Manufacturing method of carpet for vehicle and carpet for vehicle

By using PET upright cotton as the bottom layer and injecting the PU surface layer in automotive carpets, the complex structure and environmental protection problems of traditional automotive carpets are solved, and the wear resistance, waterproof, easy cleaning and low VOC effects are achieved, and production is improved Efficiency and environmental protection.

CN118906487APending Publication Date: 2024-11-08GUANGZHOU AUTOMOBILE GROUP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410969738.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-18
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Traditional automotive carpets have problems such as complex structure, cumbersome molding process, low production efficiency, high cost, large odor, high VOC release and not environmentally friendly. At the same time, the surface layer is easily contaminated with dust and dirt, is not waterproof and not easy to clean.

Method used

PET upright cotton is used as the base layer, and the surface layer is formed by injecting PU raw material into the injection mold after preforming. The upper surface of the upright cotton is injected by closed-mold injection, and the pressure-keeping and cooling are fixed to form a double-layer structure of automotive carpet, which is simplified. Process, reduce costs.

Benefits of technology

It realizes the wear resistance, waterproof, easy cleaning, sound insulation, low odor, low VOC release and environmental protection effects of automotive carpets, while improving production efficiency and material utilization.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118906487A_ABST
    Figure CN118906487A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a carpet for a vehicle and the carpet for the vehicle. The manufacturing method of the carpet for the vehicle comprises the following steps: performing pre-forming treatment on PET (Polyethylene Terephthalate) vertical cotton to form a bottom layer; putting the PU raw material into a high-pressure tank; the preformed PET vertical cotton is put into an injection mold, and the mold is closed; injecting the PU raw material in the high-pressure tank into the upper surface of the PET upright cotton in the injection mold in a mold-closing injection manner to form a surface layer, and maintaining the pressure for a first preset time; and cooling and shaping the bottom layer and the surface layer in the injection mold. According to the manufacturing method of the carpet for the vehicle, the manufacturing method of the carpet for the vehicle is simple, high in efficiency and low in cost, and the manufactured carpet for the vehicle has the effects of being resistant to abrasion, waterproof, easy to clean, sound-proof, low in odor, low in VOC release amount, environmentally friendly and high in comfort degree.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of carpets, in particular to a manufacturing method of a vehicle carpet and the vehicle carpet. Background Art

[0002] In the related art, carpet is an important interior decoration of automobiles, and plays an important role in the beautiful decoration of automobile interiors, sound insulation and noise reduction in the car, etc. Traditional automotive carpets generally use polyester fibers such as PET (Polyethylene glycol terephthalate) as the surface layer, EPDM (Ethylene Propylene Diene Monomer) or EVA (Ethylene Vinyl Acetate Copolymer) as the middle sound insulation layer, and PET upright cotton felt as the bottom layer. The layers are bonded and compounded by PE (polyethylene), PP (polypropylene) or hot melt adhesives, and then molded. There are a series of disadvantages such as complex structure, cumbersome molding process, low production efficiency, high cost, strong odor, high VOC (Volatile Organic Compounds) release, and environmental protection. At the same time, the surface layer of polyester fibers such as PET is easily contaminated with dust and dirt, is not waterproof, and is not easy to clean.

[0003] In addition, the area covered by the car carpet is the main activity area for people in the car. The car carpet is stepped on by drivers and passengers for a long time. Its surface is prone to wear problems such as pilling and deformation due to contact and friction with the soles of shoes. Therefore, high requirements are placed on the surface strength and wear resistance of the car carpet. Summary of the invention

[0004] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the present invention provides a method for manufacturing a vehicle carpet, which is simple, efficient and low-cost, and the manufactured vehicle carpet has the effects of wear resistance, waterproofness, easy cleaning, sound insulation, low odor, low VOC emission, environmental protection and high comfort.

[0005] The present invention also provides a vehicle carpet, which is manufactured by the above-mentioned vehicle carpet manufacturing method.

[0006] The method for manufacturing a car carpet according to an embodiment of the present invention includes: preforming PET upright cotton to form a bottom layer; placing PU (polyurethane) raw materials in a high-pressure tank; placing the preformed PET upright cotton in an injection mold and closing the mold; injecting the PU raw materials in the high-pressure tank into the upper surface of the PET upright cotton in the injection mold by a closed mold injection method to form a surface layer, and maintaining the pressure for a first preset time; and cooling and shaping the bottom layer and the surface layer inside the injection mold.

