric material, such as doped silicon dioxide, organic polymers, and porous materials.

[0093] like Figure 6 As shown, the substrate 211 further has a second surface 211 b opposite to the first surface 211 a ; the isolation structure 212 extends from the first surface 211 a toward the second surface 211 a .

[0094] refer to Figures 7 to 14 After providing the substrate 211, the step of forming the base 210 further includes: forming a shielding metal RM (such as Fig.11 and Fig.14 ) and word lines WL (as shown Fig.13 and Fig.14 shown).

[0095] like Figure 7 and Figure 8 As shown, Figure 8 yes Figure 7 Specifically, the step of forming the shielding metal RM and the word line WL in the substrate 211 includes: forming a first trench 219a and a second trench 219b in the substrate 211.

[0096] Specifically, the first groove 219a and the second groove 219b extend from the first surface 211a to the second surface 211b. In some embodiments, the depth of the first groove 219a and the second groove 219b is less than the depth of the isolation structure 212; along the direction from the first surface 211a to the second surface 211b, the size of the first groove 219a and the second groove 219b is less than the size of the isolation structure 212. For example, the first groove 219a and the second groove 219b can be formed by photolithography and etching.

[0097] like Figure 7As shown, the first trench 219a and the second trench 219b extend along the second direction y and are parallel to each other along the first direction x. The first trench 219a and the second trench 219b pass through a plurality of isolation structures 212 along the second direction y and cross a plurality of active regions.

[0098] For example, in the step of forming the first groove 219a and the second groove 219b in the substrate 211, the first groove 219a and the second groove 219b are formed in the substrate 211 with an interval between them, and the first groove 219a is located between two adjacent second grooves 219b, and the second groove 219b is located between two adjacent second grooves 219b.

[0099] like Fig. 9 and Fig.10 As shown, Fig.10 yes Fig. 9 After forming the first groove 219a and the second groove 219b, the first groove 219a (such as Figure 7 and Figure 8 As shown), a sacrificial material 219 is filled inside.

[0100] The sacrificial material 219 is suitable for filling the first groove 219a. Specifically, the sacrificial material 210 is a SOC material (Spin On Carbon, SOC). SOC material is a polymer with a high C content. For example, the sacrificial material 219 can be filled in the first groove 219a by spin coating.

[0101] Specifically, the step of filling the sacrificial material 219 in the first groove 219a includes: filling the first groove 219a and the second groove 219b with prefabricated sacrificial material (not shown in the figure); removing the prefabricated sacrificial material in the second groove 219b, and retaining the prefabricated sacrificial material in the first groove 210a to form the sacrificial material 219.

[0102] like Fig.11 and Fig.12 As shown, Fig.12 yes Fig.11 Schematic diagram of the cross-sectional structure along the D1D2 line. Figure 7 and Figure 8 After the sacrificial material 219 is filled in the second trench 219b, a shielding metal RM is formed in the second trench 219b.

[0103] In some embodiments, the shielding metal RM is located in the dielectric material, that is, in the second groove 210b, and the shielding metal RM is surrounded by the dielectric material. For example, the steps of forming the shielding metal RM in the second groove 219b include: forming a dielectric layer in the second groove 219b; forming a dielectric material in the second groove 219b with a dielectric layer formed on the inner wall; etching back the dielectric material filled in the second groove 219b so that the top surface of the remaining dielectric material is lower than the first surface 211a; filling the shielding metal material on the remaining dielectric material; etching back the shielding metal material to form the shielding metal RM, the top surface of the shielding metal RM is lower than the first surface 211a; filling the dielectric material on the shielding metal RM again, and the top surface of the dielectric material filled again is flush with the first surface 211a.

[0104] In some exemplary embodiments, in the step of forming a dielectric layer in the second groove 219b, the dielectric layer may be silicon oxide. In other embodiments, the dielectric layer may also be other low-K dielectric materials or ultra-low-K dielectric materials, such as doped silicon dioxide, organic polymers, and porous materials. Specifically, the dielectric layer may be formed in the second groove 219b by deposition, wherein the deposition method may be chemical vapor deposition, physical vapor deposition, or atomic layer deposition.

[0105] In some exemplary embodiments, in at least one of the step of forming a dielectric material in the second trench 219b and the step of refilling the dielectric material on the shielding metal RM, the dielectric material may be silicon oxide. In other embodiments, the dielectric material may also be other low-K dielectric materials or ultra-low-K dielectric materials, such as doped silicon dioxide, organic polymers, and porous materials. Specifically, the dielectric material may be formed by deposition, wherein the deposition method may be chemical vapor deposition, physical vapor deposition, or atomic layer deposition.

[0106] In some exemplary embodiments, in the step of filling the shielding metal material on the remaining dielectric material, the shielding metal material may be titanium nitride. Specifically, the shielding metal material may be filled by deposition, wherein the deposition method may be chemical vapor deposition, physical vapor deposition, or atomic layer deposition. In other embodiments of the present invention, the shielding metal material may also be other conductive materials.

