Flexible 2T0C-DRAM and preparation method thereof
By using methods such as ultraviolet lithography, physical vapor deposition, and vacuum thermal evaporation on flexible substrates to fabricate flexible 2T0C-DRAM, the problems of fabrication complexity and high cost have been solved, realizing the fabrication and bendability of flexible memory, and meeting the needs of wearable devices.
Patent Information
- Application Number
- CN202410974688.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-19
- Publication Date
- 2024-11-05
AI Technical Summary
The existing 2T0C-DRAM manufacturing process is complex, resulting in high production costs and the inability to manufacture flexible memory, which cannot meet the storage needs of wearable devices.
Flexible 2TOC-DRAM is fabricated on a flexible substrate using methods such as ultraviolet lithography, physical vapor deposition, atomic layer deposition, and vacuum thermal evaporation. Flexible and bendable transistor channels are formed by growing metal layers, depositing dielectric layers, forming interconnect vias, and depositing organic materials on the flexible substrate.
This reduced production costs and enabled the fabrication of flexible 2T0C-DRAM, which boasts excellent storage performance and bendability, meeting the storage needs of wearable devices.
Smart Images

Figure CN118900560A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of organic memory, and in particular to a flexible 2TOC-DRAM and a preparation method thereof. Background Art
[0002] At present, with the rapid development of science and technology, data storage technology has become an indispensable part of modern society. Dynamic Random Access Memory (DRAM) is the mainstream method of data storage at present, and plays a vital role in many fields such as medical equipment, smart phones, computers, etc. DRAM storage cells are made of a single transistor and a single capacitor, that is, the 1T1C (1Transistor1Capacitor)-DRAM architecture design. This storage cell turns on the transistor when writing, and the charge is pushed into the capacitor (i.e., high voltage, recorded as state 1) or removed from the capacitor (i.e., low voltage, recorded as state 0). The capacitor charging and discharging process in the working principle of traditional DRAM not only limits the storage speed, but also leads to an increase in power consumption. Moreover, as the memory moves towards high capacity and high density, the number of capacitors increases sharply, and the device size decreases significantly. These changes not only make the process very complicated, but also increase the risk of leakage. Therefore, traditional DRAM faces technical bottlenecks in the pursuit of higher storage speed and lower power consumption.
[0003] In order to overcome these limitations of traditional DRAM, researchers have proposed a new storage structure in recent years - 2T0C-DRAM. 2T0C-DRAM uses two transistors to form a storage unit, one of which replaces the capacitor in traditional DRAM, thus solving the problem of capacitor charging and discharging. This new structure not only improves storage speed, but also reduces power consumption, opening up a new path for the development of data storage technology.
[0004] However, the preparation process of 2T0C-DRAM is too complicated, resulting in high production costs, and traditional processes cannot produce flexible 2T0C-DRAM, resulting in the inability of existing 2T0C-DRAM to meet the storage needs of wearable devices, limiting the development of the flexible electronics field.
[0005] Therefore, there is an urgent need for a flexible 2T0C-DRAM and a method for preparing the same. Summary of the invention
[0006] The object of the present invention is to provide a flexible 2T0C-DRAM and a preparation method thereof, reduce the production cost of 2T0C-DRAM, and realize the preparation of flexible 2T0C-DRAM.
[0007] In a first aspect, the present invention provides a method for preparing a flexible 2TOC-DRAM, comprising:
[0008] providing a flexible substrate;
[0009] Growing a first metal layer on the substrate by ultraviolet lithography and physical vapor deposition to serve as a gate of a single transistor of the memory;
[0010] depositing a dielectric layer on the first metal layer by atomic layer deposition;
[0011] forming a connecting through hole by dry etching;
[0012] growing a second metal layer by ultraviolet lithography and physical vapor deposition to serve as source and drain electrodes of a single transistor of the memory;
[0013] The organic material is deposited on the second metal layer by vacuum thermal evaporation to form a flexible and bendable transistor channel to obtain a flexible 2T0C-DRAM.