[0007] According to the method for making a car carpet of an embodiment of the present invention, the PET upright cotton is preformed to form a bottom layer, and then the PU raw material is placed in a high-pressure tank and the synthesized PU is injected into the upper surface of the PET upright cotton placed in the injection mold by closed mold injection to form a surface layer, and then after pressure holding, cooling and shaping, and cutting, a double-layer car carpet with PET upright cotton as the bottom layer and PU layer as the surface layer can be formed. The structure and processing process are simple, the types of materials required are small, it is easy to produce and the production and molding efficiency is high, which can reduce production costs. The car carpet made by the above-mentioned production method can not only ensure good elasticity and softness, provide a comfortable stepping experience, but also achieve the effects of wear resistance, waterproofness, easy cleaning, sound insulation, low odor, low VOC emission and environmental protection.

[0008] According to some embodiments of the present invention, the preforming of the PET upright cotton to form the bottom layer includes: placing the PET upright cotton into a preforming mold for molding to form the bottom layer, and maintaining the pressure for a second preset time.

[0009] In some embodiments of the present invention, the mold temperature of the preforming mold is 70-80°C.

[0010] In some embodiments of the present invention, the second preset time is 2 to 3 minutes.

[0011] According to some embodiments of the present invention, the PU raw material includes isocyanate and polyol functional groups. After placing the PU raw material into a high-pressure tank, the method for manufacturing the automotive carpet further includes: uniformly mixing the isocyanate and the polyol functional groups in the high-pressure tank.

[0012] In some embodiments of the present invention, the mixing pressure of the isocyanate and the polyol functional group in the high-pressure tank is 110-160 bar.

[0013] In some embodiments of the present invention, the ratio of the isocyanate to the polyol functional group is 3.0:1 to 2.0:1.

[0014] According to some embodiments of the present invention, the mold temperature of the injection mold is 75-90°C.

[0015] According to some embodiments of the present invention, the thickness of the surface layer is 1.5-3.0 mm.

[0016] According to some embodiments of the present invention, the first preset time is 3 to 5 minutes.

[0017] According to some embodiments of the present invention, when the PU raw material in the high-pressure tank is injected onto the upper surface of the PET upright cotton in the injection mold by closed mold injection, the injection flow rate of the high-pressure tank is 200-350 g / s.

[0018] According to some embodiments of the present invention, the injection mold has 1 to 4 injection ports.

[0019] The automotive carpet according to the embodiment of the present invention is composed of a surface layer and a bottom layer stacked in layers, wherein the surface layer is a PU layer and the bottom layer is a PET layer.

[0020] According to the automotive carpet of the embodiment of the present invention, the automotive carpet is composed of a PU layer surface layer and a PET layer bottom layer stacked by the above-mentioned manufacturing method, and the structure and processing process are simple, which can ensure good elasticity and softness, provide a comfortable stepping experience, and achieve the effects of wear resistance, waterproofness, easy cleaning, sound insulation, low odor, low VOC emission and environmental protection. In addition, the types of materials required to make the automotive carpet are small, easy to produce and high in production and molding efficiency, which can reduce production costs.

[0021] In some embodiments of the present invention, the density of the PU layer is 1.05-1.15 g / cm3; and / or the density of the PET layer is 540-660 g / m3; and / or the hardness of the PU layer is 60-90 HA; and / or the thickness of the surface layer is 1.5-3.0 mm.

[0022] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:

[0024] Figure 1 is a cross-sectional view of a vehicle carpet according to an embodiment of the present invention;

[0025] Figure 2 Schematic diagram of a method for manufacturing a vehicle carpet according to an embodiment of the present invention.

[0026] Reference numerals:

[0027] 10. Car carpet;

[0028] 1. Bottom layer;

[0029] 2. Surface layer. DETAILED DESCRIPTION

[0030] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.

[0031] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In addition, features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "multiple" means two or more.

[0032] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0033] Reference below Figure 1-Figure 2 A method for manufacturing the automotive carpet 10 according to an embodiment of the present invention is described.

[0034] like Figure 2 As shown, the method for manufacturing the automotive carpet 10 according to the embodiment of the present invention includes:

[0035] The PET upright cotton is preformed to form a bottom layer 1;

[0036] Put the PU raw materials into the high-pressure tank;

[0037] Place the preformed PET upright cotton into the injection mold and close the mold;

[0038] The PU raw material in the high-pressure tank is injected into the upper surface of the PET upright cotton in the injection mold by closed mold injection to form a surface layer 2, and the pressure is maintained for a first preset time;

[0039] The bottom layer 1 and the surface layer 2 inside the injection mold are cooled and shaped.