[0107] In some exemplary embodiments, at least one of the steps of etching back the dielectric material filled in the second groove 219b and etching back the shielding metal material to form a shielding metal RM can be performed by at least one of dry etching and wet etching.

[0108] like Fig.13and Fig.14 As shown, Fig.14 yes Fig.13 After forming the shielding metal RM in the second trench 219b, a word line WL is formed in the first trench 219a.

[0109] In some embodiments, the word line WL is located in a dielectric material, that is, in the first trench 219a, and the word line WL is surrounded by a dielectric material. For example, the step of forming the word line WL in the first trench 219a includes: forming a dielectric layer in the first trench 219a, the dielectric layer covering the sidewalls and the bottom of the first trench 219a; forming a word line layer in the first trench 219a with the dielectric layer formed on the inner wall, the word line layer covering the dielectric layer in the first trench 219a; after forming the word line layer, filling the first trench 219a with a dielectric material; etching the word line layer and the dielectric material in the first trench 219a so that the top surface of the word line layer is lower than the first surface 211a, forming the word line WL; and filling the dielectric material again on the word line WL, the top surface of the dielectric material filled again being flush with the first surface 211a.

[0110] In some exemplary embodiments, in the step of forming a dielectric layer in the first groove 219a, the dielectric layer may be silicon oxide. In other embodiments, the dielectric layer may also be other low-K dielectric materials or ultra-low-K dielectric materials, such as doped silicon dioxide, organic polymers, and porous materials. Specifically, the dielectric layer may be formed in the first groove 219a by deposition, wherein the deposition method may be chemical vapor deposition, physical vapor deposition, or atomic layer deposition.

[0111] In some exemplary embodiments, in at least one of the step of filling the first trench 219a with a dielectric material and the step of filling the word line WL with a dielectric material again, the dielectric material may be silicon oxide. In other embodiments, the dielectric material may also be other low-K dielectric materials or ultra-low-K dielectric materials, such as doped silicon dioxide, organic polymers, and porous materials. Specifically, the dielectric material may be formed by deposition, wherein the deposition method may be chemical vapor deposition, physical vapor deposition, or atomic layer deposition.

[0112] In some exemplary embodiments, in the step of forming a word line layer in the first trench 219a having the dielectric layer formed on the inner wall, the word line layer may be titanium nitride and tungsten. Specifically, the word line layer may be formed by deposition, wherein the deposition method may be chemical vapor deposition, physical vapor deposition, or atomic layer deposition. In other embodiments of the present invention, the word line layer may also be other conductive materials.

[0113] In some exemplary embodiments, in the step of etching the word line layer and the dielectric material in the first trench 219 a , the etching back may be performed by at least one of dry etching and wet etching.

[0114] It should be noted that, in some embodiments, after forming the shielding metal RM in the second trench 219b and before forming the word line WL in the first trench 219a, the formation method further includes: removing the sacrificial material 219 in the first trench 219a to open the first trench 219a.

[0115] Therefore, if Fig.13 As shown, in a plane parallel to the first surface 211 a , the shielding metal RM and the word line WL are in the shape of long strips extending along the second direction y, and the extending directions of the shielding metal RM and the word line WL are perpendicular to the extending direction of the isolation structure 212 .

[0116] For example, in the step of forming a shielding metal RM and a word line WL in the substrate 211 , a plurality of shielding metals RM and a plurality of word lines WL are formed in the substrate 211 , and the plurality of shielding metals RM and the plurality of word lines WL are parallel to each other along a first direction x.

[0117] Specifically, the plurality of shielding metal RMs and the plurality of word lines WLs are arranged at intervals, one shielding metal RM is located between two adjacent word lines WL, and one word line WL is located between two adjacent shielding metal RMs.

[0118] It should be noted that Figures 5 to 14 In some embodiments shown, after forming the shielding metal RM in the second trench 219b, the word line WL is formed in the first trench 219a. In other embodiments of the present invention, after forming the word line in the first trench, the shielding metal may be formed in the second trench. The present invention does not limit the order of forming the shielding metal and the word line.

[0119] refer to Fig.15 and Fig.16 , among which Fig.16 yes Fig.15 Schematic diagram of the cross-sectional structure along the F1F2 line.

[0120] In some embodiments, the step of forming the substrate 210 further includes: forming a storage capacitor CP on the first surface 211a of the substrate 211. Fig.16 In some of the embodiments shown, the step of forming a storage capacitor CP on the first surface 211a of the substrate 211 includes: sequentially forming a first electrode layer (not shown in the figure), a capacitor dielectric layer CPI and a second electrode layer (not shown in the figure) on the first surface 211a of the substrate 211.

[0121] The capacitor dielectric layer CPI is located between the first electrode layer and the second electrode layer to achieve electrical insulation between the first electrode layer and the second electrode layer.

[0122] In some specific embodiments, in the step of sequentially forming a first electrode layer, a capacitor dielectric layer CPI, and a second electrode layer on the first surface 211a of the substrate 211, the material of the capacitor dielectric layer CPI is a high-K dielectric material. Setting the material of the capacitor dielectric layer CPI to a high-K dielectric material can increase the capacitance of the storage capacitor CP while minimizing the distance between the first electrode layer and the second electrode layer to control the size of the storage unit.

