Temperature-adaptive laser-assisted turning method

CN118905257AActive Publication Date: 2024-11-08NAT UNIV OF DEFENSE TECH

Patent Information

Application Number
CN202411184634.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-08
Estimated Expiration
2044-08-27

AI Technical Summary

Technical Problem

During laser-assisted turning, due to the high-speed rotation of the workpiece, the movement speed of the inner and outer ring spots is large, and the constant traditional laser parameters lead to uneven heating effects, resulting in too high or too low temperatures, reducing optical surface quality and tool life.

Method used

By simulating the laser heating temperature at different positions of the workpiece, adjusting the laser power or spot size, recording and applying adaptive change rules, keeping the temperature at different positions of the workpiece constant, and using adjustable laser body and laser shaping components to achieve laser power or spot Real-time adjustment of size.

Benefits of technology

The uniform heating effect of the workpiece is achieved in full diameter, the surface quality and tool life are improved, and the uniformity and processing quality of the surface structure of the workpiece are significantly improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118905257A_ABST
    Figure CN118905257A_ABST
Patent Text Reader

Abstract

The invention discloses a temperature self-adaptive laser-assisted turning method which comprises the following steps: S1, simulating laser heating temperatures of different positions of a workpiece, keeping the temperatures of the different positions of the workpiece constant by adjusting laser power or light spot size, recording the corresponding laser power or light spot size, and calculating the laser heating temperatures of the different positions of the workpiece; the self-adaptive change rule of the laser power or the light spot size is further obtained; and S2, during actual machining of the turning tool, the laser power is adjusted by the laser device body according to the laser power self-adaptive change rule, or the spot size is adjusted by the laser shaping assembly according to the spot size self-adaptive change rule, so that the heating temperature of the workpiece is kept constant. The laser with variable power or variable size is adopted to assist in ultra-precision turning, a more uniform laser heating effect can be obtained at the full aperture of a workpiece, the temperature stability during turning is guaranteed, the uniformity of inner and outer ring (sub) surface tissues of the turning surface is improved, the service life of a cutter is prolonged, and existing laser-assisted turning equipment does not need to be greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of precision machining methods, and in particular to a temperature-adaptive laser-assisted turning method. Background Art

[0002] High-performance hard and brittle materials are widely used in high-energy lasers, aerospace and other fields, such as single crystal silicon, silicon carbide, fused quartz, glass and ceramics. These materials have the characteristics of high hardness, high brittleness and poor machining performance. When single-point diamond turning is used for processing, problems such as severe tool wear, poor workpiece surface quality and high sub-surface damage of the workpiece are prone to occur, which seriously restricts the application of such materials.

[0003] In order to solve the above problems, in recent years, the laser energy field assisted method has been introduced into the single-point diamond ultra-precision turning process, forming the laser-assisted ultra-precision turning technology. This technology controls the laser to follow the edge movement, heats the material in the turning area in real time, reduces the hardness of the material in the turning area, thereby improving the machinability of the local material and realizing high-precision and low-damage ultra-precision turning of hard and brittle materials. This method has been widely verified to reduce tool wear, reduce cutting force, improve surface integrity and produce high-quality optical surfaces. However, due to the high-speed rotation of the workpiece during turning, the movement speed of the laser spot at different positions of the inner and outer rings of the workpiece is very different. The spot movement speed of the inner ring is infinitely close to 0m / s, and the movement speed of the outer ring can reach 20m / s or even higher. The laser parameters in traditional laser-assisted equipment are often constant. Different spot movement speeds lead to huge differences in the heating effect of the laser on different positions of the workpiece. The larger the diameter of the workpiece, the more obvious this difference. This phenomenon can lead to problems such as insufficient temperature when processing the outer ring and excessive temperature when processing the inner ring. Too high or too low temperature will reduce the surface quality of the optical surface (sub-), shorten the tool life, destroy the consistency of the optical surface microstructure, and restrict the high-quality processing and manufacturing of optical components made of hard and brittle materials.

[0004] Therefore, how to ensure that the laser heating effect on different positions of the workpiece is similar or consistent, so as to control the machinability and surface quality of different areas of the workpiece has become an urgent problem to be solved. Summary of the invention

[0005] The technical problem to be solved by the present invention is to overcome the deficiencies of the prior art and provide a temperature-adaptive laser-assisted turning method that is easy to implement and can achieve a more uniform heating effect over the entire aperture of the workpiece, thereby improving the surface quality of the workpiece and the life of the tool.

