Shaft sleeve part machining process method
Through the HT250 material, the furnace annealing and multiple heat treatments combined with high-precision processing steps, the problem of deformation of precision sleeve parts during processing is solved, and the high-precision requirements of the dimensional stability and shape tolerance of the parts are achieved, which extends the Service life and improve productivity.
Patent Information
- Application Number
- CN202410958218.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-11-08
AI Technical Summary
Precision sleeve parts are prone to deformation during processing, especially when the temperature difference is large, resulting in slight deformation of the dimensions, which is difficult to meet the requirements of high precision.
The cast blank made of HT250 is used for furnace annealing and natural air-cooling, combined with medium and low temperature aging treatment, laser quenching and high-precision turning and grinding processes, through multiple heat treatment and precision processing steps, including rough processing, semi-finishing processing, and precise processing. , peripheral finishing and internal cylindrical grinding, and online detection and temperature monitoring are used to ensure the dimensional stability of the parts and the accuracy of shape and position tolerances.
It effectively eliminates residual stress and deformation inside the casting, improves the uniformity of the material and processing accuracy, ensures that the shape and position tolerance of the parts meets the design requirements, extends the service life, and improves production efficiency and quality.
Smart Images

Figure CN118905560A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of shaft sleeve parts processing, in particular to a shaft sleeve parts processing method. Background Art
[0002] As a key basic component in the field of mechanical engineering, sleeve parts are carefully manufactured through multiple processes such as precision casting, turning, grinding and heat treatment. They are widely used in many industries such as automobiles, aerospace, machinery manufacturing, electricity and chemical industry. They are made of carbon steel, alloy steel, cast iron, copper alloy and non-metallic materials. The design includes structures such as outer circle, inner hole and thread to achieve functions such as support, guidance and load transfer. Its processing technology and technology are directly related to the performance, durability and operation efficiency of the equipment, reflecting the deep integration of materials science, mechanical processing and modern engineering technology. Since sleeve parts are made of castings (HT250), they have reliable quality, compact structure, high processing accuracy, flexible forming and low cost. Characteristics of castings: high thermal strength, strong corrosion resistance, strong wear resistance and strong impact resistance.
[0003] However, the size of the casting will be slightly deformed when the temperature difference is relatively large, which is not allowed in machinery with high precision requirements. In order to eliminate the internal stress and slight deformation, and overcome the combined effects of internal material uniformity, poor processing technology, clamping force, residual stress, etc. in the casting, it is not easy to ensure the processing quality. Therefore, how to reduce and control the processing deformation of such precision sleeve parts has always been a difficult problem in the parts manufacturing industry.
[0004] Therefore, those skilled in the art have proposed a processing method for shaft sleeve parts to solve the problems raised by the background technology. Summary of the invention
[0005] In order to solve the above technical problems, the present invention provides a processing method for sleeve parts to solve the problem of machining deformation of precision sleeve parts in the prior art.
[0006] A method for machining a shaft sleeve part comprises the following steps:
[0007] S1. Precision casting and heat treatment: Use HT250 material to cast the blank, implement furnace annealing process, and then natural air cooling; this step is to eliminate casting stress and improve metallographic structure;
[0008] S2. Rough machining pretreatment: Rough turning of the outer circle, inner hole and stopper, leaving a 2mm machining allowance on one side to lay the foundation for subsequent machining;
[0009] S3, semi-finishing lifting: the first semi-finishing operation, outer circle, inner hole, stopper and stopper end face;
[0010] S4, Precision Semi-finishing: The second semi-finishing machining, outer circle, inner hole, stopper and stopper end face, ensures that the size is close to the final requirements;
[0011] S5, peripheral finishing: Complete the drilling of peripheral holes and threaded holes, use a drilling jig to ensure accuracy, and the peripheral processing is now completed;
[0012] S6, External cylindrical grinding: High-precision fixtures are used to grind the external cylindrical surface and the end surface of the shaft shoulder to ensure that the surface roughness meets the standard and the shape and position tolerances meet the design requirements. At the same time, the online detection system is used to monitor the processing status in real time to achieve precise control;
[0013] S7, Internal grinding and temperature management: Based on the inner circle and both end faces, finely grind the inner hole and its end faces.
[0014] The parts involved in this method are made of ZL114 sand mold low-pressure casting HT250, with a maximum size of Φ260×289×(inner hole Φ90-Φ125), and extremely high processing accuracy requirements (dimensions in mm); such as the bearing holes at both ends are φ125, the cylindricity is 0.0035 and 0.004, the coaxiality requirement is φ0.006, the surface finish is 0.4μm, and the material is cast iron HT250.