[0123] Form the substrate 210 (eg Fig.15 After that, the forming method further comprises: removing the substrate 210. Fig.17 As shown, in the step of performing a removal process on the base 210, the removal process thins the second surface 211b of the substrate 211. Fig.17 yes Fig.16 Schematic diagram of the cross-sectional structure at the corresponding position.

[0124] In some embodiments, the substrate 211 is a silicon substrate; the second surface 211b is a silicon surface; and the second surface 211b is a silicon surface of the base 210. In the step of thinning the second surface 211b of the substrate 211 by removing the substrate 211, the removal is performed on the silicon surface of the base 210.

[0125] In some embodiments, the step of removing the second surface 211b of the substrate 211 by thinning the second surface 211b includes: flattening the second surface 211b of the substrate 211; and etching the flattened second surface 211b. In other embodiments of the present invention, the second surface 211b of the substrate 211 may also be flattened or etched.

[0126] It should be noted that the removal process is performed on the second surface 211b of the substrate 211; Fig.17 As shown, the formation method also includes: after forming the base 210 and before removing the base 210, bonding a carrier wafer 301 on the first surface 211a; after bonding the carrier wafer 301, inverting the base 210 to thin the second surface 211 of the substrate 211.

[0127] like Fig.17As shown, the substrate 210 also has an interlayer dielectric material, and the storage capacitor CP is located in the interlayer dielectric material. Specifically, the first surface 211a of the substrate 211 is sequentially covered with a first interlayer dielectric layer 218 and a second interlayer dielectric layer 217, and the storage capacitor CP is partially located in the first interlayer dielectric layer 218, and the remaining part is located in the second interlayer dielectric layer 217; and the second interlayer dielectric layer 217 also covers the top surface of the storage capacitor CP.

[0128] The carrier wafer 301 has a wafer body 302 and a dielectric layer 303 located on the surface of the wafer body 302; in the step of bonding the carrier wafer 301 on the first surface 211a, the surface of the carrier wafer 301 is relatively attached to and connected to the surface of the second dielectric layer 217 to achieve bonding of the carrier wafer 301.

[0129] Specifically, the step of removing the second surface 211b of the substrate 211 to reduce the thickness includes: Fig.18 As shown, the second surface 211b of the substrate 211 is planarized to expose the isolation structure 212; Fig.19 As shown, the isolation structure 212 exposed by the second surface 211b after planarization is etched back, and the etching back exposes the word line WL in the substrate 210; in addition, the substrate 210 also has a shielding metal RM, and in the step of etching back the isolation structure 212 exposed by the second surface 211b after planarization, the etching back also exposes the shielding metal RM in the substrate 210.

[0130] It should be noted that Fig.18 yes Fig.17 A schematic diagram of the structure viewed from above along the A direction; Fig.17 yes Fig.19 Schematic diagram of the cross-sectional structure along line G1G2.

[0131] like Figures 17 to 20 As shown, after the isolation structure 212 exposed by the planarized second surface 211b is etched back, a gap 214 is formed between adjacent active areas AA in the substrate 211, and the gap exposes the word line WL and the shielding metal; in addition, a cavity 216 is formed between the active area AA and the word line WL, and the cavity 216 is connected to the gap 214 between the adjacent active areas AA, and the word line WL is also exposed; a cavity 215 is formed between the active area AA and the shielding metal RM, and the cavity 215 is connected to the gap 214 between the adjacent active areas AA, and the shielding metal RM is also exposed.

[0132] After the substrate 210 is subjected to the removal treatment, the forming method further comprises: performing a cleaning treatment on the surface of the substrate 210 subjected to the removal treatment.

[0133] Specifically, Figures 17 to 20 As shown, in the step of cleaning the surface of the substrate 210 that has been removed, the surfaces of the exposed active area AA, the isolation structure 212, the word line WL and the shielding metal RM are cleaned to remove residues on the surfaces of the active area AA, the isolation structure 212, the word line WL and the shielding metal RM.

[0134] After the cleaning process, the formation method further includes: forming an adsorption layer 220 on the surface of the cleaned substrate 210. The adsorption layer 220 can effectively absorb and fix residual impurities, effectively isolate residual defects, and effectively eliminate the leakage risk caused by impurities, which is beneficial to improving device performance and ensuring device stability.

[0135] Specifically, Fig.21 and Fig. 22 As shown, in the step of forming the adsorption layer 220 on the surface of the cleaned substrate 210, the adsorption layer 220 (eg, Fig.21 Medium red, Fig. 22 shown in green).

[0136] Moreover, a word line WL is formed in the substrate 210, and the word line WL is exposed on the second surface 211b of the thinned substrate 211. Therefore, in the step of forming an adsorption layer 220 on the surface of the cleaned substrate 210, the adsorption layer 220 covers the word line WL exposed on the second surface 211b.

