Method for preparing anti-freezing solution from industrial wastewater generated in preparation of aluminum oxide from fly ash, anti-freezing solution and application of anti-freezing solution
By stirring and mixing the industrial wastewater from fly ash made of alumina with calcium hydroxide aqueous solution, solid-liquid separation and evaporation and concentration, low-cost antifreeze is prepared, which solves the problem of wastewater unutilization and environmental protection, and realizes the wastewater Recycling and utilization and antifreeze to reduce costs and increase efficiency.
Patent Information
- Application Number
- CN202410938176.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-05
AI Technical Summary
In the prior art, the industrial wastewater from fly ash made of alumina has not been fully recycled, and traditional treatment methods make it difficult to recycle salts in the wastewater, affecting environmental protection and cost.
By stirring and mixing the industrial wastewater from fly ash to alumina with calcium hydroxide aqueous solution, adjusting the pH to 6 to 7, solid-liquid separation and evaporation and concentration, a specific content of calcium chloride solution was obtained, and it was used to increase the thickness and corrosion inhibitor and reduce corrosion. Mix the agent to prepare antifreeze.
It realizes effective recycling of wastewater, prepares antifreeze liquid with low freezing point and good antifreeze effect, reduces production costs, solves the environmental protection problems of wastewater in the alumina production process, and reduces the production costs of antifreeze liquid.
Smart Images

Figure BDA0004942065840000091 
Figure BDA0004942065840000092 
Figure BDA0004942065840000101
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of industrial wastewater reuse, and in particular to a method for preparing antifreeze liquid by utilizing fly ash wastewater from an aluminum oxide production industry, the antifreeze liquid and applications thereof. Background Art
[0002] In recent years, with the development of coal resources in western my country and the construction of large-scale thermal power plants, high-aluminum fly ash has gradually attracted attention as a new type of fly ash. 2 O 3 The content is usually up to 50%, which is equivalent to the content of medium-grade bauxite in my country. It is a valuable recycled aluminum-containing mineral resource. Using high-aluminum fly ash to produce alumina can alleviate the plight of bauxite resource shortage in my country, which has great practical significance and long-term strategic significance.
[0003] In order to make better use of the above-mentioned characteristics of fly ash, the prior art has proposed a "one-step acid dissolution method" process, developed a process for extracting alumina from fly ash by acid leaching, and conducted industrial research. However, in addition to alumina, fly ash also contains impurities such as potassium, sodium, iron, calcium and magnesium. During the hydrochloric acid dissolution process, these impurities will also enter the slurry, ultimately affecting the quality of alumina. The prior art CN103803617A proposes a water-soluble aluminum extraction technology, which uses low-temperature roasting and hydrothermal impurity removal coupling technology to replace the calcium removal system and crystalline aluminum chloride washing system in the traditional process, achieving a one-time removal of multiple impurities and significantly reducing investment costs. During the water-soluble aluminum extraction process, impurities will enter the aqueous solution to form fly ash alumina industrial wastewater.
[0004] The above wastewater is a light salt water mainly composed of calcium chloride. The traditional treatment method usually uses sodium hydroxide to neutralize the wastewater, and then concentrates it through ultrafiltration and reverse osmosis filtration, and then evaporates and dries it to obtain salt for storage. Although the above method achieves zero discharge of wastewater, its evaporation concentration is too high, which will cause crystallization and blockage of the evaporator, and the produced salt is difficult to dispose of. Although the traditional method of treating fly ash alumina industrial wastewater reduces the mass of pollutants, it does not achieve the actual recovery and utilization of salts in the wastewater. Summary of the invention
[0005] The main purpose of the present invention is to provide a method for preparing antifreeze liquid using fly ash alumina industrial wastewater, antifreeze liquid and its application, so as to solve the problem that fly ash alumina industrial wastewater is not fully recycled in the prior art.
