Anti-falling ceramic tile mold and pressing method

By introducing components such as secondary concave mechanism and retention push block into the tile mold, the two-stage shaping and depression depth are increased, which solves the pores and fracture problems caused by insufficient dry material shaping ability and improves the molding quality of the tile and laying stability.

CN118906184AInactive Publication Date: 2024-11-08JIANGXI YIMEI CERAMICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411260748.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-10
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the production process of ceramic tile, when the deeper depression is stamped in a single time, the dry material has insufficient shaping ability, which can easily lead to pores and subsequent breakage.

Method used

A type of anti-falling tile mold is adopted, including a secondary concave pressing mechanism on the hydraulic mold. Through the cooperation of the concave limiting plate and the secondary pressure chamber, the space of the restriction groove is gradually expanded, the two-stage shaping is realized, and the risk of depression fracture is reduced. By retaining components such as push-blocking and push-blocking blocks, the depth of depression and side wall thickness are increased.

Benefits of technology

It effectively reduces the risk of depression and fracture, improves the forming quality and laying stability of ceramic tiles, and prevents the occurrence of fall off.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118906184A_ABST
    Figure CN118906184A_ABST
Patent Text Reader

Abstract

The invention discloses an anti-falling ceramic tile mold and a pressing method, and particularly relates to ceramic tile production equipment, the anti-falling ceramic tile mold comprises a hydraulic mold arranged on a hydraulic machine, the hydraulic mold comprises an upper mold and a lower mold, a secondary indenting mechanism is arranged on the upper mold, and a plurality of concave-convex parts are arranged on the upper mold in a linear array; the secondary indenting mechanism comprises a secondary pressure bin, the secondary pressure bin is arranged on the upper die, and a hydraulic head on a hydraulic machine is arranged on the secondary pressure bin. When hydraulic pressure is carried out on material distribution, firstly, a blank is pressed out through closing of a hydraulic mold, at the moment, the depth of a concave in the blank is limited to a shallower position by a concave limiting plate, then after a hydraulic head continues to move to press a secondary pressure bin, the concave limiting plate gradually moves to expand the space of a limiting groove, and therefore shaping continues on the concave after hydraulic pressure is carried out; and the problem of subsequent sunken breakage is reduced in a two-section molding manner by increasing the sunken depth.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of tile production, in particular to an anti-falling tile mould and a pressing method. Background Art

[0002] A tile mold is a mold used to press and shape the mixed and dried tile powder into a dry embryo, usually using a hydraulic press.

[0003] Checkered tiles are one-piece tiles that look similar to mosaic tiles, but are larger, stronger and harder. The grids on the tiles are one-piece, so there is no risk of them falling off.

[0004] According to patent number CN114670314A, publication (announcement) date: 2022-06-28, a quickly positioned forming mold for ceramic tile production is disclosed, including a workbench, a lower mold group is arranged on the workbench, a driving mechanism is arranged at the bottom of the workbench, a lifting mechanism is arranged on the workbench and above the lower mold group, an upper mold group is arranged on the lifting mechanism, the upper mold group includes a slide rod, a slide cylinder, a mounting plate and an upper mold, and two slide rods are fixedly installed on the lifting mechanism, the outer sides of the two slide rods are sleeved with slide cylinders, and the opposite sides of the two slide cylinders are fixedly connected to the mounting plate. The quickly positioned forming mold for ceramic tile production, through the upper mold group, when the hydraulic push rod is operated to move the upper mold downward, the slide cylinder slides on the slide rod to position the moving direction of the upper mold, so that the upper mold will not deviate during the descent process, so that the upper mold and the lower mold can be quickly positioned and fitted, which helps to improve the forming efficiency of ceramic tiles.

[0005] In the prior art including the above-mentioned patents, thin plate tiles are widely promoted due to their advantages of being light, hard, and able to save energy and cost. When lattice tiles are made into thin plate styles, grooves need to be pressed out of the front through a mold to form a lattice, and depressions need to be pressed out of the back through a mold to retain cement mortar and prevent it from falling off. The grooves and depressions are realized on the thin plate tiles at the same time, which will cause the overlapping wall thickness of the grooves and depressions to be too small, which is easy to break and damage. When the depth of the depression is reduced, it is easy to cause the tile mold to fall off during subsequent laying. When a deeper depression is punched out in a single time, pores will appear due to the problem of dry material shaping ability, which is easy to break during subsequent use. Summary of the invention

[0006] The purpose of the present invention is to provide an anti-falling tile mold and a pressing method, aiming to solve the problem that when a deeper depression is punched out in a single time, pores appear due to the problem of dry material shaping ability, and it is easy to break during subsequent use.