[0137] In addition, a shielding metal RM is formed in the base 210, and the shielding metal RM is exposed on the second surface 211b of the thinned substrate 211. Therefore, in the step of forming an adsorption layer 220 on the surface of the base 210 after the cleaning treatment, the adsorption layer 220 also covers the shielding metal RM exposed on the second surface 211b.

[0138] like Fig. 20 As shown, the gap 214 between adjacent active areas AA, the cavity 216 between the active area AA and the word line WL, and the cavity 215 between the active area AA and the shielding metal RM are all interconnected, and the word line WL and the shielding metal RM are exposed from the space where the gap 214, the cavity 216, and the cavity 215 are connected; in the step of forming the adsorption layer 220 on the surface of the substrate 210 that has been cleaned, the adsorption layer 220 covers the gap 214, the cavity 216, and the inner wall of the cavity 215.

[0139] In some embodiments, the substrate 211 is a silicon substrate, and the active area AA is a substrate 212 between adjacent isolation structures 212; therefore, the inner wall of the gap 214 between adjacent active areas AA, the inner wall of the gap 216 formed by the active area AA, and the inner wall of the cavity 215 formed by the active area AA are all cleaned silicon surfaces; therefore, in the step of forming an adsorption layer 220 on the cleaned surface of the substrate 210, the adsorption layer 220 covers the cleaned silicon surface.

[0140] In some embodiments, in the step of forming an adsorption layer 220 on the surface of the substrate 210 that has been cleaned, the material of the adsorption layer 220 is oxide, that is, the process of forming the adsorption layer 220 has an oxidizing effect. The introduction of oxidation can repair surface defects and effectively improve surface quality.

[0141] In some embodiments, in the step of forming the adsorption layer 220 on the surface of the substrate 210 after the cleaning treatment, the material of the adsorption layer 220 is a high-K dielectric material. The method of setting the adsorption layer 220 as a high-K dielectric material can not only increase the energy of the conduction band bottom to suppress leakage, but also control the process risk to effectively reduce the damage probability of the capacitor dielectric layer CPI of the storage capacitor CP in the substrate 210. In some exemplary embodiments, the material of the adsorption layer 220 is the same as the material of the capacitor dielectric layer CPI.

[0142] refer to Figure 22 to Figure 24 In some embodiments of the present invention, the forming method further comprises: forming a bit line BL on the second surface 211b of the substrate 211. Fig. 22 yes Fig.18 and Fig.19 Schematic diagram of the top view structure at the corresponding angle, Fig.23 yes Fig. 22 Schematic diagram of the cross-sectional structure at the H1H2 line position. Fig.24 yes Fig. 20 Schematic diagram of the three-dimensional structure at the corresponding angle.

[0143] Specifically, in a plane parallel to the second surface 211b, the word line BL is in a strip shape extending along the first direction x; the extending direction of the word line BL is perpendicular to the extending directions of the shielding metal RM and the word line WL. Moreover, in the step of forming the bit line BL on the second surface 211b of the substrate 211, the bit line BL is formed on the second surface 211b of the substrate 211, and a plurality of the bit lines BL are arranged in parallel along the second direction y.

[0144] In some embodiments of the present invention, in the step of forming the bit line BL on the second surface 211 b of the substrate 211 , the position of the bit line BL corresponds to the position of the active area AA.

[0145] In some embodiments, in the step of forming the bit line BL on the second surface 211b of the substrate 211, the bit line BL is formed on the second surface 211b of the substrate 211 in a self-aligned manner. For example, a metal material is formed on the second surface 211b of the substrate 211; an annealing process is performed to react the metal material with the silicon surface of the active area AA to form the bit line BL; and unreacted metal material is removed; therefore, the material of the formed bit line BL is a metal silicide, such as a silicon-nickel intermetallic compound.

[0146] In some embodiments of the present invention, the forming method further comprises: after forming the bit line BL on the second surface 211b of the substrate 211, at least filling the gap 214 (such as Fig. 20 As shown in Fig.23 As shown, the step of filling at least the gap 214 between adjacent active areas AA includes: filling the interlayer dielectric material 230 between the adjacent active areas AA, and the interlayer dielectric material 230 also fills part of the cavity 216 (such as Fig. 20 as shown) and a portion of the cavity 215 (as shown Fig. 20 As shown in FIG. 4 , the interlayer dielectric material further extends to the top surface of the bit line BL, covering the bit line BL.

[0147] In some embodiments of the present invention, the forming method further comprises: Fig.25 As shown, after filling the gap 214 between adjacent active areas AA, a back end of line (BEOL) process is performed on the second surface 211b to form an interconnection layer beol; a control wafer 410 is bonded to the surface of the interconnection layer beol and the control wafer is electrically connected to the word line WL; as shown in FIG. Fig.26 As shown, after bonding the control wafer 410, external interconnect pads po (Pad out), through silicon vias tsv (through silicon via, TSV) and redistribution layers (redistribution layer, RDL) (not shown in the figure) are formed.

[0148] Correspondingly, the present invention also provides a semiconductor structure.