[0006] In order to achieve the above-mentioned purpose, according to one aspect of the present invention, a method for preparing antifreeze liquid using fly ash aluminum oxide industrial wastewater is provided. The fly ash aluminum oxide industrial wastewater is industrial wastewater obtained by acid dissolving fly ash and then dissolving it in water to extract aluminum. The method comprises the following steps: step S1, first stirring and mixing the fly ash aluminum oxide industrial wastewater with a calcium hydroxide aqueous solution, adjusting the pH to 6-7, and obtaining a mixture; step S2, performing solid-liquid separation on the mixture to obtain a filter cake and a filtrate; step S3, evaporating and concentrating the filtrate to obtain a calcium chloride solution; the weight percentage of the calcium chloride solution is 30-40%; step S4, second stirring and mixing the calcium chloride solution with a thickener and a corrosion inhibitor to obtain an antifreeze liquid.
[0007] Furthermore, in step S1, the weight percentage of the calcium hydroxide aqueous solution is 15-25%, and the temperature is 20-60° C.; and / or the volume ratio of fly ash aluminum oxide industrial wastewater to the calcium hydroxide aqueous solution is 1:(0.5-1); and / or the speed of the first stirring and mixing is 30-60 rpm, and the time is 20-60 min.
[0008] Furthermore, in step S2, the solid-liquid separation time is 20 to 60 minutes; and / or the solid-liquid separation method includes one or more of vacuum filtration, filter pressing and centrifugation; and / or step S2 also includes the step of returning the filter cake to the alumina production batching system.
[0009] Furthermore, in step S3, the temperature of evaporation and concentration is 70-110° C.; and / or the method of evaporation and concentration includes one or more of forced circulation evaporation, natural circulation evaporation, vacuum evaporation and thin film evaporation.
[0010] Furthermore, the weight percentage of the calcium chloride solution is 30-35%.
[0011] Further, in step S4, in the antifreeze solution, the thickener accounts for 0.1-0.5% by weight; and / or the corrosion inhibitor accounts for 0.2-0.6%; preferably, the weight ratio of the calcium chloride solution to the thickener is (150-1000):1; and / or the weight ratio of the calcium chloride solution to the corrosion inhibitor is (170-500):1; more preferably, the weight ratio of the thickener to the corrosion inhibitor is 1:(0.5-2).
[0012] Furthermore, the thickener includes polyacrylamide and / or hydroxypropyl cellulose; and / or the corrosion inhibitor includes one or more of borax, triethanolamine and polyethylene glycol; preferably, the second stirring and mixing has a rotation speed of 20 to 90 rpm and a time of 30 to 120 min.
[0013] Furthermore, the weight percentage of calcium chloride in the fly ash-based alumina industrial wastewater is 2.4-2.87%; preferably, by weight percentage, calcium chloride accounts for 2.4-2.87%, aluminum chloride accounts for 0.34-0.62%, magnesium chloride accounts for 0.18-0.26%, potassium chloride accounts for 0.31-0.51%, and sodium chloride accounts for 0.32-0.45%; and / or the pH value of the fly ash-based alumina industrial wastewater is 5-6.
[0014] According to another aspect of the present invention, an antifreeze liquid is provided, which is obtained according to the above method.
[0015] According to another aspect of the present invention, there is provided the use of the antifreeze liquid in the fields of coal railway transportation and mining.
[0016] By applying the technical scheme of the present invention, the fly ash aluminum oxide industrial wastewater is subjected to acidity adjustment, solid-liquid separation, and evaporation concentration in sequence to obtain a calcium chloride solution with a specific content, which is then used as one of the raw materials to prepare an antifreeze solution. The antifreeze solution obtained by the method of the present invention has a low freezing point, good antifreeze effect, can be directly sprayed, and has low cost. The antifreeze solution of the present invention is used in the fields of coal railway transportation and mining, which can not only effectively solve the environmental protection problem of wastewater in the aluminum oxide production process, but also can prepare a low-cost antifreeze solution for use, which can play a role in reducing costs and increasing efficiency. DETAILED DESCRIPTION
[0017] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present invention will be described in detail below in conjunction with the embodiments.
[0018] As described in the background technology of the present invention, there is a problem in the prior art that fly ash-made alumina industrial wastewater is not fully recycled. In order to solve the above problem, in a typical embodiment of the present invention, a method for preparing antifreeze using fly ash-made alumina industrial wastewater is provided. Fly ash-made alumina industrial wastewater is industrial wastewater obtained by acid dissolving fly ash and then dissolving it in water to extract aluminum. The method includes the following steps: step S1, first stirring and mixing fly ash-made alumina industrial wastewater with calcium hydroxide aqueous solution, adjusting the pH to 6-7, and obtaining a mixture; step S2, performing solid-liquid separation on the mixture to obtain a filter cake and a filtrate; step S3, evaporating and concentrating the filtrate to obtain a calcium chloride solution; the weight percentage of the calcium chloride solution is 30-40%; step S4, second stirring and mixing the calcium chloride solution with a thickener and a corrosion inhibitor to obtain an antifreeze.
