Method for manufacturing frequency selective wave-absorbing flexible film material by using maskless femtosecond laser
The array structure is prepared on the composite film through maskless femtosecond laser direct writing technology, which solves the cumbersome problem of the existing integrated material preparation method, and realizes the performance of infrared high-wave absorption and microwave high-wave transmission, which is suitable for stealth Radar and other applications.
Patent Information
- Application Number
- CN202410951979.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-05
AI Technical Summary
The existing methods of absorbing and permeable materials are cumbersome and difficult to operate, making it difficult to achieve efficient frequency selective wave absorption and wave transmission performance, especially in applications in infrared and microwave bands.
The array structure is prepared on the surface of the composite film by maskless femtosecond laser direct writing technology, and the gold film and silicon dioxide film are plated through magnetron sputtering method, and the patterned etching is used for femtosecond laser to form a frequency selective function. Materials, simplifying the processing process and reducing costs.
It realizes high absorption rate in the infrared band and high transmission rate in the microwave band, provides a more efficient frequency selective functional material, suitable for stealth radar and other applications, and the processing process is simple and controllable.
Smart Images

Figure CN118893318A_ABST
Abstract
Description
1. Technical Field
[0001] The invention belongs to the field of preparation of frequency selective wave absorbing and transmitting functional materials, and specifically relates to a method for manufacturing an integrated wave absorbing and transmitting flexible functional material by using a femtosecond laser direct writing technology. 2. Background Technology
[0002] The integrated absorbent and penetrating material has a wide range of applications in stealth radars, antenna covers, etc. It is an important difficulty at this stage to be able to easily prepare this material and ensure its excellent performance. At present, most of the frequency-selective surfaces that are integrated with absorbent and penetrating use multi-layer patch materials. The frequency-selective wave absorption function is achieved through the superposition structure of metal patches and intermediate dielectric metal patches. Different patch sizes, shapes, materials, thickness of the intermediate dielectric layer, etc. have an impact on the frequency band and absorption performance. As shown in patent 202210120202.4, this method achieves broadband wave transmission within the X-band by superimposing a square ring-shaped metal patch and a cross-shaped metal patch on the upper layer, two square ring-shaped metal patches on the lower layer, and resistor patches welded on the two square ring-shaped metal patches. The effect of obtaining a higher absorption rate outside the band is obtained by loading resistors. Although the desired effect can be achieved, its disadvantages are cumbersome preparation and difficult operation.
[0003] Surface micro-nano structures have a wide range of applications in the fields of anti-reflection, hydrophobicity, hydrophilicity, wear resistance, and stealth materials. Due to the many excellent physical and chemical properties of surface micro-nano structures, they have a wide range of application values and have received extensive attention from the scientific community in recent years. Among them, recent studies have found that after the surface micro-nano structure of a material is processed, the material will have an impact on the absorptivity and transmittance of different bands. This discovery provides a new idea for various absorbent and transmittance-in-one materials.
[0004] The surface micro-nano structure is applied to the frequency selective surface. Compared with the metal patch method, the method is simple and has good controllability. It is a more excellent preparation method. For example, patent 202310454879.6, this method etches an opening array structure of different sizes on a metal film to form a surface plasma enhanced light transmittance effect for light of a specific wavelength, and at the same time, a quartz film is coated on the second layer to achieve absorption in the infrared response band. The combination and superposition of different materials and different surface micro-nano morphologies will affect the material absorption band and absorption effect, which needs to be continuously explored. III. Summary of the invention
[0005] The purpose of the present invention is to prepare infrared absorbing microwave wave-transmitting frequency selective functional materials in a more convenient way. The method provided is to prepare frequency selective functional materials by directly writing array structures on the surface of composite thin films with femtosecond lasers. This laser direct writing method does not require a mask, a vacuum environment during processing, and no subsequent treatment of the materials after processing. The processing is very convenient and the price is relatively low. By controlling with a computer program, an ideal surface micro-nano structure can be processed, so that the composite film has the function of infrared absorbing microwave wave-transmitting, providing a more efficient option for stealth radar.