[0006] In order to solve the above technical problems, the present invention adopts the following technical solutions:

[0007] A temperature-adaptive laser-assisted turning method, wherein the turning equipment used comprises a laser body, a laser shaping component and a turning tool, wherein the laser body is used to generate laser light and at least adjust the power of the laser light, and the laser shaping component is used to transform the laser light generated by the laser body and at least adjust the spot size of the laser light. The temperature-adaptive laser-assisted turning method comprises the following steps:

[0008] S1. Simulate the laser heating temperature at different positions of the workpiece, keep the temperature at different positions of the workpiece constant by adjusting the laser power or spot size, record the corresponding laser power or spot size, and then obtain the adaptive change law of the laser power or spot size;

[0009] S2. During actual machining of the turning tool, the laser body adjusts the laser power according to the adaptive change law of the laser power or the laser shaping component adjusts the spot size according to the adaptive change law of the spot size to keep the heating temperature of the workpiece constant.

[0010] As a further improvement of the above technical solution: Step S1 is specifically as follows:

[0011] The heat difference between the input and output workpiece can be expressed as:

[0012] Δq=q l -q conv -q rad (1)

[0013] Among them, q l Indicates the laser energy input to the workpiece:

[0014]

[0015] Where P is the laser power, S is the laser coverage area, and E(x(t), y(t), t) represents the position and energy distribution of the laser, which is related to the laser center coordinates x, y and time t;

[0016] q in formula 1 conv Represents the heat dissipated by convection:

[0017] q conv =K conv (T-T0) (3)

[0018] Among them, K conv It represents the heat transfer coefficient of heat flow, T is the material temperature, T0 is the ambient temperature;

[0019] q in formula 1 rad Represents the heat flux lost from the workpiece surface by thermal radiation:

[0020] q rad =εσ Si (T4 -T0 4 ) (4)

[0021] Where ε is the Boltzmann constant, σ Si is the emissivity of the material:

[0022]

[0023] Among them, K cond is the thermal conductivity of the material.

[0024] As a further improvement of the above technical solution: the maximum grid size of the laser motion area is at least one order of magnitude lower than the minimum spot size.

[0025] As a further improvement of the above technical solution: the laser power adjustment range of the laser body is 0W to 100W, and the wavelength adjustment range is 500nm to 1μm.

[0026] As a further improvement of the above technical solution: the laser body can also emit visible light, which is used as a guiding light to determine the positional relationship between the laser and the turning tool, so that the laser acts on the center position of the turning tool edge, and the visible light is concentric with the laser.

[0027] As a further improvement of the above technical solution: the spot size adjustment range of the laser shaping component is 100 μm to 1000 μm.

[0028] As a further improvement of the above technical solution: the spot shape adjustment of the laser shaping component includes circular, square and elliptical shapes.

[0029] As a further improvement of the above technical solution: the spot energy distribution types of the laser shaping component include Gaussian, flat-top and ring types.

[0030] As a further improvement of the above technical solution: the laser shaping assembly includes a beam expander, a shaping mirror and a focusing mirror. The beam expander is used to shape the original laser spot into a collimated Gaussian spot of a fixed size so that the spot meets the entrance condition of the shaping mirror; the shaping mirror is used to shape the Gaussian spot into a required spot shape; the focusing mirror is used to focus the spot into a spot of a specific size.

[0031] As a further improvement of the above technical solution: the turning tool is a diamond tool, the rake angle range is -15 to -65°, the back angle range is 5 to 20°, and the tool tip arc radius range is 0.3 to 1.5 mm.

[0032] Compared with the prior art, the advantages of the present invention are:

[0033] 1) The present invention uses variable power or variable size laser to assist ultra-precision turning, which can obtain a more uniform laser heating effect over the entire aperture of the workpiece, avoiding the problem of low outer ring temperature and excessively high inner ring temperature, and ensuring temperature stability during turning.

[0034] 2) The present invention can significantly improve the uniformity of the (sub)surface structure of the inner and outer rings of the turning surface, thereby improving the surface quality of the workpiece and the life of the tool.

[0035] 3) The present invention does not require substantial improvements to existing laser-assisted turning equipment, and only requires inputting change instructions to the laser body or the laser shaping component.

[0036] Other features and advantages of the present invention will be described in detail in the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 It is a comparative schematic diagram of the effects of constant laser parameters and the adaptive laser parameters of the present invention on a workpiece.

[0038] Figure 2 It is a laser heating temperature simulation model, where (a) is the simulation three-dimensional model; (b) is the grid division; (a1) and (a2) are the laser motion process.

