Mixed bed resin for hydrogen fuel cell vehicle and preparation method thereof
The preparation of hydrogen fuel cell vehicle mixed bed resin with reasonable crosslinking and particle size through suspension polymerization method solves the problem that the male resin is not fully utilized after the consumption of the female resin, extends the service life of the ion exchanger and improves the resources Utilization.
Patent Information
- Application Number
- CN202411400525.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-09
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-10-09
AI Technical Summary
In the existing hydrogen fuel cell system, after the anode resin is consumed, the anode resin is not fully utilized, resulting in the early scrapping of the overall ion exchanger, resulting in waste of resources and degradation of the system insulation performance.
Styrene-based gel-type strong acid and alkali-negative resin with reasonable crosslinking degree and particle size were prepared by suspension polymerization, and mixed at a ratio of 1:4 to form a hydrogen fuel cell vehicle mixed bed resin to prolong ion exchange The service life of the device.
It extends the service life of the ion exchanger, reduces the waste of positive resin, and improves the insulation performance and resource utilization of the system.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of fuel cell cooling systems, in particular to a mixed bed resin for hydrogen fuel cell vehicles and a preparation method thereof. Background Art
[0002] As a green energy, hydrogen meets the demand for zero-carbon energy emission. Hydrogen fuel cell (PEMFC) vehicles are vehicles that use hydrogen and oxygen to produce electrochemical reactions to release electrical energy for driving. Due to the characteristics of its structure and working principle, the hydrogen fuel cell system will generate a lot of heat during operation. Because the temperature is too high or too low, the performance of the hydrogen fuel cell system will be reduced. Therefore, the hydrogen fuel cell system needs to be equipped with a thermal management system module to ensure that the hydrogen fuel cell system works at an appropriate temperature. In the application of high-power hydrogen fuel cell commercial vehicles, the system adopts a water circulation thermal management control method, but when the fuel cell system is running, the pipelines and some components in the system will precipitate ions, which will increase the conductivity of the water circulation coolant. At this time, a high voltage is generated on the bipolar plate of the battery stack, which will be transmitted to the entire cooling circulation flow channel through the coolant. If the conductivity of the coolant is too high, the working mode under high voltage will reduce the insulation performance of the entire system and affect the safety performance of the vehicle. Therefore, an ion exchanger with a built-in mixed bed resin is currently installed in the cooling circulation system to reduce the conductivity of the coolant to maintain the normal operation of the fuel cell system.
[0003] At present, after the hydrogen fuel cell car is running, the personnel analyzed the mixed bed resin inside the replaced ion exchanger and found that the anion resin has been completely consumed, but the cation resin still has more than 60% of the exchange capacity that has not been consumed. According to the characteristics of the mixed bed resin, once a single resin is ineffective, the overall mixed bed resin can no longer reduce the conductivity of the fuel cell coolant, which reduces the insulation performance of the battery system. Therefore, it is necessary to replace the ion exchanger in the battery cooling system as a whole, resulting in a huge waste of material costs. Summary of the invention
[0004] The purpose of the present invention is to overcome the disadvantages in the prior art that the anionic resin in the ion exchanger of the battery stack system is completely consumed while the cationic resin is not consumed in large quantities, and to provide a mixed bed resin for hydrogen fuel cell vehicles and a preparation method thereof.