[0007] In order to achieve the above-mentioned object, the present invention provides the following technical solutions: an anti-falling tile mold, comprising a hydraulic mold arranged on a hydraulic press, the hydraulic mold comprising an upper mold and a lower mold, the upper mold being provided with a secondary denting mechanism, the upper mold being provided with a plurality of protrusions and concavities in a linear array, and a limiting groove being provided between the protrusions and concavities, the secondary denting mechanism comprising:

[0008] A secondary pressure chamber is arranged on the upper mold, and a hydraulic head on the hydraulic press is arranged on the secondary pressure chamber;

[0009] A limiting concave plate, which is slidably connected in the limiting groove;

[0010] Wherein, the limiting concave plate is driven by the secondary pressure chamber to slide along the limiting groove to expand the space of the limiting groove in the mold cavity.

[0011] Preferably, the first end of the secondary pressure chamber is fixedly connected to a diversion chamber, and a bearing slide head is provided on the limiting recess plate. The bearing slide head is slidably connected in the diversion chamber, and an active space is provided between the two. The pressure in the secondary pressure chamber increases to drive the bearing slide head to slide along the active space, thereby driving the limiting recess plate.

[0012] Preferably, a cavity is opened in the protrusion, and a retention push block is symmetrically arranged in the cavity. The cavity is fixedly connected to the diversion chamber, and the retention push block extends out of the protrusion as the pressure in the diversion chamber increases.

[0013] Preferably, a push-against inclined block is slidably connected in the cavity, the push-against inclined block fits the inclined surface provided on the retention push block, and a second elastic member is provided between the two retention push blocks.

[0014] Preferably, a continuous pressing assembly is further included, which includes a side shift block and a hydraulic pipe slidably connected to the lower mold, and both ends of the hydraulic pipe are movably provided with a pushing head. A pushing rod is provided on the upper mold, and the hydraulic mold is driven to close the mold to drive the pushing rod to push the pushing head, thereby pushing the side shift block to move between the hydraulic molds.

[0015] Preferably, a side wall limiting plate is rotatably connected to the side shift block, and the side wall limiting plate flips over as the hydraulic mold is closed.

[0016] Preferably, a shunt pipe is provided at the first end of the hydraulic pipe, and a push head is provided on the shunt pipe. A stop groove is provided on the push head, and threaded holes are provided in a linear array on the shunt pipe. A limiting screw that fits the stop groove is threadedly connected to the threaded hole.

[0017] Preferably, it also includes a shock storage mechanism, which includes an energy storage shaft and a vibration bar arranged in the lower mold, the energy storage shaft moves with the side shift block to store energy, and the energy storage shaft rotates with the hydraulic mold closing to strike the vibration bar.

[0018] Preferably, a connecting shaft coupled to the side wall of the lateral displacement block is symmetrically rotatably connected in the lower mold, and ratchet heads are arranged in a circular array on the connecting shaft, and the ratchet heads are coupled to the energy storage shaft.

[0019] A method for pressing anti-falling tiles, specifically comprising the following steps:

[0020] S01, adding the tile mixture to the lower mold, and driving the hydraulic mold to close the mold;

[0021] S02, the hydraulic mold is initially closed to press out the outline of the tile, which includes lattice seams and shallow depressions;

[0022] S03, the hydraulic mold continues to close the mold, compacting the tile blank and deepening the depression, and pressing out a retention groove on the side wall of the depression;

[0023] S04. The hydraulic mold is completely closed and vibrated before opening the mold to separate the mold cavity and the tile blank.

[0024] In the above technical scheme, the present invention provides an anti-falling tile mold and pressing method, which have the following beneficial effects: when the divided material is hydraulically pressed, the blank is first pressed out by closing the hydraulic mold. At this time, the depth of the depression on the blank is limited to a shallower position by the limiting concave plate. Then, when the hydraulic head continues to move to press the secondary pressure chamber, the limiting concave plate gradually moves to expand the space of the limiting groove, thereby continuing to shape the depression after hydraulic pressure to increase the depth of the depression. The two-stage shaping method reduces the problem of subsequent depression breakage. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For ordinary technicians in this field, other drawings can also be obtained based on these drawings.