[0014] The method of the present invention has the following beneficial effects: a first metal layer is grown on a flexible substrate by ultraviolet lithography and physical vapor deposition to serve as a gate of a single transistor of a memory; a dielectric layer is deposited on the first metal layer by atomic layer deposition; a connecting through hole is formed by dry etching; a second metal layer is grown by ultraviolet lithography and physical vapor deposition to serve as a source-drain electrode of a single transistor of the memory; an organic material is deposited on the second metal layer by vacuum thermal evaporation to form a flexible and bendable transistor channel to obtain a flexible 2T0C-DRAM, and a laminated structure is manufactured by ultraviolet lithography, physical vapor deposition, atomic layer deposition and vacuum thermal evaporation, which is easy to prepare and reduces production costs, and a flexible and bendable memory unit transistor channel is realized by organic vapor deposition of organic materials, so that the prepared 2T0C-DRAM has excellent storage performance while having excellent flexibility and bendability, thereby meeting the storage requirements of wearable devices.
[0015] Optionally, an organic material is deposited on the second metal layer by vacuum thermal evaporation to form a flexible and bendable transistor channel, and the flexible 2T0C-DRAM includes:
[0016] The entire device was immersed in a 0.5 mg / L perfluorobutyl mercaptan solution for 20 min to form a monolayer;
[0017] The hard mask alignment mark mask protects the device, and the vacuum thermal evaporation deposits the organic material as the channel of the transistor to obtain a flexible 2T0C-DRAM.
[0018] Optionally, the organic material is C8-BTBT. When depositing the organic material C8-BTBT as a channel of a transistor, the temperature is 160 degrees Celsius, the deposition rate is 3 nm / min, and the thickness of the deposited channel is 50 nm.
[0019] Optionally, a first metal layer is grown on the substrate by ultraviolet lithography and physical vapor deposition, and the gate of a single transistor of the memory includes:
[0020] The flexible substrate is protected by an ultraviolet lithography alignment mark reticle, and a first metal layer is grown by physical vapor deposition as a gate of a single transistor, wherein the first metal layer is a Ti / Pt stack, and the thickness of the Ti layer is 10nm, and the thickness of the Pt layer is 70nm.
[0021] Optionally, a second metal layer is grown by ultraviolet lithography and physical vapor deposition, and the second metal layer is used as a source and drain electrode of a single transistor of the memory, including:
[0022] The source and drain regions of a single transistor are defined by alignment marks through ultraviolet photolithography, and a second metal layer is grown by physical vapor deposition to serve as the source and drain electrodes of the single transistor, wherein the second metal layer is a Ti / Au stack.
[0023] Optionally, before growing the first metal layer on the substrate, the method further includes:
[0024] Coating an adhesion layer and a photoresist on the upper surface of the substrate respectively;
[0025] After growing the first metal layer on the substrate, the method further comprises:
[0026] Remove the photoresist.
[0027] Optionally, forming the connecting through hole by dry etching includes:
[0028] Alignment marks were made by UV photolithography and through holes were dry etched.
[0029] In a second aspect, the present invention further provides a flexible 2T0C-DRAM, which is prepared by the method for preparing the flexible 2T0C-DRAM in any possible combination of the first aspect above, wherein the flexible 2T0C-DRAM includes a flexible substrate and a gate, a dielectric layer and a source-drain electrode formed in sequence from bottom to top on the flexible substrate; the source-drain electrode forms a flexible and bendable transistor channel.
[0030] Optionally, the dielectric layer is Al2O3 with a thickness of 15 nm; and / or the gate is a Ti / Pt stack, wherein the thickness of the Ti layer is 10 nm and the thickness of the Pt layer is 70 nm.
[0031] Optionally, the source and drain electrodes are Ti / Au stacks; and / or the material of the channel is C8-BTBT with a thickness of 50 nm.