[0005] The purpose of the present invention is achieved through the following technical solution: A method for preparing a mixed bed resin for a hydrogen fuel cell vehicle comprises the following steps: S1. The styrene and divinylbenzene are produced by suspension polymerization to obtain styrene-divinylbenzene copolymer white balls, the obtained white balls are sulfonated using H2SO4, and the crosslinking degree of 10%, the particle size of 0.525mm, and the wet apparent density of 0.75-0.85g / ml of styrene-based gel-type strong acid cationic resin are obtained by changing the ratio of styrene and divinylbenzene components; S2. Using styrene and divinylbenzene to produce styrene-divinylbenzene copolymer white balls by suspension polymerization, immersing the obtained white balls in chloromethylation raw materials, and then preparing chlorine balls under the action of chloromethylation catalyst, and then placing the obtained chlorine balls in a reactor, and sequentially undergoing swelling with a swelling agent, reaction with an alkyl tertiary amine and washing with pure water, and obtaining a styrene-based gel-type strong base anionic resin with a crosslinking degree of 7%, a particle size of 0.63 mm, and a wet apparent density of 0.67-0.72 g / ml by changing the ratio of styrene and divinylbenzene components; S3. Mix and fill the prepared strong acid cation resin and strong base anion resin in a volume ratio of 1:4.
[0006] Preferably, the suspension polymerization method is carried out according to the following steps: styrene, divinylbenzene and an initiator are added to a reaction system, and pure water, an organic dispersant, an auxiliary crosslinking agent and an inhibitor are added to fully carry out suspension polymerization, adjust the pH, and wash the product with water until it is neutral, thereby obtaining the styrene-divinylbenzene copolymer white ball.
[0007] Preferably, the initiator is one or more of benzoyl peroxide, azobisisobutyronitrile, isopropylbenzene hydroperoxide, and lauroyl peroxide; the organic dispersant is one or more of polyvinyl alcohol, gelatin, starch, methyl cellulose, and derivatives thereof; the auxiliary crosslinking agent is acrylonitrile; and the inhibitor is methylene blue.
[0008] Preferably, the chloromethylation raw material is paraformaldehyde, formaldehyde aqueous solution, methylal dimethanol, chloromethyl ether, dichloromethyl ether, or chlorosulfonic acid.
[0009] Preferably, the chloromethylation catalyst is one or more of zinc chloride or ferric chloride.
[0010] Preferably, the swelling agent is one or more of ethylene dichloride, carbon tetrachloride, benzene, and dichloroethane.
[0011] Preferably, the tertiary alkyl amine is trimethylamine.
[0012] The present invention also aims to provide a mixed bed resin for hydrogen fuel cell vehicles prepared according to the above method.
[0013] The present invention has the following advantages: the cross-linking degree of the resin determines the volume exchange capacity in the resin, and the volume exchange capacity can be increased by increasing the ratio of the anionic and cation resins. However, the cross-linking degree of the resin cannot be increased infinitely, and the particle size and pore size of the resin must be comprehensively considered. By reasonably selecting the cross-linking degree of the anionic and cation resins, not only the volume exchange capacity in the anionic and cation resins is increased, but also ion exchange is facilitated. At the same time, the mixed bed ratio of the anionic and cation resins is controlled to avoid the occurrence of a single resin being consumed in large quantities in advance, resulting in the overall scrapping of the ion exchanger, thereby extending the service life of the ion exchanger. DETAILED DESCRIPTION
[0014] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in combination with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments.
[0015] A mixed bed resin for a hydrogen fuel cell vehicle is prepared according to the following method, comprising the following steps: S1. Add 90% styrene, 10% divinylbenzene and 1% initiator benzoyl peroxide to the reaction system, add pure water, 0.5% organic dispersant polyvinyl alcohol, 1% auxiliary crosslinking agent acrylonitrile, and 0.1% inhibitor methylene blue, fully carry out suspension polymerization, adjust the pH, and wash the product to neutrality to obtain the styrene-divinylbenzene copolymer white ball, and sulfonate the obtained white ball using H2SO4 to obtain a styrene-based gel-type strong acid cationic resin with a crosslinking degree of 10%, an average particle size of 0.525 mm, and a wet apparent density of 0.75-0.85 g / ml; S2. 93% styrene, 7% divinylbenzene and 1% initiator benzoyl peroxide are added to the reaction system, and pure water, 0.5% organic dispersant polyvinyl alcohol, 1% auxiliary crosslinking agent acrylonitrile and 0.1% inhibitor methylene blue are added to fully carry out suspension polymerization, adjust the pH, wash the product to neutrality, and obtain the styrene-divinylbenzene copolymer white ball, immerse the obtained white ball in 400% chloromethyl ether, and then obtain a chlorine ball under the action of 50% chloromethylation catalyst ferric chloride, and then place the obtained chlorine ball in a reactor, and successively undergo swelling with a swelling agent ethylene dichloride, reaction with a trimethylamine solution and washing with pure water to obtain a styrene-based gel-type strong crosslinking degree of 7%, an average particle size of 0.63mm and a wet apparent density of 0.67-0.72g / ml; S3. Mix and fill the prepared strong acid cation resin and strong base anion resin in a volume ratio of 1:4.