[0006] To achieve the above-mentioned purpose, the present invention is implemented by the following technical solutions:
[0007] A method for manufacturing wave-absorbing and wave-transmitting flexible thin film materials by using a maskless femtosecond laser comprises the following steps:
[0008] Step 1: Build a femtosecond laser processing system;
[0009] Step 2: using magnetron sputtering to sequentially plate gold film, silicon dioxide film, and gold film of different thicknesses on a polyimide substrate to form a Pi-Au-SiO2-Au composite film;
[0010] Step 3: Using femtosecond laser direct writing technology, the composite film prepared in step 2 is subjected to pattern etching, and the etching process is controlled by a computer program;
[0011] Step 4: Using femtosecond laser direct writing technology, perform a second patterning process on the composite film prepared in step 3, and control the etching process with a computer program;
[0012] Step 5: Testing the wave absorption and wave transmittance performance of the prepared patterned composite film.
[0013] Furthermore, the thickness of the nanofilm in step 2 is controlled by the coating time, and the thickness ranges from 50 to 200 nm.
[0014] Furthermore, the thickness of the first layer of gold plating from bottom to top in step 2 is 100 nm.
[0015] Furthermore, the thickness of the second layer of silicon dioxide coating from bottom to top in step 2 is 50 nm.
[0016] Furthermore, the thickness of the third layer of gold plating from bottom to top in step 2 is 50 nm.
[0017] Furthermore, in the femtosecond laser patterned etching process described in step three, the etching depth and shape can be controlled by a computer program.
[0018] Furthermore, the pattern prepared by the femtosecond laser direct writing processing technology in step 3 is a square column structure, and the height of the square column is the total depth of the three layers of gold film, silicon dioxide film, and gold film in step 2. The laser energy when processing the square column by the femtosecond laser is 0.05-0.1J / cm 2 , processing speed is 500-1500μm / s, spacing is 0.9-1.0mm;
[0019] Furthermore, in step 4, the second patterning process using femtosecond laser direct writing technology is performed to groove each square column and process it into an array of micro-nano square columns, and the height of the micro-nano square columns is the total depth of the two layers of gold film and silicon dioxide film in step 2. The laser energy when processing the micro-nano square columns by femtosecond laser is 0.01-0.05J / cm 2 , processing speed is 500-1500μm / s, spacing is 0.8-1.2μm;
[0020] Preferably, when the femtosecond laser is used to process the square column array in step 3, the laser energy is 0.06 J / cm 2 ,The processing speed is 800μm / s, the spacing is 1mm, and the groove width is 0.1mm;
[0021] Preferably, when the femtosecond laser is used to process the micro-nano square pillar array in step 4, the laser energy is 0.015 J / cm 2 , the processing speed is 800μm / s, the spacing is 1μm, and the groove width is 0.22μm. IV. Description of the drawings
[0022] Figure 1 This is an example diagram of the femtosecond laser processing system of the present invention
[0023] Figure 2 The flowchart of preparing functional materials according to the embodiment of the present invention; wherein, (a) is a polyimide substrate; (b) is a schematic diagram of the Pi-Au-SiO2-Au composite thin film structure generated by magnetron sputtering of gold plating, silicon dioxide film and gold plating; (c) is a schematic diagram of the first processing process of femtosecond laser direct writing patterning; (d) is a schematic diagram of the second processing process of femtosecond laser direct writing patterning. V. Specific implementation methods
[0024] The present invention will be further described below in conjunction with the accompanying drawings and embodiments.