[0039] Figure 3 It is a schematic diagram of the relationship between the stable temperature and the rotation radius of the workpiece.

[0040] Figure 4 It is a schematic diagram of the relationship between the temperature-stabilized laser power and the workpiece rotation radius.

[0041] Figure 5 It is a schematic diagram of the relationship between the temperature stable spot radius and the workpiece rotation radius. DETAILED DESCRIPTION

[0042] In the description of the present invention, it should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0043] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0044] In the present invention, unless otherwise clearly specified and limited, the terms "assemble", "connect", "connect", "fix" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0045] The present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.

[0046] Figures 1 to 5 An embodiment of the temperature-adaptive laser-assisted turning method of the present invention is shown. The turning equipment used in the temperature-adaptive laser-assisted turning method of this embodiment mainly includes four parts: a tool holder body, a laser body, a laser shaping component, and a diamond turning tool.

[0047] The tool holder body can adjust the spatial position of the diamond tool and the laser shaping component (adjustment accuracy is ±10μm), and is also the connecting and fastening part for installing the laser-assisted turning equipment on the ultra-precision lathe.

[0048] The laser body is the key element for generating lasers. It can control the laser power, wavelength, continuity and other parameters. The power adjustment range is: 0W ~ 100W, and the wavelength adjustment range is: 500nm ~ 1μm. Among them, the power adjustment can be controlled by the program and changed in real time during the processing. In addition, the laser body can emit visible light (such as visible red light). Visible light is used as a guide light to determine the positional relationship between the laser and the turning tool, ensuring that the laser acts accurately on the center of the turning tool edge, and the laser and the visible light are completely concentric.

[0049] The laser shaping component can transform the original laser emitted by the laser. It can control the parameters such as the shape, size and energy distribution of the laser. The shapes include: round, square, elliptical, etc. The size adjustment range is: 100μm~1000μm, and the energy distribution includes: Gaussian, flat-top, ring, etc. The laser shaping component includes a beam expander, a shaping mirror and a focusing mirror. Its purpose is to obtain a laser spot of a specific shape, size and energy distribution. The function of the beam expander is to shape the original laser spot into a collimated Gaussian spot of a fixed size so that the spot reaches the entrance condition of the shaping mirror. The function of the shaping mirror is to shape the Gaussian spot into the required spot shape. The shaping mirror can be a diffraction element, a transmission element, and an electrically controlled liquid crystal element. The function of the focusing mirror is to focus a larger spot into a spot of a specific size. It should be noted that the size of the spot can be adjusted by adjusting the position of the focusing mirror. Thereby, the energy density of the laser is changed in real time during the processing process, and the temperature is adaptively adjusted.

[0050] The diamond turning tool is a tool for cutting hard and brittle materials. Preferably, the tool rake angle ranges from -15 to -65°, the back angle ranges from 5 to 20°, and the tool tip arc radius ranges from 0.3 to 1.5 mm.

[0051] The laser body and the laser shaping component cooperate with each other to control various parameters of the auxiliary laser. Figure 1 As shown, when constant laser parameters are used, since the workpiece is in a high-speed rotation state (500-5000rad / min), there is a large linear speed difference between the inner and outer circles, so the temperature difference between the inner and outer circles is large, and it is necessary to control the laser parameters in real time during the processing process to keep the temperature constant. This embodiment provides two methods to achieve the adaptive temperature adjustment function: real-time adjustment of the laser power or spot size according to the different processing positions of the workpiece, as described below.

[0052] Using COMSOL software to perform finite element simulation of laser heating, we first make assumptions about the simulation conditions:

[0053] (1) Since the material removed during ultra-precision machining is at the nanoscale, the heat generated is several orders of magnitude lower than the heat input by the laser, so the cutting heat can be ignored;

[0054] (2) The heating position changes at a constant speed and the workpiece does not vibrate;

[0055] (3) Ignore material deformation caused by cutting or laser;

[0056] (4) The workpiece is in contact only with air and the suction cup.

[0057] The single crystal silicon model is a cylinder with a diameter of 6 mm and a height of 3 mm. Figure 2To ensure the accuracy and stability of the simulation results, the maximum grid size of the laser motion area is 10 μm, which is one order of magnitude lower than the minimum laser spot size. The heat difference between the input and output workpieces can be expressed as:

[0058] Δq=q l -q conv -q rad (1)

[0059] Among them, q l Indicates the laser energy input to the workpiece, which is related to laser parameters such as power, shape, size and energy distribution:

[0060]

[0061] Where P is the laser power, S is the laser coverage area, and E(x(t), y(t), t) represents the position and energy distribution of the laser, which is related to the laser center coordinates x, y and time t.