[0019] In the preparation method of the present invention, the fly ash aluminum oxide industrial wastewater is first stirred and mixed with the calcium hydroxide aqueous solution, the acidity is adjusted, and the pH is adjusted to 6-7. While effectively increasing the calcium chloride content in the mixture, the trace soluble impurities in the wastewater can also be precipitated through neutralization, such as: aluminum and magnesium ions are formed into hydroxide precipitation, and HCl is neutralized into salt, which is conducive to the formation of a salt solution mainly composed of calcium chloride. It should be noted that in the prior art, calcium oxide is usually used to adjust the pH value of the calcium-rich solution. The inventors especially consider that calcium oxide releases heat violently when dissolving, has high operating risks, and is not easy to dissolve. The present invention particularly selects a calcium hydroxide aqueous solution to effectively increase the calcium chloride content in the mixture and neutralize impurity ions, which is conducive to reducing operating risks and improving the utilization rate of calcium ions.
[0020] Secondly, the mixture is separated into solid and liquid, and the filtrate is evaporated and concentrated, and the weight percentage of the calcium chloride solution is controlled to be 30-40%, so as to control the freezing point of the final antifreeze solution to be below -45°C and effectively reduce the precipitation of calcium chloride crystals. Finally, the calcium chloride solution is stirred and mixed with a thickener and a corrosion inhibitor for a second time to prepare an antifreeze solution, which can turn waste water into treasure and effectively solve the problem that fly ash aluminum oxide industrial wastewater cannot be fully recycled.
[0021] Regarding calcium chloride solution, in the prior art, it can be obtained by adding hydrochloric acid to fly ash and then enriching calcium chloride. However, fly ash itself contains about 3wt% of sulfate substances. In the process of enriching calcium chloride, sulfate substances may be enriched in the evaporator in the form of calcium sulfate, which can easily lead to reduced evaporation efficiency or damage to the evaporator. Compared with the preparation of calcium chloride solution using fly ash as raw material, the fly ash aluminum extraction wastewater of the present invention is decomposed in the early fly ash aluminum extraction-low temperature pyrolysis process, so that the fly ash aluminum extraction wastewater does not contain sulfate, so the efficiency of evaporation and concentration to prepare calcium chloride solution is higher and the probability of evaporator damage is lower. Moreover, there are heavy metal oxides such as lead, mercury, cadmium, and zinc in the fly ash itself, and hydrochloric acid will also dissolve some heavy metal oxides in the process of dissolving fly ash. If there is no corresponding heavy metal removal process, it may cause the heavy metals in the subsequent prepared calcium chloride solution to exceed the standard. The fly ash aluminum extraction wastewater of the present invention, because the early aluminum extraction process has removed heavy metal ions such as iron, the obtained calcium chloride solution does not contain heavy metal pollutants and can be used for high value.
[0022] Compared with commercially available crystallized calcium chloride, the antifreeze prepared by the present invention using fly ash aluminum extraction wastewater as raw material contains a small amount of potassium chloride and sodium chloride, has a low freezing point at the same calcium chloride concentration, has a good antifreeze effect, and can be directly sprayed. In addition, the price of crystallized calcium chloride, the raw material required for commercial antifreeze, is relatively high (900 to 1000 yuan / ton), resulting in a relatively high cost of the antifreeze product (about 400 yuan / ton). The raw materials of the calcium chloride solution of the present invention are fly ash aluminum oxide industrial wastewater and calcium hydroxide aqueous solution, and there is no need to expand equipment on the existing basis, so that the composition of the calcium chloride solution is greatly reduced. On the basis of the calcium chloride solution of the present invention, additives (thickener, corrosion inhibitor) can be added to obtain the antifreeze product, so the cost of the antifreeze product is relatively low (about 150 yuan / ton).