[0040] Specifically, Figure 1 and Figure 2 As shown, the operator can cut the PET upright cotton of the corresponding area according to the required carpet area, and then pre-treat the PET upright cotton so that the PET upright cotton is pre-formed into the bottom layer 1. For example, after the pre-forming mold reaches a preset mold temperature, the PET upright cotton can be placed in the pre-forming mold for heating and pressurizing for a certain period of time to be molded into the bottom layer 1 of the automotive carpet 10.

[0041] Among them, PET upright cotton has the characteristics of high resilience and high compression resistance, so that the car carpet 10 can maintain good elasticity and softness during use, providing a comfortable stepping experience. At the same time, PET upright cotton has good softness, so that the car carpet 10 with PET upright cotton as the bottom layer 1 can adapt to the unevenness of the vehicle floor, and the car carpet 10 can be in uniform contact with the vehicle floor to ensure the support of the car carpet 10. In addition, compared with traditional sponges, the production process and pre-forming process of PET upright cotton belong to physical change processes, without the need to add chemical agents, and the product can be recycled and reused, without harming the environment. Therefore, the car carpet 10 with PET upright cotton as the bottom layer 1 and its production method have the advantage of environmental protection.

[0042] Furthermore, after the bottom layer 1 of the automotive carpet 10 is manufactured, the operator can put the raw materials for synthesizing PU into a high-pressure tank and mix them to form the required PU material for use in subsequent manufacturing steps. For example, isocyanate and polyol functional groups can be put into a high-pressure tank in a certain proportion and fully mixed to form a PU material with a required density. Then the operator can take the bottom layer 1 of the automotive carpet 10 formed by the PET upright cotton out of the pre-molding mold, transfer it into the injection mold when the injection mold reaches the preset mold temperature, and then close the mold to fix the bottom layer 1 of the automotive carpet 10 and prepare for the subsequent manufacturing steps.

[0043] After completing the above preparations, the staff can inject the mixed PU raw materials in the high-pressure tank into the upper surface of the PET upright cotton in the injection mold by closed mold injection to form a PU layer of a certain thickness, that is, to form a surface layer 2 on the upper surface of the bottom layer 1 of the automotive carpet 10. The bottom layer 1 and the surface layer 2 do not need to be compounded by gluing, laminating, etc., and the structural stability is higher and the molding process is more efficient. Then, after the injection is completed, the bottom layer 1 and the surface layer 2 are kept in the injection mold for the first preset time, so that the PU raw materials injected from the high-pressure tank to the upper surface of the PET upright cotton can fully flow to form a uniform surface, avoiding wrinkles in the local area of ​​the PU layer, thereby affecting the appearance of the product.

[0044] Furthermore, the operator can cool and shape the bottom layer 1 and the surface layer 2 that have been injected and held in the injection mold to form a carpet, and then take out the molded carpet and cut it according to the specific conditions of the vehicle to form a vehicle carpet 10.

[0045] It can be understood that the automotive carpet 10 processed by the above-mentioned manufacturing method has a two-layer structure of a bottom layer 1 and a surface layer 2. Through the injection molding process, a PU layer is injected on the upper surface of the bottom layer 1 formed by PET upright cotton to form the surface layer 2. The structure is simple, and the two-layer structure does not need to be compounded by processes such as gluing and laminating, nor does it need to be formed through multiple processes such as molding, roller coating, bonding and laminating, and needle punching. The process is simple and easy to produce, with lower energy consumption and carbon emissions, thereby reducing production costs. At the same time, the structural stability of the automotive carpet 10 can be higher and the production and molding can be more efficient.

[0046] Among them, the surface layer 2 formed by PU is wear-resistant, water-proof and dust-proof. The dirt on the surface of the surface layer 2 can be easily cleaned by wiping, so it has the effects of wear resistance, waterproof and easy cleaning. Compared with the current traditional PET felt carpet as the surface layer 2, it has the characteristics of being more resistant to dirt, easier to clean and more wear-resistant.

[0047] At the same time, the surface layer 2 is made of high-damping and vibration-reducing PU material, which itself has a good sound insulation effect, so that the vehicle carpet 10 no longer needs to add sound insulation films such as EPDM or EVA, which can not only reduce the types of materials required and simplify the processing process, but also achieve an environmental protection effect while ensuring the sound insulation effect of the vehicle carpet 10.