[0149] refer to Figure 4 , showing a schematic cross-sectional structure diagram of an embodiment of a semiconductor structure of the present invention.

[0150] In some embodiments of the present invention, the semiconductor structure may be formed by the method for forming a semiconductor structure of the present invention, and thus the specific technical solution of the semiconductor structure may refer to the embodiments of the method for forming a semiconductor structure described above.

[0151] The semiconductor structure includes a substrate 110. The substrate 110 is used to provide a process foundation and mechanical support.

[0152] In some embodiments, the substrate 110 has a silicon surface. Figure 4 In some embodiments shown, the base 110 has a substrate 111, and the substrate 111 is used to provide mechanical support. For example, the substrate 111 is a silicon substrate, and the material of the substrate 111 is silicon. Specifically, the material of the substrate 111 can be selected from single crystal silicon, polycrystalline silicon or amorphous silicon.

[0153] In other embodiments, the material of the substrate may also be selected from silicon, germanium, gallium arsenide or silicon germanium compound; the substrate may also be selected from having an epitaxial layer or a silicon structure on an epitaxial layer; the substrate may also be other semiconductor materials.

[0154] The surface of the substrate is subjected to a removal treatment and a cleaning treatment after the removal treatment. Although the cleaning treatment can remove most of the impurities and defects remaining on the surface of the substrate; Figure 4 As shown, after the cleaning process, impurities and defects still remain on the surface of the substrate, and the remaining impurities and defects may cause leakage hazards to the formed semiconductor structure.

[0155] The semiconductor structure further includes an adsorption layer 120 , and the adsorption layer 120 is located on the surface of the substrate 110 .

[0156] The adsorption layer 120 is used to absorb and fix impurities remaining on the surface of the substrate after the cleaning process.

[0157] The adsorption layer 120 can effectively absorb and fix impurities remaining on the surface of the substrate, can effectively isolate defects remaining on the surface of the substrate, can effectively eliminate the leakage risk caused by impurities, and is beneficial to improving device performance and ensuring device stability.

[0158] In some embodiments, the substrate 110 has a silicon surface, and the adsorption layer 120 covers the silicon surface. Figure 4 As shown, the surface of the substrate 111 is subjected to a removal treatment and a cleaning treatment after the removal treatment, and the adsorption layer 120 covers the surface of the substrate 111 .

[0159] In some embodiments of the present invention, the material of the adsorption layer 120 is oxide. The oxidation reaction of the oxide can repair the defects on the surface of the substrate, effectively improve the quality of the substrate surface, effectively eliminate the leakage current caused by the defects, and is beneficial to improving the performance of the device and ensuring the stability of the device.

[0160] In some embodiments, the material of the adsorption layer 120 is a high-K dielectric material. The formation of the high-K dielectric material adsorption layer 120 can introduce heavy metal elements into the adsorption layer 120; the heavy metal elements are easy to form dipoles with the elements of the base material, thereby effectively improving the energy of the conduction band bottom and effectively reducing the probability of leakage. For example, the material of the adsorption layer 120 includes: at least one of hafnium oxide, zirconium oxide, titanium oxide and aluminum oxide.

[0161] In some embodiments of the present invention, the thickness of the adsorption layer 120 is less than 10 nm. The thickness of the adsorption layer 120 is appropriate, which can eliminate the leakage risk and control the process cost and process time.

[0162] In some embodiments of the present invention, the adsorption layer 120 is conformally covered on the surface of the substrate. The conformally covered adsorption layer 120 can effectively reduce process risks, and the material film layer has high quality, which can better ensure the elimination of leakage hazards.

[0163] In some embodiments of the present invention, the adsorption layer 120 covers the entire substrate surface. The adsorption layer 120 completely covers the entire substrate surface so that the impurities and defects remaining on the substrate surface can be absorbed, fixed and isolated by the adsorption layer 120 as much as possible, thereby ensuring the elimination of leakage hazards as much as possible.

[0164] refer to Fig.24 and Fig.25 , showing a schematic structural diagram of another embodiment of the semiconductor structure of the present invention; wherein Fig.24 yes Fig.25 A schematic three-dimensional structure diagram of a semiconductor structure embodiment is shown.

[0165] The present invention will not repeat the same points as the above embodiments. In some embodiments of the present invention, the semiconductor structure is a dynamic random access memory (DRAM). Dynamic random access memory is a volatile memory. The dynamic random access memory includes: a plurality of memory cells, the memory cells include: a transistor and a capacitor controlled by the transistor, and each memory cell is electrically connected to each other through a word line and a bit line.

[0166] like Fig.24 and Fig.25 As shown, the semiconductor structure has a substrate 210 .

[0167] In some embodiments of the present invention, the base 210 includes: a substrate 211. Specifically, the substrate 211 is a silicon substrate, and the material of the substrate 211 is silicon. Specifically, the material of the substrate 211 can be selected from single crystal silicon, polycrystalline silicon or amorphous silicon. In other embodiments, the material of the substrate can also be selected from silicon, germanium, gallium arsenide or silicon germanium compound; the substrate can also be selected from having an epitaxial layer or a silicon structure on an epitaxial layer; the substrate can also be other semiconductor materials.