[0026] Figure 1 An overall schematic diagram provided for an embodiment of the present invention;

[0027] Figure 2 An overall explosion diagram provided for an embodiment of the present invention;

[0028] Figure 3 An exploded schematic diagram of a secondary denting mechanism provided by an embodiment of the present invention;

[0029] Figure 4 for Figure 3 The enlarged schematic diagram at A in the middle;

[0030] Figure 5 An exploded schematic diagram of a connecting and pressing assembly provided in an embodiment of the present invention;

[0031] Figure 6 for Figure 5 The enlarged schematic diagram of point B in the middle;

[0032] Figure 7 An overall cross-sectional schematic diagram provided for an embodiment of the present invention;

[0033] Figure 8 for Figure 7 The enlarged schematic diagram at C in the middle;

[0034] Fig. 9 for Figure 7 Enlarged schematic diagram at point D in the middle.

[0035] Description of reference numerals:

[0036] 1. Hydraulic mold; 10. Hydraulic head; 11. Upper mold; 110. Concave and convex protrusion; 1101. Slide; 111. Upper cover; 112. Side pressure edge; 113. Secondary pressure chamber; 114. Restriction groove; 12. Lower mold; 121. Grid restriction strip; 122. Movable groove; 13. Diversion chamber; 131. Connecting pipe; 132. Movable chamber; 14. Pushing inclined block; 141. First elastic member; 15. Retention push block; 151. Second elastic member; 16. Liquid connecting plate; 161. Butt pipe; 162. Butt hole; 2. Secondary concave Mechanism; 21. connecting plate; 22. limiting concave plate; 23. bearing slide head; 3. connecting pressure assembly; 31. side displacement block; 311. side wall limiting plate; 32. hydraulic pipe; 321. shunt pipe; 322. push head; 323. stop groove; 324. limiting screw; 33. push rod; 34. connecting strip; 4. shock storage mechanism; 41. base plate; 411. push strip; 42. energy storage shaft; 421. push plate; 422. energy storage elastic member; 43. connecting shaft; 431. ratchet head; 432. guide block; 44. connecting belt; 45. vibration strip. DETAILED DESCRIPTION

[0037] In order to make the purpose, technical solution and advantages of the embodiments of the present disclosure clearer, the technical solution of the embodiments of the present disclosure will be clearly and completely described below in conjunction with the drawings of the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, not all of the embodiments. Based on the described embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present disclosure.

[0038] Embodiment 1

[0039] like Figure 1-9 As shown, an anti-falling tile mold includes a hydraulic mold 1 arranged on a hydraulic press, the hydraulic mold 1 includes an upper mold 11 and a lower mold 12, a secondary denting mechanism 2 is arranged on the upper mold 11, a plurality of protrusions 110 are arranged in a linear array on the upper mold 11, and a limiting groove 114 is opened between the protrusions 110, and the secondary denting mechanism 2 includes:

[0040] A secondary pressure chamber 113 is disposed on the upper mold 11, and a hydraulic head 10 on the hydraulic press is disposed on the secondary pressure chamber 113;

[0041] The limiting concave plate 22 is slidably connected in the limiting groove 114;

[0042] The limiting concave plate 22 is driven by the secondary pressure chamber 113 to slide along the limiting groove 114 to expand the space of the limiting groove 114 in the mold cavity.

[0043] Specifically, the upper mold 11 is provided with an upper cover 111, which covers the upper mold 11 for shielding and protection. The lower mold 12 is fixedly arranged on the bottom plate of the hydraulic press and cannot be moved. The lower mold 12 is provided with a grid limiting strip 121 for limiting the blank to have a grid-shaped mark. The mold concave and convex 110 is a part of the mold cavity, which is used to press out a plurality of concave grooves when the blank is pressed by the mold, so that after the subsequent ceramic tiles are fired and formed, cement mortar is retained through the concave grooves during laying, thereby increasing friction for connection and fixing. The limiting groove 114 is located between the plurality of concave and convex 110. The deeper the depth of the limiting groove 114, the deeper the side wall of the formed concave groove. There is a side pressure edge 112, which is used to squeeze out excess powder from the mold. When pressing, the hydraulic press first drives the upper mold 11 to move toward the lower mold 12 to press the powder on the lower mold 12 into a blank. At this time, the limiting concave plate 22 does not move, resulting in the protrusion 110 forming a shallower concave groove as the pressing proceeds. Then the hydraulic press continues to press, and the side pressure edge 112 squeezes excess material out of the mold. At the same time, the secondary pressure chamber 113 is pressurized and moved by the hydraulic head 10, and the limiting concave plate 22 is pushed by the liquid to slide along the limiting groove 114 to expand the space of the limiting groove 114 in the mold cavity, thereby subjecting the blank to secondary shaping to extend the side wall of the concave groove and achieve deepening of the concave groove pressing.