[0048] In addition, the automotive carpet 10 is directly compounded using an injection molding process, and no glue is used in the entire production process. Therefore, it has the characteristics of low odor and low VOC emissions. The production process and products are more environmentally friendly and can also enhance the user's comfort and experience.

[0049] According to the manufacturing method of the automotive carpet 10 of the embodiment of the present invention, the PET upright cotton is preformed to form a bottom layer 1, and then the PU raw material is placed in a high-pressure tank and the synthesized PU is injected into the upper surface of the PET upright cotton placed in the injection mold by closed mold injection to form a surface layer 2, and then after pressure holding, cooling and shaping, and cutting, a double-layer structure automotive carpet 10 with PET upright cotton as the bottom layer 1 and PU layer as the surface layer 2 can be formed. The structure and processing process are simple, the types of materials required are small, it is easy to produce and the production molding efficiency is high, which can reduce the production cost. The automotive carpet 10 made by the above-mentioned manufacturing method can not only ensure good elasticity and softness, provide a comfortable stepping experience, but also achieve the effects of wear resistance, waterproofness, easy cleaning, sound insulation, low odor, low VOC emission and environmental protection.

[0050] In some embodiments of the present invention, Figure 2 As shown, the PET upright cotton is preformed to form a bottom layer 1, which includes:

[0051] The PET upright cotton is placed in a preforming mold for molding to form a bottom layer 1, and the pressure is maintained for a second preset time.

[0052] It is understandable that compression molding can form the PET upright cotton material into precise shapes and sizes. A cavity is provided in the preforming mold. The PET upright cotton is placed in the cavity of the preforming mold and processed under high temperature and high pressure conditions. It can be molded into the required shape and size to form the bottom layer 1 of the automotive carpet 10. The molding efficiency is high and the loss of raw materials is small, which can improve production efficiency and reduce production costs. At the same time, the PET upright cotton needs to be kept under pressure in the preforming mold for a second preset time, which can ensure that after the preforming mold is closed, the PET upright cotton has enough time to fully fill the cavity of the preforming mold under the action of pressure, so that it reaches the expected density, thereby obtaining a high-quality product. The PET upright cotton can also be fully cooled in the preforming mold to avoid deformation and shrinkage of the bottom layer 1 formed in the preforming mold, so as to ensure the quality stability of the product.

[0053] In some embodiments of the present invention, Figure 2As shown, the mold temperature of the preforming mold is 70-80°C. If the mold temperature of the preforming mold is less than 70°C, the temperature is too low, and the fluidity of the molten PET upright cotton in the preforming mold becomes poor, which is not conducive to the full flow of the PET upright cotton and filling the cavity of the preforming mold, so that it is difficult to form the desired shape and size, and the speed of the PET upright cotton molding is also reduced. If the mold temperature of the preforming mold is greater than 80°C, the temperature is too high, and the preforming mold is affected by thermal expansion, which is easy to cause the size of the preforming mold to change and cause the PET upright cotton to curl, affecting the molding shape, reducing the processing accuracy, and even causing the preforming mold to fail, while increasing energy consumption. Controlling the mold temperature of the preforming mold within the range of 70-80°C can ensure the molding shape and molding speed of the PET upright cotton, improve the processing accuracy, and control the energy consumption within a reasonable range.

[0054] In some embodiments of the present invention, Figure 2 As shown, the second preset time is 2 to 3 minutes. If the second preset time is less than 2 minutes, the holding time of the PET upright cotton in the preforming mold is too short, and the PET upright cotton may not be able to fully fill the cavity of the preforming mold to achieve the expected shape and size, and the molding quality cannot be guaranteed. If the second preset time is greater than 3 minutes, the holding time of the PET upright cotton in the preforming mold is too long, which will increase the production cycle, thereby reducing production efficiency and increasing energy consumption. Controlling the second preset time to 2 to 3 minutes can not only ensure the molding quality of the PET upright cotton, but also ensure production efficiency and control energy consumption.

[0055] In some embodiments of the present invention, Figure 2 As shown, the PU raw material includes isocyanate and polyol functional groups. After the PU raw material is placed in a high-pressure tank, the method for making the automotive carpet 10 further includes:

[0056] Mix the isocyanate and polyol functional groups in a high pressure tank until uniform.