[0168] like Figure 5 and Figure 6 As shown, the base 210 further includes: an isolation structure 212, and the isolation structure 212 is located in the first surface 211a of the substrate 211. Figure 5 yes Fig.23 A schematic top view of the first surface 211a of the substrate 211 in the semiconductor structure shown; Figure 6 yes Figure 5 A schematic diagram of the cross-sectional structure of the position of the A1A2 line in the semiconductor structure shown.

[0169] Specifically, in a plane parallel to the first surface 211a, the isolation structure 212 is in the shape of a long strip extending along the first direction x. Figure 5 As shown, the substrate 210 has a plurality of isolation structures 212, and the plurality of isolation structures 212 are separated from each other, and an active area AA (such as Fig.24 and Fig.25 shown).

[0170] The plurality of isolation structures 212 are arranged in parallel along a second direction y, wherein the second direction y and the first direction x are both parallel to the first surface 211 a , and the second direction y and the first direction x are perpendicular to each other.

[0171] For example, the material of the isolation structure 212 is silicon oxide. In other embodiments of the present invention, the isolation structure 212 may also be a low-K dielectric material or an ultra-low-K dielectric material, such as doped silicon dioxide, organic polymers, and porous materials.

[0172] like Figure 6 As shown, the substrate 211 further has a second surface 211 b opposite to the first surface 211 a ; the isolation structure 212 extends from the first surface 211 a toward the second surface 211 a .

[0173] like Fig.24 and Fig.25 As shown, the semiconductor structure further comprises an adsorption layer 220 located on the surface of the substrate 210. Specifically, as Fig.23 and Fig.24 As shown, the adsorption layer 220 covers the exposed active area AA and the surface of the isolation structure 212 .

[0174] For example, the active area AA and the isolation structure 212 are exposed from the second surface 211 b of the substrate 211 , and the adsorption layer 220 covers the surface of the active area AA and the isolation structure 212 exposed from the second surface 211 b of the substrate 211 .

[0175] The adsorption layer 220 can effectively absorb and fix residual impurities, can effectively isolate residual defects, can effectively eliminate the leakage hidden danger caused by impurities, is beneficial to improving device performance, and is beneficial to ensuring device stability.

[0176] In some embodiments, the substrate 211 is a silicon substrate, and the active area AA is a substrate 212 between adjacent isolation structures 212; therefore, the inner wall of the gap 214 between adjacent active areas AA, the inner wall of the gap 216 formed by the active area AA, and the inner wall of the cavity 215 formed by the active area AA are all cleaned silicon surfaces; therefore, the adsorption layer 220 covers the exposed silicon surface of the substrate 210.

[0177] In some embodiments, the material of the adsorption layer 220 is oxide, that is, the process of forming the adsorption layer 220 has an oxidation effect, and the introduction of the oxidation effect can repair surface defects and effectively improve the surface quality.

[0178] In some embodiments of the present invention, the substrate 210 further comprises a word line WL, and the word line WL is located in the first surface 211a of the substrate 211. In addition, in some embodiments, the substrate 210 further comprises a shielding metal RM, and the shielding metal RM is located in the first surface 211a of the substrate 211.

[0179] Combined with reference Fig. 22 , in a plane parallel to the first surface 211a, the shielding metal RM and the word line WL are in the shape of a strip extending along the second direction y, and the extending directions of the shielding metal RM and the word line WL are perpendicular to the extending direction of the isolation structure 212. For example, the substrate 211 has a plurality of shielding metal RMs and a plurality of word lines WL, and the plurality of shielding metal RMs and the plurality of word lines WL are parallel to each other along the first direction x.

[0180] In addition, the plurality of shielding metal RMs and the plurality of word lines WLs are arranged at intervals, one shielding metal RM is located between two adjacent word lines WL, and one word line WL is located between two adjacent shielding metal RMs.

[0181] like Fig. 22As shown, the word line WL is exposed from the second surface 211b of the substrate 211, and the adsorption layer 220 covers the word line WL exposed from the second surface 211b; the shielding metal RM is exposed from the second surface 211b of the substrate 211, and the adsorption layer 220 also covers the shielding metal RM exposed from the second surface 211b.

[0182] like Fig. 20 As shown, the gap 214 between adjacent active areas AA, the cavity 216 between the active area AA and the word line WL, and the cavity 215 between the active area AA and the shielding metal RM are all interconnected, and the word line WL and the shielding metal RM are exposed from the space where the gap 214, the cavity 216, and the cavity 215 are connected; the adsorption layer 220 covers the inner walls of the gap 214, the cavity 216, and the cavity 215.

[0183] Continue to refer Fig.24 and Fig.25 In some embodiments of the present invention, the substrate 210 further includes: a storage capacitor CP, and the storage capacitor CP is located on the first surface 211a of the substrate 211. For example, the storage capacitor CP includes: a first electrode layer (not shown in the figure), a capacitor dielectric layer CPI, and a second electrode layer (not shown in the figure) sequentially located on the first surface 211a.