[0062] q in formula 1 conv Indicates the heat dissipated by thermal convection, which is the heat loss caused by the macroscopic movement of the workpiece. Due to the high-speed rotation of the workpiece, thermal convection cannot be ignored:

[0063] q conv =K conv (T-T0) (3)

[0064] Among them, K conv It represents the heat transfer coefficient for heat flow, which is related to the viscosity, density, thermal diffusion coefficient and expansion coefficient of air. T is the material temperature and T0 is the ambient temperature.

[0065] q in formula 1 rad It indicates the heat flow dissipated from the surface of the workpiece through thermal radiation. Any object, as long as it has temperature, will emit thermal radiation and dissipate energy to the outside world in the form of electromagnetic waves:

[0066] q rad =εσ Si (T 4 -T0 4 ) (4) where ε is the Boltzmann constant, σ Si is the emissivity of the material.

[0067] In addition, heat conduction inside the workpiece is also an important factor affecting laser heating, which can be expressed as:

[0068]

[0069] Among them, K cond It is the thermal conductivity of the material, which is generally related to the type of material and the local temperature distribution.

[0070] By changing x, y, and t in equation 2, the laser heating temperature at different positions can be simulated. l The laser power or laser size in the laser beam can keep the temperature at different positions constant. By recording the laser power or laser size at this time, the adaptive change law of the laser power or size can be obtained to keep the laser heating temperature constant. Finally, the adaptive temperature change law is input into the laser transmitter or laser shaping component to achieve the stability of the workpiece processing temperature.

[0071] Take a 100mm-diameter single crystal silicon as an example: the workpiece rotation speed is 4500rad / min; the laser energy distribution is Gaussian; the laser power is 48W; and the laser diameter is 500μm. At this time, Equation 2 can be rewritten as:

[0072]

[0073] Among them, σ is the variance of Gaussian distribution, which is related to the laser radius, and r is the distance from a point on the surface of single crystal silicon to the center of the laser spot. The spot moves uniformly along the x-axis at a speed of 23.55m / s, corresponding to the linear velocity at a rotation radius of 50mm, so r can be expressed as:

[0074]

[0075] x l =23.55t (8)

[0076] y l =0 (9) where x l and l represents the coordinates of the laser center, and x and y represent the coordinates of a point on the workpiece surface. Equation 7 adds a coefficient of 2.8 on the x-axis, which describes the phenomenon that the laser is compressed after passing through the diamond tool edge. The total simulation time is 10 -4 s, time step is 10 -5 s. It is stipulated that the spot radius is determined by taking 95% of the laser energy as the limit, taking σ=R / 2, R is the spot radius, and combining with formula 6, we can get:

[0077]

[0078] Among them, K is the absorption rate of single crystal silicon to laser energy, which is 0.9 here. Other simulation parameters are shown in Table 1.

[0079] Table 1 A set of typical laser heating simulation parameters

[0080]

[0081] The simulation results are as follows Figure 3As shown in the figure, the temperature drops sharply with the increase of the rotation radius. The most suitable cutting temperature for single crystal silicon is 350℃-1000℃. When the laser parameters remain constant, the temperature of the inner and outer circles of the workpiece does not meet the requirements. In order to improve the temperature stability, only the laser power is changed for simulation to ensure that the temperature is constant at 437±5℃. At this time, the relationship between the laser power and the workpiece rotation radius is shown in the figure. Figure 4 As shown, the functional relationship between the two can be expressed as a linear function:

[0082] P=1.1347r+11.91 (11)

[0083] Among them, P is the laser power, the unit is W; r is the rotation radius of the processing position, the unit is mm. By introducing it into the laser body, the adaptive change of power can be achieved to form a stable laser-assisted heating, such as Figure 3 shown.

[0084] In addition, the temperature can be kept constant by changing the laser spot size. In order to ensure a constant temperature of 437±5℃, the relationship between the laser spot radius and the rotation radius of the processing position is as follows: Figure 5 As shown, the functional relationship between the two can be expressed as a power function:

[0085] R=-32.64r 0.3282 +163 (12)

[0086] Where R is the laser spot radius in μm. By importing it into the laser shaping component, the adaptive change of the spot size can be achieved to form a stable laser-assisted heating, such as Figure 3 shown.