[0023] In summary, the technical scheme of the present invention is applied to the fly ash alumina industrial wastewater, and the acidity is adjusted, the solid-liquid separation is carried out, and the evaporation concentration is carried out in sequence to obtain a calcium chloride solution, which is then used as one of the raw materials to prepare an antifreeze solution. The antifreeze solution of the present invention contains a small amount of potassium chloride and sodium chloride, and has a low freezing point at the same calcium chloride content, a good antifreeze effect, can be directly sprayed, and has low cost. The method of the present invention can not only effectively solve the environmental protection problem of wastewater in the alumina production process, but also can prepare a low-cost antifreeze solution, which plays a role in reducing costs and increasing efficiency.
[0024] In order to make the calcium hydroxide aqueous solution contact and react with the fly ash alumina industrial wastewater more fully and effectively, and at the same time be more conducive to increasing the calcium chloride content in the mixture to form a salt solution mainly composed of calcium chloride, in a preferred embodiment, in step S1, the weight percentage of the calcium hydroxide aqueous solution is 15-25%, and the temperature is 20-60°C; and / or the volume ratio of the fly ash alumina industrial wastewater to the calcium hydroxide aqueous solution is 1:(0.5-1), preferably 1:(0.5-0.75); and / or the rotation speed of the first stirring and mixing is 30-60rpm, preferably 30-50rpm, and the mixing time is 20-60min.
[0025] In order to separate the solid and liquid more fully, thereby further reducing the impurities in the antifreeze solution, in a preferred embodiment, in step S2, the solid-liquid separation time is 20 to 60 minutes; and / or the solid-liquid separation method is one or more of vacuum filtration, filter pressing and centrifugation. In a preferred embodiment, step S2 also includes the step of returning the filter cake to the alumina production batching system to further recycle the aluminum element in the wastewater.
[0026] In a preferred embodiment, in step S3, the temperature of evaporation and concentration is 70-110° C.; and / or the evaporation and concentration method is one or more of forced circulation evaporation, natural circulation evaporation, vacuum evaporation and thin film evaporation. Under the above conditions, the evaporation and concentration efficiency is higher, the energy consumption is less, and the concentration of the calcium chloride solution can be controlled more quickly and effectively.
[0027] In order to more conveniently control the freezing point of the prepared antifreeze solution below -45°C, in a preferred embodiment, the weight percentage of the calcium chloride solution is 30-35%. Within this range, calcium chloride crystals are less likely to precipitate.
[0028] In order to make the antifreeze liquid meet the viscosity and anti-corrosion requirements of TB / T3208-2008 "Antifreeze liquid for bulk particle transportation", in a preferred embodiment, by weight percentage, the thickener accounts for 0.1-0.5%; and / or the corrosion inhibitor accounts for 0.2-0.6%. If the thickener content is too much, it may cause the antifreeze liquid to be difficult to spray, and the wettability to the treated material is poor, making the antifreeze area incomplete. If the thickener content is too little, it is easy to cause the antifreeze liquid to have poor adhesion to the treated material, and the antifreeze effect needs to be improved. If the amount of corrosion inhibitor added is too much, it will lead to high costs. If the amount added is too little, the corrosion inhibition effect is not good.
[0029] For the purpose of making the antifreeze liquid lower in cost and more suitable in viscosity, in a preferred embodiment, the weight ratio of the calcium chloride solution to the thickener is (150-1000):1; and / or the weight ratio of the calcium chloride solution to the corrosion inhibitor is (170-500):1; more preferably, the weight ratio of the thickener to the corrosion inhibitor is 1:(0.5-2), and further preferably 1:(1-2). The antifreeze liquid under the above conditions can better meet the viscosity and corrosion protection requirements of TB / T3208-2008 "Antifreeze liquid for transport of bulk particles", can more effectively improve the stability and lubricity of the antifreeze liquid in actual use, reduce the wear and corrosion of the cooling system, further ensure the effectiveness of the antifreeze liquid in a low temperature environment and the safety of the cooling system, and is more convenient for practical application.