[0057] It is understandable that the operator can put the isocyanate and polyol functional groups into the high-pressure tank in a certain ratio so that the isocyanate and polyol functional groups can be fully mixed in the high-pressure tank. The operation process is simple and easy to implement, thereby obtaining a PU material of the required density, ensuring the performance of the PU, and further ensuring the wear resistance, waterproofness, sound insulation and other properties of the automotive carpet 10. Among them, the polyol functional group is a bio-based polyol, not extracted from a petroleum base or a chemical base, so the synthesized PU material and the automotive carpet 10 made of the PU material have the effect of low carbon and environmental protection.

[0058] In some embodiments of the present invention, Figure 2As shown in the figure, the mixing pressure of isocyanate and polyol functional groups in the high-pressure tank is 110-160 bar. If the mixing pressure is less than 110 bar, the mixing pressure in the high-pressure tank is too small, which may cause the isocyanate and polyol functional groups to be unable to be fully mixed or mixed unevenly, and thus the PU of the required density cannot be obtained. If the mixing pressure is greater than 160 bar, the mixing pressure in the high-pressure tank is too high, which will increase energy consumption and reduce the safety of the high-pressure tank itself. Therefore, controlling the mixing pressure at 110-160 bar can not only ensure that the isocyanate and polyol functional groups are fully mixed and evenly mixed in the high-pressure tank, but also control energy consumption and improve the safety factor of the high-pressure tank.

[0059] Preferably, the mixing pressure of isocyanate and polyol functional groups in the high-pressure tank is 130-150 bar, which can further ensure the sufficiency and uniformity of the mixing of isocyanate and polyol functional groups in the high-pressure tank, while further controlling energy consumption and improving the safety factor of the high-pressure tank.

[0060] In some embodiments of the present invention, Figure 2 As shown, the ratio of isocyanate and polyol functional groups is a, and a is 3.0:1 to 2.0:1, wherein the ratio of isocyanate and polyol functional groups is a mass fraction ratio. If a is greater than 3.0:1, the mixed material is too viscous and has poor fluidity, which is not conducive to the implementation of the subsequent injection process, and will cause the hardness of the synthesized PU material to be too hard, thereby affecting the installation and use of the automotive carpet 10. If a is less than 2.0:1, the mixed material is too thin, which will cause the hardness of the synthesized PU material to be too soft, thereby reducing the wear resistance of the automotive carpet 10. Controlling a within 3.0:1 to 2.0:1 can ensure that the viscosity of the mixed material is moderate, which is helpful for the implementation of the injection process, thereby ensuring the processing quality, and can obtain the PU material of the required density, thereby ensuring the wear resistance and use of the automotive carpet 10.

[0061] Preferably, the ratio of isocyanate to polyol functional groups is 2.5:1 to 2.0:1, which can further ensure that the mixed material has a moderate viscosity, improve the injection and processing quality, and more accurately obtain the PU material of the required density, thereby ensuring the wear resistance and usability of the automotive carpet 10.

[0062] In some embodiments of the present invention, Figure 2As shown in the figure, the mold temperature of the injection mold is 75-90℃. If the mold temperature of the injection mold is less than 75℃, the temperature is too low, and the fluidity of PU deteriorates during the injection process, which is not conducive to injecting PU onto the surface of PET upright cotton, and the quality of the PU layer cannot be guaranteed, and the injection speed is also reduced. If the mold temperature of the injection mold is greater than 90℃, the temperature is too high, and the injection mold is affected by thermal expansion, which can easily cause the size of the injection mold to change and cause the PET upright cotton to curl, affecting the injection molding shape, reducing the processing accuracy, and even causing the injection mold to fail, while increasing energy consumption. Controlling the mold temperature of the injection mold within the range of 75-90℃ allows PU to be better injected and combined onto the surface of the PET upright cotton, which can ensure the injection speed and injection quality of the PU layer, improve processing accuracy, and control energy consumption within a reasonable range.

[0063] In some embodiments of the present invention, Figure 2 As shown, the thickness of the surface layer 2 is 1.5 to 3.0 mm. If the thickness of the surface layer 2 is less than 1.5 mm, the thickness is too thin, which will affect the wear resistance and sound insulation effect of the PU layer; if the thickness of the surface layer 2 is greater than 3.0 mm, the thickness is too thick, which will cause the PU layer to be too hard, affecting the user's foot feel, and will also increase the occupied space in the thickness direction of the automotive carpet 10, making it inconvenient to assemble. Controlling the thickness of the surface layer 2 to 1.5 to 3.0 mm can ensure the wear resistance and sound insulation effect of the automotive carpet 10, as well as the stepping comfort and assembly convenience of the automotive carpet 10.