[0016] In the process of preparing styrene-divinylbenzene copolymer white balls, in addition to benzoyl peroxide, other azo initiators or peroxide initiators can also be used as initiators, including azobisisobutyronitrile, isopropylbenzene hydroperoxide, and lauroyl peroxide. In addition to polyvinyl alcohol, gelatin, starch, methyl cellulose and its derivatives can also be used as organic dispersants. In the step of chloromethylation of white balls, in addition to chloromethyl ether, other chloromethylation raw materials can also be used for reaction, including polyformaldehyde, formaldehyde aqueous solution, methylal dimethanol, dichloromethyl ether, and chlorosulfonic acid. At the same time, the chloromethylation catalyst ferric chloride can also be replaced by zinc chloride. In addition to ethylene dichloride, carbon tetrachloride, benzene, and dichlorocyclopentane can also be used as swelling agents.
[0017] In the existing mixed bed ratios on the market, the volume exchange capacity of cation resins is between 2.0-2.5, and the volume exchange capacity of anion resins is between 1.0-1.2. Therefore, in order to ensure that the mixed bed resin has a 1:1 stoichiometric equivalent of cation and anion exchange capacity, the mixed bed ratio between cation resins and anion resins is usually between 1:1.5-1:3. Mixed bed ratios of 1:1.5 and 1:2 were selected for comparative experiments.
[0018] Comparative Example 1 A 1:1.5 mixed bed resin for hydrogen fuel cell vehicles, wherein the strong acid cation resin is selected to have a crosslinking degree of 12%, an average particle size of 0.65 mm, and a wet apparent density of 0.77-0.79 g / ml, and the strong base anion resin is selected to have a crosslinking degree of 10%, an average particle size of 0.55 mm, and a wet apparent density of 0.67-0.72 g / ml.
[0019] Comparative Example 2 A 1:2 mixed bed resin for hydrogen fuel cell vehicles, wherein the strong acid cation resin is selected to have a crosslinking degree of 10%, an average particle size of 0.65 mm, and a wet apparent density of 0.77-0.79 g / ml, and the strong base anion resin is selected to have a crosslinking degree of 7%, an average particle size of 0.55 mm, and a wet apparent density of 0.67-0.72 g / ml.
[0020] The mixed bed resins of the above embodiment and comparative examples 1 and 2 were mixed and placed on a sports car for actual experiments. The vehicle ran at an average speed of 50 km / h. The test results are shown in the following table.
[0021] Ratio (Yang:Yin) result Example 1:4 After 400h (17 days) of testing, the anion resin had a remaining OH- conversion rate of 86.64%, and the cation resin had a remaining H+ conversion rate of 99.08%. After 900h of operation, the cation resin had a remaining 19.81% and the anion resin had a remaining 0%. Comparative Example 1 1:1.5 After running for 200 hours, the remaining amount of cation resin was 94.79% and the remaining amount of anion resin was 0%. Comparative Example 2 1:2 After running for 400 hours, the cation resin remained 84.12% and the anion resin remained 0%. It can be seen from the above table that when the single-component anion resin is used up, the improved mixed bed resin has only 19.81% of the cation resin remaining after the equipment is operated, compared with the mixed bed resin of the control ratio, reducing the waste of cation resin by 74.98%. At the same time, the operating time is extended from the original 200h to 900h, greatly increasing the service life of the equipment.