[0030] The thickener and corrosion inhibitor of the present invention can be of the commonly used types in the technical field. In order to make the thickener and corrosion inhibitor more compatible with the calcium chloride solution obtained from fly ash aluminum oxide industrial wastewater as raw materials, the inventor has optimized the types of thickener and sustained-release agent after a large number of experiments. In a preferred embodiment, the thickener includes polyacrylamide and / or hydroxypropyl cellulose; the corrosion inhibitor includes one or more of borax, triethanolamine and polyethylene glycol. Preferably, the second stirring and mixing speed is 20 to 90 rpm, and the time is 30 to 120 min, and more preferably the second stirring and mixing speed is 60 to 90 rpm, and the time is 30 to 60 min. Under the above conditions, the antifreeze has better comprehensive performance and is more convenient for practical application.
[0031] In a preferred embodiment, the weight percentage of calcium chloride in fly ash alumina industrial wastewater is 2.4-2.87%; preferably, by weight percentage, calcium chloride accounts for 2.4-2.87%, aluminum chloride accounts for 0.34-0.62%, magnesium chloride accounts for 0.18-0.26%, potassium chloride accounts for 0.31-0.51%, sodium chloride accounts for 0.32-0.45%, and the pH value is 5-6. Under the above conditions, it is more conducive to preparing a calcium chloride solution with a specific weight percentage, and it is more conducive to lowering the freezing point of the antifreeze.
[0032] In another typical embodiment of the present invention, an antifreeze solution is provided, which is obtained according to the above method. The antifreeze solution of the present invention uses fly ash aluminum oxide industrial wastewater as raw material, has low cost, and, because it contains a small amount of potassium chloride and sodium chloride, has a lower freezing point at the same calcium chloride concentration, has a good antifreeze effect, and can be directly sprayed.
[0033] In another typical embodiment of the present invention, the application of the above antifreeze in the field of coal railway transportation and mining is also provided. By comparing the chemical composition of fly ash aluminum oxide industrial wastewater with the existing coal railway transportation antifreeze and mining antifreeze, the inventor unexpectedly found that the chemical composition is similar and the performance is equivalent, which is conducive to solving the environmental protection problem of wastewater in the aluminum oxide production process. On the other hand, it can also provide low-cost antifreeze for the coal railway transportation and mining fields, which plays a role in reducing costs and increasing efficiency.
[0034] Typically, but not limited to, the pH of the mixture is adjusted to a value between 6, 6.5, 7, or any two thereof.
[0035] Typically but not limiting, the weight percentage of the calcium chloride solution is 30%, 31%, 32%, 33%, 34%, 35%, 40% or a range value composed of any two of them.
[0036] Typically but non-limitingly, the weight percentage of the calcium hydroxide aqueous solution is 15%, 20%, 25% or the range value composed of any two of them, and the temperature is 20°C, 25°C, 30°C, 35°C, 40°C, 45°C, 50°C, 55°C, 60°C or the range value composed of any two of them.
[0037] Typically but not limiting, the volume ratio of fly ash alumina industrial wastewater to calcium hydroxide aqueous solution is 1:0.5, 1:0.6, 1:0.7, 1:0.75, 1:0.8, 1:0.9, 1:1 or a range consisting of any two of them.
[0038] Typically, but not limitedly, the temperature of evaporation concentration is 70°C, 90°C, 110°C or a range consisting of any two of them.
[0039] Typically but not limiting, the thickener accounts for 0.1%, 0.2%, 0.3%, 0.4%, 0.5% or a range consisting of any two of them, the corrosion inhibitor accounts for 0.2%, 0.3%, 0.4%, 0.5%, 0.6% or a range consisting of any two of them, and the weight ratio of the thickener to the corrosion inhibitor is 1:0.5, 1:0.6, 1:0.7, 1:0.8, 1:0.9, 1:1, 1:1.5, 1:2 or a range consisting of any two of them.
[0040] Typically, but not limiting, the pH value of fly ash alumina industrial wastewater is 5, 5.5, 6 or a range consisting of any two of them.
[0041] The present application is further described in detail below in conjunction with specific embodiments. These embodiments should not be construed as limiting the scope of protection claimed in the present application.
[0042] Example 1
[0043] The specific composition of fly ash alumina industrial wastewater is shown in Table 1.