[0064] In some embodiments of the present invention, Figure 2 As shown, the first preset time is 3 to 5 minutes. If the first preset time is less than 3 minutes, the holding time of the closed mold injection process is too short, and the PU injected from the high-pressure tank to the upper surface of the PET upright cotton may not be able to fully flow to form a uniform surface. The PU layer may wrinkle in local areas, thereby affecting the appearance of the product and failing to ensure product quality. If the first preset time is greater than 5 minutes, the holding time of the closed mold injection process is too long, which will increase the production cycle, thereby reducing production efficiency and increasing energy consumption. Controlling the first preset time to 3 to 5 minutes can ensure that the PU injected into the upper surface of the PET upright cotton can fully flow to form a uniform surface to ensure product quality and product appearance, while ensuring production efficiency and controlling energy consumption.

[0065] In some embodiments of the present invention, Figure 2As shown, when the PU raw material in the high-pressure tank is injected into the upper surface of the PET upright cotton in the injection mold by closed mold injection, the injection flow rate of the high-pressure tank is 200-350g / s. If the injection flow rate of the high-pressure tank is less than 200g / s, it is easy to cause under-injection, so that part of the upper surface of the PET upright cotton is not covered by the PU layer, affecting the product quality and performance of the automotive carpet 10, and at the same time reducing the injection speed. If the injection flow rate of the high-pressure tank is greater than 350g / s, it is easy to cause the thickness of the PU injected from the high-pressure tank to the upper surface of the PET upright cotton to be uneven, affecting the product quality and appearance of the automotive carpet 10. Controlling the injection flow rate of the high-pressure tank at 200-350g / s can ensure that the thickness of the PU layer injected into the upper surface of the PET upright cotton is uniform, thereby ensuring the product quality and performance of the automotive carpet 10, and at the same time can also ensure the injection speed, thereby ensuring production efficiency.

[0066] In some embodiments of the present invention, Figure 2 As shown, the injection mold has 1 to 4 injection ports. It is understandable that the synthesized PU can be injected from the high-pressure tank to the upper surface of the PET upright cotton through the injection ports. Multiple injection ports can simultaneously inject material into the upper surface of the PET upright cotton in the injection mold, which can improve the injection efficiency and thus improve the production efficiency. However, if the injection mold has more than 4 injection ports, there are too many injection ports, which may easily produce too many material flow impact flow marks and welding marks, thus affecting the appearance. The injection mold has 2 to 4 injection ports, which can not only ensure the injection quality and product appearance, but also improve the injection efficiency and production efficiency.

[0067] Preferably, the injection mold has one injection port, which can avoid the generation of material flow impact flow marks and welding marks, thereby improving the injection quality and product quality, and also improving the appearance of the automotive carpet 10.

[0068] Next, a vehicle carpet 10 according to an embodiment of the present invention will be described.

[0069] The automotive carpet 10 according to the embodiment of the present invention is composed of a surface layer 2 and a bottom layer 1 stacked in layers.

[0070] Specifically, Figure 1 and Figure 2As shown, the surface layer 2 is a PU layer, and the bottom layer 1 is a PET layer. Among them, the PET upright cotton has the characteristics of high resilience and high compression resistance, so that the automotive carpet 10 can maintain good elasticity and softness during use, providing a comfortable stepping experience. At the same time, the PET upright cotton has good softness, so that the automotive carpet 10 with PET upright cotton as the bottom layer 1 can adapt to the unevenness of the vehicle floor, and the automotive carpet 10 can be in uniform contact with the vehicle floor to ensure the support of the automotive carpet 10. In addition, compared with traditional sponges, the production process and pre-forming process of PET upright cotton belong to physical change processes, without the need to add chemical agents, and the product can be recycled and reused, without harming the environment. Therefore, the automotive carpet 10 with PET upright cotton as the bottom layer 1 and its production method have the advantage of environmental protection.

[0071] In addition, the surface layer 2 formed by PU is wear-resistant, water-proof and dust-proof. The dirt on the surface of the surface layer 2 can be easily cleaned by wiping, etc., so it has the effects of wear resistance, waterproof and easy cleaning. Compared with the current traditional PET felt carpet as the surface layer 2, it has the characteristics of being more resistant to dirt, easier to clean and more wear-resistant.