[0015] Preferably, in S1, the blank is slowly heated to 50-100°C / H until the temperature reaches 500-550°C, kept at this temperature for 3-5 hours, then cooled to 200°C at a rate of 20-50°C / H, and then naturally air-cooled.
[0016] Preferably, the S2 also includes the following steps: S201, the first medium and low temperature aging treatment: using an intelligent temperature control furnace, heating to 500-550°C at a rate not exceeding 100°C / H, keeping warm for 4-6 hours, then cooling to 200°C at a rate of 20-30°C / H, and natural air cooling. This step enhances the stability of the material and reduces subsequent processing deformation.
[0017] Preferably, in the semi-finishing turning operation in S3, a single-sided margin of 1 mm is retained.
[0018] Preferably, the S3 further includes the following steps: S301, second medium-low temperature aging treatment: repeating the aging treatment process of step S201 to further stabilize the part size and reduce residual stress.
[0019] Preferably, S302, laser quenching surface strengthening: after semi-finishing, the outer surface is laser quenched to improve wear resistance and fatigue strength, while maintaining the toughness of the core material and reducing the impact of subsequent processing hardening layer.
[0020] Preferably, in the second semi-finishing turning operation in S4, a single-side margin of 0.15 mm is retained.
[0021] Preferably, the S7 further includes the following steps: S701, temperature monitoring, using a far-infrared thermometer to measure the workpiece temperature every 0.1-0.2 minutes during the processing.
[0022] Compared with the prior art, the present invention has the following beneficial effects:
[0023] This method starts from the selection of blanks, the formulation of process routes, the design of tooling, the heat treatment process, the interspersed multiple heat treatments and the formulation of parameters, the selection of processing equipment and tools, and finally through the design of special turning and grinding fixtures, combined with double micrometer alignment and workpiece temperature measurement technology, it finally achieved very good results and cleverly solved the problem of residual stress and temperature difference deformation of precision shaft sleeve parts, ensuring that the processed parts meet the various geometric tolerance accuracy levels required by the drawings after inspection. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 is a process flow chart of the present invention;
[0025] Figure 2 It is a schematic diagram of the cross-sectional structure of the bearing seat of the present invention;
[0026] Figure 3 It is a cross-sectional view of the bearing seat of the present invention in the assembled state. DETAILED DESCRIPTION
[0027] The following is a further detailed description of the embodiments of the present invention in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention but are not intended to limit the scope of the present invention.
[0028] Example: As attached Figure 1 To Attachment Figure 3 As shown: The present invention provides a method for machining a sleeve-type part, comprising the following steps:
[0029] S1. Precision casting and heat treatment: Use HT250 material to cast the blank, implement furnace annealing process, and then naturally air cool; this step is to eliminate casting stress and improve metallographic structure; the blank is slowly heated to 50-100℃ / H until the temperature reaches 500-550℃, after keeping warm for 3-5 hours, it is cooled to 200℃ at a rate of 20-50℃ / H, and then naturally air cooled.
[0030] S2. Rough machining pretreatment: Rough turning of the outer circle, inner hole and stopper, leaving a 2mm machining allowance on one side to lay the foundation for subsequent machining;
[0031] S201, the first medium and low temperature aging treatment: using an intelligent temperature control furnace, heating to 500-550℃ at a rate not exceeding 100℃ / H, keeping warm for 4-6 hours, then cooling to 200℃ at a rate of 20-30℃ / H, and natural air cooling. This step enhances the stability of the material and reduces subsequent processing deformation.
[0032] S3, semi-finishing improvement: the first semi-finishing operation, the outer circle, inner hole, stopper and stopper end face, retain 1mm single-sided allowance;
[0033] S301, second medium and low temperature aging treatment: repeat the aging treatment process of step S201 to further stabilize the part size and reduce residual stress.
[0034] S302, laser quenching surface strengthening: After semi-finishing, the outer surface is laser quenched to improve wear resistance and fatigue strength, while maintaining the toughness of the core material and reducing the impact of subsequent processing hardening layer.
[0035] S4. Precision semi-finishing: For the second semi-finishing, the outer circle, inner hole, stopper and stopper end face are left with a single-sided allowance of 0.15mm to ensure that the size is close to the final requirement.
[0036] S5, peripheral finishing: Complete the drilling of peripheral holes and threaded holes, and use drilling jigs to ensure accuracy. At this point, the peripheral processing is completed.
[0037] S6. External cylindrical grinding: High-precision tooling is used to grind the external cylindrical surface and the end face of the shaft shoulder to ensure that the surface roughness meets the standard and the form and position tolerances meet the design requirements. At the same time, the online detection system is used to monitor the processing status in real time to achieve precise control.