[0044] In the above technical solution, when hydraulic pressure is applied to the divided material, the blank is first pressed out by closing the hydraulic mold 1. At this time, the depth of the depression on the blank is limited to a shallow position by the limiting concave plate 22. Then, when the hydraulic head 10 continues to move to press the secondary pressure chamber 113, the limiting concave plate 22 gradually moves to expand the space of the limiting groove 114, thereby continuing to shape the depression after hydraulic pressure to increase the depth of the depression. The two-stage shaping method reduces the problem of subsequent depression breakage.

[0045] As an embodiment provided by the present invention, the first end of the secondary pressure chamber 113 is fixedly connected to the diversion chamber 13, and a bearing slide head 23 is arranged on the limiting recess plate 22. The bearing slide head 23 is slidably connected in the diversion chamber 13, and an active space is arranged between the two. The pressure of the secondary pressure chamber 113 increases to drive the bearing slide head 23 to slide along the active space, thereby driving the limiting recess plate 22.

[0046] Specifically, the first end of the secondary pressure chamber 113 (with Figure 2 , 7 , 8 are for reference, the first end is the lower end, and the second end is the upper end) is fixedly connected with a diverter bin 13, a sliding column is arranged on the diagonal line of the limiting concave plate 22, the sliding column is slidably connected to the upper mold 11, a connecting plate 21 is arranged between the sliding columns, a bearing slide 23 is arranged on the connecting plate 21, a movable bin 132 is fixedly connected in the diverter bin 13, the bearing slide 23 is slidably connected in the movable bin 132, and an active space is arranged between the two, and a pressure piece is arranged in the active space (the pressure piece can be a gas, liquid or metal elastic piece with compression ability and pressure). When the secondary pressure bin 113 is pressed by the hydraulic head 10 and the pressure exceeds the upper limit of the pressure piece in the active space, the active space is compressed so that the bearing slide 23 is pushed by the liquid in the secondary pressure bin 113 and moves toward the second end of the secondary pressure bin 113, thereby driving the limiting concave plate 22 to slide along the limiting groove 114.

[0047] First, the upper mold 11 moves toward the lower mold 12 to press the powder into a blank. At this time, the limiting concave plate 22 does not move, and the concave groove of the blank is shallow. Then the hydraulic press continues to press. At this time, the side pressure edge 112 squeezes the excess material out of the mold. At the same time, the active space is compressed so that the bearing slider 23 is pushed by the liquid in the secondary pressure chamber 113 to expand the space of the limiting groove 114 in the mold cavity, thereby performing a secondary shaping of the blank to extend the side wall of the concave groove and achieve a deeper concave groove pressing.

[0048] As an embodiment provided by the present invention, a cavity is opened in the protrusion 110, and the cavity is symmetrically provided with a retention push block 15. The cavity is fixedly connected to the diversion chamber 13, and the retention push block 15 extends out of the protrusion 110 as the pressure in the diversion chamber 13 increases.

[0049] Specifically, the diversion bin 13 is fixedly connected with a connecting pipe 131, a docking hole 162 is provided on the cavity, and a plurality of docking holes 162 are fixedly connected with a liquid connecting plate 16, and the liquid connecting plate 16 is provided with a docking pipe 161 fixedly connected with the connecting pipe 131, and a slide groove 1101 for the retention push block 15 to slide is provided on the cavity. When the liquid in the secondary pressure bin 113 increases and is pushed, the liquid will enter the cavity along the liquid connecting plate 16 and push the retention push block 15 to extend the protrusion 110, so as to squeeze the concave groove on the blank, and squeeze out the retention groove in the concave groove. The retention groove can retain more moisture in the tile soaking step before installation, so as to make up for the small water content of thin plate tiles, and the moisture is easily absorbed by cement mortar and wall transition to produce cavities. The blank when squeezing the retention groove can also make up for the extra blank in the deepened concave groove, thereby reducing the squeezing of the blank body.

[0050] First, the upper mold 11 moves toward the lower mold 12 to press the powder into a blank. At this time, the limiting concave plate 22 does not move, and the concave groove of the blank is shallow. Then the hydraulic press continues to press. At this time, the side pressure edge 112 squeezes the excess material out of the mold. At the same time, the active space is compressed so that the bearing slider 23 is pushed by the liquid in the secondary pressure chamber 113 to expand the space of the limiting groove 114 in the mold cavity, thereby reshaping the blank to extend the side wall of the concave groove. At the same time, the liquid will enter the cavity along the liquid connecting plate 16 to push the retention push block 15 to extend the molding concave protrusion 110, and squeeze out a retention groove in the concave groove.