[0072] At the same time, the surface layer 2 is made of high-damping and vibration-reducing PU material, which itself has a good sound insulation effect, so that the vehicle carpet 10 no longer needs to add sound insulation films such as EPDM or EVA, which can not only reduce the types of materials required and simplify the processing process, but also achieve an environmental protection effect while ensuring the sound insulation effect of the vehicle carpet 10.

[0073] Furthermore, the manufacturing method of the automotive carpet 10 is as follows: the operator can cut the PET upright cotton of the corresponding area according to the required carpet area, and then pre-treat the PET upright cotton so that the PET upright cotton is pre-formed into the bottom layer 1. For example, the PET upright cotton can be placed in a preforming mold and heated and pressurized for a certain period of time to be molded into the bottom layer 1 of the automotive carpet 10.

[0074] After the bottom layer 1 of the automotive carpet 10 is manufactured, the operator can put the raw materials for synthesizing PU into a high-pressure tank and mix them to form the required PU material for use in subsequent manufacturing steps. For example, isocyanate and polyol functional groups can be put into a high-pressure tank in a certain proportion and fully mixed to form a PU material with a required density. Then the operator can take the bottom layer 1 of the automotive carpet 10 formed by the PET upright cotton out of the pre-molding mold, transfer it into the injection mold and close the mold to fix the bottom layer 1 of the automotive carpet 10 and prepare for the subsequent manufacturing steps.

[0075] After completing the above preparations, the staff can inject the mixed PU raw materials in the high-pressure tank into the upper surface of the PET upright cotton in the injection mold by closed mold injection to form a PU layer of a certain thickness, that is, to form a surface layer 2 on the upper surface of the bottom layer 1 of the automotive carpet 10. The bottom layer 1 and the surface layer 2 do not need to be compounded by gluing, laminating, etc., and the structural stability is higher and the molding process is more efficient. Then, after the injection is completed, the bottom layer 1 and the surface layer 2 are kept in the injection mold for the first preset time, so that the PU raw materials injected from the high-pressure tank to the upper surface of the PET upright cotton can fully flow to form a uniform surface, avoiding wrinkles in the local area of ​​the PU layer, thereby affecting the appearance of the product.

[0076] Furthermore, the operator can cool and shape the bottom layer 1 and the surface layer 2 that have been injected and held in the injection mold to form a carpet, and then take out the molded carpet and cut it according to the specific conditions of the vehicle to form a vehicle carpet 10.

[0077] It can be understood that the automotive carpet 10 processed by the above-mentioned manufacturing method has a two-layer structure of a bottom layer 1 and a surface layer 2. Through the injection molding process, a PU layer is injected on the upper surface of the bottom layer 1 formed by PET upright cotton to form the surface layer 2. The structure is simple, and the two-layer structure does not need to be compounded by processes such as gluing and laminating, nor does it need to be formed through multiple processes such as molding, roller coating, bonding and laminating, and needle punching. The process is simple and easy to produce, with lower energy consumption and carbon emissions, thereby reducing production costs. At the same time, the structural stability of the automotive carpet 10 can be higher and the production and molding can be more efficient.

[0078] In addition, the automotive carpet 10 is directly compounded using an injection molding process, and no glue is used in the entire production process. Therefore, it has the characteristics of low odor and low VOC emissions. The production process and products are more environmentally friendly and can also enhance the user's comfort and experience.

[0079] According to the automotive carpet 10 of the embodiment of the present invention, the automotive carpet 10 is composed of a PU layer surface layer 2 and a PET layer bottom layer 1 stacked by the above-mentioned manufacturing method, and the structure and processing process are simple, which can not only ensure good elasticity and softness, provide a comfortable stepping experience, but also achieve the effects of wear resistance, waterproofness, easy cleaning, sound insulation, low odor, low VOC emission and environmental protection. In addition, the types of materials required to make the automotive carpet 10 are small, easy to produce and high in production and molding efficiency, which can reduce production costs.

[0080] In some embodiments of the present invention, Figure 2As shown, the density of the PU layer is 1.05-1.15 g / cm3, which can ensure the sound insulation and noise reduction effect of the PU layer and avoid the PU layer being too heavy, thereby ensuring the sound insulation and lightness of the automotive carpet 10.