[0038] S7, Internal grinding and temperature management: Based on the inner circle and two end faces, finely grind the inner hole and its end faces;
[0039] S701, temperature monitoring, use a far-infrared thermometer to measure the workpiece temperature every 0.1-0.2 minutes during the processing.
[0040] The parts involved in this method are made of ZL114 sand mold low-pressure casting HT250, with a maximum size of Φ260×289×(inner hole Φ90-Φ125), and extremely high processing accuracy requirements (dimensions in mm); such as the bearing holes at both ends are φ125, the cylindricity is 0.0035 and 0.004, the coaxiality requirement is φ0.006, the surface finish is 0.4μm, and the material is cast iron HT250.
[0041] As soon as the casting comes out of the furnace, it is annealed with the furnace. The purpose is to soften the material of the parts and eliminate some internal stress, which is beneficial to subsequent processing. During processing, the outer circle, inner hole and stopper are rough-turned first, leaving a 2mm margin, and medium and low temperature aging treatment is interspersed in the meantime. Then, the outer circle, inner hole and stopper are semi-finished, leaving a 1mm margin. The inner hole without tolerance can be processed to size, and then medium and low temperature aging treatment is performed again to eliminate internal stress. The second semi-finishing machining of the outer circle and inner hole, with tolerance and roughness of 0.4mm and 0.8mm, leaving grinding allowance, threads and empty tool grooves can be machined to size, and the holes and threaded holes on the periphery are also machined to size; the rest of the peripheral work needs to be completed before finishing. During finishing, special tooling is used to grind out the processing references such as the outer circle and end face, and then the stopper holes and end faces of the two end faces are fine-ground to achieve various shape and position tolerances.
[0042] It is important to note the alignment method, error size and position of the workpiece during finishing, and the difficulty in detecting the coaxiality error after grinding, unless there is a V-frame that is large enough and has a grade 0 accuracy.
[0043] In practice, the dimensions marked on the drawings and the measurement environment temperature are (20℃±2℃), but due to the heat generated by cutting, the temperature of the parts during measurement often exceeds 20℃, which can easily lead to dimensional measurement errors in precision machining. If not taken seriously, it can easily cause economic losses such as scrapping of parts due to tolerance exceeding the tolerance. The two aging treatments in the middle of the present invention, as well as the detection of the workpiece processing temperature and the calculation of the value of the increase or decrease in the workpiece tolerance, ensure the dimensional accuracy of the parts after machining and the requirements of various form and position tolerances, and improve production efficiency and quality.
[0044] As can be seen from the above, the selection of HT250 material ensures good mechanical properties and castability. The furnace annealing process effectively eliminates the residual stress inside the casting, improves the microstructure, and improves the overall uniformity and machinability of the material. The slow heating and cooling rates control the generation of thermal stress, avoid deformation and cracks, and provide a stable base for subsequent processing.
[0045] Rough machining retains sufficient machining allowance to provide sufficient machining space for subsequent processes. At the same time, the first low-temperature aging treatment further stabilizes the material properties, reduces the deformation that may occur during the machining process, ensures dimensional stability, and lays the foundation for subsequent high-precision machining.
[0046] Semi-finishing gradually approaches the final size, retaining 1mm machining allowance, improving the size and shape accuracy; the second aging treatment strengthens the dimensional stability of the parts, almost eliminates residual stress, and creates more stable processing conditions for subsequent finishing;
[0047] Laser quenching enhances the surface hardness and wear resistance of parts, maintains the toughness of the core, optimizes the overall mechanical properties, and significantly improves the surface wear resistance and fatigue strength of parts through local surface hardening treatment, effectively extending the service life. At the same time, it avoids the overall hardening and deformation problems that may be caused by traditional quenching, and maintains the internal machinability of the parts.
[0048] Precise semi-finishing reduces the machining allowance to 0.15mm, further approaching the design size, preparing for final finishing and ensuring dimensional accuracy and surface quality;
[0049] Peripheral finishing completes the processing of all peripheral holes and threaded holes, ensuring the accuracy and interchangeability of all external features to meet assembly and use requirements;
[0050] External cylindrical grinding ensures the shape accuracy and surface roughness of the external circle and end face, which meets the design tolerance requirements. The application of fixtures and online detection systems realizes real-time monitoring and control of the processing process, improving the accuracy and efficiency of processing.
[0051] Internal grinding ensures the ultimate accuracy of the inner hole size and end face, while real-time temperature monitoring effectively controls the dimensional error caused by temperature changes by adjusting the processing parameters, ensuring that the processing accuracy is not affected by thermal deformation, and further improving the processing stability and dimensional consistency of parts.