[0022] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for preparing a mixed bed resin for a hydrogen fuel cell vehicle, characterized in that: The following steps are included: S1. The styrene and divinylbenzene are produced by suspension polymerization to obtain styrene-divinylbenzene copolymer white balls, the obtained white balls are sulfonated using H2SO4, and the crosslinking degree of 10%, the particle size of 0.525mm, and the wet apparent density of 0.75-0.85g / ml of styrene-based gel-type strong acid cationic resin are obtained by changing the ratio of styrene and divinylbenzene components; S2. Using styrene and divinylbenzene to produce styrene-divinylbenzene copolymer white balls by suspension polymerization, immersing the obtained white balls in chloromethylation raw materials, and then preparing chlorine balls under the action of chloromethylation catalyst, and then placing the obtained chlorine balls in a reactor, and sequentially undergoing swelling with a swelling agent, reaction with an alkyl tertiary amine and washing with pure water, and obtaining a styrene-based gel-type strong base anionic resin with a crosslinking degree of 7%, a particle size of 0.63 mm, and a wet apparent density of 0.67-0.72 g / ml by changing the ratio of styrene and divinylbenzene components; S3. Mix and fill the prepared strong acid cation resin and strong base anion resin in a volume ratio of 1:
4.
2. The method for preparing a mixed bed resin for a hydrogen fuel cell vehicle according to claim 1, characterized in that: The suspension polymerization method is carried out according to the following steps: styrene, divinylbenzene and an initiator are added to a reaction system, and pure water, an organic dispersant, an auxiliary crosslinking agent and an inhibitor are added to fully carry out suspension polymerization, adjust the pH, and wash the product with water until it is neutral, so as to obtain the styrene-divinylbenzene copolymer white ball.
3. The method for preparing a mixed bed resin for a hydrogen fuel cell vehicle according to claim 2, characterized in that: The initiator is one or more of benzoyl peroxide, azobisisobutyronitrile, isopropylbenzene hydroperoxide and lauroyl peroxide; the organic dispersant is one or more of polyvinyl alcohol, gelatin, starch, methyl cellulose and derivatives thereof; the auxiliary crosslinking agent is acrylonitrile; and the inhibitor is methylene blue.
4. The method for preparing a mixed bed resin for a hydrogen fuel cell vehicle according to claim 1, characterized in that: The chloromethylation raw materials are paraformaldehyde, formaldehyde aqueous solution, methylal dimethanol, chloromethyl ether, dichloromethyl ether and chlorosulfonic acid.
5. The method for preparing a mixed bed resin for a hydrogen fuel cell vehicle according to claim 1, characterized in that: The chloromethylation catalyst is one or more of zinc chloride or ferric chloride.
6. The method for preparing a mixed bed resin for a hydrogen fuel cell vehicle according to claim 1, characterized in that: The swelling agent is one or more of ethylene dichloride, carbon tetrachloride, benzene and dichloroethane.
7. The method for preparing a mixed bed resin for a hydrogen fuel cell vehicle according to claim 1, characterized in that: The tertiary alkyl amine is trimethylamine.
8. A mixed bed resin for hydrogen fuel cell vehicles prepared according to a method according to any one of claims 1 to 7.
Citation Information
Patent Citations
Process for synthesizing powdered ion-exchange resin
CN102557191A
Gel-type strong-base anion exchange resin
CN105367689A
Preparation method for gel-type strongly-alkaline anion exchange resin
CN105418819A
Strong-alkality anion exchange resin for amphoteric homogeneous mixed bed and preparation method of strong-basicity anion exchange resin
CN113814006A
Method for preparing cinnamene copolymerization homogeneous resin and its preparing method
CN1431233A