[0184] The capacitor dielectric layer CPI is located between the first electrode layer and the second electrode layer to achieve electrical insulation between the first electrode layer and the second electrode layer.

[0185] In some specific embodiments, the material of the capacitor dielectric layer CPI is a high-K dielectric material. Setting the material of the capacitor dielectric layer CPI to a high-K dielectric material can increase the capacitance of the storage capacitor CP while minimizing the distance between the first electrode layer and the second electrode layer to control the size of the storage unit.

[0186] In some embodiments, the material of the adsorption layer 220 is a high-K dielectric material. The adsorption layer 220 made of a high-K dielectric material can not only increase the energy of the conduction band bottom to suppress leakage, but also control the process risk to effectively reduce the damage probability of the capacitor dielectric layer CPI of the storage capacitor CP in the substrate 210. In some exemplary embodiments, the material of the adsorption layer 220 is the same as the material of the capacitor dielectric layer CPI.

[0187] like Fig.24 and Fig.25 As shown, in some embodiments of the present invention, the semiconductor structure further includes: a bit line BL, and the bit line BL is located on the second surface 211 b of the substrate 211 .

[0188] like Fig. 22 As shown, in a plane parallel to the second surface 211b, the word line BL is in the shape of a long strip extending along the first direction x; the extending direction of the word line BL is perpendicular to the extending direction of the shielding metal RM and the word line WL. Moreover, in the step of forming the bit line BL on the second surface 211b of the substrate 211, the bit line BL is formed on the second surface 211b of the substrate 211, and a plurality of the bit lines BL are arranged in parallel along the second direction y. Specifically, the position of the bit line BL corresponds to the position of the active area AA. In some embodiments, the material of the bit line BL is a metal silicide formed in a self-aligned manner, such as a silicon-nickel intermetallic compound.

[0189] like Fig.25 In some embodiments shown in the figure, the semiconductor structure further includes: an interlayer dielectric material 230, the interlayer dielectric material 230 at least fills the gap between adjacent active areas AA; for example, the interlayer dielectric material 230 also fills part of the cavity 216 (such as Fig. 20 as shown) and a portion of the cavity 215 (as shown Fig. 20 As shown in FIG. 4 , the interlayer dielectric material further extends to the top surface of the bit line BL, covering the bit line BL.

[0190] In addition, if Fig.25 As shown, in some embodiments, the semiconductor structure further includes: an interconnection layer beol, the interconnection layer beol is located on the second surface; a control wafer 410, the control wafer 410 is bonded to the surface of the interconnection layer beol and is electrically connected to the control wafer and the word line WL.

[0191] like Fig.26 In some embodiments shown, the semiconductor structure further includes: an external interconnection pad po (Pad out), a through silicon via tsv (TSV) and a redistribution layer (RDL) (not shown in the figure). The external interconnection pad po is located on the first surface 211a of the substrate 211; the through silicon via tsv extends from the side of the storage capacitor CP away from the substrate 211 to the interconnection layer beol on the second surface 211b of the substrate 211.

[0192] In summary, after the removal process, the surface of the substrate subjected to the removal process is cleaned; an adsorption layer is formed on the surface of the substrate subjected to the cleaning process. The adsorption layer can effectively fix the impurities remaining on the surface of the substrate, can effectively eliminate the leakage risk caused by the impurities, is beneficial to improving the performance of the device, and is beneficial to ensuring the stability of the device.

[0193] Moreover, the material of the adsorption layer is an oxide. The material of the adsorption layer is set to an oxide, and an oxidation effect needs to be introduced in the process of forming the adsorption layer. The process of forming the adsorption layer can repair the defects on the surface of the substrate, can effectively improve the quality of the surface of the substrate, can effectively eliminate the leakage current caused by the defects, is conducive to improving the performance of the device, and is conducive to ensuring the stability of the device.

[0194] In addition, the material of the adsorption layer is set to be a high-K dielectric material. The introduction of the high-K dielectric material can introduce heavy metal elements into the substrate; the heavy metal elements and the substrate material are prone to generate dipoles, which can effectively increase the energy of the conduction band bottom of the substrate material, thereby effectively reducing the probability of leakage.

[0195] In addition, in the step of forming the adsorption layer, the formation temperature is controlled within the range of 300° C. to 400° C. The lower the temperature of forming the adsorption layer, the more effectively the thermal budget in the process of forming the semiconductor structure can be reduced, the more effectively the process risk can be controlled, and the more favorable the device performance, the more stable the device and the more favorable the manufacturing yield can be.

[0196] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A method for forming a semiconductor structure, characterized in that: include: forming a base; performing a removal process on the substrate; Cleaning the surface of the substrate after the removal treatment; An adsorption layer is formed on the surface of the substrate after the cleaning treatment.

2. The forming method according to claim 1, characterized in that: In the step of performing a removal treatment on the substrate, the removal treatment includes at least one of a planarization treatment and an etching treatment.