[0025] Taking a polyimide substrate as an example, the implementation process of a method for manufacturing a wave-absorbing and wave-transmitting flexible thin film material by using a maskless femtosecond laser of the present invention is specifically described below, and the method comprises the following steps:
[0026] (1) Build Figure 1The femtosecond laser processing system shown in the figure is composed of a femtosecond laser 1, an aperture 2, an attenuation plate 3, an optical shutter 4, a dichroic mirror 5, an objective lens 6, a material to be processed 7, a three-dimensional displacement platform 8, a charge coupled device (CCD) 9, and a computer 10. After the femtosecond laser with a wavelength of 1035nm, a pulse width of 130fs, and a repetition frequency of 5000Hz is generated by the femtosecond laser 1, it passes through the aperture 2, the attenuation plate 3, and the optical shutter 4, and is reflected by the dichroic mirror 5 to the objective lens 6. After being focused by the objective lens 6, the femtosecond laser is focused on the surface of the material to be processed 7. The image of the material to be processed 7 is reflected through the dichroic mirror 5 and presented on the charge coupled device (CCD) 9. After being controlled by the computer 10, the image in the charge coupled device (CCD) 9 can be presented on the computer screen. The size of the laser flux can be adjusted by controlling the attenuation plate 3. The optical shutter 4 can be controlled by the computer 10.
[0027] (2) Figure 2 As shown, a gold film, a silicon dioxide film, and a gold film with different nanometer thicknesses are successively plated on a polyimide substrate by magnetron sputtering, thereby preparing a Pi-Au-SiO2-Au composite film; in this embodiment, the thickness of the polyimide substrate is 0.05 mm, the thickness of the first gold coating layer from bottom to top is 100 nm, the thickness of the second silicon dioxide coating layer is 50 nm, and the thickness of the third gold coating layer is 50 nm. Different thicknesses have different effects on the wave absorption and transmission properties of the final product.
[0028] (3) Figure 2 As shown, the prepared composite film is patterned and etched twice using femtosecond laser direct writing technology. The pattern prepared by the first etching is a square column structure. The height of the square column is the total depth of the three layers of gold film, silicon dioxide film, and gold film in step 2; the side length of the square column in this embodiment is 0.9 mm.
[0029] (4) Figure 2 As shown, the second patterning process using femtosecond laser direct writing technology is used to groove each square pillar and process it into an array of micro-nano square pillars. The height of the micro-nano square pillars is the total depth of the two layers of gold film and silicon dioxide film plated in step 2; the side length of the micro-nano square pillars in this embodiment is 0.78μm.
[0030] VI. Implementation Effects of the Invention
[0031] The present invention is a method for manufacturing frequency selective wave absorbing flexible thin film materials by using a maskless femtosecond laser, aiming to prepare a flexible functional material with absorption and transmission in one by a relatively simple method. The processed functional material is characterized in that its absorption rate in the 1.05μm infrared band reaches more than 75%, and its transmittance in the 8-12GHz microwave band reaches more than 80%, which can meet the requirements of infrared stealth radar.
[0032] Compared with the prior art, the present invention has the following beneficial effects:
[0033] 1. The maskless femtosecond laser manufacturing method of the present invention for frequency selective wave absorbing flexible thin film materials does not require the use of a mask, but uses femtosecond laser direct writing to prepare functional materials. The processing method is simpler than the existing method.
[0034] 2. During the processing of the maskless femtosecond laser method for manufacturing a frequency selective wave absorbing flexible thin film material of the present invention, the etching shape and etching depth can be controlled by a computer program to achieve ideal experimental results.
[0035] 3. The multilayer film of the method for manufacturing frequency selective wave absorbing flexible film material by maskless femtosecond laser of the present invention can also control the thickness of each layer of the film by coating time to adjust the optimal parameters.
[0036] 4. The functional material prepared by the maskless femtosecond laser method of the present invention for manufacturing frequency-selective wave-absorbing flexible thin film materials has wave-absorbing properties in the infrared band and wave-transmitting properties in the microwave band, which has a good inspiration for stealth radar.
[0037] 5. The functional material prepared by the maskless femtosecond laser method of the present invention is a flexible film that can adapt to a variety of different usage environment requirements.