[0087] Although the present invention has been disclosed as above with preferred embodiments, it is not intended to limit the present invention. Any technician familiar with the art can make many possible changes and modifications to the technical solution of the present invention by using the technical content disclosed above without departing from the scope of the technical solution of the present invention, or modify it into an equivalent embodiment of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention should fall within the scope of protection of the technical solution of the present invention.

Claims

1. A temperature-adaptive laser-assisted turning method, characterized in that: The turning equipment used includes a laser body, a laser shaping component and a turning tool. The laser body is used to generate laser and at least adjust the power of the laser. The laser shaping component is used to transform the laser generated by the laser body and at least adjust the spot size of the laser. The temperature-adaptive laser-assisted turning method includes the following steps: S1. Simulate the laser heating temperature at different positions of the workpiece, keep the temperature at different positions of the workpiece constant by adjusting the laser power or spot size, record the corresponding laser power or spot size, and then obtain the adaptive change law of the laser power or spot size; S2. During actual machining of the turning tool, the laser body adjusts the laser power according to the adaptive change law of the laser power or the laser shaping component adjusts the spot size according to the adaptive change law of the spot size to keep the heating temperature of the workpiece constant.

2. The temperature-adaptive laser-assisted turning method according to claim 1, characterized in that: Step S1 is specifically as follows: The heat difference between the input and output workpiece can be expressed as: Δq=q l -q conv -q rad (1) Among them, q l Indicates the laser energy input to the workpiece: Where P is the laser power, S is the laser coverage area, and E(x(t), y(t), t) represents the position and energy distribution of the laser, which is related to the laser center coordinates x, y and time t; q in formula 1 conv Represents the heat dissipated by convection: q conv =K conv (T-T0) (3) Where K conv It represents the heat transfer coefficient of heat flow, T is the material temperature, and T0 is the ambient temperature; q in formula 1 rad Represents the heat flux lost from the workpiece surface by thermal radiation: q rad =εσ Si (T 4 -T0 4 ) (4) Where ε is the Boltzmann constant, σ Si is the emissivity of the material: Among them, q cond is the thermal conductivity of the material.

3. The temperature-adaptive laser-assisted turning method according to claim 2, characterized in that: The maximum grid size in the laser motion area is at least one order of magnitude lower than the minimum spot size.

4. The temperature-adaptive laser-assisted turning method according to any one of claims 1 to 3, characterized in that: The laser power adjustment range of the laser body is 0W-100W, and the wavelength adjustment range is 500nm-1μm.

5. The temperature-adaptive laser-assisted turning method according to any one of claims 1 to 3, characterized in that: The laser body can also emit visible light, which is used as a guiding light to determine the positional relationship between the laser and the turning tool, so that the laser acts on the center position of the turning tool edge, and the visible light is concentric with the laser.

6. The temperature-adaptive laser-assisted turning method according to any one of claims 1 to 3, characterized in that: The spot size adjustment range of the laser shaping component is 100 μm to 1000 μm.

7. The temperature-adaptive laser-assisted turning method according to claim 6, characterized in that: The laser shaping component spot shape adjustment includes circular, square and elliptical.

8. The temperature-adaptive laser-assisted turning method according to claim 6, characterized in that: The light spot energy distribution types of the laser shaping component include Gaussian type, flat top type and ring type.

9. The temperature-adaptive laser-assisted turning method according to any one of claims 1 to 3, characterized in that: The laser shaping component includes a beam expander, a shaping mirror and a focusing mirror. The beam expander is used to shape the original laser spot into a collimated Gaussian spot of a fixed size so that the spot reaches the entrance condition of the shaping mirror; the shaping mirror is used to shape the Gaussian spot into a required spot shape; the focusing mirror is used to focus the spot into a spot of a specific size.

10. The temperature-adaptive laser-assisted turning method according to any one of claims 1 to 3, characterized in that: The turning tool is a diamond tool, with a rake angle ranging from -15 to -65 degrees, a back angle ranging from 5 to 20 degrees, and a tool tip arc radius ranging from 0.3 to 1.5 mm.

Citation Information

Patent Citations

  • Method and device for finish turning a work of hardenable steel

    EP0799669A1

  • Surface machining method

    JP2007290052A

  • Machine tool for machining a micromechanical component, and machining method implemented by said machine tool

    WO2022253801A1

Cited By

  • Flat-topped laser-assisted ultra-precision turning method for high-gradient hard and brittle optical element

    CN121316119A