[0044] Step S1, at room temperature (25° C.), the wastewater and a calcium hydroxide aqueous solution with a weight percentage of 20% and a temperature of 30° C. are first stirred and mixed at 30 rpm for 30 minutes, and the pH is adjusted to 6.5 to obtain a mixture; wherein the volume ratio of fly ash aluminum oxide industrial wastewater to the calcium hydroxide aqueous solution is 1:0.5;
[0045] Step S2, using a plate and frame filter press to filter the mixture for 30 minutes to obtain a filter cake and a filtrate, wherein the filter cake is mainly aluminum hydroxide precipitate, which is returned to the alumina production batching system for use. The specific composition of the filter cake is shown in Table 2;
[0046] Step S3, using a triple-effect forced circulation evaporator, under the conditions of 40 min and 100° C., evaporating and concentrating the filtrate to obtain a calcium chloride solution and condensed water; the evaporation and concentration temperature is controlled to be 90° C., and the weight percentage of the calcium chloride solution is 30%; the specific composition of the calcium chloride solution is shown in Table 3;
[0047] Step S4, the calcium chloride solution, the thickener (polyacrylamide), and the corrosion inhibitor (boric acid) are stirred and mixed for a second time at 60 rpm for 90 minutes to prepare an antifreeze solution for railway transportation of coal, wherein the thickener accounts for 0.2% by weight of the antifreeze solution, and the corrosion inhibitor accounts for 0.3% by weight.
[0048] Example 2
[0049] The specific composition of fly ash alumina industrial wastewater is shown in Table 1.
[0050] Step S1, at room temperature (25° C.), the wastewater and a calcium hydroxide aqueous solution with a weight percentage of 20% and a temperature of 50° C. are first stirred and mixed at 40 rpm for 30 minutes, and the pH is adjusted to 7 to obtain a mixture; wherein the volume ratio of fly ash aluminum oxide industrial wastewater to the calcium hydroxide aqueous solution is 1:0.6;
[0051] Step S2, using a plate and frame filter press to filter the mixture for 30 minutes to obtain a filter cake and a filtrate, wherein the filter cake is mainly aluminum hydroxide precipitate, which is returned to the alumina production batching system for use. The specific composition of the filter cake is shown in Table 2;
[0052] Step S3, using a triple-effect forced circulation evaporator, under the conditions of 1h and 90°C, evaporating and concentrating the filtrate to obtain a calcium chloride solution and condensed water; the evaporation and concentration temperature is controlled to be 90°C, and the weight percentage of the calcium chloride solution is 35%; the specific composition of the calcium chloride solution is shown in Table 3;
[0053] Step S4, the calcium chloride solution, the thickener (polyacrylamide), and the corrosion inhibitor (boric acid) are stirred and mixed for a second time at 90 rpm for 30 minutes to prepare an antifreeze solution for railway transportation of coal, wherein the thickener accounts for 0.3% by weight of the antifreeze solution, and the corrosion inhibitor accounts for 0.4% by weight.
[0054] Example 3
[0055] The specific composition of fly ash alumina industrial wastewater is shown in Table 1.
[0056] Step S1, at 40° C., the wastewater and a calcium hydroxide aqueous solution with a weight percentage of 15% and a temperature of 20° C. are first stirred and mixed at 50 rpm for 20 minutes, and the pH is adjusted to 6 to obtain a mixture; wherein the volume ratio of fly ash aluminum oxide industrial wastewater to the calcium hydroxide aqueous solution is 1:0.75;
[0057] Step S2, using a plate and frame filter press to filter the mixture for 40 minutes to obtain a filter cake and a filtrate, wherein the filter cake is mainly aluminum hydroxide precipitate, which is returned to the alumina production batching system for use. The specific composition of the filter cake is shown in Table 2;
[0058] Step S3, subjecting the filtrate to natural circulation evaporation to obtain a calcium chloride solution and condensed water; the evaporation and concentration temperature is controlled to be 70° C., and the weight percentage of the calcium chloride solution is 30%; the specific composition of the calcium chloride solution is shown in Table 3;
[0059] Step S4, the calcium chloride solution, the thickener (polyacrylamide), and the corrosion inhibitor (boric acid) are stirred and mixed for a second time at 20 rpm for 120 minutes to prepare an antifreeze solution for use in mining, wherein the thickener accounts for 0.1% by weight of the antifreeze solution, and the corrosion inhibitor accounts for 0.2% by weight.