[0051] As an embodiment provided by the present invention, a push-against inclined block 14 is slidably connected in the cavity, and the push-against inclined block 14 fits the inclined surface provided on the retention push block 15 . A second elastic member 151 is provided between the two retention push blocks 15 .

[0052] Specifically, a push-against inclined block 14 is slidably connected in the cavity, and a first elastic member 141 can be provided between the push-against inclined block 14 and the cavity. The push-against inclined block 14 fits the inclined surface provided on the retention push block 15. When the liquid in the cavity pushes the push-against inclined block 14, the push-against inclined block 14 squeezes the upper inclined surfaces of the two retention push blocks 15 to drive the second elastic member 151 to stretch, and push the retention push block 15 out of the protrusion 110 to form a retention groove in the recessed groove.

[0053] Furthermore, the first elastic member 141 and the second elastic member 151 may both be metal springs.

[0054] First, the upper mold 11 moves toward the lower mold 12 to press the powder into a blank. At this time, the limiting concave plate 22 does not move, and the concave groove of the blank is shallow. Then the hydraulic press continues to press. At this time, the side pressure edge 112 squeezes the excess material out of the mold. At the same time, the active space is compressed so that the bearing slider 23 is pushed by the liquid in the secondary pressure chamber 113 to expand the space of the limiting groove 114 in the mold cavity, thereby performing secondary shaping of the blank to extend the side wall of the concave groove. At the same time, the liquid will enter the cavity along the liquid connecting plate 16 and push the push-pull inclined block 14. The push-pull inclined block 14 pushes the symmetrical retention push block 15 to extend the mold concave protrusion 110, and squeeze out the retention groove in the concave groove.

[0055] As an embodiment provided by the present invention, it also includes a continuous pressing assembly 3, which includes a side shift block 31 and a hydraulic pipe 32 slidably connected to the lower mold 12, and both ends of the hydraulic pipe 32 are movably provided with a pushing head 322, and a pushing rod 33 is provided on the upper mold 11. The hydraulic mold 1 is driven to close the mold to drive the pushing rod 33 to push the pushing head 322, thereby pushing the side shift block 31 to move between the hydraulic molds 1.

[0056] Specifically, the hydraulic pipe 32 is fixed on the profile, and the side shift blocks 31 are slidably connected to the two sides of the lower mold 12. Two connecting strips 34 are arranged between the two side shift blocks 31. The connecting strips 34 and the side shift blocks 31 are wrapped into a side frame to be sleeved on the lower mold 12. Pushing heads 322 are movably arranged at both ends of the hydraulic pipe 32. When the hydraulic press pushes the upper mold 11 and the lower mold 12 to close the mold, the pushing rod 33 on the upper mold 11 will push one of the pushing heads 322, so that the other pushing head 322 pushes the side shift block 31, and moves the side frame between the hydraulic molds 1 (that is, between the upper mold 11 and the lower mold 12) to press the powder.

[0057] First, the upper mold 11 moves toward the lower mold 12. At this time, the upper mold 11 will drive the side frame to move between the hydraulic molds 1 to press the powder into a blank. At this time, the limiting concave plate 22 has not moved, and the concave groove of the blank is shallow. Then the hydraulic press continues to press. At this time, the side pressure edge 112 squeezes the excess material out of the mold. At the same time, the active space is compressed so that the bearing slider 23 is pushed by the liquid in the secondary pressure chamber 113 to expand the space of the limiting groove 114 in the mold cavity, thereby performing secondary shaping of the blank to extend the side wall of the concave groove. At the same time, the liquid will enter the cavity along the liquid connecting plate 16 and push the push-pushing inclined block 14. The push-pushing inclined block 14 pushes the symmetrical retention push block 15 to extend the mold concave protrusion 110, and squeeze out the retention groove in the concave groove.

[0058] As an embodiment provided by the present invention, a side wall limiting plate 311 is rotatably connected to the side shift block 31 , and the side wall limiting plate 311 turns over as the hydraulic mold 1 is closed.

[0059] Specifically, the side shift block 31 is rotatably connected to a side wall limiting plate 311, which can flip over when the hydraulic mold 1 is closed to press a slope on the side wall of the blank, and the rotation direction of the side wall limiting plate 311 can be controlled to make the side wall angles of different batches of blanks complementary, thereby reducing the manual bevel grinding steps during subsequent laying, so as to facilitate the laying of tiles and the filling of seams after laying. When the side wall limiting plate 311 flips toward the mold cavity, it assists in compacting the side blank, and when the side wall limiting plate 311 flips toward the outside (i.e., the opposite direction of flipping toward the mold cavity), the side space will be expanded to increase the edge thickness.