[0032] The beneficial effect of the flexible 2T0C-DRAM of the present invention is that: by using the gate as a Ti / Pt stack, the source and drain electrodes as a Ti / Au stack, and the material of the channel as C8-BTBT with a thickness of 50nm, a smaller storage unit can be achieved, a higher storage density can be obtained, and the flexible 2T0C-DRAM can have excellent storage performance while having excellent flexibility and bendability. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 A schematic diagram of a process for preparing a flexible 2T0C-DRAM provided in an embodiment of the present invention;
[0034] Figure 2 A schematic structural diagram of a substrate and a first metal layer provided in an embodiment of the present invention;
[0035] Figure 3 A schematic diagram of the structure of a first metal layer and a dielectric layer provided in an embodiment of the present invention;
[0036] Figure 4 A schematic diagram of the structure of the first metal layer and Al2O3 provided in an embodiment of the present invention;
[0037] Figure 5 A schematic diagram of the structure of Al2O3 and a through hole provided in an embodiment of the present invention;
[0038] Figure 6 A schematic diagram of the structure of a PFBT monolayer provided in an embodiment of the present invention;
[0039] Figure 7 A schematic diagram of a flexible 2T0C-DRAM structure after depositing an organic material C8-BTBT as a channel provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0040] In order to make the purpose, technical solutions and advantages of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Unless otherwise defined, the technical terms or scientific terms used herein should be understood by people with general skills in the field to which the present invention belongs. "Including" and similar words used in this article mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects.
[0041] like Figure 1 As shown, the present invention provides a method for preparing a flexible 2T0C-DRAM, comprising:
[0042] S101, providing a flexible substrate. Exemplarily, the flexible substrate may be MICA (mica).
[0043] In some embodiments, before growing the first metal layer on the substrate, the method further includes: coating an adhesion layer and a photoresist on the upper surface of the substrate respectively; and after growing the first metal layer on the substrate, the method further includes: removing the photoresist. The adhesion layer and the photoresist are preferably coated by spin coating (i.e., coating is performed while the substrate is rotating) to improve the uniformity of coating the adhesion layer and the photoresist.
[0044] S102 , growing a first metal layer on the substrate by ultraviolet lithography and physical vapor deposition to serve as a gate of a single transistor of the memory.
[0045] In some embodiments, a first metal layer is grown on the substrate by ultraviolet lithography and physical vapor deposition as a gate of a single transistor of the memory, including: protecting the flexible substrate by ultraviolet lithography alignment mark reticle, and growing the first metal layer by physical vapor deposition as a gate of a single transistor, wherein the first metal layer is a Ti / Pt stack, and the thickness of the Ti layer is 10nm, and the thickness of the Pt layer is 70nm. Ultraviolet lithography, with its high precision and high resolution, can accurately depict the microstructure of the device, while physical vapor deposition can deposit materials layer by layer on the substrate through a physical process in a vacuum environment to form a desired structure. The combination of the two can simply and effectively prepare the stack and improve production efficiency.
[0046] S103, depositing a dielectric layer on the first metal layer by atomic layer deposition. Exemplarily, the dielectric layer is preferably Al2O3, and PMMA (polymethyl methacrylate) can be deposited on the first metal layer first, and then the dielectric layer is deposited on PMMA. High-k (high dielectric constant) material Al2O3 is preferred, which has the characteristics of high dielectric constant and low leakage rate, and can effectively prevent transistor leakage, thereby improving the reliability and stability of the device. At the same time, Al2O3 also has excellent thermal stability and chemical stability, and can maintain stable performance under various environments, and the use of atomic layer deposition can make the growth process of the dielectric film more accurate and controllable. By accurately controlling the deposition thickness and growth rate of each layer, a highly conformal and high-quality dielectric film can be obtained. This film not only has excellent insulation properties, but also can effectively prevent the leakage and diffusion of charge, thereby improving the performance and life of the flexible 2TOC-DRAM prepared by the present invention.
[0047] S104, forming a connecting through hole by dry etching.
[0048] In some embodiments, forming the connecting vias by dry etching includes: aligning marks by ultraviolet photolithography and dry etching the vias.
[0049] S105, growing a second metal layer by ultraviolet lithography and physical vapor deposition as the source and drain electrodes of a single transistor of the memory. Again using ultraviolet lithography and physical vapor deposition, the two are combined with each other, which is not only simple to operate and easy to control, but can also accurately depict various parts of the memory, and can also ensure that the prepared flexible 2T0C-DRAM memory has excellent performance and stability by optimizing process parameters and operation procedures.