[0052] First, use a three-jaw automatic centering chuck to hold one end in the CNC lathe processing center, and use a threaded plug to plug the center hole of the tailstock to support the other end. Then turn around and clamp and push to complete the first and second semi-finishing turning. Use a double micrometer when aligning the workpiece to ensure the various form and position tolerances of the workpiece after processing. When grinding the outer circle, use a threaded plug on both end faces to plug the center hole seat. The center hole needs to be re-ground. The two top grindings ensure the coaxiality and verticality of each outer circle and end face (later used as the processing reference and alignment reference), and also ensure the relevant dimensions of the next step of grinding the inner hole. When grinding the inner hole, first clamp one end of the outer circle to align the other end of the outer circle (because the workpiece protrudes too long, you can use a tool holder), align with a double micrometer, grind the bearing holes and end faces of the two end faces to the size (pay attention to temperature control, handheld far-infrared thermometer, measurement interval 0.1--0.2m), measure the workpiece temperature at intervals, so as to calculate the plus and minus variable tolerances of the workpiece tolerance.
[0053] The embodiments of the present invention are provided for the purpose of illustration and description. Although the embodiments of the present invention have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations of the present invention. Ordinary technicians in this field can change, modify, replace and modify the above embodiments within the scope of the present invention.
[0054] In the description of the present invention, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. "Multiple" means two or more, unless otherwise clearly and specifically defined.
[0055] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0056] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0057] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "examples", "specific examples" or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine different embodiments or examples described in this specification and the features of different embodiments or examples, unless they are contradictory.
[0058] In the drawings of the embodiments disclosed in the present invention, only the structures involved in the embodiments disclosed in the present invention are involved, and other structures can refer to the general design. In the absence of conflict, the same embodiment and different embodiments of the present invention can be combined with each other.
[0059] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for processing sleeve parts, characterized in that: The following steps are involved: S1. Precision casting and heat treatment: Use HT250 material to cast the blank, implement furnace annealing process, and then natural air cooling; S2, rough machining pretreatment: rough turning the outer circle, inner hole and stopper, leaving a single-side 2mm machining allowance; S3, semi-finishing lifting: the first semi-finishing operation, outer circle, inner hole, stopper and stopper end face; S4, Precision semi-finishing: The second semi-finishing turning, the outer circle, inner hole, stopper and stopper end face, only retain 0.15mm single-sided allowance; S5, peripheral finishing: complete the drilling of peripheral holes and threaded holes, and use drilling jigs to ensure accuracy; S6, external cylindrical grinding: high-precision fixture clamping is used to grind the external cylindrical surface and the end surface of the shaft shoulder; S7, Internal grinding and temperature management: Based on the inner circle and both end faces, finely grind the inner hole and its end faces.
2. A method for processing sleeve parts as claimed in claim 1, characterized in that: In S1, the blank is slowly heated to 50-100°C / H until the temperature reaches 500-550°C, kept at this temperature for 3-5 hours, and then cooled to 200°C at a speed of 20-50°C / H, and then naturally air-cooled.
3. A method for processing sleeve parts as claimed in claim 2, characterized in that: The S2 also includes the following steps: S201, the first medium and low temperature aging treatment: using an intelligent temperature control furnace, heating to 500-550°C at a rate not exceeding 100°C / H, keeping warm for 4-6 hours, then cooling to 200°C at a rate of 20-30°C / H, and natural air cooling.
4. A method for processing sleeve parts as claimed in claim 3, characterized in that: In the semi-finishing turning operation in S3, a single-sided allowance of 1 mm is retained.
5. A method for processing a sleeve-type part as claimed in claim 4, characterized in that: The S3 also includes the following steps: S301, second medium-low temperature aging treatment: repeating the aging treatment process of step S201.
6. A method for processing a sleeve-type part as claimed in claim 5, characterized in that: S302, laser quenching surface strengthening: After semi-finishing, the outer surface is laser quenched.
7. A method for processing a sleeve-type part as claimed in claim 1, characterized in that: In the second semi-finishing turning operation in S4, a single-side margin of 0.15 mm is retained.
8. A method for processing sleeve parts as claimed in claim 6, characterized in that: The S7 also includes the following steps: S701, temperature monitoring, using a far-infrared thermometer to measure the temperature of the workpiece every 0.1-0.2 minutes during the processing.
Citation Information
Patent Citations
Machining technology for bearing ring
CN106624645A
Processing method of polytetrafluoroethylene thin-wall telescopic air bag
CN110524006A
Method for preparing thin-wall bushing by adopting laser quenching
CN112442576A
Precision numerical control machining method for titanium alloy thin-walled lens barrel part
WO2023070921A1
Cited By
Precision machining process for metal part
CN121339841A
Machining method for improving ball run-out precision of precision valve needle part hole
CN121374327A