[0060] Example 4
[0061] The specific composition of fly ash alumina industrial wastewater is shown in Table 1.
[0062] Step S1, at 30° C., the wastewater and a calcium hydroxide aqueous solution with a weight percentage of 25% and a temperature of 60° C. are first stirred and mixed at 60 rpm for 60 minutes, and the pH is adjusted to 7 to obtain a mixture; wherein the volume ratio of the fly ash aluminum oxide industrial wastewater to the calcium hydroxide aqueous solution is 1:1;
[0063] Step S2, vacuum filtering the mixture for 2 hours to obtain a filter cake and a filtrate, wherein the filter cake is mainly aluminum hydroxide precipitate, the specific composition of which is shown in Table 2, and the filter cake is returned to the alumina production batching system for use;
[0064] Step S3, vacuum evaporating the filtrate at 80° C. for 2.5 h to obtain a calcium chloride solution and condensed water; the evaporation and concentration temperature is controlled to be 110° C., and the weight percentage of the calcium chloride solution is 35%; the specific composition of the calcium chloride solution is shown in Table 3;
[0065] Step S4, the calcium chloride solution, the thickener (polyacrylamide), and the corrosion inhibitor (boric acid) are stirred and mixed for a second time at 45 rpm for 90 minutes to prepare an antifreeze solution for use in mining, wherein the thickener accounts for 0.5% by weight of the antifreeze solution, and the corrosion inhibitor accounts for 0.6% by weight.
[0066] Example 5
[0067] The only difference from Example 1 is:
[0068] In the antifreeze liquid, the weight percentage of thickener (hydroxypropyl cellulose) in the antifreeze liquid is 0.3%, and the weight percentage of corrosion inhibitor (triethanolamine) in the antifreeze liquid is 0.2%.
[0069] Example 6
[0070] The only difference from Example 1 is:
[0071] In the antifreeze liquid, the weight percentage of thickener (hydroxypropyl cellulose) in the antifreeze liquid is 0.4%, and the weight percentage of corrosion inhibitor (triethanolamine) in the antifreeze liquid is 0.3%.
[0072] Example 7
[0073] The only difference from Example 1 is:
[0074] In the antifreeze liquid, the weight percentage of thickener (hydroxypropyl cellulose) is 0.6%, and the weight percentage of corrosion inhibitor (polyethylene glycol) is 0.3%.
[0075] Example 8
[0076] The only difference from Example 1 is:
[0077] In the antifreeze liquid, the weight percentage of thickener (hydroxypropyl cellulose) in the antifreeze liquid is 0.3%, and the weight percentage of corrosion inhibitor (polyethylene glycol) in the antifreeze liquid is 0.3%.
[0078] Comparative Example 1
[0079] The fly ash alumina industrial wastewater is replaced by fly ash hydrochloric acid solution.
[0080] Comparative Example 2
[0081] The existing antifreeze product CN102146279A has the following main ingredients.
[0082] Element Weight percentage (%) Calcium chloride 28~32 Benzotriazole 0.05~0.3 Triple B 0.5~4 Sodium Nitrite 0.5~3 Sodium acetate 0.5~3 EDTA 0.1~1.7 water 60~66.35
[0083] The performance test results of the antifreeze solutions prepared in the above examples and comparative examples are shown in Table 4.
[0084] Test method:
[0085] Freezing point, boiling point, flash point, density, viscosity, pH value: Test: Refer to TB / T 3208-2008 for testing.
[0086] Metal corrosion test: refer to JB / T 7901-1999 for testing.
[0087] Heavy metal content test: refer to GB / T 7475-1987 for testing.
[0088] Impact test on rubber used in railway vehicles: Test with reference to GB / T 1960-2006.
[0089] Impact test on alkyd paint for railway freight cars: refer to SH / T 0084-2001 for testing.
[0090] Table 1
[0091]
[0092] Table 2
[0093]
[0094] Table 3
[0095]
[0096] Table 4
[0097]
[0098]
[0099] In comparative example 1, the antifreeze solution was prepared by using the hydrochloric acid solution of fly ash, and the antifreeze product was unqualified due to the interference of heavy metal impurities. In the antifreeze solution of comparative example 2, the additive formula would cause the cost of the antifreeze solution to increase significantly.