[0050] In some embodiments, growing a second metal layer by ultraviolet lithography and physical vapor deposition to serve as the source and drain electrodes of a single transistor of the memory includes: aligning marks by ultraviolet lithography to define the source and drain regions of a single transistor, and growing a second metal layer by physical vapor deposition to serve as the source and drain electrodes of a single transistor, wherein the second metal layer is a Ti / Au stack.
[0051] S106, depositing an organic material on the second metal layer by vacuum thermal evaporation to form a flexible and bendable transistor channel, thereby obtaining a flexible 2T0C-DRAM.
[0052] In some embodiments, an organic material is deposited on the second metal layer by vacuum thermal evaporation to form a flexible and bendable transistor channel, and obtaining a flexible 2T0C-DRAM includes: immersing the entire device in a 0.5 mg / L perfluorobutyl mercaptan solution for 20 minutes to form a monolayer; a hard mask alignment mark mask protects the device, and vacuum thermal evaporation deposits an organic material as a transistor channel to obtain a flexible 2T0C-DRAM.
[0053] In some specific embodiments, the organic material is C8-BTBT. When depositing the organic material C8-BTBT as a channel of a transistor, the temperature is 160 degrees Celsius, the deposition rate is 3 nm / min, and the thickness of the deposited channel is 50 nm.
[0054] The advantages of the embodiments of the present invention are that the laminated structure is made by ultraviolet lithography, physical vapor deposition, atomic layer deposition and vacuum thermal evaporation, which is easy to prepare and reduces the production cost. Moreover, the flexible and bendable storage unit transistor channel is realized by depositing organic materials by organic evaporation, and the preparation of flexible 2T0C-DRAM memory is realized. The memory not only has excellent storage performance, but also has excellent flexibility and bendability, which meets the storage needs of wearable devices. As an important development direction of modern science and technology, wearable devices have higher and higher requirements for memory. Traditional rigid memory is difficult to meet its use requirements in complex scenes such as bending and folding. The flexible 2T0C-DRAM of the present invention just solves this problem, and provides a stable and reliable storage solution for wearable devices, and has good storage performance.
[0055] For ease of understanding, this embodiment further describes the specific implementation process of the above method in combination with a specific application scenario system. Figure 2-7 As shown, in this embodiment, MICA (mica) is used as a flexible substrate 1, a Ti / Pt stack is used as a gate (i.e., a first metal layer 2), Al2O3 is used as a dielectric layer 3, a Ti / Au stack is used as a source-drain electrode (i.e., a second metal layer 5), PFBT is used as a monomolecular layer 6, and an organic material C8-BTBT is used as a channel 7, and specifically includes the following steps:
[0056] Step a: spin-coating an adhesion layer (not shown) and a photoresist (not shown) on a MICA (mica) substrate 1 .
[0057] Step b, such as Figure 2 As shown, a MICA (mica) substrate 1 is protected by an ultraviolet lithography alignment mark reticle, and a first metal layer 2 (10 nm Ti and 70 nm Pt) is grown by physical vapor deposition (PVD) to serve as the gate of a single transistor of the memory.
[0058] Step c: removing the photoresist (not shown).
[0059] Step d, such as Figure 3 As shown, PMMA (not shown) is first deposited on the first metal layer, and an Al2O3 dielectric layer 3 with a thickness of 15 nm is deposited on the PMMA by atomic layer deposition.
[0060] Step e, such as Figure 4 As shown, the alignment mark is formed by ultraviolet photolithography, and the through hole 4 is dry-etched.
[0061] Step f, such as Figure 5 As shown, the single transistor source and drain regions are defined by alignment marks through ultraviolet photolithography, and the second metal layer 5 (Ti / Au) is grown by physical vapor deposition as the source and drain electrodes of the single transistor.
[0062] Step g, such as Figure 6 As shown, the entire device was immersed in a 0.5 mg / L PFBT (perfluorobutyl mercaptan) solution for 20 min to form a PFBT monolayer 6.