3. The forming method according to claim 1, characterized in that: In the step of forming a substrate, the substrate has a silicon surface; In the step of performing a removal treatment on the substrate, a silicon surface of the substrate is removed; In the step of cleaning the substrate surface after the removal treatment, the silicon surface after the removal treatment is cleaned; In the step of forming an adsorption layer on the surface of the cleaned substrate, an adsorption layer is formed on the surface of the cleaned silicon.

4. The forming method according to any one of claims 1 to 3, characterized in that: In the step of forming an adsorption layer on the surface of the cleaned substrate, the material of the adsorption layer is oxide.

5. The forming method according to claim 4, characterized in that: In the step of forming an adsorption layer on the surface of the cleaned substrate, the material of the adsorption layer is a high-K dielectric material.

6. The forming method according to claim 5, characterized in that: The material of the adsorption layer includes at least one of hafnium oxide, zirconium oxide, titanium oxide and aluminum oxide.

7. The forming method according to any one of claims 1 to 3, characterized in that: In the step of forming an adsorption layer on the surface of the cleaned substrate, the formation temperature is in the range of 300°C to 400°C.

8. The forming method according to any one of claims 1 to 3, characterized in that: In the step of forming an adsorption layer on the surface of the cleaned substrate, the thickness of the adsorption layer is less than 10 nm.

9. The forming method according to any one of claims 1 to 3, characterized in that: In the step of forming an adsorption layer on the surface of the cleaned substrate, the adsorption layer is formed by atomic layer deposition.

10. The forming method according to any one of claims 1 to 3, characterized in that: In the step of forming an adsorption layer on the surface of the cleaned substrate, the adsorption layer covers the entire surface of the substrate.

11. The forming method according to claim 1, characterized in that: The semiconductor structure is a dynamic random access memory.

12. The forming method according to claim 1, characterized in that: The steps of forming the substrate include: providing a substrate; forming word lines in the first surface of the substrate; In the step of performing a removal treatment on the substrate, the removal treatment thins the second surface of the substrate, wherein the second surface is disposed opposite to the first surface; In the step of forming an adsorption layer on the surface of the cleaned substrate, the adsorption layer covers the word lines exposed on the second surface.

13. The forming method according to claim 12, characterized in that: The step of forming the base also includes: forming a shielding metal within the first surface of the substrate; In the step of forming an adsorption layer on the surface of the cleaned substrate, the adsorption layer also covers the word lines exposed on the second surface.

14. The forming method according to claim 12, characterized in that: The step of forming a substrate further includes: forming a storage capacitor on the first surface of the substrate.

15. The forming method according to claim 14, characterized in that: The step of forming a storage capacitor on the first surface of the substrate comprises: A first electrode layer, a capacitor dielectric layer and a second electrode layer are sequentially formed on the first surface of the substrate.

16. The forming method according to claim 15, characterized in that: In the step of sequentially forming a first electrode layer, a capacitor dielectric layer and a second electrode layer on the first surface of the substrate, the capacitor dielectric layer is made of a high-K dielectric material.

17. The forming method according to claim 12, characterized in that: Also includes: A bit line is formed on the second surface of the substrate.

18. A semiconductor structure, characterized in that: include: substrate; The adsorption layer is located on the surface of the substrate.

19. The semiconductor structure according to claim 18, wherein: The substrate has a silicon surface; the adsorption layer is located on the silicon surface.

20. The semiconductor structure according to claim 18, wherein: The material of the adsorption layer is oxide.

21. The semiconductor structure according to claim 20, wherein: The material of the adsorption layer is a high-K dielectric material.

22. The semiconductor structure according to claim 21, wherein: The material of the adsorption layer includes at least one of hafnium oxide, zirconium oxide, titanium oxide and aluminum oxide.

23. The semiconductor structure according to claim 18, wherein: The thickness of the adsorption layer is less than 10 nm.

24. The semiconductor structure according to claim 18, wherein: The adsorption layer conformally covers the surface of the substrate.

25. The semiconductor structure according to claim 18, wherein: The adsorption layer covers the entire surface of the substrate.

26. The semiconductor structure according to claim 18, wherein: The semiconductor structure is a dynamic random access memory.

27. The semiconductor structure according to claim 18, wherein: The substrate comprises: substrate; A word line, the word line being located within the first surface of the substrate; The adsorption layer also covers the word lines exposed on the second surface, wherein the second surface is arranged opposite to the first surface.

28. The semiconductor structure according to claim 27, wherein: The base also includes: a shielding metal, the shielding metal is located within the first surface of the substrate; The adsorption layer also covers the shielding metal exposed on the second surface.

29. The semiconductor structure according to claim 27, wherein: The substrate further includes a storage capacitor, and the storage capacitor is located on the first surface of the substrate.

30. The semiconductor structure according to claim 29, wherein: The storage capacitor comprises: a first electrode layer, a capacitor dielectric layer and a second electrode layer which are sequentially located on the first surface.

31. The semiconductor structure according to claim 30, wherein: The material of the capacitor dielectric layer is a high-K dielectric material.

32. The semiconductor structure of claim 27, wherein: Also includes: A bit line is located on the second surface of the substrate.