[0060] First, the upper mold 11 moves toward the lower mold 12. At this time, the upper mold 11 will drive the side frame to move between the hydraulic mold 1, and the side wall limiting plate 311 will flip over to press the powder into a blank. At this time, the limiting concave plate 22 has not moved, and the concave groove of the blank is shallow. Then the hydraulic press continues to press. At this time, the side pressure edge 112 squeezes the excess material out of the mold. At the same time, the active space is compressed so that the bearing slider 23 is pushed by the liquid in the secondary pressure chamber 113 to expand the space of the limiting groove 114 in the mold cavity, thereby reshaping the blank to extend the side wall of the concave groove. At the same time, the liquid will enter the cavity along the liquid connecting plate 16 and push the push-bevel block 14. The push-bevel block 14 pushes the symmetrical retention push block 15 to extend the mold protrusion 110, and squeeze out the retention groove in the concave groove.

[0061] As an embodiment provided by the present invention, a shunt pipe 321 is provided at the first end of the hydraulic pipe 32, and a push head 322 is provided on the shunt pipe 321. A stop groove 323 is provided on the push head 322, and threaded holes are provided in a linear array on the shunt pipe 321. A limiting screw 324 that fits the stop groove 323 is threadedly connected to the threaded hole.

[0062] Specifically, the first end of the hydraulic pipe 32 (with Figure 5 For reference, the end close to the central axis of the lower mold 12 is the first end, and the end away from the central axis of the lower mold 12 is the second end) is provided with a shunt pipe 321, and a stop groove 323 is provided on the pushing head 322. According to the required flipping angle, the limiting screw 324 is threadedly connected to the corresponding threaded hole, and when the second end of the hydraulic pipe 32 is pushed by the pushing rod 33, the two pushing heads 322 on the shunt pipe 321 will first move at the same time, and with the pushing, the stop groove 323 on one of the pushing heads 322 is first restricted by the limiting screw 324 and cannot move, so that the other pushing head 322 will slide along the side wall limiting plate 311 while pushing the side wall limiting plate 311 to rotate, so as to realize the pressing of the inclined side of the blank.

[0063] First, the upper mold 11 moves toward the lower mold 12. At this time, the upper mold 11 will drive the side frame to move between the hydraulic mold 1, and the push head 322 on the diverter pipe 321 will move and stagger, so that the side wall limiting plate 311 will flip over to press the powder into a blank. At this time, the limiting concave plate 22 has not moved, and the concave groove of the blank is shallow. Then the hydraulic press continues to press. At this time, the side pressure edge 112 squeezes the excess material out of the mold, and the active space is compressed at the same time, so that the bearing slider 23 is pushed by the liquid in the secondary pressure chamber 113 to expand the space of the limiting groove 114 in the mold cavity, thereby reshaping the blank to extend the side wall of the concave groove. At the same time, the liquid will enter the cavity along the connecting liquid plate 16 and push the push inclined block 14. The push inclined block 14 pushes the symmetrical retention push block 15 to extend the mold protrusion 110, and squeeze out the retention groove in the concave groove.

[0064] As an embodiment provided by the present invention, it also includes a shock storage mechanism 4, which includes an energy storage shaft 42 and a vibration bar 45 arranged in the lower mold 12. The energy storage shaft 42 moves with the side shift block 31 to store energy, and the energy storage shaft 42 rotates with the hydraulic mold 1 to hit the vibration bar 45.

[0065] Specifically, a movable groove 122 is opened on the lower mold 12, and the energy storage shaft 42 is rotatably connected in the movable groove 122. The vibration bar 45 is arranged in the lower mold 12 and is fixed and cannot move. The energy storage shaft 42 is symmetrically arranged along the lower mold 12, and the two ends of the vibration bar 45 extend into the movable groove 122 respectively. A plurality of push plates 421 are arranged on the energy storage shaft 42 in a circular array. When the energy storage shaft 42 rotates, the plurality of push plates 421 strike the extended parts at both ends of the vibration bar 45 to vibrate the lower mold 12, thereby assisting in separating the lower mold 12 and the blank.