[0063] Step h, such as Figure 7 As shown, the hard mask alignment mark mask protects the device, and C8-BTBT with a thickness of 50 nm is deposited by vacuum thermal evaporation as the channel 7 of the transistor, the temperature is 160 degrees Celsius, and the deposition rate is 3 nm / min.
[0064] It is worth mentioning that Figure 2-7 The reference numeral a represents a top view, and the reference numeral b represents a cross-sectional view.
[0065] The advantage of the embodiment of the present invention is that by first growing a first metal layer 2 (Ti / Pt stack) as the WWL (write word line) of the memory on a MICA (mica) substrate 1 by photolithography and physical vapor deposition, different numbers of WWLs can be made as needed; Al2O3 is deposited on PMMA (polymethyl methacrylate) by atomic layer deposition; dry etching forms connecting through holes; and a second metal layer 5 (Ti / Au) is grown again by ultraviolet photolithography and physical vapor deposition as the WBL (write bit line), RBL (read bit line) and RWL (read word line) of the memory. The organic material C8-BTBT is deposited on the substrate 1 by vacuum thermal evaporation. Ti / Au and Ti / Pt are grown by ultraviolet photolithography and physical vapor deposition as the source, drain and gate of a single organic transistor, and connected as the WWL, WBL, RWL and RBL of the memory storage unit. A flexible and bendable memory cell transistor channel is realized by organic vapor deposition of organic material C8-BTBT. The method is simple and effective. The laminated structure is made by ultraviolet lithography, physical vapor deposition, atomic layer deposition and vacuum thermal evaporation, which is easy to prepare. High-k material Al2O3 is selected as the device dielectric layer to prevent transistor leakage. The dielectric film is grown by atomic layer deposition technology, and the thickness of the film can be accurately controlled to obtain a highly conformal and high-quality dielectric film. The ultraviolet lithography and physical vapor deposition are simple to prepare the WWL, WBL, RWL and RBL of the flexible 2T0C-DRAM memory.
[0066] like Figure 7 As shown, based on the above-mentioned method for preparing a flexible 2T0C-DRAM, the present invention also provides a flexible 2T0C-DRAM, which is prepared using the above-mentioned method for preparing a flexible 2T0C-DRAM. The flexible 2T0C-DRAM includes a flexible substrate and a gate, a dielectric layer and a source-drain electrode formed in sequence from bottom to top on the flexible substrate; the source-drain electrode forms a flexible and bendable transistor channel.
[0067] Optionally, the dielectric layer is Al2O3 with a thickness of 15nm; the gate is a Ti / Pt stack, wherein the thickness of the Ti layer is 10nm and the thickness of the Pt layer is 70nm; the source and drain electrodes are Ti / Au stacks; the material of the channel is C8-BTBT with a thickness of 50nm.
[0068] The beneficial effect of the flexible 2T0C-DRAM of the present invention is that by using the gate as a Ti / Pt stack, the source and drain electrodes as a Ti / Au stack, and the material of the channel as C8-BTBT with a thickness of 50nm, a smaller storage unit can be achieved, a higher storage density can be obtained, and a flexible 2T0C-DRAM can be obtained.
[0069] like Figure 7As shown, based on the above-mentioned flexible 2T0C-DRAM, the present invention also provides a wearable device, including the above-mentioned flexible 2T0C-DRAM, and the wearable device is one of a smart watch, a smart bracelet, smart glasses, smart headphones, smart clothing, a pedometer and smart shoes.
[0070] The beneficial effect of the wearable device of the present invention is that traditional rigid memory is difficult to meet its usage requirements in complex scenarios such as bending and folding. The flexible 2T0C-DRAM memory of the present invention not only has excellent storage performance, but also has excellent flexibility and bendability, which meets the storage needs of wearable devices and is conducive to the development of the field of flexible electronics.
[0071] It should be understood that the above-mentioned flexible 2TOC-DRAM of the present invention can be applied to wearable devices as well as terminal devices, and the terminal can be implemented in various forms. For example, the terminal described in the present invention may include mobile terminals such as mobile phones, tablet computers, laptop computers, PDAs, portable media players (PMPs), navigation devices, and fixed terminals such as digital TVs and desktop computers. It will be understood by those skilled in the art that, in addition to components specifically used for mobile purposes, the construction according to the embodiments of the present invention can also be applied to fixed-type terminals.