[0100] As can be seen from the above, compared with the comparative example, the wastewater of the present invention based on the "one-step acid dissolution method" for extracting aluminum oxide and water-soluble impurities does not contain heavy metal impurities, and the wastewater from the specific source is sequentially subjected to solid-liquid separation and evaporation concentration to obtain a calcium chloride solution of a specific concentration, which is then used as one of the raw materials to prepare antifreeze. The obtained antifreeze has a low freezing point, good antifreeze effect, can be directly sprayed, and has the advantage of low cost. It can not only effectively solve the environmental protection problem of wastewater in the production process of aluminum oxide, but also can prepare low-cost antifreeze for application, which can play a role in reducing costs and increasing efficiency, and has strong industry competitiveness.
[0101] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for preparing antifreeze solution using fly ash alumina industrial wastewater, characterized in that: The fly ash alumina production industrial wastewater is industrial wastewater obtained by subjecting fly ash to acid dissolution and then water dissolution for aluminum extraction. The method comprises the following steps: Step S1, first stirring and mixing the fly ash aluminum oxide industrial wastewater and the calcium hydroxide aqueous solution, adjusting the pH to 6-7, to obtain a mixture; Step S2, separating the mixture into solid and liquid to obtain a filter cake and a filtrate; Step S3, evaporating and concentrating the filtrate to obtain a calcium chloride solution; the weight percentage of the calcium chloride solution is 30-40%; Step S4, performing a second stirring mixing on the calcium chloride solution, the thickener and the corrosion inhibitor to obtain the antifreeze solution.
2. The method according to claim 1, characterized in that In the step S1, The calcium hydroxide aqueous solution has a weight percentage of 15-25% and a temperature of 20-60° C.; and / or The volume ratio of the fly ash aluminum oxide industrial wastewater to the calcium hydroxide aqueous solution is 1:(0.5-1); and / or The first stirring and mixing is performed at a rotation speed of 30 to 60 rpm and a time of 20 to 60 min.
3. The method according to claim 1 or 2, characterized in that: In the step S2, The solid-liquid separation time is 20 to 60 minutes; and / or The solid-liquid separation method includes one or more of vacuum filtration, filter pressing and centrifugation; and / or The step S2 also includes the step of returning the filter cake to the alumina production batching system.
4. The method according to any one of claims 1 to 3, characterized in that In step S3, the evaporation concentration temperature is 70-110° C.; and / or The evaporation and concentration method includes one or more of forced circulation evaporation, natural circulation evaporation, vacuum evaporation and thin film evaporation.
5. The method according to any one of claims 1 to 4, characterized in that The weight percentage of the calcium chloride solution is 30-35%.
6. The method according to any one of claims 1 to 5, characterized in that In step S4, the antifreeze solution contains, by weight percentage, The thickener accounts for 0.1-0.5%; and / or The corrosion inhibitor accounts for 0.2-0.6%; Preferably, the weight ratio of the calcium chloride solution to the thickener is (150-1000):1; and / or The weight ratio of the calcium chloride solution to the corrosion inhibitor is (170-500):1; More preferably, the weight ratio of the thickener to the corrosion inhibitor is 1:(0.5-2).
7. The method according to any one of claims 1 to 6, characterized in that The thickener comprises polyacrylamide and / or hydroxypropyl cellulose; and / or The corrosion inhibitor includes one or more of borax, triethanolamine and polyethylene glycol; Preferably, the second stirring and mixing has a rotation speed of 20 to 90 rpm and a time of 30 to 120 min.
8. The method according to any one of claims 1 to 7, characterized in that The weight percentage of calcium chloride in the fly ash alumina industrial wastewater is 2.4-2.87%; Preferably, in the fly ash alumina industrial wastewater, by weight percentage, calcium chloride accounts for 2.4-2.87%, aluminum chloride accounts for 0.34-0.62%, magnesium chloride accounts for 0.18-0.26%, potassium chloride accounts for 0.31-0.51%, and sodium chloride accounts for 0.32-0.45%; and / or The pH value of the fly ash-based alumina industrial wastewater is 5-6.
9. An antifreeze solution, characterized in that: Obtained according to the method according to any one of claims 1 to 8.
10. Use of the antifreeze liquid according to claim 9 in the fields of coal railway transportation and mining.