[0066] First, the upper mold 11 moves to the lower mold 12. At this time, the upper mold 11 drives the side frame to move between the hydraulic mold 1, and the push head 322 on the shunt pipe 321 moves and staggers, so that the side wall limit plate 311 will flip to press the powder into a blank. At this time, the limit concave plate 22 does not move, and the concave groove of the blank is shallow. Then the hydraulic press continues to press. At this time, the side pressure edge 112 squeezes the excess material out of the mold, and the active space is compressed, so that the bearing slide head 23 is pressed by the secondary pressure. The liquid in the force bin 113 pushes to expand the space of the limiting groove 114 in the mold cavity, thereby reshaping the blank to extend the side wall of the recessed groove. At the same time, the liquid will enter the cavity along the liquid connecting plate 16 to push the push-pull inclined block 14, and the push-pull inclined block 14 pushes the symmetrical retention push block 15 to extend the molding protrusion 110, and squeeze out a retention groove in the recessed groove. After the preparation for mold closing is completed, the energy storage shaft 42 rotates through multiple push plates 421 to knock the vibration bar 45 to generate vibration.

[0067] As the optimal embodiment provided by the present invention, a connecting shaft 43 symmetrically rotated and connected to the side wall of the coupling side shift block 31 is provided in the lower mold 12 , and ratchet heads 431 are arranged in a circular array on the connecting shaft 43 , and the ratchet heads 431 are coupled to the energy storage shaft 42 .

[0068] Specifically, an energy storage elastic member 422 (the energy storage elastic member 422 can be a metal spring) is arranged between the energy storage rotating shaft 42 and the movable groove 122, and a connecting rotating shaft 43 is symmetrically rotatably connected in the lower mold 12. Both connecting rotating shafts 43 are sleeved with connecting rotating belts 44, and the connecting rotating belts 44 are rotatably connected to the lower mold 12. The connecting rotating belts 44 fit the side shift block 31, and the connecting rotating belts 44 can rotate with the movement of the side shift block 31. A plurality of ratchet heads 431 are arranged in a circular array on the connecting rotating shaft 43, and the ratchet heads 431 pull the one-way coupled energy storage rotating shaft 42 through the elastic member, and the two groups of ratchet heads 431 The coupling direction is opposite to that of the lateral displacement block 31, so that the energy storage shaft 42 can rotate in the same direction to store energy when the side shift block 31 moves up and down. A guide block 432 is fixedly connected to the connecting shaft 43, and a base plate 41 is provided on the upper mold 11. A push bar 411 is provided on the base plate 41. When the mold is closed to the final position, the push bar 411 will push along the guide block 432 with the movement of the upper mold 11 to pull the connecting shaft 43, and the two sets of ratchet heads 431 will disengage from the energy storage shaft 42 to uncouple the energy storage shaft 42, thereby rotating the energy storage shaft 42 to generate vibration at the end of mold closing to assist in demolding.

[0069] First, the upper mold 11 moves to the lower mold 12. At this time, the upper mold 11 will drive the side frame to move between the hydraulic molds 1, and the push heads 322 on the diverter pipe 321 will move and stagger, so that the side wall limiting plates 311 will flip over to press the powder into blanks. At the same time, when the side shift block 31 moves up and down, the connecting shaft 43 rotates to store energy on the energy storage shaft 42, and after the mold is closed, the energy storage shaft 42 rotates through multiple push plates 421 to knock the vibration bar 45 to generate vibration. At this time, the concave plate 22 does not move, and the concave groove of the blank is shallow. Then the hydraulic press continues to press. At this time, the side pressure edge 112 squeezes the excess material out of the mold. At the same time, the active space is compressed, so that the bearing slider 23 is pushed by the liquid in the secondary pressure chamber 113 to expand the space of the limiting groove 114 in the mold cavity, thereby reshaping the blank to extend the side wall of the concave groove. At the same time, the liquid will enter the cavity along the liquid connecting plate 16 to push the push-pull inclined block 14, and the push-pull inclined block 14 pushes the symmetrical retention push block 15 to extend the mold concave protrusion 110, squeezing out a retention groove in the concave groove.

[0070] Embodiment 2

[0071] A method for pressing anti-falling tiles, specifically comprising the following steps:

[0072] S01, adding the tile mixture to the lower mold 12, and driving the hydraulic mold 1 to close the mold;

[0073] S02, the hydraulic mold 1 is initially closed to press out the outline of the tile, and the outline of the tile includes lattice seams and shallow depressions;

[0074] S03, the hydraulic mold 1 is continuously closed to compact the tile blank and deepen the depression, and a retention groove is pressed out on the side wall of the depression;

[0075] S04. The hydraulic mold 1 is completely closed and vibrated before opening the mold to separate the mold cavity and the tile blank.