[0072] Although the embodiments of the present invention are described in detail above, it is obvious to those skilled in the art that various modifications and variations can be made to these embodiments. However, it should be understood that such modifications and variations are within the scope and spirit of the present invention as described in the claims. Moreover, the present invention described herein may have other embodiments and may be implemented or realized in a variety of ways.
Claims
1. A method for preparing a flexible 2TOC-DRAM, characterized in that: include: providing a flexible substrate; Growing a first metal layer on the substrate by ultraviolet lithography and physical vapor deposition to serve as a gate of a single transistor of the memory; depositing a dielectric layer on the first metal layer by atomic layer deposition; forming a connecting through hole by dry etching; growing a second metal layer by ultraviolet lithography and physical vapor deposition to serve as source and drain electrodes of a single transistor of the memory; The organic material is deposited on the second metal layer by vacuum thermal evaporation to form a flexible and bendable transistor channel to obtain a flexible 2T0C-DRAM.
2. The method according to claim 1, characterized in that: Depositing an organic material on the second metal layer by vacuum thermal evaporation to form a flexible and bendable transistor channel, and obtaining a flexible 2T0C-DRAM includes: The entire device was immersed in a 0.5 mg / L perfluorobutyl mercaptan solution for 20 min to form a monolayer; The hard mask alignment mark mask protects the device, and the vacuum thermal evaporation deposits the organic material as the channel of the transistor to obtain a flexible 2T0C-DRAM.
3. The method according to claim 2, characterized in that The organic material is C8-BTBT. When the organic material C8-BTBT is deposited as a channel of a transistor, the temperature is 160 degrees Celsius, the deposition rate is 3 nm / min, and the thickness of the deposited channel is 50 nm.
4. The method according to claim 1, characterized in that: A first metal layer is grown on the substrate by ultraviolet lithography and physical vapor deposition, and the gate of a single transistor of the memory includes: The flexible substrate is protected by an ultraviolet lithography alignment mark reticle, and a first metal layer is grown by physical vapor deposition as a gate of a single transistor, wherein the first metal layer is a Ti / Pt stack, and the thickness of the Ti layer is 10nm, and the thickness of the Pt layer is 70nm.
5. The method according to claim 1, characterized in that The second metal layer is grown by ultraviolet lithography and physical vapor deposition, and the source and drain electrodes of a single transistor of the memory include: The source and drain regions of a single transistor are defined by alignment marks through ultraviolet photolithography, and a second metal layer is grown by physical vapor deposition to serve as the source and drain electrodes of the single transistor, wherein the second metal layer is a Ti / Au stack.
6. The method according to claim 1, characterized in that Before growing the first metal layer on the substrate, the method further comprises: Coating an adhesion layer and a photoresist on the upper surface of the substrate respectively; After growing the first metal layer on the substrate, the method further comprises: Remove the photoresist.
7. The method according to claim 1, characterized in that Forming connecting vias by dry etching includes: Alignment marks were made by UV photolithography and through holes were dry etched.
8. A flexible 2T0C-DRAM, manufactured by the method for manufacturing a flexible 2T0C-DRAM according to any one of claims 1 to 7, characterized in that: The flexible 2TOC-DRAM includes a flexible substrate and a gate, a dielectric layer and a source-drain electrode formed sequentially from bottom to top on the flexible substrate; the source-drain electrode forms a flexible and bendable transistor channel.
9. The flexible 2T0C-DRAM according to claim 8, characterized in that: The dielectric layer is Al2O3 with a thickness of 15 nm; and / or the gate is a Ti / Pt stack, wherein the thickness of the Ti layer is 10 nm and the thickness of the Pt layer is 70 nm.
10. The flexible 2T0C-DRAM according to claim 8, characterized in that: The source-drain electrodes are Ti / Au stacks; and / or the material of the channel is C8-BTBT with a thickness of 50 nm.