Claims
1. A method for manufacturing frequency selective wave absorbing flexible thin film materials by using a maskless femtosecond laser, characterized in that: The following steps are involved: Step 1: Build a femtosecond laser processing system; the femtosecond laser processing system consists of a femtosecond laser, an aperture, an attenuation plate, an optical shutter, a dichroic mirror, an objective lens, a material to be processed, a three-dimensional mobile platform, an electrical coupling element, and a computer. The femtosecond laser with a wavelength of 1035nm, a pulse width of 130fs, and a repetition frequency of 5000Hz is generated by the femtosecond laser, passes through the aperture, the attenuation plate, and the optical shutter, and is reflected by the dichroic mirror to the objective lens. After being focused by the objective lens, the femtosecond laser is focused on the surface of the material to be processed; Step 2: using magnetron sputtering coating method to coat gold film, silicon dioxide film and gold film of different nanometer thickness on the polyimide substrate in turn, so as to prepare Pi-Au-SiO2-Au composite film; Step 3: Using femtosecond laser direct writing technology, laser patterning is performed on the composite thin film material prepared in step 2. The pattern prepared is a square column structure, and the height of the square column is the total depth of the three layers of gold film, silicon dioxide film, and gold film in step 2. The laser energy when processing the square column by femtosecond laser is 0.05-0.1J / cm 2 , processing speed is 500-1500μm / s, spacing is 0.9-1.0mm; Step 4: Use a femtosecond laser to further process the material prepared in step 3, groove each square column, and process it into an array of micro-nano square columns. The height of the micro-nano square column is the total depth of the two layers of gold film and silicon dioxide film in step 2. The laser energy when processing the micro-nano square column by the femtosecond laser is 0.01-0.05J / cm 2 , processing speed is 500-1500μm / s, spacing is 0.8-1.2μm; Step 5: Conduct wave absorption and wave transmittance performance tests on the composite material prepared by femtosecond laser in step 4 to ensure that the absorbance of the prepared functional material in the infrared band and the transmittance in the microwave band meet the expected requirements.
2. The maskless femtosecond laser manufacturing frequency selective wave absorbing flexible thin film material according to claim 1, characterized in that: The thickness of the nano-thickness film in step 2 is controlled by the coating time, and the thickness ranges from 50 to 200 nm.
3. The maskless femtosecond laser manufacturing frequency selective wave absorbing flexible thin film material according to claim 1, characterized in that: The thickness of the first layer of gold plating from bottom to top described in step 2 is 100 nm.
4. The maskless femtosecond laser manufacturing frequency selective wave absorbing flexible thin film material according to claim 1, characterized in that: The thickness of the second layer of silicon dioxide coating from bottom to top described in step 2 is 50nm.
5. The maskless femtosecond laser manufacturing frequency selective wave absorbing flexible thin film material according to claim 1, characterized in that: The thickness of the third layer of gold plating from bottom to top described in step 2 is 50nm.
6. The maskless femtosecond laser manufacturing frequency selective wave absorbing flexible thin film material according to claim 1, characterized in that: When the femtosecond laser is used to process the square column array in step 3, the laser energy is 0.06 J / cm2, the processing speed is 800 μm / s, and the spacing is 1 mm.
7. The maskless femtosecond laser manufacturing frequency selective wave absorbing flexible thin film material according to claim 1, characterized in that: When the femtosecond laser is used to process the micro-nano square pillar array in step 4, the laser energy is 0.015 J / cm2, the processing speed is 800 μm / s, and the spacing is 1 μm.
8. The maskless femtosecond laser manufacturing frequency selective wave absorbing flexible thin film material according to claim 1, characterized in that: The 1.05 μm infrared absorption rate described in step five is required to be above 75%, and the 8-12 GHz microwave transmittance is required to be above 80%.
Citation Information
Patent Citations
X-band absorption and transmission integrated frequency selective surface unit structure and surface structure
CN114421174A
High-energy laser / microwave integrated protective radome with narrow-band light absorption function
CN116505255A
Cited By
Preparation method of metamaterial wave absorber based on PDMS (Polydimethylsiloxane) micro-channel filled with liquid metal
CN120473748A