[0081] In some embodiments of the present invention, Figure 2 As shown, the density of the PET layer is 540-660 g / m3, which can ensure the elasticity and softness of the PET layer and avoid the PET layer being too heavy, thereby ensuring the comfort and lightness of the automotive carpet 10.

[0082] In some embodiments of the present invention, Figure 2 As shown, the hardness of the PU layer is 60-90HA, wherein the hardness of the PU layer is based on the Shore A hardness, that is, the hardness of the PU layer is (Shore A) 60-90. This can ensure the wear resistance of the automotive carpet 10 and the user's comfort.

[0083] In some embodiments of the present invention, Figure 2 As shown, the thickness of the surface layer 2 is 1.5 to 3.0 mm. If the thickness of the surface layer 2 is less than 1.5 mm, the thickness is too thin, which will affect the wear resistance and sound insulation effect of the PU layer; if the thickness of the surface layer 2 is greater than 3.0 mm, the thickness is too thick, which will cause the PU layer to be too hard, affecting the user's foot feel, and will also increase the occupied space in the thickness direction of the automotive carpet 10, making it inconvenient to assemble. Controlling the thickness of the surface layer 2 to 1.5 to 3.0 mm can ensure the wear resistance and sound insulation effect of the automotive carpet 10, as well as the stepping comfort and assembly convenience of the automotive carpet 10.

[0084] Other components of the automotive carpet 10 according to the embodiment of the present invention, such as isocyanate and polyol functional groups for synthesizing PU, are well known to those skilled in the art and will not be described in detail herein.

[0085] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.

[0086] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.

Claims

1. A method for manufacturing a vehicle carpet, characterized in that: include: The PET upright cotton is preformed to form a bottom layer; Put the PU raw materials into the high-pressure tank; Put the preformed PET upright cotton into the injection mold and close the mold; The PU raw material in the high-pressure tank is injected into the upper surface of the PET upright cotton in the injection mold by closed mold injection to form a surface layer, and the pressure is maintained for a first preset time; The bottom layer and the surface layer inside the injection mold are cooled and shaped.

2. The method for manufacturing a vehicle carpet according to claim 1, characterized in that: The preforming of the PET upright cotton to form a bottom layer comprises: The PET upright cotton is placed in a preforming mold for molding to form a bottom layer, and the pressure is maintained for a second preset time.

3. The method for manufacturing a vehicle carpet according to claim 2, characterized in that: The mold temperature of the preforming mold is 70-80°C.

4. The method for manufacturing a vehicle carpet according to claim 2, characterized in that: The second preset time is 2 to 3 minutes.

5. The method for manufacturing a vehicle carpet according to claim 1, characterized in that: The PU raw material includes isocyanate and polyol functional groups. After the PU raw material is placed in a high-pressure tank, the method for making the automotive carpet further includes: The isocyanate and the polyol functional group are mixed uniformly in the high pressure tank.

6. The method for manufacturing a vehicle carpet according to claim 5, characterized in that: The mixing pressure of the isocyanate and the polyol functional group in the high-pressure tank is 110 to 160 bar.

7. The method for manufacturing a vehicle carpet according to claim 5, characterized in that: The ratio of the isocyanate to the polyol functional group is 3.0:1 to 2.0:

1.

8. The method for manufacturing a vehicle carpet according to claim 1, characterized in that: The mold temperature of the injection mold is 75-90°C.

9. The method for manufacturing a vehicle carpet according to claim 1, characterized in that: The thickness of the surface layer is 1.5 to 3.0 mm.

10. The method for manufacturing a vehicle carpet according to claim 1, characterized in that: The first preset time is 3 to 5 minutes.

11. The method for manufacturing a vehicle carpet according to claim 1, characterized in that: When the PU raw material in the high-pressure tank is injected onto the upper surface of the PET upright cotton in the injection mold by closed mold injection, the injection flow rate of the high-pressure tank is 200-350 g / s.

12. The method for manufacturing a vehicle carpet according to claim 1, characterized in that: The injection mold has 1 to 4 injection ports.

13. A vehicle carpet, characterized in that: The invention is composed of a surface layer and a bottom layer stacked together, wherein the surface layer is a PU layer and the bottom layer is a PET layer.

14. The automotive carpet according to claim 13, characterized in that: The density of the PU layer is 1.05-1.15 g / cm 3 ; And / or, the density of the PET layer is 540-660 g / m 3 ; And / or, the hardness of the PU layer is 60-90HA; And / or, the thickness of the surface layer is 1.5 to 3.0 mm.