[0076] The above description is only by way of illustration of certain exemplary embodiments of the present invention. It is undoubted that those skilled in the art can modify the described embodiments in various ways without departing from the spirit and scope of the present invention. Therefore, the above drawings and descriptions are illustrative in nature and should not be construed as limiting the scope of protection of the claims of the present invention.

Claims

1. An anti-falling tile mold, comprising a hydraulic mold (1) arranged on a hydraulic press, the hydraulic mold (1) comprising an upper mold (11) and a lower mold (12), characterized in that: The upper mold (11) is provided with a secondary denting mechanism (2), the upper mold (11) is provided with a plurality of protrusions (110) in a linear array, and limiting grooves (114) are provided between the protrusions (110). The secondary denting mechanism (2) comprises: A secondary pressure chamber (113) is arranged on the upper mold (11), and a hydraulic head (10) on a hydraulic press is arranged on the secondary pressure chamber (113); A limiting concave plate (22) slidably connected in the limiting groove (114); The limiting concave plate (22) is driven by the secondary pressure chamber (113) to slide along the limiting groove (114) to expand the space of the limiting groove (114) in the mold cavity.

2. The anti-falling tile mold according to claim 1, characterized in that: The first end of the secondary pressure chamber (113) is fixedly connected to the diversion chamber (13), and a bearing slide (23) is provided on the limiting concave plate (22). The bearing slide (23) is slidably connected to the diversion chamber (13), and an activity space is provided between the two. When the pressure of the secondary pressure chamber (113) increases, the bearing slide (23) is driven to slide along the activity space, thereby driving the limiting concave plate (22).

3. The anti-falling tile mold according to claim 2, characterized in that: A cavity is provided in the protrusion (110), and a retention push block (15) is symmetrically arranged in the cavity. The cavity is fixedly connected to the diversion chamber (13), and the retention push block (15) extends out of the protrusion (110) as the pressure in the diversion chamber (13) increases.

4. The anti-falling tile mold according to claim 3, characterized in that: A push-against inclined block (14) is slidably connected in the cavity, and the push-against inclined block (14) fits the inclined surface provided on the retention push block (15). A second elastic member (151) is provided between the two retention push blocks (15).

5. The anti-falling tile mold according to claim 1, characterized in that: It also includes a continuous pressing assembly (3), which includes a side shift block (31) and a hydraulic pipe (32) slidably connected to the lower mold (12), and both ends of the hydraulic pipe (32) are movably provided with a push head (322), and a push rod (33) is provided on the upper mold (11), and the hydraulic mold (1) is driven to close the mold to drive the push rod (33) to push the push head (322), thereby pushing the side shift block (31) to move between the hydraulic molds (1).

6. The anti-falling tile mold according to claim 5, characterized in that: The side shift block (31) is rotatably connected to a side wall limiting plate (311), and the side wall limiting plate (311) turns over as the hydraulic mold (1) is closed.

7. The anti-falling tile mold according to claim 6, characterized in that: A shunt pipe (321) is provided at the first end of the hydraulic pipe (32), and a push head (322) is provided on each of the shunt pipes (321). A stop groove (323) is provided on the push head (322). Threaded holes are provided in a linear array on the shunt pipe (321), and a limiting screw (324) is threadedly connected to the threaded hole and fits the stop groove (323).

8. The anti-falling tile mold according to claim 5, characterized in that: It also includes a shock storage mechanism (4), which includes an energy storage rotating shaft (42) and a vibration bar (45) arranged in the lower mold (12), the energy storage rotating shaft (42) moves with the side shift block (31) to store energy, and the energy storage rotating shaft (42) rotates with the hydraulic mold (1) to close the mold and strike the vibration bar (45).

9. The anti-falling tile mold according to claim 8, characterized in that: A connecting shaft (43) coupled to the side wall of the lateral displacement block (31) is symmetrically rotatably connected inside the lower mold (12), and ratchet heads (431) are arranged in a circular array on the connecting shaft (43), and the ratchet heads (431) are coupled to the energy storage shaft (42).

10. A method for pressing tiles to prevent falling off, characterized in that: The anti-falling tile mold according to claims 1 to 8 comprises the following steps: S01, adding the tile mixture to the lower mold (12), and driving the hydraulic mold (1) to close the mold; S02, the hydraulic mold (1) is initially closed to press out the outline of the tile, and the outline of the tile includes lattice seams and shallow depressions; S03, the hydraulic mold (1) is continuously closed to compact the tile blank and deepen the depression, and a retention groove is pressed out on the side wall of the depression; S04. The hydraulic mold (1) is completely closed and vibrated before opening the mold to separate the mold cavity and the tile blank.